A reference electrode and a three-electrode cell and a three-electrode battery including the reference electrode.
By using porous copper wires as a flat reference electrode, the problem of lithium-ion diffusion obstruction in lithium-ion batteries is solved, enabling accurate measurement of negative electrode potential and reducing the risk of lithium plating, thereby improving battery safety and testing accuracy.
Patent Information
- Application Number
- CN202522330842.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-11-03
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2035-11-03
AI Technical Summary
In existing lithium-ion batteries, the design of the reference electrode hinders lithium-ion diffusion and migration, leading to inaccurate negative electrode potential measurement and the potential for lithium plating. Current technologies cannot effectively solve this problem.
A porous copper wire is used as the reference electrode, designed with a flat structure, and a membrane is placed between the positive and negative electrodes. A lithium deposition layer is attached to the surface of the porous copper wire, providing additional lithium ion transport channels to ensure the uniformity and safety of lithium deposition.
It improves the accuracy of negative electrode potential measurement, reduces the risk of lithium plating, and enhances battery safety and testing accuracy.
Smart Images

Figure CN224986262U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of electrode technology, and in particular to a reference electrode and a three-electrode cell and a three-electrode battery including the reference electrode. Background Technology
[0002] During the charging and discharging process of lithium-ion batteries, if the negative electrode potential falls below the lithium deposition potential, lithium plating may occur, causing capacity decay and even safety risks. Therefore, accurate monitoring of this potential has become a core requirement for battery development and service evaluation.
[0003] Existing technology involves embedding bare copper wires between the positive and negative electrodes, followed by low-current lithium plating to form a Li / Cu reference electrode. While this method is simple and inexpensive, the cylindrical copper wires create columnar barriers between the electrodes, hindering the flow of Li into the surrounding electrolyte. + The diffusion and migration of lithium lead to uneven distribution of local liquid phase current density, and the measured negative electrode potential generally deviates from the true value, making it easy to misjudge the lithium deposition critical point. In order to avoid short circuit between the reference electrode and the electrode, a separator must be added to both sides of the copper wire, which prolongs the ion transport path and increases the equivalent series impedance, further amplifying the potential measurement error. If the diameter of the copper wire is reduced to reduce interference, it will break under the stress of winding, liquid injection and cyclic expansion due to insufficient mechanical strength, and the thickness of the separator is already close to the physical limit and cannot be further reduced. The uniformity of lithium plating on the surface of the solid smooth copper wire is poor, and the dendrites preferentially deposited at the edges may pierce the separator, bringing additional hidden dangers.
[0004] Therefore, there is an urgent need for a reference electrode and a three-electrode cell and a three-electrode battery that include it. Utility Model Content
[0005] The present invention aims to overcome the shortcomings of the prior art, and therefore adopts the following technical solution: The first aspect of this utility model is to provide a reference electrode, comprising: a porous copper wire; wherein... The porous copper wire is disposed between the positive and negative electrodes of the three-electrode cell, and a first diaphragm is disposed between the positive electrode and the porous copper wire, and a second diaphragm is disposed between the porous copper wire and the negative electrode. The porous copper wire has a flat structure, and the flat structure has a first dimension along the height direction of the positive electrode and a second dimension along the width direction of the positive electrode, wherein the ratio of the first dimension to the second dimension does not exceed 0.3.
[0006] Preferably, the first size is 15μm-30μm.
[0007] Preferably, the second dimension is 120μm-240μm.
[0008] Preferably, the porosity of the porous copper wire is 10%-50%.
[0009] Preferably, the pore size of the porous copper wire is 0.6μm-6μm.
[0010] Preferably, it further includes: a lithium deposition layer; The lithium deposition layer is attached to the outer surface of the porous copper wire.
[0011] A second aspect of this utility model is to provide a three-electrode battery cell, comprising: a reference electrode, a positive electrode, a negative electrode, a first separator, and a second separator as described above; wherein, The reference electrode is disposed between the positive electrode and the negative electrode, the first diaphragm is disposed between the positive electrode and the reference electrode, and the second diaphragm is disposed between the reference electrode and the negative electrode.
[0012] Preferably, the positive electrode comprises: a positive electrode current collector and a positive electrode active layer; wherein, The positive electrode active layer is disposed on the surface of the positive electrode current collector.
[0013] Preferably, the negative electrode comprises: a negative electrode current collector and a negative electrode active layer; wherein, The negative electrode active layer is disposed on the surface of the negative electrode current collector.
[0014] A third aspect of this utility model is to provide a three-electrode battery, comprising: a three-electrode cell, an electrolyte, and a casing as described above; wherein, The three-electrode battery cell and the electrolyte are both disposed inside the housing, and the three-electrode battery cell is immersed in the electrolyte.
[0015] Compared with the prior art, the beneficial effects of this utility model are reflected in: The reference electrode of this invention has a flat structure, and the thickness space occupied by the reference electrode between the electrode sheets is significantly compressed, allowing the electrolyte to flow simultaneously on the upper and lower surfaces and within the internal pores of the reference electrode. + The concentration gradient is quickly smoothed out, the liquid phase current distribution tends to be uniform, and the negative electrode potential reading no longer drifts due to local concentration differences, thus significantly improving the test accuracy. Attached Figure Description
[0016] Figure 1 This is an isometric structural diagram of the three-electrode battery in this utility model; Figure 2 This is a cross-sectional view of the three-electrode battery cell in this utility model. The reference numerals in the figures include: Reference electrode 1; positive electrode 2; negative electrode 3; first diaphragm 4; second diaphragm 5; height direction H; width direction W. Detailed Implementation
[0017] The specific embodiments of this utility model will be described in detail below.
[0018] Unless otherwise defined, the technical or scientific terms used in the claims and description shall have the ordinary meaning as understood by one of ordinary skill in the art to which this utility model pertains.
[0019] The word "comprising" or similar terms used in this utility model patent application specification and claims mean that the objects preceding "comprising" include the objects listed after "comprising" or their equivalents, and do not exclude other objects.
[0020] The numerical values mentioned in this invention include all values increasing one unit at a time from low to high, assuming that there is at least a two-unit interval between any lower and higher value. For example, if a component quantity or a physical quantity is said to be better from 1 to 100, 10 to 90, and 20 to 80, it means that values such as 5 to 95, 14 to 76, 23 to 67, 32 to 58, and 41 to 49 are clearly listed in this specification; for values less than 1, 0.0001, 0.001, 0.01, or 0.1 are considered suitable units. The foregoing examples are for illustrative purposes only; in practice, all combinations of values between the lowest and highest listed values are considered to be clearly listed in this specification in a similar manner.
[0021] Example 1 This embodiment provides a reference electrode 1, comprising: a porous copper wire and a lithium deposition layer; wherein... The porous copper wire is disposed between the positive electrode 2 and the negative electrode 3 of the three-electrode cell, and a first diaphragm 4 is disposed between the positive electrode 2 and the porous copper wire, and a second diaphragm 5 is disposed between the porous copper wire and the negative electrode 3. The porous copper wire has a flat structure, and the flat structure has a first dimension along the height direction H of the positive electrode 2 and a second dimension along the width direction W of the positive electrode 2. The ratio of the first dimension to the second dimension does not exceed 0.3. The porosity of the porous copper wire is 10%-50%, and the pore diameter of the porous copper wire is 0.6μm-6μm. The lithium deposition layer is attached to the outer surface of the porous copper wire. The pores inside the porous copper wire provide additional transport channels for lithium ions. During lithium plating, the deposition surface expands from a single outer wall to the entire three-dimensional surface. The lithium deposition layer grows uniformly and densely, avoiding local protrusions and dendrite problems, while reducing the polarization of the reference electrode itself.
[0022] In some preferred embodiments, the flat structure has a rectangular cross-section, which works in conjunction with the porous skeleton to form a continuous micro-truss structure. This significantly improves the flexibility and bending resistance of the porous copper wire, making it less prone to breakage during winding, stacking, and subsequent cyclic expansion, and its reliability is superior to that of traditional thin cylindrical copper wire.
[0023] In some preferred embodiments, the first size is 15μm-30μm and the second size is 120μm-240μm.
[0024] In some preferred embodiments, the first dimension is 15 μm and the second dimension is 240 μm.
[0025] In some preferred embodiments, the first dimension is 30 μm and the second dimension is 120 μm.
[0026] Example 2 like Figure 2 As shown, this embodiment provides a three-electrode battery cell, including: a reference electrode 1, a positive electrode 2, a negative electrode 3, a first separator 4, and a second separator 5 as described in Embodiment 1; wherein, The reference electrode 1 is disposed between the positive electrode 2 and the negative electrode 3, the first diaphragm 4 is disposed between the positive electrode 2 and the reference electrode 1, and the second diaphragm 5 is disposed between the reference electrode 1 and the negative electrode 3; The positive electrode 2 includes: a positive electrode current collector and a positive electrode active layer; The positive electrode active layer is disposed on the surface of the positive electrode current collector; The negative electrode 3 includes: a negative electrode current collector and a negative electrode active layer; The negative electrode active layer is disposed on the surface of the negative electrode current collector.
[0027] In some preferred embodiments, the ratio of the first dimension to the height of the positive electrode 2 or the negative electrode 3 does not exceed 0.5.
[0028] Example 3 like Figure 1 As shown, this embodiment provides a three-electrode battery, including: a three-electrode cell as described in Embodiment 2, an electrolyte, and a casing; wherein, The three-electrode battery cell and the electrolyte are both disposed inside the housing, and the three-electrode battery cell is immersed in the electrolyte.
[0029] This embodiment also provides a method for potential monitoring and lithium plating analysis using the three-electrode battery as described above, the steps of which include: S1. Prepare porous copper wires with uniformly distributed porous structure. The pore diameter and porosity are selected according to actual needs. The first and second dimensions of the porous copper wires are determined based on the cell size and testing requirements. Also prepare positive electrode, negative electrode, separator and electrolyte according to the normal cell manufacturing process. S2. According to the requirements of cell stacking operation, place the negative electrode, separator, and positive electrode in sequence to ensure the correct stacking order and maintain the stability of the cell structure; clean and degrease the porous copper wires to ensure surface cleanliness and activity; place the treated porous copper wires between the positive and negative electrode tabs and fix them with tape to prevent displacement; after the stacking is completed, perform encapsulation, electrolyte injection and formation, with process parameters consistent with conventional cells; S3. The completed battery cell is adjusted to the predetermined charging state through a charging and discharging device, which can be achieved by constant current or constant voltage. Electrochemical lithium deposition is performed on the surface of the porous copper wire: constant current charging at a small rate is used to control the current and time so that the lithium deposition layer is deposited uniformly, and a lithium deposition layer with uniform thickness and complete coverage is obtained to form a reference electrode. S4. Place the three-electrode cell in the charge / discharge machine, connecting the positive, negative, and reference electrodes to their respective channels, ensuring a secure connection. Conduct tests under different charge / discharge rates and temperatures, acquiring and recording the potential changes between the positive and negative electrodes, the positive and reference electrodes, and the negative and reference electrodes in real time. Based on the measured potential data, compare the negative electrode potential with the lithium deposition potential (0V vs. Li / Li). + If the negative electrode potential is lower than this value, it is determined that lithium plating is present.
[0030] Comparative Example 1 This comparative example provides another reference electrode, which differs from Example 1 in that it is a cylindrical copper wire (without holes, i.e., both porosity and pore diameter are 0), and its first dimension and second dimension are both its bottom diameter, so the ratio of the two is 1.
[0031] Generally, the ratio of the first dimension to the height of the positive electrode 2 or the negative electrode 3 is also 1.
[0032] Comparative Example 2 This comparative example provides another reference electrode, which differs from Example 1 in that it is a porous copper wire with a cylindrical structure, the first dimension and the second dimension of which are both the diameter of its bottom surface, so the ratio of the two is 1.
[0033] Generally, the porosity does not exceed 70%, and the ratio of the first dimension to the height of the positive electrode 2 or negative electrode 3 is 1.
[0034] Under high-rate charging (e.g., ≥3C), the difference between the measured negative electrode potential and the true potential in Example 1 is approximately -10mV, in Comparative Example 1 it is approximately -30mV, and in Comparative Example 2 it is approximately -20mV. This indicates that the reference electrode of this invention has a flat structure, and the thickness space occupied by the reference electrode between the electrodes is significantly compressed, allowing the electrolyte to flow simultaneously on the upper and lower surfaces and within the internal pores of the reference electrode. + The concentration gradient is quickly smoothed out, the liquid phase current distribution tends to be uniform, and the negative electrode potential reading no longer drifts due to local concentration differences, thus significantly improving the test accuracy.
[0035] The above description is only a preferred embodiment of the present utility model and does not limit the implementation method and protection scope of the present utility model. Those skilled in the art should realize that all solutions obtained by equivalent substitutions and obvious changes made based on the description and illustrations of the present utility model should be included within the protection scope of the present utility model.
Claims
1. A reference electrode (1), characterized in that, include: Multi-hole copper wire; among which, The porous copper wire is disposed between the positive electrode (2) and the negative electrode (3) of the three-electrode cell, and a first diaphragm (4) is disposed between the positive electrode (2) and the porous copper wire, and a second diaphragm (5) is disposed between the porous copper wire and the negative electrode (3). The porous copper wire has a flat structure, and the flat structure has a first dimension along the height direction (H) of the positive electrode (2) and a second dimension along the width direction (W) of the positive electrode (2), the ratio of the first dimension to the second dimension not exceeding 0.
3.
2. The reference electrode (1) according to claim 1, characterized in that, The first size is 15μm-30μm.
3. The reference electrode (1) according to claim 1, characterized in that, The second dimension is 120μm-240μm.
4. The reference electrode (1) according to claim 1, characterized in that, The porosity of the porous copper wire is 10%-50%.
5. The reference electrode (1) according to claim 1, characterized in that, The pore size of the porous copper wire is 0.6μm-6μm.
6. The reference electrode (1) according to any one of claims 1-5, characterized in that, Also includes: Lithium deposition layer; The lithium deposition layer is attached to the outer surface of the porous copper wire.
7. A three-electrode battery cell, characterized in that, include: The reference electrode (1), positive electrode (2), negative electrode (3), first diaphragm (4), and second diaphragm (5) are as described in any one of claims 1-6; wherein, The reference electrode (1) is disposed between the positive electrode (2) and the negative electrode (3), the first diaphragm (4) is disposed between the positive electrode (2) and the reference electrode (1), and the second diaphragm (5) is disposed between the reference electrode (1) and the negative electrode (3).
8. The three-electrode cell according to claim 7, characterized in that, The positive electrode (2) includes: a positive electrode current collector and a positive electrode active layer; wherein, The positive electrode active layer is disposed on the surface of the positive electrode current collector.
9. The three-electrode battery cell according to claim 7, characterized in that, The negative electrode (3) includes: a negative electrode current collector and a negative electrode active layer; wherein, The negative electrode active layer is disposed on the surface of the negative electrode current collector.
10. A three-electrode battery, characterized in that, include: The three-electrode cell, electrolyte, and housing as described in any one of claims 7-9; wherein, The three-electrode battery cell and the electrolyte are both disposed inside the housing, and the three-electrode battery cell is immersed in the electrolyte.