Packaging structure
By using high glass transition temperature nano-modified epoxy resin micro-area dispensing and layered dispensing processes at the bonding wire corners, the problem of bonding wire fatigue cracks caused by the mismatch of thermal expansion coefficients between the module shell and the copper substrate was solved, improving the temperature cycling reliability and lifespan of the power module.
Patent Information
- Application Number
- CN202522753031.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-12-25
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2035-12-25
AI Technical Summary
In the reliability verification of automotive-grade power modules, the mismatch of the thermal expansion coefficients between the module shell and the copper substrate causes periodic alternating shear stress at the corners of the bonding wires, leading to fatigue cracks and fractures in the bonding wires, which is difficult to effectively solve with existing technologies.
Micro-area dispensing using nano-modified epoxy resin with high glass transition temperature is applied to the corners of the bonding lines for targeted coating. Combined with a multi-layer dispensing process, this ensures that the extension angle of the bending section is within a reasonable range, reducing alternating shear stress, and provides overall protection through a silicone gel potting layer.
It significantly improves the reliability and lifespan of power modules under temperature cycling scenarios, avoids fatigue cracks and fractures at the corners of bond lines, reduces the problem of increased thermal resistance, and balances material utilization and process compatibility.
Smart Images

Figure CN224988037U_ABST
Abstract
Description
Technical Field
[0001] This disclosure relates to the semiconductor field with a packaging structure, and more particularly to a packaging structure. Background Technology
[0002] In the reliability verification of automotive-grade power modules, temperature cycling testing from -40°C to 125°C is the core scenario for assessing package reliability. The core potential failure stems from the severe mismatch in the coefficients of thermal expansion (CTE) between the module casing (commonly PBT plastic, CTE≈60-80ppm / °C) and the copper substrate (CTE≈17ppm / °C). When the temperature fluctuates drastically, the uncoordinated expansion / contraction of the two materials generates periodic alternating shear stress at the corners of the bonding wires connecting the signal terminals and the copper substrate. This causes the corner curvature to change randomly, ultimately leading to fatigue cracks and fractures in the bonding wires. Industry data shows that bonding wire failures account for more than 70% of temperature cycling failures in power modules, with the highest risk of fracture occurring at low temperatures (-40°C). Utility Model Content
[0003] This disclosure provides a packaging structure to solve the technical problem of easy fatigue cracking and breakage of bonding wires in the prior art.
[0004] This disclosure provides a packaging structure, including: a module housing, a copper substrate, signal terminals, bonding wires, and micro-area dispensing. The copper substrate is disposed within the module housing. The signal terminals are located on the inner wall of the module housing and are spaced apart from the copper substrate. The bonding wires connect the signal terminals and the copper substrate to achieve electrical conduction. A corner is formed in the region of the bonding wire near the connection point between the signal terminal and the copper substrate. The corner includes a straight segment at a distal end and a curved segment at a proximal end. The micro-area dispensing covers a portion of the straight segment at the distal end of the bonding wire, such that the angle at which the curved segment extends beyond the micro-area dispensing remains within a first threshold range. The micro-area dispensing is a high glass transition temperature nano-modified epoxy resin.
[0005] The micro-area dispensing has a Tg > 150℃ and CTE < 40ppm / ℃, which is used to reduce the alternating shear stress at the corner of the bonding line during the temperature cycling process from -40 to 125℃.
[0006] Wherein, the coating center of the micro-area dispensing is a point on the straight segment near the curved segment in the corner of the bonding line, the curvature of the straight segment covered by the micro-area dispensing is 0, and the curvature extending from the micro-area dispensing to one side of the curved segment is greater than 0.
[0007] The micro-area dispensing path includes: using the point with the maximum curvature of the bonding line corner as the center, dispensing in layers and multiple times to form the shape.
[0008] The total encapsulation volume of the micro-area dispensing is approximately 0.0002 mm³.
[0009] The layered dispensing includes a first layer, a second layer, and a third layer stacked from bottom to top, wherein the first layer, the second layer, and the third layer are respectively made by different dispensing processes; The first layer has a coating diameter of 0.3 mm and a thickness of 50 μm; The second layer has a coating diameter of 0.25 mm and a thickness of 30 μm; The third layer has a coating diameter of 0.2 mm and a thickness of 20 μm.
[0010] Wherein, when the arc height of the bent section in the bonding wire is 4.15mm, the length of the bonding wire extending out of the micro-area dispensing is 6.9mm-17.69mm; When the arc height of the bent section in the bonding wire is 5.4 mm, the length of the bonding wire extending out of the micro-area dispensing is 9.1 mm to 18.7 mm.
[0011] The first threshold range is 42°-60°; When the arc height of the bent section in the bonding wire is 4.15 mm, the angle at which the bent section extends out of the micro-area dispensing is 42°-45°. When the arc height of the bent section in the bonding wire is 5.4 mm, the angle at which the bent section extends out of the micro-area dispensing is 58°-60°.
[0012] It also includes a silicone gel potting layer, which is disposed inside the module housing and covers the micro-area dispensing and the bonding wires.
[0013] The bonding wire is made of aluminum or copper; the thermal conductivity of the micro-area dispensing is 0.6 W / m. K-0.7W / m K, the elongation at break of the micro-area dispensing is 3%-5%.
[0014] The technical solutions provided in this disclosure have the following advantages compared with the prior art: The packaging structure provided in this embodiment, through targeted coating of the straight segment at the distal end of the bonding line with micro-area adhesive, can keep the angle of the bent segment extending from the micro-area adhesive within a first threshold range, that is, fix the position of the bent segment, effectively suppressing the random change in the bending degree of the bonding line corner caused by the mismatch of the thermal expansion coefficients between the module shell and the copper substrate, and avoiding fatigue cracks and fractures caused by stress concentration at the corner; at the same time, the characteristics of the high glass transition temperature nano-modified epoxy resin ensure dimensional stability in a wide temperature range, significantly improving the reliability and lifespan of the power module in temperature cycling scenarios, and the micro-area coating design avoids the problem of increased thermal resistance caused by redundant materials. Attached Figure Description
[0015] The accompanying drawings, which are incorporated in and form part of this specification, illustrate embodiments consistent with the present invention and, together with the description, serve to explain the principles of the present invention.
[0016] To more clearly illustrate the technical solutions in the embodiments of this utility model or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, for those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0017] One or more embodiments are illustrated by way of example with reference numerals in the accompanying drawings. These illustrations do not constitute a limitation on the embodiments. Elements with the same reference numerals in the drawings are denoted as similar elements. Unless otherwise stated, the figures in the drawings are not to be limited by scale.
[0018] Figure 1 This is a partial side view of the packaging structure provided in an embodiment of the present disclosure; Figure 2 This is a partial top view of the packaging structure provided in the embodiments of this disclosure; Figure 3 This is a top view of the overall packaging structure provided in an embodiment of the present disclosure; Figure 4 This is a schematic diagram showing the angle of the bond wire bending segment provided in an embodiment of this disclosure.
[0019] Explanation of reference numerals in the attached figures: 1. Copper substrate; 2. Signal terminal; 3. Bonding wire; 3A. Corner; 31. Straight segment; 32. Bending segment; 4. Micro-area dispensing; 5. Module housing; a. Angle between bonding wire and horizontal direction. Detailed Implementation
[0020] To make the objectives, technical solutions, and advantages of the embodiments of this disclosure clearer, the technical solutions of the embodiments of this disclosure will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some, not all, of the embodiments of this disclosure. Based on the embodiments of this disclosure, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this disclosure.
[0021] The following disclosure provides numerous different embodiments or examples for implementing various structures of the present invention. To simplify the disclosure, specific examples of components and arrangements are described below. These are merely examples and are not intended to limit the scope of the invention. Furthermore, reference numerals and / or letters may be repeated in different examples. Such repetition is for simplification and clarity and does not in itself indicate a relationship between the various embodiments and / or arrangements discussed.
[0022] For ease of description, spatial relative terms may be used in this text to describe the relative position or movement of one element or feature relative to another element or feature, as shown in the figure. These relative terms include, for example, inside, outside, inner side, outer side, below, below, above, front, back, etc. Such spatial relative terms are intended to include different orientations of the device in use or operation, other than those depicted in the figure. For example, if the device in the figure undergoes a positional flip, orientation change, or change of motion, these directional indications will change accordingly; for example, an element described as being below or under other elements or features will subsequently be oriented above or above other elements or features. Therefore, the example term "below" can include orientations of "above" and "below". The device may be otherwise oriented (rotated 90 degrees or in other directions), and the spatial relative descriptors used in this text will be interpreted accordingly.
[0023] Existing bonding wire protection technologies struggle to address the issue of corner bending stability. The hybrid bonding line scheme only optimizes strength by replacing the material in the high-stress area, without changing the stress state and bending stability at the corner; The copper strip bonding and epoxy integral molding solution works on the entire bonding line, which can disperse stress but cannot precisely control the local curvature at the corners. While high-Tg epoxy resin local potting solutions cover the bond line area, they lack a coordinated design for the straight and curved sections at corners. Furthermore, traditional epoxy materials suffer from low thermal conductivity (<0.2W / m). The defects of K) and insufficient low-temperature toughness (sharp drop in elongation at break at -40℃) not only fail to ensure that the corner curvature is stable within a reasonable threshold range, but may also exacerbate fatigue failure due to material mismatch. At the same time, the existing dispensing process is difficult to achieve precise micro-area coating, which further limits the controllability of corner curvature.
[0024] To alleviate the above problems, refer to Figures 1-4 This disclosure provides a packaging structure that addresses the problem that the mismatch in thermal expansion coefficients between the module housing 5 and the copper substrate 1 can cause stress concentration at the corner 3A of the bonding wire 3, leading to bending changes and eventual failure. The structure provides a signal terminal 2 between the copper substrate 1 and the inner wall within the module housing 5, and uses the bonding wire 3 to connect the two to achieve electrical conduction. Furthermore, at a position on the far straight segment 31 of the bonding wire 3 near the corner 3A formed by the connection end, a micro-area adhesive 4 made of nano-modified epoxy resin with a high glass transition temperature is applied.
[0025] Specifically, this disclosure provides a packaging structure including: a module housing 5, a copper substrate 1, a signal terminal 2, a bonding wire 3, and micro-area dispensing 4. The copper substrate 1 is disposed inside the module housing 5; the signal terminal 2 is located on the inner wall of the module housing 5 and is spaced apart from the copper substrate 1; the bonding wire 3 connects the signal terminal 2 and the copper substrate 1 to achieve electrical conduction; the area of the bonding wire 3 near the connection end between the signal terminal 2 and the copper substrate 1 forms a corner 3A, which includes a straight segment 31 at the distal end and a curved segment 32 at the proximal end; the micro-area dispensing 4 covers a position of the straight segment 31 at the distal end of the bonding wire 3 so that the angle of the curved segment 32 extending out of the micro-area dispensing 4 is kept within a first threshold range, that is, the curvature of the corner 3A can be fixed and will not change; the micro-area dispensing 4 is a high glass transition temperature nano-modified epoxy resin.
[0026] For example, the corner 3A is a structure formed in the region of the bonding wire 3 near the connection end between the signal terminal 2 and the copper substrate 1. The straight segment 31 at the far end refers to the part of the bonding wire 3 that is far from the bending center and has a straight shape, while the curved segment 32 at the near end refers to the part of the bonding wire 3 that is close to the bending center and has an arc-shaped bend.
[0027] For example, micro-area dispensing 4 is applied to a specific location on the straight segment 31 at the distal end of the bonding line 3, at the junction of the straight segment 31 and the curved segment 32.
[0028] For example, the first threshold range refers to the angle range of the micro-area adhesive 4 extending from the bent section 32 that ensures that the corner 3A of the bonding line 3 is not prone to stress concentration during temperature cycling and avoids abnormal changes in the curvature of the corner 3A. The curvature of the corner 3A is kept fixed by the covering effect of the micro-area adhesive 4.
[0029] For example, the first threshold range can be 42°-60°. This first threshold range is the angle α between the bonding line and the horizontal direction.
[0030] For example, high glass transition temperature nano-modified epoxy resin refers to epoxy resin with a high glass transition temperature that has been modified by nanomaterials. Its high glass transition temperature characteristic can ensure dimensional stability over a wide temperature range, while nano-modification helps to improve the overall performance of the material to meet the protection requirements of the 3A corner of the bond line.
[0031] In this way, by applying micro-area adhesive 4 to the targeted coating of the straight segment 31 at the far end of the bonding line 3, the random change in curvature of the corner 3A of the bonding line 3 caused by the mismatch of the thermal expansion coefficients between the module shell 5 and the copper substrate 1 is effectively suppressed, avoiding fatigue cracks and fractures caused by stress concentration at the corner 3A. At the same time, the characteristics of the high glass transition temperature nano-modified epoxy resin ensure dimensional stability over a wide temperature range, significantly improving the reliability and lifespan of the power module under temperature cycling scenarios. Furthermore, the micro-area coating setting avoids the problem of increased thermal resistance caused by redundant materials.
[0032] Consider setting a micro-area dispensing 4 with specific performance parameters in the encapsulation structure, namely, the glass transition temperature of the micro-area dispensing 4 is greater than 150℃ and the coefficient of thermal expansion is less than 40ppm / ℃, and take advantage of its dimensional stability and low thermal expansion characteristics over a wide temperature range to specifically act on the corner 3A region of the bonding line 3.
[0033] In some embodiments, the micro-area dispensing 4 has a Tg > 150°C and CTE < 40ppm / °C, which is used to reduce the alternating shear stress at the corner 3A of the bonding line 3 during temperature cycling from -40°C to 125°C.
[0034] For example, Tg refers to the glass transition temperature of the micro-area dispensing material 4. When the glass transition temperature of the micro-area dispensing material 4 is greater than 150°C, the material will not change from a rigid state to a flexible state within the temperature cycling range of -40°C to 125°C, and will always maintain a stable structural morphology to effectively support the corner 3A of the bonding line 3.
[0035] For example, CTE refers to the coefficient of thermal expansion of the micro-area dispensing material 4. When the coefficient of thermal expansion is less than 40ppm / ℃, the material expands or contracts less when the temperature changes, which can better match the thermal expansion characteristics of the bonding wire 3 and the copper substrate 1, and reduce the additional stress caused by the difference in thermal expansion.
[0036] For example, the temperature environment in which the packaging structure is located alternates periodically between -40°C and 125°C. This process is the core scenario for evaluating the reliability of the power module packaging and can easily cause uncoordinated expansion or contraction between the module shell 5 and the copper substrate 1.
[0037] For example, during temperature cycling from -40 to 125°C, due to the different coefficients of thermal expansion between the module housing 5 and the copper substrate 1, their expansion or contraction amplitudes are inconsistent, resulting in periodically changing shear stress in the corner 3A area of the bonding wire 3 connecting the two. This stress will continuously damage the bonding wire 3 and may eventually lead to breakage.
[0038] Thus, the Tg > 150℃ characteristic of the micro-area dispensing 4 ensures that it maintains structural rigidity within a temperature cycling range of -40 to 125℃, avoiding brittle fracture at low temperatures or deformation failure at high temperatures; the CTE < 40ppm / ℃ characteristic reduces the difference in thermal expansion between the micro-area dispensing 4, the bonding wire 3, and the copper substrate 1, reducing additional stress generated during temperature fluctuations. The synergistic effect of these two characteristics effectively reduces the alternating shear stress at the corner 3A of the bonding wire 3, reducing the initiation and propagation of fatigue cracks in this area, significantly improving the reliability and lifespan of the power module under temperature cycling conditions, and preventing module malfunctions due to bonding wire 3 failure.
[0039] By positioning the coating center of the micro-area adhesive 4 at a point near the curved section 32 of the straight segment 31 in the corner 3A of the bonding line 3, the micro-area adhesive 4 can only coat the straight segment 31 with a curvature of 0, while retaining the bonding line 3 with a curvature greater than 0 that extends from the micro-area adhesive 4 to the side of the curved section 32. This achieves precise targeted protection of the critical stress transfer area at the corner 3A of the bonding line 3.
[0040] In some embodiments, the coating center of the micro-area dispensing 4 is a point on the straight segment 31 near the curved segment 32 in the corner 3A of the bonding line 3. The curvature of the straight segment 31 covered by the micro-area dispensing 4 is 0, and the curvature extending from the micro-area dispensing 4 to one side of the curved segment 32 is greater than 0.
[0041] For example, the corner 3A of the bonding line 3 is composed of a straight segment 31 and a curved segment 32. The coverage center is the center of the coverage area of the micro-area dispensing 4. This position is on the straight segment 31 and adjacent to the curved segment 32, that is, near the junction area of the straight segment 31 and the curved segment 32. It is the core position of the precise coverage of the micro-area dispensing 4.
[0042] For example, the straight segment 31 of the bonding line 3 covered by the micro-area dispensing 4 has a straight shape and a curvature value of 0. After the micro-area dispensing 4 is applied, it can maintain the stability of the straight shape and avoid the bonding line 3 from bending or deforming due to temperature changes.
[0043] For example, the bonding line 3 portion extending outward from the coverage area of the micro-area adhesive 4 and extending toward the curved section 32 has a curved shape with a curvature value greater than 0. This portion of the bonding line 3 maintains its own curved structure and is not covered by the micro-area adhesive 4 to retain its original stress buffering capacity.
[0044] In this way, the region where the straight segment 31 is close to the curved segment 32 is the starting point for stress transmission from the straight segment 31 to the curved segment 32 during temperature fluctuations. The straight segment 31, with a curvature of 0, can fix the structural shape of this region and reduce stress accumulation. Meanwhile, the bonding line 3 extending to one side of the curved segment 32 maintains its original curved shape with a curvature greater than 0, which can maintain its own stress buffering capacity and avoid secondary stress caused by excessive constraint. Ultimately, this effectively reduces the alternating shear stress at the corner 3A of the bonding line 3, reduces the initiation of fatigue cracks, and improves the reliability and lifespan of the power module under temperature cycling from -40 to 125°C. At the same time, the micro-area coating setting avoids the increase in thermal resistance caused by material redundancy and does not interfere with the layout of adjacent devices.
[0045] By setting the path center of the micro-area dispensing 4 to the point of maximum curvature at the corner 3A of the bonding line 3, i.e. the core area with the most concentrated stress, and by using a layered, multi-stage dispensing method, precise targeted coverage of the stress peak area at the corner 3A of the bonding line 3 can be achieved. This avoids problems such as material redundancy and interference with adjacent devices caused by overall or whole-section coverage in existing solutions. At the same time, the layered, multi-stage operation ensures the adhesion between the dispensing layer and the bonding line 3.
[0046] In some embodiments, the path of the micro-area dispensing 4 includes: using layered dispensing with the point of maximum curvature at the corner 3A of the bonding line 3 as the center, dispensing multiple times to form the shape.
[0047] For example, the bonding wire 3 has the most significant bending and the largest curvature value in the corner 3A region formed near the connection end between the signal terminal 2 and the copper substrate 1. This point is the core location of stress concentration at the corner 3A of the bonding wire 3, and it is also the key area where the micro-area dispensing 4 needs to be applied precisely.
[0048] For example, in the micro-area dispensing process 4, the dispensing operation is divided into multiple layers and performed sequentially. Each layer corresponds to a specific coverage area and coating thickness. The complete micro-area dispensing 4 encapsulation structure is formed by stacking the layers, rather than completing all dispensing operations at once.
[0049] For example, the overall molding process of micro-area dispensing 4 is gradually completed through multiple independent dispensing actions, ensuring that the amount of material and the coverage position of each dispensing are precisely controllable, so as to ensure the morphological stability of the final dispensing layer and the adhesion to the corner 3A of the bonding line 3.
[0050] In this way, layered, multi-stage dispensing effectively controls the amount and coverage of adhesive, reducing material waste and avoiding interference with the layout of adjacent devices. Furthermore, layered molding reduces curing shrinkage stress caused by excessive single dispensing thickness, minimizing the risk of cracking in the dispensing layer itself and ensuring stable support of the dispensing layer for the corner 3A of bond line 3. Ultimately, this significantly reduces the alternating shear stress at the corner 3A of bond line 3, inhibits fatigue crack initiation, and improves the reliability and lifespan of the power module under temperature cycling conditions from -40°C to 125°C, all without requiring significant modifications to existing equipment.
[0051] By limiting the total encapsulation volume of the micro-area dispensing 4, we can achieve targeted encapsulation of only a very small area of the core region where stress is concentrated at the corner 3A of the bonding line 3, thus avoiding the dispensing material from extending to unnecessary areas.
[0052] In some embodiments, the total encapsulation volume of the micro-area dispensing 4 is approximately 0.0002 mm³.
[0053] For example, this volume is the total material volume of the corner 3A region of the bonding line 3 covered by the micro-area dispensing 4, formed by the accumulation of the dispensing volumes of each layer during the layered dispensing process. This volume can only cover the core area of stress concentration at the corner 3A of the bonding line 3, and will not extend to the straight segment 31 of the bonding line 3 or the area of adjacent devices. It is a key parameter for achieving micro-area targeted protection, ensuring that the dispensing material is accurately applied to the area that needs protection, while avoiding material waste and increased thermal resistance.
[0054] In this way, compared with traditional partial potting, covering the entire bonding line 3 improves material utilization and avoids the problem of increased thermal resistance caused by redundant materials. At the same time, the extremely small volume of about 0.0002 mm³ can be precisely confined to the corner 3A area of the bonding line 3, without covering adjacent devices or unprotected areas, thus eliminating interference with the surrounding layout. In addition, the small volume can also reduce the shrinkage stress during the curing process of the dispensing layer, reduce the risk of cracking of the dispensing layer itself, ensure its stable support for the corner 3A of the bonding line 3, effectively reduce alternating shear stress, and improve the reliability and lifespan of the power module under temperature cycling at -40~125℃.
[0055] Consider setting the powder layer dispensing to a first, second, and third layer stacked from bottom to top, with each of the three layers made through a different dispensing process, while specifying the coating size of each layer, in order to achieve precise layered coating of the bonding line 3 corner 3A.
[0056] In some embodiments, the layered dispensing includes a first layer, a second layer, and a third layer stacked from bottom to top, wherein the first layer, the second layer, and the third layer are respectively made by different dispensing processes; The first coating layer has a diameter of 0.3 mm and a thickness of 50 μm; The second coating layer has a diameter of 0.25 mm and a thickness of 30 μm; The third layer has a diameter of 0.2 mm and a thickness of 20 μm.
[0057] For example, the layered dispensing is a protective structure covering the corner 3A of the bonding line 3. The structure consists of three independent layers, which are stacked sequentially from bottom to top. The first layer is located at the bottom and directly contacts the surface of the corner 3A of the bonding line 3. The third layer is located at the top, and the second layer is sandwiched between the first and third layers, together forming a complete covering structure.
[0058] For example, when making the first, second and third layers, it is necessary to complete the process through three independent dispensing operations. Each dispensing operation corresponds to only one layer, and the dispensing path, dispensing amount and other parameters of each operation are adapted to the coating diameter and thickness requirements of the corresponding layer to ensure that the shape of each layer is accurate and controllable.
[0059] For example, the first layer is the bottom layer of the layered adhesive, which has a diameter of 0.3 mm in the circular covering area formed in the direction parallel to the surface of the bonding line 3 corner 3A, and a height of 50 μm in the direction perpendicular to the surface, i.e., the layer thickness, to achieve full adhesion with the bonding line 3 corner 3A and provide basic support.
[0060] For example, the second layer is an intermediate layer of layered dispensing, with a circular coverage area having a diameter of 0.25 mm, which is smaller than the coating diameter of the first layer, and a layer thickness of 30 μm. It is used to further reduce the coverage area based on the first layer and focus on the stress core area of the bonding line 3 corner 3A.
[0061] For example, the third layer is the top layer of the powder coating, with a circular coverage area having a diameter of 0.2 mm, smaller than the coating diameter of the second layer, and a layer thickness of 20 μm. This layer is used to precisely lock the stress concentration core area at the corner 3A of the bonding line 3, avoiding material redundancy.
[0062] In this layered dispensing structure, the three-layer structure produced by different dispensing processes allows for precise control of the coverage and thickness of each layer: the larger diameter of the bottom layer stably adheres to the corner 3A area of the bonding line 3, providing basic support; the decreasing diameter of the upper layers focuses on the stress concentration core area, reducing redundant material usage and avoiding the increased thermal resistance caused by traditional full-segment encapsulation; simultaneously, layered manufacturing reduces curing shrinkage stress caused by excessive single dispensing thickness, reduces the risk of cracking of the dispensing layer itself, and improves adhesion to the bonding line 3. Ultimately, it effectively disperses the alternating shear stress at the corner 3A of the bonding line 3, inhibits the initiation and propagation of fatigue cracks, significantly improves the reliability and lifespan of the power module under temperature cycling from -40 to 125°C, and increases material utilization by more than 70%, adapting to mass production process requirements.
[0063] Consider matching the specific length of the extended micro-area adhesive 4 according to the different arc heights of the bending segment 32 of the bonding line 3, to ensure that the micro-area adhesive 4 precisely covers only the stress concentration area near the bending segment 32.
[0064] In some embodiments, when the arc height of the bent section 32 in the bonding wire 3 is 4.15 mm, the length of the bonding wire 3 extending out of the micro-area dispensing 4 is 6.9 mm to 17.69 mm. When the arc height of the bent section 32 in the bonding wire 3 is 5.4mm, the length of the bonding wire 3 extending out of the micro-area dispensing 4 is 9.1mm-18.7mm.
[0065] For example, the arc height refers to the vertical distance from the highest point of the bending segment 32 of the bonding wire 3 to the line connecting the two ends of the bending segment 32 (one end connects to the signal terminal 2, and the other end transitions to the straight segment 31). This distance is a key parameter for measuring the degree of bending of the bonding wire 3 and directly affects the stress distribution state of the bending segment 32.
[0066] For example, the length of the bonding wire 3 extending out of the micro-area adhesive 4 refers to the distance that the bonding wire 3 extends outward from the covering edge of the micro-area adhesive 4, that is, the length of the portion of the bonding wire 3 not covered by the micro-area adhesive 4. Its value needs to match the arc height of the bending segment 32 to ensure that the micro-area adhesive 4 accurately covers the stress concentration area near the bending segment 32, while not covering unnecessary portions of the bonding wire 3.
[0067] For example, when the vertical distance from the highest point of the bending section 32 of the bonding wire 3 to the line connecting its two ends is 4.15 mm, the length of the bonding wire 3 extending outward from the edge of the micro-area dispensing 4 needs to be controlled between 6.9 mm and 17.69 mm to adapt to the stress distribution under this degree of bending and achieve precise protection.
[0068] For example, when the arc height of the bent section 32 in the bonding wire 3 is 5.4mm, the length of the bonding wire 3 extending out of the micro-area dispensing 4 is 9.1mm-18.7mm. When the vertical distance from the highest point of the bent section 32 of the bonding wire 3 to the line connecting its two ends is 5.4mm, the length of the bonding wire 3 extending outward from the edge of the micro-area dispensing 4 needs to be controlled between 9.1mm and 18.7mm to match the stress concentration range under this degree of bending, ensuring the protective effect while avoiding material waste.
[0069] Thus, when the arc height of the bending section 32 is small, i.e., 4.15mm, the shorter extension length of 6.9mm-17.69mm reduces material redundancy and avoids interference with adjacent devices. When the arc height is large, i.e., 5.4mm, the corresponding longer extension length of 9.1mm-18.7mm ensures that the critical stress area of the bending section 32 is completely covered. In both cases, the alternating shear stress of the bending section 32 of the bonding wire 3 can be effectively dispersed, reducing the initiation of fatigue cracks. At the same time, it avoids the increase in thermal resistance caused by redundant adhesive material. Compared with traditional local potting, the increase in thermal resistance is reduced, significantly improving the reliability and lifespan of the power module under temperature cycling at -40~125℃. It is also compatible with bonding wires 3 with different bending shapes, making it more compatible.
[0070] Consider matching the specific angle of the extended micro-area dispensing 4 with the bending shape of the bending segment 32 according to the different arc heights of the bending segment 32 of the bonding line 3, to ensure that the micro-area dispensing 4 and the bending shape of the bending segment 32 are accurately matched.
[0071] In some embodiments, when the arc height of the bent section 32 in the bonding wire 3 is 4.15 mm, the angle at which the bent section 32 extends out of the micro-area dispensing 4 is 42°-45°. When the arc height of the bent section 32 in the bonding wire 3 is 5.4mm, the angle at which the bent section 32 extends out of the micro-area dispensing 4 is 58°-60°.
[0072] For example, the arc height refers to the vertical distance from the highest point of the bending segment 32 of the bonding wire 3 to the line connecting the two ends of the bending segment 32. One end connects to the signal terminal 2, and the other end transitions to the straight segment 31. It is a key parameter for measuring the degree of bending of the bonding wire 3 and directly affects the stress distribution state of the bending segment 32.
[0073] For example, the angle at which the curved segment 32 extends out of the micro-area dispensing 4 refers to the angle formed between the portion of the curved segment 32 of the bonding line 3 extending outward from the covering edge of the micro-area dispensing 4 and the reference direction of the covering surface of the micro-area dispensing 4. This angle needs to match the arc height of the curved segment 32 to ensure that the constraint force of the micro-area dispensing 4 on the curved segment 32 is adapted to its bending shape.
[0074] For example, when the vertical distance from the highest point of the bending section 32 of the bonding wire 3 to the line connecting its two ends is 4.15 mm, the angle formed between the portion of the bending section 32 extending outward from the edge of the micro-area dispensing 4 and the reference direction of the micro-area dispensing 4 coating surface needs to be controlled between 42 degrees and 45 degrees to adapt to the stress distribution under this degree of bending.
[0075] For example, when the vertical distance from the highest point of the bending section 32 of the bonding wire 3 to the line connecting its two ends is 5.4 mm, the angle formed by the portion of the bending section 32 extending outward from the edge of the micro-area dispensing 4 and the reference direction of the micro-area dispensing 4 coating surface needs to be controlled between 58 degrees and 60 degrees to match the stress concentration range under this degree of bending.
[0076] Thus, when the arc height of the bending section 32 is small, i.e., 4.15mm, the extension angle of 42°-45° can adapt to its gentler bending shape, avoiding additional stress caused by the adhesive layer pulling on the bending section 32; when the arc height is large, i.e., 5.4mm, the extension angle of 58°-60° can match its steeper bending shape, ensuring that the critical stress area of the bending section 32 is completely covered. In both cases, the alternating shear stress of the bending section 32 can be effectively dispersed, reducing the initiation and propagation of fatigue cracks, and significantly improving the reliability and lifespan of the power module under temperature cycling. At the same time, this setting is adaptable to bonding wires 3 with different bending shapes, without the need to adjust the overall structure of the dispensing equipment, with strong process compatibility, which is conducive to mass production.
[0077] Consider setting a silicone gel potting layer inside the module shell 5 to cover the micro-area dispensing 4 and the entire bonding line 3, forming a synergistic structure of precise micro-area suppression of corner 3A stress and overall silicone gel protection.
[0078] In some embodiments, a silicone gel potting layer is also included, which is disposed inside the module housing 5 and covers the micro-area dispensing 4 and bonding wires 3.
[0079] For example, the silicone gel potting layer is a protective structure that fills the internal space surrounded by the module shell 5. Its entirety is within the boundary of the module shell 5 and does not exceed the outer contour of the shell. Together with the module shell 5, it forms a protective barrier for the internal bonding lines 3, micro-area dispensing 4, and other structures.
[0080] For example, the coverage of the silicone gel potting layer includes two parts: one part is the micro-area dispensing 4 covering the corner 3A of the bonding line 3, and the other part is the entire bonding line 3 connecting the signal terminal 2 and the copper substrate 1. The silicone gel will completely cover the micro-area dispensing 4 and the bonding line 3, ensuring that both are within the protection range of the silicone gel and there is no exposed area.
[0081] In this way, after the silicone gel potting layer covers the micro-area dispensing 4 and bonding wires 3, it can effectively isolate moisture, dust and other impurities inside the module shell 5, preventing them from corroding the solder joints of the bonding wires 3 or the micro-area dispensing 4 layer, and preventing the degradation of electrical insulation performance due to impurities. At the same time, the silicone gel has good flexibility, which can buffer the slight relative displacement between the module shell 5 and the copper substrate 1 during temperature cycling from -40 to 125°C, and disperse the secondary stress in the non-corner 3A area of the bonding wires 3, complementing the principal stress at the corner 3A suppressed by the micro-area dispensing 4. Ultimately, this further improves the reliability and lifespan of the power module under temperature cycling, and the thermal conductivity of the silicone gel is adapted to the low resistance setting of the micro-area dispensing 4, without adding significant additional thermal resistance, avoiding the heat dissipation problems caused by traditional integral epoxy molding, and is compatible with mass production process requirements.
[0082] Consider using bonding wire 3 material to adapt to different cost and strength requirements, while controlling the thermal conductivity and elongation at break of micro-area dispensing 4 within a certain range, so that micro-area dispensing 4 has both good thermal conductivity to avoid hindering heat dissipation of bonding wire 3 and sufficient toughness to cope with stress in low-temperature environments.
[0083] In some embodiments, the bonding wire 3 is an aluminum wire or a copper wire; the thermal conductivity of the micro-area dispensing 4 is 0.6 W / m. K-0.7W / m K, the elongation at break of micro-area dispensing 4 is 3%-5%.
[0084] For example, the bonding wire 3 is a conductive structure connecting the signal terminal 2 and the copper substrate 1, and can be made of either aluminum or copper wire. Aluminum wire has the advantage of lower cost and is suitable for cost-sensitive and relatively low-stress scenarios; copper wire has higher strength and is suitable for high-stress scenarios where the tensile and compressive strength of the bonding wire 3 is more important.
[0085] For example, thermal conductivity is a parameter that measures the heat conduction capability of micro-area dispensing 4. When the thermal conductivity of micro-area dispensing 4 is between 0.6 W / m Kelvin and 0.7 W / m Kelvin, it can effectively conduct the heat generated by the bonding wire 3 during operation and temperature cycling, and prevent heat from accumulating at the corner 3A of the bonding wire 3, thereby reducing the thermal fatigue damage of the bonding wire 3.
[0086] For example, the elongation at break is a parameter that measures the maximum elongation deformation that the micro-area adhesive 4 can withstand before fracture. When this value is between 3% and 5%, the micro-area adhesive 4 is not prone to cracking due to insufficient toughness at the low temperature stage of -40℃. It can adapt to the slight deformation of the bonding line 3 and always maintain the coverage and stress dispersion effect on the corner 3A of the bonding line 3, thus avoiding cracking itself and forming new stress gaps.
[0087] Thus, choosing either aluminum or copper wire as the bonding wire 3 allows for flexible adaptation to the cost and strength requirements of different power modules. Aluminum wire meets the needs of low-cost scenarios, while copper wire is suitable for high-stress areas; micro-area dispensing 40.6W / m K-0.7W / m The thermal conductivity of K effectively conducts the heat generated during the operation of the bonding wire 3, avoiding the heat accumulation and accelerated thermal fatigue problems caused by traditional low thermal conductivity epoxy materials. The 3%-5% elongation at break ensures that the micro-area adhesive 4 is not easily brittle at -40℃, maintaining stable coverage and stress dispersion at the corner 3A of the bonding wire 3. The synergy of these three factors reduces the risk of bonding wire 3 failure in the power module under temperature cycling from -40℃ to 125℃, significantly improving fatigue life while also considering cost-effectiveness and process compatibility.
[0088] It should be understood that the terminology used herein is for the purpose of describing particular exemplary embodiments only and is not intended to be limiting. Unless the context clearly indicates otherwise, the singular forms "one," "an," and "described" as used herein may also mean including the plural forms. The terms "comprising," "including," "containing," and "having" are inclusive and therefore indicate the presence of the stated features, steps, operations, elements, and / or components, but do not exclude the presence or addition of one or more other features, steps, operations, elements, components, and / or combinations thereof. The method steps, processes, and operations described herein are not construed as requiring them to be performed in a particular order described or illustrated unless the order of performance is explicitly indicated. It should also be understood that additional or alternative steps may be used.
[0089] Although terms such as first, second, third, etc., may be used in this document to describe multiple elements, components, regions, layers, and / or segments, these elements, components, regions, layers, and / or segments should not be limited by these terms. These terms may be used only to distinguish one element, component, region, layer, or segment from another. Unless the context clearly indicates otherwise, terms such as first, second, and other numerical terms used herein do not imply order or sequence. Therefore, the first element, component, region, layer, or segment discussed below may be referred to as a second element, component, region, layer, or segment without departing from the teachings of the exemplary embodiments.
[0090] The above description is merely a specific embodiment of the present invention, enabling those skilled in the art to understand or implement the present invention. Various modifications to these embodiments will be readily apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention is not to be limited to the embodiments shown herein, but is to be accorded the widest scope consistent with the principles and novel features disclosed herein.
Claims
1. A packaging structure, characterized in that, include: Module casing; A copper substrate, wherein the copper substrate is disposed within the module housing; The signal terminal is located on the inner wall of the module housing and is spaced apart from the copper substrate; A bonding wire is connected between the signal terminal and the copper substrate to achieve electrical conduction. The bonding wire forms a corner near the connection end between the signal terminal and the copper substrate. The corner includes a straight segment at the far end and a curved segment at the near end. Micro-area dispensing, wherein the micro-area dispensing covers a position of a straight segment at the distal end of the bonding line, such that the angle at which the curved segment extends out of the micro-area dispensing remains within a first threshold range. The micro-area dispensing is a nano-modified epoxy resin with a high glass transition temperature (Tg).
2. The packaging structure according to claim 1, characterized in that, The micro-area dispensing has a Tg > 150℃ and CTE < 40ppm / ℃, which is used to reduce the alternating shear stress at the corner of the bonding line during temperature cycling from -40 to 125℃.
3. The packaging structure according to claim 1, characterized in that, The coating center of the micro-area dispensing is a point on the straight segment near the curved segment in the corner of the bonding line. The curvature of the straight segment covered by the micro-area dispensing is 0, and the curvature extending from the micro-area dispensing to one side of the curved segment is greater than 0.
4. The packaging structure according to claim 1, characterized in that, The micro-area dispensing path includes: using the point with the maximum curvature of the bonding line corner as the center, dispensing in layers and multiple times to form the shape.
5. The packaging structure according to claim 4, characterized in that, The total encapsulation volume of the micro-area dispensing is approximately 0.0002 mm³.
6. The packaging structure according to claim 4, characterized in that, The layered dispensing includes a first layer, a second layer, and a third layer stacked from bottom to top, wherein the first layer, the second layer, and the third layer are respectively made by different dispensing processes; The first layer has a coating diameter of 0.3 mm and a thickness of 50 μm; The second layer has a coating diameter of 0.25 mm and a thickness of 30 μm; The third layer has a coating diameter of 0.2 mm and a thickness of 20 μm.
7. The packaging structure according to claim 3, characterized in that, When the arc height of the bent section in the bonding wire is 4.15mm, the length of the bonding wire extending out of the micro-area dispensing is 6.9mm-17.69mm; When the arc height of the bent section in the bonding wire is 5.4 mm, the length of the bonding wire extending out of the micro-area dispensing is 9.1 mm to 18.7 mm.
8. The packaging structure according to claim 3, characterized in that, The first threshold range is 42°-60°; When the arc height of the bent section in the bonding wire is 4.15 mm, the angle at which the bent section extends out of the micro-area dispensing is 42°-45°. When the arc height of the bent section in the bonding wire is 5.4 mm, the angle at which the bent section extends out of the micro-area dispensing is 58°-60°.
9. The packaging structure according to claim 1, characterized in that, It also includes a silicone gel potting layer, which is disposed inside the module housing and covers the micro-area dispensing and the bonding wires.
10. The packaging structure according to claim 1, characterized in that, The bonding wire is made of aluminum or copper; the thermal conductivity of the micro-area dispensing is 0.6 W / m. K-0.7W / m K, the elongation at break of the micro-area dispensing is 3%-5%.