Semiconductor component and its manufacture

The multi-layer channel and active region structure in semiconductor devices addresses issues of short channel control and resistance by optimizing dopant gradients, leading to improved performance and reduced variations.

DE102015104456B4Active Publication Date: 2024-11-21TAIWAN SEMICONDUCTOR MANUFACTURING CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
DE102015104456
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2014-04-21
Filing Date
2015-03-25
Publication Date
2024-11-21
Estimated Expiration
2035-03-25

AI Technical Summary

Technical Problem

Existing semiconductor devices face challenges in achieving optimal dopant concentration gradients and layer structures to enhance short channel control, reduce contact resistance, and minimize variations in dopant saturation and line edge roughness.

Method used

A semiconductor device is formed with a multi-layer channel structure comprising a first channel layer of silicon or germanium, a second channel layer with added carbon, and a third channel layer of silicon, along with a multi-layer active region structure featuring graded germanium concentrations and varying dopant concentrations to improve short channel control and reduce resistance.

Benefits of technology

The multi-layer structure enhances short channel control, reduces contact resistance, and minimizes variations in dopant saturation and line edge roughness, thereby improving drive current and overall device performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

Semiconductor device comprising the following: an active area that includes the following: a first active area layer (220) with a first dopant concentration, wherein the first active area layer (220) contains germanium and the percentage of germanium increases from the bottom (220b) of the first active area layer (220) to its top (220a); a second active region layer (222) with a second dopant concentration, wherein the second active region layer is located above the first active region layer; and a third active region layer (224) with a third dopant concentration, wherein the third active region layer is located above the second active region layer and extends over a top surface of a semiconductor composite within which the first active region layer and the second active region layer are formed, wherein the first dopant concentration is lower than the second dopant concentration and the second dopant concentration is lower than the third dopant concentration.
Need to check novelty before this filing date? Find Prior Art

Description

BACKGROUND

[0001] In a semiconductor device, current flows through a channel region between a source region and a drain region upon application of a sufficient voltage or bias to a gate of the device. When current flows through the channel region, the device is generally considered to be in an "on" state, and when no current flows through the channel region, the device is generally considered to be in an "off" state. US 2013 / 0069123 A1 describes a semiconductor device with a three-layer source / drain region comprising a first layer of silicon and germanium, a second layer of silicon and germanium with a higher germanium content and dopant concentration than the first layer, and a third layer of monocrystalline silicon.

[0002] US 2008 / 0 224 218 A1 describes a CMOS structure comprising an n-FET device with an n-FET channel region and a p-FET device with a p-FET channel region. The n-FET channel region comprises a first silicon material layer located on a silicon-germanium alloy material layer. The p-FET channel comprises a second silicon material layer located on a silicon-germanium-carbon alloy material layer. The silicon-germanium alloy material layer induces a desired tensile stress in the n-FET channel. The silicon-germanium-carbon alloy material layer suppresses an undesired tensile stress within the p-FET channel region.A silicon-germanium-carbon alloy material from which the silicon-germanium-carbon alloy material layer is composed can be formed by selectively incorporating carbon into a silicon-germanium alloy material from which the silicon-germanium alloy material layer is formed. DESCRIPTION OF THE DRAWINGS

[0003] Aspects of the present disclosure will be understood from the following detailed description when read in conjunction with the accompanying figures. It should be noted that elements and / or structures are not necessarily drawn to scale. Accordingly, the dimensions of illustrated structural elements may be enlarged and / or reduced as needed for clarity of discussion. Fig. 1 is a flowchart illustrating a method of forming a semiconductor device, according to some embodiments. Fig. 2 is an illustration of a semiconductor device according to some embodiments. Fig. 3 is an illustration of a semiconductor device according to some embodiments. Fig. 4 is an illustration of a semiconductor device according to some embodiments. Fig. 5 is an illustration of a semiconductor device according to some embodiments. Fig. 6 is an illustration of a semiconductor device according to some embodiments. Fig. 7 is an illustration of a semiconductor device according to some embodiments. Fig. 8 is an illustration of a semiconductor device according to some embodiments. Fig. 9 is an illustration of a semiconductor device according to some embodiments. Fig. 10 is an illustration of a semiconductor device according to some embodiments. Fig. 11 is an illustration of a semiconductor device according to some embodiments. Fig. 12 is an illustration of a semiconductor device according to some embodiments. Fig. 13 is an illustration of a semiconductor device according to some embodiments. Fig. 14 is an illustration of a semiconductor device according to some embodiments. Fig. 15 is an illustration of a semiconductor device according to some embodiments. DETAILED DESCRIPTION

[0004] In this text, one or more techniques for forming a semiconductor device and resulting structures formed thereby are provided.

[0005] A method 100 for forming a semiconductor device 200 and a semiconductor device 300 according to some embodiments is described in Fig. 1, and one or more structures formed thereby are shown at various stages of manufacture in the Fig. 2-15. According to some embodiments, a semiconductor device 200 includes a semiconductor compound 205 as shown in Fig. 11. In some embodiments, a semiconductor composite 205 includes a first channel layer 202, a second channel layer 206, and a third channel layer 208. In some embodiments, the semiconductor device 200 includes an active region 207 within the semiconductor composite 205 and adjacent to a gate 210. In some embodiments, the active region 207 includes a first active region layer 220 having a first dopant concentration, a second active region layer 222 having a second dopant concentration, the second active region layer 222 being located above the first active region layer 220, and a third active region layer 224 having a third dopant concentration, the third active region layer 224 being located above the second active region layer 222 and above a top surface 205a of the semiconductor composite 205.In some embodiments, the first dopant concentration, the second dopant concentration, and the third dopant concentration of semiconductor device 200 comprise a p-type dopant. In some embodiments, semiconductor device 300 comprises semiconductor compound 205, as shown in FIG. Fig. 15. In some embodiments, the semiconductor device 300 includes an active region 307 within the semiconductor compound 205 and adjacent to a gate 210. In some embodiments, the active region 307 includes a first active region layer 320 having a first dopant concentration and a second active region layer 322 having a second dopant concentration, wherein the second active region layer 322 is located above the first active region layer 320. In some embodiments, the active region 307 includes a third active region layer 324 having a third dopant concentration, wherein the third active region layer 324 is located above the second active region layer 322 and above the top surface 205a of the semiconductor compound 205. In some embodiments, the first dopant concentration, the second dopant concentration, and the third dopant concentration of the semiconductor device 300 include an n-type dopant.

[0006] At 102, a first channel layer 202 is formed in a substrate 203 to form the semiconductor device 200, as shown in the Fig. 2-3, or to form the semiconductor device 300 according to some embodiments. Let us turn Fig. 2. A substrate 203 is located between shallow trench isolation (STI) regions 204. In some embodiments, the substrate 203 comprises at least one of silicon or germanium. According to some embodiments, the substrate 203 comprises at least one of an epitaxial layer, a silicon-on-insulator (SOI) structure, a wafer, or a chip formed from a wafer. In some embodiments, the STI region 204 comprises a dielectric material, such as silicon oxide (SiO2). In some embodiments, a first channel layer implant is implanted into the substrate 203. In some embodiments, the first channel layer implant comprises germanium. In some embodiments, a first anneal is performed on the substrate 203. In some embodiments, the first anneal comprises applying a high temperature between above 400°C to about 1000°C to the semiconductor device.In some embodiments, the annealing repairs damage to the lattice structure in substrate 203 caused by the first channel layer implant. In some embodiments, substrate 203 is recessed, such as by etching, to form first channel layer 202.

[0007] At 104, the second channel layer 206 is formed over the first channel layer 202 to form the semiconductor device 200, as shown in Fig. 3, or to form the semiconductor device 300 according to some embodiments. In some embodiments, the second channel layer 206 is grown, such as by epitaxial growth. In some embodiments, the second channel layer 206 comprises at least one of silicon or carbon. In some embodiments, the second channel layer 206 comprises less than about 1% carbon. In some embodiments, the second channel layer 206 has a second channel layer height between about 2 nm and about 15 nm. In some embodiments, the carbon is added to the composition of the second channel layer 206 by in-situ doping.

[0008] At 106, the third channel layer 208 is formed over the second channel layer 206 to form the semiconductor device 200, as shown in Fig. 3, or to form the semiconductor device 300 according to some embodiments. In some embodiments, the third channel layer 208 is grown, such as by epitaxial growth. In some embodiments, the third channel layer 208 comprises silicon. In some embodiments, the third channel layer 208 has a third channel layer height between about 5 nm to about 30 nm. In some embodiments, the first channel layer 202, the second channel layer 206, and the third channel layer 208 form a semiconductor composite 205. In some embodiments, an oxide layer 209 is formed over the third channel layer 208 and the STI region 204, as shown in Fig. 3. Let us turn to the Fig. 4-15, where a cross-sectional view of the semiconductor device is illustrated, viewed from a perspective indicated by arrows on line 4-4 in Fig. 3. In some embodiments, a gate 210 is formed over the oxide layer 209, as shown in Fig. 5. In some embodiments, a gate material is formed over the oxide layer 209, and the gate material and the oxide layer 209 are patterned to form a gate structure 213. In some embodiments, the gate 210 comprises at least one of a metal or a polysilicon. In some embodiments, the gate structure 213 comprises a hard mask (not shown) over the gate 210. In some embodiments, first sidewall spacers 212 are formed on sidewalls of the gate 210. In some embodiments, the first sidewall spacers 212 comprise oxide. In some embodiments, a halo implantation 214 is performed on the semiconductor compound 205 to form a halo region 211, as shown in Fig. 6. In some embodiments, the halo implantation 214 comprises implanting at least one of a p-type dopant or an n-type dopant. In some embodiments, a second anneal is performed on the semiconductor composite 205. In some embodiments, the second anneal comprises applying a high temperature between about 400°C and about 1000°C to the semiconductor composite 205. In some embodiments, the second anneal repairs damage to a lattice structure in the semiconductor composite 205 caused by the halo implantation 214 and extends the halo region 211 such that the halo region 211 lies further beneath the gate structure 213 than the halo region 211 was prior to the second anneal, as shown in Fig. 7. In some embodiments, a second sidewall spacer 216 is formed adjacent to the first sidewall spacer 212, as shown in Fig. 8. In some embodiments, the second sidewall spacer comprises a nitride. In some embodiments, an LDD implantation (not shown) follows the halo implantation 214. In some embodiments, the LDD implantation is performed at an angle of less than 20° relative to a line perpendicular to the top surface 205a of the first semiconductor package 205.

[0009] At 108, a first active region layer 220 having a first dopant concentration is formed in the semiconductor compound 205 to form the semiconductor device 200, as shown in Fig. 9. Before Fig. 9, a first opening 218 is formed in the semiconductor compound 205 such that the first opening 218 lies partially under the gate structure 213 and extends into the first channel layer 202, as shown in Fig. 8. In some embodiments, the first opening 218 is formed by etching. In some embodiments, the first opening 218 comprises at least one of a triangular or a convex quadrangular shape. In some embodiments, the first active area layer 220 is formed in the first opening 218, as shown in Fig. 9. In some embodiments, the first active region layer 220 comprises at least one of silicon or germanium. In some embodiments, a first germanium gradient is created during growth of the first active region layer 220 such that a percentage of germanium increases from a bottom surface 220b of the first active region layer 220 to a lowermost top surface 220a of the first active region layer 220. In some embodiments, the bottom surface 220b of the first active region layer 220 has a concentration between about 10% germanium and about 30% germanium, and the lowermost top surface 220a of the first active region layer 220 has a concentration between about 15% germanium and about 40% germanium. In some embodiments, the first dopant comprises a first p-type dopant, such as boron or undoped intrinsic boron. In some embodiments, the first dopant concentration is below 1 10 19 cm-3of the first p-type dopant. In some embodiments, the first active region layer 220 is undoped. In some embodiments, the first active region layer 220 is grown in the presence of the first p-type dopant in the first opening 218, such as by epitaxial growth. In some embodiments, the first active region layer 220 is grown conformally to the first opening 218 such that the first active region layer 220 comprises at least one of a triangular or convex quadrangular shape. In some embodiments, the first active region layer 220 has a uniform thickness. In some embodiments, the first active region layer 220 does not have a uniform thickness.In some embodiments, the first active area layer 220 has a first active area layer thickness 229 between about 5 nm and about 30 nm, where the thickness is measured from the bottom surface 220b of the first active area layer 220 to the lowermost top surface 220a of the first active area layer 220. In some embodiments, the first active area layer 220 includes a tip portion 231 that extends furthest below the gate structure 213. In some embodiments, the tip portion 231 is separated from a bottom surface of the gate structure 213 by a first distance 230, where the first distance 230 is less than about 10 nm. In some embodiments, the tip portion 231 is located a second distance 234 below the gate structure 213, where the second distance is between about 2 nm and about 10 nm.In some embodiments, the first active area layer 220 has a first active area depth 227, measured from the bottom surface 220b of the first active area layer 220 to the top surface 205a of the semiconductor device 205, as shown in FIG. Fig. 9. In some embodiments, the first active region depth 227 is greater than a sum of the second channel layer height and the third channel layer height 228.

[0010] At 110, a second active region layer 222 having a second dopant concentration is formed over the first active region layer 220 in the semiconductor compound 205 to form the semiconductor device 200, as shown in Fig. 10 illustrates, according to some embodiments. In some embodiments, the second active region layer 222 comprises at least one of silicon or germanium. In some embodiments, the second dopant comprises a second p-type dopant, such as boron or heavy intrinsic boron. In some embodiments, the second dopant concentration is greater than the first dopant concentration. In some embodiments, a second germanium gradient is created during formation of the second active region layer 222 such that a percentage of germanium increases from a bottom surface of the second active region layer 222 to a top surface 222a of the second active region layer 222.In some embodiments, the bottom surface of the second active region layer 222 has a concentration between about 20% germanium and about 50% germanium, and the top surface 222a of the second active region layer 222 has a concentration between about 30% germanium and about 60% germanium. In some embodiments, the second active region layer 222 has a constant germanium mole fraction between about 30% germanium and about 60% germanium. In some embodiments, the second dopant concentration is between about 5 10 . 19 cm -3 and about 5·10 20 cm -3of the second p-type dopant. In some embodiments, the second active region layer 222 is grown in the presence of the second p-type dopant in the first opening 218 over the first active region layer 220, such as by epitaxial growth. In some embodiments, the second active region layer 222 is grown such that the second active region layer 222 fills the first opening 218. In some embodiments, the second active region layer 222 has a second active region layer thickness between about 10 nm and about 40 nm, where the second active region layer thickness is measured from the lowest top surface 220a of the first active region layer 220 to the top surface 222a of the second active region layer 222.

[0011] At 112, a third active region layer 224 having a third dopant concentration is formed over the second active region layer 222 and over the semiconductor compound 205 to form the semiconductor device 200, as shown in Fig. 11, according to some embodiments. In some embodiments, the first active region layer 220, the second active region layer 222, and the third active region layer 224 comprise an active region 207. In some embodiments, the third active region layer 224 comprises at least one of silicon or germanium. In some embodiments, the third active region layer 224 has a concentration of less than 50% germanium. In some embodiments, the third dopant comprises a third p-type dopant, such as boron or heavy intrinsic boron. In some embodiments, the third dopant concentration is greater than the second dopant concentration. In some embodiments, the third dopant concentration comprises between about 3 10 20 cm -3 and about 5·10 21 cm -3of the third p-type dopant. In some embodiments, the third active region layer 224 is grown in the presence of the third p-type dopant over the second active region layer 222 and over the top surface 205a of the semiconductor composite 205, such as by epitaxial growth, such that the third active region layer 224 is adjacent to the gate structure 213. In some embodiments, the third active region layer 224 is grown such that the third active region layer 224 is on the top surface 222a of the second active region layer 222 and the first active region layer 220. In some embodiments, the third active region layer 224 is patterned such that the third active region layer 224 is on the top surface 222a of the second active region layer 222 and not the topmost top surface 220c of the first active region layer 220.In some embodiments, the third active region layer 224 has a third active region layer thickness between about 5 nm and about 20 nm, where the third active region layer thickness is measured from the top surface 222a of the second active region layer 222 to a top surface 224a of the third active region layer 224. In some embodiments, the second spacer 216 is removed. In some embodiments, the active region 207 includes at least one of a source or a drain. In some embodiments, a channel 219 is formed under the gate structure 213 and adjacent to the active region 207. In some embodiments, the boron and the first germanium gradient in the first active region layer 220 provide short channel control compared to an active region that does not include at least one of a first germanium gradient or the first dopant concentration.In some embodiments, the increased second dopant concentration in the second active area layer 222 reduces a source / drain extension resistance and a source / drain spreading resistance compared to an active area not including the second active area layer 222. In some embodiments, the third active area layer reduces a silicon contact resistance compared to an active area not having the third active area layer 224. In some embodiments, the semiconductor device 200 has less local variation compared to a device not including the structure of the semiconductor device 200. In some embodiments, the local variation includes a variation in dopant saturation in a first semiconductor device on a chip compared to a dopant saturation on a second semiconductor device on the chip.In some embodiments, the local variation includes line edge roughness (LER) variation in a first semiconductor device on a chip compared to the LER of a second semiconductor device on the chip. In some embodiments, the semiconductor device 200 has less global variation compared to a device that does not include the structure of the semiconductor device 200. In some embodiments, the global variation includes a dimensional variation in a channel width of a first semiconductor device on a chip compared to a channel width of a second semiconductor device on the chip. The configuration of the active areas improves drive current and reduces contact resistance, and the channel configuration improves short channel control compared to a semiconductor device without the configuration of the active areas and channels.

[0012] At 108, a first active region layer 320 having a first dopant concentration is formed in the semiconductor compound 205 to form the semiconductor device 300, as shown in Fig. 13. Before Fig. 13, a first opening 318 is formed in the semiconductor compound 205 such that the first opening 318 lies partially under the gate structure 213 and extends into the first channel layer 202, as shown in Fig. 12. In some embodiments, the first opening 318 is formed by etching. In some embodiments, the first opening 318 comprises at least one of a pentagonal shape or another shape comprising a polygon. In some embodiments, the first active area layer 320 is formed in the first opening, as shown in Fig. 13. In some embodiments, the first active region layer 320 comprises silicon. In some embodiments, the first dopant comprises a first n-type dopant, such as phosphorus or intrinsically doped phosphorus. In some embodiments, the first active region layer 320 comprises less than about 5% carbon. In some embodiments, the first dopant concentration comprises between about 1 10 20 cm -3 and about 3·10 20 cm -3of the first n-type dopant. In some embodiments, the first active area layer 320 is grown in the presence of the first n-type dopant in the first opening 318, such as by epitaxial growth. In some embodiments, the first active area layer 320 is grown conformal to the first opening 318 such that the first active area layer 320 comprises at least one of a pentagonal shape or another shape comprising a polygon. In some embodiments, the first active area layer 320 has a uniform thickness. In some embodiments, the first active area layer 320 does not have a uniform thickness. In some embodiments, the first active area layer 320 has a first active area layer thickness 329 between about 10 nm and about 25 nm, such that the thickness is measured from a bottom surface 320b of the first active area layer 320 to a lowermost top surface 320a of the first active area layer 320.In some embodiments, the first active area layer 320 includes a tip portion 331 that extends furthest below the gate structure 213. In some embodiments, the tip portion 331 is separated from the bottom surface of the gate structure 213 by a first distance 330, where the first distance 330 is less than about 10 nm. In some embodiments, the tip portion 331 is located a second distance 334 below the gate structure 213, where the second distance is between about 2 nm and about 10 nm. In some embodiments, the first active area layer 320 has a first active area depth 327, measured from the bottom surface 320b of the first active area layer 320 to the top surface 205a of the semiconductor composite 205, as shown in FIG. Fig. 13. In some embodiments, the first active region depth 327 is greater than a sum of the second channel layer height and the third channel layer height 228.

[0013] At 110, a second active region layer 322 having a second dopant concentration is formed over the first active region layer 320 in the semiconductor compound 205 to form the semiconductor device 300, as shown in Fig. 14, according to some embodiments. In some embodiments, the second active area layer 322 comprises silicon.

[0014] In some embodiments, the second dopant comprises a second n-type dopant, such as phosphorus or highly intrinsically doped phosphorus. In some embodiments, the second dopant concentration is greater than the first dopant concentration. In some embodiments, the second dopant concentration comprises between about 15% and about 35% of the second n-type dopant. In some embodiments, the second dopant concentration comprises between about 2 10 20 cm -3 and about 7·10 20 cm -3of the second n-type dopant. In some embodiments, the second active region layer 322 is grown in the presence of the second n-type dopant in the first opening 318 over the first active region layer 320, such as by epitaxial growth. In some embodiments, the second active region layer 322 is grown such that the second active region layer 322 fills the first opening 318. In some embodiments, the second active region layer 322 has a second active region layer thickness between about 3 nm and about 15 nm, where the second active region layer thickness is measured from the lowest top surface 320a of the first active region layer 320 to a top surface 322a of the second active region layer 322.

[0015] At 112, a third active region layer 324 having a third dopant concentration is formed over the second active region layer 322 and over the semiconductor compound 205 to form the semiconductor device 300, as shown in Fig. 15 illustrates, according to some embodiments. In some embodiments, the first active region layer 320, the second active region layer 322, and the third active region layer 324 comprise an active region 307. In some embodiments, the third active region layer 324 comprises silicon. In some embodiments, the third dopant comprises a third n-type dopant such as phosphorus or highly intrinsically doped phosphorus. In some embodiments, the third dopant concentration comprises between about 3 10 20 cm -3 and about 5·10 21 cm -3of the third n-type dopant. In some embodiments, the third dopant concentration is greater than the second dopant concentration. In some embodiments, the third active region layer 324 is grown in the presence of the third n-type dopant over the second active region layer 322 and over the top surface 205a of the semiconductor composite 205, such as by epitaxial growth, such that the third active region layer 324 is adjacent to the gate structure 213. In some embodiments, the third active region layer 324 is grown such that the third active region layer 324 lies on the top surface 322a of the second active region layer 322 and an uppermost top surface 320c of the first active region layer 320.In some embodiments, the third active region layer 324 is patterned such that the third active region layer 324 lies on the top surface 322a of the second active region layer 322 and not on a top surface 320c of the first active region layer 320. In some embodiments, the third active region layer 324 has a third active region layer thickness between about 5 nm and about 25 nm, where the third active region layer thickness is measured from the top surface 322a of the second active region layer 322 to a top surface 324a of the third active region layer 324. In some embodiments, the second spacer 216 is removed. In some embodiments, the active region 307 includes at least one of a source or a drain. In some embodiments, a channel 319 is formed under the gate structure 213 and adjacent to the active region 307.In some embodiments, the first dopant concentration comprising phosphorus in the first active area layer 320 provides short-channel control compared to an active area not having the first dopant concentration. In some embodiments, the increased second dopant concentration comprising phosphorus in the second active area layer 322 reduces a source / drain extension resistance and a source / drain spreading resistance compared to an active area not including the second active area layer 322. In some embodiments, the third active area layer 324 reduces a silicon contact resistance compared to an active area not having the third active area layer 324. In some embodiments, the semiconductor device 300 has less local variation compared to a device not including the structure of the semiconductor device 300.In some embodiments, semiconductor device 300 has less global variation compared to a device that does not include the structure of semiconductor device 300. The active region configuration improves drive current and reduces contact resistance, and the channel configuration improves short-channel control compared to a semiconductor device without the active region and channel configuration.

[0016] According to some embodiments, a semiconductor device comprises an active region. In some embodiments, an active region comprises a first active region layer having a first dopant concentration, wherein the first active region layer comprises germanium and the percentage of germanium increases from the bottom of the first active region layer to its top surface 220a, a second active region layer having a second dopant concentration, wherein the second active region layer overlies the first active region layer, and a third active region layer having a third dopant concentration. In some embodiments, the third active region layer overlies the second active region layer and extends over a top surface of a semiconductor composite within which the first active region layer and the second active region layer are formed.In some embodiments, the first dopant concentration is lower than the second dopant concentration, and the second dopant concentration is lower than the third dopant concentration.

[0017] According to some embodiments, a method of forming a semiconductor device comprises forming a channel and forming an active region adjacent to the channel. In some embodiments, forming a channel comprises forming a first channel layer in a substrate, forming a second channel layer over the first channel layer, and forming a third channel layer over the second channel layer. In some embodiments, a semiconductor composite comprises the first channel layer, the second channel layer, and the third channel layer.In some embodiments, forming an active region adjacent to the channel comprises forming a first active region layer in the semiconductor compound, the first active region layer having a first dopant concentration, the first active region layer comprising germanium and the percentage of germanium increasing from the bottom of the first active region layer to its top surface 220a, forming a second active region layer in the semiconductor compound, the second active region layer having a second dopant concentration and formed over the first active region layer, and forming a third active region layer over a top surface of the semiconductor compound, the third active region layer having a third dopant concentration and formed over the second active region layer.

[0018] According to some embodiments, a semiconductor device comprises an active region adjacent to a channel. In some embodiments, an active region comprises a first active region layer having a first dopant concentration, wherein the first active region layer comprises germanium, the percentage of germanium increasing from the bottom of the first active region layer to its top surface 220a, a second active region layer having a second dopant concentration, the second active region layer overlying the first active region layer, and a third active region layer having a third dopant concentration. In some embodiments, the third active region layer is overlying the second active region layer and extends over a top surface of a semiconductor assemblage within which the first active region layer and the second active region layer are formed.In some embodiments, the first dopant concentration is lower than the second dopant concentration, and the second dopant concentration is lower than the third dopant concentration.

Claims

[1] Semiconductor device comprising: an active area that includes: a first active region layer (220) having a first dopant concentration, wherein the first active region layer (220) comprises germanium and the percentage of germanium increases from the bottom surface (220b) of the first active region layer (220) to its top surface (220a); a second active region layer (222) having a second dopant concentration, the second active region layer overlying the first active region layer; and a third active region layer (224) having a third dopant concentration, the third active region layer overlying the second active region layer and extending over a top surface of a semiconductor composite within which the first active region layer and the second active region layer are formed, the first dopant concentration being lower than the second dopant concentration and the second dopant concentration being lower than the third dopant concentration. [2] A semiconductor device according to claim 1, comprising: a channel within the semiconductor device and adjacent to the active region, the channel comprising: a first channel layer (202); a second channel layer (206) above the first channel layer; and a third channel layer (208) above the second channel layer. [3] The semiconductor device of claim 2, wherein the first active region layer (220) has a first active region layer depth, the second channel layer (206) has a second channel layer height, and the third channel layer (208) has a third channel layer height, the first active region layer depth being greater than a sum of the second channel layer height and the third channel layer height. [4] The semiconductor device of claim 3, wherein the sum of the second channel layer height and the third channel layer height is at most about 40 nm. [5] A semiconductor device according to any one of claims 2 to 4, wherein the second channel layer (206) comprises at least one of silicon or carbon. [6] The semiconductor device of claim 5, wherein the second channel layer (206) comprises less than about 5% carbon. [7] A semiconductor device according to any one of the preceding claims, wherein: the first dopant concentration below 1·10 19 cm-3 a first p-type dopant; and / or the first dopant concentration between about 1·10 20 cm -3 and about 3·10 20 cm -3 of a first n-type dopant. [8] A semiconductor device according to any one of the preceding claims, wherein: the second dopant concentration between about 5·10 19 cm -3 and about 5·10 20 cm -3 a second p-type dopant; and / or the second dopant concentration between about 2·10 20 cm -3 and about 7·10 20 cm -3 second n-type dopant. [9] A semiconductor device according to any one of the preceding claims, wherein: the third dopant concentration between about 3·10 20 cm -3 and about 5·10 21 cm -3 a third p-type dopant; and / or the third dopant concentration between about 3·10 20 cm-3 and about 5·10 21 cm -3 a third n-type dopant. [10] A semiconductor device according to any one of the preceding claims, wherein the first active region layer (220) has a first germanium gradient and the second active region layer (222) has a second germanium gradient such that a percentage of germanium increases from the first active region layer to the second active region layer. [11] A semiconductor device according to claim 10, wherein: the first germanium gradient comprises between about 10% germanium and about 40% germanium; and / or the second germanium gradient comprises between about 20% germanium and about 60% germanium. [12] A semiconductor device according to any one of the preceding claims 2-11, comprising a gate structure (210) over the channel and adjacent to the third active region layer (224). [13] The semiconductor device of claim 12, wherein a tip portion of the first active area layer (220) extending furthest below the gate structure (210) is separated from a bottom surface of the gate structure (210) by a first distance, the first distance being less than about 10 nm. [14] A method of forming a semiconductor device comprising: Forming a channel, which includes: Forming a first channel layer (202) in a substrate; Forming a second channel layer (206) over the first channel layer; and Forming a third channel layer (208) over the second channel layer, wherein a semiconductor compound comprises the first channel layer, the second channel layer, and the third channel layer; and Forming an active area adjacent to the channel, which includes: Forming a first active region layer (220) in the semiconductor compound, the first active region layer having a first dopant concentration, the first active region layer (220) comprising germanium and the percentage of germanium increasing from the bottom surface (220b) of the first active region layer (220) to its top surface (220a); Forming a second active region layer (222) in the semiconductor compound, the second active region layer having a second dopant concentration and being formed over the first active region layer; and Forming a third active region layer (224) over a top surface of the semiconductor composite, the third active region layer having a third dopant concentration and being formed over the second active region layer. [15] The method of claim 14, wherein forming a channel comprises: implanting a first dopant into the substrate and annealing to form the first channel layer (202); Growing silicon carbide over the first channel layer to form the second channel layer (206); and Growing silicon over the second channel layer to form the third channel layer (208). [16] A method according to claim 14 or claim 15, comprising: Performing a halo implantation into the semiconductor composite before forming the first active region layer (220). [17] The method of any one of claims 14 to 16, wherein forming the first active region layer (220) comprises: Forming a first opening (218) in the semiconductor composite; and Growing at least one of silicon or germanium in the first opening in the presence of at least one of a first n-type dopant or a first p-type dopant, such that the first active region layer (220) comprises at least one of the following: the first dopant concentration below 1·10 19 cm -3 of the first p-type dopant; or the first dopant concentration between about 1·10 20 cm -3 and about 3·10 20 cm -3 of the first n-type dopant. [18] The method of any one of claims 14 to 17, wherein forming the second active region layer (222) comprises: Growing at least one of silicon or germanium over the first active region layer (220) in the presence of at least one of a second n-type dopant or a second p-type dopant such that the second active region layer (222) comprises at least one of the following: the second dopant concentration between about 5·10 19 cm -3 and about 5·10 20 cm -3 the second p-type dopant; or which has a second dopant concentration between about 2·10 20 cm -3 and about 7·10 20 cm -3 of the second n-type dopant. [19] The method of any one of claims 14 to 18, wherein forming the third active region layer (224) comprises: Growing at least one of silicon or germanium over the second active region layer (222) in the presence of at least one of a third n-type dopant or a third p-type dopant such that the third active region layer (224) comprises at least one of the following: the third dopant concentration between about 3·10 20 cm -3 and about 5·10 21 cm -3 the third p-type dopant; or the third dopant concentration between about 3·10 20 cm -3 and about 5·10 21 cm -3 of the third n-type dopant. [20] Semiconductor device comprising: an active area adjacent to a channel that includes: a first active region layer (220) in a semiconductor compound, the first active region layer having a first dopant concentration, the first active region layer (220) comprising germanium and the percentage of germanium increasing from the bottom surface (220b) of the first active region layer (220) to its top surface (220a); a second active region layer (222) in the semiconductor compound, the second active region layer having a second dopant concentration and formed over the first active region layer; and a third active region layer (224) over a top surface of the semiconductor composite, the third active region layer having a third dopant concentration and formed over the second active region layer, the first dopant concentration being lower than the second dopant concentration and the second dopant concentration being lower than the third dopant concentration.

Citation Information

Patent Citations

  • CMOS structure including differential channel stressing layer compositions

    US20080224218A1

  • CMOS semiconductor devices having stressor regions and related fabrication methods

    US20130069123A1