Formation of a higher-k interface in ferroelectric field-effect devices
By replacing low-k interface layers with higher-k materials like hafnium dioxide in FE-FETs, the issues of high electric and depolarization fields are mitigated, enhancing data retention and reducing power consumption.
Patent Information
- Application Number
- DE102017219741
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2017-05-24
- Filing Date
- 2017-11-07
- Publication Date
- 2024-11-07
- Estimated Expiration
- 2037-11-07
AI Technical Summary
Existing ferroelectric field effect transistors (FE-FETs) face issues with high electric fields and depolarization fields due to low-k interface layers, leading to instability in the stored state and insufficient switching capabilities.
Replace the low-k silicon dioxide or silicon oxide nitride interface layers with higher-k interface layers, such as hafnium dioxide, to reduce permittivity differences and lower operating voltages, thereby reducing depolarization fields and improving data retention.
The higher-k interface layers enhance data retention, reduce power consumption, and minimize charge trapping, resulting in improved ferroelectric response and extended service life.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
[0001] Embodiments relate to a ferroelectric semiconductor component, and in particular to a ferroelectric field-effect device. Further embodiments relate to a method for fabricating a ferroelectric field-effect device. Some embodiments relate to the formation of a higher-k interface in ferroelectric field-effect devices.
[0002] Fig. Figure 1 shows a schematic cross-sectional view of a typical perovskite-based ferroelectric field-effect transistor (FE-FET). The FE-FET includes a silicon substrate 10, a silicon oxide (SiO2) layer 12 formed on the silicon substrate 10, an interface layer 14 formed on the silicon oxide layer 12, a perovskite-based ferroelectric layer 16 formed on the interface layer 14, and a gate 18 formed on the perovskite-based ferroelectric layer 16. The perovskite-based ferroelectric layer 16 may have a thickness greater than 100 nm and a dielectric constant much greater than 100 (k>>100). The silicon oxide layer 12 may have a thickness of approximately 1 nm and a dielectric constant of approximately 4 (k ~ 4). The interface layer 14 may comprise hafnium dioxide (HfO2) or zirconium dioxide (ZrO2) and may have a thickness of approximately10 to 20 nm and a dielectric constant of approximately 10 - 40 (k ~ 10-40). As shown in . Fig. As shown in Figure 1, both the silicon oxide layer 12 and the interface layer 14 are paraelectric layers. Thus, the silicon oxide layer 12 grows during the deposition of the interface layer 14 and / or during other FE-FET fabrication processes. However, the silicon oxide layer 12 does not have a negative impact on the functionality of the FE-FET due to the field distribution in the layer stack of the FE-FET. In contrast to the silicon oxide layer 12, the interface layer 14 is intentionally formed as an interface between the silicon oxide layer 12 and the perovskite-based ferroelectric layer 16, since perovskite (e.g., lead zirconate titanate (PZT)) is not stable on silicon.
[0003] US 2009 / 0261395 A1 and US 9,269,785 B2 disclose a ferroelectric field effect transistor (FE-FET) with doped / undoped hafnium dioxide (HfO2), wherein a top electrode which is conductive and has a low temperature results in a metal ferroelectric insulator semiconductor (MFIS) structure type in a CMOS compatible process flow, as in Fig. 2 is shown.
[0004] In detail, Fig. 2 shows a schematic cross-sectional view of a conventional ferroelectric field-effect transistor. The ferroelectric field-effect transistor includes a semiconductor substrate 20, an insulator layer (or interface layer) 22 formed on the semiconductor substrate 20, a ferroelectric layer 24 comprising doped / undoped hafnium dioxide (HfO2) formed on the insulator layer 22, and a metal gate 26 formed on the ferroelectric layer 24.
[0005] MFIS structures in state-of-the-art applications ( Fig. 2) utilize a low-k interface layer 22 based on silicon dioxide (SiO2) or silicon oxide nitride (SiON), resulting in a capacitor divider between the interface layer 22 and the ferroelectric layer 24, as shown in Fig. 3 is specified.
[0006] The prior art low-k interface layer 22, based on silicon dioxide (SiO2) or silicon oxynitride (SiON or SiOxNy), results in the following disadvantages. First, a sufficient switching field in the ferroelectric layer 24 causes a high electric field in the interface layer 22 (close to the breakdown voltage). Second, the capacitor divider generates a depolarization field in the stack, causing a stored state in the ferroelectric layer 24 to become unstable.
[0007] US 2006 / 0 017 120 A1 describes a ferroelectric memory cell with a substrate, an interface layer, a ferroelectric layer, and a gate electrode, wherein the ferroelectric layer can comprise SrBi2Ta2O9, SrBi2(Ta1-zNbz)2O9, Bi4Ti3O12, Bi4-zLazTi3O12, PbZr1-zTizO3, and YMnO3, and wherein the interface layer can comprise HfO2+u.
[0008] US 2006 / 0 044 863 A1 describes a memory cell with a substrate, a dielectric layer, a trapping layer and a control layer, wherein the trapping layer can comprise HfOx, and wherein the dielectric layer can comprise SiN or SiON.
[0009] Therefore, it is the object of the present invention to create a concept that makes it possible to reduce the high electric fields in the interface layer of the FE-FET and to reduce the electric depolarization field in the layer stack of the FE-FET.
[0010] This problem is solved by the independent patent claims.
[0011] Advantageous implementations are dealt with in the dependent patent claims.
[0012] Embodiments already provide a semiconductor component comprising a semiconductor substrate, an interface layer formed on the semiconductor substrate, an at least partially ferroelectric layer formed on the interface layer, and a connection layer formed on the at least partially ferroelectric layer. Thus, the interface layer between the semiconductor substrate and the at least partially ferroelectric layer has a dielectric constant greater than 5.
[0013] According to the concept of the present invention, the silicon dioxide (SiO2) or silicon oxide nitride (SiON or SiO x N y) low-k interface layer is replaced with a higher-k interface layer, i.e., an interface layer with a dielectric constant greater than 5. This has the advantage of reducing the electric depolarization field caused by the permittivity difference between the interface layer and the ferroelectric layer. Furthermore, the operating voltage can be lowered, data retention performance can be improved, and interface trapping can be reduced.
[0014] Advantageous implementations of the semiconductor device are described below.
[0015] In embodiments, the interface layer may be formed directly on the semiconductor substrate, ie, without another layer between them.
[0016] In embodiments, an interface layer (k>5) may be formed directly on the substrate layer, ie, without a further layer, for example a SiO2 layer, between them.
[0017] In embodiments, the at least partially ferroelectric layer may be formed directly on the interface layer, ie, without a further layer between them.
[0018] In embodiments, the connection layer may be formed directly on the at least partially ferroelectric layer, ie, without a further layer between them.
[0019] In embodiments, the interface layer may be a paraelectric layer.
[0020] In embodiments, the at least partially ferroelectric layer may have a dielectric constant between 10 and 50.
[0021] In embodiments, the interface layer may have a layer thickness between 0.1 and 3 nm.
[0022] In embodiments, the at least partially ferroelectric layer may have a layer thickness between 3 and 50 nm.
[0023] In embodiments, the at least partially ferroelectric layer may comprise hafnium dioxide (HfO2) or ferroelectric hafnium dioxide (HfO2).
[0024] In embodiments, the at least partially ferroelectric layer may be doped with at least one of the following: silicon (Si), zirconium (Zr), lanthanum (La), yttrium (Y), aluminum (Al), gadolinium (Gd), and strontium (Sr).
[0025] In embodiments, the at least partially ferroelectric layer may be a ferroelectric hafnium dioxide (HfO2) layer or an at least partially ferroelectric hafnium dioxide (HfO2) layer. For example, the at least partially ferroelectric layer may be a hafnium dioxide (HfO2) layer that is doped or at least partially doped (e.g., doped regions or implants). Furthermore, the at least partially ferroelectric layer may be an undoped hafnium dioxide (HfO2) layer.
[0026] In embodiments, the at least partially ferroelectric layer may comprise at least two hafnium dioxide (HfO2) sublayers with an intercalation of a metallic or dielectric layer.
[0027] In embodiments, the at least one of the at least two hafnium dioxide (HfO2) sublayers may be doped with at least one of the following: silicon (Si), zirconium (Zr), lanthanum (La), yttrium (Y), aluminum (Al), gadolinium (Gd), and strontium (Sr).
[0028] In embodiments, the interface layer may be an insulating layer.
[0029] In embodiments, the interface layer may comprise aluminum(III) oxide (Al2O3), rare earth dioxide, aluminum nitride (AIN) or silicon nitride (Si3N4).
[0030] In embodiments, the semiconductor device may be a ferroelectric field effect device such as a ferroelectric field effect transistor or a ferroelectric memory cell.
[0031] Further embodiments provide a semiconductor device comprising a semiconductor substrate, an interface layer formed on the semiconductor substrate, a hafnium dioxide (HfO2) layer formed on the interface layer, wherein the hafnium dioxide (HfO2) layer is ferroelectric or at least partially ferroelectric, and a gate layer formed on the hafnium dioxide (HfO2) layer. Thus, the interface layer between the substrate and the HfO2 layer has a dielectric constant greater than 5.
[0032] Further embodiments provide a method for producing a semiconductor component. The method comprises a step of providing a semiconductor substrate. The method further comprises a step of providing an interface layer on the substrate, wherein the interface layer has a dielectric constant greater than 5. The method further comprises a step of providing a hafnium dioxide (HfO2) layer on the interface layer, wherein the hafnium dioxide (HfO2) layer is ferroelectric or at least partially ferroelectric. The method further comprises a step of providing a gate layer on the hafnium dioxide (HfO2) layer.
[0033] In embodiments, the method may further comprise a step of removing an oxide layer from the semiconductor substrate before providing the interface layer on the substrate layer.
[0034] In embodiments, the step of providing the interface layer may comprise depositing the interface layer on the substrate while avoiding silicon dioxide (SiO2) growth.
[0035] In embodiments, the step of providing an interface layer may comprise applying an oxygen-free layer as the interface layer, wherein process chemicals used during the application of the interface layer do not comprise oxidation sources.
[0036] In embodiments, the step of depositing the interfacial layer may comprise low-temperature deposition of an interfacial layer comprising oxygen, wherein process chemicals used during deposition of the interfacial layer comprise only a weak oxidation source.
[0037] In embodiments, the step of providing the hafnium dioxide (HfO2) layer comprises depositing the HfO2 layer on the interfacial layer while avoiding SiO2 growth.
[0038] In embodiments, the hafnium dioxide (HfO2) layer may be deposited using a temperature lower than a temperature required for silicon dioxide (SiO2) growth.
[0039] In embodiments, an oxygen source may be reduced while the hafnium dioxide (HfO2) layer is applied.
[0040] Embodiments of the present invention are described herein with reference to the attached drawings. Fig. 1 shows a schematic cross-sectional view of a prior art perovskite-based ferroelectric field-effect transistor (FE-FET); Fig. Figure 2 shows a schematic cross-sectional view of a prior art doped / undoped hafnium dioxide (HfO2) FE-FET based on a metal-ferroelectric-insulator-semiconductor (MFIS) structure; Fig. 3 shows an equivalent circuit of the Fig. 2 shows the prior art FE-FET based on the MFIS structure; Fig. 4 shows a schematic cross-sectional view of a semiconductor device according to an embodiment; Fig. 5 shows a flowchart of a method for manufacturing a semiconductor device according to an embodiment; Fig. Figure 6 shows a TEM image illustrating interface-free growth of a higher-k layer and ferroelectric hafnium dioxide (HfO2); and Fig. Figure 7 shows a diagram of the depolarization field plotted across a permittivity of the interface layer.
[0041] Identical or equivalent elements or elements with identical or equivalent functionality are identified by identical or equivalent reference symbols in the following description.
[0042] In the following description, numerous details are set forth to provide a more thorough explanation of embodiments of the present invention. However, it will be apparent to those skilled in the art that embodiments of the present invention may be practiced without these specific details. In other instances, well-known structures and devices are shown in block diagram form rather than in detail to avoid obscuring embodiments of the present invention. Furthermore, features of the various embodiments described below may be combined with one another unless expressly stated otherwise.
[0043] Fig. 4 shows a schematic cross-sectional view of a semiconductor device 100 according to an embodiment. The semiconductor device 100 includes a semiconductor substrate 102, an interface layer 104 formed on the semiconductor substrate 102, an at least partially ferroelectric layer 106 formed on the interface layer 104, and a terminal layer 108 formed on the at least partially ferroelectric layer 106. Thus, the interface layer 104 between the semiconductor substrate 102 and the at least partially ferroelectric layer 106 has a dielectric constant greater than 5.
[0044] As in Fig. 4, the conventional silicon dioxide (SiO2) / silicon oxynitride (SiON)-based low-k interface layer (k<5) (cf. Fig. 2) by an interface layer with a higher dielectric constant (permittivity) k int replaced.
[0045] In embodiments, the interface layer 104 may be formed directly on the semiconductor substrate (e.g., silicon substrate) 102, i.e., without a silicon dioxide (SiO2) or silicon oxide nitride (SiON or SiO x N y ) layer between them. The interface layer 104 can have a layer thickness between 0.5 and 1.5 nm and / or a dielectric constant greater than 5, e.g., between 7 and 20. The interface layer 104 can, for example, have a dielectric constant between 8 and 10 for aluminum dioxide (Al2O3), between 7 and 8 for silicon nitride (SiN or SiO x N y ), between 9 and 10 for aluminum nitride (AIN) and between 10 and 20 for rare earth dioxides.
[0046] The interface layer 104 may, for example, comprise or include aluminum(III) oxide (Al2O3), rare earth dioxide, aluminum nitride (AIN) or silicon nitride (Si3N4).
[0047] In embodiments, the at least partially ferroelectric layer 106 may be formed directly on the interface layer 104, i.e., without another layer between them. The at least partially ferroelectric layer 106 may have a layer thickness between 5 and 20 nm and / or a dielectric constant between 10 and 40.
[0048] The at least partially ferroelectric layer 106 may comprise, for example, hafnium dioxide (HfO2) or ferroelectric hafnium dioxide (HfO2) and may optionally be doped or partially doped with one of the following: silicon (Si), zirconium (Zr), lanthanum (La), yttrium (Y), aluminum (Al), gadolinium (Gd), and strontium (Sr).
[0049] The at least partially ferroelectric layer 106 can, for example, comprise at least two hafnium dioxide (HfO2) sublayers with an intercalation of a metallic or dielectric layer. Thus, at least one of the at least two hafnium dioxide (HfO2) sublayers can be doped with at least one of the following: silicon (Si), zirconium (Zr), lanthanum (La), yttrium (Y), aluminum (Al), gadolinium (Gd), and strontium (Sr).
[0050] Fig. 5 shows a flowchart of a method 200 for manufacturing a semiconductor device. The method 200 comprises a step 202 of providing a substrate. The method 200 further comprises a step 204 of providing an interface layer on the substrate, wherein the interface layer has a dielectric constant greater than 5. The method 200 further comprises a step 206 of providing an HfO2 layer on the interface layer, wherein the HfO2 layer is ferroelectric or at least partially ferroelectric. The method 200 further comprises a step 208 of providing a gate layer on the HfO2 layer.
[0051] In embodiments, the method 200 may further include a step of removing an oxide layer from the semiconductor substrate 102 before the interface layer 104 is provided on the semiconductor substrate 102.
[0052] In embodiments, the interface layer 104 passivates the surface of the semiconductor substrate (e.g., the silicon substrate) 102 to such an extent that no oxidation (so-called SiO2 restoration) of the semiconductor substrate 102 occurs during the subsequent processes of manufacturing the semiconductor device 100, or at least to such an extent that the oxidation of the semiconductor substrate 102 can be reduced or even minimized during the subsequent processes of manufacturing the semiconductor device 100.
[0053] In embodiments, the step of providing the interface layer may comprise depositing the interface layer on the semiconductor substrate while avoiding silicon dioxide (SiO2) growth.
[0054] For example, the step of depositing the interfacial layer 104 may include depositing an oxygen-free layer such as aluminum nitride (AIN) or silicon nitride (Si3N4) as the interfacial layer, wherein process chemicals used during the depositing of the interfacial layer 104 do not have oxidation sources, so that no silicon dioxide (SiO2) growth is possible.
[0055] For example, the step of depositing the interfacial layer may comprise low-temperature deposition of an interfacial layer comprising oxygen, for example, aluminum(III) oxide (Al2O3), wherein process chemicals used during deposition of the interfacial layer comprise only a weak oxidation source in a low concentration, for example, water (H2O).
[0056] In embodiments, the step of providing the hafnium dioxide (HfO2) layer comprises depositing the HfO2 layer on the interfacial layer while avoiding SiO2 growth.
[0057] For example, the hafnium dioxide (HfO2) layer may be deposited using a temperature lower than a temperature required for silicon dioxide (SiO2) growth, such that the interfacial layer 104 passivates a surface of the semiconductor substrate.
[0058] For example, an oxygen source can be reduced while the hafnium dioxide (HfO2) layer is deposited depending on the required process temperature to avoid silicon dioxide (SiO2) growth.
[0059] In embodiments, method 200 provides a cleaning sequence to remove a silicon dioxide (SiO2) interfacial layer and perform subsequent ALD (atomic layer deposition) without silicon dioxide (SiO2) interfacial restoration.
[0060] In embodiments, method 200 provides an ALD process to deposit a higher-k interfacial layer without silicon dioxide (SiO2) growth on a cleaned silicon interfacial layer.
[0061] Fig. Figure 6 shows a TEM image illustrating interface-free growth of a higher-k layer and ferroelectric hafnium dioxide (HfO2).
[0062] The embodiments described herein offer the following advantages. An increase in k int reduces the stack-inherent depolarization field and the operating voltage: Edep=k*P1+kint*dFEkFe*dInt
[0063] Fig. Figure 7 shows a diagram of the depolarization field which is generated over a permittivity of the interface layer 104 k int is shown across.
[0064] The advantage of the reduced depolarization field improves the device's data retention. The advantage of the lower operating voltage leads to a reduced interface field, which reduces the amount of trapped charge and thus improves lifetime. Furthermore, the advantage of the lower operating voltage leads to lower power consumption and less or no charge pumping.
[0065] In embodiments, a low-k interface layer is replaced by a high-k interface layer to reduce an electric depolarization field caused by the permittivity difference between the interface layer and ferroelectric hafnium dioxide (FE-HfO).
[0066] Embodiments provide a sequence of removing a low-k interface followed by ALD of higher-k material with process parameters to suppress interface growth.
[0067] Embodiments described herein are applicable to all CMOS process flows: HKMG (HKMG = high k metal gate), RMG (RMG = replacement metal gate), FinFET, SOI (SOl = silicon on insulator).
[0068] Embodiments offer the following key advantages: First, lower operating voltages. Second, better data retention. Third, reduced interfacial layer trapping.
[0069] Embodiments described herein improve the ferroelectric response, lifetime, and maintenance of a new ferroelectric hafnium dioxide (HfO2)-based material system that provides benefits for ferroelectric memory applications by improving the capacitor divider between the interface and the ferroelectric HfO2, thereby reducing the inherent depolarization field (E dep ) and lowering operating voltages, which are essential for parasitic charge trapping.
[0070] In embodiments, ferroelectric HfO2 is defined as undoped and doped (Si, Zr, La, Y, Al, Gd, Sr) hafnium dioxide (HfO2) and as a combination in multilayer structures of doped (Si, Zr, La, Y, Al, Gd, Sr - with unlimited amount of dopant and number of dopants) or undoped HfO2 layers with an intercalation of thin films (metallic or dielectric).
[0071] Although some aspects have been described in the context of an apparatus, it should be understood that these aspects also represent a description of the corresponding method, so that a block or component may also be understood as a corresponding method step or as a feature of a method step. Analogously, aspects described in the context of a method step also represent a description of a corresponding block, detail, or feature of a corresponding apparatus. Some or all of the method steps may be performed by or using a hardware device, such as a microprocessor, a programmable computer, or electronic circuitry. In some embodiments, one or more of the key method steps may be performed by such an apparatus.
[0072] Depending on specific implementation requirements, embodiments of the invention may be implemented in hardware or software. The implementation may be performed using a digital storage medium, such as a floppy disk, DVD, Blu-ray, CD, ROM, PROM, EPROM, EEPROM, or FLASH memory, on which electronically readable control signals are stored that can interact or interact with a programmable computer system to perform the respective method. Therefore, the digital storage medium may be computer-readable.
[0073] Some embodiments according to the invention comprise a data carrier having electronically readable control signals capable of interacting with a programmable computer system such that one of the methods described herein is carried out.
[0074] In general, embodiments of the present invention can be implemented as a computer program product with program code, wherein the program code is effective to perform one of the methods when the computer program product is run on a computer. The program code can, for example, be stored on a machine-readable medium.
[0075] Other embodiments include the computer program for performing one of the methods described herein, wherein the computer program is stored on a machine-readable carrier.
[0076] In other words, an embodiment of the method according to the invention is thus a computer program which has a program code for carrying out one of the methods described herein when the computer program runs on a computer.
[0077] A further embodiment of the method according to the invention is thus a data carrier (or a digital storage medium or a computer-readable medium) on which the computer program for performing one of the methods described herein is recorded. The data carrier, the digital storage medium, or the recorded medium is typically tangible and / or non-volatile.
[0078] A further embodiment of the method according to the invention is thus a data stream or a sequence of signals that represents the computer program for carrying out one of the methods described herein. The data stream or the sequence of signals can be configured, for example, to be transferred via a data communication connection, for example, via the Internet.
[0079] A further embodiment comprises a processing device, for example a computer or a programmable logic device, which is configured or adapted to carry out one of the methods described herein.
[0080] A further embodiment comprises a computer on which the computer program for performing one of the methods described herein is installed.
[0081] A further embodiment according to the invention comprises a device or system configured to transmit a computer program for performing one of the methods described herein to a recipient. The transmission may, for example, be electronic or optical. The recipient may, for example, be a computer, a mobile device, a storage device, or a similar device. The device or system may, for example, comprise a file server for transmitting the computer program to the recipient.
[0082] In some embodiments, a programmable logic device (e.g., a field-programmable gate array, an FPGA) may be used to perform some or all of the functionality of the methods described herein. In some embodiments, a field-programmable gate array may interact with a microprocessor to perform any of the methods described herein. In general, the methods are preferably performed by any hardware device.
[0083] The apparatus described herein may be implemented using a hardware device or using a computer or using a combination of a hardware device and a computer.
[0084] The device described herein or any components of the device described herein may be implemented at least partially in hardware and / or in software.
[0085] The methods described herein may be performed using a hardware device or using a computer or using a combination of a hardware device and a computer.
[0086] The methods described herein or any components of the apparatus described herein may be performed at least partially by hardware and / or by software.
Claims
[1] A semiconductor device (100) having the following features: a substrate (102); an interface layer (104) formed on the substrate (102); an at least partially ferroelectric layer (106) formed on the interface layer (104); a terminal layer (108) formed on the at least partially ferroelectric layer (106); wherein the interface layer (104) between the substrate (102) and the at least partially ferroelectric layer (106) has a dielectric constant greater than 5; wherein the at least partially ferroelectric layer (106) comprises HfO2 or ferroelectric HfO2; and wherein the interface layer (104) comprises Al2O3, rare earth oxides (oxides of Sc, Y, La, Ce, Pr, Nd, Pm, Sm, Eu, Gd, Rb, Dy, Ho, Er, Tm, Yb, Lu), AlN or Si3N4. [2] The semiconductor device (100) according to the preceding claim, wherein the interface layer (104) is formed directly on the substrate (102). [3] The semiconductor device (100) according to one of the preceding claims, wherein the connection layer (108) is formed directly on the at least partially ferroelectric layer (106) and / or wherein the at least partially ferroelectric layer (106) is formed directly on the interface layer (104). [4] The semiconductor device (100) according to any one of the preceding claims, wherein the interface layer (104) is a paraelectric layer. [5] The semiconductor device (100) according to any one of the preceding claims, wherein the at least partially ferroelectric layer (106) has a dielectric constant between 10 and 50. [6] The semiconductor device (100) according to any one of the preceding claims, wherein the interface layer (104) has a layer thickness between 0.1 and 3 nm. [7] The semiconductor component (100) according to one of the preceding claims, wherein the at least partially ferroelectric layer (106) has a layer thickness between 5 and 20 nm. [8] The semiconductor device (100) according to any one of the preceding claims, wherein the at least partially ferroelectric layer (106) is doped with at least one of the following: Si, Zr, La, Y, Al, Gd and Sr. [9] The semiconductor device (100) according to any one of the preceding claims, wherein the at least partially ferroelectric layer (106) is a ferroelectric HfO2 layer or an at least partially ferroelectric HfO2 layer. [10] The semiconductor component (100) according to one of the preceding claims, wherein the at least partially ferroelectric layer (106) comprises at least two HfO2 sub-layers with an intercalation of a metallic or dielectric layer. [11] The semiconductor device (100) according to the preceding claim, wherein at least one of the at least two HfO2 sublayers is doped with at least one of the following: Si, Zr, La, Y, Al, Gd and Sr. [12] The semiconductor device (100) according to any one of the preceding claims, wherein the interface layer (104) is an insulating layer. [13] The semiconductor device (100) according to any one of the preceding claims, wherein the semiconductor device (100) is a ferroelectric field effect transistor or a ferroelectric memory cell. [14] A semiconductor device (100) having the following features: a substrate (102); an interface layer (104) formed on the substrate; an HfO2 layer (106) formed on the interface layer (104), wherein the HfO2 layer (106) is ferroelectric or at least partially ferroelectric; a gate layer (108) formed on the HfO2 layer (106); wherein the interface layer (104) between the substrate (102) and the HfO2 layer (106) has a dielectric constant greater than 5; wherein the interface layer (104) comprises Al2O3, rare earth oxides (oxides of Sc, Y, La, Ce, Pr, Nd, Pm, Sm, Eu, Gd, Rb, Dy, Ho, Er, Tm, Yb, Lu), AlN or Si3N4. [15] A method (200) for manufacturing a semiconductor device, the method comprising the following steps: Providing (202) a substrate; Providing (204) an interface layer on the substrate, the interface layer having a dielectric constant greater than 5; Providing (206) an HfO2 layer on the interface layer, wherein the HfO2 layer is ferroelectric or at least partially ferroelectric; and Providing (208) a gate layer on the HfO2 layer; wherein the interface layer (104) comprises Al2O3, rare earth oxides (oxides of Sc, Y, La, Ce, Pr, Nd, Pm, Sm, Eu, Gd, Rb, Dy, Ho, Er, Tm, Yb, Lu), AlN or Si3N4. [16] The method (200) of manufacturing according to the preceding claim, wherein the method comprises the following step: Removing an oxide layer from the substrate before providing the interface layer on the substrate layer. [17] The method (200) of manufacturing according to any one of the preceding claims, wherein providing the interfacial layer comprises depositing the interfacial layer on the substrate while avoiding SiO2 growth. [18] The method (200) of claim 17, wherein depositing the interfacial layer comprises depositing an O-free layer as the interfacial layer, wherein process chemicals used during depositing the interfacial layer do not comprise oxidation sources. [19] The method (200) of claim 17, wherein depositing the interfacial layer comprises low temperature depositing of an interfacial layer comprising O, wherein process chemicals used during depositing the interfacial layer comprise only a weak oxidation source. [20] The method (200) of manufacturing according to any one of the preceding claims, wherein providing the HfO2 layer comprises depositing the HfO2 layer on the interface layer while avoiding SiO2 growth. [21] The method (200) of claim 20, wherein the HfO2 layer is deposited using a temperature lower than a temperature required for SiO2 growth. [22] The method (200) of claim 20 or 21, wherein the dose of the O source is reduced while the HfO2 layer is deposited.
Citation Information
Patent Citations
Integrated Circuit Including a Ferroelectric Memory Cell and Method of Manufacturing the Same
US20090261395A1
Semiconductor device with ferroelectric hafnium oxide and method for forming semiconductor device
US9269785B2
Semiconductor-ferroelectric storage device and its manufacturing method
US20060017120A1
One-transistor composite-gate memory
US20060044863A1