Ether-based electrolyte system for improving or supporting the anodic stability of electrochemical cells with lithium-containing anodes
Patent Information
- Application Number
- DE102018119769
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2017-08-15
- Filing Date
- 2018-08-14
- Publication Date
- 2024-10-31
- Estimated Expiration
- 2038-08-14
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
INTRODUCTION The following section provides background information to the present disclosure, which is not necessarily prior art. The present disclosure relates to a highly concentrated ether-based electrolyte system of an electrochemical cell having a high-energy cathode and a lithium-containing anode, as well as methods for preparing the highly concentrated electrolyte system and electrochemical cells including the highly concentrated electrolyte system. The electrolyte system includes a bound portion comprising one or more salts associated with and / or bound to an ether-based solvent, wherein the one or more salts have a concentration in the electrolyte system of greater than about 4 M and a molar ratio of the one or more salts to the ether of the ether-based solvent is greater than or equal to about 1 to less than or equal to about 1.5. The bound portion of the electrolyte system enhances or supports the anodic stability of the electrochemical cell. Background: High-energy-density electrochemical cells, such as lithium-ion batteries and lithium-sulfur batteries, can be used in a variety of consumer products and vehicles, such as hybrid electric vehicles (HEVs) and electric vehicles (EVs). Typical lithium-ion batteries include a first electrode, a second electrode, an electrolyte material, and a separator. One electrode serves as the positive electrode, or cathode, and another serves as the negative electrode, or anode. A stack of lithium-ion battery cells can be electrically connected to increase overall power. Conventional rechargeable lithium-ion batteries operate by reversibly shunting lithium ions back and forth between the negative electrode and the positive electrode. A separator and an electrolyte are disposed between the negative electrode and the positive electrode.The electrolyte is suitable for conducting lithium ions and can be in solid (e.g., solid-state diffusion) or liquid form. When charging the battery, lithium ions move from a cathode (positive electrode) to an anode (negative electrode), and when discharging the battery, they move in the opposite direction. Many different materials can be used to manufacture components for a lithium-ion battery. As a non-limiting example, cathode materials for lithium-ion batteries typically comprise an electroactive material that can be intercalated or alloyed with lithium ions, such as lithium transition metal oxides or spinel-type mixed oxides, for example, including spinel LiMn2O4, LiCoO2, LiNiO2, LiMn1.5Ni0.5O4, LiNi(1-xy)CoxMyO2 (where 0 <x<1, y<1, und M können Al, Mn oder dergleichen sein) oder Lithium-Eisenphosphate. Der Elektrolyt enthält typischerweise ein oder mehrere Lithiumsalze, die in einem nichtwässrigen Lösungsmittel gelöst und ionisiert sein können.Common negative electrode materials include lithium insertion materials or alloy host materials, such as lithium graphite intercalation compounds or lithium silicon compounds, lithium tin alloys, and lithium titanate Li4+xTi5O12, where 0 ≤ x ≤ 3, such as Li4Ti5O12(LTO). The negative electrode can also be made of a lithium-containing material such as metallic lithium, so the electrochemical cell is considered a lithium-metal battery or cell. Metallic lithium for use in the negative electrode of a rechargeable battery has several potential advantages, including the highest theoretical capacity and the lowest electrochemical potential. For example, batteries with lithium-metal anodes can have a higher energy density, which can potentially double the storage capacity, allowing the battery to be half the size but still have the same cycle life as other lithium-ion batteries. Thus, lithium-metal batteries are one of the most promising candidates for high-energy storage. However, lithium-metal batteries also have potential disadvantages, including potentially unreliable or reduced performance and possible premature failure of electrochemical cells. Such and comparable electrolyte systems are described, for example, in US 2016 / 0 233 549 A1 and DE 10 2015 121 342 A1. For example, side reactions can occur between the lithium metal and the species in the adjacent electrolyte located between the positive and negative electrodes, promoting power degradation with the negative lithium electrodes, which can impair the coulombic efficiency and lifetime of rechargeable lithium batteries. Accordingly, it would be desirable to develop materials for use in high-energy lithium-ion batteries that reduce or suppress lithium metal side reactions and thereby suppress or minimize the resulting effects. SUMMARY This part provides a general summary of the disclosure and is not a complete disclosure of the full scope or all features.In various aspects, the present disclosure provides a method for preparing an electrolyte system that improves or optimizes the anodic stability of an electrochemical cell that may include a positive and a negative electrode. The positive electrode may include a positive electroactive lithium-based material and have a maximum potential greater than or equal to about 5V. The positive electroactive material is selected from a lithium-based material selected from the group consisting of nickel-manganese-cobalt 811 (NMC811), nickel-manganese-cobalt 622 (NMC622), and combinations thereof. The negative electrode may include a negative electroactive material including lithium.The method may involve mixing one or more salts selected from the group consisting of: lithium bis(fluorosulfonyl)imide (LiFSI), sodium bis(fluorosulfonyl)imide (NaFSI), potassium bis(fluorosulfonyl)imide (KFSI), and combinations thereof, including dimethoxyethane (DME), to form a bound moiety. The bound moiety may have an ionization potential greater than an electron affinity to form an electrolyte system substantially free of unbound dimethoxyethane (DME) and unbound bis(fluorosulfonyl)imide (FSI-). The one or more salts may have a concentration in the electrolyte system of greater than about 4M. A molar ratio of one or more salts to dimethoxyethane (DME) may be greater than or equal to about 1 to less than or equal to about 1.5. In one aspect, the electrolyte system may have a dynamic viscosity of less than about 0.1 Pa*s (100 centipoise (cP)). In one aspect, the electrochemical cell may have an energy density of greater than about 900 Wh / L. In one aspect, the electrolyte system may include one or more electrolyte additives. The electrolyte additives may be selected from the group consisting of: organic silane electrolyte additives, borate-based electrolyte additives, and combinations thereof. In one aspect, the one or more electrolyte additives may include an organic silane electrolyte additive selected from the group consisting of: fluorinated methoxysilanes, fluorinated chlorosilanes, and combinations thereof. In one aspect, the electrolyte system may include one or more electrolyte additives selected from the group consisting of: 3,3,3-trifluoropropylmethyldimethoxysilane, (3,3,3-trifluoropropyl)trimethoxysilane, 1H,1H,2H,2H-perfluorooctylmethyldimethoxysilane, 1H,1H,2H,2H-perfluorooctyltrimethoxysilane, 1H,1H,2H,2H-perfluorooctyldimethylchlorosilane, 1H,1H,2H,2H-perfluorooctylmethyldichlorosilane, (1H,1H,2H,2Hyl-n-hexyl)methyldichlorosilane, 1H,1H,2H,2H-perfluorooctyltrichlorosilane, and combinations thereof. In another variation (not according to the invention), the present disclosure provides another method for improving or optimizing the anodic stability of an electrochemical cell that cycles lithium ions. The method may include introducing an electrolyte system into the electrochemical cell. The electrolyte system may include a bound moiety having an ionization potential greater than an electron affinity. The electrolyte system may include one or more salts bound to a solvent. The electrolyte system may include one or more salts having a concentration in the electrolyte system of greater than 4M. The one or more salts may be selected from the group consisting of: lithium bis(fluorosulfonyl)imide (LiFSI), sodium bis(fluorosulfonyl)imide (NaFSI), potassium bis(fluorosulfonyl)imide (KFSI), and combinations thereof, and the solvent may comprise dimethoxyethane (DME).A molar ratio of one or more salts to dimethoxyethane (DME) may be greater than or equal to about 1 to less than or equal to about 1.5. The electrolyte system may be substantially free of unbound dimethoxyethane (DME) and unbound bis(fluorosulfonyl)imide (FSI). At one point, the electrochemical cell may include a positive and a negative electrode. The positive electrode may include a positive lithium-based electroactive material and have a maximum potential greater than or equal to approximately 5V. The negative electrode may include a negative lithium electrolyte material. In one aspect, the electrolyte system may have a dynamic viscosity of 0.1 Pa*s (100 centipoise (cP)). In one aspect, the electrochemical cell may have an energy density of greater than about 900 Wh / L. In one aspect, the electrolyte system may include one or more electrolyte additives. The electrolyte additives may be selected from the group consisting of: organic silane electrolyte additives, borate-based electrolyte additives, and combinations thereof. In another variation (not according to the invention), the present disclosure provides an electrochemical cell that cycles lithium ions with improved or optimized anodic stability. The electrochemical cell may include a positive electrode, a separator, a negative electrode, and an electrolyte system. The positive electrode may include a positive electroactive lithium-based material and have a maximum potential greater than or equal to about 5V. The negative electrode may include a negative electroactive material including lithium. The electrolyte system may include a bound moiety with an ionization potential greater than an electron affinity and may include one or more salts bound to a solvent.The one or more salts can be selected from the group consisting of: lithium bis(fluorosulfonyl)imide (LiFSI), sodium bis(fluorosulfonyl)imide (NaFSI), potassium bis(fluorosulfonyl)imide (KFSI), and combinations thereof, and the solvent can comprise dimethoxyethane (DME). The one or more salts can have a concentration in the electrolyte system of greater than 4M. A molar ratio of one or more salts to dimethoxyethane (DME) can be greater than or equal to about 1 to less than or equal to about 1.5. The electrolyte system can be substantially free of unbound dimethoxyethane (DME) and unbound bis(fluorosulfonyl)imide (FSI-). In one aspect, the electrolyte system may have a dynamic viscosity of 0.1 Pa*s (100 centipoise (cP)). In one aspect, the electrochemical cell may have an energy density of greater than about 900 Wh / L. In one aspect, the electrolyte system may include one or more electrolyte additives. The electrolyte additives may be selected from the group consisting of: organic silane electrolyte additives, borate-based electrolyte additives, and combinations thereof. In one aspect, the one or more electrolyte additives may include an organic silane electrolyte additive selected from the group consisting of: fluorinated methoxysilanes, fluorinated chlorosilanes, and combinations thereof. In one aspect, the electrolyte system may include one or more electrolyte additives selected from the group consisting of: 3,3,3-trifluoropropylmethyldimethoxysilane, (3,3,3-trifluoropropyl)trimethoxysilane, 1H,1H,2H,2H-perfluorooctylmethyldimethoxysilane, 1H,1H,2H,2H-perfluorooctyltrimethoxysilane, 1H,1H,2H,2H-perfluorooctyldimethylchlorosilane, 1H,1H,2H,2H-perfluorooctylmethyldichlorosilane, (1H,1H,2H,2Hyl-n-hexyl)methyldichlorosilane, 1H,1H,2H,2H,2H-perfluorooctyltrichlorosilane, and combinations thereof. Further areas of applicability will become apparent from the description presented herein. The description and specific examples in this summary are for illustrative purposes only and are in no way intended to limit the scope of the present disclosure. BRIEF DESCRIPTION OF THE DRAWINGS The drawings described herein are for illustrating selected embodiments only and do not represent all possible implementations, nor are they intended to limit the scope of the present disclosure. Fig. 1 is a schematic of an exemplary electrochemical battery cell having a lithium-containing negative electrode; Fig. 2 shows an electrolyte system in which one or more salts have a concentration in the electrolyte system of less than about 4M; Fig. 3 shows an electrolyte system in which one or more salts have a concentration in the electrolyte system of about 5M; Fig. 4 is a graphical representation of the electron affinities and ionization potentials of comparative electrolyte systems; and Fig. 5 is a graphical representation of the capacity retention per cycle of exemplary electrochemical cells. Like reference numerals in the different views of the drawings refer to the same parts. DETAILED DESCRIPTION Example embodiments are provided so that this disclosure will be thorough and will fully convey the scope thereof to those skilled in the art. Numerous specific details are set forth, such as examples of specific compositions, components, devices, and methods, in order to provide a thorough understanding of embodiments of the present disclosure. Those skilled in the art will recognize that specific details may not be required, that example embodiments may be embodied in many different forms, and that no embodiment should be construed to limit the scope of the disclosure. In some example embodiments, well-known methods, well-known device structures, and well-known techniques are not described in detail. The terminology used herein is for the purpose of describing particular exemplary embodiments only and is not intended to be limiting in any way. As used herein, the singular forms "a," "an," and "the" optionally include the plural forms, unless the context clearly precludes them. The terms "comprises," "comprising," "included," and "having" are inclusive and therefore indicate the presence of the specified features, elements, compositions, steps, integers, acts, and / or components, but do not preclude the presence or addition of one or more other features, integers, steps, acts, elements, components, and / or groups thereof.Although the broadly construed term "comprising" is intended to be a non-limiting term used to describe and claim various embodiments set forth herein, in certain aspects, the term may be alternatively understood, such as instead being a more limiting and restrictive term, such as "consisting of" or "consisting essentially of." Thus, any embodiment of the present disclosure that recites compositions, materials, components, elements, functions, integers, operations, and / or method steps expressly includes embodiments of the present disclosure consisting of, or consisting essentially of, such recited compositions, materials, components, elements, functions, integers, operations, and / or method steps.With "consisting of", the alternative embodiment excludes any additional compositions, materials, components, elements, functions, integers, operations, and / or method steps, while with "consisting essentially of", any additional compositions, materials, components, elements, functions, integers, operations, and / or method steps that materially impair the basic and novel properties are excluded from such embodiment, but any compositions, materials, components, elements, functions, integers, operations, and / or method steps that materially do not impair the basic and novel properties may be included in the embodiment. All method steps, processes, and operations described herein should not be construed as requiring the order described or illustrated unless specifically stated as the order of performance. It should also be understood that additional or alternative steps may be used unless otherwise noted. When a component, element, or layer is described as being "on / upon," "engaging with," "connected to," or "coupled to" another component, element, or layer, it may either be directly on / upon, engaged with, connected to, or coupled to the other component, element, or layer, or there may be intervening elements or layers. Conversely, when an element is described as being "directly on / upon," "directly engaging with," "directly connected to," or "directly coupled to" another element or layer, there may be no intervening elements or layers. Other words used to describe the relationship between elements should be understood in the same way (e.g., "between" and "directly between," "adjacent" and "directly adjacent," etc.).As used herein, the term “and / or” includes all combinations of one or more of the related listed items. Although the terms first, second, third, etc. may be used herein to describe various steps, elements, components, regions, layers, and / or sections, these steps, elements, components, regions, layers, and / or sections are not intended to be limiting. These terms are used only to distinguish one step, element, component, region, layer, or section from another step, element, region, layer, or section. Terms such as "first," "second," and other numerical terms, when used herein, do not imply a sequence or order unless clearly indicated by the context.Thus, a first step, discussed first element, discussed component, discussed region, discussed layer, or discussed section discussed below could be referred to as a second step, a second element, a second component, a second region, a second layer, or a second section without departing from the teachings of the exemplary embodiments. Spatial or temporal terms such as "before," "after," "inner," "outer," "below," "below," "lower," "above," "upper," and the like may be used herein to better describe the relationship of one element or characteristic to other element(s) or characteristic(s) as illustrated in the figures. Spatial or temporal terms may be intended to describe various arrangements of the device or system in use or operation, in addition to the orientation illustrated in the figures.Throughout this disclosure, numerical values generally represent approximate measurements or limits of ranges, such as minor deviations from the specific values, and are intended to include embodiments that approximately have the stated value, as well as those having the exact stated value. Contrary to the application examples provided at the end of the detailed description, all numerical values of parameters (e.g., quantities or conditions) in this specification, including the appended claims, are intended in all cases to be understood by the term "approximate," regardless of whether or not "approximately" actually appears before the numerical value. "Approximately" indicates that the disclosed numerical value allows for some imprecision (with some approximation to exactness in the value; approximately or realistically close to the value; approximately).If the imprecision provided by "about" is not otherwise understood by those skilled in the art to have this ordinary meaning, then "about," as used herein, indicates at least variations resulting from ordinary measurement techniques and the use of such parameters. For example, "about" may encompass a variation of less than or equal to 5%, optionally less than or equal to 4%, optionally less than or equal to 3%, optionally less than or equal to 2%, optionally less than or equal to 1%, optionally less than or equal to 0.5%, and under certain circumstances, optionally less than or equal to 0.1%. In addition, the disclosure of ranges includes the disclosure of all values and further subdivided ranges within the entire range, including the endpoints and subranges specified for the ranges. Exemplary embodiments will now be described in more detail with reference to the accompanying drawings. The present technology relates to improved electrochemical cells, particularly lithium-ion or, more specifically, lithium-metal batteries, that can be used in vehicle applications. However, current technology can also be used in other electrochemical devices, particularly those containing lithium, such as lithium-sulfur batteries. Therefore, the discussion of a lithium-ion battery is not limiting herein. An exemplary and schematic representation of a battery 20 that performs lithium-ion cycling is shown in Fig. 1. The battery 20 includes a negative electrode 22, a positive electrode 24, and a porous separator 26 (e.g., a microporous or nanoporous polymeric separator) disposed between the two electrodes 22, 24. The separator 26 includes an electrolyte 30, which may also be present in the negative electrode 22 and the positive electrode 24. A negative electrode current collector 32 may be disposed at or near the negative electrode 22, and a positive electrode current collector 34 may be positioned at or near the positive electrode 24. The negative electrode current collector 32 and the positive electrode current collector 34 each collect the electrons and transport the free electrons to and from an external circuit 40.An interruptible external circuit 40 and load 42 connects the negative electrode 22 (via its current collector 32) and the positive electrode 24 (via its current collector 34). The porous separator 26, which serves as both an electrical insulator and mechanical support, is sandwiched between the negative electrode 22 and the positive electrode 24 to prevent physical contact and thereby avoid the occurrence of a short circuit. In addition to providing a physical barrier between the two electrodes 22, 24, the porous separator 26 can provide a minimal resistance path for the internal passage of lithium ions (and associated anions) during lithium ion cycling, facilitating the function of the battery 20. While in lithium-ion batteries, lithium is incorporated into the active materials of the electrode, in a lithium-sulfur battery, the lithium dissolves from the negative electrode and migrates to the positive electrode, where it reacts, or plates, during discharge while remaining on the negative electrode during charge. The battery 20 can be recharged and reactivated at any time by connecting an external power source to the battery 20 to reverse the electroactive reactions of the battery discharge. Connecting an external power source to the battery 20 forces the generation of electrons and the release of lithium ions from the positive electrode 25. The electrons flowing through the external circuit 40 back to the negative electrode 22 and the lithium ions transported by the electrolyte 30 through the separator 26 back to the negative electrode 22 recombine at the negative electrode 22 and replenish it with stored lithium for use in the next battery discharge cycle. Thus, each discharge and charge event is considered a cycle in which lithium ions are switched between the positive electrode 24 and the negative electrode 22. The external power source that can be used to charge the battery 20 can vary in size, construction, and specific end use of the battery 20. Some notable and exemplary external sources include, but are not limited to, an AC wall outlet and a motor vehicle alternator. In many lithium-ion battery configurations, the negative current collector 32, the negative electrode 22, the separator 26, the positive electrode 24, and the positive current collector 34 are each fabricated as relatively thin sheets (e.g., from a few micrometers to a millimeter or less in thickness) and assembled in layers that are electrically connected together in parallel to provide a suitable power package. Furthermore, the battery 20 may include a variety of other components that, although not illustrated here, are well known to those skilled in the art. For example, the battery 20 may include a housing, gaskets, terminal covers, tabs, battery terminals, and any other conventional components or materials that may be located within the battery 20, including between or around the negative electrode 22, the positive electrode 24, and / or the separator 26, as a non-limiting example. As noted above, the size and shape of the battery 20 may vary depending on the particular application for which it is designed. Battery-powered vehicles and portable consumer electronic devices, for example, are two examples where the battery 20 would likely have a different size, capacity, and power output.The lithium-ion battery 20 may also be connected in series or parallel with other similar lithium-ion cells or batteries to produce greater voltage output, energy, and power when required by the load 42. Accordingly, the battery 20 can generate electrical power at a load 42, which can be operatively connected to the external circuit 40. While the load 42 can be any number of electrically powered devices, some specific examples of power-consuming load devices include an electric motor for a hybrid or all-electric vehicle, a laptop computer, a tablet computer, a cell phone, and a cordless power tool or household appliance, as non-limiting examples. However, the load device 42 can also be a power generating device that charges the battery 20 to store the energy. In some other variations, the electrochemical cell can be a supercapacitor, such as a lithium-ion-based supercapacitor. Referring again to Fig. 1, in certain cases, the porous separator 26 may comprise a microporous polymeric separator, including a polyolefin as a non-limiting example. The polyolefin may be a homopolymer (derived from a single monomer component) or a heteropolymer (derived from more than one monomer component), which may be either linear or branched. When a heteropolymer is derived from two monomer components, the polyolefin may adopt any copolymer chain arrangement, including those of a block copolymer or a random copolymer. Likewise, a polyolefin that is a heteropolymer derived from more than two monomer components may also be a block copolymer or a random copolymer.In certain aspects, the polyolefin can be polyethylene (PE), polypropylene (PP), a blend of PE and PP, or a multilayer structured porous film of PE and / or PP. Commercially available polyolefin microporous polymer membranes 26 include CELGARD®2500 (a single-layer polypropylene separator) and CELGARD®2320 (a three-layer polypropylene / polyethylene / polypropylene separator) from Celgard LLC. When the porous separator 26 is a microporous polymeric separator, it may be a single layer or a multi-layer laminate manufactured via either a dry or wet process. For example, in one embodiment, a single layer of polyolefin may constitute the entire microporous polymeric separator 26. In further aspects, the separator 26 may be a fibrous membrane having a multitude of pores extending between opposing surfaces and may, for example, have a thickness of less than one millimeter. However, as another example, the microporous polymeric separator 26 may also be composed of multiple separate layers of the same or a dissimilar polyolefin. Furthermore, the porous separator 26 may be blended with a ceramic material or its surface may be coated with a ceramic material.A ceramic coating may include, for example, aluminum oxide (Al2O3), silicon dioxide (SiO2), or combinations thereof. Various conventional polymers and commercial products for forming the separator 26 are considered, as well as the many manufacturing processes that can be used to produce such a microporous polymeric separator 26. In various cases, the positive electrode 24 may be formed from a lithium-based active material that can undergo sufficient lithium intercalation and de-intercalation, alloying and de-alloying, or plating and stripping while serving as the positive terminal of the battery 20. The electroactive materials of the positive electrode 24 may include one or more transition metals, such as manganese (Mn), nickel (Ni), cobalt (Co), and not according to the invention, chromium (Cr), iron (Fe), vanadium (V), and combinations thereof. Two exemplary common classes of known electroactive materials that can be used to form the positive electrode 24 are layered lithium transition metal oxides and spinel phase lithium transition metal oxides. In certain variations, the electroactive material used to form the positive electrode 24 may have a maximum potential of greater than or equal to about 4V, optionally greater than or equal to about 4.8V, and in certain aspects, greater than or equal to about 5V. In certain cases, the positive electrode 24 may include, for example, a lithium-based positive electroactive material selected from the group consisting of nickel manganese cobalt 811 (NMC811); nickel manganese cobalt 622 (NMC622); lithium cobalt oxide (LiCoO2); lithium iron phosphate (LiFePO4); high energy nickel manganese cobalt oxide (HENMC) (e.g., overlithed layered oxide cathode or lithium-rich NMC); lithium manganese nickel oxide (LMNO); and combinations thereof. In certain variations, the positive active materials can be blended with an optional electrically conductive material and at least one polymeric binder material to structurally reinforce the lithium-based active material, along with an optional electrically conductive particle dispersed therein. The active materials and optional conductive materials can be cast, for example, with binders such as polyvinylidene difluoride (PVdF), polytetrafluoroethylene (PTFE), ethylene propylene diene monomer (EPDM), carboxymethoxycellulose (CMC), nitrile butadiene rubber (NBR), lithium polyacrylate (LiPAA), sodium polyacrylate (NaPAA), sodium alginate, or lithium alginate. Electrically conductive materials can be graphite, carbon-based materials, nickel powder, metal particles, or a conductive polymer.Carbonaceous materials may include, by way of non-limiting example, KETCHEN™ carbon black, DENKA™ carbon black, acetylene black, carbon black, and the like. Examples of a conductive polymer include polyaniline, polythiophene, polyacetylene, polypyrrole, and the like. In certain aspects, blends of conductive materials may be used. The positive current collector 34 may be made of aluminum (Al) or any other suitable electrically conductive material. In various aspects, the negative electrode 22 includes an electroactive material that can serve as the negative terminal of a battery 20. The negative electrode 22 can thus include the electroactive material and optionally another electrically conductive material, as well as one or more polymeric binder materials for structurally holding the lithium host material together. The electroactive material consists of lithium in various respects and can be lithium metal. In certain variations, the negative electrode 22 is a film or layer of lithium metal or a lithium alloy. As mentioned above, metallic lithium for use in the negative electrode (e.g., 22) of a secondary battery (e.g., 20) has various potential advantages, including the highest theoretical capacity (e.g., around 3860 mAh / g (LiC6: 339 mAh / g; Li3.75Si: 1860 mAh / g)) and the lowest electrochemical potential. In addition, batteries (e.g.,, 20) with lithium metal anodes (e.g., 22) have a higher energy density (e.g., greater than or equal to about 800 Wh / l and 350 Wh / Kg), which can double the storage capacity. In some variations, the negative electrode 22 may optionally include another electrically conductive material as well as one or more polymeric binder materials for structurally holding the lithium host material together. As a non-limiting example, the negative electrode 22 may include an active material containing lithium metal particles (e.g., lithium foil) mixed with a binder material selected from the group consisting of: polyvinylidene difluoride (PVdF), polytetrafluoroethylene (PTFE), ethylene propylene diene monomer (EPDM), or carboxymethoxycellulose (CMC), a nitrile butadiene rubber (NBR), lithium polyacrylate (LiPAA), sodium polyacrylate (NaPAA), sodium alginate, lithium alginate, and combinations thereof. Suitable additional electrically conductive materials may include carbonaceous materials or a conductive polymer.Carbonaceous materials may include, by way of non-limiting example, KETCHEN™ carbon black, DENKA™ carbon black, acetylene black, carbon black, and the like. Examples of a conductive polymer include polyaniline, polythiophene, polyacetylene, polypyrrole, and the like. In certain aspects, blends of conductive materials may be used. The negative electrode current collector 32 may be made of copper (Cu) or any other suitable electrically conductive material, as known to those skilled in the art. As previously mentioned, each of the separators 26, the negative electrode 22, and the positive electrode 24 may include an electrolyte system 30 capable of conducting lithium ions between the negative electrode 22 and the positive electrode 24. The electrolyte system 30 may be a non-aqueous liquid electrolyte solution having a bound portion. The bound portion may comprise one or more salts associated with or bound to an organic solvent or a mixture of organic solvents. In certain cases, the one or more lithium salts may be selected from the group consisting of: lithium bis(fluorosulfonyl)imide (LiFSI), sodium bis(fluorosulfonyl)imide (NaFSI), potassium bis(fluorosulfonyl)imide (KFSI), and combinations thereof, and the solvent may comprise an ether-based solvent.For example, the bound portion of the electrolyte system 30 may comprise one or more lithium salts selected from the group consisting of: lithium bis(fluorosulfonyl)imide (LiFSI), sodium bis(fluorosulfonyl)imide (NaFSI), potassium bis(fluorosulfonyl)imide (KFSI), and combinations thereof, including dimethoxyethane (DME). A molar ratio of one or more salts to dimethoxyethane (DME) may be greater than or equal to about 1 to less than or equal to about 1.5 M. The one or more salts may have a concentration in the electrolyte system 30 of greater than 4 M, optionally greater than or equal to about 4.5 M, and in certain aspects, greater than or equal to about 5 M. In various aspects, the electrolyte system 30 has an ionization potential that is greater than an electron affinity. For example, the electrolyte system 30 may have a calculated electron affinity less than or equal to about 1.5 eV and a calculated ionization potential greater than or equal to about 10 eV. In certain cases, the electrolyte system 30 may have a dynamic viscosity of less than about 0.1 Pa*s (100 centipoise (cP)), and a battery 20 including the electrolyte system 30 may have an energy density greater than about 900 Wh / L. In various aspects, the bound portion of the electrolyte system 30 improves or supports the anodic stability of the battery 20 by suppressing or minimizing side reactions that can occur when the solvent and / or salts are unbound or free species in the electrolyte system 30 that can react with the lithium (Li) metal of the negative electrode 22. Side reactions can affect the coulombic efficiency and lifetime of rechargeable batteries by consuming the lithium (Li) metal and the electrolyte. Ether-based electrolyte systems are generally compatible with lithium (Li) metal. For example, dimethoxyethane (DME) has an electron affinity of approximately 1.5 eV, making it generally compatible with lithium (Li) metal.However, ether-based electrolyte systems with low concentrations (less than about 4M, and in certain aspects, less than about 3M) may exhibit poor anodic stability and may only be suitable for use with low-voltage cathodes, such as Li-S, Li-MoS2, and LiFePO4 batteries, where the cathodes have maximum potentials of less than about 3.7V. For example, dimethoxyethane (DME) has an ionization potential of less than about 7.2 eV, allowing for easy oxidation (electron loss) at the cathode. Providing electrolyte systems 30 with higher salt concentrations (e.g., greater than 4M, optionally greater than or equal to about 4.5M, and in certain aspects, optionally greater than or equal to about 5M) may increase anodic stability and enable the use of higher voltage cathodes (e.g., cathodes with a maximum potential greater than or equal to about 4V, optionally greater than or equal to about 4.8V, and in certain aspects, optionally greater than or equal to about 5V) at least in part because increased salt concentration increases the ionization potential of dimethoxyethane (DME) to greater than or equal to about 10 eV. Electrolyte system 30 with an increased salt concentration and a molar ratio of the one or more salts to dimethoxyethane (DME) greater than or equal to about 1 to less than or equal to about 1.5 may therefore be substantially free of such free or unbound compounds that promote such side reactions (e.g., oxidation at the cathode).Electrolyte system 30 may comprise less than or equal to about 0.5 wt.%, optionally less than or equal to about 0.25 wt.%, optionally less than or equal to about 0.1 wt.%, and in certain aspects, 0 wt.% of free or unbound undesirable species, such as unbound salt(s) or unbound solvent(s) (e.g., dimethoxyethane (DME)). In certain cases, the electrolyte system 30 may include one or more electrolyte additives. For example, the electrolyte system 30 may include one or more electrolyte additives selected from the group consisting of: organic silane electrolyte additives, borate-based electrolyte additives, and combinations thereof. The organic silane electrolyte additive may be selected from the group consisting of: fluorinated methoxysilanes, fluorinated chlorosilanes, and combinations thereof.In certain cases, the electrolyte system 30 may include one or more electrolyte additives that may be selected from the group consisting of: 3,3,3-trifluoropropylmethyldimethoxysilane, (3,3,3-trifluoropropyl)trimethoxysilane, 1H,1H,2H,2H-perfluorooctylmethyldimethoxysilane, 1H,1H,2H,2H-perfluorooctyltrimethoxysilane, 1H,1H,2H,2H-perfluorooctyldimethylchlorosilane, 1H,1H,2H,2H-perfluorooctylmethyldichlorosilane, (1H,1H,2H,2Hyl-n-hexyl)methyldichlorosilane, 1H,1H,2H,2H,-perfluorooctyltrichlorosilane, or combinations thereof. The electrolyte system 30 may include greater than or equal to about 0.1 weight percent (wt%) to less than or equal to about 10 weight percent (wt%) of the one or more electrolyte additives. The embodiments of the present technique are further illustrated by the following non-examples. Example 1 Fig. 2 shows an electrolyte system 55 constructed in accordance with certain aspects of the present disclosure. Specifically, Fig. 2 shows an electrolyte system 55 comprising one or more salts bonded to a solvent to form a bonded moiety. Electrolyte system 55 includes a bonded moiety including lithium bis(fluorosulfonyl)imide (LiFSI) and dimethoxyethane (DME). Electrolyte system 55 includes a lithium bis(fluorosulfonyl)imide (LiFSI) concentration of about 5M and a molar ratio of lithium bis(fluorosulfonyl)imide (LiFSI) to dimethoxyethane (DME) of greater than or equal to about 1 to less than or equal to about 1.5. As illustrated, substantially all dimethoxyethane (DME) molecules bind to lithium (Li+). Thus, dimethoxyethane (DME) and bis(fluorosulfonyl)imide (FSI-) can be immobilized, and the electrolyte system 55 can be substantially free of free or unbound dimethoxyethane (DME) and free or unbound bis(fluorosulfonyl)imide (FSI-). The electrolyte system 55 comprises less than or equal to about 0.5 wt. %, optionally less than or equal to about 0.25 wt. %, optionally less than or equal to about 0.1 wt. %, and in certain aspects, 0 wt. % of the free or unbound undesirable species, free or unbound dimethoxyethane (DME), and free or unbound bis(fluorosulfonyl)imide (FSI-). This eliminates or reduces harmful side reactions and increases the anodic stability of the batteries, including the electrolyte system 55. Figure 3 shows a comparative electrolyte system 50 with a salt concentration of less than about 4M. Electrolyte system 50 includes a lithium bis(fluorosulfonyl)imide (LiFSI) concentration of less than about 4M and a molar ratio of lithium bis(fluorosulfonyl)imide (LiFSI) to dimethoxyethane (DME) of about 0.4 (e.g., LiFSI:DME = 1:2.5). As shown, in such cases, an equilibrium state exists between [Li+(2-dimethoxyethane (DME)) + free bis(fluorosulfonyl)imide (FSI-)] and [Li+((dimethoxyethane (DME) + bis(fluorosulfonyl)imide (FSI-)) + free [dimethoxyethane (DME)]. The free or unbound bis(fluorosulfonyl)imide (FSI-) is highly reactive with lithium (Li) and can cause low lithium (Li) cycling efficiency (e.g., about 98.4% efficiency). The free or unbound dimethoxyethane (DME) can react with high-voltage cathodes (greater than about 4V) and thereby cause low full-cell efficiency (e.g., less than about 99.5%).In particular, free dimethoxyethane (DME) can oxidize on one or more surfaces of the cathode and form an internal redox species, which can lead to low columbine efficiency. Thus, providing electrolyte systems 55 with higher salt concentrations can increase anodic stability and offer the possibility of using higher voltage cathodes by fully binding one or more salts and solvents. As can be seen in Figure 4, the presence of the bound moiety in the electrolyte system 55 increases the ionization potential (eV) of the electrolyte system 55 without increasing the electron affinity (eV). The y-axis or vertical axis 60 of Figure 4 represents the electron affinity (eV), while the x-axis or horizontal axis 70 represents the ionization potential (eV). The electrolyte system 55 including the bound moiety can have a calculated electron affinity of less than or equal to about 1.5 eV and a calculated ionization potential of greater than or equal to about 10 eV.While the electrolyte system 50 without a bound portion may have a calculated electron affinity of less than or equal to about 1.5 eV and a calculated ionization potential of less than or equal to about 8 eV, and in certain cases, optionally less than or equal to about 7.2 eV. By suppressing or minimizing free or unbound dimethoxyethane (DME) and free or unbound bis(fluorosulfonyl)imide (FSI), a battery including electrolyte system 55 may include a high-voltage positive electrode having a maximum potential greater than or equal to about 4V, optionally greater than or equal to about 4.8V, and in certain aspects, optionally greater than or equal to about 5V. For example, the positive lithium-based electroactive material of the positive electrode may be selected from the group consisting of nickel manganese cobalt 811 (NMC811); nickel manganese cobalt 622 (NMC622); lithium cobalt oxide (LiCoO2); lithium iron phosphate (LiFePO4); high-energy nickel manganese cobalt oxide (HENMC) (e.g., overlithed layered oxide cathode or lithium-rich NMC); Lithium manganese nickel oxide (LMNO); and combinations thereof. Example 2 Fig. 5 shows the charge and discharge profiles (e.g., cycle life) of comparatively high-performance 20 µm Li-NMC 622 electrochemical cells 100, 200, and 300, including negative electrodes comprising metallic lithium and various electrolyte systems comprising lithium bis(fluorosulfonyl)imide (LiFSI) and dimethoxyethane (DME). The y-axis or vertical axis 80 represents capacity retention in milliampere-hours (mAh), while the cycle number is displayed on the x-axis 90. The electrochemical cell 100 includes an electrolyte system prepared in accordance with certain aspects of the present disclosure. In particular, the electrolyte system of the electrochemical cell 100 includes a bonded portion and has a lithium bis(fluorosulfonyl)imide (LiFSI) salt concentration of about 5M and a molar ratio of lithium bis(fluorosulfonyl)imide (LiFSI) to dimethoxyethane (DME) of about 1.The electrolyte system of the electrochemical cell 200 has a lithium bis(fluorosulfonyl)imide (LiFSI) salt concentration of about 4M and the electrolyte system of the electrochemical cell 300 has a lithium bis(fluorosulfonyl)imide (LiFSI) salt concentration of about 1.5M. As can be seen, electrochemical cell 100 has demonstrated long-term improvements over electrochemical cells 200 and 300. In particular, electrochemical cell 200 with a salt concentration of approximately 4M exhibits rapid capacity decay, while electrochemical cell 300 with a salt concentration of approximately 1.5M cannot maintain stable cycling. Accordingly, electrochemical cell 100 fabricated according to certain aspects of the present disclosure exhibits significantly improved cycling performance and reduced capacity decay. The electrolyte system of electrochemical cell 100 is compatible with both negative electrodes (e.g., anodes) made of metallic lithium and NMC cathodes.
Claims
A method for preparing an electrolyte system that increases or optimizes anodic stability of an electrochemical cell, comprising a positive electrode comprising a positive lithium-based electroactive material having a maximum potential greater than or equal to about 5V, wherein the positive lithium-based electroactive material is selected from the group consisting of nickel-manganese-cobalt 811 (NMC811), nickel-manganese-cobalt 622 (NMC622), and combinations thereof, and a negative electrode having a negative electroactive material comprising lithium, the method comprising: mixing one or more salts selected from the group consisting of: lithium bis(fluorosulfonyl)imide (LiFSI), sodium bis(fluorosulfonyl)imide (NaFSI), potassium bis(fluorosulfonyl)imide (KFSI), and combinations thereof, and a solvent comprising dimethoxyethane (DME) that forms a bonded moiety with an ionization potential greater than an electron affinity,to form an electrolyte system substantially free of unbound dimethoxyethane (DME) and unbound bis(fluorosulfonyl)imide (FSI-), wherein the one or more salts have a concentration in the electrolyte system of greater than 4M and a molar ratio of the one or more salts to dimethoxyethane (DME) is greater than or equal to about 1 to less than or equal to about 1.
5. The method of claim 1, wherein the electrolyte system has a dynamic viscosity of less than about 0.1 Pa*s and the electrochemical cell has an energy density of more than about 900 Wh / L. The method of claim 1, wherein the electrolyte system includes one or more electrolyte additives selected from the group consisting of: organic silane electrolyte additives, borate-based electrolyte additives, and combinations thereof. The method of claim 3, wherein the one or more electrolyte additives comprise an organic silane electrolyte additive selected from the group consisting of: fluorinated methoxysilanes, fluorinated chlorosilanes, and combinations thereof. The method of claim 1, wherein the electrolyte system includes one or more electrolyte additives selected from the group consisting of: 3,3,3-trifluoropropylmethyldimethoxysilane, (3,3,3-trifluoropropyl)trimethoxysilane, 1H,1H,2H,2H-perfluorooctylmethyldimethoxysilane, 1H,1H,2H,2H-perfluorooctyltrimethoxysilane, 1H,1H,2H,2H-perfluorooctyldimethylchlorosilane, 1H,1H,2H,2H-perfluorooctylmethyldichlorosilane, (1H,1H,2H,2Hyl-n-hexyl)methyldichlorosilane, 1H,1H,2H,2H-perfluorooctyltrichlorosilane, and combinations thereof.
Citation Information
Patent Citations
ELECTROLYTE, NEGATIVE ELECTRODE STRUCTURE AND METHOD OF MAKING A SOLID ELECTROLYTE INTERFACIAL LAYER ON A SURFACE OF A LITHIUM ELECTRODE
DE102015121342A1
High Salt Concentration Electrolytes For Rechargeable Lithium Battery
US20160233549A1