Method for changing the STIR of the edge of a SOI by applying a film
Patent Information
- Application Number
- DE102018132009
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2018-05-28
- Filing Date
- 2018-12-12
- Publication Date
- 2024-10-02
- Estimated Expiration
- Not applicable · inactive patent
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
TECHNICAL FIELD The present invention relates to the field of manufacturing SOI elements (SOI = Silicon-On-Insulator, i.e. silicon on insulator, in which structures a buried oxidation layer is introduced between an upper silicon layer and a lower substrate) and, in particular, provides a method for modifying the STIR (site total indicator reading, local flatness deviation) of the edge of an SOI by bonding a foil. STATE OF THE ART With the advancement of silicon processing technology in China, processing quality and inspection procedures in wafer processing are becoming increasingly important. Quality inspection is a critical component of the processing process. The inspection and inspection procedures for some key parameters, such as curvature, thickness, and total thickness variation, during wafer processing are of particular interest to wafer manufacturers and their equipment manufacturers. Wafer inspection systems with a high degree of automation have already been developed. For example, the American companies ADE, TENCOR, TROPEL, and SILTEC have developed automated inspection systems that can meet user wafer inspection requirements. One example is the Type-700 wafer inspection system from ADE.Such a system has a modular design and can measure various parameters, including curvature, thickness, and total thickness variation, in addition to testing wafer curvature (TIR), thickness (FPD), and total thickness variation (LSL). Furthermore, various tests are possible, such as electrical resistivity, doping intensity, and surface gloss. With a high degree of automation, 60 wafers can be handled per hour. Also available is the Type 900 Auto-Sort Wafer Inspection System from TROPEL, which is said to be the most feature-rich automatic wafer inspection system currently available. When processing wafers, wafer inspection requirements and applications vary from manufacturer to manufacturer. Thus, there is a need for a method to modify the STIR of the edge of an SOI with high flexibility and feasibility. The patent application publication DE 10 2017 118 860 A1 describes a manufacturing method for an SOI wafer in the form of a thin film, which comprises the steps of providing a silicon wafer with high resistance, providing a silicon wafer with low resistance, performing a hydrogen ion implantation, bonding the silicon wafers, cleaving the unit from both silicon wafers, cleaning the cleaved unit, annealing the cleaved unit and cleaning again. Patent application publication US 2015 / 0 243 550 A1 also discloses a method for producing an SOI wafer in which a PVC film is used to protect a desired oxide layer from being removed by an etching solution used during production. OBJECT OF THE INVENTION The present invention is based on the object of providing a method for changing the STIR of the edge of an SOI by bonding a film. OBJECT OF THE INVENTION According to the invention, the above object is achieved by a method for changing the STIR of the edge of an SOI by bonding a film having the features of claim 1. Advantageous further developments are the subject of the dependent claims. The method according to the invention for changing the STIR of the edge of an SOI by bonding a film is characterized in that after providing a silicon wafer as a raw material, oxidation, implantation, bonding, wafer splitting and film bonding are carried out in sequence, wherein the film bonding is carried out according to the following technical requirements: scratching on the front and back of the SOI wafer should be avoided during film bonding by using a film bonding system and the silicon wafer should not fall off when it is sucked into the system, wherein a film with a thickness of greater than 0 to 0.5 mm is used and any blue film used in the semiconductor industry can be used, wherein the film is bonded to the back of the silicon wafer so that the film is arranged on the back of the silicon wafer.Next, an oxidation layer formed on the front edge of the silicon wafer is removed using concentrated hydrofluoric acid (since the foil is arranged on the back side, the back side of the SOI is not damaged). The foil is then removed from the back side of the SOI using a concentrated SC1 solution. Following this, cleaning is carried out with SC1 and SC2 (SC1 and SC2 cleaning is carried out according to the relevant industry standard). The STIR of the SOI edge is tested using an appropriate test device, e.g., Type 9600. The STIR is less than 0.3 µm. The specific electrical resistance and crystal orientation of the wafer used as the raw material are selected depending on the actual requirements. The process for changing the STIR of the edge of an SOI by bonding a foil is preferably carried out under the technical conditions explained below. The oxidation step specifically involves oxidizing the surface of one side of the raw silicon wafer to obtain a silicon wafer with an oxidation layer. Subsequent washing removes impurities from the surface, and various parameters, including the number of particles on the surface of the silicon wafer with an oxidation layer and the thickness of the oxidation layer, are tested using an inspection device. A silicon wafer that meets the requirements is selected for future use. The implantation step specifically involves implanting H+ ions into a silicon wafer coated with an oxidation layer. The implantation is carried out to a desired depth, with specific implantation conditions being selected for the implantation, namely the energy, dosage amount, beam size, and angle. Following the implantation, washing is carried out according to the conditions described below. Specifically, washing is carried out with a concentrated sulfur column, SC1 and SC2, to remove impurities from the surface.Subsequently, various parameters, including the particles on the surface of the silicon wafer implanted with an oxidation layer, and the geometric parameters are tested using a test fixture, and a silicon wafer that meets the conditions for a desired application (given the different requirements in different products, no generalization is possible) is selected for subsequent use. The bonding step specifically involves providing another silicon wafer, either oxidized or bare (untreated), whose specific electrical resistance and crystal orientation are selected according to requirements. Washing the surface of the second silicon wafer removes the natural oxidation layer and impurities.Next, the particles on the surface of the silicon wafer are inspected using an inspection device, and a silicon wafer that meets the requirements (particle requirements vary from product to product, so no specific data can be given) is bonded to the first silicon wafer provided with an implanted oxidation layer. After a certain activation time for the two wafers, the bonded wafer is subjected to a low-temperature annealing process at 100 to 350 °C to thereby obtain an implanted bonded wafer. The wafer splitting process is carried out by placing the bonded wafer into a wafer splitting machine and subjecting it to a wafer splitting process in which the wafer is first heated in a chamber to 100 to 200 °C, then kept warm for 10 to 30 minutes, and then a microwave magnetron head is switched on to initiate a wafer splitting process which lasts 1 to 10 minutes, after which an SOI product is obtained. The low-temperature annealing process includes the following steps: Performing a low-temperature annealing process at a temperature of 100 to 300 °C for 2 to 5 hours after the bonding step and before the wafer splitting step. The design of the present invention follows the following principles and is characterized by the advantageous effects mentioned below: 1. In the method according to the present invention, steps for oxidation, implantation, bonding and a low-temperature annealing process are carried out, wherein a wafer splitting process is carried out for a bonded silicon wafer by means of a microwave wafer splitting process, in order to thereby form an SOI structure, wherein a film is stuck to the back of the SOI and the oxidation layer on the edge of the front side of the wafer is removed using concentrated hydrofluoric acid, while the oxidation layer on the back side is retained by sticking it with the film, wherein the film is then removed again, thus obtaining an SOI structure whose STIR is less than 0.3 µm.In conventional methods, chamfering is usually carried out, so that a high SITR is to be expected. In contrast, in the method according to the invention, after adhering a film, in particular blue film, the oxidation layer on the edge is removed, thus achieving a low SITR. 2. The method according to the invention for changing the STIR of the edge of an SOI by adhering a film has a significantly improved technical effect compared to a chamfering method. After completion of a chamfering process, an SOI has a large STIR that is greater than 0.5 µm, whereas in the present invention the chamfering process is omitted, thus enabling an improved STIR for the SOI structure. 3. The method according to the invention for changing the STIR of the edge of an SOI by adhering a film is suitable for industrial production and enables series production.In the present invention, a chamfering process is replaced by a film bonding process, which enables increased efficiency and improved yield. Compared to the prior art, the present invention is characterized by significantly better technical properties of the product and high achievable economic and social values. BRIEF DESCRIPTION OF THE DRAWINGS Fig. 1 shows a process flow diagram of a method according to the invention for changing the STIR of the edge of an SOI by bonding a film, and Fig. 2 shows a process flow diagram of a method according to the prior art as a comparative example. DETAILED DESCRIPTION OF THE EMBODIMENTS First embodiment In a method according to the invention for changing the STIR of the edge of an SOI by bonding a foil, a first silicon wafer is first provided as raw material, for which an oxidation step, an implantation step, a bonding step, a wafer splitting step, and a foil bonding step are carried out in sequence. The foil bonding is carried out according to the technical requirements in such a way that scratching on the front and back of the SOI wafer is avoided during the foil bonding process using a foil bonding system and the silicon wafer cannot fall off when sucked into the system. A blue foil with a thickness of greater than 0 to 0.5 mm is used, and any blue foil used in the semiconductor industry is conceivable for application. The blue foil is bonded to the back of the silicon wafer so that a blue foil now adheres to the back of the silicon wafer.Next, the oxidation layer on the front edge of the silicon wafer is removed using concentrated hydrofluoric acid. Due to the presence of the blue foil on the back, the back of the SOI is not damaged. The blue foil is then removed from the back of the SOI using a concentrated SC1 solution. Following this, cleaning with SC1 and SC2 is carried out (SC1 and SC2 cleaning is carried out according to the relevant industry standard, so no further explanation is given here). Using an appropriate testing device, e.g., Type 9600, the STIR of the edge of the SOI is tested; this STIR is now less than 0.3 µm. The specific electrical resistance and crystal orientation of the wafer used as the raw material are selected according to actual requirements. For the SC1 cleaning fluid, the ratio of ammonia water : hydrogen peroxide : water is 1:1:5 - 1:2:7, and for the SC2 cleaning fluid, the ratio of hydrogen chloride : hydrogen peroxide : water is 1:1:6 - 1:2:8, with the concentration of hydrogen chloride, ammonia water and hydrogen peroxide being 37%, 27% and 30% respectively. The oxidation step involves oxidizing the surface of one side of the first silicon wafer used as a raw material to obtain a silicon wafer with an oxidation layer. The wafer is then washed to remove impurities from the surface and subjected to inspection of various parameters, including the number of particles on the surface of the silicon wafer with an oxidation layer and the thickness of the oxidation layer, using an appropriate inspection device. A silicon wafer meeting certain requirements is selected for later use. The implantation step comprises implanting H+ ions into the silicon wafer provided with an oxidation layer to a desired depth, the implantation being carried out according to certain implantation conditions, i.e. depending on the energy, the dosage amount, the beam size and the angle, the wafer being washed after implantation, the washing being carried out with a concentrated sulfur column, SC1 and SC2, in order to remove impurities from the surface, followed by an inspection of various parameters, including the particles on the surface of the silicon wafer provided with an implanted oxidation layer, and the geometric parameters using an inspection device, a silicon wafer that meets certain conditions (given the different conditions for different products, no generalization is possible) is selected for later use. The bonding step comprises the following steps: providing another silicon wafer, which is an oxidized or bare wafer, whose specific electrical resistance and crystal orientation are selected according to requirements, washing the surface of the newly provided second silicon wafer to remove the natural oxidation layer and impurities from its surface, and then inspecting the particles on the surface of the silicon wafer using an appropriate inspection device, whereby a silicon wafer that meets certain requirements (the particle requirements vary from product to product, so no specific data can be given) is bonded to the silicon wafer provided with an implanted oxidation layer,wherein the bonded wafer is subjected to a low-temperature annealing process at 100 to 350 °C after a certain activation time for the two wafers has elapsed, thereby obtaining an implanted bonded wafer. The wafer splitting process comprises the following steps: placing the bonded wafer into a wafer splitting machine and subjecting it to a wafer splitting process in which the wafer is heated in a chamber to 100 to 200 °C and kept warm for 10 to 30 minutes, after which a microwave magnetron head is switched on to initiate a wafer splitting process which lasts for 1 to 10 minutes, after which an SOI product is obtained. The low-temperature annealing process involves performing a low-temperature annealing process at a temperature of 100 to 300 °C for 2 to 5 hours after bonding and before wafer splitting. The inventive method according to the present embodiment follows the following principles and is characterized by the advantageous effects explained below: 1. In the method according to the present invention, an oxidation step, an implantation step, a bonding step and a low-temperature annealing process are carried out successively, wherein a wafer splitting process is carried out for a bonded silicon wafer by means of a microwave wafer splitting process in order to form an SOI structure, wherein a blue foil is adhered to the back of the SOI structure and the oxidation layer on the edge of the front side is removed using concentrated hydrofluoric acid, while the oxidation layer on the back side remains, wherein the blue foil is then removed again from the back side, wherein the STIR of the SOI structure treated in this way is less than 0.3 µm.In conventional methods, chamfering is carried out for this purpose, so that a high SITR is to be expected. In contrast, in the method according to the present invention, the oxidation layer on the edge is removed after a film has been adhered, thus achieving a low SITR. 2. The method according to the invention for changing the STIR of the edge of an SOI by adhering a blue film has significantly better technical properties compared to a conventional chamfering method (cf. Fig. 2 ). After completion of a chamfering process, a conventional SOI structure has a high STIR that is greater than 0.5 µm, whereas with the present invention the chamfering process is omitted and thus an improved STIR of the SOI is achieved. 3. The method according to the invention for changing the STIR of the edge of an SOI by adhering a blue film is suitable for industrial production and enables series production.A chamfering process is replaced by a film bonding process, which enables increased efficiency and improved yield. Compared to the prior art, the present invention is characterized by a significantly better technical effect and great achievable economic and social values. Second embodiment A method for changing the STIR of the edge of an SOI by bonding a foil (referring to Fig. 1, the essential innovative contents of the present invention are shown in the block in the lower left corner) is explained in detail below and comprises: 1. Selection of an 8-inch Type-P silicon wafer whose crystal orientation <100> or <111> and whose specific electrical resistance can reach a high level through weak doping. 2.Producing an oxidation layer (silicon dioxide layer) on the silicon wafer, wherein for this purpose an oxidation of the surface of one side of the silicon wafer from step 1 is carried out (alternatively, an oxidation of two silicon wafers is also conceivable, each of which should be carried out depending on the practical process conditions) in order to obtain a silicon wafer with an oxidation layer (silicon dioxide as the oxidation layer of the SOI), wherein the oxidation is carried out using a conventional method and the produced oxidation layer (silicon oxide) has a thickness of greater than 0 to 3000 nm. The silicon wafer thus produced with an oxidation layer is then cleaned successively using SC1 and SC2 in order to remove contaminants from the surface of the silicon wafer.Next, the particles on the surface of the silicon wafer are inspected using a test fixture, the thickness of silicon oxide is inspected, and other parameters (e.g., the particles of the silicon oxide layer and electrical parameters) are inspected using a suitable test fixture. A silicon wafer that meets certain requirements is selected for use in the subsequent steps. 3. Ion implantation into a silicon wafer with an oxidation layer or a bare wafer, with the implantation depth being determined according to requirements. 4.Providing an 8-inch silicon wafer (bare wafer) whose specific electrical resistance and crystal orientation are selected according to requirements, and cleaning the surface of the silicon wafer successively using DHF, SC1, and SC2 to remove the natural oxidation layer on the surface and any contaminants present on the surface layer. Subsequently, the particles on the surface of the silicon wafer are inspected using an appropriate inspection device, and a silicon wafer that meets specific requirements is selected for later use. 5.Bonding: Bonding the hydrogen ion-implanted silicon wafer obtained in step 3 to a silicon wafer from step 4 that meets the defined requirements. The wafers are activated for a specific time and then subjected to low-temperature annealing for a specific time at an annealing temperature of 100 to 350°C. After the annealing process, an implanted bonded wafer is obtained. 6. Microwave wafer splitting of the bonded wafer from step 5. The wafer splitting of the bonded wafer is performed using a wafer splitting process selected as needed, for example, using a microwave wafer splitting method from SY Silicon Technology Co., Ltd. Thus, an SOI product is obtained. 7.Foil bonding step, in which a foil is bonded to the back of the 8-inch SOI wafer obtained in step 6 using a professional foil bonding system. Following this, etching is performed with concentrated hydrofluoric acid to remove the oxidation layer on the edge of the front side of the wafer. The foil is then removed from the back of the silicon wafer with concentrated SC1 solution, and the silicon wafer is cleaned (with SC1 and SC2), resulting in an SOI structure with an edge STIR of less than 0.3 µm. 8. Furthermore, the 8-inch SOI from step 6 are recycled according to the company's specifications. Comparison example A method for changing the STIR of the edge of an SOI according to the prior art is explained in detail below with reference to Fig. 2. It comprises the following steps: 1. Selection of an 8-inch Type-P silicon wafer whose crystal orientation <100> or <111> and whose specific electrical resistance can reach a high level through weak doping. 2. Forming an oxidation layer (silicon dioxide) on the silicon wafer, wherein the surface of one side of the silicon wafer from step 1 is oxidized (alternatively, oxidation of two silicon wafers is also conceivable, each of which should be carried out according to the practical process conditions) to obtain a silicon wafer with an oxidation layer (silicon dioxide as the BOX layer (oxidation layer) of the SOI), wherein the oxidation is carried out using a conventional method,wherein the produced oxidation layer (silicon oxide) has a thickness of greater than 0 to 3000 nm, wherein the produced silicon wafer provided with an oxidation layer is subsequently cleaned with SC1 and SC2 to remove impurities from the surface of the silicon wafer, wherein the particles on the surface of the silicon wafer are subsequently examined using an appropriate inspection device, as well as the thickness of silicon oxide and the inspection of other parameters (for example, the particles of the silicon oxide layer and the electrical parameters) using an appropriate inspection device, wherein a silicon wafer that meets certain requirements is selected for use in the subsequent steps. 3. Implantation of ions into a silicon wafer provided with an oxidation layer or a bare wafer,The implantation depth is determined according to the requirements. 4. Providing an 8-inch silicon wafer (bare wafer), whose specific electrical resistance and crystal orientation are selected according to the requirements. The surface is then cleaned successively using DHF, SC1, and SC2 to remove the natural oxidation layer on the surface and any contaminants present on the surface layer. Subsequently, the particles on the surface of the silicon wafer are examined using an appropriate inspection device, and a silicon wafer that meets the requirements is selected for later use. 5. Bonding: Bonding a hydrogen ion-implanted silicon wafer obtained in step 3 and a silicon wafer from step 4 that meets the requirements is performed.Activation of the bonded wafer is performed for a specific time, followed by low-temperature annealing for a specific time at an annealing temperature of 100 to 350°C, resulting in an implanted bonded wafer. 6. Microwave wafer splitting of the bonded wafer, wherein the bonded wafer is split using a wafer splitting process selected as needed, for example, using a microwave wafer splitting method from SY Silicon Technology Co., Ltd. Thus, an SOI product is obtained. 7. Chamfering, in which an 8-inch SOI wafer obtained in step 6 is chamfered to remove the oxidation layer from the edge. Due to the insufficient accuracy of a chamfering machine and the special nature of an 8-inch silicon wafer, a positioning notch is present and the position of the positioning notch must be ground (special requirement for a silicon substrate).The SITR at the edge of the chamfered SOI is greater than 0.3 µm, which does not meet the product's design requirements. 8. The 8-inch SOIs from step 6 are recycled according to the company's specifications.
Claims
A method for changing the STIR of the edge of an SOI by bonding a foil, characterized in that a silicon wafer is provided as raw material, for which oxidation, implantation, bonding, wafer splitting, and foil bonding are first carried out in sequence. The foil bonding is carried out in such a way that scratching on the front and back of the SOI wafer is avoided during the foil bonding by means of a foil bonding system and the silicon wafer cannot fall off when sucked into the system. A foil with a thickness of greater than 0 to 0.5 mm is used. The foil is bonded to the back of the silicon wafer so that the foil adheres to the back of the silicon wafer. The oxidation layer on the edge of the front of the silicon wafer is then removed using concentrated hydrofluoric acid.Due to the foil present on the back, the back of the SOI is not damaged. The foil is then removed from the back of the SOI using a concentrated SC1 solution, followed by cleaning with SC1 and SC2. The STIR of the edge of the SOI is checked using a device, which is now less than 0.3 µm. A method for changing the STIR of the edge of an SOI by adhering a film according to claim 1, characterized in that the oxidation step comprises oxidizing the surface of one side of the silicon wafer used as a raw material to obtain a silicon wafer with an oxidation layer, washing it to remove the impurities from the surface and inspecting various parameters including the particles on the surface of the silicon wafer provided with an oxidation layer and the thickness of the oxidation layer using an inspection device, whereby a silicon wafer that meets certain requirements is selected for later use. A method for changing the STIR of the edge of an SOI by adhering a film according to claim 2, characterized in that the implantation step comprises implanting H+ ions into a silicon wafer having an oxidation layer to a desired depth, wherein the implantation is carried out under specific implantation conditions including the energy, dosage amount, beam size and angle, and wherein after the implantation, washing with a concentrated sulfur column, SC1 and SC2, is carried out to remove impurities from the surface, followed by an inspection of various parameters including the particles on the surface of the silicon wafer formed with an implanted oxidation layer and the geometric parameters using an inspection device, wherein a silicon wafer satisfying specific conditions is selected for later use. A method for changing the STIR of the edge of an SOI by adhering a film according to claim 3, characterized in that the bonding step comprises providing another silicon wafer which is an oxidized or bare wafer whose specific electrical resistance and crystal orientation are selected according to requirements, wherein the surface of the new silicon wafer is washed to remove the natural oxidation layer and impurities from the surface, followed by an inspection of the particles on the surface of the silicon wafer using an inspection device, wherein a silicon wafer which meets the requirements is bonded to the implanted silicon wafer, and the bonded wafer is subjected to a low-temperature annealing process at 100 to 350 °C after a certain activation time for the two wafers has elapsed, thus obtaining an implanted bonded wafer. A method for changing the STIR of the edge of an SOI by bonding a film according to claim 4, characterized in that the wafer splitting process is carried out by placing the bonded wafer in a wafer splitting machine and treating it with a wafer splitting process which comprises heating the wafer in a chamber up to 100 to 200 °C and holding it warm for 10 to 30 minutes and switching on a microwave magnetron head to initiate a wafer splitting process which lasts 1 to 10 minutes, after which an SOI product is obtained. A method for changing the STIR of the edge of an SOI by bonding a film according to claim 5, characterized in that the low-temperature annealing process defines carrying out a low-temperature annealing process at a temperature of 100 to 300 °C for 2 to 5 hours after bonding and before wafer splitting.
Citation Information
Patent Citations
manufacturing process for a thin film
DE102017118860A1
Method for manufacturing SOI wafer
US20150243550A1