Bond structure using two oxide layers with different strain levels and corresponding method

A dual oxide layer bonding structure with varying stress and density levels addresses the challenge of achieving strong chip-to-wafer bonding without damaging existing components, enhancing bond strength and thermal protection in integrated circuits.

DE102023120847B4Active Publication Date: 2024-11-07GLOBALFOUNDRIES US INC
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
DE102023120847
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2022-09-06
Filing Date
2023-08-07
Publication Date
2024-11-07
Estimated Expiration
2043-08-07

AI Technical Summary

Technical Problem

Existing methods for chip-to-wafer and wafer-to-wafer bonding in integrated circuits face challenges in achieving sufficient bond strength while minimizing stress and avoiding damage to existing components, particularly when using thick oxide layers.

Method used

A bonding structure comprising a first oxide layer with a lower stress and higher thickness, and a second oxide layer with higher stress and density, which is thinner than the first, is used to enhance bond strength without damaging existing components, formed at low temperatures using PECVD processes.

Benefits of technology

The proposed bonding structure achieves bond strengths of at least 1.0 J/m², significantly stronger than conventional methods, while maintaining low thermal stress and preventing voids, suitable for various semiconductor applications.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

Bond structure (100) for a semiconductor substrate (114), wherein the bond structure (100) comprises: a first oxide layer (110) on the semiconductor substrate (114); and a second oxide layer (120) on the first oxide layer (110), wherein the second oxide layer (120) serves to connect with another structure (130), wherein the second oxide layer (120) has a higher stress level than the first oxide layer (110) and the second oxide layer (120) is thinner than the first oxide layer (110).
Need to check novelty before this filing date? Find Prior Art

Description

background

[0001] The present invention relates to the fabrication of integrated circuits (ICs) and, more particularly, to a structure and method for bonding structures, such as chips to wafers or wafers to wafers, using two oxide layers to achieve improved bond strength.

[0002] Die-to-wafer and wafer-to-wafer bonding has the potential to improve the performance of a variety of silicon technologies. Achieving a bond with sufficient strength at low stresses and high-density thin films is challenging. One approach forms a thick oxide (e.g., 1,000–15,000 nanometers) at a low deposition temperature for bonding to another wafer. The low deposition temperature prevents damage to devices on the substrate but results in a low-density, low-stress layer that lacks sufficient bond strength. Densifying the thick layer increases wafer bond strength, but the stresses are unacceptably high. Other approaches treat the wafer surface with ammonia to increase bond strength.Other approaches have attempted to bond at elevated temperatures and under pressure, or to subject the surface to a water plasma treatment. These approaches do not provide sufficient bond strength and / or can damage existing components.

[0003] The document CN 1 08 461 512 A shows a wafer bonding structure with a device wafer, a first oxide layer, wherein the first oxide layer is formed on the device wafer, a second oxide layer formed on the device wafer, wherein the second oxide layer covers the first oxide layer and the second oxide layer is denser than the first oxide layer and has a high density, a load wafer which is bonded to the device wafer at the second oxide layer. Summary

[0004] All aspects, examples and features mentioned below can be combined in any technically possible way.

[0005] One aspect of the invention provides a bonding structure for a semiconductor substrate, the bonding structure comprising: a first oxide layer on the semiconductor substrate; and a second oxide layer on the first oxide layer, the second oxide layer for connecting to another structure or for bonding to another structure, the second oxide layer having a higher stress level than the first oxide layer, and the second oxide layer being thinner than the first oxide layer.

[0006] Another aspect of the invention includes any of the preceding aspects and the second oxide layer has a higher density than the first oxide layer.

[0007] One aspect includes a semiconductor device comprising: a semiconductor substrate; and a first bonding structure between the semiconductor substrate and a first structure, the first bonding structure comprising: a first oxide layer on the semiconductor substrate and a second oxide layer on the first oxide layer connected to the first structure, the second oxide layer having a higher stress level than the first oxide layer, and the second oxide layer being thinner than the first oxide layer.

[0008] Another aspect of the invention comprises any of the preceding aspects and the second oxide layer has a higher density than the first oxide layer.

[0009] A further aspect of the invention comprises any of the preceding aspects and the first oxide layer has a density in the range of 2.31 - 2.37 grams per cubic centimeter (g / cm 3 ) and the second oxide layer has a density in the range of 2.43 - 2.52 g / cm3 on.

[0010] Another aspect of the invention comprises one of the preceding aspects and further comprises a second bonding structure for connecting a second structure to the first structure, the second bonding structure comprising: a third oxide layer on the first structure and a fourth oxide layer on the third oxide layer, the fourth oxide layer having a higher density and a higher stress level than the third oxide layer, and the fourth oxide layer being thinner than the third oxide layer.

[0011] Another aspect of the invention comprises any of the preceding aspects and the first oxide layer has a thickness in the range of 5,000 to 15,000 nanometers (nm) and the second oxide layer has a thickness in the range of 250 to 750 nm.

[0012] Another aspect of the invention comprises any of the preceding aspects and the first oxide layer has a compressive stress in the range of 70 to 100 megapascals (MPa) and the second oxide layer has a compressive stress in the range of 300 to 350 MPa.

[0013] Another aspect of the invention comprises any of the preceding aspects and at least one of the first oxide layer and the second oxide layer has a surface with a root mean square roughness in the range of 0.1 to 0.5 nanometers.

[0014] A further aspect of the invention comprises any of the preceding aspects and the bond strength between the second oxide layer and the first structure is at least 1.0 joule per square meter (J / m 2 ).

[0015] One aspect of the invention includes a method comprising: forming a first bonding structure, the forming comprising: forming a first oxide layer on a first structure; forming a second oxide layer on the first oxide layer, the second oxide layer having a higher stress level than the first oxide layer and the second oxide layer being thinner than the first oxide layer; and bonding the second oxide layer to a second structure.

[0016] Another aspect of the invention comprises any of the preceding aspects and the second oxide layer has a higher density than the first oxide layer.

[0017] A further aspect of the invention comprises any of the preceding aspects and the first oxide layer has a density in a range of 2.31 - 2.37 grams per cubic centimeter (g / cm 3 ) and the second oxide layer has a density in the range of 2.43 - 2.52 g / cm 3 on.

[0018] Another aspect of the invention includes any of the preceding aspects and forming the first oxide layer and forming the second oxide layer each occur at a temperature of less than 300° Celsius (°C).

[0019] A further aspect of the invention comprises any of the preceding aspects and forming the first oxide layer comprises depositing the first oxide layer to a thickness in the range of 5 to 15 µm, and wherein forming the second oxide layer comprises depositing the second oxide layer to a thickness in the range of 0.25 to 0.75 µm.

[0020] A further aspect of the invention comprises one of the preceding aspects and the first oxide layer has a compressive stress in a range of 70 - 100 MPa and the second oxide layer has a compressive stress in a range of 300 - 350 MPa.

[0021] Another aspect of the invention comprises any of the preceding aspects and at least one of the methods for forming the first oxide layer and for forming the second oxide layer comprises planarizing a surface of the respective oxide layer to have a root mean square roughness in the range of 0.1 to 0.5 nanometers.

[0022] A further aspect of the invention comprises one of the preceding aspects and a bond strength between the second oxide layer and the first structure is at least 1.6 J / m 2 .

[0023] Another aspect of the invention includes any one of the preceding aspects and further includes: forming a second bonding structure on the second structure, comprising: forming a third oxide layer on the second structure and forming a fourth oxide layer on the third oxide layer, wherein the fourth oxide layer has a higher density and a higher stress level than the third oxide layer, and the fourth oxide layer is thinner than the third oxide layer; and bonding a third structure to the fourth oxide layer.

[0024] A further aspect of the invention comprises any of the preceding aspects and forming the third oxide layer comprises depositing the third oxide layer to a thickness in a range of 5 to 15 µm, and forming the fourth oxide layer comprises depositing the fourth oxide layer to a thickness in a range of 0.25 to 0.75 µm.

[0025] Two or more aspects described in this specification, including those described in this summary section, may be combined to form implementations not specifically described herein.

[0026] The details of one or more embodiments are set forth in the accompanying drawings and the description below. Further features, objects, and advantages will become apparent from the description and drawings, as well as from the claims. Short description of the drawings

[0027] The embodiments of this invention are described in detail with reference to the following figures, wherein like reference numerals denote like elements and wherein: Fig. 1 shows a cross-sectional view of a formation of a first oxide layer of a first bond structure according to embodiments of the invention. Fig. 2 shows a cross-sectional view of a formation of a second oxide layer of a first bond structure according to embodiments of the invention. Fig. 3 shows a cross-sectional view of connecting a structure in the form of IC chips to another structure using the first bonding structure according to embodiments of the invention. Fig. 4 shows a cross-sectional view of a planarization of the IC chips using the first bonding structure according to embodiments of the invention. Fig. 5 shows a cross-sectional view of connecting a structure to the IC chips after deposition of another thick oxide layer for encapsulating the IC chips and removal of another structure according to embodiments of the invention. Fig. 6 a cross-sectional view of connecting another structure to the structure of Fig. 5 after rotation thereof according to embodiments of the invention. Fig. 7 shows a cross-sectional view of a semiconductor device using the first bonding structure according to embodiments of the invention. Fig. 8 shows a cross-sectional view of a formation of a second bond structure according to embodiments of the invention. Fig. 9 a cross-sectional view of connecting another structure to the structure of Fig. 8 after rotation thereof according to embodiments of the invention. Fig. 10 shows a cross-sectional view of a semiconductor device using a first and a second bond structure according to embodiments of the invention. Fig. 11 shows a cross-sectional view of connecting substrates from front to back using a bonding structure according to embodiments of the invention. Fig. 12 shows a cross-sectional view of front-to-back bonding of substrates using bond structures according to embodiments of the invention. Fig. 13 shows a cross-sectional view of connecting IC chips to a carrier wafer using a bonding structure according to embodiments of the invention. Fig. 14 a cross-sectional view of connecting the IC chips of Fig. 13 shows a front-to-back view of another wafer using bond structures according to embodiments of the invention. Fig. 15 shows a cross-sectional view of thinning a substrate after bonding using one or more bond structures according to embodiments of the invention. Fig. 16 shows a cross-sectional view of one or more semiconductor bond structures according to other embodiments of the invention.

[0028] It should be noted that the drawings of the invention are not necessarily to scale. The drawings are intended to illustrate only typical aspects of the invention and are therefore not to be considered limiting the scope of the invention. In the drawings, like reference numerals designate like elements between the drawings. Detailed description

[0029] In the following description, reference is made to the accompanying drawings, which form a part hereof, and in which is shown by way of illustration specific embodiments in which the present invention may be practiced. These embodiments have been described in sufficient detail to enable those skilled in the art to practice the present invention, and it is to be understood that other embodiments may be utilized and changes may be made without departing from the scope of the present invention. The following description, therefore, is for purposes of illustration only.

[0030] When an element such as a layer, region, or substrate is described as being "on" or "over" another element, it may be directly on top of the other element, or there may be intervening elements. On the other hand, when an element is described as being "directly on" or "directly over" another element, there may not necessarily be any intervening elements. When an element is described as being "connected" or "coupled" to another element, it may be directly connected or coupled to the other element, or there may be any intervening elements. On the other hand, when an element is described as being "directly connected" or "directly coupled" to another element, there are no intervening elements.

[0031] Reference in the specification to "one embodiment" or "an embodiment" of the present invention, as well as other variations thereof, means that a particular feature, structure, characteristic, etc. described in connection with the embodiment is provided in at least one embodiment of the present invention. Therefore, the phrases "in one embodiment," as well as any other variations appearing at various points in the specification, do not necessarily all refer to the same embodiment. It is to be understood that the use of " / ," "and / or," and "at least one of," e.g., in the cases "A / B," "A and / or B," and "at least one of A and B," is intended to encompass only the selection of the first listed option (A), only the selection of the second listed option (B), or the selection of both options (A and B).Another example: In the cases of "A, B and / or C" and "at least one of options A, B and C", this wording is intended to cover only the first listed option (A), or only the selection of the second listed option (B), or only the selection of the third listed option (C), or the selection of the first and second listed options (A and B), or the selection of the first and third listed options (A and C), or the selection of the second and third listed options (B and C), or the selection of all three options (A and B and C). This can be extended to any number of listed options, as will be readily apparent to a person skilled in the art.

[0032] Embodiments of the invention include a bonding structure for a semiconductor substrate and a corresponding method. The bonding structure comprises a first oxide layer on the semiconductor substrate and a further, second oxide layer on the first oxide layer, wherein the second oxide layer is connected to another structure, e.g., another substrate (wafer) or chips. The bonding structure can be used to bond or connect chips to wafers or wafers to wafers, with or without conductor-to-conductor features. In any case, the second oxide layer has a higher stress level than the first oxide layer, and the second oxide layer is thinner than the first oxide layer. The second oxide layer can also have a higher density than the first oxide layer. One or more of the bonding structures can be used in a single device. The bonding structure provides greater bond strength than just a thick oxide layer, e.g.,at least 1.0 joule per square meter (J / m. 2 ) compared to about 0.6 J / m 2 a conventional thick oxide layer. In other embodiments, the bond strength can be at least 1.6 J / m 2 The bond structure is free of voids within it. The process for forming the bond structure requires no modifications to the tool. Low temperatures are used during each oxide formation step, which do not damage existing devices. While the invention is described with respect to oxide layers, the teachings of the invention are equally applicable to silicon carbon nitride (SiCN) layers.

[0033] Fig. 1-2 show cross-sectional views of a method for forming a first bond structure 100 ( Fig. 2) according to the embodiments of the invention. Fig. 1-2 illustrate the formation of the first bond structure 100 in a general manner applicable to a variety of applications. As described herein, the first bond structure 100 (hereinafter "bond structure 100") can be used in a variety of semiconductor manufacturing situations to increase bond strength, e.g., in die-to-wafer and / or wafer-to-wafer bonding situations.

[0034] Fig. 1 shows a formation of a first oxide layer 110 on a first structure 112. In the example shown, the first structure 112 may include a semiconductor substrate 114, which in some cases may be referred to as a handle wafer. As used herein, any semiconductor substrate (e.g., substrate 114) may include, for example, a silicon or silicon-based substrate (e.g., a silicon carbide (SiC) substrate or other material that supports epitaxial growth of semiconductors), a sapphire substrate, or another suitable substrate for a III-V semiconductor device. A III-V semiconductor refers to a compound obtained by combining Group III elements, such as aluminum (Al), gallium (Ga), or indium (In), with Group V elements, such as nitrogen (N), phosphorus (P), arsenic (As), or antimony (Sb) (e.g., GaN, InP, GaAs, or GaP). The substrate may or may not include components (not shown), e.g.Transistors or related passive components such as capacitors, resistors, etc. The terms “wafer” and “substrate” can be used interchangeably here.

[0035] The first oxide layer 110 can be formed, for example, by plasma-enhanced chemical vapor deposition (PECVD) based on silane (SiH4), wherein a silicon oxide (SiO x). A gas ratio of silicon hydride (SiH4) to nitrous oxide (N2O) during PECVD can, for example, be in the range of 1:25 to 1:35. In any case, the temperature of PECVD is below 300° Celsius (°C), which protects existing components, e.g., transistors in the semiconductor substrate 114, from thermally induced damage. The first oxide layer 110 can be deposited to a thickness in the range of 5,000 to 15,000 nanometers (nm). The deposition of the first oxide layer 110 can occur at a rate of, for example, 350 - 500 nanometers per minute (nm / min). After deposition is complete, the first oxide layer 110 can have a density in the range of 2.31 - 2.37 grams per cubic centimeter (g / cm 3). The first oxide layer 110 has a relatively low compressive stress in the range of, for example, 70-100 megapascals (MPa). The first oxide layer 110 can have a dielectric constant in the range of, for example, 4.7 to 6.0.

[0036] As part of the manufacturing process, the first oxide layer 110 may be planarized using a known or later developed planarization technique, such as chemical mechanical polishing (CMP) (denoted by a curved arrow). In certain embodiments, the surface of the first oxide layer 110 has a root mean square (RMS) roughness in the range of 0.1-0.5 nanometers (nm).

[0037] Fig. 2 shows the formation of a second oxide layer 120 on the first oxide layer 110, creating the bond structure 100. As described below, the second oxide layer 120 has a higher stress level than the first oxide layer 110. For example, in contrast to the first oxide layer 110, the second oxide layer 120 may have a relatively high compressive stress in a range of, for example, 300-350 MPa. The second oxide layer 120 may also have a higher density than the first oxide layer 110b. Furthermore, the second oxide layer 120 is shown to be thinner than the first oxide layer 110, e.g., T2 <T1. Die zweite Oxidschicht 120 kann mit einer Dicke im Bereich von 0,25 bis 0,75 µm abgeschieden werden. Die zweite Oxidschicht 120 kann z.B. durch PECVD auf Silanbasis (SiH4) gebildet werden, wodurch ein Siliziumoxid (SiO x ) is generated.

[0038] A higher concentration of silane is used to form the second oxide layer 120 than to form the first oxide layer 110. Furthermore, the gas ratio of silicon hydride (SiH4) to nitrous oxide (N2O) during PECVD can range from, for example, 1:200 to 1:250. In any case, the PECVD temperature for the second oxide layer 120 is below 300°C, which further protects existing components, e.g., in the semiconductor substrate 114, from thermally induced damage. The deposition of the second oxide layer 120 can be performed at a rate of, for example, 80–100 nm / min (800–1,000 Å / min). The deposition time of the second oxide layer 120 may therefore be longer than that of the first oxide layer 110, even though the layer 120 is thinner than the layer 110. After completion, the second oxide layer 120 may have a density in the range of 2.43 - 2.52 g / cm 3The second oxide layer 120 may have a dielectric constant in the range of, for example, 4.0 to 4.5. Due to the higher density of the second oxide layer 120, the bond strength between the second oxide layer 120 and the structure to be connected is greater than with a single thick oxide layer. In certain embodiments, the bond strength may be at least 1.0 J / m 2 In other embodiments, the bond strength may be at least 1.6 J / m 2 The bond strength of the bond structure 100 is thus significantly stronger than that of a conventional bond structure with a single thick oxide layer, which typically has a bond strength of about 0.6 J / m 2 The bond structure 100 may include any known or later developed alignment marks (not shown) for aligning other structures thereto. As described below, hybrid bond pads may be formed by the bond structure 100.

[0039] As part of its formation, the second oxide layer 120 may be planarized using a known or later developed planarization process, such as, without limitation, CMP (indicated by a curved arrow). In certain embodiments, a surface of the second oxide layer 120 has an RMS roughness in the range of 0.1-0.5 nm.

[0040] Fig. Figure 2 shows the bonding structure 100 for a semiconductor substrate 114 and a semiconductor device 102 according to embodiments of the invention. The bonding structure 100 comprises a first oxide layer 110 on the semiconductor substrate 114 and a second oxide layer 120 on the first oxide layer 110. The second oxide layer 120 may be used for connecting to another structure, e.g., as shown in Fig. 3, a second structure 130 with IC chips 132. The second oxide layer 120 has a higher stress level than the first oxide layer 110. In contrast to the first oxide layer 110 with a compressive stress of, for example, 70-100 MPa, the second oxide layer 120 may have a relatively high compressive stress in a range of, for example, 300-350 MPa. The second oxide layer 120 may also have a higher density than the first oxide layer 110. Furthermore, the second oxide layer 120 is thinner than the first oxide layer 110. For example, the first oxide layer 110 may have a thickness in the range of 5 to 15 µm and the second oxide layer 120 may have a thickness in the range of 0.25 to 0.75 µm.

[0041] Fig. 3-15 show cross-sectional views of various ways of using the bond structure 100 according to embodiments of the invention.

[0042] Fig. 3-4 show cross-sectional views for one type of use of the bond structure 100. In particular, Fig. 3 illustrates bonding of the second oxide layer 120 of the bonding structure 100 to a second structure 130. In this example, the second structure 130 comprises a plurality of integrated circuit chips (IC chips) 132, each having a dielectric layer 134 (e.g., silicon oxide or silicon nitride) thereover, which may extend over various thicknesses. The second structure 130 may be connected to the structure 100 in any manner known today or later developed, e.g., by detaching chips from a tape, chips on a tape frame, or chips removed from a chipset. After positioning, the structures 100 and 130 may be annealed (curved arrows in Fig. 3). According to the presentation in Fig. 4, planarization (e.g., CMP) of the dielectric layer 134 can then be performed. The bond structure 100 provides sufficient bond strength to prevent the IC chips 132 from being removed during the planarization process.

[0043] Fig. 5-7 show cross-sectional views of another possible use of the bond structure 100. Fig. 5 shows forming a third oxide layer 140 over the second structure 130 (as in Fig. 4). The third oxide layer 140 may be formed using the methods described herein with respect to the first oxide layer 110. The third oxide layer 140 may be formed, for example, by silane-based PECVD (SiH4), forming a silicon oxide (SiO x). The gas ratio of silicon hydride (SiH2) to nitrous oxide (N2O) during PECVD can, for example, range from 1:25 to 1:35. In any case, the temperature of the PECVD process is below 300°C, which protects existing components such as IC chips 132 from thermal damage. The third oxide layer 140 can be deposited to a thickness in the range of 5 to 15 µm and can encapsulate the IC chips 132 of the second structure 130. The deposition of the third oxide layer 140 can occur at a rate in the range of, for example, 350 - 500 nm / min (3,500 - 5,000 Å / min). Upon completion, the third oxide layer 140 can have a density in the range of 2.31-2.37 g / cm 3The third oxide layer 140 has a relatively low compressive stress in the range of, for example, 70 - 100 MPa. The third oxide layer 140 may have a dielectric constant in the range of, for example, 4.7 to 6.0. After fabrication, the third oxide layer 140 may be planarized (see planarization and thinning described in Fig. 5 are indicated by dashed boxes), using all processes known today or later developed, e.g. CVD layer planarization and / or CMP.

[0044] According to the presentation in Fig. 5, in certain embodiments, a third structure 150 may then be connected to the third oxide layer 140 - see upper arrow in Fig. 5. In the example shown, the third structure 150 may include a semiconductor substrate 152, which may include any form of integrated circuit and / or bonding structure, e.g., additional transistors, metal wires and contacts, etc. The semiconductor substrate 152 may include any semiconductor material, such as silicon, silicon germanium, silicon carbide, etc., and may or may not include semiconductor devices (not shown). The first structure 112 may then be removed using any known or later developed technique, which may thin the first oxide layer 110.

[0045] Fig. 6 shows the structure after rotating the second structure 150, as in Fig. 5 so that it is located under the bond structure 100. Fig. 6 and Fig. 7 show bonding of a fourth structure 160 to a third structure 150 using the bond structure 100. Here, the first oxide layer 110 of the bond structure 100 bonds to the fourth structure 160. In the example shown, the fourth structure 160 may comprise a substrate 162, which may, for example, comprise any form of bond structure such as metal wires and contacts, etc.

[0046] With further reference to Fig. 5 and with reference to Fig. 8-10, a second bond structure 170 ( Fig. 8) may be used in another embodiment with the first bond structure 100. Fig. 8 shows forming the second bond structure 170 on the second structure 130 (as in Fig. 4). According to the description in relation to Fig. 5, the method comprises forming a third oxide layer 140 on the second structure 130. In contrast to the embodiment in Fig. 5, the procedure as in Fig. 8, may also include forming a fourth oxide layer 180 on the third oxide layer 140. The fourth oxide layer 180 is formed as described in connection with the second oxide layer 120. That is, the fourth oxide layer 180 may be formed, for example, by silane-based (SiH4) PECVD, wherein a silicon oxide (SiO x). A higher concentration of silane is used in the formation of the fourth oxide layer 180 than in the formation of the first or third oxide layers 110, 140. In addition, a gas ratio of silicon hydride (SiH2) to nitrous oxide (N2O) in PECVD can be in a range of, for example, 1:20 to 1:25. In any case, the PECVD temperature for the fourth oxide layer 180 is below 300°C, while pre-existing components, e.g., IC chips 132 or other components in the first structure 114, are still protected from thermally induced damage. The fourth oxide layer 180 can be planarized as described with respect to the second oxide layer 120, e.g., to a surface RMS roughness in the range of 0.1 to 0.5 nm.

[0047] The fourth oxide layer 180 has a higher stress level than the third oxide layer 140. For example, in contrast to the third oxide layer 140 (and similar to the second oxide layer 120), the fourth oxide layer 180 may have a relatively high compressive stress in a range of, for example, 300-350 MPa. The fourth oxide layer 180 may also have a higher density than the third oxide layer 140. In addition, as shown, the fourth oxide layer 180 is thinner than the third oxide layer 110 (i.e., T3 <T4). Die vierte Oxidschicht 180 kann mit einer Dicke im Bereich von 0,25 bis 0,75 µm abgeschieden werden. Die Abscheidung der vierten Oxidschicht 180 kann mit einer Geschwindigkeit von beispielsweise 80 - 100 nm / min (800 - 1.000 Å / min) erfolgen. Die Dauer der Abscheidung der vierten Oxidschicht 180 könnte somit länger sein als die der ersten und dritten Oxidschicht 110, 140, obwohl die Schicht 180 dünner ist als die Schichten 110, 140.After completion, the fourth oxide layer 180 may have a density in the range of 2.43 - 2.52 g / cm. 3 The fourth oxide layer 180 may have a dielectric constant in the range of, for example, 4.0 to 4.5. Due to the higher voltage in the fourth oxide layer 180, the bond strength between the fourth oxide layer 180 and another structure is at least 1.0 J / m 2 when the fourth oxide layer 180 is used to connect to another structure. In other embodiments, the bond strength may be at least 1.6 J / m 2 The bond strength of the second bond structure 170 is thus significantly stronger than that of a conventional bond structure with a single thick oxide layer, which typically has a bond strength of about 0.6 J / m 2The second bond structure 170 may include any known or later developed alignment marks (not shown) for aligning other structures thereto. Hybrid bond pads (not shown) may be formed by the second bond structure 170 if desired.

[0048] According to the presentation in Fig. 8, the third structure 150 is connected to the second bonding structure 170, and in particular to the fourth oxide layer 180. The connection or bonding can be performed using any method known today or later developed. The first structure 112 can then be removed using any technique known or later developed, thereby making the first oxide layer 110 thinner.

[0049] Fig. Figure 9 shows the structure after rotating the second structure 150 so that it is located under the first bond structure 100 (and the second bond structure 170). Fig. 9 and Fig. 10 illustrates bonding of a fourth structure 160 to a third structure 150 using the first bond structure 100. Here, the first oxide layer 110 connects to the fourth structure 160. In the example shown, the fourth structure 160 may include a substrate 162, which may include any form of bond structures, e.g., metal wires and contacts. The bonding may include any method known today or later developed.

[0050] Fig. 10 also shows the semiconductor device 102 with a second bonding structure 170 for bonding the fourth structure 160 to another structure, e.g., IC chips 132 of the second structure and / or the third structure 150. As already mentioned, the second bonding structure 170 comprises a third oxide layer 140 on the structure 150 and a fourth oxide layer 180 on the third oxide layer 140. As described, the fourth oxide layer 180 has a higher density and a higher stress level than the third oxide layer 140, and the fourth oxide layer 180 is thinner than the third oxide layer 140. The bonding strength of the second bonding structure 170 between the fourth oxide layer 180 and the structure 150 is at least 1.0 joule per square meter (J / m 2 ). In other embodiments, the bond strength may be at least 1.6 J / m 2 be.

[0051] With reference to the Fig. 11 to 15 show cross-sectional views of alternative embodiments and / or applications of the bond structure(s) 100, 170. These embodiments include various processes, some of which may be referred to as hybrid bonding processes, in which another device, a wafer, or IC chips are bonded with a direct conductor-to-conductor connection.

[0052] Fig. 11 shows a bonding process similar to that of Fig. 6 with a front-to-back wafer-to-wafer hybrid bonding. In Fig. 11, the structure 100 is formed with the oxide layers 110 and 120 on the structure 200 (e.g., a silicon carrier), including the through silicon vias (TSVs) 202 on the backside(s) of the devices 204 and the associated interconnect layers 206 therein. The oxide layers 110, 120 may be formed as described herein after exposure of the TSVs 202, e.g., by a grinding, etching, and planarization process. Hybrid bond pads 208 would then be formed on the TSVs 202 in any known or later developed manner, e.g., a simple copper damascene process and planarization. The structure 200 is then bonded to a front side of another structure 210 comprising similar, aligned hybrid bond pads 212. The hybrid bond pads 208, 212 form a direct conductor-to-conductor (e.g., Cu-Cu) hybrid connection in a known manner.However, the bond structure 100 provides a stronger bond strength between the structures 200, 210, as described herein. Although illustrated on only one structure 200, the bond structure 100 may be formed on both structures 200, 210.

[0053] Fig. 12 shows a bonding process similar to that in Fig. 11, but with front-to-front wafer hybrid bonding. Each structure 200, 210 has hybrid bond pads 202, 212 on a front side of the devices 204, 214. In this case, the oxide layers 110, 120 may be formed on the front side of the structures 200, 210 as described, i.e., before formation of the hybrid bond pads. The hybrid bond pads 202, 212 would then be formed in the respective structures 200, 210 in any manner known today or later developed, e.g., by a dual copper damascene process for connecting to the devices 204, 214, followed by planarization. A front side of the structure 200 may be connected to the front side of the structure 210 using aligned hybrid bond pads 202, 212. The hybrid bond pads 202, 212 form a direct conductor-to-conductor (e.g., Cu-Cu) hybrid connection in a known manner.However, the bond structure 100 provides a stronger bond strength between the structures 200, 210, as described herein. The bond structure 100 may be formed on only one of the structures 200, 210, although it is shown on both structures 200, 210.

[0054] Fig. 13 to 14 show cross-sectional views of another application. According to the illustration in Fig. 13, in this application, IC chips 132 with the bond structure 100 thereon can be prepared and singulated. The IC chips 132 can originate from separate wafers with different IC structures and functions, e.g., logic and memory chips, or the IC chips 132 can originate from different IP nodes. The IC chips 132 can be tested and classified as "known good dies" with high yield before the IC chips from different sources are bonded to a carrier wafer 220. The IC chips 132 are bonded by direct bonding (fusion bonding) to a first carrier wafer 220, which also includes the bond structure 100. As shown in Fig. 14, the IC chips 132 are encapsulated in a dielectric layer 222 and removed together from the first carrier wafer 220 ( Fig. 13). The IC chips 132 are then connected to a second carrier wafer 224 by direct bonding (fusion bonding). The second carrier wafer 224 may also include the bond structure(s) 100. The Fig. The structures shown in Figure 15 are then connected to another structure 230 comprising the connections provided therein, e.g., metal wires and vias, by direct front-to-front bonding using the bond structures 100. The bond structure(s) 100 have sufficient bond strength to prevent separation of the structures.

[0055] Fig. 15 and Fig. 16 show cross-sectional views of thinning structures, such as semiconductor substrates, e.g., using planarization (curved arrow). Fig. 15 shows a thinning of the embodiment of Fig. 12 and Fig. 16 shows a thinning of the embodiment of Fig.14. In both cases, the bond structure(s) 100 provide improved bond strength to withstand the planarization process.

[0056] Embodiments of the invention offer various technical and commercial advantages, examples of which are described herein. One or more of the bond structures 100, 170 may be used in a single device. The bond structure(s) 100, 170 provide(s) higher bond strength than a thick oxide layer alone, e.g., at least 1.0 joule per square meter (J / m 2 ) compared to about 0.6 J / m 2 In other embodiments, the bond strength may be at least 1.6 J / m 2Furthermore, the bond structure(s) 100, 170 are free of voids therein. The process for fabricating the bond structure(s) 100, 170 requires no tool modification, and all oxide formation steps utilize low temperatures that do not damage existing components.

[0057] The process described above is used in the manufacturing and packaging of integrated circuit chips. The package can be part of either (a) an intermediate product, such as a motherboard, or (b) a final product. The final product can be any product incorporating integrated circuit chips, ranging from toys and other simple applications to sophisticated computer products with a screen, keyboard or other input device, and a central processor. Final products can also include mobile displays and other microLED products, as well as RF chips and corresponding mobile displays.

[0058] The terminology used herein is for the purpose of describing particular embodiments only and is not intended to be limiting of the invention. As used herein, the singular forms “a,” “an,” and “the” include the plural forms unless the context clearly indicates otherwise. It is further understood that the terms “comprises” and / or “comprising,” when used in this description, specify the presence of certain features, integers, steps, operations, elements, and / or components, but do not preclude the presence or addition of one or more other features, integers, steps, operations, elements, components, and / or groups thereof. “Optional” means that the subsequently described event or circumstance may or may not occur, and that the description includes instances where the event occurs and instances where it does not occur.

[0059] Vague language, as used herein in the specification and claims, can be used to modify any quantitative representation that could permissibly vary without resulting in a change in the basic function to which it relates. Accordingly, a value modified by one or more terms such as "approximately," "approximately," and "substantially" is not limited to the precisely stated value. In at least some cases, the vague language may correspond to the accuracy of an instrument for measuring the value. Here and throughout the specification and claims, range limits may be combined and / or interchanged; such ranges are identified and include all subranges encompassed therein, unless the context or language indicates otherwise.The term "approximately", when referring to a specific value within a range, applies to both values ​​and, unless otherwise dependent on the precision of the measuring instrument, may mean + / - 10% of the stated value(s).

Claims

[1] Bond structure (100) for a semiconductor substrate (114), the bond structure (100) comprising: a first oxide layer (110) on the semiconductor substrate (114); and a second oxide layer (120) on the first oxide layer (110), the second oxide layer (120) serving to connect to another structure (130), wherein the second oxide layer (120) has a higher stress level than the first oxide layer (110) and the second oxide layer (120) is thinner than the first oxide layer (110). [2] The bonding structure (100) of claim 1, wherein the second oxide layer (120) has a higher density than the first oxide layer (110). [3] A semiconductor device (102) comprising: a semiconductor substrate (114); and a first bond structure (100) between the semiconductor substrate (114) and a first structure (112), the first bond structure (100) comprising: a first oxide layer (110) on the semiconductor substrate (114), and a second oxide layer (120) on the first oxide layer (110) connected to the first structure (112); wherein the second oxide layer (120) has a higher stress level than the first oxide layer (110) and the second oxide layer (120) is thinner than the first oxide layer (110). [4] The semiconductor device (102) of claim 3, wherein the second oxide layer (120) has a higher density than the first oxide layer (110). [5] Semiconductor device (102) according to claim 4, wherein the first oxide layer (110) has a density in a range of 2.31 to 2.37 g / cm 3 and the second oxide layer (120) has a density in a range of 2.43 to 2.52 g / cm 3 has. [6] The semiconductor device (102) of claim 3, further comprising a second bonding structure (170) for connecting a second structure (150) to the first structure (112), the second bonding structure (170) comprising: a third oxide layer (140) on the first structure (112), and a fourth oxide layer (180) on the third oxide layer (140), wherein the fourth oxide layer (180) has a higher density and a higher stress level than the third oxide layer (140) and the fourth oxide layer (180) is thinner than the third oxide layer (140). [7] The semiconductor device (102) of claim 3, wherein the first oxide layer (110) has a thickness in the range of 5,000 to 15,000 nm and the second oxide layer (120) has a thickness in the range of 250 to 750 nm. [8] The semiconductor device (102) of claim 3, wherein the first oxide layer (110) has a compressive stress in a range of 70 to 100 MPa and the second oxide layer (120) has a compressive stress in a range of 300 to 350 MPa. [9] The semiconductor device (102) of claim 3, wherein at least one of the first oxide layer (110) and the second oxide layer (120) has a surface with a root mean square roughness in the range of 0.1 to 0.5 nm. [10] The semiconductor device (102) of claim 3, wherein a bond strength between the second oxide layer (120) and the first structure (112) is at least 1.0 J / m 2 amounts. [11] A method comprising: forming a first bond structure (100), wherein the forming comprises: forming a first oxide layer (110) on a first structure (112); forming a second oxide layer (120) on the first oxide layer (110), wherein the second oxide layer (120) has a higher stress level than the first oxide layer (110) and the second oxide layer (120) is thinner than the first oxide layer (110); and connecting the second oxide layer (110) to a second structure (130). [12] The method of claim 11, wherein the second oxide layer (120) has a higher density than the first oxide layer (110). [13] The method of claim 12, wherein the first oxide layer (110) has a density in a range of 2.31 to 2.37 g / cm 3 and the second oxide layer (120) has a density in a range of 2.43 to 2.52 g / cm 3 has. [14] The method of claim 11, wherein the formation of the first oxide layer (110) and the formation of the second oxide layer (120) each occur at a temperature of less than 300°C. [15] The method of claim 11, wherein forming the first oxide layer (110) comprises depositing the first oxide layer (110) to a thickness in the range of 5,000 to 15,000 nm, and wherein forming the second oxide layer (120) comprises depositing the second oxide layer (120) to a thickness in the range of 250 to 750 nm. [16] The method of claim 11, wherein the first oxide layer (110) has a compressive stress in the range of 70 to 100 MPa and the second oxide layer (120) has a compressive stress in the range of 300 to 350 MPa. [17] The method of claim 11, wherein at least one of forming the first oxide layer (110) and forming the second oxide layer (120) comprises planarizing a surface of the respective oxide layer to have a root mean square roughness in the range of 0.1 to 0.5 nanometers. [18] The method of claim 11, wherein a bond strength between the second oxide layer (120) and the first structure (112) is at least 1.0 J / m 2 amounts. [19] The method of claim 11, further comprising: forming a second bond structure (170) on the second structure (130), comprising: forming a third oxide layer (140) on the second structure (130), and forming a fourth oxide layer (180) on the third oxide layer (140), wherein the fourth oxide layer (180) has a higher density and a higher stress level than the third oxide layer (140) and the fourth oxide layer (180) is thinner than the third oxide layer (140); and connecting a third structure (150) to the fourth oxide layer (180). [20] The method of claim 19, wherein forming the third oxide layer (140) comprises depositing the third oxide layer (140) to a thickness in a range of 5,000 to 15,000 nm and forming the fourth oxide layer (180) comprises depositing the fourth oxide layer (180) to a thickness in a range of 250 to 750 nm.

Citation Information

Patent Citations

  • Wafer bonding structure and wafer bonding method

    CN108461512A