Power storage module and manufacturing process for it
By integrating a thickness setting component that aligns with the first sealing sections, the bipolar battery module addresses thickness deviations, ensuring accurate stacking and reducing sealing errors, thus improving the module's airtightness and durability.
Patent Information
- Application Number
- DE112019004787
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2019-09-25
- Publication Date
- 2024-10-24
- Estimated Expiration
- 2039-09-25
AI Technical Summary
Existing bipolar battery modules face issues with sealing errors due to deviations in the thickness of the electrode stack body, leading to potential form and sealing defects.
Incorporation of a thickness setting component that is arranged to overlap the first sealing sections in the stacking direction, allowing for precise control of the electrode stack body thickness, ensuring accurate alignment and simplifying the design by using the same material as the first sealing sections.
This approach effectively suppresses sealing errors and maintains the form of the electrode stack body, reducing position deviations and simplifying the manufacturing process while enhancing the airtightness and durability of the module.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
Technical area
[0001] The present disclosure relates to a power storage module and a manufacturing method thereof. Technical background
[0002] As a power storage module in the prior art, a bipolar battery is known that has bipolar electrodes in which a positive electrode is formed on one surface of a metal plate and a negative electrode is formed on the other surface (see, for example, Patent Literature 1). The bipolar battery has an electrode stack body obtained by stacking a plurality of bipolar electrodes via a separator. A sealing body that seals a space between bipolar electrodes adjacent in a stacking direction is provided on one side surface of the electrode stack body, and an electrolytic solution is stored in an internal space formed between the bipolar electrodes. Citation listPatent literature
[0003] Patent literature 1: JP 2011- 204 386 A
[0004] US 2013 / 0 095 366 A1 discloses a power storage module comprising: an electrode stack body having a stack body in which a plurality of bipolar electrodes are stacked, a pair of terminal electrodes located on an outer side of the stack body in a stacking direction of the bipolar electrodes, and a plurality of metal plates constituting the stack body and the pair of terminal electrodes;and a sealing body provided to surround a side surface of the electrode stack body, the sealing body having a plurality of first sealing portions coupled to edge portions of the plurality of metal plates and a second sealing portion coupling the first sealing portions to each other, and a thickness adjustment member that adjusts the thickness of the electrode stack body in the stacking direction is arranged in the electrode stack body at a position of overlapping the first sealing portions as viewed from the stacking direction.
[0005] JP 2010-92662 A and JP 2010-272266 A each disclose a power storage module comprising: an electrode stack body including a stacked body in which a plurality of bipolar electrodes are stacked, a pair of terminal electrodes located on an outer side of the stacked body in a stacking direction of the bipolar electrodes, and a plurality of metal plates constituting the stack body and the pair of terminal electrodes; and a sealing body provided to surround a side surface of the electrode stack body, the sealing body having a plurality of first sealing portions coupled to edge portions of the plurality of metal plates, and a thickness adjustment member that adjusts the thickness of the electrode stack body in the stacking direction, disposed in the electrode stack body at a position of overlapping the first sealing portions as viewed from the stacking direction. Summary of the inventionTechnical problem
[0006] For example, in the power storage module as described above, a first sealing portion is formed in each edge portion of the metal plate of the bipolar electrode, and a plurality of the first sealing portions are coupled by a second sealing portion formed by injection molding or the like, thereby forming a sealing body. When forming the second sealing portion, it is important to properly manage the thickness of the electrode stack body having the first sealing portions in a stacking direction. If the thickness of the electrode stack body deviates from the standard in the stacking direction, this will result in a molding error of the second sealing portion, and there is a concern that a sealing failure of the power storage module may be caused.
[0007] The present disclosure has been made to solve the problem, and it is an object thereof to provide a power storage module and a manufacturing method thereof capable of suppressing a sealing failure. Solution to the problem
[0008] The object of the invention is achieved with a power storage module according to claim 1 and a method for producing a power storage module according to claim 18. Advantageous developments of the invention are the subject matter of claim 18 of the dependent claims.
[0009] According to one aspect of the present invention, there is provided a power storage module comprising: an electrode stack body including a stacked body in which a plurality of bipolar electrodes are stacked, a pair of terminal electrodes located on an outer side of the stacked body in a stacking direction of the bipolar electrodes, and a plurality of metal plates constituting the stack body and the pair of terminal electrodes; and a sealing body provided to surround a side surface of the electrode stack body. The sealing body has a plurality of first sealing portions coupled to edge portions of the plurality of metal plates, and a second sealing portion coupling the first sealing portions to each other.A thickness adjustment member that adjusts the thickness of the electrode stack body in the stacking direction is arranged in the electrode stack body at a position of overlapping the first sealing portions as viewed from the stacking direction.
[0010] In the power storage module, the thickness adjustment member that adjusts the thickness of the electrode stack body in the stacking direction is arranged. Since the thickness of the electrode stack body having the first sealing portions in the stacking direction is adjusted by the thickness adjustment member, the thickness of the electrode stack body having the first sealing portion in the stacking direction can be easily set within the standard when forming the second sealing portion. Furthermore, since the thickness adjustment member is arranged at a position where the first sealing portions overlap as viewed from the stacking direction, a shape of the entire electrode stack body including the first sealing portion can be maintained even after the thickness adjustment member is arranged.Accordingly, the occurrence of a molding error of the second sealing portion can be suppressed, and the occurrence of a sealing error of the electrode stack body can be suppressed. Furthermore, since the thickness adjustment member is arranged at the position where the thickness adjustment member overlaps the first sealing portions when viewed from the stacking direction, the thickness adjustment member and the first sealing portions can be set to the same shape when viewed from the stacking direction. As a result, when the thickness adjustment member and the first sealing portion are formed by punching, a punching die for the thickness adjustment member and the first sealing portion can be made common to each other.
[0011] The thickness adjustment member may be formed of the same material as the first sealing portions and may be configured separately from the first sealing portions. Accordingly, the material of the thickness adjustment member and the material of the first sealing portions may be made common to each other, and a simplification of the design of the power storage module may be realized. The thickness adjustment member may be configured through the first sealing portions.
[0012] One of the pair of terminal electrodes may be a negative terminal electrode, the other of the pair of terminal electrodes may be a positive terminal electrode, and the thickness adjusting member may be arranged on at least one side between the stacked body and the negative terminal electrode and between the stacked body and the positive terminal electrode in the stacking direction.
[0013] The thickness adjustment member may be disposed between the stacked body and the negative terminal electrode, and at an edge portion of an inner surface of the metal plate of the negative terminal electrode in the stacking direction. The thickness adjustment member may be disposed between the stacked body and the positive terminal electrode, and at the first sealing portion coupled to an edge portion of an inner surface of the metal plate of the positive terminal electrode in the stacking direction. In this case, since the thickness adjustment member is sandwiched between the first sealing portions adjacent to each other, the occurrence of positional deviation between the first sealing portions and the thickness adjustment member can be suppressed.
[0014] The thickness adjustment member can be arranged both between the stacked body and the negative terminal electrode and between the stacked body and the positive terminal electrode in the stacking direction. In this case, since the thickness adjustment member can be arranged when the negative terminal electrode and the positive terminal electrode are stacked on the stacked body of the bipolar electrodes, arrangement of the thickness adjustment member on the electrode stacked body can be made easy. Furthermore, the thickness of the electrode stacked body can be finely adjusted in the stacking direction by a combination of the thickness adjustment member arranged between the stacked body and the negative terminal electrode and the thickness adjustment member arranged between the stacked body and the positive terminal electrode.
[0015] The thickness of the thickness adjustment member disposed between the stack body and the negative terminal electrode and the thickness of the thickness adjustment member disposed between the stack body and the positive terminal electrode can be the same for both. In this case, fine adjustment of the thickness of the electrode stack body in the stacking direction and simplification of design of the power storage module can be made compatible with each other. Furthermore, in this case, an internal space close to the negative terminal electrode of the electrode stack body and an internal space close to the positive terminal electrode of the electrode stack body can be made equal. As a result, a change in the internal space between respective electrodes in the electrode stack body can be suppressed to the minimum, and a deviation in a state of charge (SOC) between the respective electrodes can be reduced.
[0016] The thickness adjustment component can be arranged anywhere between the stacked body and the negative terminal electrode, and between the stacked body and the positive terminal electrode in the stacking direction. In this case, the thickness of the electrode stacked body can be adjusted in the stacking direction while avoiding an increase in the number of parts.
[0017] According to the invention, the electrode stack body further includes an outermost metal plate located on an outer side of one of the pair of terminal electrodes in the stacking direction, and the stack body further includes separators stacked alternately with the bipolar electrodes along the stacking direction. The first sealing portions are coupled to edge portions of the metal plates and the outermost metal plate, and the second sealing portion covers one side surface of the plurality of first sealing portions. The thickness adjustment member is located between one of the pair of terminal electrodes and the outermost metal plate and adjusts the thickness of the electrode stack body in the stacking direction. In this case, the thickness adjustment member is located between one of the pair of terminal electrodes and the outermost metal plate and at a position overlapping the first sealing portions in the stacking direction.Accordingly, at the time of manufacturing the power storage module, the thickness adjustment member can be arranged in the position before the second sealing portion is formed. Accordingly, a total thickness of the electrode stack body and the thickness adjustment member in the stacking direction can be set to a standard thickness determined in advance before forming the second sealing portion. Therefore, when the second sealing portion is formed, occurrence of a formation error of the second sealing portion can be suppressed. As a result, it is possible to provide a power storage module that can suppress occurrence of the sealing error.
[0018] One of the pair of terminal electrodes may be a negative terminal electrode, the thickness adjustment member may be in contact with the outermost metal plate and the first sealing portion coupled to the metal plate of the negative terminal electrode, and the thickness adjustment member may be spaced apart from the negative terminal electrode. In this case, since the negative terminal electrode is protected from an external environment by the outermost metal plate, deterioration of the negative terminal electrode can be suppressed. Furthermore, since the thickness adjustment member is spaced apart from the negative terminal electrode, a function exhibited by the thickness adjustment member is less likely to be adversely affected by the negative terminal electrode.
[0019] One of the pair of terminal electrodes may be a negative terminal electrode, and the thickness adjusting member may be in contact with the negative terminal electrode and the outermost metal plate.
[0020] One of the pair of terminal electrodes may be a positive terminal electrode, and the thickness adjustment component may be in contact with the positive terminal electrode and the outermost metal plate. In this case, since the positive terminal electrode is protected from the external environment by the outermost metal plate, deterioration of the positive terminal electrode can be suppressed. Furthermore, the thickness adjustment component is firmly fixed by the positive terminal electrode and the outermost metal plate.
[0021] The electrode stack body may further include an additional outermost metal plate located on an outer side of the other of the pair of terminal electrodes in the stacking direction, and an additional thickness adjustment member that adjusts the thickness of the electrode stack body in the stacking direction may be located between the other of the pair of terminal electrodes and the additional outermost metal plate, and at a position overlapping the first sealing portions in the stacking direction. In this case, a total thickness of the electrode stack body and each thickness adjustment member along the stacking direction can be adjusted to a standard thickness with accuracy before the second sealing portion is formed.
[0022] An alkaline electrolytic solution may be stored in an internal space formed by the electrode stack body and the sealing body, and an excess space may be formed by the negative terminal electrode, the first sealing portion coupled to the metal plate of the negative terminal electrode, the outermost metal plate, and the thickness adjustment member. There is a concern that the alkaline electrolytic solution stored in the internal space may leak to the outside of the power storage module through a gap between the first sealing portion and the metal plate of the negative terminal electrode due to a so-called alkali creep phenomenon. In contrast, since the electrode stack body has the outermost metal plate located on an outer side of the terminal electrode in the stacking direction, the excess space is formed.Accordingly, the flowing alkaline electrolytic solution can be suppressed from escaping to the outside of the power storage module. Furthermore, penetration of moisture contained in outside air from the gap between the negative terminal electrode and the first sealing portion can also be suppressed. Accordingly, acceleration of the alkaline creep phenomenon caused by the moisture can be suppressed. As a result, flow of the alkaline electrolytic solution to the outside of the power storage module can be satisfactorily suppressed.
[0023] The first sealing portion may be coupled to an edge portion of the additional outermost metal plate, and the second sealing portion may couple the first sealing portions coupled to the metal plates of the bipolar electrodes, the first sealing portion coupled to the outermost metal plate, and the first sealing portion coupled to the additional outermost metal plate. In this case, the electrode stack body including the bipolar electrodes, the outermost metal plate, and the additional outermost metal plate can be tightly integrated.
[0024] A distance from one of the pair of terminal electrodes to the edge portion of the outermost metal plate along the stacking direction may be different from a distance from the other of the pair of terminal electrodes to an edge portion of the additional outermost metal plate along the stacking direction.
[0025] The outermost metal plate may have a first contact portion in contact with one of the pair of terminal electrodes, the additional outermost metal plate may have a second contact portion in contact with the other of the pair of terminal electrodes, and a region of the first contact portion may be different from a region of the second contact portion when viewed from the stacking direction.
[0026] The other of the pair of terminal electrodes may be a negative terminal electrode. The electrode stack body may further include an additional outermost metal plate located on an outer side of the negative terminal electrode in the stacking direction. An alkaline electrolytic solution may be stored in an internal space formed by the electrode stack body and the sealing body, and a first excess space may be formed by the negative terminal electrode, the first sealing portion coupled to the metal plate of the negative terminal electrode, and the additional outermost metal plate. Even in this case, as described above, flow of the alkaline electrolytic solution to the outside of the power storage module due to the alkali creep phenomenon can be satisfactorily suppressed.Moreover, since the first excess space is formed without using the thickness adjustment member, a shape and a volume of the first excess space can be strictly defined, and airtightness of the first excess space can be ensured.
[0027] A second excess space may be formed by the negative terminal electrode, the first sealing portion coupled to the metal plate of the negative terminal electrode, the first sealing portion coupled to the metal plate of the bipolar electrode adjacent to the negative terminal electrode in the stacking direction, and the second sealing portion. In this case, the flow of the alkaline electrolytic solution to the outside of the power storage module due to the alkali creep phenomenon can be more satisfactorily suppressed.
[0028] The thickness adjustment member may include a plurality of layered members stacked along the stacking direction. In this case, the thickness of the thickness adjustment member can be easily adjusted by changing the number of layered members included in the thickness adjustment member. Accordingly, a thickness adjustment member corresponding to each power storage module can be easily provided.
[0029] Each of the thickness adjustment member and the plurality of first sealing portions may contain an alkali-resistant thermoplastic resin. In this case, when the second sealing portion is formed, the first sealing portion and the second sealing portion can be coupled in a satisfactory manner.
[0030] According to another aspect of the present invention, a method for manufacturing a power storage module is provided.The method includes the steps of: forming a stacked body by alternately stacking bipolar electrodes, to which first sealing portions are respectively coupled, and separators along a stacking direction; measuring the thickness of the stacked body along the stacking direction; calculating the difference between the thickness of the stacked body and a standard thickness of the stacked body along the stacking direction; stacking a thickness adjustment member having a thickness corresponding to the difference at the first sealing portion in the stacking direction; stacking an outermost metal plate, to which an additional first sealing portion is coupled, on the stacked body over the thickness adjustment member; and forming a second sealing portion that couples the first sealing portions, the thickness adjustment member, and the additional first sealing portion.
[0031] In the method for manufacturing the power storage module, the thickness adjustment member having a thickness corresponding to a difference between a dimension of the stacked body along the stacking direction and a standard thickness of the stacked body is placed on or over the first sealing portion before forming the second sealing portion. Accordingly, before forming the second sealing portion, it is possible to adjust a total thickness of the first sealing portions included in the stacked body, the thickness adjustment member, and the outermost metal plate along the stacking direction to the standard thickness determined in advance. Accordingly, when forming the second sealing portion, occurrence of a formation error of the second sealing portion can be suppressed. Accordingly, according to the manufacturing method, occurrence of the sealing error of the power storage module can be suppressed.
[0032] The thickness of the thickness adjustment member may correspond to a difference between a total value obtained by adding the thickness of the outermost metal plate along the stacking direction to the thickness of the stacked body and a total standard value obtained by adding a standard thickness of the outermost metal plate along the stacking direction to the standard thickness of the stacked body along the stacking direction. In this case, the total thickness can be accurately adjusted within a range of the total standard value.
[0033] The formation of the stacked body and the measurement of the stacked body thickness can be performed simultaneously. In this case, it is possible to shorten the time required to manufacture the power storage module. Advantageous effects of the invention
[0034] According to the power storage module and the manufacturing method thereof, occurrence of a sealing failure can be suppressed. Short description of the drawings Fig. 1 is a schematic cross-sectional view illustrating a power storage device including a power storage module according to a first embodiment, which is not covered by the claims but is useful for understanding the invention. Fig. 2 is a schematic cross-sectional view illustrating an internal configuration of the power storage module used in Fig. 1 is shown. Fig. 3 is an enlarged cross-sectional view showing a part of the power storage module used in Fig. 2 is shown. Fig. 4 is a schematic cross-sectional view illustrating an internal configuration of a power storage module according to a first modification example of the first embodiment, which is not covered by the claims but is useful for understanding the invention. Fig. 5 is a schematic cross-sectional view illustrating an internal configuration of a power storage module according to a second modification example of the first embodiment, which is not covered by the claims but is useful for understanding the invention. Fig. 6 is a schematic cross-sectional view illustrating an internal configuration of a power storage module according to a second embodiment. Fig. 7 is an enlarged view of a main area in Fig. 6. Fig. 8 is a flowchart illustrating a method of manufacturing the power storage module used in Fig. 6 is shown. Fig. 9 is a schematic cross-sectional view illustrating an internal configuration of a power storage module according to a first modification example of the second embodiment. Fig. 10 is a schematic cross-sectional view illustrating an internal configuration of a power storage module according to a second modification example of the second embodiment. Fig. 11 is a schematic cross-sectional view illustrating an internal configuration of a power storage module according to a third modification example of the second embodiment. Fig. 12 is a schematic cross-sectional view illustrating an internal configuration of a power storage module according to a fourth modification example of the second embodiment. Description of embodiments[First embodiment]
[0035] Fig. 1 is a schematic cross-sectional view illustrating a power storage device 1 with a power storage module 4 according to a first embodiment. The power storage device 1 shown in Fig. 1 is used, for example, as batteries of various vehicles such as a forklift, a hybrid vehicle, and an electric vehicle. The power storage device 1 includes a module stack body 2 having a plurality of power storage modules 4 stacked together, and a restraining member 3 that applies a restraining load to the module stack body 2 in a stacking direction of the module stack body 2.
[0036] The module stack body 2 includes a plurality (three in this embodiment) of the power storage modules 4 and a plurality (four in this embodiment) of the conductive structural bodies 5. Each of the power storage modules 4 is a bipolar battery and has an approximately rectangular shape when viewed from a stacking direction. For example, the power storage module 4 is a secondary battery such as a nickel-hydrogen secondary battery and a lithium-ion secondary battery, or an electric double-layer capacitor. In the following description, the nickel-hydrogen secondary battery is exemplified as the power storage module 4.
[0037] The power storage modules 4, which are adjacent to each other in the stacking direction, are electrically connected via the conductive structural body 5. The conductive structural body 5 is arranged between the power storage modules 4, which are adjacent to each other in the stacking direction, and on an outer side of the power storage modules 4, which are respectively located at stack ends. A positive electrode terminal 6 is connected to one of the conductive structural bodies 5, which is arranged on an outer side of the power storage modules 4, which are respectively located at the stack ends. A negative electrode terminal 7 is connected to the other conductive structural body 5, which is arranged on an outer side of the other power storage module 4, which is respectively located at the stack ends.For example, the positive electrode terminal 6 and the negative electrode terminal 7 extend from edge portions of the conductive structural bodies 5 in a direction intersecting the stacking direction. Charging and discharging of the power storage device 1 are performed through the positive electrode terminal 6 and the negative electrode terminal 7. In the power storage device 1, the power storage module 4 may be arranged at one end and the other end, respectively, in the stacking direction D. That is, the outermost layer (i.e., an outermost stacked layer) of a stacked body of the power storage module 4 and the conductive structural body 5 in the power storage device 1 may be the power storage module 4. In this case, the negative electrode terminal 7 or the positive electrode terminal 6 is connected to the power storage module 4, which forms the outermost stacked layer.
[0038] A plurality of flow passages 5a through which a coolant, such as air, circulates are provided inside the conductive structural body 5. For example, the flow passages 5a extend along a direction intersecting the stacking direction and the extending direction of the positive electrode terminal 6 and the negative electrode terminal 7 (in one example, it is perpendicular to these). The conductive structural body 5 has a function as a connecting member that electrically connects the power storage modules 4 that are adjacent to each other, and a function as a heat dissipation plate for dissipating heat from the power storage module 4 by circulating a cooling fluid through the flow passages 5a. In the example shown in Fig. 1, an area of the conductive structural body 5 is smaller than an area of the power storage module 4 when viewed from the stacking direction. However, the area of the conductive structural body 5 may be equal to the area of the power storage module 4 or may be larger than the area of the power storage module 4 from the viewpoint of improving heat dissipation.
[0039] The restriction member 3 includes a pair of end plates 8 between which the module stack body 2 is arranged in the stacking direction, and a fastening bolt 9 and a nut 10 that fasten the end plates 8 together. Each of the end plates 8 is an approximately rectangular metal plate with an area slightly larger than the areas of the power storage module 4 and the conductive structural body 5 when viewed from the stacking direction. A film F having an electrical insulation property is provided on one surface of the end plates 8 on the side of the module stack body 2. Each of the end plates 8 and the conductive structural body 5 are insulated from each other by the film F.
[0040] An insertion hole 8a is provided in an edge portion of the end plate 8 at a position on a more outer side compared to the module stack body 2. The fastening bolt 9 passes from the insertion hole 8a of one of the end plates 8 to the insertion hole 8a of the other end plate 8. The nut 10 is screwed onto a tip end portion of the fastening bolt 9 protruding from the insertion hole 8a of the other end plate 8. Accordingly, the power storage module 4 and the conductive structural body 5 are sandwiched by the end plates 8 to form a unit as the module stack body 2. Moreover, a restraining force is applied to the module stack body 2 as the unit in the stacking direction.
[0041] Next, a design of the power storage module 4 is described in detail. Fig. 2 is a schematic cross-sectional view illustrating an internal configuration of the power storage module 4. As shown in Fig. 2, the power storage module 4 includes an electrode stack body 11 and a sealing body 12 formed of a resin and sealing the electrode stack body 11. The electrode stack body 11 includes a plurality of electrodes stacked via a separator 13 along the stacking direction D of the power storage module 4. The electrode stack body 11 includes a stack body S composed of a plurality of bipolar electrodes 14, a negative terminal electrode 18 disposed on one outer side of the stack body S in the stacking direction D, and a positive terminal electrode 19 disposed on the other outer side of the stack body S in the stacking direction D.
[0042] Each of the bipolar electrodes 14 includes a metal plate 15 having one surface 15a and the other surface 15b on a side opposite to the one surface 15a, a positive electrode 16 provided on the one surface 15a, and a negative electrode 17 provided on the other surface 15b. The positive electrode 16 is a positive electrode active material layer formed by coating a positive electrode active material on the metal plate 15. The negative electrode 17 is a negative electrode active material layer formed by coating a negative electrode active material on the metal plate 15. In the electrode stack body 11, the positive electrode 16 of one of the bipolar electrodes 14 faces the negative electrode 17 of the other bipolar electrode 14, which is adjacent on one side in the stacking direction D, with the separator 13 interposed therebetween.In the electrode stack body 11, the negative electrode 17 of one of the bipolar electrodes 14 faces the positive electrode 16 of another bipolar electrode 14 adjacent to the other side of the stacking direction D, with the separator 13 being arranged therebetween.
[0043] The negative terminal electrode 18 has the metal plate 15 and the negative electrode 17 provided on the other surface 15b of the metal plate 15. The negative terminal electrode 18 is arranged at one end in the stacking direction D such that the other surface 15b faces an inner side (i.e., a middle side) in the stacking direction D in the electrode stack body 11. One surface 15a of the metal plate 15 of the negative terminal electrode 18 forms an outer surface of the electrode stack body 11 in the stacking direction D and is connected to a conductive structural body 5 (see Fig. 1) which is adjacent to the power storage module 4. The negative electrode 17 provided on the other surface 15b of the metal plate 15 of the negative terminal electrode 18 faces the positive electrode 16 of the bipolar electrode at one end in the stacking direction D via the separator 13.
[0044] The positive terminal electrode 19 includes the metal plate 15 and the positive electrode 16 provided on one surface 15a of the metal plate 15. The positive terminal electrode 19 is arranged at the other end in the stacking direction D such that the one surface 15a faces an inner side in the stacking direction D in the electrode stack body 11. The positive electrode 16 provided on one surface 15a of the positive terminal electrode 19 faces the negative electrode 17 of the bipolar electrode 14 at the other end in the stacking direction D via the separator 13. The other surface 15b of the metal plate 15 of the positive terminal electrode 19 forms the other outer surface of the electrode stack body 11 in the stacking direction D and is electrically connected to the other conductive structural body 5 adjacent to the power storage module 4.
[0045] For example, the metal plate 15 is formed of a metal such as nickel and a nickel-plated steel plate. As an example, the metal plate 15 is an approximately rectangular metal foil formed of nickel. A peripheral edge portion 15c of the metal plate 15 has an approximately rectangular shape and is defined as an uncoated region that is not coated with the positive electrode active material and the negative electrode active material. Examples of the positive electrode active material constituting the positive electrode 16 include nickel hydroxide. Examples of the negative electrode active material constituting the negative electrode 17 include a hydrogen-occluding alloy. In this embodiment, a formation region of the negative electrode 17 on the other surface 15b of the metal plate 15 is slightly larger than a formation region of the positive electrode 16 on the one surface 15a of the metal plate 15.
[0046] For example, the separator is formed in a plate or sheet shape. For example, the separator 13 is a porous film made of a polyolefin-based resin such as polyethylene (PE) and polypropylene (PP). The separator 13 may be a woven fabric, a nonwoven fabric, or the like made of polypropylene, methylcellulose, or the like. The separator 13 may be reinforced with a vinylidene fluoride resin composite. The separator 13 may have a pocket shape, without limitation to the sheet shape.
[0047] For example, the sealing body 12 is formed from an insulating resin in a rectangular tubular shape as a whole. The sealing body 12 is provided on a side surface 11a of the electrode stack body 11 to surround the peripheral edge portion 15c of the metal plate 15. The sealing body 12 holds the peripheral edge portion 15c on the side surface 11a. The sealing body 12 has a plurality of first sealing portions 21 coupled to a plurality of the peripheral edge portions 15c of a plurality of the metal plates 15, and a second sealing portion 22 surrounding the first sealing portions 21 from an outer side along the side surface 11a and coupling the first sealing portions 21. For example, each of the first sealing portions 21 and the second sealing portion 22 is an alkali-resistant insulating resin.Examples of a constituent material of each of the first sealing portions 21 and the second sealing portion 22 include polypropylene (PP), polyphenylene sulfide (PPS), modified polyphenylene ether (modified PPE), and the like.
[0048] The first sealing portions 21 are provided continuously over the entire circumference of the peripheral edge portions 15c in the metal plates 15 and have a rectangular shape as viewed from the stacking direction D. For example, each of the first sealing portions 21 is a film having a predetermined thickness in the stacking direction D. An inner edge portion of the first sealing portion 21 is provided in each of the peripheral edge portion 15c on the one surface 15a of the metal plate 15 of the bipolar electrode 14, the peripheral edge portion 15c on the one surface 15a of the metal plate 15 of the negative terminal electrode 18, and the peripheral edge portion 15c on the one surface 15a and the other surface 15b of the metal plate 15 of the positive terminal electrode 19 as viewed from the stacking direction D.
[0049] For example, the inner edge portion of the first sealing portion 21 is welded to the peripheral edge portion 15c of the metal plate 15 by ultrasonic waves or heat and is hermetically coupled thereto. An outer edge portion of the first sealing portion 21 extends to an outer side compared to an outer edge of the metal plate 15 as viewed from the stacking direction D and is held by the second sealing portion 22. The first sealing portions 21, which are adjacent to each other along the stacking direction D, may be spaced from each other or may be in contact with each other.
[0050] A region where the peripheral edge portion 15c of one surface 15a in the metal plate 15 and the first sealing portion 21 overlap each other, and a region where the peripheral edge portion 15c of the other surface 15d in the metal plate 15 of the positive terminal electrode 19 and the first sealing portion 21 overlap each other are defined as a coupling region K of the metal plate 15 and the first sealing portion 21. A surface of the metal plate 15 in the coupling region K is roughened. In this embodiment, the entirety of the one surface 15a of the metal plates 15 and the entirety of the other surface 15b in the metal plate 15 of the positive terminal electrode 19 are roughened. However, only the coupling region K of one surface 15a in each of the metal plates 15 may be roughened, and only the coupling region K of the other surface 15b in the metal plate 15 of the positive terminal electrode 19 may be roughened.
[0051] For example, roughening can be realized by forming a plurality of protrusions by electrolytic plating. For example, when the one surface 15a of the metal plate 15 is roughened, a plurality of protrusions are formed on the one surface 15a at a joining interface between the one surface 15a of the metal plate 15 and the first sealing portion 21, and thus, a resin in a molten state penetrates between the plurality of protrusions. Accordingly, an anchoring effect is exhibited, and thus a coupling strength between the metal plate 15 and the first sealing portion 21 can be improved. For example, the protrusion formed at the time of roughening has a shape tapered from a base end to a tip end. Accordingly, a cross-sectional shape between adjacent protrusions becomes an undercut shape, and the anchoring effect can be increased.
[0052] The second sealing portion 22 is provided on an outer side of the electrode stack body 11 and the first sealing portion 21, and forms an outer wall (i.e., a casing) of the power storage module 4. For example, the second sealing portion 22 is formed by injection molding a resin and extends over the entire length of the electrode stack body 11 along the stacking direction D. The second sealing portion 22 has a rectangular tubular shape (i.e., an annular shape) extending with the stacking direction D set as an axial direction. For example, the second sealing portion 22 is heat-welded to outer surfaces of the first sealing portions 21 at the time of injection molding.
[0053] The first sealing portions 21 and the second sealing portion 22 form an internal space V between adjacent electrodes and seal the internal space V. Specifically, the second sealing portion 22 seals a space between the bipolar electrodes 14 adjacent to each other along the stacking direction D, a space between the negative terminal electrode 18 and the bipolar electrode 14 adjacent to each other along the stacking direction D, and a space between the positive terminal electrode 19 and the bipolar electrode 14 adjacent to each other along the stacking direction, in combination with the first sealing portions 21.Accordingly, a plurality of internal spaces V, which are hermetically separated from each other, are formed between the bipolar electrodes 14 adjacent to each other, between the negative terminal electrode 18 and the bipolar electrode 14, and between the positive terminal electrode 19 and the bipolar electrode 14, respectively. For example, an electrolytic solution (not shown) comprising an alkali solution such as an aqueous potassium hydroxide solution is stored in the internal spaces V. The electrolytic solution is impregnated in the separator 13, the positive electrode 16, and the negative electrode 17.
[0054] A thickness adjustment member 30 is arranged in the electrode stack body 11 of the power storage module 4 at a position where the first sealing portions 21 overlap as viewed from the stacking direction D. The thickness adjustment member 30 adjusts the thickness T of the electrode stack body 11 in the stacking direction D by adjusting the thickness of the thickness adjustment member 30 in the stacking direction D. In this embodiment, the "thickness of the electrode stack body 11" represents the thickness of the entirety of the electrode stack body 11 and all the first sealing portions 21 coupled to the electrode stack body 11 in the stacking direction D. The thickness adjustment member 30 is a film having a predetermined thickness in the stacking direction D and is divided into a plurality of sheets in the stacking direction D. Specifically, the thickness member 30 is divided into two parts including a thickness adjustment member 30A and a thickness adjustment member 30B.
[0055] In this embodiment, the thickness adjustment members 30A and 30B have the same configuration. Specifically, each of the thickness adjustment members 30A and 30B has the same shape (i.e., a rectangular frame shape) as the shape of the first sealing portions 21 as viewed from the stacking direction D. An outer edge and an inner edge of the thickness adjustment member 30A overlap an outer edge and an inner edge of each of the first sealing portions 21, respectively, as viewed from the stacking direction D. Similarly, an outer edge and an inner edge of the thickness adjustment member 30B overlap the outer edge and the inner edge of the first sealing portion 21, respectively, as viewed from the stacking direction D. The thickness adjustment members 30A and 30B have the same thickness.
[0056] The thickness adjustment members 30A and 30B are formed of the same material. Specifically, the thickness adjustment members 30A and 30B are formed of, for example, an alkali-resistant insulating resin, that is, the same material as that used in the first sealing portion 21. Examples of constituent materials of the thickness adjustment members 30A and 30B include polypropylene (PP), polyphenylene sulfide (PPS), modified polyphenylene ether (modified PPE), and the like.
[0057] In the electrode stack body 11, the thickness adjustment members 30A and 30B are arranged at positions different from each other in the stacking direction D. The thickness adjustment member 30A is arranged near the negative terminal electrode 18 of the electrode stack body 11 in the stacking direction D. In this embodiment, the thickness adjustment member 30A is arranged between the stack body 11 and the negative terminal electrode 18 in the stacking direction D and at the peripheral edge portion 15c of the other surface 15b (inner surface) in the metal plate 15 of the negative terminal electrode 18.Specifically, the thickness adjustment member 30A is disposed between the peripheral edge portion 15c of the other surface 15b in the metal plate 15 of the negative terminal electrode 18 and the first sealing portion 21 (hereinafter referred to as “first sealing portion 21A”) disposed on the peripheral edge portion 15c of the one surface 15a in the metal plate 15 of the bipolar electrode 14 adjacent to the negative terminal electrode 18 in the stacking direction D.
[0058] On the other hand, the thickness adjustment member 30B is arranged near the positive terminal electrode 19 of the electrode stack body 11 in the stacking direction D. In this embodiment, the thickness adjustment member 30B is arranged between the stack body 11 and the positive terminal electrode 19 in the stacking direction D, and at the first sealing portion 21 (hereinafter referred to as "first sealing portion 21B") coupled to the peripheral edge portion 15c of one surface 15a (inner surface) of the metal plate 15 of the positive terminal electrode 19. Specifically, the thickness adjustment member 30B is arranged between the first sealing portion 21B and the peripheral edge portion 15c of the other surface 15b of the metal plate 15 of the bipolar electrode 14, which is adjacent to the positive terminal electrode 19, in the stacking direction D.
[0059] Next, a configuration of the thickness adjustment member 30 will be described in detail with reference to Fig. 3 described. Fig. 3 is an enlarged view illustrating the surroundings of the thickness adjustment member 30A of the power storage module 4. In this embodiment, as described above, the thickness adjustment members 30A and 30B have the same configuration. Accordingly, in the following description, a configuration of the thickness adjustment member 30A will be described in detail as an illustration of the thickness adjustment members 30A and 30B. However, the configuration of the thickness adjustment member 30B will be described in a similar manner to the thickness adjustment member 30A.
[0060] As in Fig. 3, the thickness adjustment member 30A has one surface 30a and the other surface 30b on a side opposite to the one surface 30a. The one surface 30a faces the other surface 15b of the metal plate 15 of the negative terminal electrode 18 in the stacking direction D, and the other surface 30b faces the first sealing portion 21A in the stacking direction D. In this embodiment, the one surface 30a is in contact with the other surface 15b of the metal plate 15 of the negative terminal electrode 18, and the other surface 30b is in contact with a surface of the first sealing portion 21A in the stacking direction D. The one surface 30a is not coupled to the other surface 15b of the metal plate 15 of the negative terminal electrode 18, and the other surface 30b is not coupled to the one surface of the first sealing portion 21A.Accordingly, the thickness adjustment member 30A is not integrated with the first sealing portion 21A and is designed separately from the first sealing portion 21A.
[0061] The thickness adjustment member 30A has a thickness (i.e., a distance between one surface 30a and the other surface 30b) Ta in the stacking direction D. The thickness adjustment member 30B also has the same thickness Ta as the thickness adjustment member 30A. The thickness Ta is set in accordance with the thickness of the electrode stack body 11 before arranging the thickness adjustment members 30A and 30B. Specifically, in a measurement step before a secondary forming step described later, the thickness Ta is set in accordance with a difference between a measured value of the entire thickness of the stack body in which respective electrodes are stacked (i.e., the thickness of the electrode stack body 11 before arranging the thickness adjustment members 30A and 30B) and the standard value of the thickness of the electrode stack body 11.Specifically, the thickness Ta is set so that a total value (i.e., a value twice the thickness Ta) of the thickness Ta of each of the thickness adjustment members 30A and 30B becomes the same as the difference.
[0062] For example, if the standard value of the thickness of the electrode stack body 11 is 9 mm, and a measured value of the thickness of the electrode stack body 11 before disposing the thickness adjustment components 30A and 30B is 8.9 mm, a difference between the standard value and the measured value is 0.1 mm. In this case, if the thickness Ta is set to 0.05 mm, the sum of the thicknesses Ta of the thickness adjustment components 30A and 30B becomes 0.1 mm and becomes the same as the difference. Accordingly, if the thickness adjustment components 30A and 30B with the thickness Ta are arranged in the electrode stack body 11, the thickness T of the electrode stack body 11 after disposing the thickness adjustment components 30A and 30B can be made to be close to 9 mm, which is the standard value.
[0063] Next, an example of a method for manufacturing the power storage module 4 will be described. The method for manufacturing the power storage module 4 includes a primary molding step, a measuring step, a stacking step, a secondary molding step, and an injection step. In the primary molding step, a predetermined number of the bipolar electrodes 14, the negative terminal electrode 18, and the positive terminal electrode 19 are provided, and the first sealing portion 21 is welded to one surface 15a of the peripheral edge portion 15c of each of the metal plates 15. In addition, the first sealing portion 21 is also welded to the other surface 15b of the peripheral edge portion 15c of the metal plate 15 of the positive terminal electrode 19.
[0064] In the measuring step, the thickness of the bipolar electrodes 14, the thickness of the negative terminal electrode 18, and the thickness of the positive terminal electrode 19 are measured one by one. Here, the thickness of the bipolar electrodes 14 represents a total thickness of the bipolar electrodes 14 and the first sealing portions 21 welded to one surface 15a of the metal plates 15 of the bipolar electrodes 14. The thickness of the negative terminal electrode 18 represents the total thickness of the negative terminal electrode 18 and the first sealing portion 21 welded to one surface 15a of the metal plate 15 of the negative terminal electrode 18. The thickness of the positive terminal electrode 19 represents the total thickness of the positive terminal electrode 19 and the first sealing portions 21 welded to one surface 15a and the other surface 15b of the metal plate 15 of the positive terminal electrode 19.
[0065] Next, the thickness of the entire stacked body in which the respective electrodes are stacked is calculated from the measurement result of the thickness of the respective electrodes in the measuring step. The thickness of the stacked body corresponds to the thickness of the electrode stacked body 11 formed in the subsequent stacking step. Furthermore, a difference between the calculated thickness of the stacked body and the standard value of the thickness of the electrode stacked body 11 is calculated. Next, the thickness Ta of each of the thickness adjustment members 30A and 30B is set according to the difference. Specifically, the thickness Ta is set to a value equal to approximately half of the difference. Furthermore, the thickness adjustment members 30A and 30B having the thickness Ta set as described above are provided.
[0066] In the stacking step, the bipolar electrodes 14 are stacked over the separator 13 along the stacking direction D. Then, the thickness adjustment member 30A provided in the measuring step is arranged on the peripheral edge portion 15c of the other surface 15b in the metal plate 15 of the negative terminal electrode 18. Furthermore, the thickness adjustment member 30B provided in the measuring step is arranged on the first sealing portion 21B welded to the peripheral edge portion 15c of the one surface 15a in the metal plate 15 of the positive terminal electrode 19.Then, the negative terminal electrode 18 in which the thickness adjustment member 30A is arranged is stacked on one outer side of the stacked body S in which the bipolar electrodes 14 are stacked in the stacking direction D, and the positive terminal electrode 19 in which the thickness adjustment member 30B is arranged is stacked on the other outer side of the stacked body S in the stacking direction D. Accordingly, the electrode stacked body 11 in which the thickness adjustment members 30A and 30B are arranged is formed.
[0067] In the secondary molding step, the electrode stack body 11 formed in the stacking step is placed inside an injection mold (not shown). Next, molten resin is injected into the mold to form the second sealing portion 22 surrounding the electrode stack body 11 and the first sealing portions 21 welded to the electrode stack body 11. Accordingly, the sealing body 12 is formed on the side surface 11a of the electrode stack body 11. In the injection step, an electrolytic solution is injected into the internal space V between the bipolar electrodes 14 after the secondary molding step. Thus, the power storage module 4 is obtained.
[0068] Next, an operating effect of the power storage module 4 will be described. In the power storage module 4 of this embodiment, as described above, the thickness adjustment members 30A and 30B that adjust the thickness T of the electrode stack body 11 are arranged. Since the thickness T of the electrode stack body 11 is adjusted by the thickness adjustment members 30A and 30B, when the second sealing portion 22 is formed, the thickness T of the electrode stack body 11 can be easily set within the standard. Moreover, since the thickness adjustment members 30A and 30B are arranged at positions where the first sealing portions 21 overlap, as viewed from the stacking direction D, even after the thickness adjustment members 30A and 30B are arranged, a shape of the entirety of the electrode stack body 11 including that of the first sealing portions 21 can be maintained.Accordingly, the occurrence of a molding failure of the second sealing portion 22 can be suppressed, and the occurrence of a sealing failure of the electrode stack body 11 can be suppressed. Furthermore, since the thickness adjustment members 30A and 30B are arranged at positions where the first sealing portions 21 overlap as viewed from the stacking direction D, the thickness adjustment members 30A and 30B and the first sealing portions can be set to the same shape as viewed from the stacking direction D. As a result, when the thickness adjustment members 30A and 30B and the first sealing portions 21 are formed by punching, punching dies of the thickness adjustment members 30A and 30B and the first sealing portions 21 can be made common to each other.
[0069] In the power storage module 4, the thickness adjustment members 30A and 30B are formed of the same material as the first sealing portions 21. Accordingly, since the material of the thickness adjustment members 30A and 30B and the material of the first sealing portions 21 can be made common to each other, simplification of the design of the power storage module 4 is realized.
[0070] In the power storage module 4, the thickness adjustment members 30A and 30B are arranged between the stacked body S and the negative terminal electrode 18 and between the stacked body S and the positive terminal electrode 19, respectively, in the stacking direction D. In this case, since the thickness adjustment members 30A and 30B can be arranged when the negative terminal electrode 18 and the positive terminal electrode 19 are stacked on the stacked body S of the bipolar electrodes 14, arrangement of the thickness adjustment members 30A and 30B on the electrode stacked body 11 becomes easy. In this embodiment, the thickness and the number of sheets of the thickness adjustment member 30A are equal to the thickness and the number of sheets of the thickness adjustment member 30B.However, the thickness T of the electrode stack body 11 can be finely adjusted by adjusting the thickness and the number of sheets of the thickness adjusting member 30A arranged between the stack body S and the negative terminal electrode 18 and the thickness and the number of sheets of the thickness adjusting member 30B arranged between the stack body S and the positive terminal electrode 19.
[0071] In the power storage module 4, the thickness adjustment member 30A, which is arranged between the stacked body S and the negative terminal electrode 18, is arranged at the peripheral edge portion 15c of the other surface 15b in the metal plate 15 of the negative terminal electrode 18. The thickness adjustment member 30B, which is arranged between the stacked body S and the positive terminal electrode 19, is arranged at the first sealing portion 21B, which is coupled to the peripheral edge portion 15c of the one surface 15a in the metal plate 15 of the positive terminal electrode 19. In this case, since each of the thickness adjustment members 30A and 30B is arranged between the first sealing portions 21, which are adjacent to each other, the occurrence of positional deviation between each of the thickness adjustment members 30A and 30B and the first sealing portions 21 can be suppressed.
[0072] In the power storage module 4, the thickness Ta of the thickness adjustment member 30A disposed between the stack body S and the negative terminal electrode 18 and the thickness Ta of the thickness adjustment member 30B disposed between the stack body S and the positive terminal electrode 19 are equal to each other. In this case, fine adjustment of the thickness T of the electrode stack body 11 and simplification of the design of the power storage module 4 can be made compatible with each other. Furthermore, the internal space close to the negative terminal electrode 18 of the electrode stack body 11 and the internal space close to the positive terminal electrode 19 of the electrode stack body 11 can be made equal.As a result, a change in the internal space between respective electrodes in the electrode stack body 11 can be suppressed to the minimum, and a deviation of a state of charge (SOC) between the respective electrodes can be reduced.
[0073] The first embodiment of the present invention has been described above, but the present invention is not limited to the first embodiment, and various modifications may be made. For example, various modification aspects described in Fig. 4 and Fig. 5 are used.
[0074] Fig. 4 is a schematic cross-sectional view illustrating an internal configuration of a power storage module 4A according to a first modification example of the first embodiment. A difference between this modification example and the first embodiment is a configuration of the thickness adjustment member. That is, in the first embodiment, the thickness adjustment member 30 is divided into the thickness adjustment members 30A and 30B in the stacking direction D. However, in this modification example, a thickness adjustment member 30C is not divided in the stacking direction D and is integrally formed (i.e., one sheet of film). In this case, the thickness adjustment member 30C is disposed at an arbitrary position between the stacked body S and the negative terminal electrode 18 and between the stacked body S and the positive terminal electrode 19.
[0075] In this modification example, the thickness adjustment member 30C is disposed between the stacked body S and the positive terminal electrode 19. Specifically, the thickness adjustment member 30C is disposed at the first sealing portion 21B, which is coupled to the peripheral edge portion 15c of one surface 15a (inner surface) in the metal plate 15 of the positive terminal electrode 19. Specifically, the thickness adjustment member 30C is disposed between the first sealing portion 21B and the peripheral edge portion 15c of the other surface 15b of the metal plate 15 of the bipolar electrode 14, which is adjacent to the positive terminal electrode 19, in the stacking direction D.
[0076] The thickness adjustment member 30C has the same configuration as the thickness adjustment members 30A and 30B, except that the thickness Tb of the thickness adjustment member 30C differs from the thickness Ta of each of the thickness adjustment members 30A and 30B. The thickness Tb of the thickness adjustment member 30C is greater than the thickness Ta of each of the thickness adjustment members 30A and 30B and is equal to a total value of the thicknesses Ta. Accordingly, the thickness Tb is set to be equal to the difference between the measured value of the thickness of the entire stacked body in which the respective electrodes are stacked in the measuring step and the standard value of the thickness of the electrode stacked body 11A.
[0077] In this modification example, since the thickness adjustment member 30C is disposed only between the stacked body S and the positive terminal electrode 19, the thickness T of the electrode stacked body 11A can be adjusted while avoiding an increase in the number of parts compared to the case where the thickness adjustment members are disposed between the stacked body S and the negative terminal electrode 18 and between the stacked body S and the positive terminal electrode 19, respectively. Moreover, the thickness adjustment member 30C is disposed on the first sealing portion 21B, which is coupled to the peripheral edge portion 15c of the one surface 15a in the metal plate 15 of the positive terminal electrode 19.In this case, since the thickness adjustment member 30C is sandwiched between the first sealing portions 21 adjacent to each other, occurrence of positional deviation between the first sealing portions 21 and the thickness adjustment member 30C can be suppressed.
[0078] In this modification example, a case has been described where the thickness adjustment member 30C is disposed only between the stacked body S and the positive terminal electrode 19. However, the thickness adjustment member 30C may be disposed only between the stacked body S and the negative terminal electrode 18. In this case, for example, the thickness adjustment member 30C is disposed on the peripheral edge portion 15c of the other surface 15b (inner surface) in the metal plate 15 of the negative terminal electrode 18. Specifically, the thickness adjustment member 30C is disposed between the other surface 15b of the peripheral edge portion 15c in the metal plate 15 of the negative terminal electrode 18 and the first sealing portion 21A connected to the peripheral edge portion 15c of the one surface 15a in the metal plate 15 of the bipolar electrode 14 adjacent to the negative terminal electrode 18 in the stacking direction D.In this way, even if the thickness adjustment member 30C is arranged only between the stack body S and the negative terminal electrode 18, it is possible to obtain the same effect as when the thickness adjustment member 30C is arranged only between the stack body S and the positive terminal electrode 19.
[0079] Fig. 5 is a schematic cross-sectional view illustrating an internal configuration of a power storage module 4B according to a second modification example of the first embodiment. A difference between this modification example and the first embodiment is a configuration of the electrode stack body. That is, in this modification example, in an electrode stack body 11B, an outermost metal plate 40 is further stacked on an outer side of the negative terminal electrode 18 in the stacking direction D. The outermost metal plate 40 is formed by the same material as the material of the metal plate 15 of the bipolar electrode 14. The positive electrode active material and the negative electrode active material are not coated on one surface 40a and the other surface 40b of the outermost metal plate 40, and an entire area of the one surface 40a and the other surface 40b is set as an uncoated region.In this embodiment, the one surface 40a forms an outer surface of the electrode stack body 11B in the stacking direction D.
[0080] A peripheral edge portion 40c of the other surface 40b of the outermost metal plate 40 is welded to the first sealing portion 21 welded in the peripheral edge portion 15c of the metal plate 15 of the negative terminal electrode 18, for example, by ultrasonic waves or heat, and is hermetically coupled thereto. As with the bipolar electrodes 14 and the negative terminal electrode 18, the first sealing portion 21 (hereinafter referred to as "first sealing portion 21C") is provided in the peripheral edge portion 40c of one surface 40a of the outermost metal plate 40. An inner edge portion of the first sealing portion 21C overlaps the peripheral edge portion 40c of the one surface 40a of the outermost metal plate 40 as viewed from the stacking direction D and is welded to the peripheral edge portion 40c, for example, by ultrasonic waves or heat, and is hermetically coupled thereto.A central portion 40d of the outermost metal plate 40 is in contact with the one surface 15a of the metal plate 15 of the negative terminal electrode 18 in a state of being recessed from the negative terminal electrode 18 by a constraining force applied to an inner side of the stacking direction D when the module stacked body 2 is constrained by the constraining member 3. Due to the contact, the metal plate 15 of the negative terminal electrode 18 and the conductive structural body 5 adjacent to the power storage module 4B are electrically connected through the outermost metal plate 40.
[0081] At the peripheral edge portion 40c of the outermost metal plate 40, a region where one surface 40a and the first sealing portion 21C overlap each other, and a region where the other surface 40b and the first sealing portion 21C provided in the peripheral edge portion 15c of the metal plate 15 of the negative terminal electrode 18 overlap each other are defined as a coupling region K between the outermost metal plate 40 and the first sealing portion 21. In the electrode stack body 11B, an excess space VA in which the electrolytic solution is not stored is formed between the outermost metal plate 40 and the negative terminal electrode 18.The excess space VA is surrounded by one surface 15a of the metal plate 15 of the negative terminal electrode 18, the other surface 40b of the outermost metal plate 40, and the first sealing portion 21 coupled to the peripheral edge portion 15c of the one surface 15a in the metal plate 15 of the negative terminal electrode 18.
[0082] There is a concern that the alkaline electrolytic solution stored in the internal space V may pass through a region between the metal plate 15 of the negative terminal electrode 18 and the first sealing portion 21 coupled to the metal plate 15 due to a so-called alkali creep phenomenon and leak to the outside of the power storage module 4B. Here, in this modification example, since the outermost metal plate 40 is arranged on an outer side of the metal plate 15 of the negative terminal electrode 18 in the stacking direction D, the excess space VA is formed on a movement route of the alkaline electrolytic solution.By forming the excess space VA, it is possible to suppress the intrusion of moisture contained in the outside air into a gap between the metal plate 15 of the negative terminal electrode 18 and the first sealing portion 21 coupled to the metal plate 15, which is a starting point for leakage of the alkaline electrolytic solution. As a result, it is possible to suppress the influence of external moisture, which becomes an accelerating condition for the alkali creep phenomenon, and to suppress the leakage of the alkaline electrolytic solution to the outside of the power storage module 4B.
[0083] In the present invention, various other modifications can be made. For example, the first embodiment and the respective modification examples can be combined in accordance with a necessary object and a necessary effect. Furthermore, the configuration and arrangement aspect of the thickness adjustment member can be appropriately changed. For example, the thickness adjustment member may have a shape different from the shape of the first sealing portion 21 when viewed from the stacking direction D, or may be formed of a material different from the material of the first sealing portion 21.The thickness adjustment member between the stacked body S and the negative terminal electrode 18 may be disposed at the first sealing portion 21 coupled to the peripheral edge portion 15c of one surface 15a (i.e., an outer surface) in the metal plate 15 of the negative terminal electrode 18. The thickness adjustment member between the stacked body S and the positive terminal electrode 19 may be disposed at the first sealing portion 21 coupled to the peripheral edge portion 15c of the other surface 15b (i.e., an outer surface) in the metal plate 15 of the positive terminal electrode 19.
[0084] Furthermore, in the first embodiment, the thickness adjustment members 30A and 30B have the same configuration. However, the thickness adjustment members 30A and 30B may have configurations that differ from each other. For example, the thickness adjustment members 30A and 30B may be formed of different materials or may have different shapes. For example, the thickness adjustment members 30A and 30B may have different thicknesses or may have different shapes from each other when viewed from the stacking direction. In the measuring step of the first embodiment, the thickness of the bipolar electrodes 14, the thickness of the negative terminal electrode 18, and the thickness of the positive terminal electrode 19 are measured one after another.However, the thickness of the bipolar electrodes 14, the thickness of the negative terminal electrode 18, and the thickness of the positive terminal electrode 19 may be measured at a time in a state where they are actually stacked. [Second embodiment]
[0085] Next, a power storage module 400 according to a second embodiment will be described with reference to Fig. 6. The second embodiment differs from the first embodiment in that outermost metal plates (conductive plates) 40 and 50 are arranged on an outer side of the positive terminal electrode 19 in the stacking direction D and an outer side of the negative terminal electrode 18 in the stacking direction D, respectively, and a thickness adjusting member 30 is located between the negative terminal electrode 18 and the outermost metal plate 50 in the stacking direction D. In the following second embodiment, description of portions redundant with the first embodiment will be appropriately omitted. Accordingly, portions different from the first embodiment will be mainly described below.
[0086] Fig. 6 is a schematic cross-sectional view illustrating an internal configuration of the power storage module 400 according to the second embodiment. As shown in Fig. As shown in Fig. 6, the power storage module 400 includes an electrode stack body 11, the thickness adjustment member 30 located on the electrode stack body 11, and a sealing body 12 that integrates the electrode stack body 11 and the thickness adjustment member 30. Although not shown, an electrolytic solution is stored in the power storage module 400 (details of which will be described later).
[0087] The electrode stack body 11 has a stack body S with bipolar electrodes 14 and separators 13 that are alternately stacked along a stacking direction D, the negative terminal electrode 18 located at one end of the stack body S in the stacking direction D, and the positive terminal electrode 19 located at the other end of the stack body S in the stacking direction D. That is, a pair of terminal electrodes is located on an outer side of the stack body S in the stacking direction D. In Fig. 6, the stacked body S has the bipolar electrodes 14 and the separators 13 located within a region indicated by a dashed line. Furthermore, the electrode stacked body 11 further includes the outermost metal plate 40 located on an outer side of the positive terminal electrode 19 in the stacking direction D, and the outermost metal plate 50 located on an outer side of the negative terminal electrode 18 in the stacking direction D.
[0088] The bipolar electrodes 14 and the separators 13 included in the stacked body S are stacked along the stacking direction D and have, for example, a rectangular shape in a plan view (i.e., as viewed from the stacking direction D). Each of the separators 13 is arranged between the bipolar electrodes 14 that are adjacent to each other. Each of the bipolar electrodes 14 includes the metal plate 15 having one surface 15a and the other surface 15b on a side opposite to the one surface 15a, a positive electrode 16 provided on the one surface 15a, and a negative electrode 17 provided on the other surface 15b.
[0089] The metal plate 15 is a conductive body (current collector) having a plate shape extending in a horizontal direction intersecting or perpendicular to the stacking direction D, and has flexibility. Accordingly, the horizontal direction can be referred to as an extending direction of the metal plate 15. For example, the metal plate 15 is a nickel foil, a steel plate subjected to plating, or a stainless steel plate subjected to plating. Examples of the steel plate include a cold-rolled steel plate (SPCC or the like) defined in JIS G3141:2005. Examples of the stainless steel plate include SUS304, SUS316, SUS316L, and the like defined in JIS G4305:2015. For example, the thickness of the metal plate 15 is 0.1 μm to 1000 μm. When the metal plate 15 is the nickel foil, the nickel foil may be subjected to plating.
[0090] Next, a configuration of the outermost metal plates 40 and 50 will be described. The outermost metal plate 40 is a plate-shaped member provided for suppressing deterioration of the electrode stack body 11, and has conductivity and flexibility. Each of the one surface 40a and the other surface 40b of the outermost metal plate 40 is not coated with the positive electrode active material and the negative electrode active material. Accordingly, all surfaces of the one surface 40a and the other surface 40b are defined as uncoated regions. That is, the outermost metal plate 40 is an uncoated sheet in which an active material layer is not formed. The one surface 40a is a surface facing the conductive structural body 5 in the stacking direction D.The other surface 40b is a surface located on a side opposite to the one surface 40a and facing the electrode stack body 11 in the stacking direction D. In this embodiment, the outermost metal plate 40 is located on an outer side of the positive terminal electrode 19 in the stacking direction D. Accordingly, the other surface 40b faces the positive terminal electrode 19. The outermost metal plate 40 is stacked in combination with other electrodes along the stacking direction D. Accordingly, the positive terminal electrode 19 is arranged between the outermost metal plate 40 and the bipolar electrode 14 along the stacking direction D. In other words, in the power storage module 400, the outermost metal plate 40 is provided on a more outer side of the positive terminal electrode 19.
[0091] The outermost metal plate 40 has a central portion 41 in contact with the conductive structural body 5 and a rectangular annular peripheral edge portion 42 surrounding the central portion 41 in a plan view. The central portion 41 and the peripheral edge portion 42 are continuous from each other. The central portion 41 of the outermost metal plate 40 is recessed toward the center of the electrode stack body 11 and is pressed against the positive terminal electrode 19 due to the restraining force of the restraining member 3 applied to the electrode stack body 11 via the conductive structural body 5. Accordingly, the central portion 41 becomes a contact portion in contact with the positive terminal electrode 19, and the outermost metal plate 40 can function as a positive electrode terminal in the power storage module 400.On the other hand, the peripheral edge portion 42 is a portion spaced apart from the positive terminal electrode 19. One part 42a of the peripheral edge portion 42 is a portion held by the seal body 12 and the thickness adjustment member 30, and is located on an outer side of the electrode stack body 11 compared to the central portion 41 in the stacking direction D. The other portion 42b of the peripheral edge portion 42 is a portion connecting the part 42a and the central portion 41, and is located closer to the center of the outermost metal plate 40 in the horizontal direction than the seal body 12.
[0092] The outermost metal plate 50 is an uncoated foil that has the same function as the outermost metal plate 40. One surface 50a of the outermost metal plate 50 is a surface facing the conductive structural body 5 in the stacking direction D. The other surface 50b is a surface located on a side opposite to the one surface 50a and facing the electrode stack body 11 in the stacking direction D. In this embodiment, the outermost metal plate 50 is located on an outer side of the negative terminal electrode 18 in the stacking direction D. Accordingly, the other surface 50b faces the negative terminal electrode 18. The outermost metal plate 50 is stacked in combination with other electrodes along the stacking direction D. Accordingly, the negative terminal electrode 18 is arranged between the outermost metal plate 50 and the bipolar electrode 14 along the stacking direction D.In other words, in the power storage module 400, the outermost metal plate 50 is provided on a more outer side of the negative terminal electrode 18.
[0093] The outermost metal plate 50 has a central portion 51 in contact with the conductive structural body 5, and a peripheral edge portion 52 surrounding the central portion 51 in a plan view. The central portion 51 and the peripheral edge portion 52 are continuous from each other. As in the outermost metal plate 40, the central portion 51 of the outermost metal plate 50 is recessed toward the center of the electrode stack body 11 and is pressed against the negative terminal electrode 18. Accordingly, the central portion 51 becomes a contact portion in contact with the negative terminal electrode 18, and the outermost metal plate 50 can function as a negative electrode terminal in the power storage module 400.A part 52a of the peripheral edge portion 52 is a portion held by the seal body 12 and is located on an outer side of the electrode stack body 11 compared to the central portion 51 in the stacking direction D. The other portion 52b of the peripheral edge portion 52 is a portion connecting the part 52a and the central portion 51.
[0094] As in the metal plate 15, for example, each of the outermost metal plates 40 and 50 is a nickel foil, a steel plate subjected to plating, or a stainless steel plate subjected to plating. From the viewpoint of corrosion resistance, for example, each of the outermost metal plates 40 and 50 may be the nickel foil or the stainless steel plate subjected to plating. Furthermore, from the viewpoint of cost, each of the outermost metal plates 40 and 50 may be SUS316 or 316L subjected to plating. In this case, for example, a nickel-plated layer (not shown) functioning as a surface protection layer is formed in each of the outermost metal plates 40 and 50. For example, the thickness of the nickel-plated layer is 1 μm to 10 μm. The nickel-plated layer may have a single-layer structure or a multi-layer structure.For example, the nickel-plated layer may have a nickel-plated base layer and a nickel-plated main layer. In the following description, the thickness T11 represents the thickness (see ). Fig. 7, which will be described later) of the outermost metal plate 40 along the stacking direction D represents the thickness of the entirety of the outermost metal plate 40 and a first sealing portion 21, which will be described later. That is, the thickness T11 of the outermost metal plate 40 represents the thickness of the entirety of the outermost metal plate 40 before deformation, and of the first sealing portion 21 coupled to the outermost metal plate 40. Accordingly, for example, the thickness of the outermost metal plate 40 is 0.1 μm to 1000 μm, but the thickness T11 of the outermost metal plate 40 is not limited to this range. The thickness of the outermost metal plate 50 is defined as the thickness T11 of the outermost metal plate 40.
[0095] The sealing body 12 is provided to surround the peripheral edge portion 15c of the metal plate 15, the part 42a of the peripheral edge portion 42 of the outermost metal plate 40, the part 52a of the peripheral edge portion 52 of the outermost metal plate 50, and the thickness adjustment member 30. For example, the sealing body 12 is formed of an insulating resin and has a rectangular tubular shape as a whole. For example, the insulating resin is a thermoplastic resin that has alkali resistance. Examples of the thermoplastic resin include PP, polyphenylene sulfide (PPS), modified polyphenylene ether (modified PPE), and the like.The seal body 12 has a plurality of first seal portions coupled to a plurality of the peripheral edge portions 15c of a plurality of the metal plates 15, the part 42a of the outermost metal plate 40, and the part 52a of the outermost metal plate 50, and a second seal portion 22 disposed on the periphery of the first seal portions 21.
[0096] The first sealing portions 21 are resin members coupled to edge portions of the bipolar electrodes 14, the negative terminal electrode 18, the positive terminal electrode 19, and the outermost metal plates 40 and 50. Specifically, the first sealing portions 21 are rectangular frames coupled to the peripheral edge portion 42 of the outermost metal plate 40, the peripheral edge portion 52 of the outermost metal plate 50, and the peripheral edge portions 15c of the metal plates 15 included in the bipolar electrodes 14, the negative terminal electrode 18, and the positive terminal electrode 19. The first sealing portions 21 are continuously provided over the entire circumference of the respective peripheral edge portions 15c or the peripheral edge portions 42 and 52. Accordingly, the first sealing portion 21 has a rectangular frame shape when viewed from the stacking direction D.For example, each of the first sealing portions 21 is a resin film having a predetermined thickness in the stacking direction D. The first sealing portion 21 may be formed by punching a resin sheet, may be formed by arranging a plurality of resin sheets in a frame shape, or may be formed by injection molding using a mold. In this embodiment, the first sealing portion 21 is formed by punching a resin sheet. For example, the thickness of the first sealing portion 21 is 50 μm to 250 μm.
[0097] For example, an inner portion of the first sealing portion 21, in a plan view, is welded to each of the peripheral edge portions 15c or the peripheral edge portions 42 and 52 by ultrasonic waves or heat. In this embodiment, the inner portion is welded to one surface 15a of the peripheral edge portions 15c in the bipolar electrodes 14, one surface 15a of the peripheral edge portion 15c in the negative terminal electrode 18, one surface 15a of the peripheral edge portion 15c in the positive terminal electrode 19, one surface 40a of the peripheral edge portion 42 in the outermost metal plate 40, and one surface 50a of the peripheral edge portion 52 in the outermost metal plate 50. Each of the metal plates 15 and each of the first sealing portions 21 is airtightly coupled. Similarly, each of the outermost metal plates 40 and 50 and the first sealing portion 21 are hermetically coupled.
[0098] An outer portion of the first sealing portion 21 in a plan view is located on an outer side relative to the metal plate 15 in the horizontal direction. At least a part of the outer portion is held by the second sealing portion 22. The first sealing portions 21, which are adjacent to each other along the stacking direction D, may be spaced apart from each other or may be in contact with each other. When the first sealing portions 21, which are adjacent to each other, are in contact with each other, the first sealing portions 21 may be welded together in a liquid-tight and airtight manner.
[0099] In the following description, a region where the metal plate 15 or the outermost metal plate 40 and the first sealing portion 21 are coupled to each other in the stacking direction D is defined as a coupling region K. In each of the metal plates 15 and the outermost metal plate 40, a surface included at least in the coupling region K is roughened. In this embodiment, the entirety of the one surface 15a of the metal plates 15 included in the bipolar electrodes 14 and the negative terminal electrode 18, the entirety of the metal plate 15 included in the positive terminal electrode 19, and the entirety of the one surface 40a of the outermost metal plate 40 are roughened.
[0100] The second sealing portion 22 is a member that forms an outer wall (i.e., a casing) of the power storage module 400 and covers outer surfaces (at least side surfaces) of the first sealing portions 21. For example, the second sealing portion 22 is formed by injection molding a resin and extends over the entire length of the electrode stack body 11 along the stacking direction D. Moreover, the second sealing portion 22 extends to the first sealing portion 21, which is coupled to the outermost metal plate 40, beyond the electrode stack body 11 in the stacking direction D. The second sealing portion 22 has a rectangular tubular shape (i.e., an annular shape) that extends with the stacking direction D defined as an axial direction. For example, the second sealing portion 22 is heat-welded to outer surfaces of the first sealing portions 21 at the time of injection molding.Accordingly, the second sealing portion 22 couples the first sealing portions 21.
[0101] The first sealing portions 21 and the second sealing portion 22 form an internal space V inside the electrode stack body 11 and seal the internal space V. Specifically, the second sealing portion 22 seals a space between the bipolar electrodes 14 adjacent to each other along the stacking direction D, a space between the negative terminal electrode 18 and the bipolar electrode 14 adjacent to each other along the stacking direction D, and a space between the positive terminal electrode 19 and the bipolar electrode 14 adjacent to each other along the stacking direction D, in combination with the first sealing portions 21. Accordingly, the internal space V is formed by the electrode stack body 11 and the sealing body 12.Specifically, a plurality of airtightly separated inner spaces V are formed between the bipolar electrodes 14 adjacent to each other, between the negative terminal electrode 18 and the bipolar electrode 14, and between the positive terminal electrode 19 and the bipolar electrode 14. For example, an aqueous solution-based electrolytic solution (an alkaline electrolytic solution such as an aqueous potassium hydroxide solution, an aqueous lithium hydroxide solution, and a mixed solution of these as a specific example) is stored in the inner spaces V. The electrolytic solution is stored in the inner space V through a communication hole (not shown) provided in the first sealing portions 21. The electrolytic solution may be impregnated in the separator 13, the positive electrode 16, and the negative electrode 17.The connection hole is sealed, for example, with a pressure-adjusting valve after the electrolytic solution is injected. Note that when described as "a volume of an internal space," the description represents a volume including the cavities of the separator 13.
[0102] Here, the peripheral edge portion 52 of the outermost metal plate 50 is also welded to the first sealing portion 21 coupled to the negative terminal electrode 18. Accordingly, an excess space EV1 (first excess space) is formed by the negative terminal electrode 18 (specifically, the metal plate 15 of the negative terminal electrode 18), the first sealing portion 21 coupled to the negative terminal electrode 18, and the outermost metal plate 50. In other words, since the first sealing portion 21 coupled to the negative terminal electrode 18 is also coupled to the outermost metal plate 50, the excess space EV1 is formed. Since the central portion 51 of the outermost metal plate 50 is formed toward the negative terminal electrode 18, the excess space EV1 is restricted to be narrow.
[0103] The excess space EV1 is formed to surround the periphery of the outermost metal plate 50. Viewed from a cross section along the stacking direction D, the excess space EV1 has an approximately triangular shape whose height (i.e., a dimension along the stacking direction D) decreases as it extends from the first sealing portion 21 to the middle portion 51. In this embodiment, the other surface 50b of the outermost metal plate 50 is welded to the first sealing portion 21, which is coupled to the negative terminal electrode 18, to ensure airtightness of the excess space EV1. In addition, the power storage module 400 has another excess space EV2 (a second excess space) in which the electrolytic solution is not stored.The excess space EV2 is formed by the negative terminal electrode 18 (specifically, the metal plate 15 of the negative terminal electrode 18), the first sealing portion 21 coupled to the negative terminal electrode 18, the first sealing portion 21 coupled to the bipolar electrode 14, and the second sealing portion 22. The excess space EV2 is formed to surround an edge of the metal plate 15 of the negative terminal electrode 18. Viewed from a cross section along the stacking direction D, the excess space EV2 has an approximately rectangular frame shape.
[0104] Next, a configuration of the thickness adjustment member 30 will be described. The thickness adjustment member 30 is a resin member for adjusting the thickness of the electrode stack body 11 in the stacking direction D. In this embodiment, the thickness adjustment member 30 is located between the positive terminal electrode 19 and the outermost metal plate 40, and at a position overlapping the first sealing portion 21 in the stacking direction D. Specifically, the thickness adjustment member 30 is located between the positive terminal electrode 19 and the first sealing portion 21 coupled to the positive terminal electrode 19 and the part 42a of the peripheral edge portion 42 of the outermost metal plate 40, and the first sealing portion 21 coupled to the outermost metal plate 40.Furthermore, the thickness adjustment member 30 is in contact with the positive terminal electrode 19, the part 42a of the outermost metal plate 40, and the first sealing portion 21 coupled to the outermost metal plate 40. The thickness adjustment member 30 may be welded to at least one of the metal plate 15 of the positive terminal electrode 19 and the outermost metal plate 40.
[0105] For example, the thickness adjustment member 30 has a rectangular frame shape in a plan view. In this embodiment, the shape of the thickness adjustment member 30 in a plan view is the same as or substantially the same as the shape of the first sealing portion 21 in a plan view. Moreover, in this embodiment, the thickness adjustment member 30 is arranged to overlap the first sealing portion 21 in the stacking direction D. Specifically, an outer edge of the thickness adjustment member 30 and an outer edge of the first sealing portion 21 are aligned with each other, and an inner edge of the thickness adjustment member 30 and an inner edge of the first sealing portion 21 are aligned with each other. The thickness adjustment member 30 is formed by an insulating resin as in the sealing body 12. For example, the insulating resin is a thermoplastic resin having alkali resistance.Examples of the thermoplastic resin include PP, PPS, modified PPE, and the like. The resin constituting the thickness adjustment member 30 and the resin constituting the seal body 12 may be the same or may be different from each other. In this embodiment, the thickness adjustment member 30 is formed by the same material as the first seal portion 21. As with the first seal portion 21, the thickness adjustment member 30 may be formed by punching a resin sheet or may be formed by injection molding using a die. In this embodiment, the thickness adjustment member 30 is formed by punching the resin sheet. In this case, a die for forming the thickness adjustment member 30 and a die for forming the first seal portion 21 may be made common to each other.Accordingly, a plan view shape of the thickness adjustment member 30 and a plan view shape of the first seal portion 21 are satisfactorily matched. Furthermore, since the number of dies can be reduced, a reduction in cost is also realized.
[0106] Here, a detailed design of the thickness adjustment member 30 is described with reference to Fig. 7 described. Fig. 7 is an enlarged view of a main area in Fig. 6. As in Fig. As shown in Fig. 7, the thickness adjustment member 30 includes one surface 30a and the other surface 30b located on a side opposite to the one surface 30a in the stacking direction D. The one surface 30a is in contact with the positive terminal electrode 19. The other surface 30b is in contact with the part 42a of the peripheral edge portion 42 of the outermost metal plate 40 and the first sealing portion 21 coupled to the outermost metal plate 40. The one surface 30a is not coupled to the outermost metal plate 40. An inner portion of the thickness adjustment member 30 is in contact with the positive terminal electrode 19 and the outermost metal plate 40, and an outer portion of the thickness adjustment member 30 is in contact with the first sealing portion 21 coupled to the outermost metal plate 40.The outer portion may be in contact with the first sealing portion 21, which is coupled to the positive terminal electrode 19. In this embodiment, the thickness adjustment member 30 is configured separately from the first sealing portion 21. That is, the thickness adjustment member 30 and the first sealing portion 21 are not integrated. However, the thickness adjustment member 30 and the first sealing portion 21 may be joined together.
[0107] The thickness Ta of the thickness adjustment member 30 along the stacking direction D (that is, a distance between one surface 30a and the other surface 30b along the stacking direction D) is in accordance with the thickness TA of a stacked body SA (see Fig. 6) along the stacking direction D. Here, the stacked body SA represents the electrode stacked body 11 before stacking the outermost metal plates 40 and 50, that is, the stacked body S in which the negative terminal electrode 18 and the positive terminal electrode 19 are stacked. For example, the thickness Ta is set in accordance with a difference between a measured value of the thickness TA of the stacked body SA and a standard value (i.e., a standard thickness) of the thickness of the stacked body SA. For example, the standard thickness of the stacked body SA is within a range including an error of approximately ±0.2 mm (or approximately ±0.1 mm) from an ideal thickness of the stacked body SA, and is determined in advance.For example, if the standard thickness of the stacked body SA is 9 mm and an actual measured value of the thickness TA of the stacked body SA before disposing the thickness adjustment component 30 is 8.9 mm, a difference between the standard thickness and the actual measured value is 0.1 mm. In this case, the difference can be removed by using the thickness adjustment component 30 with a thickness of 0.1 mm. The thickness TA of the stacked body SA represents the thickness of the entirety of components, including the first sealing portions 21 coupled to the bipolar electrodes 14, rather than a total thickness of only the separators 13 and the bipolar electrodes 14 that are stacked. In this way, the thickness T of the electrode stack body 11 including the outermost metal plates 40 and 50 can be adjusted by arranging the thickness adjusting member 30 according to the difference between the thickness TA of the stack body SA and the standard thickness of the stack body SA.
[0108] The thickness TA of the thickness adjustment member 30 may correspond to a difference between a total value obtained by adding the thickness T11 of the outermost metal plate 40 to the thickness TA of the stacked body SA and a total standard value obtained by adding the standard thickness of the outermost metal plate 40 to the standard thickness of the stacked body SA. In the total values, the thickness TA of the stacked body SA and the thickness T11 of the outermost metal plate 40 are actually measured values. As a definition of the thickness T11 of the outermost metal plate 40, the standard thickness of the outermost metal plate 40 along the stacking direction D represents a standard thickness in the entirety of the outermost metal plate 40 and the first sealing portion 21 coupled to the outermost metal plate 40.For example, the standard thickness of the outermost metal plate 40 is within a range that includes an error of approximately ±50 μm from an ideal thickness of the outermost metal plate 40. For example, if a total standard value of the stacked body SA and the outermost metal plate 40 is 10 mm, and a total value of the thickness TA of the stacked body SA and the thickness T11 of the outermost metal plate 40 is 9.8 mm, a difference between the total standard value and the total value is 0.2 mm. In this case, the difference can be removed by using the thickness adjustment member 30 with a thickness of 0.2 mm. Alternatively, for example, the difference can be reduced by using the thickness adjustment member 30 with a thickness of 0.15 mm.
[0109] The thickness TA of the stacked body SA and the thickness T11 of the outermost metal plate 40 can vary. The thickness adjustment member 30 may include a plurality of layered members stacked along the stacking direction D to accommodate the variation. In this case, the thickness of the thickness adjustment member 30 can be changed in multiple stages by adjusting the number of layered members. For example, the thickness of the layered members is 10 μm to 150 μm. In this case, breakage of the layered member can be satisfactorily suppressed and can satisfy the variation. The thicknesses of the layered members may be equal to each other or may be different from each other.When the thicknesses of the layered components are different from each other, the thickness of the thickness adjustment component 30 can be changed in further several stages by a combination of the layered components.
[0110] In this embodiment, the stacked body SA and the outermost metal plates 40 and 50 overlap each other in the stacking direction D. Accordingly, the thickness Ta of the thickness adjustment member 30 may correspond to a difference between a total value obtained by adding the thickness T11 of the outermost metal plate 40 and the thickness of the outermost metal plate 50 to the thickness TA of the stacked body SA and a total standard value obtained by adding the standard thicknesses of the outermost metal plates 40 and 50 to the standard thickness of the stacked body SA. The standard thickness of the outermost metal plate 50 along the stacking direction D is similar to the definition of the thickness T11 of the outermost metal plate 40. For example, the standard thickness of the outermost metal plate 50 is within a range including an error of approximately ±50 µm from the ideal thickness of the outermost metal plate 50.
[0111] In this embodiment, the stacked body SA is made thinner than the standard thickness of the stacked body SA. Accordingly, the thickness of the power storage module 400 can be reliably set within a predetermined range by using the thickness adjustment member 30.
[0112] Next, a method of manufacturing the power storage module 400 according to this embodiment will be described with reference to Fig. 8 described. Fig. 8 is a flowchart illustrating the method of manufacturing the power storage module 400.
[0113] As in Fig. As shown in Fig. 8, the first sealing portion 21 is formed with respect to the bipolar electrodes 14, the negative terminal electrode 18, the positive terminal electrode 19, and the outermost metal plates 40 and 50 (step S1). In step S1, first, the bipolar electrodes 14, the negative terminal electrode 18, the positive terminal electrode 19, and the outermost metal plates 40 and 50 are provided. Next, the first sealing portions 21 are welded to the one surface 15a of the metal plates 15 included in the bipolar electrodes 14, the negative terminal electrode 18, and the positive terminal electrode 19, the one surface 40a of the outermost metal plate 40, and the one surface 50a of the outermost metal plate 50. Accordingly, the first sealing portion 21 is coupled to each of the bipolar electrodes 14, the negative terminal electrode 18, the positive terminal electrode 19, and the outermost metal plates 40 and 50.
[0114] Next, the stacked body SA is formed (step S2). In step S2, first, the bipolar electrodes 14 to which the first sealing portion 21 is coupled and the separators 13 are alternately stacked along the stacking direction D to form the stacked body S. Next, the negative terminal electrode 18 is arranged at one end of the stacked body S in the stacking direction D, and the positive terminal electrode 19 is arranged at the other end of the stacked body S in the stacking direction D. Accordingly, the stacked body Sa is formed.
[0115] Furthermore, the thickness TA of the stacked body SA is measured along the stacking direction D (step S3). In this embodiment, steps S2 and S3 are performed simultaneously. Accordingly, the thickness TA of the stacked body SA is measured during formation of the stacked body SA. In step S3, the thickness TA can be measured continuously during formation of the stacked body SA, or the thickness TA can be measured at intervals.
[0116] Next, a difference between the measured thickness TA of the stacked body SA and the standard thickness of the stacked body SA along the stacking direction D is calculated (step S4). In step S4, for example, a device that measures the thickness TA of the stacked body SA performs a comparison with the standard thickness stored in a memory or the like. The difference is calculated accordingly.
[0117] Next, the thickness adjustment member 30 is stacked with a thickness corresponding to the difference on the first sealing portion 21 in the stacking direction D (step S5). In step S5, the thickness adjustment member 30 is arranged on the first sealing portion 21 coupled to the positive terminal electrode 19. Accordingly, the difference is reduced or eliminated.
[0118] Next, the outermost metal plate 40, to which the first sealing portion 41 is coupled, is stacked on the positive terminal electrode 19 through the thickness adjustment member 30 (step S6). In step S6, the first sealing portion 21 coupled to the outermost metal plate 40 is arranged on the thickness adjustment member 30. Accordingly, the thickness adjustment member 30 is located between the first sealing portion 21 coupled to the positive terminal electrode 19 and the first sealing portion 21 coupled to the outermost metal plate 40. Furthermore, in step S6, the outermost metal plate 50, to which the first sealing portion 21 is coupled, is stacked on the negative terminal electrode 18. The outermost metal plate 50 is arranged on an outer side of the negative terminal electrode 18 in the stacking direction. Accordingly, the electrode stack body 11 is formed.
[0119] Next, the second sealing portion 22 coupled to the respective first sealing portions 21 and the thickness adjustment member 30 is formed (step S7). In step S7, for example, a resin is injection-molded onto outer peripheral surfaces of the respective first sealing portions 21 and an outer peripheral surface of the thickness adjustment member 30 using a die. Furthermore, the resin is cured by cooling, thereby forming the second sealing portion 22. Accordingly, the seal body 12 including the first sealing portions 21 and the second sealing portion 22 is formed. At this time, the outermost metal plate 40 may be welded to the thickness adjustment member 30, or the outermost metal plate 50 may be welded to the first sealing portion 21 coupled to the negative terminal electrode 18.Although not shown, after step S7, an electrolytic solution is injected into the respective interior spaces V. The power storage module 400 is manufactured through the steps described above.
[0120] The power storage module 400 manufactured by the above-described manufacturing method according to this embodiment has the thickness adjustment member 30 that adjusts the thickness of the power storage module 400 in the stacking direction D. The thickness adjustment member 30 is located between the positive terminal electrode 19 and the outermost metal plate 40 and at a position overlapping the first sealing portion 21 in the stacking direction D. Here, the thickness Ta of the thickness adjustment member 30 is set in accordance with a difference between the measured thickness TA of the stacked body SA and the standard thickness of the stacked body SA along the stacking direction D. Accordingly, at the time of manufacturing the power storage module 400, the thickness adjustment member 30 is arranged at the position before the second sealing portion 22 is formed.Accordingly, the total thickness of the electrode stack body 11 and the thickness adjustment member 30 along the stacking direction D can be adjusted to the standard thickness determined in advance before the second sealing portion 22 is formed. Therefore, when the second sealing portion 22 is formed, the occurrence of a formation error of the second sealing portion 22 can be suppressed. As a result, it is possible to provide the power storage module 400 capable of suppressing the occurrence of the sealing error.
[0121] Furthermore, in this embodiment, the thickness adjustment member 30 is arranged on an outer side of the stacked body SA. In this case, a distance between the bipolar electrodes 14 in the stacked body SA can be set constant or approximately constant. Accordingly, variation in the state of charge (SOC) in the bipolar electrodes 14 can be reduced.
[0122] In this embodiment, the thickness adjustment member 30 is in contact with the positive terminal electrode 19 and the outermost metal plate 40. In this case, since the positive terminal electrode 19 is protected from the external environment by the outermost metal plate 40, deterioration of the positive terminal electrode 19 can be suppressed. Accordingly, leakage of the electrolytic solution due to breakage of the positive terminal electrode 19 can be suppressed. Moreover, the thickness adjustment member is firmly fixed by the positive terminal electrode 19 and the outermost metal plate 40. Examples of deterioration of the positive terminal electrode 19 include corrosion (e.g., rust) of the positive terminal electrode 19. For example, corrosion of the positive terminal electrode 19 occurs in the metal plate 15 exposed due to a defect in a plated layer.Examples of breakage of the positive terminal electrode 19 include formation of a through hole according to progress of corrosion.
[0123] In this embodiment, the electrode stack body 11 has the outermost metal plate 50 located on an outer side of the negative terminal electrode 18 in the stacking direction D. In this case, since the negative terminal electrode 18 is protected from the external environment by the outermost metal plate 50, deterioration of the negative terminal electrode 18 can be suppressed. Accordingly, leakage of the electrolytic solution due to breakage of the negative terminal electrode 18 can be suppressed. The deterioration and breakage of the negative terminal electrode 18 are similar to the deterioration and breakage of the positive terminal electrode 19.
[0124] An alkaline electrolytic solution is stored in the internal space V formed by the electrode stack body 11 and the sealing body 12, and the excess space EV1 is formed by the negative terminal electrode 18, the first sealing portion 21 coupled to the negative terminal electrode 18, and the outermost metal plate 50. Here, in this embodiment, the thickness adjustment member 30 is located between the positive terminal electrode 19 and the outermost metal plate 40 in the stacking direction D and is not located between the negative terminal electrode 18 and the outermost metal plate 50. Accordingly, even when the thickness adjustment member 30 is used, the shape and volume of the excess space EV1 in the stacking direction D can be accurately defined. Accordingly, the amount of water vapor contained in the excess space EV1 can be accurately defined.Accordingly, the amount of electrolytic solution leakage when an alkali creep phenomenon, which will be described later, occurs can be satisfactorily defined. Furthermore, since the thickness adjustment member 30 is not located between the negative terminal electrode 18 and the outermost metal plate 50, airtightness of the excess space EV1 can be ensured. Furthermore, in this embodiment, the excess space EV2 is formed by the negative terminal electrode 18, the first sealing portion 21 coupled to the negative terminal electrode 18, the first sealing portion 21 coupled to the bipolar electrode 14 adjacent to the negative terminal electrode 18 in the stacking direction D, and the second sealing portion 22.
[0125] In the power storage module 400, the electrolytic solution is transferred to the metal plate 15 of the negative terminal electrode 18 due to the so-called alkali creep phenomenon and passes through a gap between the first sealing portion 21 and the negative terminal electrode 18, and thus the electrolytic solution may leak onto one surface 15a of the metal plate 15. The alkali creep phenomenon may occur during charging, discharging, and a no-load state of the power storage device due to an electrochemical factor, a fluid phenomenon, and the like. The alkali creep phenomenon is caused by the presence of a negative electrode potential, moisture, and a path for the electrolytic solution.
[0126] Examples of a movement route of the electrolytic solution expected when the alkali creep phenomenon occurs in the power storage module 400 include a gap between the negative terminal electrode 18 and the first sealing portion 21 coupled to the bipolar electrode 14 adjacent to the negative terminal electrode 18, the excess space EV2, a gap between the metal plate 15 of the negative terminal electrode 18 and the first sealing portion 21 coupled to the negative terminal electrode 18, the excess space EV1, and a gap between the first sealing portion 21 coupled to the outermost metal plate 50 and the outermost metal plate 50. That is, both excess spaces EV1 and EV2 are provided on the movement route of the electrolytic solution due to the alkali creep phenomenon.
[0127] In this embodiment, the alkaline electrolytic solution is stored in the internal space V. There is a concern that the alkaline electrolytic solution may flow to the outside of the power storage module 400 through a gap between the negative terminal electrode 18 and the first sealing portion 21 due to the so-called alkali creep phenomenon. In contrast, the power storage module 400 according to this embodiment has the excess spaces EV1 and EV2 in which the electrolytic solution is not stored on the movement route of the electrolytic solution.In this way, since the excess spaces EV1 and EV2 are provided on the movement route of the electrolytic solution, it is possible to satisfactorily suppress the intrusion of moisture in the air into the module from a gap between the negative terminal electrode 18 and the first sealing portion 21, which is the starting point of the spreading of the electrolytic solution. Accordingly, the influence of external humidity, which becomes an accelerating condition of the alkali creep phenomenon, is suppressed. Consequently, leakage of the electrolytic solution to the outside of the power storage module 400 is suppressed, and thus, the reliability of the power storage module 400 is improved.
[0128] In the embodiment, the thickness adjustment member 30 may include a plurality of layered members stacked along the stacking direction D. In this case, the thickness Ta of the thickness adjustment member 30 can be easily adjusted by changing the number of layered members included in the thickness adjustment member 30. Accordingly, the thickness adjustment member 30 corresponding to the power storage module 400 can be easily provided.
[0129] In this embodiment, the thickness adjustment member 30 may be formed of the same material as the first sealing portion 21. In this case, a reduction in the cost of the power storage module 400 can be realized.
[0130] In this embodiment, each of the thickness adjustment member 30 and a plurality of the first sealing portions 21 may contain an alkali-resistant thermoplastic resin. In this case, when the second sealing portion 22 is formed, the first sealing portions 21 and the thickness adjustment member 30 and the second sealing portion 22 can be satisfactorily coupled.
[0131] In this embodiment, the thickness Ta of the thickness adjustment member 30 may correspond to a difference between a total value obtained by adding the thickness T11 of the outermost metal plate 40 to the thickness TA of the stacked body SA and a total standard value obtained by adding the standard thickness of the outermost metal plate 40 along the stacking direction D to the standard thickness of the stacked body SA along the stacking direction D. In this case, the total thickness can be adjusted with accuracy within a range of the total standard value.In this embodiment, the thickness Ta of the thickness adjustment member 30 may correspond to a difference between a total value obtained by adding the thickness T11 of the outermost metal plate 40 and the thickness of the outermost metal plate 50 to the thickness TA of the stacked body SA, and a total standard value obtained by adding the standard thickness of the outermost metal plates 40 and 50 along the stacking direction D to the standard thickness of the stacked body SA along the stacking direction D. In this case, the total thickness can be adjusted within a range of the total standard value with greater accuracy.
[0132] In this embodiment, step S2 of forming the stacked body SA and step S3 of measuring the thickness TA of the stacked body SA are performed simultaneously. Consequently, the time required to manufacture the power storage module 400 can be shortened.
[0133] Here, respective modification examples of the second embodiment will be described with reference to Fig. 9 to 12. In the following modification example, a description of a portion redundant with the second embodiment will be omitted. Accordingly, the following description will mainly describe a portion different from the second embodiment.
[0134] Fig. 9 is a schematic cross-sectional view illustrating an internal configuration of a power storage module 400A according to a first modification example of the second embodiment. The power storage module 400A shown in Fig. 9 has a thickness adjustment member 30A located on an outer side of the negative terminal electrode 18 in the stacking direction D. On the other hand, the power storage module 400A is not provided with the thickness adjustment member 30 and the outermost metal plate 40 located on an outer side of the positive terminal electrode 19 in the stacking direction D, unlike the power storage module 400 according to the second embodiment. In addition, two first sealing portions 21 are coupled to the positive terminal electrode 19 included in the power storage module 400A. Specifically, first sealing portions 21 different from each other are coupled to one surface 15a and the other surface 15b of the metal plate 15 included in the positive terminal electrode 19.
[0135] The thickness adjustment member 30A has the same configuration as the thickness adjustment member 30 of the second embodiment. The thickness adjustment member 30A is located between the negative terminal electrode 18 and the outermost metal plate 50 in the stacking direction D and overlaps the first sealing portion 21 in the stacking direction D. The thickness adjustment member 30A is in contact with the first sealing portion 21, which is coupled to the negative terminal electrode 18 and the outermost metal plate 50. The thickness adjustment member 30A and the negative terminal electrode 18 are spaced apart from each other. The thickness adjustment member 30A may include a plurality of layered members.
[0136] Even in the power storage module 400A described above, since the thickness adjustment member 30A is used, when forming the second sealing portion 22, the occurrence of a formation error of the second sealing portion 22 can be suppressed. Moreover, the thickness adjustment member 30A is firmly fixed by the negative terminal electrode 18 and the outermost metal plate 50.
[0137] In the power storage module 400A, the thickness adjustment member 30A is in contact with the outermost metal plate 50 and the first sealing portion 21 coupled to the negative terminal electrode 18, and the thickness adjustment member 30A and the negative terminal electrode 18 are spaced apart from each other. In this way, since the thickness adjustment member 30A is spaced apart from the negative terminal electrode 18, the function exhibited by the thickness adjustment member 30A is less likely to be adversely affected by the negative terminal electrode 18.
[0138] Fig. 10 is a schematic cross-sectional view showing an internal configuration of a power storage module 400B according to a second modification example of the second embodiment. The power storage module 400B shown in Fig. 10 is not provided with the outermost metal plate 50 in contact with the negative terminal electrode 18, unlike the power storage module 400 according to the second embodiment. Even in the power storage module 400B, the same operating effect as in the second embodiment is exhibited by using the thickness adjustment member 30. Moreover, in the power storage module 400B, since the outermost metal plate 50 is not used, a method for manufacturing the power storage module 400B can be simplified.
[0139] Fig. 11 is a schematic cross-sectional view illustrating an internal configuration of a power storage module 400C according to a third modification example of the second embodiment. The power storage module 400C shown in Fig. 11 has both thickness adjustment members 30 and 30A. Accordingly, in the power storage module 400C, the thickness adjustment member 30 is located at one end portion of the electrode stack body 11 in the stacking direction D, and the thickness adjustment member 30A is located at the other end portion of the electrode stack body 11 in the stacking direction D. Moreover, the thickness adjustment member 30 is sandwiched between the positive terminal electrode 19 and the outermost metal plate 40, and the thickness adjustment member 30A is sandwiched between the negative terminal electrode 18 and the outermost metal plate 50.
[0140] In the power storage module 400C, the first sealing portion 21 coupled to the negative terminal electrode 18 and the thickness adjustment member 30A are located between the peripheral edge portion 15c of the metal plate 15 of the negative terminal electrode 18 and the part 42a of the peripheral edge portion 42 of the outermost metal plate 40. Accordingly, a distance from the positive terminal electrode 19 to the part 42a of the outermost metal plate 40 along the stacking direction D may differ from a distance from the negative terminal electrode 18 to the part 52a of the outermost metal plate 50 along the stacking direction D. For example, the distance from the positive terminal electrode 19 to the part 42a of the outermost metal plate 40 is shorter than the distance from the negative terminal electrode 18 to the part 52a of the outermost metal plate 50.In this case, since a recessed distance of the positive terminal electrode 19 is shorter than a recessed distance of the negative terminal electrode 18, a region of the other portion 42b in the peripheral edge portion 42 of the outermost metal plate 40 can be narrowed. Furthermore, in a plan view, an area of the central portion 41 (second contact portion) of the outermost metal plate 40 can be enlarged compared to an area of the central portion 51 (first contact portion) of the outermost metal plate 50.
[0141] Even in the power storage module 400C described above, the same operating effect as in the second embodiment is exhibited. Furthermore, a total thickness of the electrode stack body 11 and the thickness adjustment members 30 and 30A along the stacking direction D can be accurately adjusted to the standard thickness before the second sealing portion 22 is formed.
[0142] Fig. 12 is a schematic cross-sectional view illustrating an internal configuration of a power storage module 400D according to a fourth modification example of the second embodiment. In the power storage module 400D shown in Fig.As shown in Fig. 12, the first sealing portion 21 is formed by folding an outer edge portion of a film constituting the first sealing portion 21 toward an inner side. Thus, the thickness adjustment member 30 is formed by the first sealing portion 21 coupled to the outermost metal plate 40, and the thickness adjustment member 30A is formed by the first sealing portion 21 coupled to the outermost metal plate 50. The first sealing portion 21, which is coupled to the outermost metal plate 40, sandwiches the peripheral edge portion 42 of the outermost metal plate 40 in the stacking direction D and is in contact with one surface 40a and the other surface 40b of the peripheral edge portion 42. The first sealing portion 21, which is in contact with the other surface 40b, is also in contact with the other surface 15b of the metal plate 15 of the positive terminal electrode 19.The first sealing portion 21, coupled to the outermost metal plate 50, sandwiches the peripheral edge portion 52 of the outermost metal plate 50 in the stacking direction D and is in contact with one surface 50a and the other surface 50b of the peripheral edge portion 52. The first sealing portion 21, which is in contact with the other surface 50b, is also in contact with the one surface 15a of the metal plate 15 of the negative terminal electrode 18.
[0143] In the power storage module 400D, a variety of types of different thicknesses are provided as the first sealing portions 21 coupled to the outermost metal plates 40 and 50, respectively. In addition, when the outermost plates 40 and 50 are stacked, the thickness of the first sealing portion 21 coupled to each of the outermost metal plates 40 and 50 is selected so that the thickness T of the electrode stack body 11 becomes the standard thickness. Accordingly, the thickness T of the electrode stack body 11 can be set to the standard thickness determined in advance. Even in this aspect, the same effect as in the second embodiment can be exhibited.Note that in the power storage module 400D, only the thickness adjustment member 30 may be configured by the first sealing portion 21 coupled to the outermost metal plate 40, or only the thickness adjustment member 30A may be configured by the first sealing portion 21 coupled to the outermost metal plate 50. The thickness adjustment member 30A may be configured by the first sealing portion 21 coupled to the other surface 15b of the metal plate 15 of the negative terminal electrode 18, instead of the first sealing portion 21 coupled to the outermost metal plate 50.
[0144] The power storage module and the manufacturing method thereof according to the present invention are not limited to the second embodiment and the respective modification examples thereof, and various modifications can be made. For example, in the second embodiment and the respective modification examples thereof, one surface in each of the metal plates is roughened, but there is no limitation thereto. For example, only a location included in the coupling region in the one surface may be roughened. In the one surface of the outermost metal plate, only a location included in the coupling region may be roughened.In the second embodiment and the second modification example and the third modification example thereof, only one surface of the metal plate included in the positive terminal electrode may be roughened, or only a place included in the coupling region in the one surface may be roughened.
[0145] In the second embodiment and the respective modification examples thereof, each of the metal plates and the outermost metal plate has an approximately rectangular shape in plan view, but this is not limited to this. Each of the metal plates and the outermost metal plate may have a polygonal shape in plan view, a circular shape, or an elliptical shape. Similarly, each of the end plates, the separators, the seal body (specifically, the first seal portions and the second seal portion), and the thickness adjustment members may have an approximately rectangular frame shape in plan view.
[0146] In the second embodiment and the respective modification examples thereof, the thickness adjustment members are arranged to be aligned with the first sealing portions in the stacking direction, but there is no limitation thereto. Accordingly, an outer edge of each of the thickness adjustment members and an outer edge of each of the first sealing portions need not be aligned with each other. At this time, the outer edge of the thickness adjustment member may be located closer to the center of the electrode stack body compared to the outer edge of the first sealing portion. Only parts of the outer edge of the thickness adjustment member and the outer edge of the first sealing portion may be aligned with each other. Similarly, an inner edge of the thickness adjustment member and an inner edge of the first sealing portion need not be aligned with each other.At this time, the inner edge of the thickness adjustment member may be located closer to the center of the electrode stack body than the inner edge of the first sealing portion, or may be located closer to the outer edge than the inner edge of the first sealing portion. Parts of the inner edge of the thickness adjustment member and the inner edge of the first sealing portion may be aligned with each other.
[0147] In the second embodiment and the respective modification examples thereof, when the first sealing portions adjacent to each other in the stacking direction are in contact with each other, the first sealing portions may be temporarily coupled to each other before the second sealing portion is formed. For example, the first sealing portions adjacent to each other may be welded together. In this case, intrusion of the second sealing portion into a space between the first sealing portions can be suppressed. The first sealing portion and the thickness adjustment member adjacent to each other in the stacking direction may be temporarily coupled to each other.
[0148] In the second embodiment and the respective modification examples thereof, a measurement of the thickness of the stacked body is performed simultaneously with the formation of the stacked body, but this is not limited to this. A measurement of the thickness of the stacked body may be performed after the step of forming the stacked body. The thickness of the stacked body may be measured by adding the thicknesses of respective constituent elements included in the stacked body. For example, the thicknesses of each of the bipolar electrodes, each of the separators, the positive terminal electrode, and the negative terminal electrode may be measured before the step of forming the stacked body.
[0149] In the second embodiment, when the outermost metal plates are not recessed, the shape and area of one of the outermost metal plates, viewed from one side of the stacking direction, are approximately the same as the shape and area of the other outermost metal plate, viewed from the other side of the stacking direction. Therefore, it may be difficult to determine a positive side and a negative side of the power storage module only by viewing the outermost metal plates from an outer side. To prevent this problem in advance, the shape of the seal body, viewed from one side of the stacking direction, and the shape of the seal body, viewed from the other side of the stacking direction, may be different from each other. For example, a cutout portion, a protrusion, or the like may be provided only on an inner peripheral side of the seal body, viewed from the one side of the stacking direction.Accordingly, the positive side and the negative side of the power storage module can be easily determined. Here, when a structural body such as the protrusion or the like is provided in the sealing body, for example, there is a concern that the structure and the conductive structural body and the like may interfere with each other when the power storage module is manufactured. The cutout portion may be provided in the sealing body from the viewpoint of preventing interference. When the cutout portion is provided in the sealing body, the cutout portion may be formed in the vicinity of the negative terminal electrode in the stacking direction from the viewpoint of suppressing leakage of the electrolytic solution through the cutout portion due to the alkali creep phenomenon. The cutout portion and the like may be formed in the sealing body of the modified examples.
[0150] In the second embodiment and the first and third modifications thereof, the power storage module has two surplus spaces, but this is not limited to this. The power storage module may have at least one surplus space along a movement route of the electrolytic solution when the alkali creep phenomenon occurs.
[0151] In the second embodiment and the first and third modification examples thereof, the power storage modules may include, for example, a water-repellent material, a liquid-absorbing member, or the like. For example, the water-repellent material is provided in a region in the metal plates and the outermost metal plate that is not subjected to welding. Accordingly, the electrolytic solution is less likely to be transferred to the metal plates. For example, the liquid-absorbing member is provided on the one surface of the outermost metal plate adjacent to the negative terminal electrode to surround the conductive structural body. Accordingly, moisture in the air is less likely to penetrate into the interior of the power storage module.For example, the water-repellent material is a film-shaped object made of a fluorine-based resin material, a fluororubber, a polymer having a fluorine-based and a methyl-based functional group, or the like. For example, the liquid-absorbent member is a nonwoven fabric having a sheet shape, or the like. From the perspective of improving water absorption, the liquid-absorbent member may be subjected to plasma treatment.
[0152] In the second embodiment and the second and third modifications thereof, the thickness adjustment member is in contact with the positive terminal electrode, but this is not limited to this. The thickness adjustment member and the positive terminal electrode may be spaced apart from each other. For example, the first sealing portion coupled to the metal plate of the positive terminal electrode may be provided between the thickness adjustment member and the positive terminal electrode.
[0153] In the third modification example of the second embodiment, the thickness adjustment members 30 and 30A may have the same configuration or may have configurations different from each other. The thickness adjustment members 30A and 30A may have thicknesses different from each other. List of reference symbols 4, 4A, 4B, 400, 400A, 400B, 400C, 400D power storage module 11, 11A, 11B electrode stack body 11a Side surface 12 sealing bodies 14 Bipolar electrode 15 metal plate 15a a surface (inner surface) 15b other area (inner area) 15c edge section 18 negative connection electrode 19 positive connection electrode 21, 21A, 21B, 21C first sealing section 22 second sealing section 30, 30A, 30B, 30C Thickness adjustment component 40 outermost metal plate 41 middle section (second contact section) 50 outermost metal plate 51 middle section (first contact section) D Stacking direction EV1 surplus space (first surplus space) EV2 surplus space (second surplus space) S, SA stacked body T, TA, Ta, Tb, T11 thickness V Interior VA surplus space
Claims
[1] Power storage module (400, 400A, 400B, 400C, 400D) with: an electrode stack body (11) comprising a stack body (SA) in which a plurality of bipolar electrodes (14) are stacked, a pair of terminal electrodes (18, 19) located on an outer side of the stack body (SA) in a stacking direction (D) of the bipolar electrodes, and a plurality of metal plates (15) forming the stack body (SA) and the pair of terminal electrodes (18, 19); and a sealing body (12) provided to surround a side surface of the electrode stack body (11), wherein the sealing body (12) has a plurality of first sealing portions (21) coupled to edge portions of the plurality of metal plates (15), and a second sealing portion (22) coupling the first sealing portions (21) to each other, a thickness adjustment member (30, 30A) which adjusts the thickness of the electrode stack body (11) in the stacking direction (D), is arranged in the electrode stack body (11) at a position of overlapping the first sealing portions as viewed from the stacking direction (D), the electrode stack body (11) further has an outermost metal plate (40, 50) located on an outer side of one of the pair of terminal electrodes (18, 19) in the stacking direction (D), the stacked body (SA) further comprises separators (13) stacked alternately with the bipolar electrodes (14) along the stacking direction (D), the first sealing sections (21) are coupled to edge sections of the metal plates (15) and the outermost metal plate (40, 50), the second sealing portion (22) covers side surfaces of the plurality of first sealing portions (21), and the thickness adjustment member (30, 30A) is located between one of the pair of terminal electrodes (18, 19) and the outermost metal plate (40) and adjusts the thickness of the electrode stack body (11) in the stacking direction (D). [2] The power storage module (400, 400A, 400B, 400C) according to claim 1, wherein the thickness adjustment member (30, 30A) is formed of the same material as in the first sealing portions (21) and is designed separately from the first sealing portions (21). [3] The power storage module (400D) according to claim 1, wherein the thickness adjustment member (30, 30A) is configured by the first sealing portions (21). [4] Power storage module (400, 400A, 400B, 400C) according to one of claims 1 to 3, wherein one of the pair of terminal electrodes (18, 19) is a negative terminal electrode (18), the other of the pair of terminal electrodes (18, 19) is a positive terminal electrode (19), and the thickness adjustment member (30, 30A) is arranged at least between the stack body (SA) and the negative terminal electrode (18) or between the stack body (SA) and the positive terminal electrode (19) in the stacking direction. [5] The power storage module (400, 400A, 400B, 400C) according to claim 4, wherein the thickness adjustment member (30, 30A) is arranged between the stacked body (SA) and the negative terminal electrode (18) and at an edge portion of an inner surface of the metal plate (15) of the negative terminal electrode (18) in the stacking direction (D). [6] The power storage module (400, 400A, 400B, 400C) according to claim 4, wherein the thickness adjustment member (30, 30A) is disposed between the stacked body (SA) and the positive terminal electrode (19) and at the first sealing portion (21) coupled to an edge portion of an inner surface of the metal plate (15) of the positive terminal electrode (19) in the stacking direction (D). [7] The power storage module (400, 400A, 400B, 400C) according to claim 4, wherein the thickness adjustment member (30, 30A) is arranged both between the stacked body (SA) and the negative terminal electrode (18) and between the stacked body (SA) and the positive terminal electrode (19) in the stacking direction (D). [8] The power storage module (400, 400A, 400B, 400C) according to claim 7, wherein the thickness of the thickness adjustment member (30, 30A) disposed between the stacked body (SA) and the negative terminal electrode (18) and the thickness of the thickness adjustment member (30, 30A) disposed between the stacked body (SA) and the positive terminal electrode (19) are equal to each other. [9] Power storage module (400A, 400C) according to one of claims 1 to 8, wherein one of the pair of terminal electrodes (18, 19) is a negative terminal electrode (18), the thickness adjustment member (30A) is in contact with the outermost metal plate (50) and the first sealing portion (21) coupled to the metal plate of the negative terminal electrode (18), and the thickness adjustment component (30A) is spaced from the negative terminal electrode (18). [10] Power storage module (400D) according to one of claims 1 to 8, wherein one of the pair of terminal electrodes (18, 19) is a negative terminal electrode (18), and the thickness adjustment member (30A) is in contact with the negative terminal electrode (18) and the outermost metal plate (50). [11] Power storage module (400, 400B, 400D) according to one of claims 1 to 8, wherein one of the pair of terminal electrodes (18, 19) is a positive terminal electrode (19), and the thickness adjustment member (30) is in contact with the positive terminal electrode (19) and the outermost metal plate (40). [12] Power storage module (400, 400A, 400B, 400C, 400D) according to one of claims 1 to 11, wherein the electrode stack body (11) further has an additional outermost metal plate (40, 50) located on an outer side of the other of the pair of terminal electrodes (18, 19) in the stacking direction (D), and an additional thickness adjustment member (30, 30A) that adjusts the thickness of the electrode stack body (11) in the stacking direction (D), between the other of the pair of terminal electrodes (18, 19) and the additional outermost metal plate (40, 50) and located at a position that overlaps the first sealing portions (21) in the stacking direction (D). [13] Power storage module (400, 400A) according to one of claims 1 to 8, wherein the other of the pair of terminal electrodes (18, 19) is a negative terminal electrode (18), the electrode stack body (11) further has an additional outermost metal plate (40, 50) located on an outer side of the negative terminal electrode (18) in the stacking direction (D), an alkaline electrolytic solution is stored in an interior space formed by the electrode stack body (11) and the sealing body (12), and a first excess space (EV1) is formed by the negative terminal electrode (18), the first sealing portion (21) coupled to the metal plate (15) of the negative terminal electrode (18), and the additional outermost metal plate (50). [14] The power storage module (400, 400A, 400B, 400C) according to claim 12 or 13, wherein a distance from one of the pair of terminal electrodes (18, 19) to the edge portion of the outermost metal plate (40, 50) along the stacking direction (D) is different from a distance from the other of the pair of terminal electrodes (18, 19) to an edge portion of the additional outermost metal plate (40, 50) along the stacking direction (D). [15] Power storage module (400, 400C, 400D) according to one of claims 12 to 14, wherein the outermost metal plate (50) has a first contact portion (51) which is in contact with one of the pair of terminal electrodes (18, 19), the additional outermost metal plate (40) has a second contact portion (41) in contact with the other of the pair of terminal electrodes (18, 19), and a region of the first contact portion (51) differs from a region of the second contact portion (41) as viewed from the stacking direction (D). [16] The power storage module (400, 400A, 400B, 400C, 400D) according to any one of claims 1 to 15, wherein the thickness adjustment member (30, 30A) has a plurality of layered members stacked along the stacking direction (D). [17] The power storage module (400, 400A, 400B, 400C, 400D) according to any one of claims 1 to 16, wherein each of the thickness adjustment member (30, 30A) and the plurality of first sealing portions (21) contains an alkali-resistant thermoplastic resin. [18] A method for manufacturing a power storage module (400, 400A, 400B, 400C, 400D) comprising the following steps: Forming a stacked body (SA) by alternately stacking bipolar electrodes (14), to which first sealing sections (21) are correspondingly coupled, and separators (13) along a stacking direction (D); Measuring the thickness of the stack body (SA) along the stack direction (D); Calculating a difference between the thickness of the stack body (SA) and a standard thickness of the stack body (SA) along the stacking direction (D); Stacking a thickness adjustment member (30, 30A) having a thickness corresponding to the difference at the first sealing portion (21) in the stacking direction (D); Stacking an outermost metal plate (40, 50) to which an additional first sealing portion (21) is coupled on the stacked body (SA) via the thickness adjustment member (30, 30A); and Forming a second sealing portion (22) coupling the first sealing portions (21), the thickness adjusting member (30, 30A) and the additional first sealing portion (21). [19] The method for manufacturing a power storage module (400, 400A, 400B, 400C, 400D) according to claim 18, wherein the thickness of the thickness adjustment member (30, 30A) corresponds to a difference between a total value obtained by adding the thickness of the outermost metal plate (40, 50) along the stacking direction (D) to the thickness of the stacked body (SA) and a total standard value obtained by adding a standard thickness of the outermost metal plate (40, 50) along the stacking direction (D) to the standard thickness of the stacked body along the stacking direction (D). [20] A method for manufacturing a power storage module (400, 400A, 400B, 400C, 400D) according to claim 18 or 19, wherein forming the stacked body (SA) and measuring the thickness of the stacked body (SA) are performed simultaneously.
Citation Information
Patent Citations
Sealing structure of bipolar type battery
JP2011204386A
Secondary battery, battery pack of the secondary battery, and vehicle using them
JP2010092662A
Electrode member for lithium ion battery, lithium ion battery, and its manufacturing method
JP2010272266A
Stacked constructions for electrochemical batteries
US20130095366A1
JP002010092662A