CONTINUOUS EXPANSION PROCESS FOR METAL-CONTAINING BULK MATERIAL AND METAL POWDER EXPANSION PRESSING PLANT
Patent Information
- Application Number
- DE502017016523
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2017-01-18
- Filing Date
- 2017-12-20
- Publication Date
- 2024-11-14
- Estimated Expiration
- 2037-12-20
AI Technical Summary
Industrial implementation of continuous extrusion processes for metal powder mixtures is hindered by unstable process control, leading to powder adhesions, reduced volume flow, and incomplete compaction due to insufficient pressure buildup, resulting in pressing errors and quality issues.
The implementation of a continuous extrusion process using three circumferentially arranged sealing plates that can be cooled individually to control temperature, preventing powder adhesion and ensuring consistent pressure, along with targeted cooling of pressing tool components to optimize the extrusion process.
This approach stabilizes the extrusion process, prevents adhesion, and ensures high-quality production of extruded bodies by maintaining a consistent powder supply and sufficient pressure, thereby overcoming the limitations of conventional processes.
Description
[0001] The invention relates to a continuous extrusion process and a metal powder extrusion plant according to the independent claims.
[0002] The term "metal-containing bulk material" used in this application includes, among other things, metal-containing powders, powder mixtures, granules, and chips. These can also be mixtures of metal powders with ceramic fibers or particles, i.e., composite materials.
[0003] Various methods have already been proposed to compact metal-containing bulk materials.
[0004] Components made from powder metallurgical materials can be used, for example, in the automotive industry, aerospace engineering, and general mechanical engineering. Continuous extrusion is a cost-effective alternative for compacting metal-containing bulk materials, especially metal powder. Originally, this process, also known as the conform process, was used to convert cast or rolled wire made of aluminum or copper alloys into more complex geometries in a single step. Later, pressing processes were developed to process granules or powders. It has become apparent that stable process control is difficult. Therefore, such extrusion processes for metal-containing bulk materials have not yet been used industrially.
[0005] A conventional powder extrusion press suitable for the extrusion process comprises a rotating extrusion wheel with a circumferential groove and a stationary shoe that encloses the feed plate arranged in the deflection area and the counterholder. The die is connected to the feed plate, which has an opening. The pressing tool components forming the inlet area and the deflection area extend over approximately a quarter of the circumference of the extrusion wheel. The metal-containing bulk material, in particular a metal-containing powder, is drawn into the inlet area and the deflection area by friction as the extrusion wheel rotates. The metal-containing powder is accumulated and compacted on the counterholder. The compacted powder is deflected by the counterholder to the feed plate, which has the opening, and to a die.The individual cold powder particles fuse together due to shear forces to form a fully compacted strand without melting. The frictional and deformation forces caused by the rotation of the extrusion wheel generate the required temperatures and pressures for continuous extrusion through the die.
[0006] In the dissertation Stadelmann, C.: Extrusion of metal powders by continuous powder extrusion, Friedrich-Alexander-University Erlangen-Nuremberg, 2009, investigations are described in which metal powder mixtures are continuously pressed into a strand using a modified pressing system.
[0007] A similar continuous extrusion process is known from DE 10 2006 004 622 A1.
[0008] WO 2008 / 003275 A1 describes a process for producing molded parts from dispersion-strengthened metal alloys.
[0009] The documents JP H01 309716 A, GB 2 372 955 A, KR 101 580 975 B1, EP 2 683 502 A1, JP 2009 148827 A and JP H11 197737 A each relate to similar methods and devices.
[0010] Extrusion processes for metal powder mixtures have not yet been implemented industrially because stable process control is usually not possible. During the extrusion process, powder buildup occurs in the powder feed area, clogging the extrusion channel and preventing consistent dosing of the powder mixture.
[0011] If the yield stress becomes too low during the extrusion process, complete compaction of the powder is not possible. The pressure required to completely weld particles of the metal-containing bulk material, especially powder particles, together is not sufficiently high.
[0012] The volume flow per wheel revolution transported during the feeding of the metal-containing bulk material is reduced due to the given bulk density. The strand exit speeds therefore differ significantly from those during wire feeding. This, in turn, results in longer residence times of the metal-containing, partially compacted bulk material in the die's extrusion channel, increasing the risk of adhesion and thus extrusion defects on the sealing plates and die.
[0013] The invention is therefore based on the object of providing a continuous extrusion process for a metal-containing bulk material which enables stable process control.
[0014] To solve this problem, an extrusion method having the features of claim 1 is provided.
[0015] In the extrusion process according to the invention, three sealing plates arranged in the circumferential direction are used, each of which can be cooled in a graduated manner by associated cooling devices, wherein a cooling device comprises cooling channels integrated in the sealing plates through which a cooling medium flows, wherein temperature sensors are integrated in the sealing plates and are connected to a controller for the individual and separate control of the temperature of the sealing plates, wherein each sealing plate is assigned its own control circuit.
[0016] Surprisingly, it was found that a stable process can be ensured through controlled temperature control of press tool components in the form of cooling. This is surprising, as one would initially assume that heating would be beneficial for a stable process. One might assume that the powder flows more easily due to rearrangement and that less heat is therefore generated through plastic deformation (adiabatic heating). The lower internal heat generation should actually be compensated for by stronger heating. Instead, tests have surprisingly shown that targeted, graduated temperature control in the form of cooling has a process-stabilizing effect. The cooling provided according to the invention enables an extruded body to be produced in a continuous process with high quality.It was found that cooling the inlet area of the press channel can prevent powder adhesion to the sealing plates. This ensures a continuous powder feed and a uniform pressure build-up.
[0017] In the area of the counterholder, cooling the press tool components, especially the feed plate, creates a sufficiently high pressing pressure, which leads to the breaking up of oxide skins and the welding of metal particles in the metal-containing bulk material. In an extrusion process involving the feeding of a wire, however, cooling in the area of the counterholder would result in high pressing pressures and increased chip formation, which could potentially impede or stop the entire process.
[0018] In the method according to the invention, it is preferred that at least one pressing tool component arranged in the deflection region, namely the feed plate and / or the counterholder, is / are cooled by means of a cooling device. The pressing tool components form a pressing channel with the extrusion wheel. The counterholder deflects the material flow through the feed plate toward the die. The cooling provided according to the invention prevents adhesion of the metal powder mixture, which could lead to unstable process conditions and pressing defects. Furthermore, sufficiently high pressures are generated.
[0019] The extrusion process according to the invention is carried out in a metal powder extrusion plant with three sealing plates arranged in the circumferential direction.
[0020] In the method according to the invention, it is preferred that a sealing plate be cooled to a temperature between 80 °C and 130 °C when processing copper or a copper alloy. This cooling prevents powder adhesion and ensures that a sufficiently high pressing pressure is built up.
[0021] Similarly, in the extrusion process according to the invention, it can be provided that, when processing aluminum or an aluminum alloy, a sealing plate is cooled to a temperature between 50 °C and 100 °C. In contrast, in conventional processes that are carried out without cooling, temperatures between approximately 300 °C and 330 °C occur.
[0022] With the method according to the invention, several sealing plates as pressing tool components arranged in the inlet area, as well as the feed plate and / or the counterholder as pressing tool components arranged in the deflection area, can be cooled. The respective cooled pressing tool components are selected to optimize the process, allowing a desired temperature profile to be specifically set in the inlet area and, if necessary, also in the deflection area.
[0023] In the extrusion process according to the invention, it is also possible that, when processing copper or a copper alloy, at least one pressing tool component arranged in the deflection region, in particular the feed plate, is cooled to a temperature between 310 °C and 380 °C. In contrast, when the process is carried out without cooling, temperatures of more than 440 °C occur.
[0024] Similarly, when processing aluminum or an aluminum alloy, it may be provided that at least one pressing tool component arranged in the deflection region, in particular the feed plate, is cooled to a temperature between 340 °C and 420 °C.
[0025] In addition to cooling one or more press tool components, it is also possible to cool the counterholder. When processing copper or a copper alloy, the counterholder is preferably cooled to a temperature between 340 °C and 430 °C. On the other hand, in the extrusion process according to the invention, when processing aluminum or an aluminum alloy, the counterholder can be cooled to a temperature between 300 °C and 380 °C.
[0026] The die of the metal powder extrusion press is not cooled. Instead, it is heated to a temperature between 370 °C and 420 °C when processing copper or a copper alloy. When processing aluminum or an aluminum alloy, the die is heated to a temperature between 400 °C and 430 °C.
[0027] The specified temperature ranges are examples for alloys containing copper or aluminum as their main component. The process control, especially the temperature control, must be adapted depending on the alloy used. Other influencing factors include the particle size of the metallic bulk material, the particle roughness, the oxide content of the particles, and the particle shape. If one of these influencing factors changes, the extrusion behavior also changes, requiring the temperature control to be adjusted. The temperature range suitable for processing also depends on the speed of the extrusion wheel and its diameter, and thus on the rotational speed.
[0028] In addition, the invention relates to a metal powder extrusion press which is designed for the continuous extrusion of a metal-containing bulk material, with the features of claim 10. The metal powder extrusion press according to the invention has a press channel which is delimited by an extrusion wheel and press tool components which comprise an inlet area having sealing plates and a deflection area with a counterholder and a feed plate.The metal powder extrusion press according to the invention is characterized in that it has cooling devices with which three sealing plates arranged in the circumferential direction in the inlet area can each be cooled in a graduated manner, wherein a cooling device comprises cooling channels integrated in a sealing plate through which a cooling medium can flow, wherein temperature sensors are integrated in the sealing plates and are connected to a controller for the individual and separate control of the temperature of the sealing plates, wherein each sealing plate is assigned its own control circuit.
[0029] The metal powder extrusion system according to the invention comprises a controller configured to cool at least one sealing plate to a specified temperature. Preferably, the controller is also configured to cool the feed plate and / or the counterholder.
[0030] The cooling device of the metal powder extrusion press according to the invention comprises cooling channels integrated into the sealing plates through which a cooling medium can flow. Analogously, the feed plate and the counterholder can also have corresponding cooling channels.
[0031] The invention is explained below using an exemplary embodiment with reference to the drawings. The drawings are schematic representations and show: Fig. 1 is a sectional view of a metal powder extrusion press according to the invention in the region of the press channel when carrying out the method according to the invention, and Fig. 2 is an enlarged view of Fig. 1 in the area of the press channel.
[0032] Fig. 1 shows the essential components of a metal powder extrusion plant 1, which is suitable for producing extruded bodies from a metal powder mixture by an extrusion process.
[0033] The metal powder extrusion press 1 comprises a rotating extrusion wheel 2 having a circumferential groove 3 on its outer surface. The extrusion wheel 2 is driven at a fixed speed by a drive motor (not shown).
[0034] Sealing plates 5, 6, 7 are arranged side by side along a circular segment-shaped path on a stationary tool shoe 4. The sealing plates 5, 6, 7, together with the extrusion wheel 2, form a press channel 8. A metal powder mixture is introduced into the press channel 8 via a tubular feed 9 in this embodiment. As best seen in the enlarged view of Fig. 2As can be seen, the pressing tool components in the deflection area comprise a feed plate 10 with an opening for the compacted metallic bulk material 13. During the extrusion process, the compacted metallic bulk material flows through the opening to a die. Also arranged in the deflection area is a counterholder 11, which deflects the already almost completely compacted metallic bulk material 13 by approximately 90°. After passing through the opening of the feed plate 10, the almost completely compacted metallic bulk material 13 reaches a die 12, which defines the outer contour of the produced extruded body. Alternative designs are also possible in which a die defines the inner contour or both the inner contour and the outer contour of the extruded body. The die 12 can, for example, have a circular, rectangular or more complex cross-section.
[0035] To produce an extruded body, bulk metallic material in the form of a metal powder mixture is introduced via feed 9. In the present embodiment, the metal powder mixture is a copper alloy. The powder particles enter the press channel 8, which is formed on the one hand by the groove 3 of the extrusion wheel 2 and on the other hand by the sealing plates 5, 6, 7 as press tool components. As it passes through the press channel 8, the metal powder mixture is compacted. The pressure created as it passes through the press channel 8 causes the metallic powder particles to be compacted. In the area of the counterholder 11, the compacted metal powder mixture 13 is deflected by 90°. The compacted metal powder mixture 13 is then extruded through the die 12. To ensure a stable process, it is essential that the sealing plates 5, 6, 7 are cooled.The fact that cooling of the sealing plates 5, 6, 7 and thus cooling of the metal powder mixture 13 to be compacted is necessary is surprising, since it was previously assumed that the heat generated during compaction facilitates the flow of the metal powder mixture. However, tests have shown that at high process temperatures, which arise from compaction in the press channel 8, a low yield stress is present. In this case, a sufficiently high pressing pressure is not built up to completely weld the metallic powder particles together. Therefore, the sealing plates 5, 6, 7 are each cooled in a graduated manner by dedicated cooling devices.
[0036] A cooling device comprises cooling channels integrated into a sealing plate 5, 6, 7, through which a cooling medium flows. In the illustrated embodiment, water serves as the cooling medium. Heat generated during the compaction of the metal powder mixture 13 is dissipated in a controlled manner by means of the cooled sealing plates 5, 6, 7. Furthermore, a cooling device with cooling channels is also assigned to the feed plate 10 to cool the feed plate 10.
[0037] In contrast, the die 12 is not cooled. Instead, a heating device (not shown) is assigned to it. Furthermore, alternative designs are possible in which the die can optionally be cooled. The inlet area in front of the extrusion chamber, a pre-chamber, or a spacer ring arranged in front of the die can be cooled.
[0038] Temperature sensors are arranged along the sealing plates. These sensors are designed as thermocouples and are integrated into the component to be cooled, i.e. either in a sealing plate 5, 6, 7 or in the feed plate 10. The sealing plate 5 has a cooling channel 15. The sealing plate 6 has a cooling channel 16. The sealing plate 7 has a cooling channel 17. A temperature sensor 18 is integrated into the sealing plate 5. The sealing plates 6, 7 have corresponding temperature sensors 19, 20. A temperature sensor 21 is integrated into the feed plate 10, which has a cooling channel 22. The cooling channels 15, 16, 17, 22 of the sealing plates 5, 6, 7 and the feed plate 10 each form a separate cooling circuit. Each cooling circuit includes a pump that moves the coolant around the circuit. The temperature sensors 18, 19, 20, 21 are connected to a controller 14 via cables not shown.The controller 14 uses temperature sensors to regulate the cooling process. This allows the sealing plates 5, 6, 7 and the feed plate 10 to be individually and separately controlled to set a specific temperature or temperature range in each section of the extrusion channel 8. Each sealing plate 5, 6, 7 and the feed plate 10 is assigned its own control loop. Controlled cooling allows a stable, quasi-stationary state to be created, allowing the extrusion process to be carried out continuously.
[0039] The choice of a suitable temperature range depends on the metal powder mixture to be processed. For copper or copper alloys, the second sealing plate 6 in this embodiment is cooled to a temperature of 80°C to 140°C. The adjacent sealing plates 5 and 7 can be cooled to a lower or higher temperature, respectively. The feed plate 10 is cooled to a temperature between 320°C and 380°C. The counterholder 11 is cooled to a temperature between 360°C and 430°C. The die 12 is heated to a temperature between 350°C and 450°C.
[0040] For processing aluminum, i.e., pure aluminum, as well as aluminum alloys, the following temperatures have proven suitable: The second sealing plate 6 is cooled to a temperature between 40 °C and 100 °C. The feed plate 10 is cooled to a temperature between 340 °C and 430 °C. The counterholder 11 is cooled to a temperature between 310 °C and 380 °C. The die is heated to a temperature between 380 °C and 450 °C.
[0041] The temperatures given are examples that must be adjusted depending on the metallic bulk material used and the powder characteristics (particle size, particle shape, particle surface area, mixing ratio of multiple components). The temperature of the die must be adjusted to the metallic bulk material to be processed and the profile to be produced (cross-sectional area, multiple perforations, expansion behavior).
[0042] During the extrusion process, targeted cooling prevents heating of the sealing plates 5, 6, and 7. This results in the advantages of reduced tool load, no loss of the required pressing pressure, and significantly improved feed behavior of the added metal powder mixture.
[0043] A further effect of cooling in the intake area of the press channel 8 is that the temperature in the extrusion area at the die 12 remains constant. Heating the die 12 is particularly necessary for small extruded body cross-sections, since otherwise the pressing pressure becomes so great that the compacted material does not flow through the die 12 but is squeezed out as chips laterally past the counterholder 11. In this undesirable case, the temperatures at the feed plate 10 and the counterholder 11 are significantly higher than at the die 12. However, if this temperature difference is compensated by heating the die 12 and cooling the feed plate 10, the desired extrusion through the die 12 occurs.
[0044] The continuous extrusion process for bulk metallic material enables the production of an extruded body with high and consistent quality. List of reference symbols
[0045] 1Metal powder extrusion press 2Extrusion wheel 3Groove 4Tool shoe 5, 6, 7Sealing plate 8Press channel 9Feeder 10Feed plate 11Counterholder 12Die 13Metal powder mixture 14Controller 15, 16, 17Cooling channel 18, 19, 20, 21Temperature sensor 22Cooling channel
Claims
1. Continuous extrusion process for a metal-containing bulk material (13) for producing an extruded body, comprising the following steps: - introducing the metal-containing bulk material (13) into a press channel (8) of a metal powder extrusion plant (1) which is bounded by a rotating extrusion wheel (2) and press tool components which comprise an inlet region having sealing plates (5, 6, 7) and a deflection region with a counterholder (11) and a feed plate (10), - feeding the metal-containing bulk material (13) via a circumferential groove (3) of the rotating extrusion wheel (2) to the counterholder (11) and deflecting the compacted metal-containing bulk material (13) in the deflection region through the feed plate (10), which has an opening, to a die (12), characterized in that three sealing plates (5, 6, 7) arranged in the circumferential direction are used, each of which can be cooled in a graded manner by associated cooling devices, one cooling device comprising cooling channels (15, 16, 17) which are integrated in the sealing plates (5, 6, 7) and through which a cooling medium flows, wherein temperature sensors (18, 19, 20) are integrated in the sealing plates (5, 6, 7), which are connected to a controller (14) for individual and separate control of the temperature of the sealing plates (5, 6, 7), wherein each sealing plate (5, 6, 7) is assigned its own control circuit.
2. Extrusion process according to claim 1, wherein at least one extrusion die component arranged in the deflection region, namely the feed plate (10) and / or the mating die (11), is or are cooled by means of one or more cooling devices.
3. Extrusion process according to claim 1 or 2, wherein a sealing plate (5, 6, 7) is cooled to a temperature between 80 °C and 130 °C during the processing of copper or a copper alloy.
4. Extrusion process according to one of the preceding claims, wherein during the processing of copper or a copper alloy the feed plate (10) is cooled to a temperature between 310 °C and 380 °C.
5. Extrusion process according to one of the preceding claims, wherein during the processing of copper or a copper alloy the counterholder (11) is cooled to a temperature between 340 °C and 430 °C.
6. Extrusion process according to one of the preceding claims, wherein the die (12) is heated to a temperature between 370 °C and 420 °C during the processing of copper or a copper alloy.
7. Extrusion process according to claim 1 or 2, wherein a sealing plate (5, 6, 7) is cooled to a temperature between 50 °C and 100 °C during the processing of aluminum or an aluminum alloy.
8. Extrusion process according to one of claims 1, 2 or 7, wherein during the processing of aluminum or an aluminum alloy, the feed plate (10) is cooled to a temperature between 340 °C and 420 °C.
9. Extrusion process according to one of claims 1, 2, 7 or 8, wherein the counterholder (11) is cooled to a temperature between 300 °C and 380 °C during the processing of aluminum or an aluminum alloy.
10. Extrusion process according to one of claims 1, 2, 7, 8 or 9, wherein the die (12) is heated to a temperature between 400 °C and 430 °C during the processing of aluminum or an aluminum alloy.
11. Metal powder extrusion plant (1), which is designed for the continuous extrusion of a metal-containing bulk material (13), with an extrusion channel (8), which is bounded by an extrusion wheel (2) and extrusion die components, which have an inlet region comprising sealing plates (5, 6, 7) and a deflection region with a counterholder (11) and a feed plate (10), characterized in that the metal powder extrusion plant (1) has cooling devices with which three sealing plates (5, 6, 7) arranged in the inlet region in circumferential direction can each be cooled in a graded manner, wherein a cooling device comprises cooling channels (15, 16, 17) which are integrated in a sealing plate (5, 6, 7) and through which a cooling medium can flow, wherein temperature sensors (18, 19, 20) are integrated in the sealing plates (5, 6, 7), which are connected to a controller (14) for individual and separate control of the temperature of the sealing plates (5, 6, 7), wherein each sealing plate (5, 6, 7) being assigned its own control circuit.