DEVICE FOR COATING A WORKPIECE WITH AT LEAST ONE HIGH-PERFORMANCE POLYMER; COATING METHOD

DE502018015159D1Active Publication Date: 2024-10-02ELOXALWERK LUDWIGSBURG HELMUT ZERRER GMBH +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
DE502018015159
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2018-02-22
Filing Date
2018-10-29
Publication Date
2024-10-02
Estimated Expiration
2038-10-29

AI Technical Summary

Technical Problem

Conventional coating processes for high-performance polymers like PEEK are inefficient for temperature-sensitive materials, as they require heating above the polymer's melting temperature, leading to property changes and are not suitable for achieving dense, adhesive coatings, and lack control over porosity and energy efficiency.

Method used

A device with at least two radiation sources, one emitting a wavelength primarily absorbed by the workpiece and the other by the high-performance polymer, along with a measuring device to regulate thermal radiation, allowing for controlled energy input and temperature management during the coating process.

Benefits of technology

This method enables the production of homogeneous or porous coatings with controlled adhesion, porosity, and surface topography on temperature-sensitive materials, reducing thermal load and achieving efficient energy use, allowing for the coating of complex geometries without preheating, and expanding the range of achievable layer thicknesses.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader
Need to check novelty before this filing date? Find Prior Art

Description

State of the art

[0001] The invention is based on a device for coating a workpiece with at least one high-performance polymer according to the preamble of claim 1 and a coating method according to the preamble of claim 4.

[0002] A promising approach for coating metallic components that have a combination of functional requirements is the use of high-performance polymers as coating materials. The key functional requirements addressed by these coatings include wear and corrosion protection, friction reduction, temperature resistance, and electrical insulation. The high-performance polymer polyetheretherketone (PEEK), in particular, is excellently suited to meeting these requirements due to its material properties and is already used industrially (E. Spyrou: Powder coatings. Chemistry and technology 3rd, rev. ed. Hanover 2012).

[0003] Conventional coating processes for this material primarily include powder-based layer application with subsequent melting of the applied layer using an oven process, as well as powder flame spraying.

[0004] For the oven-based coating process, the polymer is applied to the workpiece in powder form by electrostatic coating or as a dispersion or spray application. Other, less industrially relevant methods of material application include electrophoretic coating (I. Corni, N. Neumann, D. Eifler, AR Boccaccini: Polyetheretherketone (PEEK) Coatings on Stainless Steel by Electrophoretic Deposition. In: Advanced Engineering Materials 10 (2008) 6, pp. 559-64.) or printing processes (e.g. screen printing). Following the material application, the workpiece is heated in an oven to temperatures of typically 380 to 420 °C, so that the PEEK layer is completely melted. Typically used heating rates are on the order of 10 K / min and holding times on the order of 30 minutes to several hours. The coated workpiece is then cooled under controlled conditions.The cooling rates chosen depend on the material used and the mass of the workpiece.

[0005] In powder flame spraying, the coating material is applied to the workpiece using thermal spraying. The powder is melted by passing it through a flame in a gas stream and then applied layer by layer in a molten phase to the component. Preheating the workpiece to be coated is not mandatory, but can contribute to improving the coating properties. According to the powder manufacturer Victrex Europa GmbH (Victrex Europa GmbH: Product brochure Vicote Flame Spray 702 / 705 Coatings. Quick 10 Step Guide For Optimum Results 2016), preheating the workpiece to be coated to 230 °C is required for coating aluminum with PEEK to achieve optimal adhesion and flow properties. For steel, preheating of up to 370 °C is recommended (Victrex Europa GmbH: Product brochure Vicote Flame Spray 702 / 705 Coatings. Quick 10 Step Guide For Optimum Results 2016; P. Vuoristo: Thermal Spray Coating Processes.In: S. Hashmi, GF Batalha, CJ Van Tyne, BS Yilbas (eds.): Comprehensive materials processing. Oxford, Walltham, MA 2014).

[0006] Both of these processes are unsuitable for producing dense and adherent coatings on temperature-sensitive substrates, where heating above the melting temperature of the polymer (approximately 340 °C for PEEK) leads to a functionally relevant change in properties. In addition to the low energy efficiency associated with the use of furnace processes, site-selective coatings are often associated with significant technical and economic complexity. Targeted adjustment of porosity, especially depending on location, is not possible due to the nature of the process.

[0007] Laser-based coating processes, such as laser cladding disclosed in DE 693 00 501 T2 or laser peening disclosed in EP 1 932 928 B1, are also state of the art. In these processes, the coating material is applied to a workpiece, and the workpiece is coated or densified by simultaneous irradiation with a single laser.

[0008] EP 2 969 256 B1 discloses a method for applying a sliding coating to a piston assembly, using high-performance polymers such as PEEK as the coating material. The coating material is cured in two subsequent steps using IR, UV, or induction radiation. The nature of the radiation with regard to monochrome, coherence, or generation method is not further defined.

[0009] The invention is therefore based on the object of providing a device for coating a workpiece with at least one high-performance polymer and a coating method which eliminate the disadvantages described above.

[0010] The object is achieved by the device for coating a workpiece with at least one high-performance polymer having the features of patent claim 1 and the coating method having the features of patent claim 4.

[0011] According to the invention, the object is achieved by means of a device for coating a workpiece with at least one high-performance polymer, which device has at least two radiation sources.

[0012] This is preferably a device for coating a workpiece with at least one high-performance polymer, preferably providing wear and corrosion protection, friction reduction, temperature resistance and / or electrical insulation, which has at least two radiation sources.According to the invention, it is provided that the first radiation source is adapted to emit radiation of a first wavelength which is adapted for primary absorption by the workpiece and / or that the second radiation source is adapted to emit radiation of a second wavelength which is adapted for primary absorption by the high-performance polymer and / or that a measuring device is provided for the contactless measurement of thermal radiation of the workpiece and of the at least one high-performance polymer, wherein the measuring device is preferably designed to regulate or control the power of the two radiation sources to a constant value of emitted thermal radiation from the workpiece and the high-performance polymer.

[0013] Furthermore, the object is achieved by means of a method in which the process energy required for coating a workpiece with at least one high-performance polymer is generated at least partially by at least two radiation sources.

[0014] Preferably, a coating method is provided, in particular by means of a coating device according to one of claims 1 to 3, in which the process energy required for coating a workpiece with at least one high-performance polymer preferably providing wear and corrosion protection, friction reduction, temperature resistance and / or electrical insulation is generated at least partially by at least two radiation sources.According to the invention, it is provided that the first radiation source emits radiation of a first wavelength which is adapted for primary absorption by the workpiece and / or that the second radiation source emits radiation of a second wavelength which is adapted for primary absorption by the high-performance polymer, and / or that a measuring device for the contactless measurement of thermal radiation of the workpiece and of the at least one high-performance polymer carries out such a measurement, wherein the measuring device preferably carries out the measurement in a contactless manner and / or regulates or controls the power of the two radiation sources to a constant value of emitted thermal radiation from the workpiece and the high-performance polymer. The invention and its advantages

[0015] The device according to the invention for coating a workpiece with at least one high-performance polymer, having the features of claim 1, has the advantage that the device comprises at least two radiation sources. These can be used simultaneously or sequentially during the coating process.

[0016] According to an advantageous embodiment of the device according to the invention, the radiation from at least one radiation source is at least partially coherent.

[0017] According to a preferred embodiment of the device according to the invention, at least one radiation source is a laser. In this case, the radiation from the radiation source is completely coherent. However, it is also conceivable to use another radiation source that generates, for example, infrared radiation, ultraviolet radiation, induction radiation, microwave radiation, or particle radiation (X-rays or gamma radiation).

[0018] According to a preferred development of the device according to the invention, the wavelength of the radiation of at least one radiation source is in the wavelength range from 400 to 3000 nm.

[0019] According to a preferred development of the device according to the invention, the wavelength of the radiation of at least one radiation source is in the wavelength range from 4000 to 12000 nm.

[0020] According to a preferred embodiment of the device according to the invention, the radiation from at least one radiation source is continuous or pulsed. This allows the high-performance polymer to be completely melted to achieve a homogeneous or porous coating.

[0021] According to a preferred embodiment of the device according to the invention, the intensity of the radiation from at least one radiation source can be regulated. Thus, the power of at least one radiation source can also be adjusted to requirements.

[0022] According to a preferred embodiment of the device according to the invention, the radiation from at least one radiation source has a wavelength at which the absorption coefficient of at least one high-performance polymer is as high as possible. Thus, the radiation is primarily absorbed only by the high-performance polymer, enabling a targeted adjustment or regulation of the temperature of the high-performance polymer.

[0023] According to a preferred embodiment of the device according to the invention, the radiation from at least one radiation source has a wavelength at which the absorption coefficient of the workpiece is as high as possible. Thus, the radiation is primarily absorbed only by the workpiece, enabling targeted adjustment or regulation of the workpiece's temperature.

[0024] According to a preferred embodiment of the device according to the invention, the device comprises at least one fixed optic. The radiation from at least one radiation source is guided at least partially onto the workpiece through a fixed optic. A fixed optic has the advantage that the accuracy of the beam guidance can be optimized.

[0025] According to a preferred embodiment of the device according to the invention, the device comprises at least one scanner system for guiding the radiation. The radiation from at least one radiation source is guided at least partially over the workpiece by a scanner system. This allows the workpiece to be scanned with the radiation and thus to be irradiated at as many desired locations as possible, even if the workpiece has a complex geometry.

[0026] According to a preferred embodiment of the device according to the invention, the device comprises at least one measuring device for measuring thermal radiation and / or temperature. The temperature or thermal radiation is preferably measured contactlessly, for example, using a pyrometer or an infrared camera.

[0027] According to a preferred embodiment of the device according to the invention, the device comprises at least one positioning device. This allows the workpiece to be positioned in the required position before machining or moved during machining.

[0028] According to a preferred embodiment of the device according to the invention, the device comprises at least one application device for applying at least one high-performance polymer to the workpiece. Thus, the application of the high-performance polymer to the workpiece and the subsequent melting of the high-performance polymer can be accomplished by the same machine.

[0029] The coating method according to the invention with the features of claim 4 has the advantage that the process energy required for coating a workpiece with at least one high-performance polymer is generated at least partially by at least two radiation sources. At least two radiation sources are used simultaneously or sequentially.

[0030] According to an advantageous embodiment of the coating process according to the invention, at least one high-performance polymer is applied to the workpiece in a preceding process step. The high-performance polymer, which is preferably a polymer powder, is applied to the workpiece, for example, as a powder-based dispersion by electrostatic spraying or as a preferably water-based dispersion by spraying, printing, dipping, or doctor blade coating.

[0031] According to a preferred development of the coating method according to the invention, at least one radiation source radiates at least partially coherently.

[0032] According to a preferred embodiment of the coating method according to the invention, a laser is used as at least one radiation source. In this case, the radiation from the radiation source is completely coherent. However, it is also conceivable that another radiation source is used, which generates, for example, infrared radiation, ultraviolet radiation, induction radiation, microwave radiation, or particle radiation (X-rays or gamma radiation).

[0033] According to a preferred development of the coating method according to the invention, at least one radiation source radiates in the wavelength range from 400 to 3000 nm.

[0034] According to a preferred development of the coating method according to the invention, at least one radiation source radiates in the wavelength range from 4000 to 12000 nm.

[0035] According to a preferred embodiment of the coating method according to the invention, the radiation from at least one radiation source is temporally and / or spatially modulated. The radiation can thus be continuous, pulsed, and of increasing and / or decreasing intensity.

[0036] According to a preferred embodiment of the coating method according to the invention, the intensity of at least one radiation source is regulated during coating. This allows for continuous switching and / or switching of the radiation during coating between continuous, pulsed, increasing intensity, and / or decreasing intensity.

[0037] According to a relevant embodiment of the coating method according to the invention, at least one radiation source is regulated in such a way that a constant temperature is present on the surface of the workpiece.

[0038] According to a preferred embodiment of the coating method according to the invention, the radiation from at least one radiation source is primarily absorbed by at least one high-performance polymer. This allows for targeted adjustment or regulation of the temperature of the high-performance polymer.

[0039] According to a preferred embodiment of the coating method according to the invention, the radiation from at least one radiation source is primarily absorbed by the workpiece. This allows for targeted adjustment or regulation of the workpiece's temperature.

[0040] According to a preferred embodiment of the coating method according to the invention, the radiation from at least one radiation source is guided at least partially onto the workpiece by means of a fixed optics system. A fixed optics system has the advantage of allowing the accuracy of the beam guidance to be optimized.

[0041] According to a preferred embodiment of the coating method according to the invention, the radiation from at least one radiation source is guided at least partially over the workpiece by means of a scanner system. By moving the radiation using a scanner system, the location hit by the radiation can be varied, allowing the workpiece to be scanned with the radiation and thus irradiated as many desired locations as possible, even if the workpiece has a complex geometry.

[0042] According to a preferred embodiment of the coating method according to the invention, the thermal radiation of the workpiece and / or at least one high-performance polymer is measured contactlessly. This is possible, for example, using a pyrometer or an infrared camera, although other contactless methods for measuring thermal radiation or temperature are also conceivable.

[0043] According to a preferred embodiment of the coating method according to the invention, the workpiece is aligned and / or guided by at least one positioning device. The workpiece can thus be moved or positioned into the position required for the coating process. The position of the workpiece can thus also be changed during the coating process.

[0044] According to a preferred development of the coating method according to the invention, a device for coating a workpiece with at least one high-performance polymer according to one of claims 1 to 14 is used in the coating method.

[0045] Further advantages and advantageous embodiments of the invention can be found in the following description, the claims and the drawings. drawing

[0046] Preferred developments of the subject matter of the invention are illustrated in the drawing and explained in more detail below. It shows: Fig. 1 shows a structure for carrying out the coating method according to the invention or the device according to the invention for coating a workpiece with at least one high-performance polymer. Description of the embodiments

[0047] Fig. 1shows a setup for carrying out the coating method according to the invention or the device according to the invention for coating a workpiece 4a with at least one high-performance polymer 4b. In this exemplary embodiment, two radiation sources 1 and 2 and the measuring device 3 for measuring thermal radiation and / or temperature are arranged above the workpiece 4a to be coated. The high-performance polymer 4b has already been applied to the workpiece 4a. The workpiece 4a is brought to the correct position by means of a positioning device 5 so that the workpiece 4a or a desired location on the workpiece 4a and the high-performance polymer 4b are hit by the beams 6 and 7 from the radiation sources 1 and 2. The measuring device 3 measures the thermal radiation 9 emitted by the workpiece 4a and the high-performance polymer 4b.It is also conceivable that the measurement of the thermal radiation 8 takes place coaxially to the beam path of the radiation 6, but can also take place lateral to the beam path of the radiation 6.

[0048] The two beams of radiation 6 and 7 are modulated separately in time and space. The wavelengths are preferably selected such that one beam is primarily absorbed by the high-performance polymer 4b and the other beam is primarily absorbed by the workpiece 4a. The wavelength of one radiation 6 or 7 is preferably in the wavelength range from 400 to 3000 nm and the wavelength of a second radiation 6 or 7 is in the range from 4000 to 12000 nm. In both cases, the radiation 6 and 7 is preferably continuous or modulated or pulsed on a time scale in the range of > 10 ns. The workpiece 4a to be coated is moved by means of a manual or automated positioning device 5 (preferably a robot or axis system) either into a fixed processing position or moved and / or rotated in at least one dimension (including rotation) during the coating process. The application of the high-performance polymer 4b, e.g.of a polymer powder, takes place in a previous step. The application method preferably comprises the application of a (preferably water-based) dispersion by spraying, printing, dipping, or doctor blade methods, or the application of a polymer-based powder mixture by electrostatic spraying.

[0049] During the coating process, the power of at least one radiation source 1 or 2 is regulated or controlled to maintain a constant value for the thermal radiation 8, 9 emitted by the workpiece 4a and high-performance polymer 4b. The control or monitoring of the thermal radiation 8, 9 or the temperature is performed contactlessly using pyrometry or a camera-based system (e.g., an IR camera).

[0050] The central effect of the coating process according to the invention lies in the temporal and spatial control of the temperature profiles in the workpiece 4a and the high-performance polymer 4b during the coating process. By using (preferably water-based) high-performance polymer dispersions during the layer application, the addition of a silane and / or siloxane compound, a metal alcoholate, or other organic solvents is unnecessary and not desired. With the coating process according to the invention, adhesive coatings can be produced even without these components.

[0051] By using two wavelengths, the addition of laser absorbers such as carbon black is not required to enable energy deposition in the high-performance polymer 4b. By controlling or regulating the coating process, preferably monitored by detecting the emitted thermal radiation 8, 9 from the workpiece 4a and high-performance polymer 4b, a homogeneous processing result with regard to adhesion, porosity, and surface topography can be ensured.

[0052] The melting of the high-performance polymer 4b can be limited in time and space, enabling the site-selective production of coatings.

[0053] The thermal stress is reduced compared to the furnace process described above. This makes coating temperature-sensitive materials possible. Due to the reduction in thermal stress, the microhardness profile and the heat-affected zone in the base material are generally significantly different.

[0054] The porosity of the coating can be controlled depending on location and time due to the time-varying coating process parameters.

[0055] The coating process preferably takes place in a normal atmosphere; a protective gas or vacuum atmosphere is not required.

[0056] Compared to the coating process using a single laser beam, a wider range of achievable layer thicknesses results. For a single laser beam, this range is in the range of 1 to 50 µm. Using the coating process according to the invention, this range is extended upwards to at least 250 µm.

[0057] The technical field of application lies in the production of functional coatings on metallic components, in particular in the production of tribological and anti-corrosive coatings. The metallic components to be coated can be selected independently of material, geometry, and application. The coating process according to the invention is preferably used for coating light metals such as aluminum, magnesium, and titanium, as well as steel alloys. The application particularly includes, but is not limited to, components subject to tribological and corrosive stress. An increase in energy efficiency in the coating process is also noteworthy, since preheating is not required.

[0058] All features presented here can be essential to the invention both individually and in any combination. List of reference figures

[0059] 1 Radiation source 2 Radiation source 3 Measuring device 4a Workpiece 4b High-performance polymer 5 Positioning device 6 Radiation 7 Radiation 8 Thermal radiation 9 Thermal radiation

Claims

1. Apparatus for coating a workpiece (4a) with at least one high-performance polymer (4b) providing wear and corrosion protection, friction reduction, temperature resistance and / or electrical insulation, which has at least two radiation sources (1, 2) characterised in that the first radiation source is adapted to emit radiation of a first wavelength which is adapted to be primarily absorbed by the workpiece (4a) that the second radiation source is adapted to emit radiation of a second wavelength which is adapted to be primarily absorbed by the high-performance polymer (4b), a measuring device (3) is provided for contactless measurement of thermal radiation (9) of the workpiece (4a) and of the at least one high-performance polymer (4b), the measuring device (3) being designed to regulate or control the power of the two radiation sources (1, 2) to a constant value of thermal radiation emitted by the workpiece (4a) and high-performance polymer (4b).

2. Device according to claim 1, characterised in that the radiation (6, 7) of at least one radiation source (1, 2) is coherent.

3. Device according to claim 1 or claim 2, characterised in that at least one radiation source (1, 2) is a laser.

4. Coating process, in particular by means of a coating device according to one of claims 1 to 3, in which the process energy required for coating a workpiece (4a) with at least one high-performance polymer (4b) providing wear and corrosion protection, friction reduction, temperature resistance and / or electrical insulation is generated at least in part by at least two radiation sources (1, 2) characterised in that the first radiation source emits radiation of a first wavelength which is adapted to be primarily absorbed by the workpiece (4a), that the second radiation source emits radiation of a second wavelength which is adapted to be primarily absorbed by the high-performance polymer (4b), a measuring device (3) for contactless measurement of thermal radiation (9) of the workpiece (4a) and of the at least one high-performance polymer (4b) carries out such a measurement, the measuring device (3) carrying out the measurement without contact and regulating or controlling the power of the two radiation sources (1, 2) to a constant value of emitted thermal radiation (9) from the workpiece (4a) and high-performance polymer (4b).

5. Coating process according to claim 4, characterised in that at least one high-performance polymer (4b) is applied to the workpiece (4a) in a preceding process step.

6. Coating process according to claim 4 or claim 5, characterised in that at least one radiation source (1, 2) radiates coherently.

7. Coating process according to any one of claims 4 to 6, characterised in that a laser is used as at least one radiation source (1, 2).