AI Technical Summary
Polypropylene is difficult to paint due to poor adhesion of paints, sensitivity to environmental influences, and mechanical processability issues, making it challenging to produce decorated molded parts with high durability and low weight.
A method involving a transfer film with a decorative layer and an adhesion-promoting layer, applied to a polypropylene film, which is then back-injected or over-injected with plastic material, ensuring improved adhesion and environmental resistance.
The method enhances the adhesion of primer and lacquer layers, improves mechanical behavior, and achieves high resistance to environmental influences while reducing manufacturing costs by producing lightweight molded parts with durable decorations.
Description
Process for producing a decorated molded part
[0001] The invention relates to a method for producing a decorated molded part, a decorated molded part and the use of a transfer film for producing a decorated molded part.
[0002] For the production of decorated molded parts, particularly in the automotive sector, it is common practice to manufacture them from ABS plastic substrates, especially in rolls, sheets, or panels (ABS = acrylonitrile butadiene styrene copolymers). Due to their good processability, their ability to be decorated with wet paint systems, and their good resistance to environmental influences, especially in outdoor applications, the aforementioned ABS substrates are preferred for production. These ABS substrates are typically deep-drawn and then coated with the desired decoration.
[0003] US20120189821A1 describes an injection-molded object with refractive patterns on its surface. To produce this object, a multilayer, plate-shaped body is inserted into an injection mold and then back-injected. The multilayer, plate-shaped body has at least one heat-insulating layer that protects the refractive pattern from heat damage during the injection molding process.
[0004] US20100196651A1 relates to a component having an embedded functional element. To produce the component, a decorative transfer film is inserted into an injection molding tool, followed by an injection molding process.
[0005] EP2014440A1 describes back-injectionable films or web-like laminates comprising a carrier film with a decorative coating or a coated decorative film. The films or laminates are molded into the desired shape by compression molding.
[0006] DE69918673T2 relates to a layer for foil decoration, a method for its production, and a foil-decorated article. The layer is an in-mold decorative film with high three-dimensional processability and a multi-layer structure. The layer can comprise a polypropylene reinforcing film and is back-injected three-dimensionally with synthetic resin in an injection mold.
[0007] DE102005049521A1 relates to a method for producing molded parts comprising a film having a coating. The molded parts exhibit high dimensional stability and surface quality. DE102004027090A1 describes a composite material with a decoration. To produce the composite material, a decoration is first applied to a carrier film and then back-injected.
[0008] The invention is based on the object of providing an improved method for producing a decorated molded part.
[0009] This problem is solved by a method for producing a decorated molded part, in which the following steps are carried out: a) producing a precursor in the form of a composite body by applying a transfer layer of a transfer film to a first surface of a polypropylene film, wherein the transfer layer of the transfer film comprises at least one decorative layer, b) forming the composite body comprising the polypropylene film with the applied transfer layer of the transfer film, c) inserting the formed composite body into an injection molding tool and back-injecting and / or over-injecting and / or encapsulating the formed composite body with a plastic material, in particular a plastic material containing or consisting of polypropylene, wherein the transfer layer of the transfer film has an adhesion-promoting layer which is arranged on the side of the one or more decorative layers facing the first surface of the polypropylene film, and wherein the adhesion-promoting layer consists of two or more partial layers which are printed successively, wherein the partial layer of the adhesion-promoting layer facing the first surface of the polypropylene film is based on a polyolefin and / or wherein the partial layer of the adhesion-promoting layer facing the one or more decorative layers consists of a solvent-based polyurethane resin.
[0010] This object is further achieved by a decorated molded body, produced by the preceding method, which has a formed composite body back-injected and / or over-injected and / or over-injected with a plastic material, which has a polypropylene film with a transfer layer of a transfer film applied to a first surface, which transfer layer comprises at least one decorative layer, wherein the transfer layer of the transfer film has an adhesion-promoting layer which is arranged on the side of the one or more decorative layers facing the first surface of the polypropylene film and wherein the adhesion-promoting layer consists of two or more partial layers which are printed successively,wherein the partial layer of the adhesion-promoting layer facing the first surface of the polypropylene film is based on a polyolefin, and / or wherein the partial layer of the adhesion-promoting layer facing the one or more decorative layers consists of a solvent-based polyurethane resin. This object is further achieved by using a transfer film for producing a decorated molded article according to the method described above.
[0011] Polypropylene (PP) is a thermoplastic produced by the chain polymerization of propene. It belongs to the polyolefin group and is semi-crystalline and non-polar. A problem with the use of polypropylene is that paints adhere poorly to this plastic, which often leads to paint delamination. This is why polypropylene is considered difficult to paint. Furthermore, due to its polymer structure, polypropylene is a very sensitive material; upon activation, the formation of weakened interfaces and thus adhesion problems are inevitable. On the other hand, polypropylene has a significantly lower density than ABS, which is preferably between 0.895 g / cm³ and 0.92 g / cm³. This makes it possible to produce molded parts with a lower weight and more parts from a given mass of plastic, thus achieving cost savings.
[0012] The invention is based on the finding that by the procedure described above, on the one hand, the disadvantages of using polypropylene, i.e. its adhesion properties to applied lacquer layers, which complicates decoration, its poor resistance to environmental influences, in particular outdoors, and its poor mechanical processability, can be avoided and molded parts can be produced which are characterized by low weight, high resistance to environmental influences, in particular a decoration with high resistance to environmental influences and overall low production costs.Thus, the problems that occur with polypropylene are solved by applying the transfer layer with the decoration on the one hand and the connection by injection molding on the other hand, and these additional measures also achieve resistance to environmental influences and improved mechanical behavior.
[0013] Advantageous embodiments of the invention are defined in the subclaims.
[0014] According to a preferred embodiment, after carrying out step c), the back-injected and / or over-injected and / or over-injected formed composite body is coated in a step d) with one or more primer layers and / or one or more paint layers.
[0015] This makes it possible to further improve the durability of the decorated molded part, especially for outdoor applications. The adhesion of these one or more primer layers and / or one or more coating layers to the composite body is ensured by the fact that the preceding process steps eliminate the need to apply these one or more primer layers and / or one or more coating layers directly to the polypropylene film, thus avoiding the adhesion problems described above.
[0016] The one or more primer layers and / or one or more lacquer layers are preferably applied over the entire surface or part of the surface of the transfer layer opposite the first surface of the polypropylene film. The transfer layer thus serves as an adhesion-promoting component between the polypropylene film and the one or more primer layers and / or one or more lacquer layers.
[0017] Preferably, in step d) a wet coating with a primer is first carried out and then a wet coating with a protective varnish.
[0018] For wet coating with the primer, preferred methods include flooding and painting, in particular spray painting. It is advantageous to spray with an acrylate paint for wet coating with the primer. The primer is preferably colorless and transparent. The primer is sprayed in particular with an air pressure of 1 bar to 5 bar, in particular 2 bar to 5 bar, and a paint material pressure of 0.2 bar to 2 bar, in particular 0.5 bar to 1.5 bar, with a nozzle diameter of 0.5 mm to 2 mm, in particular 0.7 mm to 1.5 mm. After painting, the primer is dried. The drying process can be multi-stage and can include, in particular, pre-drying at room temperature for approximately 5 to 20 minutes and post-drying at a temperature of 60°C to 90°C for approximately 20 to 40 minutes.
[0019] For wet coating with the protective varnish, processes such as flooding and painting, in particular spray painting, are preferred. For wet coating with the protective varnish, it is advantageous to flood with a polyurethane varnish or an acrylate varnish or to paint over, in particular spray painting with a polyurethane varnish and / or an acrylate varnish. The protective varnish is preferably colorless and transparent and, after drying, its surface is in particular satin-matt. The protective varnish is in particular sprayed with an air pressure of 1 bar to 5 bar, in particular 2 bar to 5 bar and a material pressure of the varnish of 0.2 bar to 2 bar, in particular 0.5 bar to 1.5 bar, with a nozzle diameter of 0.5 mm to 2 mm, in particular 0.7 mm to 1.5 mm. After painting, the protective varnish is dried. The drying process can be multi-stage and, in particular, can involve pre-drying at room temperature for approx.5 minutes to 20 minutes and a final drying at a temperature of 60°C to 90°C for approximately 20 minutes to 50 minutes.
[0020] Preferably, a crosslinking varnish, especially a radiation-curable varnish, such as a UV- or electron-beam-curable varnish, is used as the varnish for these one or more primer layers. It is also possible to use a reactive, two-component varnish (2K varnish) or a thermally crosslinking varnish.
[0021] Preferably, a cross-linking varnish, especially a radiation-curable varnish, such as a UV- or electron-beam-curable varnish, is used as the varnish for these one or more varnish layers. It is also possible to use a reactive, two-component varnish (2K varnish) or a thermally cross-linking varnish. The use of such varnishes can achieve a particularly hard and resistant surface.
[0022] The layer thickness of the primer layer or primer layers applied in step d) is preferably in the range between 0.1 µm and 25 µm, in particular in the range between 0.5 µm and 15 µm.
[0023] The layer thickness of the lacquer layer or layers applied in step d) is preferably in the range between 3 µm and 50 µm, in particular in the range between 5 µm and 30 µm.
[0024] It is also possible to add dyes and / or pigments to the one or more primer layers and / or the one or more lacquer layers, which further improve the decoration of the molded part.
[0025] According to a preferred embodiment, the polypropylene film is pretreated in step a) before applying the transfer layer of the transfer film.
[0026] As a pretreatment, flame treatment of the first surface of the polypropylene film is preferably performed. This type of flame treatment allows the surface to be gently activated: As the flame intensity increases, the oxygen content and the polar functional groups on the first surface increase, while the roughness remains virtually unchanged. The flame treatment creates polar functional groups that are firmly bonded to the base material of the polypropylene film.
[0027] As a pretreatment, it has proven particularly effective to subject the first surface to a high-voltage corona treatment and / or plasma activation.
[0028] Furthermore, studies have shown that with increasing additive content in the polypropylene film on the first surface, the adhesion of the first surface of the polypropylene film decreases significantly. These additives are advantageous, in particular, for improving the mechanical and / or thermal properties of the polypropylene film. However, these additives can lead to undesirable side effects on the chemical / physical properties of the polypropylene film, particularly on its surface, and in particular reduce the adhesion of the first surface of the polypropylene film. To counteract this, it is advantageous to remove these additives on the first surface through additional cleaning during pretreatment and / or to reduce the influence of the additives on the first surface and thus further improve adhesion.Powerwash cleaning, CO2 snow jet cleaning, or water-isopropanol / ultrasonic cleaning are particularly used as pretreatment cleaning methods. Furthermore, the use of chlorinated cleaning agents during pretreatment is advantageous for removing the additives. These cleaning processes wash and / or leach the additives from the first surface. This additional cleaning is preferably performed before flame treatment.
[0029] In order to avoid a renewed migration of additives from the material interior of the polypropylene film to the first surface of the polypropylene film and thus a renewed reduction in the adhesion of the first surface, it is further advantageous to apply the transfer layer as soon as possible after the pretreatment.
[0030] Preferably, the first surface of the polypropylene film is pretreated using a corona treatment and / or one or more of the cleaning processes described above. This can further improve the adhesion of the subsequently applied transfer film.
[0031] Studies have shown that corona treatment with 1500 watts to 3000 watts at a feed speed of the polypropylene film of approx. 10 m / min, especially between 1800 watts and 2200 watts at a feed speed of the polypropylene film of approx. 10 m / min, significantly improves the adhesion of the subsequently applied transfer film.
[0032] Furthermore, this pretreatment is preferably performed immediately before applying the transfer layer. It has proven advantageous to allow no more than 24 hours, preferably no more than 6 hours, and most preferably no more than 10 minutes, to pass between the pretreatment, especially the corona treatment, and the application. This can also further improve the adhesion of the subsequently applied transfer film.
[0033] It is advantageous to apply the corona treatment and / or one or more of the cleaning processes described above also to the surface of the polypropylene film opposite the first surface in order to improve the adhesion of the plastic material to the polypropylene film in particular there.
[0034] The polypropylene film preferably has a layer thickness between 5 µm and 3 mm, preferably between 200 µm and 1000 µm.
[0035] In addition to the basic polymer building block (EN), the polypropylene film can contain a variety of other formulation components selected from release agents, additives, fillers, dyes, color pigments, functional pigments, fiber knits, fiber fabrics, single fibers and mixtures thereof, which can influence and improve the processing and usage properties of the polypropylene film.
[0036] Talc, chalk and / or glass fibers are preferred fillers.
[0037] It has proven particularly advantageous for the processing steps b) and c) if the polypropylene film is formed to achieve the mechanical properties described below by adding appropriate further formulation components: It is advantageous if the Vicat softening temperature of the polypropylene film according to VST A120 is in the range between 140°C and 145°C, measured according to DIN EN ISO 306:2014-03 ("Plastics - Thermoplastics - Determination of Vicat softening temperature (VST) (ISO 306:2013)"; date of issue: 2014-03).
[0038] Furthermore, it is advantageous if the melting temperature of the polypropylene film according to dynamic differential scanning calorimetry (DSC) (10 K / min) is in the range between 160°C and 170°C, measured according to DIN EN ISO 11357-3:2013-04 ("Plastics - Dynamic differential scanning calorimetry (DSC) - Part 3: Determination of melting and crystallization temperature and enthalpy of melting and crystallization (ISO 11357-3:2011)"; date of issue: 2013-04).
[0039] Preferably, the shrinkage of the polypropylene film at 115°C / 1h is less than 1.0%, determined according to IEC 60674-2:2016 ("Specification for plastic films for electrical purposes - Part 2: Methods of test"; Edition 2.0; Date of issue: 2016-11).
[0040] Investigations have shown that by adjusting the thermal properties of polypropylene film as described above, particularly good processability of the polypropylene film in steps b) and c) can be achieved and, in particular, undesired detachment of the transfer layer from the first surface of the polypropylene film during the implementation of these steps due to thermal stresses between the materials can be largely avoided.
[0041] The polypropylene film preferably has a tensile modulus of elasticity between 1100 MPa and 1300 MPa, determined according to DIN EN ISO 527 Part 1 to Part 3, preferably Part 3.
[0042] The polypropylene film preferably has a yield stress between 20 MPa and 30 MPa, in particular between 22 MPa and 26 MPa, determined according to DIN EN ISO 527 Part 1 to Part 3, preferably Part 3.
[0043] The polypropylene film preferably has an elongation at break of more than 100%, determined according to DIN EN ISO 527 Part 1 to Part 3, preferably Part 3.
[0044] DIN EN ISO 527 Part 1 refers to DIN EN ISO 527-1:2012-06 ("Plastics - Determination of tensile properties - Part 1: General principles (ISO 527-1:2012); Publication date: 2012-06).
[0045] DIN EN ISO 527 Part 2 refers to DIN EN ISO 527-2:2012-06 ("Plastics - Determination of tensile properties - Part 2: Test conditions for moulding and extrusion materials (ISO 527-2:2012)"; publication date: 2012-06).
[0046] DIN EN ISO 527 Part 3 refers to DIN EN ISO 527-3:2003-07 ("Plastics - Determination of tensile properties - Part 3: Test conditions for films and sheets (ISO 527-3:1995 + Corr 1:1998 + Corr 2:2001) (includes Corrigendum AC:1998 + AC:2002)"; date of issue: 2003-07).
[0047] Furthermore, the polypropylene film preferably has a hardness, measured according to Shore D / 15sec, between 60 and 65, determined according to DIN EN ISO 7619-1:2012-02 ("Rubber-rubbers or thermoplastic elastomers - Determination of indentation hardness - Part 1: Durometer method (Shore hardness) (ISO 7619-1:2010)"; issue date 2012-02).
[0048] Studies have shown that by adjusting the mechanical properties of the polypropylene film in this way, delamination of the composite body can be largely prevented, even under adverse external environmental influences during subsequent use. This is likely due to the optimized adaptation of the physical, particularly mechanical, properties of the polypropylene film to the physical, particularly mechanical, properties of the other layers / layer systems of the composite body.
[0049] According to a preferred embodiment of the invention, in step a), the transfer film is thermally laminated to the first surface of the polypropylene film, and then the carrier layer of the transfer film is peeled off the applied transfer layer. The thermal lamination preferably takes place at a temperature between 120°C and 180°C. The line pressure, particularly when using a heated laminating roller and a particularly cooled counterpressure roller in a roller nip in which the transfer film is thermally laminated to the first surface of the polypropylene film, is preferably between 4 bar and 6 bar. The thermal lamination, particularly using the parameters described above, achieves additional thermal activation of the surface of the polypropylene film, thus resulting in particularly good adhesion of the transfer layer to the first surface of the polypropylene film.
[0050] The transfer film preferably comprises a carrier layer, an optional release layer, one or more decorative layers, and an adhesion-promoting layer. According to the invention, an adhesion-promoting layer is part of the transfer film, and it is possible for a further adhesion-promoting layer to be applied, in particular laminated, printed, or sprayed, to the entire surface or to specific regions of the first surface of the polypropylene film prior to application of the transfer film.
[0051] According to the invention, the adhesion-promoting layer is part of the transfer layer of the transfer film and is arranged within the layer structure of the transfer film on the side of the one or more decorative layers facing the first surface of the polypropylene film.
[0052] The adhesion-promoting layer preferably consists of a thermally activatable adhesive layer, in particular a thermoplastic and / or thermally crosslinking adhesive. However, it is also possible for the adhesion-promoting layer to contain radiation-crosslinking components, in particular UV-crosslinking or electron beam-crosslinking components.
[0053] According to the invention, the adhesion-promoting layer consists of two or more sublayers that are printed successively. It is particularly advantageous that these sublayers are formulated differently, so that one sublayer facing the first surface is optimized for adhesion to the first surface of the polypropylene film, and a second sublayer facing the one or more decorative layers is optimized for adhesion to the decorative layer facing the adhesion-promoting layer.
[0054] According to the invention, as an alternative, it is provided that the partial layer of the adhesion-promoting layer facing the first surface of the polypropylene film is based on a polyolefin, in particular on a low-molecular-weight, maleic acid-modified polyolefin.
[0055] According to the invention, as an alternative or in addition to the previously described embodiment, the partial layer of the adhesion-promoting layer facing the one or more decorative layers consists of a solvent-based polyurethane resin, which is based in particular on a polycarbonate.
[0056] The layer thickness of the one or more sub-layers of the adhesion-promoting layer is preferably in the range between 0.5 µm and 5 µm, in particular between 1 µm and 2 µm.
[0057] Furthermore, it is also possible for the adhesion-promoting layer and / or the two or more sublayers of the adhesion-promoting layer to each consist of a varnish containing fillers. The proportion of fillers in the dry mass of the varnish preferably varies between the sublayers in order to create a corresponding mechanical adaptation of the properties of the polypropylene film and the decorative layer, and also to improve the storability of the transfer film in roll form.
[0058] The filler content is preferably between 0 wt.% and 15 wt.%, preferably between 0.1 wt.% and 10 wt.%, in each case based on the dry mass of the paint used.
[0059] It is preferred if the partial layer of the adhesion-promoting layer facing the first surface of the polypropylene film has a filler content that is at least 10 wt.% higher, based on the total weight of the solid components of the adhesion-promoting layer, than the partial layer of the adhesion-promoting layer facing the one or more decorative layers. It has been shown that the advantages described above can be achieved particularly reliably in this way.
[0060] The one or more decorative layers of the transfer film are in particular selected from: lacquer layer containing pigments and / or fillers, lacquer layer containing pigments and / or dyes, metal layer, layer containing binders and optically variable pigments, in particular interference layer pigments and / or liquid crystal pigments, magnetically alignable pigments, layer containing binders and metal pigments, layer containing thermochromic pigments and / or dyes, layer containing luminescent dyes and / or pigments, layer containing phosphorescent dyes and / or pigments, and / or lacquer layer with a molded surface relief.
[0061] In the case of a metal layer, it is advantageous to apply this metal layer by vapor deposition, physical vapor deposition (PVD), chemical vapor deposition (CVD), and / or sputtering. Different decorative layers can also consist of different, and especially differently colored, metals.
[0062] Metal layers are preferably applied over a clear coat or a pigment-containing lacquer layer. It is then advantageous to apply an additional lacquer layer to the metal layer as a metal adhesion promoter to improve the adhesion of subsequent layers.
[0063] It is also possible that any of the decorative layers described above can be combined with each other in the decorative layer structure of the transfer film.
[0064] The decorative layers can each cover the entire surface or only partially. If several decorative layers are each partially present, individual decorative elements in the decorative layers can be arranged next to one another, in particular directly adjacent to one another, or at least partially overlapping. It is also possible for a partial decorative layer to be arranged on a full-surface decorative layer, with the full-surface decorative layer serving as a background or substrate for the partial decorative layer, which contrasts particularly with the partial decorative layer in terms of color and / or brightness and / or reflectivity and / or roughness.
[0065] It is also possible for the polypropylene film to form part of the resulting decoration by combining the color and / or brightness and / or reflectivity and / or roughness of the polypropylene film with the decorative layers arranged thereon. The polypropylene film can be transparent, translucent, or opaque and / or colored with dyes and / or pigments. In particular, the polypropylene film forms a background or substrate for the decorative layers, contrasting particularly with the decorative layers in terms of color and / or brightness and / or reflectivity and / or roughness.
[0066] The decorative elements can be offset from one another or overlapped when viewed from above. However, the decorative elements can also be arranged side by side when viewed from above.
[0067] The decorative elements can also form one or more motifs. Within the meaning of the invention, a motif can be, for example, a graphically designed outline, a figurative representation, an image, a visually recognizable design element, a symbol, a logo, a portrait, a pattern, an alphanumeric character, a code, a code pattern, a cryptographic pattern, a text, a color design, and the like. The motif can also be personalized.
[0068] For the purposes of the invention, "individualized" means, in particular, that the print comprises information that is unique for each individual print, such as unique serial numbers. "Individualized" also means, in particular, that the print comprises information that is identical for a group of prints but unique for each group of prints, such as a batch number. Reference to "print" in the following can refer to an individualized print or a non-individualized print.
[0069] Advantageously, the decorative elements are arranged or formed on the decorative layers in such a way that, when viewed from above, at least some of the decorative elements or parts of some of the decorative elements form an overall motif. One or more of these decorative elements can be individualized or non-individualized. For example, one or more non-individualized decorative elements can complement one or more individualized decorative elements to form an overall motif. In particular, the prints can be arranged in register with one another.
[0070] Register or registration accuracy refers to the positioning accuracy of two or more elements and / or layers relative to one another. The registration accuracy should be within a specified tolerance and as small as possible. At the same time, the registration accuracy of several elements and / or layers relative to one another is an important feature for increasing process reliability. Precise positioning can be achieved, in particular, using sensor-based, preferably optically detectable, registration marks. These registration marks can either represent specific, separate elements, regions, or layers, or they can themselves be part of the elements, regions, or layers to be positioned.
[0071] It can also be provided that one or more transparent or translucent or transparently or translucently colored spacer layers with a thickness of, for example, 0.5 µm to 10 µm are arranged between two partial decorative layers with decorative elements, or between a partial decorative layer with decorative elements and a full-surface decorative layer with decorative elements, in order to create a three-dimensional depth effect of the decoration. In particular, shading and / or concealing effects of the decorative elements can be achieved, particularly depending on the illumination angle and / or viewing angle of the decorative layers.
[0072] In the case of a paint layer with a molded surface relief, it is advantageous to use an optically effective surface relief. The surface relief can be a surface relief that forms a structure that is optically effective and thus refractive, thus generating, in particular, a macroscopically optically and / or haptically perceptible motif. Furthermore, it is also possible for the surface relief to be a matte structure, which, for example, generates the visual impression of a matte metallic surface in combination with a corresponding metal layer in the decorative layer structure.
[0073] Furthermore, it is also possible for the surface relief to be a surface relief that forms lens structures, microlens structures, and / or freeform surface structures, which may further convey a three-dimensional impression of a motif. It is also possible for diffractive structures, such as holograms or similar, to be used as surface relief.
[0074] However, it is also possible that the molded surface relief is a surface relief that can only be perceived tactilely, for example, replicating a wooden decor or something similar.
[0075] Preferably, the transfer layer of the transfer film has a protective lacquer layer arranged on the side of the one or more decorative layers facing away from the first surface of the polypropylene film. By providing such a protective lacquer layer, the decorative layers and also the polypropylene film are protected from environmental influences, thus improving the durability of the decorated molded part and preventing delamination of the composite body.
[0076] The protective lacquer layer preferably has a thickness between 0.5 µm and 5 µm, in particular between 2 µm and 4 µm. Choosing such a layer thickness ensures that, on the one hand, appropriate protection is provided, while, on the other hand, the further processing of the composite body in steps b) and c) is still ensured, and that this does not lead to destruction of the protective lacquer layer or delamination at the interface between the protective lacquer layer and the decorative layer.
[0077] The protective lacquer layer preferably consists of a cross-linked lacquer, in particular of a polyacrylate, preferably a cross-linked polymethylacrylate system.
[0078] Furthermore, it is also possible for the protective lacquer layer to consist of two or more partial layers, which are printed in particular successive, full-surface or partial-surface prints. The two or more partial layers preferably each have a layer thickness between 0.5 µm and 5 µm. These partial layers are preferably made of a differently modified polyacrylate to ensure good adhesion between the protective lacquer layer and the decorative layer, as well as good protection against environmental influences.
[0079] The carrier layer of the transfer film preferably consists of a PET film (PET = polyethylene terephthalate), which in particular has a layer thickness between 9 µm and 100 µm, preferably between 23 µm and 75 µm.
[0080] According to a preferred embodiment, the forming of a composite body in step b) is carried out by thermoforming. The composite body is preferably heated to a temperature between 50°C and 190°C and then mechanically deformed.
[0081] Preferably, the forming is carried out by means of vacuum deep drawing or high-pressure forming.
[0082] It has proven particularly advantageous to form the composite body using vacuum deep drawing with compressed air support, preferably in a roll-to-roll process. Studies have shown that the composite body is preferably heated to a temperature between 140°C and 190°C, preferably using a negative pressure in the range of 0.4 bar to 0.8 bar, which preferably corresponds to a vacuum between 50% and 95%, in each case based on the maximum capacity of the vacuum pump of 0.85 bar, and the compressed air for the compressed air support has a pressure between 1 bar and 6 bar.
[0083] Similarly, vacuum deep drawing can be performed not in a roll-to-roll process, but in a sheet-to-sheet process. The process parameters are selected similarly. In particular, the individual sheets for the sheet-to-sheet process are divided from a film roll into corresponding individual sheets as panels using a cutting, laser cutting, milling, and / or punching process.
[0084] Studies have shown that by selecting the aforementioned parameters, a radius of 0.5 mm or larger can be achieved, and a local deformation of the surface of up to 300%, relative to the area before deformation, can also be achieved, depending on the component geometry. The process thus preferably allows a local area enlargement of up to 300% of the area, relative to the area before deformation.
[0085] Alternatively, the composite body can also be formed using high-pressure forming. Preferably, the composite body is heated to a temperature between 50°C and 180°C. Preferably, a vacuum within a range of 0.4 bar to 0.8 bar is used, which preferably corresponds to a vacuum between 50% and 95%, based on the maximum capacity of the vacuum pump of 0.85 bar, and the compressed air pressure is selected between 20 bar and 200 bar. Studies have shown that, by using the aforementioned process parameters, radii of up to 0.2 mm or larger can be achieved, and local deformation of the surface of up to 300%, based on the surface size before deformation, can be achieved, depending on the component geometry.
[0086] According to a preferred embodiment, a plastic containing or consisting of polypropylene is used as the plastic in step c). This ensures that, due to the achievable match between the mechanical and thermal properties of the polypropylene film and the injection-molding material, subsequent delamination of the molded part at the layer boundary between the polypropylene film and the injection-molded part is avoided as far as possible, and, furthermore, particularly good adhesion between the injection-molded part and the polypropylene film is achieved by carrying out step c). This is because, due to the matching material class, a particularly intimate material bond is achieved when the layer boundary is melted accordingly during step c).
[0087] It is further advantageous that a second surface of the polypropylene film, which is opposite the first surface of the polypropylene film, is bonded at least partially to the plastic material in step c) to form a monolithic laminate body. A monolithic laminate body is understood here to be a laminate body in which the adjacent layers are joined by "welding" the layer boundary rather than by using an adhesive layer. This is achieved by melting the adjacent layers.
[0088] In step c), it is particularly advantageous to use polypropylene or modified polypropylene as the plastic, which has comparable thermal and mechanical properties to those already described above with regard to the polypropylene film.
[0089] It is also possible for the plastic material to form part of the resulting decoration by combining the color and / or brightness of the plastic material with the decorative layers arranged thereon and / or the associated polypropylene film. The plastic material can be transparent, translucent, or opaque and / or colored with dyes and / or pigments. In particular, the plastic material forms a background or substrate for the decorative layers and / or the associated polypropylene film, which contrasts particularly with the decorative layers and / or the associated polypropylene film in terms of color and / or brightness and / or reflectivity and / or roughness.
[0090] It is preferred if the plastic material and the associated polypropylene film have the same or very similar optical properties with regard to refractive index and / or transparency and / or opacity and / or color and / or reflectivity and / or clarity.
[0091] For the plastic material in step c), polypropylenes and / or plastics containing polypropylene modified with various fillers and / or other additives can preferably be used. Examples include: Polypropylene with a 20 wt.% talc filler content, based on the total weight of the solid components of the plastic material (e.g. Hifax TRC 134P 3004 or Hostacom TRC 352N from LyondellBasell) Polypropylene copolymer with a 5 wt.% talc filler content, based on the total weight of the solid components of the plastic material (e.g. TKC 2007N from LyondellBasell) Polypropylene-TPO compound (TPO = olefin-based thermoplastic elastomers) with a 16 wt.% mineral filler content, based on the total weight of the solid components of the plastic material (e.g. EKC 330N from LyondellBasell) Polypropylene-TPO compound (TPO = olefin-based thermoplastic elastomers) (e.g. BMU 141 from Exxon Mobile)
[0092] Preferably, in step c), the plastic is heated to a melt temperature between 170°C and 290°C. This ensures that the layer boundary between the injection-molding material and the polypropylene film melts accordingly, thus creating a well-adhering bond between these two materials. Preferably, the injection-molding tool is heated or preheated to a tool temperature between 15°C and 80°C.
[0093] Preferably, in step c) the plastic material is back-injected and / or over-injected and / or over-injected in a layer thickness between 500 µm and 5 mm, preferably between 1 mm and 3 mm.
[0094] According to a further preferred embodiment of the invention, the composite body is processed in step b) by means of a cutting, laser cutting, milling and / or punching process and thus, for example, the composite body in the form of a film roll is divided into corresponding individual blanks, which are then further processed in step c) to produce the decorated molded part.
[0095] The decorated molded bodies are primarily used in the automotive sector as interior and / or exterior components of vehicles. Further applications for the decorated molded bodies include, in particular, the decoration of housings or housing elements for electronic devices and / or electrical appliances for use in households, industry, or medicine.
[0096] The abbreviation "wt%" used in the present patent application refers to the content "percent by weight".
[0097] In the following, the invention is explained by way of example using several embodiments with the aid of the accompanying drawings. Fig. 1 shows a process flow for producing a decorated molded part. Fig. 2 shows a schematic representation of the layer structure of a transfer film. Fig. 3 shows the schematic layer structure of a composite body. Fig. 4 shows the schematic layer structure of a formed composite body. Fig. 5 shows the schematic layer structure of a composite body machined by an injection molding process. Fig. 6 and Fig. 7 show the layer structure of composite bodies which were further coated after processing in an injection molding process.
[0098] Fig. 1 illustrates a basic process for producing a decorated molded part. This process comprises several production steps (71 to 77).
[0099] In production step 71, a transfer film 1 is produced. It is also possible to omit production step 71 and to use a correspondingly prefabricated transfer film 1.
[0100] The transfer film 1 is preferably as in Fig. 2 clearly structured: The transfer film has a carrier layer 10, an optional release layer 11, an optional protective lacquer layer 12, one or more decorative layers 13, and an optional adhesion-promoting layer 14.
[0101] The carrier layer 10 consists of a plastic film or a layered composite of one or more plastic and / or paper films. Furthermore, the carrier layer 10 can also have corresponding release layers on its upper side to enable the transfer film 1 to be provided in the form of a film roll.
[0102] The carrier layer 10 preferably consists of a PET film (PET = polyethylene terephthalate) with a layer thickness between 9 µm and 100 µm, preferably between 23 µm and 75 µm.
[0103] A release layer 11 is then preferably printed onto the carrier layer 10. The release layer 11 is preferably a wax-based layer, which improves the detachment of the carrier layer from the subsequent layers 12 to 14 of the transfer film 1, which is referred to below as the transfer layer 15, during the transfer process. The release layer 11 can also be omitted if the material properties of the carrier layer 10 and the uppermost layer of the transfer layer 15 are adjusted accordingly.
[0104] The layers of the transfer layer 15 of the transfer film are then applied sequentially to the carrier layer 10. This application is preferably carried out using a printing process, in particular gravure printing and / or screen printing. Application by slot casting, flexographic printing, or inkjet printing is also possible.
[0105] The protective lacquer layer 12 preferably has a layer thickness between 0.5 µm and 5 µm, in particular between 2 µm and 4 µm. The protective lacquer layer 12 preferably consists of two or more partial layers, which are printed successively.
[0106] The following procedure is particularly advantageous: First, a layer of polyacrylate, in particular a cross-linked polyacrylate system, is printed on. For this purpose, for example, an aliphatic polymethyl methacrylate is reacted with a reactive component, e.g. an aliphatic polyisocyanate. The polyacrylate reacts in an exothermic polyadditive reaction with the reactive cross-linking component. This lacquer is then preferably provided with fillers, preferably with a filler content in the dry mass in a range of 0.1 wt.% to 10 wt.% This lacquer is then printed on in a layer thickness of between 2 µm and 4 µm. Subsequently, a clear, transparent lacquer layer is applied, which in turn consists of a polyacrylate and has a thickness of 1 µm. Subsequently, a further lacquer layer can be applied, which in turn consists of a polyacrylate and has a thickness of approx. 1 µm.
[0107] Then one or more decorative layers are applied. The decorative layer can consist of one or more decorative layers, of which Fig. 2 the decorative layer 13 is shown.
[0108] The decorative layers, and thus the decorative layer 13, are preferably a lacquer layer containing pigments and / or dyes. Furthermore, the decorative layer can also be a metal layer, whereby different decorative layers can also consist of different, and in particular differently colored, metals. Furthermore, the decorative layer can also consist of a layer with one or more binders and metal pigments, optically variable pigments, magnetically alignable pigments, thermochromic pigments and / or dyes, luminescent dyes and / or pigments, phosphorescent dyes and / or pigments.Furthermore, it is also possible for the decorative layer 13 to consist of a lacquer layer with a molded surface relief, in particular the surface relief of a matte structure, a lens structure, a microlens structure, a refractive structure, a diffractive structure, or a haptically perceptible structure. All of these layers can be provided over the entire surface or partially and in a patterned manner in any combination in the layer structure of the transfer layer 15 in order to achieve the desired optical and / or haptic result.
[0109] The decorative layer 13 preferably consists of a polyacrylate, which is provided with appropriate pigments and / or dyes as described above. This polyacrylate can be crosslinked or uncrosslinked. In this case, the layer thickness of the decorative layer 13 is in the range between 4 µm and 8 µm.
[0110] If metal layers are used as decorative layer 13, these metal layers are preferably applied by vapor deposition, physical vapor deposition (PVD), chemical vapor deposition (CVD) and / or sputtering.
[0111] Metal layers are preferably applied over a clear coat or a pigment-containing lacquer layer. It is then advantageous to apply an additional lacquer layer to the metal layer as a metal adhesion promoter to improve the adhesion of subsequent layers.
[0112] Afterwards, preferably a Fig. 2 not shown, clear coat layer, which consists of a mixture of polyacrylate and polyvinyl chloride and has a thickness between 1 µm and 2 µm.
[0113] Next, the adhesion-promoting layer 14 is applied. The adhesion-promoting layer 14 preferably consists of one or more sublayers.
[0114] Thus, a layer consisting of a solvent-based polyurethane resin based on a polycarbonate is preferably applied as the first partial layer. The solids content is preferably 35 wt.%, and the dynamic viscosity is preferably between 0.5 mPa s and 100 mPa s, in particular between 10 mPa s and 50 mPa s at approximately 25°C. The viscosity was determined in particular according to the method described in DIN EN ISO 3219:1994-10 ("Plastics - Polymers / resins in liquid, emulsified, or dispersed state - Determination of viscosity using a rotational viscometer at a defined velocity gradient" edition date 1994-10), for example using a HAAKE Viscotester®< VT550 (Thermo Fischer Scientific Inc., Waltham, MA, USA), more preferably using a cylinder measuring device NV and a measuring cup NV.This coating can be provided with fillers, preferably with a filler content of 0.1 wt.% to 10 wt.% in the dry matter. The thickness of this layer is preferably in the range of 1 µm to 2 µm.
[0115] A second partial coat is then applied to create the final bond to the polypropylene film. This coat is preferably based on a low-molecular-weight, maleic acid-modified polyolefin (glass transition temperature Tg = 100°C). This coat can also be filled, with the filler content of the dry mass preferably being between 1% and 12% by weight. The thickness of this coat is preferably in the range of approximately 1 µm.
[0116] The transfer film 1 produced in production step 71 is subsequently used to produce a pre-product in the form of a composite body 2, the layer structure of which is Fig. 3 is shown.
[0117] The composite body 2 comprises a polypropylene film (20) with a first surface (21) and a second surface (22) opposite thereto. The transfer layer (15) of the transfer films (1) is applied to the first surface (21) of the polypropylene film (20), which, as shown in Fig. 3 shown, which has a decorative layer 13.
[0118] The polypropylene film 20 preferably has a layer thickness between 5 µm and 3 mm, more preferably between 20 µm and 1000 µm.
[0119] The polypropylene film 20 is preferably formulated as described below: The procedure for producing the precursor in the form of the composite body 2 is as follows: In an optional production step 72, the polypropylene film 20, preferably in the form of a film roll, is subjected to a pretreatment. This pretreatment improves the adhesion of the first surface 21 of the polypropylene film 20. This pretreatment preferably includes flame treatment and / or one or more cleaning processes.
[0120] For example, the following adhesion issue exists on surfaces 21 and 22 of the polypropylene film: Polypropylene is a plastic with low surface energy. Its surface energy lies between 29 dyn / cm and 36 dyn / cm, or mN / m (millinewtons per meter). Achieving a sufficient degree of adhesion on materials with low surface energy, such as polypropylene, is extremely difficult due to their smoothness. Therefore, this adhesion issue leads to printed inks being rubbed off or the ink not adhering to the surface. It can also cause adhesion problems when bonding to other layers or between the surface and any sealants applied to it.For example, polyolefins such as polypropylene have a non-polar surface and low surface energy, which makes them unsuitable for printing, binding, coating or painting unless environmentally harmful and highly labor-intensive processes are used.
[0121] The surface tension and comparative surface energy of a material are crucial for the potential for adhesion between the coating and the material itself. Because a solid has a high degree of surface energy compared to the surface tension of a liquid, the increased molecular attraction binds the adhesive, ink, and paint together, resulting in excellent bond strength. Accordingly, when the surface tension of the solid is lower than that of the liquid, the attractive forces are weakened, resulting in the repellency of the coating.
[0122] Thus, the pretreatment described below and also the structure of the adhesion-promoting layer 14 already described above ensure that the surface energy of the first surface 21 is at least 5 mN / m (dyn / cm) above the surface tension of the material lying on the first surface 21, here the lowest partial layer of the adhesion-promoting layer 14.
[0123] To pretreat the first surface of the polypropylene film 20, flame treatment, in particular in the form of corona and / or plasma surface activation and / or one or more cleaning processes, is preferably used. Such flame treatment allows the surface to be gently activated. With the flame intensity, the oxygen content and the polar functional groups on the material surface increase, while the roughness remains virtually unchanged. Therefore, flame treatment creates polar functional groups that are firmly bonded to the base material. Cleaning processes are also used to reduce the additive content on the plastic surface. Studies have shown that with increasing additive content on the plastic surface, paint adhesion decreases, thus significantly reducing the adhesive properties of the first surface 21.The cleaning methods used include power washing, CO2 snow jet cleaning, and / or water-isopropanol / ultrasonic cleaning. Furthermore, the use of a chlorinated cleaning agent is preferred to remove typical additives (antioxidants, waxes, antistatic agents, etc.). This additional cleaning preferably takes place before flame treatment.
[0124] It has proven particularly advantageous that as little time as possible elapses between the pretreatment in production step 72 and the application of the transfer layer 15 to the polypropylene film 20 in production step 73, thus ensuring that these two production steps follow one another as closely as possible. This is because the polar functional groups generated by the flame treatment significantly reduce over time, and additive substances migrate to the surface 21 from the interior of the polypropylene film 20, thereby deteriorating the adhesive properties of the first surface over time.
[0125] Investigations have shown that, if possible, no more than 24 hours, preferably no more than 6 hours, and particularly preferably no more than 10 minutes should elapse between the pretreatment in production step 72 and the application of the transfer layer 15 in production step 73.
[0126] In production step 73, the transfer layer 15 of the transfer film 1 is applied to the first surface 21 of the polypropylene film 20.
[0127] To apply the transfer layer 15, the following procedure is preferably followed: For this purpose, the transfer film 1 is thermally laminated onto the first surface 21 of the polypropylene film 20 and then the carrier layer 10 of the transfer film 1 is removed.
[0128] Thermal lamination is preferably carried out by passing the transfer films 1 and the polypropylene film 20 through a nip of a heated laminating roller and a particularly cooled counterpressure roller, and thereby bonding them to form a composite body 2 using heat and pressure. Thermal lamination is preferably carried out at a temperature between 120°C and 180°C.
[0129] In the subsequent production step 74, the composite body 2 is formed so that, as in Fig. 4indicated, a correspondingly formed composite body 3 is present.
[0130] The forming of the composite body 2 preferably takes place using a thermoforming process. Preferably, the forming takes place by vacuum deep drawing in a temperature range between 140°C and 190°C. The composite body 2 is preferably heated to such a temperature using quartz radiators, but also using other energy sources such as ceramic or infrared radiators, and then three-dimensionally formed by vacuum deep drawing, preferably with the assistance of compressed air. Preferably, a negative pressure in a range of 0.4 bar to 0.8 bar is used, which preferably corresponds to a vacuum between 50% and 95%, in each case based on the maximum capacity of the vacuum pump of 0.85 bar, and the compressed air pressure is between 1 bar and 6 bar.
[0131] As an alternative to vacuum deep drawing, it is also particularly advantageous to perform the forming process using high-pressure forming. Preferably, a film temperature between 50°C and 180°C, a vacuum in the range of 0.4 bar to 0.8 bar, which preferably corresponds to a vacuum between 50% and 95%, in each case based on the maximum capacity of the vacuum pump of 0.85 bar, and a compressed air pressure between 20 bar and 200 bar are used.
[0132] In the subsequent production step 75, the composite body is shaped accordingly by cutting or punching to achieve the desired shape of the decorated molded part. It is also possible for production step 75 to occur before production step 74. Furthermore, with the appropriate design of the polypropylene film, it is also possible to omit production step 75.
[0133] In the production step 76, the formed composite body 3 is then placed in an injection molding tool and back-injected and / or over-injected and / or over-injected with a plastic material, so that, for example, the Fig. 5 shown, back-injected composite body 4 results.
[0134] The injection molding process is preferably carried out using the following process parameters: Melt temperature of the plastic material: 170°C to 290°C Mold temperature: 15°C to 80°C
[0135] The injection pressure is further used depending on the geometry of the decorated molded part and the plastic material used.
[0136] As already stated above, the plastic material used is preferably a plastic containing or consisting of polypropylene.
[0137] Particularly preferably, the plastic material is formulated as follows: For the plastic material in step c), polypropylenes and / or plastics containing polypropylene modified with various fillers and / or other additives can preferably be used. For example, these can be: Polypropylene with a talc content of 20 wt.%, based on the total weight of the solid components of the plastic material, as a filler (e.g. Hifax TRC 134P 3004 or Hostacom TRC 352N from LyondellBasell) Polypropylene copolymer with a talc content of 5 wt.%, based on the total weight of the solid components of the plastic material, as a filler (e.g. TKC 2007N from LyondellBasell) Polypropylene-TPO compound (TPO = olefin-based thermoplastic elastomers) with a mineral content of 16 wt.%, based on the total weight of the solid components of the plastic material, as a filler (e.g. EKC 330N from LyondellBasell) Polypropylene-TPO compound (TPO = olefin-based thermoplastic elastomers) (e.g. BMU 141 from Exxon Mobile)
[0138] In the subsequent functional process step 77, the composite body 4 is overcoated with one or more primer and / or protective lacquer layers, whereby the decorated molded part is then obtained.
[0139] Furthermore, it is also possible to dispense with the production step 77 and to use the composite body 4 already present after the production step 76 has been carried out as a decorated molded part.
[0140] Preferably, in production step 77, first, as in Fig. 6 shown, a primer layer 50 and thereon, as in Fig. 7 As shown, a protective lacquer layer 51 is applied. The primer layer 50 and the protective lacquer layer 51 are applied by flooding and / or by painting, in particular spray painting. Polyurethane and / or acrylate lacquers are preferably used as lacquers for the primer layer 50 and the protective lacquer layer 51.
[0141] Preferably, the paint compositions are formulated as follows: 20% to 90% by weight of at least one binder, for example polyurethane; 5% to 25% by weight of at least one co-binder, for example acrylate, propolymer; 1% to 10% by weight of a crosslinker; 0% to 10% by weight of at least one filler, for example Aerosil; 0% to 10% by weight of at least one additive; 10% to 50% by weight of at least one solvent, for example water, in each case based on the total weight of the coating composition. List of reference symbols
[0142] 1Transfer film 2Composite body 3Composite body 4Composite body 10Carrier layer 11Release layer 12Protective lacquer layer 13Decorative layer 14Adhesion promoter layer 15Transfer layer 20Polypropylene film 21First surface 22Second surface 40Plastic material 50Primer layer 51Protective lacquer layer
Claims
1. Method for producing a decorated moulding, wherein the following steps are carried out in the method: a) producing an intermediate product in the form of a composite body (2) by means of applying a transfer layer (15) of a transfer foil (1) to a first surface (21) of a polypropylene foil (20), wherein the transfer layer (15) of the transfer foil (1) comprises at least one decorative layer (13), b) forming the composite body (2) comprising the polypropylene foil (20) with the applied transfer layer (15) of the transfer foil (1), c) inserting the formed composite body (3) into an injection mould and back injecting and / or overmoulding and / or insert moulding the formed composite body (3) with a plastic material (40). characterised in that the transfer layer (15) of the transfer foil has an adhesive layer (14), which is arranged on the side of the one or more decorative layers (13) facing towards the first surface (21) of the polypropylene foil (20) and wherein the adhesive layer (14) consists of two or more partial layers, which are printed consecutively, wherein the partial layer of the adhesive layer (14), facing towards the first surface (21) of the polypropylene foil (20), is based on a polyolefin and / or wherein the partial layer of the adhesive layer (14), facing towards the one or more decorative layers (13), consists of a solvent-based polyurethane resin.
2. Method according to claim 1, characterised in that in step (a) before applying the transfer layer (15) of the transfer foil (1), the polypropylene foil (20) is pretreated, in particular wherein the first surface (21) of the polypropylene foil (20) is pretreated by means of a corona treatment and / or wherein the pretreatment takes place immediately before carrying out the application of the transfer layer (15), in particular no more than 24 hours pass between the pretreatment and the application.
3. Method according to one of the preceding claims, characterised in that in step a) the transfer foil (1) is thermo-laminated onto the first surface (21) of the polypropylene foil (20) and subsequently the support layer (10) is removed from the transfer foil (1).
4. Method according to one of the preceding claims, characterised in that in step b) the forming of the composite body takes place by means of a thermal method, by means of vacuum thermoforming and / or by means of highpressure forming.
5. Method according to one of the preceding claims, characterised in that in step b) the composite body (2) is heated to a temperature of between 50°C and 190°C.
6. Method according to one of the preceding claims, characterised in that in step c) a plastic containing or consisting of polypropylene is used as the plastic.
7. Method according to one of the preceding claims, characterised in that in step c) a second surface (22) of the polypropylene foil (20), which is opposite the first surface (21) of the polypropylene foil, is at least partially connected to the plastic material (40) to form a monolithic laminated body.
8. Method according to one of the preceding claims, characterised in that the polypropylene foil (20) has a layer thickness of between 5 µm and 3 mm, and / or the polypropylene foil (20) has a tensile modulus of elasticity of between 1000 MPa and 1400 MPa, determined according to DIN EN ISO 527 section 1 to section 3.
9. Method according to one of the preceding claims, characterised in that the transfer layer (15) of the transfer foil (1) has a protective lacquer layer (12) which is arranged on the side of one or more decorative layers (13) facing away from the first surface (21) of the polypropylene foil (20), wherein the protective lacquer layer (12) consists of a crosslinked lacquer, in particular of a polyacrylate, and / or wherein the protective lacquer layer (12) consists of two or more partial layers, wherein the two or more partial layers each consist of a differently modified polyacrylate.
10. Method according to claim 1, characterised in that the partial layer of the adhesive layer (14) facing towards the first surface (21) of the polypropylene foil (20) is based on a low-molecular-weight, maleic-acid-modified polyolefin, and / or wherein the partial layer of the adhesive layer (14) facing towards the one or more decorative layers (13) is based on a polycarbonate, wherein the one or more partial layers of the adhesive layer (14) each have a layer thickness in the range between 0.5 µm and 5 µm.
11. Method according to claim 10, characterised in that the two or more partial layers of the adhesive layer (14) each consist of a lacquer, which is provided with filler materials, wherein the proportion of filler materials in the dry matter between the partial layers is different, in particular the partial layer of the adhesive layer facing towards the first surface (21) of the polypropylene foil (20) has an at least 10 wt. -% higher filler material proportion than the partial layer of the adhesive layer facing towards the one or more decorative layers (13).
12. Method according to one of the preceding claims, characterised in that after carrying out step c), the composite body (4) formed by back injection and / or overmoulding and / or insert moulding is, in a step d), completely or partially coated with one or more primer layers and one or more lacquer layers, wherein the primer layer is completely or partially applied onto the protective lacquer layer (12) of the composite body (4) formed by back injection and / or overmoulding and / or insert moulding, and the protective lacquer layer (51) is completely or partially applied onto the primer layer (50).
13. Decorated moulding (6), produced by a method according to one of the preceding claims, wherein the decorated moulding (6) has a composite body (4) formed by back injection and / or overmoulding and / or insert moulding with a plastic material (40), which has a polypropylene foil (20) having a transfer layer (15) of a transfer foil (1) applied onto a first surface (21), which comprises at least one decorative layer (13), wherein the transfer layer (15) of the transfer foil has an adhesive layer (14) which is arranged on the side of the one or more decorative layers (13) facing towards the first surface (21) of the polypropylene foil (20) and wherein the adhesive layer (14) consists of two or more partial layers which are printed consecutively, wherein the partial layer of the adhesive layer (14) facing towards the first surface (21) of the polypropylene foil (20) is based on a polyolefin and / or wherein the partial layer of the adhesive layer (14) facing towards the one or more decorative layers (13) consists of a solvent-based polyurethane resin.
14. Use of a transfer foil (1) to produce a decorated moulding (6) according to the preceding claim.