METHOD FOR PROVIDING AN ELECTRODE FILM FOR PRODUCEING A LITHIUM-ION ACCUMULATOR AND METHOD FOR PRODUCEING A LITHIUM-ION ACCUMULATOR

DE502020009442D1Active Publication Date: 2024-10-31PLASMATREAT GMBH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
DE502020009442
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-08-02
Filing Date
2020-07-30
Publication Date
2024-10-31
Estimated Expiration
2040-07-30

AI Technical Summary

Technical Problem

The production of lithium-ion batteries is time-consuming due to the slow penetration of electrolyte into electrode materials, and existing plasma treatment methods require complex low-pressure chambers, which are not suitable for continuous operation.

Method used

Applying an atmospheric plasma jet to the electrode material coating, generated with a plasma nozzle through high-frequency electrical discharges, to enhance electrolyte penetration without the need for vacuum environments.

Benefits of technology

This method significantly reduces the time required for electrode material saturation with electrolyte, allowing for more efficient lithium-ion battery production without the complexity and expense of vacuum systems.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The invention relates to a method for providing an electrode foil for producing a lithium-ion rechargeable battery, in which a metal foil with a coating of electrode material is provided, and in which the coating of electrode material is plasma-treated. Furthermore, the invention relates to a method for producing a lithium-ion rechargeable battery, in which a first electrode foil is provided for the negative electrode and a second electrode foil is provided for the positive electrode, in which the first and second electrode foils are arranged one above the other to form a foil stack with a separator layer interposed, and in which the stack is impregnated with a liquid electrolyte.

[0002] In the manufacture of lithium-ion batteries, for example, it is known to arrange an aluminum foil coated with lithium nickel manganese cobalt oxides for the positive electrode and a graphite coated copper foil for the negative electrode with an interposition of a separator layer in the form of a polypropylene mesh on top of each other to form a foil stack, to roll the foil stack up into a cylindrical roll or to unfold it into a rectangular block, to arrange the roll or block in a housing and to fill an electrolyte, for example lithium salts dissolved in ethylene carbonate, into the housing in order to impregnate the electrode material, i.e. the lithium nickel manganese cobalt oxide coating or graphite coating, with the electrolyte.

[0003] To produce high-performance and long-lasting batteries, it is important that the electrode material is as completely permeated as possible by the electrolyte used, allowing the lithium ions in the battery to move freely. Therefore, impregnating the electrode material with the electrolyte must be carried out with particular care and can be time-consuming during production. However, this makes the production of lithium-ion batteries relatively time-consuming, and there is a need to shorten battery production times without compromising battery performance.

[0004] To reduce the time required to soak the electrode material with electrolyte, attempts were made to treat the electrode material in low-pressure chambers using inductively or capacitively coupled plasma. These experiments were based on the idea of ​​generating a plasma in the pores of the typically porous electrode material coating, thereby increasing the surface energy to such an extent that wetting with the electrolyte would be improved.

[0005] However, this technique is quite complex due to the low-pressure chambers required and does not allow for continuous operation, which is preferred from a process engineering perspective. Furthermore, while low-pressure plasma treatment did indeed shorten the time required to completely soak the electrode material with the electrolyte (soaking time), this time advantage was partially offset by the process of transferring the electrode material into and out of the low-pressure chamber.

[0006] JP 2006 108047 A discloses a method for producing a battery in which a glow discharge is generated in a gas volume at the positive or negative electrode. Furthermore, JP H04 28174 A discloses a method in which a carbon material for an electrode is plasma-treated.

[0007] US 2013 / 183590 discloses an electrode for a lithium-ion battery and a method for its production. DE 10 2016 125 699 A1 discloses a device for generating an atmospheric plasma jet and a method for treating a material. KR 101 664 541 B1 and KR 2015 / 0122297 A disclose a device for generating an atmospheric plasma jet.

[0008] Against this background, the present invention is based on the object of providing a more efficient method for providing an electrode foil for producing a lithium-ion battery and a more efficient method for producing a lithium-ion battery.

[0009] This object is achieved according to the invention in a method for providing an electrode foil for producing a lithium-ion accumulator, in which a metal foil with a coating of electrode material is provided and in which the coating of electrode material is plasma-treated, in that the coating of electrode material is plasma-treated by exposing the coating to an atmospheric plasma jet, wherein the atmospheric plasma jet is generated with a plasma nozzle.

[0010] The investigations underlying this invention have shown that this method can achieve a considerable time saving effect when impregnating the electrode material with electrolyte.

[0011] This is surprising, as experts have previously assumed that, to achieve significant time savings during electrolyte impregnation, the electrode material must be plasma-treated essentially across its entire volume, i.e., across the entire thickness of the coating. Since the counterpressure of a gas contained in the pores of the electrode material at atmospheric pressure would counteract plasma penetration and therefore only allow a relatively superficial plasma treatment, it has previously been assumed that only vacuum plasma treatment would produce the desired results.

[0012] However, it has now been shown that a relatively superficial treatment of the electrode material using an atmospheric plasma jet is sufficient to have a significant effect on the electrode material's ability to absorb the electrolyte and thus to achieve the desired time-saving effects in the production of a lithium-ion battery without complex and expensive vacuum environments.

[0013] The treatment of electrode material with an atmospheric plasma jet to reduce the time required for the electrode material to become completely saturated with the electrolyte represents a complete departure from previous considerations.

[0014] The above-mentioned object is further achieved according to the invention in a method for producing a lithium-ion accumulator, in which a first electrode foil for the negative electrode and a second electrode foil for the positive electrode are provided, in which the first and the second electrode foil are arranged one above the other to form a foil stack with the interposition of a separator layer and in which the foil stack is impregnated with a liquid electrolyte, in that the first and / or the second electrode foil are provided using the method described above.

[0015] In other words, in the method for producing a lithium-ion accumulator, a first electrode foil is provided for the negative electrode and a second electrode foil is provided for the positive electrode, the first and second electrode foils are arranged one above the other to form a foil stack with a separator layer in between, and the foil stack is impregnated with a liquid electrolyte, wherein the first and / or second electrode foils are provided by providing a respective metal foil with a respective coating of electrode material and the coating of electrode material is plasma-treated by applying an atmospheric plasma jet.

[0016] The first electrode foil for the negative electrode comprises, in particular, a metal foil with a coating of electrode material for the negative electrode, and the second electrode foil for the positive electrode comprises, in particular, a metal foil with a coating of electrode material for the positive electrode. A plastic mesh, such as a polypropylene mesh, can be used as the separator layer. A lithium salt, such as lithium hexafluorophosphate (LiPF 6 ), lithium tetrafluoroborate (LiBF 4 ), or lithium bis(oxalato)borate (LiBOB), dissolved in an anhydrous aprotic solvent, such as ethylene carbonate, can be used as the electrolyte.

[0017] In addition to the first and second electrode foils and the separator layer, the foil stack may comprise further layers, in particular an insulator layer, in order to avoid undesired contact between the electrode foils and thus short circuits when the foil stack is rolled up or folded.

[0018] Before impregnating the stack with the liquid electrolyte, the foil stack can in particular be rolled up or folded and preferably inserted into a battery housing.

[0019] In the following, various embodiments of the previously described method for providing an electrode foil and of the previously described method for producing a lithium-ion battery are described, wherein the individual embodiments are applicable both to the method for providing an electrode foil for producing a lithium-ion battery and to the method for producing a lithium-ion battery and can also be combined with one another.

[0020] In a first embodiment, the metal foil with the coating of electrode material is provided by applying electrode material to the metal foil, in particular in the form of a water-based suspension, and the electrode material applied to the metal foil is dried and rolled, in particular calendered, wherein the coating of electrode material is plasma-treated after rolling, in particular calendering.

[0021] To obtain an electrode foil with a uniformly thin coating of electrode material, the electrode material applied to the metal foil can be calendered. In this case, the plasma treatment with the atmospheric plasma jet is preferably carried out after such calendering, since calendering after the plasma treatment would lead to a weakening of the surface treatment achieved by the plasma treatment.

[0022] In an alternative embodiment, the plasma treatment can also be performed before calendering. Since the electrode material is still unpressed before calendering, this can, in some cases, achieve a plasma treatment that penetrates deeper into the electrode material coating.

[0023] If the plasma treatment is carried out after rolling, in particular calendering, it is not absolutely necessary for the plasma treatment to be carried out immediately after rolling or calendering; rather, further process steps can be carried out between rolling or calendering and the plasma treatment, for example further drying, such as vacuum drying, of the coating of electrode material.

[0024] The electrode material can be applied to the metal foil, for example, in the form of a slurry. For this purpose, a mixture, especially a suspension, of the actual electrode material and a liquid is applied to the metal foil. The liquid is removed, for example, by drying, leaving a coating of electrode material on the metal foil.

[0025] In another embodiment, the electrode material coating is porous. This allows the electrolyte to penetrate the electrode material coating well, allowing the effect of the plasma treatment to take effect using an atmospheric plasma jet.

[0026] In one embodiment, an aluminum foil or a copper foil is used as the metal foil. An aluminum foil is used in particular to provide an electrode foil for the positive electrode, i.e., the cathode during the discharge process. A copper foil is used in particular to provide an electrode foil for the negative electrode, i.e., the anode during the discharge process.

[0027] In a further embodiment, the coating of electrode material contains one or more of the following compounds or preferably consists of at least 90 wt.% thereof: lithium cobalt(III) oxide (LiCoO 2 ), lithium nickel manganese cobalt oxides (e.g., LiNi x Co y Mn z O 2 ), Li spinels (e.g., LiMn 2 O 4 ), LiFePO 4 . These compounds are suitable as electrode material for the positive electrode.

[0028] In a further embodiment, the electrode material coating contains one or more of the following compounds, or preferably consists of at least 90 wt.% of them: graphite, other Li-intercalating carbons, nanocrystalline amorphous silicon, lithium titanates (e.g., Li 4 Ti 5 O 12 ), tin dioxide (SnO 2 ). These compounds are suitable as electrode material for the negative electrode.

[0029] The coating of electrode material may further comprise a binder, for example polyvinylidene fluoride or carboxymethylcellulose and / or styrene-butadiene rubber.

[0030] According to the invention, the atmospheric plasma jet is generated with a plasma nozzle, preferably by high-frequency electrical, in particular arc-like, discharges between electrodes in a working gas stream. The plasma nozzle has, in particular, a working gas inlet and a nozzle opening from which the plasma jet emerges.

[0031] By generating the plasma jet through high-frequency electrical discharge between electrodes in a working gas stream, a reactive yet surface-protecting plasma beam is created, allowing the coating of electrode material to be effectively plasma-treated without damaging it. The reactivity of the plasma beam is high enough to achieve sufficient plasma treatment of the coating. By directing the plasma beam onto the coating, meaning the reactive species in the plasma beam hit the coating at a relative velocity, a relatively good penetration depth of the plasma beam into the coating is achieved despite the superficial treatment at atmospheric pressure, so that the coating is plasma-treated at least starting from the surface down to a certain depth.

[0032] In a further embodiment, a plasma nozzle with a nozzle arrangement is used to generate the atmospheric plasma jet, which divides the plasma jet generated by the plasma nozzle into several partial jets emerging from several openings of the nozzle arrangement. In particular, the closer nozzle openings can be arranged along a channel of the nozzle arrangement. A suitable nozzle arrangement is known, for example, from DE 10 2016 125 699 A1. By using a plasma nozzle with such a nozzle arrangement, a larger area of ​​the coating made of electrode material can be treated simultaneously, so that the plasma treatment can be carried out more efficiently and, in particular, with a smaller number of plasma nozzles. In particular, a wider strip on the surface of the coating can be treated with a relative movement between the nozzle arrangement and the coating made of electrode material.It was found that even if the plasma beam is divided into partial beams, sufficient treatment of the electrode material coating can still be achieved.

[0033] Further features and advantages of the invention will become apparent from the following description of embodiments, with reference to the accompanying drawings. In the drawing show

[0034] Fig. 1a-e shows an embodiment of the method for providing an electrode foil for producing a lithium-ion battery, Fig. 2a shows an embodiment of the method for producing a lithium-ion battery, Fig. 3 shows an embodiment of the method from Fig. 1 usable plasma nozzle, Fig. 4 another for the process from Fig. 1usable plasma nozzle with nozzle arrangement, Fig. 5a-c another embodiment of the method for providing an electrode foil for producing a lithium-ion battery and Fig. 6a-c another embodiment of the method for producing a lithium-ion battery.

[0035] The Figures 1a-e show an embodiment of the method for providing an electrode foil for producing a lithium-ion battery in a schematic representation.

[0036] The Figures 1a-d show the preparation of a metal foil with a coating of electrode material. For this purpose, the Figure 1a In the first step shown, a metal foil 2 is first provided and coated with electrode material 4.

[0037] If an electrode foil for the positive electrode is to be produced, the metal foil 2 can in particular be an aluminum foil and the electrode material can in particular contain one or more of the following compounds or preferably consist of at least 90 wt.% thereof: lithium cobalt(III) oxide (LiCoOz), lithium nickel manganese cobalt oxides (e.g. LiNi x Co y Mn z O2), Li spinels (e.g. LiMn 2 O 4 ), LiFePO 4 .

[0038] If an electrode foil for the negative electrode is to be produced, the metal foil 2 can in particular be a copper foil and the electrode material 4 can in particular contain one or more of the following compounds or preferably consist of at least 90 wt.% thereof: graphite, other Li-intercalating carbons, nanocrystalline, amorphous silicon, lithium titanates (e.g. Li 4 Ti 5 O 12 ), tin dioxide (SnO 2 ).

[0039] The electrode material 4 can be as in Figure 1a illustrated as a slurry in the form of an aqueous suspension applied to the metal foil. Such a slurry contains the actual electrode material as well as a liquid in which the electrode material is suspended. The application of the electrode material 4 as a slurry is described in Figure 1a schematically illustrated by an application container 6, beneath which the metal foil 2 is moved (arrow 8). However, any other suitable coating method may also be used.

[0040] In the Figure 1b In the second step shown, the electrode material 4 applied as a slurry is dried, for example, in a drying oven. In this way, the liquid in the slurry evaporates, leaving the electrode material 4 as a solid coating 10 on the metal foil 2.

[0041] In the Figure 1cIn the schematically illustrated third step, the coating 10 of electrode material 4 is rolled with a rolling device 12 so that the coating 10 has a uniform layer thickness and the material is pressed. The rolling device 12 can, in particular, also be designed in the form of a calender, so that the metal foil 2 with the coating 10 is calendered.

[0042] Afterwards, you can Figure 1d In the fourth step shown, further drying, in particular vacuum drying in a vacuum oven 13, can take place so that any liquid remaining in the coating 10 evaporates.

[0043] The electrode foil 14 provided in this way with the metal foil 2 and the coating 10 is then in the Figure 1eThe coating 10 is plasma-treated in the step shown by exposing the coating 10 to an atmospheric plasma jet 16, which is generated by means of high-frequency electrical discharges between electrodes in a working gas stream in a plasma nozzle 18. In this way, the surface 20 of the coating 10 is plasma-treated to a certain depth and thus prepared for subsequent impregnation of the coating 10 with liquid electrolyte.

[0044] Alternatively, the plasma treatment of the coating 10 can also be carried out before Fig. 1d shown second drying step.

[0045] The Figures 2a-d now show an embodiment of the method for producing a lithium-ion battery in a schematic representation.

[0046] In the Figure 2aIn the first step shown, a first electrode foil 22 for the negative electrode, a second electrode foil 24 for the positive electrode, a separator layer 26, for example a polypropylene mesh, and an insulator layer 28, for example a plastic film, are provided and as shown in Figure 2a shown arranged one above the other to form a foil stack 30 such that the separator layer 26 is arranged between the two electrode foils 22, 24. The insulator layer 28 can be arranged as in Fig. 2a shown on the side of the second electrode foil 24 or instead on the side of the first electrode foil 22. The same material can be used for the insulator layer 28 as for the separator layer 26.

[0047] The first electrode foil 22 comprises a metal foil 32 and a coating 34 of electrode material for the negative electrode, for example, a copper foil with a graphite coating. The second electrode foil comprises a metal foil 36 and a coating 38 of electrode material for the positive electrode, for example, an aluminum foil with a lithium nickel manganese cobalt oxide coating. The separator layer 26 serves to prevent direct electrical contact between the two coatings 34, 38 of electrode material.

[0048] At least one, preferably both of the Fig. 2a The electrode foils 22, 24 shown are produced by a process as described in Figures 1a-e provided illustrated.

[0049] Accordingly, the coating of at least one, preferably the coatings of both electrode foils 22, 24 are plasma-treated with an atmospheric plasma jet.

[0050] Figure 2bshows the slide stack 30 from Figure 2a in plan view. Since the width of the individual foils of the foil stack 30 and thus also the width of the foil stack 30 is wider than the width required for the production of lithium-ion batteries, the foil stack 30 is divided into several strips 40, which have a width b suitable for the production of the desired lithium-ion batteries. Alternatively, the electrode foils 32, 36 and, if applicable, the separator layer 26 and, if applicable, the insulator layer 28 can also be Fig. 2a Likewise, the metal foil 2 can be divided before the plasma treatment of the coating 10 ( Fig. 1e ) or before the second drying ( Fig. 1d ) is conceivable.

[0051] In the Figure 2c In the step shown, such a strip 40 of the foil stack 30 is rolled up and then, as further in Figure 2dillustrated in sectional view, inserted into a battery case 42. Instead of rolling up to produce a cylindrical accumulator, the strip 40 can also be folded to produce a rectangular accumulator.

[0052] A liquid electrolyte 44 is filled into the housing 42, allowing the electrolyte to penetrate and thus impregnate the coatings 34, 38 of the two electrode foils 22, 24 of the strip 40. The prior treatment of the coating 34 and / or 38 with the atmospheric plasma jet 14 significantly reduces the time required to impregnate the coatings 34, 38 with the electrolyte.

[0053] In this way, the production time for lithium-ion batteries can be reduced in an economical way.

[0054] Figure 3 shows a schematic sectional view of a plasma nozzle 56 which is used in the Figure 1ecan be used in the process step shown. In particular, the plasma nozzle 16 can be designed like the plasma nozzle 56.

[0055] The plasma nozzle 56 has a metal nozzle tube 58 that tapers substantially conically to a nozzle tube orifice 60. At the end opposite the nozzle tube orifice 60, the nozzle tube 58 has a swirl device 62 with an inlet 64 for a working gas, for example, air.

[0056] An intermediate wall 66 of the swirl device 62 has a ring of circumferentially inclined bores 68 through which the working gas is swirled. The downstream, conically tapered portion of the nozzle tube 58 is therefore flowed through by the working gas in the form of a vortex 70, the core of which extends along the longitudinal axis of the nozzle tube 58.

[0057] An electrode 72 is arranged centrally on the underside 66 and projects coaxially into the nozzle tube 58 in the direction of the tapered section. The electrode 72 is electrically connected to the intermediate wall 66 and the remaining parts of the swirl device 62. The swirl device 62 is electrically insulated from the nozzle tube 58 by a ceramic tube 74. A high-frequency high voltage, generated by a transformer 76, is applied to the electrode 72 via the swirl device 62. The inlet 64 is connected via a hose (not shown) to a pressurized working gas source with a variable throughput. The nozzle tube 58 is grounded. The excited voltage creates a high-frequency discharge in the form of an arc 78 between the electrode 72 and the nozzle tube 58.

[0058] The terms "arc," "arc discharge," and "arc-like discharge" are used here to describe the discharge, as the discharge occurs in the form of an arc. The term "arc" is also used elsewhere to describe the discharge type for DC discharges with essentially constant voltage values. In this case, however, it is a high-frequency discharge in the form of an arc, i.e., a high-frequency arc-like discharge.

[0059] Due to the swirling flow of the working gas, this arc 78 is channeled in the vortex core along the axis of the nozzle tube 58, so that it only branches out toward the wall of the nozzle tube 58 in the area of ​​the nozzle tube orifice 60. The nozzle tube 58 thus represents the counter electrode.

[0060] The working gas, which rotates at a high flow velocity in the region of the vortex core and thus in the immediate vicinity of the arc 78, comes into intimate contact with the arc 78 and is thereby partially converted into the plasma state, so that an atmospheric plasma jet 80 emerges from the plasma nozzle 56 through the nozzle tube mouth 60 and through an outlet nozzle 82 adjacent to the nozzle tube mouth 60.

[0061] The plasma jet 80 emerging from the plasma nozzle 56 has a high reactivity and, due to its relatively low temperature, is gentle on the surface even at a short distance from the outlet nozzle, so that an effective treatment of the coating of electrode material can be carried out without damaging it.

[0062] Figure 4 shows a schematic sectional view of another plasma nozzle 96 with a nozzle arrangement 98, which in the Figure 1ecan be used in the process step shown. In particular, the plasma nozzle 16 can be designed as a plasma nozzle 96 with a connected nozzle arrangement 98.

[0063] The plasma nozzle 96 has in principle the same structure and the same function as the plasma nozzle 56 from Figure 3 . The actual plasma nozzle 96 is connected to the nozzle assembly 98, into which the plasma jet 80 from the plasma nozzle 96 passes. This nozzle assembly 98 has a channel 100 connected to the plasma nozzle 96 in such a way that the plasma jet from the plasma nozzle 96 passes into the channel 100.

[0064] In the channel wall of the channel 100, several nozzle openings 102 are introduced next to each other along the channel, so that the plasma jet 80 is divided into several partial jets 104, which emerge from the individual nozzle openings 102. In this way, a curtain of plasma jets is achieved, through which a larger area, in particular the coating 10 from Fig. 1e In this way, the plasma treatment of the coating 10 can be Fig. 1e efficiently and with a smaller number of plasma nozzles.

[0065] The Figure 4 shown and for the Fig. 1e The plasma nozzle 96 with nozzle arrangement 98 which can be used in the process step shown is basically known from DE 10 2016 125 699 A1, to which reference is made for further possible features and functions of this plasma nozzle with nozzle arrangement.

[0066] The Fig. 5a-cshow a further embodiment of the method for providing an electrode foil for producing a lithium-ion battery in a schematic view.

[0067] In the Fig. 5a In the first step sequence shown, a metal foil 110 is unwound from a roll 112 and guided over a roll 114, opposite which a coating nozzle 116 is arranged, with which the metal foil 110 is applied in sections with electrode material 118 in the form of an aqueous suspension, so that one side of the metal foil 110 is provided in sections with coatings 120 of electrode material.

[0068] The metal foil 110 with the sectioned coatings 120 is then dried in a flotation dryer 122, in which hot air 124 is blown against the metal foil 110 from below. In this way, a large portion of the water evaporates from the coatings 120.

[0069] After a subsequent cooling step in a cooling device 126, the metal foil 110 provided with the coatings 120 is calendered with a calender 128 and wound into a roll.

[0070] In the Fig. 5b In the second step sequence shown, the metal foil 110, which is provided on one side with section-wise coatings 120, is also provided on the opposite side with corresponding section-wise coatings 130 of electrode material 118, dried in the flotation dryer 122, cooled in the cooling device 126 and calendered with the calender 128 and rolled up into a roll 140.

[0071] In the Fig. 5c In the step shown, the roll 140 is then vacuum dried in a vacuum oven 142 so that the finished electrode foil 144 is obtained.

[0072] In order to shorten the time required for the complete saturation of the coatings 120, 130 of electrode material with an electrolyte during the subsequent production of lithium-ion batteries, the coatings 120 and 130 are exposed to an atmospheric plasma jet 146.

[0073] The application can occur, for example, after the rough drying in the flotation dryer 122 using a plasma nozzle 148 arranged behind the flotation dryer. Alternatively, the application of the plasma jet 146 can also occur after calendering using a plasma nozzle 150 arranged behind the calender 128. Alternatively, the application of the plasma jet 146 can also occur after the final drying in the vacuum furnace 142. For this purpose, the roll 140 can, for example, be unwound and exposed to atmospheric plasma jets from both sides (not shown). In this case, the electrode foil 144 is finished after the plasma treatment.

[0074] The one or more plasma nozzles used for applying the plasma jet, in particular the plasma nozzle 148 or 150, can be designed, for example, like the plasma nozzle 56 or like the plasma nozzle 96 with nozzle arrangement 98.

[0075] The Fig. 6a-c show a further embodiment of the method for producing a lithium-ion battery.

[0076] First, an electrode foil for the positive electrode and an electrode foil for the negative electrode, each with two-sided section-wise coatings of electrode material for the positive and negative electrodes, are coated with the Fig. 5a-cThe electrode foil for the positive electrode can be, in particular, the electrode foil 144, wherein an aluminum foil was used as the metal foil 110 and an electrode material 118 containing lithium nickel manganese cobalt oxide was used for the coatings 120, 130. The electrode foil for the negative electrode can be an electrode foil 154 produced in a corresponding manner, wherein a copper foil was used as the metal foil 110' and a graphite-containing electrode material 118 was used for the coatings 120', 130'.

[0077] The electrode foil 144 is in the Fig. 6a In the step shown, the electrode foil 154 is cut into sections using a cutting device 156. Similarly, in a step not shown, the electrode foil 154 is cut into sections.

[0078] The individual sections of the electrode foil 144 and 154 are then Fig. 6bAs shown, they are alternately stacked to form a stack 158, with a separator layer 160, for example in the form of a polypropylene mesh, being inserted to prevent direct electrical contact between the coatings 120, 120', 130, 130' of the successive electrode foils. The metal foils 110, 110' of the electrode foils 144 and 154 each protrude to one side to enable later contact with the respective electrode.

[0079] The finished stack 158 is as in Fig. 6c shown inserted into a battery housing 162, wherein the projecting metal foils 110 of the electrical foils 144 are electrically connected to a positive battery pole 164 provided on the battery housing 162 and the projecting metal foils 110' of the electrical foils 154 are electrically connected to a negative battery pole 166 provided on the battery housing 162.

[0080] Subsequently, the accumulator housing 162 is filled through a provided filling opening 168 with an electrolyte 170, for example with lithium salts dissolved in ethylene carbonate, which then impregnates the coatings 120, 120', 130, 130' of the electrode foils 144, 154.

[0081] The prior plasma treatment of the coatings 120, 120', 130, 130' with the atmospheric plasma jet ensures that the electrolyte 170 can penetrate better into the coatings 120, 120', 130, 130', so that the time required for the impregnation of the coatings 120, 120', 130, 130' can be significantly shortened.

[0082] Experiments were conducted to investigate the effect of plasma treatment on the electrode material. For this purpose, samples of graphite-coated copper foil and aluminum foil coated with lithium nickel manganese cobalt oxide (NMC) were provided. The graphite coating of the copper foil contained carboxymethylcellulose and styrene butadiene rubber as binders. The lithium nickel manganese cobalt oxide coating of the aluminum foil contained polyvinylidene fluoride as a binder.

[0083] The graphite coating and the lithium nickel manganese cobalt oxide coating were each plasma treated by exposing the coatings to an atmospheric plasma jet containing one of the Fig. 3 plasma nozzle corresponding to the plasma nozzle shown.

[0084] Drops of an electrolyte were then applied to the plasma-treated coatings, and the time until the drop was completely absorbed into the coating was measured using contact angle measurement. A lithium hexafluorophosphate solution in ethylene carbonate-d4 and ethyl methyl carbonate-d8 (Sigma-Aldrich, 746711) was used as the electrolyte. The time required for the drop to be absorbed into the coating is an indicator of the time required for the electrode material to be completely saturated with electrolyte.

[0085] Furthermore, comparative tests were carried out with corresponding, but not plasma-treated, samples.

[0086] The measurement results are shown in the following Table 1: Table 1 Sample material Without plasma treatment With plasma treatment Copper foil with graphite coating 23,4 s 6,13 s Aluminum foil with NMC coating 5,53 s 3,45 s

[0087] As the test results in Table 1 show, in both cases the plasma treatment achieved a reduction in the time until complete absorption of the electrolyte droplet, which accordingly indicates a reduced time until complete soaking with electrolyte.

[0088] This shows that the electrolyte uptake by the electrode material can be significantly improved using plasma treatment.

Claims

1. Method for providing an electrode foil (14, 22, 24, 144, 154) for the manufacture of a lithium-ion accumulator, - in which a metal foil (2, 32, 36, 110, 110') with a coating (10, 34, 38, 120, 120', 130, 130') of electrode material (4, 118) is provided, and - in which the coating (10, 34, 38, 120, 120', 130, 130') of electrode material (4, 118) is plasma-treated, characterised - in that the coating (10, 34, 38, 120, 120', 130, 130') of electrode material (118) is plasma-treated by exposing the coating (10, 34, 38, 120, 120', 130, 130') to an atmospheric plasma jet (16, 80, 146), the atmospheric plasma jet (16, 80, 146) being generated with a plasma nozzle (18, 56, 96, 148, 150).

2. Method according to claim 1, characterised - in that the metal foil (2, 32, 36, 110, 110') with the coating (10, 34, 38, 120, 120', 130, 130') of electrode material (4, 118) is provided by applying electrode material (4, 118) to the metal foil (2, 32, 36, 110, 110') and drying and calendering the electrode material (4, 118) applied to the metal foil (2, 32, 36, 110, 110'), and in that the coating (10, 34, 38, 120, 120', 130, 130') of electrode material (4, 118) is plasma-treated after calendering.

3. Method according to claim 1 or 2, characterised in that the coating (10, 34, 38, 120, 120', 130, 130') of electrode material (4, 118) is porous.

4. Method according to one of claims 1 to 3, characterised in that an aluminum foil or a copper foil is used as the metal foil (2, 32, 36).

5. Method according to one of claims 1 to 4, characterised in that the coating (10, 34, 38, 120, 120', 130, 130') of electrode material (4, 118) contains one or more of the following compounds, preferably consists thereof by at least 90 wt.-%: lithium cobalt(III) oxide, lithium nickel manganese cobalt oxides, Li spinels, LiFePO4.

6. Method according to any one of claims 1 to 4, characterised in that the coating (10, 34, 38, 120, 120', 130, 130') of electrode material (4, 118) contains one or more of the following compounds, preferably consists thereof by at least 90 wt.-%: graphite, other Li-intercalating carbons, nanocrystalline amorphous silicon, lithium titanates, tin dioxide.

7. Method according to one of claims 1 to 6, characterised in that the atmospheric plasma jet (16, 80, 146) is generated by high-frequency electrical discharges (78) between electrodes (72, 58) in a working gas stream.

8. Method according to claim 7, characterised in that a plasma nozzle (96) with a nozzle arrangement (98) is used to generate the atmospheric plasma jet (18, 56, 96, 146), which nozzle arrangement divides the plasma jet (80) generated with the plasma nozzle (96) into a plurality of partial jets (104) emerging from a plurality of nozzle openings (102) of the nozzle arrangement (98) arranged along a channel.

9. Method for manufacturing a lithium-ion accumulator - in which a first electrode foil (22, 154) is provided for the negative electrode and a second electrode foil (24, 144) is provided for the positive electrode, - in which the first and second electrode foils (22, 24, 144, 154) are arranged one above the other with a separator layer (26, 160) between them to form a foil stack (30, 158), and - in which the foil stack (30, 158) is impregnated with a liquid electrolyte (44, 170), characterised - in that the first and / or the second electrode foil (22, 24, 144, 154) are provided by a method according to any one of claims 1 to 8.