ACTIVE CARRIER IN PHOTOCATALYSIS
Patent Information
- Application Number
- DE602020039893
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-09-30
- Filing Date
- 2020-06-30
- Publication Date
- 2024-10-23
- Estimated Expiration
- 2040-06-30
AI Technical Summary
Existing processes using titanium oxide (TiO2) nanocrystals in photocatalysis face challenges due to their nanometric size, which poses toxicity risks and environmental dissemination concerns, and they are rarely active in visible light, making it difficult to develop environmentally friendly and effective photocatalytic materials.
A process that fixes TiO2 nanocrystals in situ on a support within an acidic aqueous medium, using titanium oxide precursors, without surfactants, to create micrometric-sized photocatalysts active in the visible range, ensuring strong covalent bonding and preventing dissemination, allowing for diverse applications like self-cleaning coatings and air filtration.
The process produces stable, reactive TiO2-based photocatalysts that are effective in visible light, reducing environmental risks and maintaining exceptional photocatalytic properties, enabling wide-ranging applications from textiles to construction materials without losing reactivity, even at larger scales.
Description
DOMAINE DE L'INVENTION
[0001] The present invention relates to a method for producing a photocatalyst support, of at least micrometric size and active in photocatalysis at least in the visible range, and having on its surface nanocrystals each composed of 80% to 100% by mole of TiO 2 and 0% to 20% by mole of at least one other metallic or semi-metallic oxide. ETAT DE LA TECHNIQUE
[0002] TiO 2 -based nanoparticles are used in many fields: cosmetics (sunscreen), food, pollution control, etc. These are inexpensive materials, hence their widespread use. In recent years, several studies have warned of the dangers of using these nanometric materials (size < 100nm).
[0003] Due to their nanometric size, these materials would pass through the protective barriers of living beings, accumulate in organisms and hypothetically affect cells. The consequences on these cells are currently highly debated: some studies report a very harmful impact even going as far as cellular destruction, others on the contrary have shown very weak to moderate consequences.
[0004] Self-cleaning or reflective coatings (textiles, paints, glass, concrete, etc.) based on TiO 2 are known, the major problem remaining the nanometric size of the titanium oxide particles, considered dangerous for living beings. In existing processes, these titanium oxide nanocrystals, once synthesized or purchased, are imported into or onto the surface of the coatings. The risk of dissemination into the environment is therefore real, since these particles can easily detach, due to the very weak bond between the coating and the materials.
[0005] In addition to the small size of these materials, their powdery nature, leading to significant dissemination in the environment, is also a concern. This is especially true since, given their exceptional properties and low production costs, it is currently impossible to eliminate these materials from existing processes. This is why it is important to be able to eliminate this toxicity, without significantly reducing the properties of the materials or increasing their formulation costs, and to develop new, more environmentally friendly processes. Document KR20030027551 describes a method for obtaining a coating composed of TiO 2 particles on a support, giving the support photocatalytic properties. Document WO2017 / 109426 describes a method for preparing a nanomaterial composed of 80 to 100 mol% TiO 2 and 0 to 20 mol% of another metal or semi-metal oxide.
[0006] Furthermore, state-of-the-art TiO2 particles are rarely active in visible light photocatalysis.
[0007] It is in this context that the invention is placed. EXPOSE DE L'INVENTION
[0008] The inventors have developed a method for fixing TiO 2 in situ inside or on the surface of a support, allowing the development of new processes and the transformation of TiO 2 into a non-powdery and non-nanometric form retaining exceptional photocatalytic properties.
[0009] The present invention uses a process for preparing an acidic aqueous reaction medium composed of 80% to 100% by mole of TiO 2 and 0% to 20% by mole of another oxide, from a titanium oxide precursor which is a titanium alkoxide, or from a mixture of a titanium oxide precursor with at least one other precursor of another metallic or semi-metallic oxide, the preparation being carried out in an acidic aqueous medium at a given pH, without the use of a surfactant, and comprising the following steps: a1) preparation and heating of an acidic aqueous solution at a given pH, between 0 and 6, and at a temperature between 20°C and 60°C, without surfactant, by adding hydrochloric acid, a2) addition of a titanium oxide precursor, or a mixture of a titanium oxide precursor and at least one other precursor of another oxide, to the acidic aqueous solution, a precipitate then forming, a3) stirring of the aqueous reaction medium, so as to dissolve the precipitate formed in step a2).
[0010] The present invention relates to a method for producing a support of at least micrometric size and active in photocatalysis at least in the visible range, containing crystals each composed of 80% to 100% by mole of TiO 2 and of 0% to 20% by mole of at least one other metallic or semi-metallic oxide, comprising the following steps, starting from the acidic aqueous reaction medium defined above at a heating temperature of between 20°C and 60°C: a4) a step of adding a titanium oxide precursor, or a mixture of a titanium oxide precursor and a precursor of the other oxide, into the acidic aqueous reaction medium, and a polymerization step (condensation of the precursors over the entire surface) on or inside the support (if the support is hollow), by: spraying onto the support or immersing the support in the aqueous reaction medium, for a determined polymerization time, a5) a heating step, the support allowing the crystals to crystallize, without the use of surfactant, in the aqueous reaction medium, a6) a rinsing step with water and a recovery step: on the one hand, the support on which the crystallization has taken place, the crystals obtained being composed of 80% to 100% by mole of TiO 2 and 0% to 20% by mole of at least one other metal or semi-metal oxide, these crystals being attached by covalent bonds to the support,and on the other hand a residual solution.
[0011] The present invention also relates to a support active in photocatalysis at least in the visible range and of at least micrometric size, produced by the process defined above, having on its surface crystals attached by covalent bonds, these crystals being composed of 80% to 100% by mole of TiO 2 and of 0% to 20% by mole of another metallic or semi-metallic oxide.
[0012] The object of the invention thus makes it possible to make supports active in photocatalysis by incorporating materials based on titanium oxide under mild conditions (respecting the criteria of green chemistry).
[0013] This innovative method has several advantages.
[0014] First, make supports active in photocatalysis. These supports can be of very diverse natures (polymers, carbon / graphite felts or activated carbon, glasses, textiles, silicates, etc.), allowing numerous applications such as self-cleaning coatings, antibacterial air filters, reflective paints, etc.
[0015] Second, to fix the titanium oxide-based nanocrystals to a surface without loss of reactivity, thus preventing any risk of dissemination into the environment.
[0016] Thus, the present invention makes it possible to create a very strong bond between the support and TiO 2, by directly developing the nanocrystals inside or on the surface of a support, without the risk of detaching and spreading into the environment.
[0017] For certain applications that do not allow in situ synthesis, such as paints for example, nanocrystals are developed on micrometric and macrometric supports, then added to the paint without loss of reactivity.
[0018] It is also possible to spray the TiO 2 reaction medium directly onto the paint which then constitutes the support.
[0019] Among the applications outlined above, we have successfully developed reactive textiles (basalt-based textiles, carbon felts, and also a fabric containing 65% polyester and 35% cotton) to eliminate, in aqueous solution, dyes, some of which include toluene (VOCs found in indoor air in buildings), and a compound that has been very problematic in recent years: glyphosate. We have also developed reactive polystyrene to eliminate a dye in water. We also have proof that our materials remain active despite their crystallization on micrometric and / or millimetric silica compounds, and also on construction materials such as sand (micrometric), suggesting that our technology can be used in the construction industry.
[0020] The range of applications is very wide, since the crystallization of TiO 2-based materials can be carried out on a large number of supports.
[0021] Furthermore, thanks to the present invention, titanium oxide TiO 2 can be scaled to micrometer or millimeter scale, without loss of reactivity, solving the problems related to its nanometer size in many other applications.
[0022] Another very important advantage of the invention is to produce an active support in photocatalysis in visible light, making this support attractive for many applications and in many fields. DESCRIPTION DES FIGURES
[0023] The present study was carried out with a TiO 2 -based material (composed of 80% to 100% by mole of TiO 2 and 0% to 20% by mole of another oxide) on basalt-based textile fabric, on felted carbon, on polymers such as polystyrene, on a cotton / polyester support (chemist's coat), on siliceous supports of variable macrometric and micrometric size (filter silica and sand).
[0024] The organic pollutants used are: methyl orange (concentration 10mg / L (or ppm)) and bromophenol blue (concentration 20mg / L (or ppm)), glyphosate and toluene (concentration 1mg / L (or ppm)); and they were subjected to 3 hours of radiation (for example with a 300 W Xenon lamp with UV filter).
[0025] The present study shows that with the TiO 2 of the present invention, photocatalysis is possible with radiation in the visible range (which provides little energy to achieve it) and is more significant than with a less active commercial TiO 2 alone. Most studies show that state-of-the-art TiO 2 mainly allow photocatalysis with UV radiation, which provides more energy to achieve it than radiation in the visible range.
[0026] The characteristics and advantages of the invention will emerge from the detailed description which follows with reference to the drawings given for illustrative and non-limiting purposes, among which: there figure 1 represents a diagram of application of TiO 2-based materials on support; the figure 2 represents the three TiO 2-based crystal structures obtained using the invention; the figure 3 represents a graph illustrating the degradation of dyes (methyl orange MO, bromophenol blue BBP) on basalt-based textile fabric; figure 3 shows the adsorption of dye molecules on the textile without treatment but greater efficiency in the presence of nanocrystals; the nanocrystals are well attached to the fibers, and there is no TiO 2 in the solution; the figure 4 represents a graph illustrating the degradation of concentrated bromophenol blue (BBP) on used basalt-based textile fabric (recycling); figure 4 shows that the reuse of textiles is possible without loss of activity, as well as the long life of textiles; figure 5 represents a graph illustrating the degradation of bromophenol blue (BBP) on carbon felt; figure 5 shows the adsorption of BBP molecules on the carbon felt but in the presence of TiO 2 even more reactivity (total disappearance of the organic molecules in solution); the nanocrystals are well attached in the felt, and there is no TiO 2 in the solution; the figure 6 represents a graph illustrating the degradation of methyl orange (MO) on polystyrene and on a polyester / cotton blend (65% / 35%); the figure 6 shows a polystyrene and polyester / cotton blend made reactive with the addition of TiO 2 ; the nanocrystals are well attached to these two supports, and there is no TiO 2 in the solution; the figure 7 represents a graph illustrating the degradation of methyl orange (MO) on Fontainebleau sand and sieve pellets (mixture of Al 2 O 3 and Fe 2 O 3 ); the sand and pellets are made reactive with the addition of TiO 2 ; TiO 2 adheres to supports based on SiO 2 but also containing Al 2 O 3 , Fe 2 O 3 , at the micrometric scale; the nanocrystals are well attached to these two supports, and there is no TiO 2 in the solution; the figure 8 represents a graph illustrating the degradation of methyl orange (MO) on filter silica (micron); micron silica is made reactive with the addition of TiO 2 ; TiO 2 adheres to SiO 2-based supports at the micron scale; the silica was treated with Cull grafting before treatment with TiO 2 to improve the amount of silanol groups on the surface, the reaction occurring without an increase in silanol groups; the figure 9 represents polystyrene beads alone with Methyl orange (left) at t=0, and polystyrene / Ti beads with Methyl orange after radiation; the figure 10 represents photos taken after irradiation and drying of the textile: textile without Ti with bromophenol blue (top), textile / Ti immersion with bromophenol blue (middle), textile / Ti by spray with bromophenol blue (bottom); the figure 11 represents a transmission electron microscopy image - Activated carbon / Ti; the figures 12a And 12b represent scanning electron microscopy images - sand / Ti. The figure 12a corresponds to an image of a grain of sand / Ti with an image width of 413 µm and the figure 12b corresponds to an image of the sand / Ti grain with an image width of 16.99 µm and shows TiO 2 crystals attached to the surface. DESCRIPTION DETAILLEE DE L'INVENTION
[0027] The present invention uses a process for preparing an aqueous reaction medium composed of 80% to 100% by mole of TiO 2 and 0% to 20% by mole of another oxide, from a titanium oxide precursor which is a titanium alkoxide, or from a mixture of this titanium oxide precursor with at least one other precursor of another metallic or semi-metallic oxide.
[0028] The preparation is carried out in an acidic aqueous medium at a given pH, without the use of surfactant, and includes the following steps: a1) preparation and heating of an acidic aqueous solution at a given pH between 0 and 6, and at a temperature between 20°C and 60°C, without surfactant, by adding hydrochloric acid, a2) addition of a titanium oxide precursor, or of a mixture of a titanium oxide precursor and at least one other precursor of another oxide to the acidic aqueous solution, a precipitate then forming, a3) vigorous stirring of the aqueous reaction medium, so as to dissolve the precipitate formed in step a2).
[0029] Advantageously, hydrochloric acid is added, for example between 30% and 37% mass / volume.
[0030] In a first embodiment of the process, in step a1), the pH of the reaction medium is chosen to be around 5, so as to obtain nanocrystals on the support having a stable Brookite crystalline form, and reactive in photocatalysis at least in the visible range.
[0031] In a second embodiment of the process, in step a1), the pH of the reaction medium is chosen around 0-2, so as to obtain nanocrystals having a Rutile crystalline form, reactive in photocatalysis at least in the visible range.
[0032] The metallic or semi-metallic oxide can be chosen from: SiO 2 , ZrO 2 , Al 2 O 3 , Fe 2 O 3 , CeO 2 , MgO, ZnO, CuO, NiO.
[0033] In a third embodiment of the process, the other metal oxide being WOs, and in step a1) the pH of the reaction medium is between 0 and 1, so as to obtain nanocrystals having an Anatase crystalline form of at least 90%, reactive in photocatalysis at least in the visible range.
[0034] The present invention relates to a method for producing a support of at least micrometric size and active in photocatalysis at least in the visible range (and a fortiori in the UV range), containing nanocrystals each composed of 80% to 100% by mole of TiO 2 and 0% to 20% by mole of at least one other metallic or semi-metallic oxide.
[0035] This process for producing the support comprises the following additional steps, starting from the acidic aqueous reaction medium obtained above at a heating temperature between 20°C and 60°C: a4) a reaction step between the precursors (titanium oxide precursor, or a mixture of a titanium oxide precursor and a precursor of the other oxide) obtained in step a3) and the support, to condense the precursors which attach to it by covalent bonds on its surface, on or inside the support, by: spraying on the support or immersing the support in the aqueous reaction medium, for the determined duration of the synthesis, a5) a heating step being between 40 and 95°C, the support allowing the nanocrystals to crystallize, without the use of surfactant, in the aqueous reaction medium, a6) a rinsing step with water and recovery: on the one hand of the support on which the crystallization took place, the nanocrystals obtained being composed of 80% to 100% by mole of TiO 2 and 0% to 2 ... moles of at least one other metallic or semi-metallic oxide, these nanocrystals being attached by covalent bonds to the support,and on the other hand a residual solution.
[0036] Thus, the invention makes it possible to produce supports active in photocatalysis by incorporating materials based on titanium oxide in mild conditions (without surfactant, aqueous medium, requiring little energy, without excessive temperatures),
[0037] This residual solution could be re-implanted in the reaction medium for a new synthesis depending on the complete stoichiometry or not of the reaction with the titanium alkoxide and the surface.
[0038] For silica, the surface was prepared upstream of step a4), to increase the (O-) attachment points (Cull grafting).
[0039] All steps of the process can be carried out in the open air, i.e. in contact with ambient air. Advantageously, the acidic aqueous solution is produced without co-solvent, in a non-limiting manner, such as alcohol.
[0040] Stirring of the acidic aqueous reaction medium can be carried out until the precipitate disappears.
[0041] The stirring of the acidic aqueous reaction medium can be carried out between 800 and 1200 rpm.
[0042] Advantageously, the technique used is not a dip coating.
[0043] When a support is added, the condensation reaction of the surfactant-free precursors in step a4) is very rapid and takes between 30 and 90 minutes. The TiO 2 precursors will form covalent bonds that attach to the surface on or inside the support and then grow crystals there.
[0044] In the present invention, the TiO 2 precursors are formed after a first precipitate formation which is vigorously stirred in order to dissolve it in the medium. Then in this medium, the TiO 2 precursors attach to the support on its surface, on or inside, and crystallize only on the surface of the support in a single step. In other words, in the present invention, the TiO 2 precursors crystallize and grow only after attachment to the support.
[0045] On the other hand, the nanocrystals obtained on the support are generally more heterogeneous in shape and size than the nanocrystals obtained without support and without surfactant with only the acidic aqueous reaction medium.
[0046] Step a5) may present: a first heating sub-step from 30° to 60°C for a first given duration; a second heating sub-step from 50° to 90°C for a second duration. For example, for the first heating sub-step of step a5), the first heating duration may be several hours; for the second heating sub-step of step a5), the second heating duration may be several hours.
[0047] In step a5), the heating time determined may be at least 24 hours to make the material active and crystalline. Note that crystallization may take place at room temperature or at a higher temperature below a temperature at which the morphology of the crystals would change.
[0048] Furthermore, in step a6), the support / materials provided with TiO2-based nanocrystals can be immersed in an HNOs bath (optional step), then rinsed in water (to remove unattached particles).
[0049] Thus, during steps a4) and a5), there are condensation reactions then crystallization and finally increase in the size of the crystals and homogenization.
[0050] TiO 2 obtained very early can for example be made up of very small crystals in the form of a square of approximately 5nm, whereas that of 24h at 50°C and 24h at 90°C presents homogeneous crystals in the form of a stick of 5nm by 25nm.
[0051] Advantageously, the duration of the condensation reaction (polymerization) of step a4) is less than 90 minutes, and the heating temperature is between 40°C and 95°C, for a heating time of at least 24 hours during the heating step a5).
[0052] Advantageously, the support is millimeter, centimeter, or metric in size.
[0053] The support can be made of the following material: polymers (polystyrene, polyester); carbon / graphite felt or activated carbon; glass; textile (cotton, basalt); micrometric silicates (filter silica, sand); cements.
[0054] To make the support, in step a1): the pH is chosen around or equal to 5, so as to obtain nanocrystals on the support having a stable Brookite crystalline form, or the pH is between 0 and 2, so as to obtain nanocrystals having a Rutile crystalline form.
[0055] The support of at least micrometric size may comprise, like the metallic or semi-metallic oxide associated with TiO 2 , the following metallic oxides from the list: SiO 2 , ZrO 2 , Al 2 O 3 , Fe 2 O 3 , CeO 2 , MgO, ZnO, CuO, NiO.
[0056] In another embodiment, the other metal oxide associated with the TiO 2 is WOs, and in step a1) the pH is between 0 and 2, so as to obtain nanocrystals having an Anatase crystalline form at least 90%, reactive in photocatalysis at least in the visible range.
[0057] When nanocrystals are produced on the support by spraying the aqueous reaction medium, the process steps can be defined more precisely as follows: the support is placed in an oven at 50°C in a hermetically sealed container (to prevent any evaporation), under static conditions, for at least 24 hours, then 90°C for at least 24 hours, the support is then rinsed thoroughly with water.
[0058] The support can then be dried in an oven at 50°C.
[0059] Advantageously, depending on the nature of the support and the type of oxides present, to increase the reactivity and if the support allows it, but in a non-obligatory and non-limiting manner, the support can then be either: (a) immersed in a 64% nitric acid bath for 10 minutes, rinsed thoroughly with water and then dried, or (b) immersed in an ammoniacal metallic solution among Ag +< , Cu 2+< , Ni 2+< , Zn 2+< , Al 3+< , Mg +< , for 10 minutes, rinsed with water, dried at room temperature and then immersed in a nitric acid bath, for example 64% and for 10 minutes, rinsed thoroughly with water.
[0060] When the nanocrystals are produced on the support by immersing the support in the acidic aqueous reaction medium, the process steps can be defined more precisely as follows: the support is immersed in the reaction medium; depending on its nature and composition, the support is either: 1) placed in the oven under static conditions, or 2) kept in the reaction medium with moderate stirring (400 rpm); in both cases, the temperature of the support is kept at 50°C for at least 24 hours then at 90°C for at least 24 hours; the support is then rinsed thoroughly with water.
[0061] The support can then be dried in an oven at 50°C.
[0062] Then, advantageously, but not obligatorily and not limitingly, to increase responsiveness and if the support allows it, the support is either: a) immersed in a 64% nitric acid bath for 10 minutes, rinsed thoroughly with water and then dried at room temperature, b) immersed in a metal solution with a pH between 10.5 and 11.5 among: Ag +< , Cu 2+< , Ni 2+< , Zn 2+< , Au 2+< , Al 3+< , Mg +< , for 10 minutes, rinsed with water, dried at room temperature, then immersed in a 64% nitric acid bath for 10 minutes, rinsed thoroughly with water, and finally dried again at room temperature.
[0063] The present invention also relates to the use of the active support in photocatalysis with the nanocrystals crystallized on its surface, for the photocatalytic degradation of compounds.
[0064] The compounds can be chosen from dyes, pharmaceutical active ingredients, herbicides, pesticides, fungicides, hormones, hydrocarbons and volatile organic compounds such as formaldehyde, BTEX.
[0065] Thus, the degradation of glyphosate and toluene from TiO 2 according to the present invention is illustrated.
[0066] Degradation of glyphosate on a textile fabric based on basalt, for example, in 3 hours:
[0067] The presence of TiO2 on the textile is essential to eliminate glyphosate molecules.
[0068] The nanocrystals are well attached to the support, and there is no TiO 2 in the solution.
[0069] Degradation of toluene on basalt-based textiles:
[0070] The addition of TiO 2 improves the elimination of toluene.
[0071] The nanocrystals are well attached to the textile, and there is no TiO 2 in the solution.
[0072] Several applications are possible for example: 1) air quality, particularly indoor (degradation of VOCs), with the development of paints or air filters, 2) water decontamination (degradation of molecules such as BTEX, pesticides, dyes, etc.), 3) antifouling or antifouling paint, with the development of paints, antibacterial treatment with the development of air filters, self-cleaning coatings (glass, cement, sand, etc.).
Claims
1. Method for producing a photocatalyst support, at least micrometric in size and photocatalytically active at least in the visible region, containing nanocrystals each made up of 80 to 100 mol% of TiO2 and 0 to 20 mol% of at least one other metal or semi-metal oxide, comprising the following steps, without using a surfactant: a1) preparing and heating an acidic aqueous solution at a given pH, between 0 and 6, and at a temperature between 20°C and 60°C, without surfactant, by adding hydrochloric acid, a2) adding a titanium oxide precursor, or a mixture of a titanium oxide precursor and at least one other precursor of another metal or semi-metal oxide, to the acidic aqueous solution, a precipitate forming in the acidic aqueous reaction medium made up of 80 to 100 mol% of TiO2 and 0 to 20 mol% of another oxide, from the titanium oxide precursor which is a titanium alkoxide, or a mixture of this titanium oxide precursor with at least one other precursor of another metal or semi-metal oxide, a3) stirring the acidic aqueous reaction medium, so as to dissolve therein the precipitate formed in step a2), a4) reaction between the precursors obtained in step a3) and the support, to condense the precursors that attach by covalent bonds to the surface of the support, by: • spraying onto the support or • immersing of the support in the aqueous reaction medium, for a determined duration, a5) heating the heating temperature being between 40°C and 95°C, the support that is at least micrometric in terms of size allowing crystallisation of the titanium oxide precursors, or of a mixture of a titanium oxide precursor and of at least one other precursor of another metal or semi-metal oxide into nanocrystals, on its surface, without use of surfactant, in the acidic aqueous reaction medium the precursors crystallising, once bonded to the surface of the support, a6) rinsing with water and recovering: on the one hand, of support on which the crystallisation took place, the nanocrystals obtained being composed from 80 to 100 mol% of TiO2 and from 0 to 20 mol% of at least one other metal or semi-metal oxide, these nanocrystals being bonded to the support by covalent bonds, and on the other hand a residual solution.
2. Method for producing a support according to claim 1, wherein the method is carried out in the open air.
3. Method for producing a support according to one of claims 1 to 2, wherein the acidic aqueous reaction medium is produced without co-solvent.
4. Method for producing a support according to claim 3, wherein the acidic aqueous reaction medium is produced without alcohol.
5. Method for producing a support according to one of claims 1 to 4, wherein step a5) has: - a first sub-step of heating from 30°C to 60°C for a first given duration; - a second sub-step of heating from 50°C to 90°C for a second duration.
6. Method for producing a support according to claim 5, wherein: - for the first heating substep of step a5), the first heating duration is several hours; - for the second heating substep of step a5), the second heating duration is several hours.
7. Method for producing a support according to claim 6, wherein: - for the first heating substep of step a5), the first heating duration is at least 24 hours; - for the second heating substep of step a5), the second heating duration is at least 24 hours.
8. Method for producing a support according to one of claims 1 to 7, wherein in step a1), - the pH is chosen equal to 5, so as to obtain nanocrystals on the support having a stable brookite crystalline form, - or the pH is between 0 and 2, so as to obtain nanocrystals having a rutile crystalline form.
9. Method for producing a support according to one of claims 1 to 8, wherein the metal or semi-metal oxide is selected from: SiO2, ZrO2, Al2O3, Fe2O3, CeO2, MgO, ZnO, CuO, NiO.
10. Method for producing a support according to one of claims 1 to 8, wherein the other metal oxide is WO3, and in step a1) the pH is between 0 and 1, so as to obtain nanocrystals having an Anatase crystalline form at at least 90%.
11. Method for producing a support according to one of claims 1 to 10, wherein the support is in step a6): (a) immersed in a nitric acid bath, rinsed with water then dried, or (b) immersed in a metal solution among Ag +, Cu 2+, Ni 2+, Zn 2+, Al 3+, Mg +, rinsed with water, dried at room temperature, then immersed in a nitric acid bath and rinsed.
12. Photocatalyst support, photocatalytically active at least in the visible region and at least micrometric in size, produced by the method according to one of claims 1 to 11, having on its surface nanocrystals bonded by covalent bonds, these nanocrystals being composed of 80 to 100 mol% of TiO2 and of 0% to 20 mol% of another metal or semi-metal oxide.
13. Photocatalytically active support according to claim 12, characterised in that the active support comprises 80 to 95 mol% of TiO2 and 5 to 20 mol% of another metal or semi-metal oxide.
14. Photocatalytically active support according to claim 12 or 13, with nanocrystals having a stable Brookite crystalline shape.
15. Photocatalytically active support according to claim 12 or 13, with nanocrystals having a Rutile crystalline shape.
16. Photocatalytically active support according to one of claims 12 to 15, wherein the metal or semi-metal oxide is selected from the following list: TiO2, ZrO2, Al2O3, Fe2O3, CeO2, MgO, ZnO, CuO, NiO.
17. Photocatalytically active support according to one of claims 12 to 15, with nanocrystals having an Anatase crystalline form at at least 90%, the other metal oxide being WO3.
18. Photocatalytically active support according to any one of claims 12 to 17, wherein the support is made of the following material: polymers; carbon / graphite felt or activated carbon; glass; textile; micrometric silicates; cements.
19. Photocatalytically active support according to any one of claims 12 to 18, wherein the support is micrometric, millimetric, centimetric, metric in size.