Adhesive film that can be rolled up and stamped

ES3084250T3Undetermined Publication Date: 2026-11-11LOHMANN GMBH & CO KG (100 00)
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
ES2018822314T
Authority / Receiving Office
ES · ES
Patent Type
Patents
Current Assignee / Owner
Filing Date
2018-12-11
Publication Date
2026-11-11
Estimated Expiration
2038-12-11

AI Technical Summary

Technical Problem

Existing adhesive systems, particularly UV-activated structural adhesive films, lack effective process control mechanisms to indicate activation and curing progress, which is crucial for ensuring proper bonding in applications like automotive manufacturing.

Method used

A UV-activated epoxy-based adhesive film with integrated dyes or pigments that change color upon activation and curing, allowing visual process control through color changes.

Benefits of technology

Enables in-process control of adhesive activation and curing, ensuring reliable bonding by visually indicating the activation and curing status, maintaining mechanical properties and adhesive strength.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000011_0000
    Figure 00000011_0000
  • Figure 00000011_0001
    Figure 00000011_0001
  • Figure 00000011_0002
    Figure 00000011_0002
Patent Text Reader

Abstract

The present invention relates to a rollable and printable adhesive film having an epoxy-based adhesive compound that can be activated thermally or by UV radiation, and a dye and / or pigment mixed into the adhesive compound to produce a first color change after activation of the adhesive compound and a second color change after curing of the adhesive compound.
Need to check novelty before this filing date? Find Prior Art

Description

Technical field

[0001] The present invention relates to a wound-curable and die-cuttable adhesive film for structural bonding, which can be activated and cured by ultraviolet (UV) radiation or thermally and which changes color upon activation, and which is adhesive in its unactivated state. In this sense, references to UV activation in the following text always also imply the equally possible thermal activation.

[0002] The terms used in the following explanations are to be understood as follows: "Adhesive film" refers to any form of flat adhesive systems, i.e. not only adhesive tapes in the narrower sense, but also adhesive films, adhesive strips, adhesive sheets or adhesive die-cut parts.

[0003] "Pressure-activated" adhesive bonds are those in which the two components are joined by an intervening adhesive layer under pressure. The bond is reversible in that it can be separated without damaging either component, because the adhesive seam is the weakest point in the joint.

[0004] Adhesive bonds are described as "structural" when the joining partners are bonded in such a way that, in the event of separation, the bond does not necessarily break at the adhesive seam. Instead, one of the joining partners may be the weakest point in the bond and thus be damaged by the separation. Structural adhesive bonds therefore possess high strength. The strengths, measured in a quasi-static tensile-shear test, exceed 6 MPa for structural bonds. Typical target values ​​for structural epoxy adhesive bonds are between 10 and 20 MPa.

[0005] "Radiation hardening" refers to a process in which reactive materials are transformed from a low molecular weight to a high molecular weight state using high-energy radiation.

[0006] In this case, UV radiation refers to "UVA" or "UVC" light.

[0007] UVA radiation lies in the wavelength range of approximately 380 to 315 nanometers (nm), while UVC radiation lies in the wavelength range of approximately 280 to 100 nm. Both are generally electromagnetic radiation with wavelengths shorter than visible light. The energy input of UVA light is approximately 3.26 to 3.95 electron volts (eV), and that of UVC light is approximately 4.43 to 12.40 eV.

[0008] "Activation" means initiating a curing process through irradiation with UV light. This means that the photoinitiators in the adhesive are activated by light exposure and trigger the curing process by initiating the formation of polymer chains. UV-curing adhesives are typically irradiated after the bonding partners have been joined. This requires substrates that are sufficiently transparent to the UV radiation used. The bond is then irradiated until the curing process is sufficiently advanced, meaning it has achieved adequate strength. Consequently, only UV-transparent substrates can be activated and bonded in this way. The final strength of the adhesive is only achieved after the curing process is complete.

[0009] "Open time" is the time between adhesive application and bonding. During the open time, a liquid hot melt adhesive, for example, spreads across the surfaces to be joined, ensuring the necessary adhesion. Since the viscosity, i.e., the thickness of an adhesive, typically increases after application, the open time of adhesives is limited.

[0010] The "curing time" is the period between the joining of the joining partners and the final strength of the connection.

[0011] The term "dark reaction" subsequently refers to the fact that a hardening reaction is initiated (triggered) by brief irradiation of the adhesive with UV light, and then complete hardening can occur without further irradiation.

[0012] Thermal activation refers to initiating the curing process by adding increased temperature, i.e., in this case, a temperature of at least 140°C.

[0013] The term "superacid" refers to the following: During cationic UV curing, ring opening occurs at the oxirane and / or oxetane (epoxy resins and vinyl ethers). This happens through photolysis of, for example, diaryliodonium salts, which results in the formation of strong protic acids, so-called superacids. The acid proton opens the epoxide ring and initiates chain growth, thus triggering the curing process. State of the art

[0014] UV-curing adhesives are often based on acrylate monomers or oligomers, which cure in a radical chain reaction induced by UV light.

[0015] In contrast, UV-curing epoxy adhesives are cured by a cationic photoinitiator. During cationic UV curing, ring opening occurs at the oxirane and / or oxetane (epoxy resins and vinyl ethers). This happens through photolysis of, for example, diaryliodonium salts, which is based on the generation of strong protic acids. The acid proton opens the epoxy ring and initiates chain growth, thus triggering curing.

[0016] In contrast to radical UV curing of acrylates, this results in lower shrinkage and good adhesion to a wide variety of substrates. Another advantage of cationic curing is its insensitivity to oxygen, which allows for high curing rates under normal atmospheric conditions. However, humidity and alkaline conditions tend to have a greater impact than with radical UV curing.

[0017] With cationic UV initiation, it is possible under certain circumstances to delay chain formation to such an extent that it can eventually proceed in the dark without further radiation exposure. It may even be possible to delay it significantly, so that it is only restarted or accelerated by heat treatment. A "trigger irradiation," i.e., a brief initial burst of radiation, is sufficient to start the curing process. Further curing then takes place in the subsequent dark reaction—outside of UV light. It may even be possible to create a certain "open time," meaning that the open adhesive layer is initially irradiated, and there is still time to bond it to the second substrate without compromising the final bond properties. This approach would then allow the bonding of substrates that are not UV-transparent.

[0018] WO 2017 / 174303 A1 discloses a self-adhesive, radiation-activated adhesive tape consisting of a radiation-activated polymerizable composition comprising: 5 to 60 parts by weight of at least one polyurethane polymer film-forming component; 40 to 95 parts by weight of at least one epoxy component; 0.1 to 10 parts by weight of at least one photoinitiator; and optionally 0.1 to 200 parts by weight of at least one additive, each based on the radiation-activated polymerizable composition, wherein the parts by weight of components A and B are complementary to 100.

[0019] WO 2018 / 153985 A1 discloses a windable and die-cuttable adhesive film with a UV-activated epoxy-based adhesive, the adhesive comprising: 2-40 wt.% film formers; 10-70 wt.% aromatic epoxy resins; cycloaliphatic epoxy resins, wherein the cycloaliphatic epoxy resins do not exceed 35 wt.%; 0.5-7 wt.% cationic initiators; 0-50 wt.% epoxidized polyether compounds; and 0-20 wt.% polyol, wherein the proportions add up to 100%.

[0020] JP 4 611463 B2 shows a UV-activated adhesive film which changes color during UV cross-linking.

[0021] WO 2018 / 008742 A1 shows a heat-activated epoxy adhesive which contains a monoazo pigment and changes color during heat crosslinking.

[0022] EP 0 889 16 A1 discloses a method for fixing a joining partner to a glass surface using an adhesive which is a product of UV crosslinking.

[0023] DE 10 2011 013 645 A1 shows an epoxy resin system which includes a dye which, during the curing of the epoxy resin system, indicates the progress or the endpoint of the curing of the epoxy resin by changing color.

[0024] In general, industrial requirements for adhesive bonds are constantly increasing, for example, regarding breaking strength, temperature resistance, resistance to climate changes, and resistance to moisture and heat. This is due to the increasing use of adhesive tapes in ever-larger quantities in automotive manufacturing, for example, for weight reasons, or because they do not necessarily require point-like connections, but rather a uniform distribution of the joining force across an adhesive seam, and not least because the joining partners are not damaged, as is the case with certain other joining methods such as screwing or riveting.

[0025] In many processes, for example in the automotive industry, the activation or curing of the adhesive / tape must be ensured and verified by the manufacturer. Accordingly, there are high demands on process control when processing these adhesives.

[0026] UV-activated liquid adhesives can provide a solution, as they are able to indicate activation by changing color. For example, EP 3 105 276 B1 describes an irreversible color change of an epoxy adhesive from blue to yellow.

[0027] Also known is the bathochromic effect, also called redshift, which describes a color shift. This involves a shift of the absorption spectrum towards the longer-wavelength, lower-energy region of the electromagnetic spectrum (see K. Schwetlick: Organikum. 15th edition, VEB Deutscher Verlag der Wissenschaften, Berlin 1976, pp. 513f.).

[0028] This color shift can also be produced by the halochrome effect ("salt coloration"), which describes the color change of a substance depending on the charge state of its molecules. An example of this is litmus, which changes color from red (acidic) to blue (basic) depending on the pH value of an aqueous solution.

[0029] Currently, existing systems can only detect the activation of liquid adhesives. Therefore, there is a need to make such process control available for structural adhesive films as well. Furthermore, in addition to determining the start of activation, process control also requires determining the point at which sufficient curing has occurred. Description of the invention

[0030] Starting from the known state of the art, it is an object of the present invention to provide a winding and die-cuttable adhesive film which, after activation by means of UV radiation, has a color change as an indicator of activation and a further color change after curing, thus enabling process control, and to provide a corresponding method for producing such a film.

[0031] The problem is solved by a wrapable and die-cuttable adhesive film with the features of claim 1. Advantageous further developments are described in the dependent claims.

[0032] Accordingly, a rollable and die-cuttable adhesive film is proposed, comprising a UV-activated epoxy-based adhesive. According to the invention, the adhesive comprises an incorporated dye or pigment to produce a first color change after activation of the adhesive and a second color change after curing of the adhesive.

[0033] This enables in-process control, which, in addition to indicating the start of adhesive activation, also color-codes the progress of the crosslinking reaction, thus visualizing the curing status. The prior art is silent regarding a UV-activated adhesive film based on epoxy resin adhesives, where, apart from the cationic photoinitiator, no further initiator is required as a radical starter for activation, and which, upon the addition of a dye or pigment, exhibits a color change after activation that can serve as process control.

[0034] The open time, storage time and curing speed of the adhesives used are not affected by the addition of appropriate dyes or pigments.

[0035] This adhesive film allows for complete process control of UV activation via color change during the joining process of various UV-activated adhesive applications. For example, by adding the dye Sudan Blue, a blue-colored adhesive can be produced, which changes to a pinkish-purple hue after UV activation. After approximately 24 hours, the adhesive's color shifts back towards blue, due to the degradation or reaction of the acid contained in the adhesive. This gives the user control over the activation and reactivity state of the adhesive film.

[0036] The adhesive can be processed and coated using a solvent or hot melt process. Processing and coating are also possible using so-called syrup technology, in which the film-forming component is built up from monomers or oligomers during the coating process.

[0037] The adhesive film is self-adhesive in its unactivated state and can therefore be processed like a "normal" pressure-sensitive adhesive tape; that is, it can be easily applied and repositioned if necessary. Die-cut parts can be produced from the tape, which can be activated by UV light before application to the respective parts to be bonded, in order to create a (semi-)structural bond after cross-linking.

[0038] Release liners are typically a component of adhesive tapes. In principle, all commonly known types of release liners can be used.

[0039] The curing of the adhesive tapes and die-cut parts is finally activated by UV light, preferably UVA or UVC light. Only then are the components permanently and structurally joined. Since the curing reaction occurs in several steps, there is still a certain period of time after activation during which the components can be finally aligned and joined; further activation after the initial curing by UV light is no longer necessary.

[0040] The duration of the dark reaction depends heavily on various factors, such as the resin component used (cycloaliphatic or aromatic epoxy resin), the chain length, the initiator type, the irradiation time, the irradiation dose (UV wavelength), and the temperature. Depending on these factors and their interaction, the curing time after irradiation can range from 10 seconds to 60 minutes.

[0041] Between 0.001 and 0.2 wt%, preferably 0.01 to 0.07 wt%, and particularly preferably 0.015 to 0.04 wt% of the dye or pigment are mixed into the adhesive. At concentrations below 0.001 wt%, the coloration of the adhesive is no longer reliably detectable visually. At concentrations above 0.2 wt%, the dye or pigment and its amine groups or nitrogen compounds create a basic environment, which prevents a reaction of the superacid with the epoxide groups and an azo group.

[0042] In a non-inventive embodiment, the dye or pigment is an azo dye or an azo pigment. The dye or pigment undergoes a color change upon exposure to an acid. Examples of azo dyes are methyl red, methyl orange, Congo red, and alizarin yellow R. In this non-inventive embodiment, dyes or pigments of the azo group are responsible for the color change. They change color upon protonation when certain pH values ​​are undershot. By way of example, the azo dye methyl red is shown below, which exists in acidic media as red and in its protonated form (right-hand structure shown below) and in basic media as yellow and in its deprotonated form (left-hand structure shown below).

[0043] Under the influence of increased humidity, the color change is less pronounced because the resulting acid particles preferentially bind to the OH ions of the water and thus less to the dye or pigment. At the same time, in these cases the cured adhesive tape is less tightly cross-linked, which is reflected in lower tensile strength and simultaneously greater elongation at break.

[0044] In a further preferred embodiment, the adhesive comprises: a. 2–50 wt.% film formers, b. 10–70 wt.% aromatic epoxy resins, c. 0.5–7 wt.% cationic initiator, d. 0.001–0.2 wt.% Sudan Blue, e. cycloaliphatic epoxy resins, wherein the cycloaliphatic epoxy resins do not exceed 35 wt.%, f. 0–50 wt.% epoxidized polyether compounds, and g. 0–20 wt.% polyol. where the shares add up to 100%.

[0045] After UV activation, the adhesive has an open time of 10 seconds to 60 minutes, during which the film is adhesive before it finally hardens completely and reaches its final strength.

[0046] In a preferred further training method, the adhesive film is available as a carrier-free, UV-activated transfer adhesive tape.

[0047] In a preferred further development, the adhesive film comprises different adhesive systems, at least one of which is a UV-activated system.

[0048] In a preferred further development, the adhesive film comprises a UV-transparent or UV-opaque carrier.

[0049] In a preferred embodiment, the adhesive film comprises at least one UV- or thermally activatable adhesive.

[0050] In a preferred embodiment, the wound and die-cuttable adhesive film is particularly suitable for the structural bonding of metals, glass, ceramics, glass fiber reinforced plastic (GFRP), carbon fiber reinforced plastic (CFRP) and other higher energy surfaces.

[0051] In a further preferred embodiment, the wound and die-cuttable adhesive film exhibits bond strengths between 6 and 20 MPa, depending on formulation details, radiation dose and substrates to be bonded.

[0052] In a further preferred embodiment, the winding and die-cuttable adhesive film is suitable for (semi-)structural bonding of plastics and other low-energy surfaces. Brief description of the characters

[0053] Preferred further embodiments of the invention are explained in more detail by the following description of the figures. These show: Figure 1Schematic representation of a UV-activated adhesive before activation Figure 2 schematically a UV activation of the UV-activatable adhesive compound Figure 1 ; Figure 3 schematically, a color change of the UV-activated adhesive immediately after activation; and Figure 4 schematically depicts a color change of the UV-activated adhesive 24 hours after activation. Detailed description of preferred embodiments

[0054] The following describes the production of an adhesive film and its UV activation with reference to the accompanying figures. Test specimens were produced using the manufacturing process described herein. These specimens were subjected to various tests to evaluate their properties. The results of these tests are also explained in more detail below.

[0055] The adhesive has the composition described above.

[0056] In Figure 1A UV-activatable adhesive 1 is schematically represented. The adhesive 1 comprises the following composition: a. 2–50 wt.% film formers, b. 10–70 wt.% aromatic epoxy resins, c. 0.5–7 wt.% cationic initiator, d. 0.001–0.2 wt.% dye or pigment, e. cycloaliphatic epoxy resins, wherein the cycloaliphatic epoxy resins do not exceed 35 wt.%, f. 0–50 wt.% epoxidized polyether compounds, and g. 0–20 wt.% polyol. where the shares add up to 100%.

[0057] After UV activation, the adhesive has an open time of 10 seconds to 60 minutes, during which the film remains adhesive.

[0058] In a non-inventive embodiment, the dye or pigment is an azo dye or an azo pigment, and in particular azo substances that exhibit a color change upon contact with acid. The dye according to the invention is listed in the table below: Table 1 Bold Blue B01 Blue anthraquinone dye from Clariant Products (Germany) GmbH

[0059] A color change after UV or thermal activation occurs at addition amounts between 0.001 and 0.2 wt% of the dye or pigment. At concentrations below 0.001 wt%, the coloration of the adhesive is no longer reliably detectable visually; at concentrations above 0.2 wt%, the dye or pigment and its amine groups or nitrogen compounds create a basic environment that prevents a reaction of the superacid with the epoxide groups and the azo group.

[0060] The experiments revealed a preferred range of 0.01 to 0.07 wt% and particularly preferably 0.015 to 0.04 wt% of the dye or pigment.

[0061] Under the influence of increased humidity, the color change is less pronounced because the resulting acid particles preferentially bind to the OH ions of the water and thus less to the dye or pigment. At the same time, in these cases the cured adhesive tape is less tightly cross-linked, which is reflected in lower tensile strength and simultaneously greater elongation at break.

[0062] The solvent-based adhesive is applied to a siliconized polyester film (50 µm thick) using a squeegee. The film is then dried for 10 minutes at room temperature and subsequently for 10 minutes at 80°C in a convection oven. The amount of adhesive applied is adjusted so that, after drying (removal of the solvent mixture), a tacky film approximately 150 µm thick remains.

[0063] No protective measures against UV light are necessary for handling the raw materials, the adhesive, or the coating. It is sufficient to work in a normal laboratory environment, away from the UV lamp. No further shielding is required.

[0064] Figure 2 Figure 1 schematically shows the UV activation of the UV-activatable adhesive 1 using a UV source 2. The UV source can be, for example, UV-C light from a discharge lamp or UV-A light from a UV-A LED source.

[0065] Experiments with a UV-C lamp are conducted using a Beltron UV laboratory system with a conveyor belt and a UV-C emitter with a radiation maximum at 256 nm. The conveyor belt operates at 2 m / min. The irradiation dose in the UV-C range, measured with a UV Power Puck II from EIT Instrument Market Group, is 197 mJ / cm².

[0066] Alternatively, the adhesives can also be activated with a UV-LED system, despite a significantly higher wavelength. Similar irradiation times are possible as with the UV-C system, and the results in terms of open time and bond strength are comparable.

[0067] Tests with a UV-LED system are conducted using a Hönle LED Spot Lamp 100, which includes a UV LED (wavelength 365 nm) and an irradiation chamber. The test specimens are irradiated in the chamber for 15 seconds. The irradiation dose, measured with a UV Power Puck II from EIT Instrument Market Group, is 5000 mJ / cm².

[0068] Figure 3 The adhesive mass 1 shows the color change after an initial color change triggered by UV activation.

[0069] In Figure 4 The diagram schematically shows the color change of a UV-activated adhesive 1 24 h after activation. This adhesive has reacted to the degree of cross-linking in relation to the temperature present during cross-linking.

[0070] The terms open time, time to handling strength and curing time are explained in more detail below.

[0071] Open time refers to the maximum possible duration between removal from the irradiation strip (UV-C) or removal from the irradiation chamber (UV-A) and the point at which the parts are joined to the second substrate. The open time is defined as the period during which the adhesive layer remains tacky. It is determined by testing the tackiness of the adhesive film's surface with a finger after irradiation. Immediately after irradiation, the adhesive film is still tacky. After a certain time, a noticeable decrease in tackiness can be observed, which then rapidly declines until the surface is tack-free. The open time is defined as the point at which the tackiness noticeably decreases, such that no tack remains.

[0072] It turns out that as long as the surfaces are still tacky, joining is possible and the subsequent curing leads to a homogeneous adhesive bond. As soon as the surfaces lose their tack, the curing process has progressed so far that joining is no longer possible. This is then reflected in significantly reduced strength values, measured by the quasi-static tensile shear strength.

[0073] Additionally, the activation of these adhesive films can be detected using a novel color change, and the open time can be determined by observing the further change in color after activation. The adhesive films are joined immediately after UV activation. Curing time:

[0074] The curing time is the period between bonding and final strength. All example formulations are fully cured after a maximum of 24 hours. Therefore, a 24-hour waiting period was usually observed before measuring the quasi-static tensile shear strength. A value above approximately 6 MPa indicates structural strength or structural bonding. The added dye or pigment allows the color of the formulation to be used to determine whether it has fully cured. This state is reached in Figure 4 shown. The adhesive compound 1 has reacted with respect to the degree of cross-linking in relation to the temperature present during cross-linking.

[0075] Sufficient open time is desired for the application. Rapid handling strength is also advantageous if the bond needs to withstand initial stress soon after joining (e.g., during transport of the parts), or to eliminate the need for clamping the parts. However, 24 hours is sufficient for complete curing, as experience has shown that the bond is only subjected to final stress (continuous or shock load) after this time.

[0076] Open time and curing time are determined by the reaction rate of the curing process. This reaction begins with UV activation and ends with the complete curing of the adhesive film. Curing is complete when the final strength of the adhesive bond is achieved. During the open time and curing time, various phases with different reaction rates can occur; delays and accelerations can happen, resulting in a specific overall open time and curing time. Open time and curing time can be controlled by the formulation, the type, intensity, and duration of UV irradiation, and by the thermal management (temperatures) during the bonding process.

[0077] The time to handling strength refers to the period after joining until the bond strength is high enough for the glued parts to be transported and further processed. Experience shows that handling strength is reached when the quasi-static tensile shear strength reaches 2 MPa. This strength provides sufficient margin for the stresses encountered in an industrial manufacturing process. Testing methods d) Color change

[0078] The color change is visually recorded and documented with photographs. This ensures immediate recording after activation. The specified color tone corresponds to the perception of five different test subjects. b) Quasi-static tensile shear test

[0079] Tensile shear tests according to DIN EN 1465 (2009) are performed to determine the strength of the bond to GRP at 23°C ± 2°C and 50% ± 5% relative humidity with a test speed of 2 mm / min. The substrates are cleaned with isopropanol and then joined. Curing is achieved by irradiation with UV light, and the mechanical test is performed 24 hours after activation. The results are given in MPa (N / mm²). The mean value of five measurements, including the standard deviation, is given in each case. c) Peeling test

[0080] The peel resistance of cured adhesive tapes on glass is determined according to DIN EN 1939 (1996) at 23°C ± 2°C and 50% ± 5% relative humidity with a test speed of 100 mm / min and a peel angle of 90°. The samples are cured using UV light and tested 24 hours after activation. The results are given in N / mm. The mean value of the peel resistance from five measurements, including the standard deviation, is given. d) Pull test

[0081] As a characteristic parameter for the strength of the pure adhesive film in the cured state, tensile tests are carried out in accordance with DIN EN ISO 527 (2012) at 23°C ± 2°C and 50% ± 5% relative humidity at a test speed of 10 mm / min. For this purpose, strips with a width of 19 mm and a length of 100 mm are cut from cured adhesive films. The layer thickness in the results shown is 0.2 mm. The samples are cured using UV light and tested 24 hours after activation. The results are given in MPa (N / mm²). The mean value of five measurements, including the standard deviation, is given in each case. Examples

[0082] Table 2 summarizes examples of compositions with regard to the selection of dyes or pigments, where the quantities are given in parts by weight. K1 is a formulation according to the invention. V1 is an adhesive transfer film without the addition of a dye or pigment. Table 2 Example: K1 K2 K3 K4 V1 Adhesive (KM) KM 1 KM 1 KM 1 KM 1 KM 1 Bold Blue B01 0,02 0,01 Orasol Yellow 081 0,02 0,02 Heliogen Green L8730 0,19

[0083] Table 3 summarizes the results of the tensile shear, tensile and peel tests as well as the color change. Table 3 Example: K1 K2 K3 K4 V1 Tensile shear strength [MPa] 6.8 ± 1.0 (CF) 7.1 ± 0.7 (CF) 7.7 ± 0.9 (CF) 0.3 ± 0.1 (AF) 6.7 ± 1.0 (AF / CF) Peeling resistance [N / mm] 0.73 ± 0.02 (AF) 0.58 ± 0.12 (AF) 0.44 ± 0.03 (AF) Not measurable 0.79 ± 0.06 (AF) Tensile strength [MPa] 1,9 ± 0,1 1,6 ± 0,1 1,7 ± 0,1 Not measurable 2,1 ± 0,5 Color change immediately after activation (visual) From cyan blue to pinkish-purple From green to colorless No color change No color change No color change Legend: AF: Adhesive fracture; CF: Cohesive fracture

[0084] The adhesive films K1, K2, K3, K4 and V1 each contain the same UV-activated adhesive. Only the respective dye or pigment was varied to highlight differences in the colorant selection.

[0085] The adhesive films according to formulations K1, K2, K3, and V1 do not differ significantly in tensile shear strength or tensile strength within the standard deviation. This demonstrates that the use of the colorant or pigment for activation or curing control has no negative impact on these mechanical properties. Similarly, the peel resistance of the adhesive films according to K1 and V1 shows no significant differences within the standard deviation. The peel resistances of formulations K2 and K3 are slightly lower, which is attributed to the influence of the yellow dye.

[0086] K4 shows no measurable tensile strength or peel resistance; the tensile shear strength is at the level of the uncured adhesive film. Thus, the upper concentration of the dye or pigment could be confirmed.

[0087] Table 4 shows the different conditioning methods used to prepare the adhesive films before activation. In example K5, the adhesive was stored without direct exposure to moisture on the bonding surface. In example K6, the adhesive was conditioned for one hour at a relative humidity of 70% and then activated. Table 4 Example: K5 K6 Adhesive (KM) KM 1 KM 1 Bold Blue B01 0,02 0,02 Temperature [°C] 23 ± 2 23 ± 2 Relative humidity [%] Without direct moisture access to the adhesive surface 70 ± 5

[0088] Table 5 summarizes the results of the tensile tests and the color change immediately after activation. Table 5 Example: K5 K6 Tensile strength [MPa] 1,4 ± 0,1 0,8 ± 0,1 Elongation at break [%] 200 ± 10 400 ± 40 Color change immediately after activation (visual) From cyan blue to pinkish-purple From cyan blue to light blue

[0089] The tensile strengths of the adhesive films K5 and K6 differ within the standard deviation with respect to tensile strength and elongation at break. The elongation at break of the adhesive film stored for one hour under elevated humidity is twice as high at 400%. The tensile strength of the adhesive film stored without direct exposure to moisture is approximately 0.6 MPa higher compared to the adhesive film conditioned at 70% relative humidity. The difference in color change is also significant. For adhesive film K5, a color change from cyan blue to pinkish-purple was detected immediately after activation, whereas for K6, only a color change from cyan blue to light blue was observed under elevated humidity.

[0090] Thus, the influence of the surrounding humidity on the color change and the tensile strength or elongation at break could be demonstrated.

[0091] Where applicable, all individual features shown in the exemplary embodiments can be combined and / or exchanged without leaving the scope of the invention.

Claims

1. Windable and stampable adhesive film, comprising a UV-activatable adhesive mass based on epoxide, which comprises a cationic photoinitiator, and 0,001 to 0,2 wt% of sudan blue which is mixed into the adheisve mass for creating a frist color change after the activation of the adhesive mass and a second color change after the curing of the adhesive mass.

2. Windable and stampable adhesive film according to claim 1, characterized in the adhesive mass further comprising: a. 2 - 50 wt% film former, b. 10 - 70 wt% aromatic epoxy resins, c. 0,5 - 7 wt% cationic initiator, d. 0,001 - 0,2 wt% sudan blue e. cycloaliphatic epoxy resins, wherein the cycloaliphatic epoxy resins constitute at most 35 wt% f. 0 - 50 wt% epoxidized polyether compounds, and g. 0 - 20 wt% polyol, wherein the components add up to 100%.

3. Windable and stampable adhesive film according to one of the preceding claims, characterized in that the adhesive film is a carrier-less UV-activatable transfer tape.

4. Windable and stampable adhesive film according to claim 3, characterized in that the adhesive film comprises different adhesive systems, of which at least one is a UV-activatable system.

5. Windable and stampable adhesive film according to claim 1 or 2, characterized in that the adhesive film comprises a UV-transparent or UV-intransparent carrier.