Double-sheathed hollow fiber coupler and method for manufacturing such a coupler

The double-clad hollow-core optical fiber coupler addresses inefficiencies in non-linear endoscopes by using a glass transition temperature lower than the damage temperature, ensuring reliable optical coupling and efficient light transmission and signal collection, enhancing the performance of non-linear endoscopes.

FR3141774B1Active Publication Date: 2024-10-25LIGHTCORE TECH +2
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
FR2022011428
Authority / Receiving Office
FR · FR
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-11-03
Publication Date
2024-10-25
Estimated Expiration
2042-11-03

AI Technical Summary

Technical Problem

Conventional non-linear endoscopes using double-clad hollow core fibers face limitations in reliability due to the misalignment of dichroic mirrors and the inability to optimize objectives for both light injection and signal collection, leading to inefficient performance in clinical environments.

Method used

A double-clad hollow-core optical fiber coupler is developed using a first fiber with a hollow core and highly multimode internal sheath, coupled with a second fiber made of glass with a lower glass transition temperature, allowing for optical coupling without damaging the core, and eliminating the need for dichroic mirrors.

Benefits of technology

The coupler enhances mechanical stability and reliability, enabling efficient non-linear imaging with improved robustness and efficiency in non-linear endoscopes by optimizing light transmission and signal collection without the use of dichroic plates.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000022_0000
    Figure 00000022_0000
  • Figure 00000022_0001
    Figure 00000022_0001
  • Figure 00000022_0002
    Figure 00000022_0002
Patent Text Reader

Abstract

This description relates, in one aspect, to a coupler (400) comprising: a first double-clad hollow-core optical fiber (430) including a hollow core (431) configured for guiding light in a first wavelength range and having a given damage temperature, and a highly multimode inner cladding (435) configured for guiding light in a second wavelength range; a second optical fiber (460) including a highly multimode glass guiding portion (461) configured for guiding light in a third wavelength range, the glass having a glass transition temperature lower than the damage temperature; and an optical coupling zone (401) between the first and second fibers generated by fusion between a region of the inner cladding of the first fiber and a region of the glass guiding portion of the second fiber. FIG. 2A
Need to check novelty before this filing date? Find Prior Art

Description

Title of the invention: Double-sheathed hollow fiber coupler and method for manufacturing such a coupler technical field

[0001] This description relates to a double-sheathed hollow fiber coupler and a method for manufacturing such a coupler. This description also relates to an endoscope comprising such a coupler. State of the art

[0002] Invasive cancers are the leading cause of death in developed countries and the second leading cause in developing countries. These figures are increasing due to aging populations and the homogenization of lifestyles. The development of non-invasive optical tools for cancer diagnosis and prognosis is therefore of paramount importance.

[0003] A major challenge arises from the fact that most tissue lesions are located deep within tissues (lungs, stomach, liver, colon) and remain inaccessible to conventional optical imaging techniques. To overcome current technological limitations, non-invasive optical imaging tools have been developed for the rapid detection of metabolic and morphological changes in tissues.

[0004] In particular, it is known [Ref. 1] to combine the advantages of non-linear imaging techniques with those of the minimally invasive endoscopic technique. Non-linear imaging techniques include, in particular, second harmonic generation (SHG for "Second Harmony Generation"), third harmonic generation (THG for "Third Harmony Generation"), two-photon excited fluorescence (2PEF for "2 photons excited fluorescence"), three-photon excited fluorescence (3PEF for "3 photons excited fluorescence"), and coherent anti-Stokes Raman scattering (CARS for "Coherent Anti-Stokes Raman Scattering"). One objective is therefore to develop an endoscope adapted to non-linear imaging, or "non-linear endoscope", minimally invasive, with performance close to that of massive non-linear microscopes (i.e. non-endoscopic), and ideally multimodal, i.e. combining several non-linear imaging modalities in the same device.

[0005] For this purpose, the endoscopic optical fiber must be optimized on the one hand to deliver short, high-optical-power light pulses to the biological tissue, so as to obtain a non-linear response from the tissue, and on the other hand to efficiently collect the non-linear signal generated by the tissue and deliver it to the detection chain.

[0006] The intrinsic dispersive and nonlinear properties of core optical fibers solid materials make these unsuitable for this problem.

[0007] A few years ago, double-sheathed hollow-core fibers were described for use in a nonlinear endoscope. See [Ref. 2]. Double-sheathed hollow-core fibers are known to exhibit low dispersion and low nonlinearity, which are suitable for transmitting short, intense pulses.

[0008] Fig.1A schematically represents a nonlinear endoscope as implemented in [Ref.2] and Fig.1B represents a double-sheathed hollow core fiber.

[0009] A double-clad hollow-core fiber as described herein generally comprises a hollow core 131 at the periphery of which is a microstructured portion, for example made of air and glass, for example formed by capillaries 132, as illustrated in [Fig. 1B]. The microstructured portion allows, for example, the guidance of light within the hollow core for the transmission of pulses to the biological sample to be analyzed. The double-clad hollow-core fiber further comprises a double sheath with an inner "guiding" sheath 135, i.e., one designed to guide the light. The role of the inner sheath, in the example of the endoscope illustrated in [Fig. 1A], is to collect the non-linear signal generated in the sample. For example, the double sheath comprises an inner glass sheath 135 and may include, as illustrated in [Fig.lB], an outer sheath 137 of low index, that is to say with a lower refractive index than the inner sheath, for example a sheath made of low index polymer. Note that the double sheath can also include an inner sheath surrounded by air to ensure its function of guiding light.

[0010] The nonlinear endoscope shown in [Fig. 1A] comprises a dichroic mirror 11 that transmits pulses emitted by a laser source 10 to the double-clad hollow-core fiber 13, typically infrared pulses. An objective 12, for example a lens or a microscope objective, allows the injection of the pulses into the core of the fiber 13. The dichroic mirror 11 reflects the nonlinear signal resulting from the interaction of the pulses with the biological sample 100, which propagates in the counter-propagating direction within the inner sheath 135 of the fiber 13, to redirect it to a detector 15 of a detection chain. The double-clad hollow-core fibers described in [Ref. 2] enabled the demonstration of the first multimodal Raman endoscope.

[0011] However, the overall performance of the nonlinear endoscope described above remains limited, particularly in terms of reliability, which prevents its use in clinical settings and confines it to specialized biophotonics laboratories. One of the limitations concerns the use of the dichroic mirror 11 placed at the entrance of the optical fiber 13. Indeed, the alignment of the free-space mirror changes with the time. Furthermore, the signal collected in the double sheath must be redirected to the detection chain by passing through the same objective 12 that was used to inject the short pulses into the central hollow core. However, the hollow core 131 and the inner sheath 135 have very different numerical apertures (NA) (0.02 versus 0.5). In addition, the two beams, transmitted and reflected, have very different wavelengths, typically a factor of 2 or 3 depending on the imaging modalities, with the transmitted pulses being in the infrared while the nonlinear signal is in the visible. For these reasons, the objective used for injection and collection cannot be simultaneously optimized for both beams, severely limiting the overall efficiency of the system.

[0012] In the field of endoscopy, a double fiber coupler is known [Ref. 3]. The coupler is made by heating and stretching two segments of two double-sheathed silica fibers to fuse them locally, thus achieving optical coupling between the two fibers. Such a doubler eliminates the need for a dichroic plate.

[0013] However, the inventors have shown that the described method is not suitable for coupling a double-clad hollow-core fiber. Indeed, the fusion requires heating the fibers to such an extent that it would inevitably cause the central hole forming the fiber core to close due to the surface tension at the interface between the glass forming the inner cladding and the air in the central core. Furthermore, the heating required for fusion would cause the capillaries to close upon themselves (or "hole collapse").

[0014] An object of the present description and a coupler adapted to a double-sheathed hollow fiber and a method for making such a coupler. Summary of the invention

[0015] In the present description, the term "include" means the same as "include" or "contain", and is inclusive or open and does not exclude other elements not described or represented.

[0016] In addition, in the present description, the term "approximately" or "substantially" is synonymous with (means the same as) a lower and / or upper margin of 10%, for example 5%, of the respective value.

[0017] According to a first aspect, the invention relates to a double-clad hollow-core optical fiber coupler comprising: - a first double-clad hollow-core optical fiber comprising: - a hollow core configured for guiding light in a first range of wavelengths and comprising a given damage temperature; and - a highly multimode inner sheath, configured for guiding light in a second wavelength range; - a second optical fiber comprising a strongly multimode guiding glass portion, configured for guiding light in a third wavelength range, the glass comprising a glass transition temperature lower than the damage temperature; - a fusion zone between a region of the inner cladding of the first fiber and a region of the glass guiding part of the second optical fiber allowing optical coupling between the first fiber and the second optical fiber.

[0018] A double-clad hollow-core fiber in a coupler according to the first aspect is described, for example, in [Ref. 4], [Ref. 5], [Ref. 6], [Ref. 7]. The hollow core generally comprises a core containing a gas, for example, air or a vacuum, and at the periphery of which is a microstructured portion, for example, made of air and glass. The core is single-mode or weakly multimode, i.e., capable of propagating one or a few modes, at most about 10 modes. The hollow core is configured for guiding light in a first wavelength range. For example, for endoscopy applications, the first wavelength range is between about 700 nm and about 1800 nm.

[0019] The double-clad hollow-core fiber in a coupler according to the first aspect further comprises a highly multimode inner cladding, i.e., an inner cladding capable of propagating from several hundred to several tens of thousands of modes, for example, between 100 and 100,000. It is configured for guiding light in a second wavelength range. For example, for endoscopy applications, the second wavelength range is within the transparency band of the glass that constitutes the inner cladding of the double-clad hollow-core fiber, for example, between approximately 350 nm and approximately 2400 nm for a silica double cladding.

[0020] The double-clad hollow-core fiber in a coupler according to the first aspect is further characterized by a hollow-core damage temperature (or darkening temperature). In this description, the damage temperature is defined as the temperature at which the optical power of a light beam transmitted through the hollow core ("transmitted optical power") falls below a predetermined threshold relative to the transmitted optical power measured under the same conditions but at room temperature. According to one or more embodiments, the predetermined threshold is greater than approximately 1%, advantageously greater than approximately 5%. For example, the predetermined threshold is approximately 10%.For known state-of-the-art double-clad hollow-core silica glass fibers, the applicants have shown that the damage temperature is between approximately 1000°C and approximately 1600°C for a damage threshold chosen at 10% of the maximum power.

[0021] The guiding glass portion of the second optical fiber is highly multimode. It is configured for guiding light in a third wavelength range. For example, for endoscopy applications, the first wavelength range is between approximately 380 nm and approximately 2200 nm.

[0022] In a coupler according to the first aspect, the glass of the guiding glass portion of the second optical fiber comprises a glass whose glass transition temperature is lower than the damage temperature of the hollow core of the first double-clad hollow-core fiber. The applicants have shown that this condition makes it possible to implement a double-clad hollow-core fiber coupler.

[0023] The glass transition temperature (also called the softening temperature) can be routinely measured using the differential scanning calorie technique, as described, for example, in [Ref. 8]. A condition for selecting the glass for the guiding glass portion of the second optical fiber is therefore that its glass transition temperature, measured, for example, by differential scanning calorie, be lower than the damage temperature defined above.

[0024] The applicants have shown that a silica multimode optical fiber, generally used for a fiber coupler, is not suitable for a coupler according to the first aspect because the glass transition temperature of silica is about 1600°C, which is on the order of the core damage temperature of double-clad hollow-core fibers, or higher.

[0025] A second optical fiber adapted for a coupler according to the first aspect is, for example, an optical fiber with a borosilicate glass guiding portion. Borosilicate glasses comprise a set of chemical compounds including, in particular, silica (SiO2), boron trioxide (B2O3), alumina (Al2O3), and alkali oxides (Na2O+K2O) [Ref.9]. The glass transition temperature of borosilicate glasses is approximately 820°C. A borosilicate glass that could be used, for example, is Simax glass® (see https: / / www.pegasus-glass.eom / Portals / 0 / technical_info.pdf) or Pyrex®.

[0026] In general, however, any glass whose glass transition temperature is lower than the damage temperature of the core of the double-clad hollow core fiber can be chosen.

[0027] In a coupler according to the first aspect, the applicants have shown that a fusion zone between the region of the inner cladding of the first fiber and the region of the glass guiding part of the second optical fiber can be obtained to allow optical coupling between the first fiber and the second optical fiber without damaging the double-clad hollow-core fiber.

[0028] Optical coupling in the present description includes a transfer of light energy between the first fiber and the second fiber.

[0029] According to one or more embodiments, the coupler in the first aspect further comprises a low-index outer cladding covering, in a region that includes the fusion zone, the inner cladding of the first fiber and the glass guide portion of the second optical fiber. Such an inner cladding has a low index, that is, a lower index than the inner cladding of the first fiber and the refractive index of the glass guide portion of the second optical fiber. In particular, it provides mechanical protection for the region.

[0030] According to one or more embodiments, the outer sheath is formed from acrylate polymer.

[0031] According to a second aspect, the present description includes an endoscope configured for nonlinear imaging comprising: - a source of ultra-short light pulses; - a detector; - a double-clad hollow-core optical fiber coupler according to any one of the preceding claims; wherein: - the hollow core of the first optical fiber is configured to carry said light pulses to a biological sample to be imaged, and the inner cladding of the first optical fiber is configured to carry an optical signal resulting from a nonlinear interaction of the pulses with the biological sample; and - the guiding glass part of the second optical fiber optically coupled with the first optical fiber is configured to direct said optical signal towards the detector.

[0032] In the present description, ultra-short pulses are understood to mean pulses of duration less than about 1 ps, advantageously less than about 200 fs.

[0033] The applicants have shown that a non-linear endoscope according to the second aspect, equipped with a coupler according to the first aspect, exhibits much better mechanical stability and robustness than a state-of-the-art endoscope, for example an endoscope as described in [Ref. 2], particularly in terms of reliability, because it does not require the use of a dichroic blade.

[0034] Although the coupler according to the first aspect is particularly well suited to a nonlinear endoscope as described according to the second aspect, other applications are possible. For example, a coupler according to the first aspect could be used with a reflector-type optical sensor with environmentally influenced reflection properties. Such a sensor could be arranged in the distal part of the double-clad hollow-core fiber. The incident light could be carried through the hollow core of the double-clad hollow-core fiber, and the reflected light carried through the inner cladding of the double-clad hollow-core fiber and then through the glass portion. guiding the second optical fiber to be routed to a detector.

[0035] In a third aspect, the present description relates to a method of manufacturing a coupler according to the first aspect.

[0036] More generally, the present description relates to a method for manufacturing a double-clad hollow-core optical fiber coupler comprising: - the provision of a first double-clad hollow-core optical fiber comprising - a hollow core configured for guiding light in a first range of wavelengths and comprising a given damage temperature; and - a double sheath comprising a strongly multimode inner sheath, configured for guiding light in a second wavelength range and an outer sheath; - the provision of a second optical fiber comprising a strongly multimode guiding glass portion, configured for guiding light in a third wavelength range, the glass comprising a glass transition temperature lower than the damage temperature, and an outer sheath; - the local stripping of said first optical fiber and the local stripping of the second optical fiber for the removal, in a given stripping zone, of the outer sheath of the first fiber and the outer sheath of the second fiber; - heating, in said stripping zone, of a first region of the inner cladding of the first optical fiber and of a second region of the glass guiding part of the second optical fiber to obtain locally a fusion of said first region and said second region and generate an optical coupling zone between the first fiber and the second optical fiber.

[0037] The process according to the first aspect makes it possible to manufacture a double-clad hollow fiber coupler without risking damage to the double-clad hollow core fiber, and this in particular thanks to the choice of the glass material used for the guiding part of the second optical fiber.

[0038] As described previously, according to embodiment examples, the guiding glass part of the second optical fiber is made of borosilicate glass.

[0039] According to exemplary embodiments, the inner cladding of the first optical fiber is made of silica glass. According to exemplary embodiments, the outer cladding of the first optical fiber is made of a low-index polymer, that is to say, a polymer with a lower refractive index than that of the inner cladding, for example, an acrylate polymer.

[0040] According to one or more embodiments, the second optical fiber comprises a glass core, an inner glass cladding with a refractive index lower than that of the core, and a low-index outer cladding with a refractive index lower than that of the core and the inner cladding. The guiding glass portion then consists of the core and the inner sheath. For example, the core and inner sheath are made of the same glass, for example, borosilicate glass, but with different compositions. For example, the low-index outer sheath is made of acrylate polymer with a lower index than borosilicate glass.

[0041] According to one or more embodiments, the second optical fiber comprises a glass core, an inner glass cladding with a refractive index lower than that of the core, and a high-index outer cladding with a refractive index higher than that of the inner cladding. The guiding glass portion is then formed by the core. For example, the high-index outer cladding is made of an acrylate polymer. For example, the core is made of borosilicate glass and the inner cladding of borosilicate glass with a refractive index lower than that of the core.

[0042] According to one or more embodiments, the second optical fiber comprises a glass core and a low-index outer cladding with a refractive index lower than that of the core. The guiding glass portion is then formed by the core. For example, the core is made of borosilicate glass. For example, the outer cladding is made of a low-index polymer, for example, an acrylate polymer.

[0043] According to one or more exemplary embodiments, heating is obtained by applying a beam of electromagnetic radiation, for example by emitting a laser beam, said beam covering said first region of the inner sheath of the first fiber and said second region of the guiding glass part of the second optical fiber.

[0044] The laser beam is for example a beam from a continuous or pulsed CO2 laser, emitting at a wavelength of about 10 pm.

[0045] Other means known to those skilled in the art are of course possible for obtaining the heat necessary for melting. For example, an electric arc between electrodes, a flame, a filament, etc., may be used.

[0046] The application of a laser beam is advantageous, however, in that it ensures repeatable performance and requires little maintenance, and also eliminates the instability due to the use of electrodes or filaments. Furthermore, by focusing the laser beam, it is possible to very precisely control the heating zone.

[0047] In practice, it will be possible to ensure that the stripping area is larger than the area in which the fusion is carried out in order to avoid damaging the unstripped regions of the outer sheath of the first optical fiber and the outer sheath of the second optical fiber.

[0048] According to one or more embodiments, the method according to the third aspect further includes clamping the first fiber and the second fiber together in a support mounted on a translating plate.

[0049] According to one or more embodiments, the process according to the third aspect includes, in addition: - the installation, at the stripping zone and after fusion, of an outer sheath covering the stripped part of the inner sheath of the first fiber and the stripped part of the glass guiding part of the second optical fiber, - the junction of said outer sheath with the outer sheath of the first optical fiber and the outer sheath of the second optical fiber. Brief description of the figures

[0050] Other advantages and features of the invention will become apparent from the description, illustrated by the following figures:

[0051] [Fig. 1 A], already described, represents a diagram illustrating a non-linear endoscope known from the state of the art;

[0052] [Fig. IB], already described, represents a diagram illustrating a known prior art double-clad hollow-core optical fiber;

[0053] [Fig.2A], represents a diagram illustrating a hollow-core optical fiber coupler double sheath according to an example conforming to this description;

[0054] [Fig. 2B], represents a diagram illustrating a nonlinear endoscope with a coupler double-clad hollow-core optical fiber, according to an example conforming to this description

[0055] [Fig.3A], represents a simplified top-view diagram illustrating, an assembly for implementing a manufacturing process for a double-clad hollow-core optical fiber coupler according to an example conforming to this description;

[0056] [Fig. 3B], represents a diagram illustrating in cross-sectional view and in a simplified manner, an element of the assembly illustrated in [Fig.3A];

[0057] [Fig.4A], represents a diagram illustrating an example of an optical fiber coupler hollow core with double sheath obtained by means of the assembly as illustrated in [Fig.3A] and [Fig.3B];

[0058] [Fig.4B], represents an image of the coupling zone between the first optical fiber and the second optical fiber, obtained by fusion, in an example of implementation;

[0059] [Fig. 5A] represents a simplified diagram of a first example of a second fiber optics with a strongly multimode guiding glass part, for implementing a manufacturing process for a coupler according to the present description;

[0060] [Fig. 5B], represents a simplified diagram of a second example of a second optical fiber with strongly multimode guiding glass part, for the implementation of a manufacturing process for a coupler according to this description;

[0061] [Fig. 6], represents cross-sectional images of examples of double-clad hollow-core fibers for the implementation of a method for manufacturing a coupler according to the present description;

[0062] [Fig.7A], represents a diagram illustrating in a simplified way an example of a setup for characterizing the damage temperature of a core of a double-clad hollow core fiber;

[0063] [Fig.7B], represents a diagram illustrating, by way of example, a power curve transmitted optics as a function of the applied temperature obtained by means of a setup for characterizing the damage temperature of a core of a double-clad hollow-core fiber as described in [Fig.7A];

[0064] [Fig.8A], shows comparative (experimental) curves illustrating, by way of example, the overlap obtained during fusion, between the region of the inner cladding of the first optical fiber and the region of the guiding glass part of the second optical fiber, as a function of the heating power applied (optical power) during the implementation of a manufacturing process for a coupler according to the present description, in the case where the second optical fiber is a silica optical fiber (in gray) and in the case where the second optical fiber is a Simax glas s ® optical fiber (in black);

[0065] [Fig.8B], comparative (experimental) curves illustrating, by way of example, the diameter of the hollow core of the double-clad hollow-core optical fiber, depending on the overlap obtained during fusion, between the region of the inner cladding of the first optical fiber and the region of the glass guiding part of the second optical fiber, when implementing a method for manufacturing a coupler according to this description, in the case where the second optical fiber is a silica optical fiber (in black) and in the case where the second optical fiber is a Simax glas s ® optical fiber (in grey);

[0066] [Fig.9A], an experimental curve showing the optical coupling obtained between the first optical fiber and second optical fiber, in an example of a coupler according to the present description, and for different wavelengths of light propagating in the coupler;

[0067] [Fig.9B], an SHG image of unlabeled mouse skin, obtained using a Example of a nonlinear endoscope according to this description, with an excitation wavelength of 920 nm and pulses of 200 fs at 80 MHz at a power of 20 mW; the scale bar is 50 pm. Detailed description of the invention

[0068] In the figures, the elements are not shown to scale for better visibility.

[0069] Figure 2A represents, for illustrative purposes, a diagram of a 400 double-clad hollow-core optical fiber coupler according to an example conforming to this description, hereinafter referred to as "HC-DCFC" according to the expression Anglo-Saxon "Hollow Core Double Clad Fiber Coupler". The coupler 400 is implemented, in this example, in a non-linear endoscope and [Fig.2B] represents an example 200 of such a non-linear endoscope.

[0070] The coupler 400 includes a first hollow core double-clad optical fiber 430, or "HC-DC" fiber for "Hollow Core Double Clad". The first optical fiber 430 generally comprises a hollow core configured for guiding light in a first wavelength range. The first optical fiber 430 also comprises a highly multimode inner cladding configured for guiding light in a second wavelength range. As will be described in more detail later, the hollow core of the HC-DC fiber has a given damage temperature. Examples of HC-DC fibers will be described in more detail later, in relation to [Fig. 6].

[0071] The coupler 400 further includes a second optical fiber 460 comprising a strongly multimode glass guiding portion configured for guiding light in a third wavelength range. As will be described later, the glass of the glass guiding portion has a glass transition temperature lower than the damage temperature. Examples of second optical fibers will be described in more detail later, in relation to [Fig. 5A], [Fig. 5B].

[0072] As illustrated in [Fig.2A], the coupler 400 further comprises an optical coupling zone 401 between the first fiber 430 and the second optical fiber 460. As will be described in more detail later, the coupling zone is generated by fusion between a region of the inner cladding of the first fiber and a region of the guiding glass portion of the second optical fiber.

[0073] In exemplary embodiments, the coupler 400 may also include, as illustrated in [Fig. 2A], a low-index outer sheath 480 covering, in a region comprising the coupling zone 401, the inner sheath of the first fiber and the glass guiding portion of the second optical fiber. The outer sheath is low-index, that is, it has a lower refractive index than the inner sheath of the first fiber and the glass guiding portion of the second optical fiber.

[0074] As illustrated in [Fig. 2B], the endoscope 200 configured for nonlinear imaging comprises a source 210 for ultrashort light pulses, a detector 250, and a double-sheathed hollow-fiber coupler 400 as described herein. The endoscope may further comprise, as illustrated in the figures, optics 220 for injecting optical pulses into one end (A, [Fig. 2A]) of the first HC-DC fiber 430 of the coupler 400 and a head 240 at the distal end (B, [Fig. 2A]) of the first fiber 430. The head 240 comprises, for example, a device for scanning the incident pulses. The detector may be connected, in a known manner, to a processing unit (not shown in [Fig. 2B]), for processing the detected optical signals. The endoscope may also include any other known units, such as a display unit, a storage unit (memory), etc.

[0075] The source is for example a laser source, for example a titanium-sapphire laser delivering femtosecond pulses.

[0076] The detector is, for example, a photomultiplier tube.

[0077] In operation, the hollow core of the first optical fiber 430 carries light pulses to a biological sample 100 to be imaged (optical path shown schematically in bold, single arrow in [Fig. 2A]) and the inner cladding of the first optical fiber carries an optical signal resulting from a nonlinear interaction of the pulses with the biological sample 100 (optical path shown schematically in bold, double arrow in [Fig. 2A]). Furthermore, the guiding glass portion of the second optical fiber 460, optically coupled with the first optical fiber, directs said optical signal to a proximal end C of the coupler (optical path shown schematically in dashed lines in [Fig. 2A]) and then to the detector 250.

[0078] Thus, as can be seen in [Fig.2B], the coupling can be achieved using the fiber coupler 400 and no other free-space optics are required for sending the nonlinear signal to the detector 250, which allows for gains in reliability, mechanical stability and robustness.

[0079] Figure 3A shows a simplified top view diagram illustrating an example of an assembly 300 for implementing a method for manufacturing a double-clad hollow-core optical fiber coupler according to this description. Figure 3B shows a simplified cross-sectional diagram illustrating an element of the assembly.

[0080] The setup 300 in this example comprises two supports 320 with V-grooves in which the fibers (locally stripped) are clamped, for example, using magnetic clips 330. The smaller diameter fiber (here, the hollow fiber 430) is placed at the bottom of the V-groove. The larger diameter fiber (here, the fiber 460) is placed on top. These supports are fixed to a plate 310, which is itself movable in a direction 315 substantially perpendicular to the direction of a laser beam 350 used for fusion. The fibers 460 and 430 are held against each other and are heated laterally by the laser beam 350. Between the V-grooves located on either side of the plate 310, the fibers are stretched so that they remain stuck to each other along the entire length between the two supports. During operation, the plate moves to heat the entire area sought for coupling.

[0081] A method for manufacturing a double-clad hollow-core optical fiber coupler according to this description, implemented for example by means of a 300 assembly as illustrated in [Fig.3A] and [Fig.3B] includes the provision of a first double-clad hollow-core optical fiber and the provision of a second optical fiber including a guiding glass portion.

[0082] Fig. 6 illustrates cross-sectional images of examples of such double-clad hollow core (HC-DC) fibers referenced 601, 602, 603, 604.

[0083] Such HC-DC fibers include, in exemplary embodiments, a hollow core 431 configured for light guidance in a first wavelength range and a double cladding. The double cladding comprises a highly multimode inner cladding 435, configured for light guidance in a second wavelength range, and an outer cladding, not shown in the images, for example, an outer cladding made of a low-index polymer, i.e., with a refractive index lower than that of the inner cladding.

[0084] The HC-DC fibers also include in these examples a micro-structured part 432 at the periphery of the hollow core, for example made of air and glass, and allowing the guidance of light in the hollow core.

[0085] The hollow core generally comprises a core containing a gas, for example air, or a vacuum. The core is single-mode or weakly multimode, that is, capable of propagating one or a few modes, up to a maximum of about 10 modes. For example, for endoscopy applications, the first wavelength range is between about 700 nm and about 1800 nm. The inner cladding is strongly multimode, that is, capable of propagating from several hundred to several tens of thousands of modes. For example, for endoscopy applications, the second wavelength range is between about 380 nm and about 2200 nm.

[0086] More specifically, the examples of HC-DC fibers illustrated by means of images 601 - 604 are described respectively in [Ref. 4], [Ref. 5], [Ref. 6], [Ref. 7]. They differ in particular by virtue of their microstructure 432 and consequently by virtue of their light guidance mechanism in the hollow core.

[0087] In a step of the process according to the present description, a second optical fiber is provided comprising a strongly multimode, glass-guided portion and an outer sheath. The glass-guided portion is configured for guiding light in a third wavelength range.

[0088] Fig. 5A and Fig. 5B represent simplified diagrams of a first example 501 of a second optical fiber with a strongly multimode guiding glass portion and of a second example 502 of a second optical fiber with a strongly multimode guiding glass portion.

[0089] In the example of [Fig. 5A], the second optical fiber 501 comprises a glass core 511, an inner glass cladding 512, and an outer cladding 513. In a first For example, the refractive index of the inner glass cladding 512 is lower than that of the core, and the outer cladding 513 is made of a low-index material with a refractive index lower than that of both the core and the inner cladding. The strongly multimode guiding glass portion then consists of the core and the inner cladding. In a second example, the refractive index of the inner glass cladding 512 is lower than that of the core 511, and the outer cladding 513 is made of a high-index material with a refractive index higher than that of the inner cladding 512. The strongly multimode guiding glass portion then consists of the core.

[0090] In the example of [Fig. 5B], the second optical fiber 502 comprises a glass core 521 and the outer cladding 522, the outer cladding being formed of a low-index material with a refractive index lower than that of the core. The guiding glass portion is then formed by the core 521.

[0091] The glass guiding portion of the second fiber is made, as will be described in more detail later, of a glass having a glass transition temperature lower than the damage temperature of the hollow core of the HC-DC fiber. For example, the applicants have shown that a suitable glass is a borosilicate glass. In the case where the glass guiding portion comprises the glass core 511 and the inner cladding 512 ([Fig. 5A]), the glass core 511 and the inner cladding 512 can be made of the same glass but with different dopings. For example, the glass core 511 and the inner cladding 512 can be made of borosilicate glass with different chemical compositions.

[0092] The process according to the present description then comprises local stripping of the first optical fiber and local stripping of the second optical fiber to remove, within a given stripping zone, the outer sheath, for example polymer, of the first fiber and the outer sheath, for example polymer, of the second fiber. Thus, the outer sheath 513 or 522 of the second fiber can be locally removed ([Fig. 5A] and [Fig. 5B]). Note that the stripping zone is chosen to be larger than the zone in which the fusion is planned in order to avoid damaging the remaining polymer outer sheaths of the fibers during heating.

[0093] The process according to the present description then includes heating, in the stripping zone, a first region of the inner cladding of the first optical fiber and a second region of the glass guiding part of the second optical fiber to obtain locally a fusion of the first region and the second region and generate an optical coupling zone between the first fiber and the second optical fiber.

[0094] Heating is achieved, for example, by applying a 350 laser beam, as illustrated in [Fig. 3A]. The laser beam is emitted in such a way as to cover the first region of the inner cladding of the first fiber and the second region of the glass guiding part of the second optical fiber.

[0095] The 460 and 430 fibers are placed in supports, for example, V-shaped slots ([Fig. 3B]), and clamped together. They are then heated laterally, for example, by means of the laser beam 350, the optical power of which is adjusted according to the type of glass of the 460 fiber. For example, the optical power is between approximately 5 pW and approximately 10 pW, for example, on the order of 8 pW, for Simax® glass.

[0096] We then obtain an HC-DCFC type coupler as described in [Fig.4A].

[0097] More specifically, the coupler includes a fusion zone 401 between the guiding glass portion 461 of the second fiber 460 and the inner cladding 435 of the HC-DC fiber 431. The fusion zone corresponds to the coupling zone, that is, the zone in which, during operation, a transfer of light energy can take place between the first fiber 430 and the second fiber 460. On either side of the fusion zone 401, there are transition regions 402, 403 in which the overlap gradually goes from a maximum value (at the level of 401) to a zero value.

[0098] Fig. 4B represents a cross-sectional image of a first HC-DC optical fiber 430 and a second optical fiber 460 with a strongly multimode guiding glass portion 461, the two fibers being optically coupled according to a method in accordance with the present description.

[0099] In one embodiment, the first HC-DC 430 fiber is a fiber of the type of fiber 604 illustrated in [Fig. 6] and described, for example, in [Ref. 7]. It comprises a hollow core 431, a microstructured portion 432 with air and glass capillaries surrounding the hollow core, and an inner cladding 435. The inner cladding 435 (gray portion) is made of silica glass, and the core 431 (black portion) contains air. The second fiber 460 in this example comprises a glass core 461, which forms the guiding portion and is made of Simax® borosilicate glass.

[0100] The coupling zone 401 is shown in the image of [Fig. 4B] by dashed lines. The width of the overlap at the coupling zone is denoted by e. The more intense the heating, the greater the overlap. Of course, the overlap must allow for optical cutting but must not be so large as to damage the hollow core 431 of the first HC-DC fiber.

[0101] The manufacturing process may optionally include the placement, at the stripping zone and after the fusion step to form the coupling zone 401, of an outer sheath covering the stripped portion of the inner cladding of the first fiber and the stripped portion of the guiding glass portion of the second optical fiber. Such an outer sheath (480, [Fig. 2A], not shown in [Fig. 4A]) provides protection and improves mechanical strength. It is advantageously made of an acrylate polymer with a lower refractive index than the glass of the fiber 430. It will then be possible to make a connection between the outer sheath and the remaining outer sheath of the first optical fiber on the one hand and the remaining outer sheath of the second optical fiber on the other hand, for example using a machine for applying the coating of optical fibers (or "recoater").

[0102] As described previously, the glass of the guiding glass portion of the second fiber 460 is chosen such that it has a glass transition temperature (or softening temperature) lower than the damage temperature of the hollow core 431 of the first double-clad hollow core fiber 430. The glass transition temperature can be routinely measured using the differential scanning calorie technique, as described, for example, in [Ref. 8].

[0103] Fig. 7A represents a simplified diagram illustrating an example of a 700 setup for characterizing the damage temperature of a core of an HC-DC 730 fiber.

[0104] The assembly 700 includes an optical source 710 for the emission of a light beam (for example a Ti:Sapphire laser delivering tunable femtosecond pulses between 650 and 1050 nm) injected into the fiber 430 and an optical power measurement device 730. The fiber is placed in an oven 720 whose temperature can be adjusted from ambient temperature to a temperature above the destruction temperature of the fiber 430 (for example 1600°C).

[0105] Fig. 7B represents, by way of illustration, a diagram showing a curve of optical power transmitted in the HC-DC 460 fiber as a function of the applied temperature.

[0106] The optical fiber is locally completely stripped, i.e., the outer polymer is removed. The optical power Pmax transmitted by the optical fiber is measured at room temperature Ta, i.e., the power of the optical beam transmitted at the fiber output. The temperature in the oven is gradually increased while measuring the optical power transmitted by the fiber under the same conditions. This optical power decreases until a temperature Td at which it reaches a predetermined threshold given as a percentage of Pmax, for example, approximately 10% of Pmax. Td then corresponds to the fiber damage temperature 430.

[0107] Figure 8A shows comparative curves illustrating, by way of example, the fusion overlap between the inner cladding region of the first optical fiber and the glass guiding region of the second optical fiber, as a function of the heating power applied during the implementation of a coupler manufacturing process according to this description. Curve 81 corresponds to the case of a second optical fiber made of Simax glass®, which belongs to the borosilicate glass family, and curve 82 corresponds to the case of a second optical fiber made of silica (prior art).

[0108] It is observed that the heating power required to reach a given recovery value (for example greater than 10 pm) is about twice as low with borosilicate glass fiber as with silica glass fiber.

[0109] Figure 8B shows comparative curves illustrating, by way of example, the diameter of the hollow core of the double-clad hollow-core optical fiber as a function of the overlap obtained during fusion (e, Figure 4B) between the inner cladding region of the first optical fiber and the glass-guiding region of the second optical fiber, during the implementation of a coupler manufacturing process according to this description. Curve 86 corresponds to the case of a second optical fiber made of silica (prior art), and curve 87 corresponds to the case of a second optical fiber made of Simax glass®, which belongs to the borosilicate glass family. The dashed straight line 85 represents the diameter of the hollow core of the HC-DC fiber before the coupler manufacturing process.

[0110] It is observed that with a silica fiber (86), as soon as the overlap increases, the hollow core shrinks, rendering the fiber ineffective. Conversely, with a borosilicate glass fiber (87), the diameter of the hollow core is independent of the overlap and remains very close to its initial value. Therefore, melting a borosilicate glass fiber does not alter the hollow core of the fiber.

[0111] Figure 9A represents an experimental curve showing optical coupling obtained between the first optical fiber and the second optical fiber, in an example of a coupler according to this description, for different wavelengths of light propagating in the coupler.

[0112] Light (for example, from a Ti:Sapphire laser delivering tunable femtosecond pulses between 650 and 1050 nm) is injected into port B of the coupler ([Fig. 2A]), and the percentage of optical power recovered in port C is measured as a function of wavelength. The results show that approximately 60% of the light injected at B is detected at C, for a wavelength between 450 and 650 nm, corresponding to the emission range of most biological markers. It is noteworthy that even in the absence of a dichroic mirror, 60% of the light power is recovered.

[0113] Figure 9B shows an SHG image of unlabeled mouse skin, obtained using an example of a nonlinear endoscope as described in Figure 2B, with an excitation wavelength of 920 nm and 200 fs pulses at 80 MHz and a power of 20 mW. The scale bar is 50 pm. This image demonstrates the feasibility of nonlinear imaging of unlabeled biological tissues using the coupler.

[0114] Although described through a number of embodiment examples, the methods and devices according to this description include different variants, modifications Modifications and improvements that will be obvious to a person skilled in the art, it being understood that these various variants, modifications, and improvements form part of the scope of the invention as defined by the following claims. REFERENCES

[0115] [Réf. 1] : V. Kucikas et al. “Two-Photon Endoscopy: State ofthe Art and Perspectives”. Mol Imaging Biol (2021).

[0116] [Réf. 2]: A. Kudlinski et al. “Double clad tubular anti-resonant hollow core fiber for nonlinear microendoscopy”, Optics Express, Vol. 28, N°10, pp 15062 - 15070 (2020)

[0117] [Réf. 3] S. Lemire-Renaud et al. "Double-clad fiber coupler for endoscopy," Optics Express Vol. 18, N°10, pp. 9755-9764 (2010)

[0118] [Réf. 4] Y. Y. Wang et al. "Eow loss broadband transmission in hypocycloid-core Kagome hollow-core photonic crystal fiber," Opt. Lett. 36, 669-671 (2011)

[0119] [Réf. 5] G. Bouwmans et al. "Properties ofa hollow-core photonic bandgap fiber at 850 nm wavelength" Opt. Express 11, 1613-1620 (2003)

[0120] [Réf. 6] F. Couny et al. "Génération and Photonic Guidance of Multi-Octave Optical-Erequency Cornbs", Vol 318, Issue 5853, pp. 1118-1121 (2007)

[0121] [Réf. 7] A. Kudlinski, et al., “Double clad tubular anti-resonant hollow core fiberfor nonlinear microendoscopy”, Opt. Express 28 (10), p. 15062-15070 (2020).

[0122] [Réf. 8] G. Hôhne et al. « Differential Scanning Calorimetry”. Springer-Verlag (2003), p. 105-180.

[0123] [Ref.9] J. David Musgraves et al., Springer Handbook of Glass, Springer 2019, chapter 14.

Claims

Claims

1. A coupler (400) for a double-clad hollow core optical fiber comprising: - a first double-clad hollow core optical fiber (430) comprising: - a hollow core (431) configured for guiding light in a first wavelength range and comprising a given damage temperature; and - a highly multimode inner cladding (435), configured for guiding light in a second wavelength range; - a second optical fiber (460) comprising a highly multimode guiding glass portion (461), configured for guiding light in a third wavelength range, the glass comprising a glass transition temperature lower than the damage temperature;- an optical coupling zone (401) between the first optical fiber and the second optical fiber generated by fusion between a region of the inner cladding of the first optical fiber and a region of the guiding glass part of the second optical fiber.;

2. A coupler according to claim 1, wherein the guiding glass portion (461) of the second optical fiber is made of bo-rosilicate glass.

3. A coupler according to any preceding claim, further comprising a low index outer cladding (480) covering in a region which includes the coupling zone (401), the inner cladding (435) of the first optical fiber and the guiding glass portion (461) of the second optical fiber.

4. An endoscope (200) configured for non-linear imaging comprising: - a source (210) of ultra-short light pulses; - a detector (250); - a double-clad hollow core optical fiber coupler (400) according to any one of the preceding claims; wherein: - the hollow core (431) of the first optical fiber (430) is configured to transport said light pulses to a biological sample to be imaged and the inner cladding (435) of the first optical fiber is configured to transport an optical signal resulting from a non-linear interaction of the pulses with the biological sample; and - the guiding glass portion (461) of the second optical fiber (460) optically coupled with the first optical fiber is configured to direct said optical signal towards the detector.

5. A method of manufacturing a double-clad hollow core fiber optic coupler comprising: - providing a first double-clad hollow core optical fiber (601 - 604) comprising - a hollow core (431) configured for guiding light in a first wavelength range and comprising a given damage temperature; and - a double cladding comprising a highly multimode inner cladding, configured for guiding light in a second wavelength range and an outer cladding; - providing a second optical fiber (460) comprising a highly multimode guiding glass portion, configured for guiding light in a third wavelength range, the glass comprising a glass transition temperature lower than the damage temperature and an outer cladding;- local stripping of said first optical fiber and local stripping of the second optical fiber for the removal, in a given stripping zone, of the outer sheath of the first optical fiber and the removal of the outer sheath of the second optical fiber; - heating, in said stripping zone, of a first region of the inner sheath of the first optical fiber and of a second region of the guiding glass part of the second optical fiber to locally obtain a fusion of said first region and of said second region and generate an optical coupling zone between the first optical fiber and the second optical fiber.;

6. The method of claim 5, wherein heating is achieved by applying a laser beam covering said first region of the inner cladding of the first fiber and said second region of the guiding glass portion of the second optical fiber.

7. A method according to any one of claims 5 or 6, wherein the second optical fiber comprises a glass core, an inner cladding made of glass with a refractive index lower than that of the core and the outer cladding, the outer cladding of the second optical fiber being formed of a low-index material with a refractive index lower than that of the core and that of the inner cladding, the guiding glass portion being made of the core and inner sheath.

8. A method according to any one of claims 5 or 6, wherein the second optical fiber comprises a glass core, an inner cladding made of glass with a refractive index lower than that of the core and the outer cladding, the outer cladding of the second optical fiber being formed of a high index material with a refractive index higher than that of the inner cladding, the guiding glass portion being made of the core.

9. A method according to any one of claims 5 or 6, wherein the second optical fiber comprises a glass core and the outer cladding, the outer cladding of the second optical fiber being formed from a low index material, having a lower refractive index than the core, the guiding glass portion being formed from the core.

10. A method according to any one of claims 5 to 9, wherein the guiding glass portion (461) of the second optical fiber is made of borosilicate glass.

11. Method according to any one of claims 5 to 10 further comprising: - the placement, at the stripping zone and after fusion, of an outer sheath covering the stripped part of the inner sheath of the first fiber and the stripped part of the guiding glass part of the second optical fiber, - the joining of said outer sheath with the outer sheath of the first optical fiber and the outer sheath of the second optical fiber.