Method for forming a part by inserting a solid-state metallic alloy into a cluster

FR3142366B1Active Publication Date: 2024-11-29SAFRAN SA
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
FR2022012323
Authority / Receiving Office
FR · FR
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-11-25
Publication Date
2024-11-29
Estimated Expiration
2042-11-25

AI Technical Summary

Technical Problem

Existing lost wax casting methods face safety risks and quality issues due to the handling of liquid metal alloys, particularly in forming bi-material parts, which require multiple pours and crucible changes, and are prone to thermal disturbances and operator errors.

Method used

A method involving the insertion of metal alloys in the solid state into a cluster, which is then melted within a furnace, eliminating the need for pouring and allowing controlled solidification and junction formation of multi-material parts.

Benefits of technology

This approach enhances safety, reduces handling risks, improves quality control, and enables the production of multi-material parts with precise junctions, while avoiding thermal disturbances and operator errors.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

Method for forming a part by inserting a solid metal alloy into a cluster. Method for forming casting parts in a cluster (100), the cluster (100) comprising a plurality of molds (103) formed by a lost-wax method, each mold of the plurality of molds (103) having a top, a middle portion and a bottom, a cup (101) configured to receive liquid metal, a ring (102) connecting the cup (101) to each top of each mold of the plurality of molds (103), a descendant (106) connected to the cup, a plurality of grain selectors (104) each connected to a bottom of a mold of the plurality of molds (103), the method comprising, the insertion of a first solid metal alloy (10) into the cluster (100), the liquefaction of the first alloy (10) inserted into the cluster (100), the directed solidification of the first alloy (10) thus liquefied. Figure for the abbreviation: Fig. 1.
Need to check novelty before this filing date? Find Prior Art

Description

Description Title of the invention: Method of forming a part by insertion of a solid state metal alloy in a cluster Technical field

[0001] — The present disclosure relates to a method of forming a metal part by a lost wax casting method.

[0002] — A method is particularly suitable for the formation of blades for turbo- aircraft machines. The formed blades can be bi-material. Prior art

[0003] — Generally, the known methods of forming parts by methods lost wax casting includes a pouring in which a metal alloy in the state liquid is poured into the crucible of a ceramic cluster. This step typically has place in a furnace. The metal alloy then fills one or more molds included in the cluster. The whole is then cooled to solidify the metal alloy, thus forming a casting.

[0004] — In order to improve the quality of the piece obtained, it is preferable to carry out the pouring under vacuum to avoid any parasitic reaction, for example oxidation of the alloy metallic in the liquid state. In addition, the pour is independently optimized for each metal alloy, since each metal alloy has properties different (melting temperature, viscosity, density, etc.). We then understand that the verse is an important issue for the person in the profession. For example, the conditions of the pouring influences the reject rate of the part to be formed.

[0005] — Furthermore, in the known processes, it appears that lodging is an obstacle to the formation of bi-material parts. Indeed, to obtain bi-material parts, it is it would then be necessary to plan two pours and two solidifications in a single oven; However, it is not possible to pour two alloys into the same crucible.

[0006] One solution could be to change the crucible after the first pour, but the changing the crucible is a non-automated operation which requires the intervention of an operator. However, such a change in the furnace in operation re- presents a considerable risk to the operator. Indeed, the oven in operation can reach temperatures above 1000°C. This also represents risks for the oven itself because opening it while in operation causes a strong modification of the oven's thermal properties, which can cause gradients significant thermal stresses that can cause cracks in the cluster and a leak of the metal alloy in the liquid state in the furnace.

[0007] = We then understand that pouring is in itself a step intrinsically comprising significant risks, both from a safety point of view and from the point of view of the quality of the part to be obtained. There is therefore a real need to improve the processes for forming parts using lost wax methods which are free, at least in part, from the inherent drawbacks mentioned above. Statement of the invention The present disclosure relates to a method for forming castings in a cluster, the cluster comprising a plurality of molds formed by a lost wax method, each mold of the plurality of molds having a top, an intermediate portion and a bottom, a cup capable of receiving liquid metal, a crown connecting the cup to each top of each mold of the plurality of molds, a descendant connected to the cup, a plurality of grain selectors each connected to a bottom of a mold of the plurality of molds, the method comprising, inserting a first metal alloy in the solid state into the cluster, liquefying the first alloy inserted into the cluster, and directed solidifying the first alloy thus liquefied. Thus, such a method makes it possible to dispense with pouring. Indeed, in the present method, the metal alloy inserted in the solid state in the cluster is melted when the cluster is inserted into a furnace. Consequently, the supply of the metal alloy in the liquid state in the plurality of molds of the cluster does not require pouring, since the liquid metal alloy is directly obtained by transformation of the solid metal alloy inserted in the cluster. Such a process is therefore safer for the operator. Furthermore, handling a metal alloy in the solid state is simpler than handling a metal alloy in the liquid state, so this process is simpler to implement. Furthermore, avoiding pouring makes it possible to circumvent the risk of pollution of the liquid metal alloy during said pouring. In addition, this makes it possible to reduce the forces applied by the liquid metal on the cluster and / or other components. Furthermore, since the liquid metal alloy is formed directly in the cluster, the risk of handling errors, for example on the part of the operator, which could lead to accidental pouring of liquid metal alloy into the furnace during the pouring stage, disappears. In some embodiments, the cluster further comprises a set of main channels, each channel of the set of main channels connecting the descendant to a grain selector. In this configuration, the cluster allows the plurality of molds to be filled from their bottom. In particular, in this configuration, a liquid metal alloy can flow from the descendant to the mold. In some embodiments, the first metal alloy is, in the solid state, a single-piece cylindrical ingot. In the present application, the expression "cylindrical" is understood in the mathematical sense of the term. A cylinder is defined as the volume obtained by the translation of a closed contour along an axis. For example, the closed contour may be a circle or a square. Using a cylindrical ingot makes it easy to calculate the volume of the liquefied metal alloy. Furthermore, in this form, the solid metal alloy is easier to insert into the cluster. In some embodiments, a clearance is provided between the solid metal alloy inserted into the cluster and the cluster. This allows for the expansion of the metal alloy under the effect of temperature to be compensated for before it melts. This therefore reduces the stresses applied to the cluster, thereby reducing the risk of leaks. In some embodiments, the method further comprises a prior cluster assembly step in which the plurality of molds, the bucket, the crown, the descender, and the plurality of grain selectors are assembled together; and in which the first solid-state metal alloy is inserted into the cluster during the prior assembly step. In some embodiments, the first metal alloy is inserted into the descendant. In some embodiments, the first metal alloy is inserted into the crown. Inserting the metal alloy in the solid state during the assembly step simplifies the integration of the first metal alloy into the cluster. This therefore represents a time saving for the operator. In particular, the insertion of the first metal alloy into the crown or descendant is particularly advantageous from this point of view. In some embodiments, the cluster further comprises a plurality of sets of secondary channels, each channel of each set of secondary channels connecting the descendant and the intermediate part of a mold, a plurality of plugs delimiting a plurality of casting paths, and in which a plurality of metal alloys in the solid state are inserted into the plurality of casting paths, the method successively comprising, for each metal alloy of the plurality of metal alloys, the selective liquefaction of the metal alloy followed by the casting of this metal alloy in one of the sets of secondary channels up to the plurality of molds, then the solidification, optionally directed, of this metal alloy liquefied metal. In this configuration, it is possible to obtain multi-material parts without resorting to pouring. In addition, this method incorporates all the previously mentioned advantages related to the insertion of solid-state metal alloys into the cluster. This configuration is particularly advantageous for forming multi-material turbomachine blades. In this disclosure, a “multi-material” part is a part comprising at least two parts made of two different materials. For example, a blade comprising two parts made of two different metal alloys is considered a “multi-material” part. Furthermore, one of the major challenges when forming multi-material blades is the junction zone between the different materials. In particular, controlling the size, position and solidification of the junction zone are concerns of interest to the person skilled in the art seeking to manufacture multi-material blades. According to this aspect, it is possible to obtain a multi-material part in a single furnace, guaranteeing good properties for the part obtained, in particular at the level of its junction zones between the different materials. Indeed, the insertion of metal alloy in the solid state makes it possible to control more precisely the volume of liquid metal alloy injected into the mold. In some embodiments, the cluster includes a top cap positioned at the junction between the bucket and the descender, and wherein the method includes: pouring a terminal metal alloy in a liquid state into the bucket, such that the terminal metal alloy flows into each mold of the plurality of molds through the crown, and solidifying the terminal metal alloy. Depending on the case, depending on the metal alloy involved and / or the part, pouring is desirable. This configuration therefore makes it possible to obtain a multi-material part by pouring the terminal metal alloy. On the other hand, this configuration represents an alternative and / or a complement for obtaining multi-material parts. In some embodiments, the cluster comprises a container, the container comprising a heating system; and the method further comprising inserting the terminal metal alloy in a solid state into the container, and liquefying the terminal metal alloy by the heating system. In some embodiments, the container is attached to the bucket. This configuration makes it possible to obtain a multi-material part while avoiding the disadvantages associated with pouring, while retaining the advantages associated with the use of the cup. Furthermore, according to this embodiment, the casting of the terminal metal alloy is faster than the pouring of this alloy, according to known methods. In some embodiments, the container includes a metal membrane at the junction between the container and the bucket. In this configuration, the container's tightness is improved. In some embodiments, the heating system imposes a temperature gradient of between 10°C and 50°C, preferably 50°C in the container. In some embodiments, the heating system imposes a temperature gradient between 10°C and 30°C. Thus, this gradient makes it possible to control the melting of the terminal metal alloy, and in particular, to liquefy it gradually. This improves the reliability of the casting of the terminal metal alloy in the plurality of molds of the cluster. In some configurations, a plurality of ceramic cores are provided in the plurality of molds. The plurality of ceramic cores allows for a greater diversity of parts. For example, this allows the production of so-called hollow or cooled blades. The present disclosure further relates to a turbomachine blade obtained by a method according to one of the preceding embodiments. In some configurations, the blade comprises at least two parts made from two different metal alloys, and a junction zone between these two parts. The above-mentioned features and advantages, as well as others, will become apparent from the following detailed description of exemplary embodiments of the proposed device and method. This detailed description refers to the attached drawings. Brief description of the drawings The attached drawings are schematic and are intended primarily to illustrate the principles of the presentation. [Fig.1] [Fig.1] schematically represents a cluster according to a first embodiment of the invention, in which a metal alloy is inserted into the descendant. [Fig.2] [Fig.2] schematically represents the cluster according to the embodiment of [Fig.1], placed in a furnace, and in which the metal alloy is liquefied. [Fig.3] [Fig.3] schematically represents the cluster according to the embodiment of [Fig.1], in which the liquid metal alloy is poured into the plurality of molds. [Fig.4] [Fig.4] schematically represents the cluster according to the embodiment of |Fig.1], in which the metal alloy is solidified. [Fig.5] [Fig.5] schematically represents the cluster according to the embodiment of [Fig.1], in which the terminal metal alloy is poured into the cup. [Fig.6] [Fig.6] schematically represents the cluster according to the embodiment of [Fig.1], in which the terminal metal alloy is solidified. [Fig.7] [Fig.7] schematically represents a cluster according to a second embodiment of the invention, in which a plurality of metal alloys are inserted into the descendant. [Fig.8] [Fig.8] schematically represents a cluster according to a third embodiment of the invention, in which a terminal alloy is inserted into a container. [Fig.9] [Fig.9] schematically represents a cluster according to the third embodiment, in which a first metal alloy is liquefied and cast into the plurality of molds. [Fig.10] [Fig.10] schematically represents a cluster according to the third embodiment, in which the terminal alloy is liquefied. [Fig.11] [Fig.11] schematically represents a cluster according to the third embodiment, in which the terminal alloy is poured into the cup. Description of the embodiments In order to make the disclosure more concrete, an example of a device is described in detail below, with reference to the attached drawings. It is recalled that the invention is not limited to this example. [Fig. 1] schematically represents a cluster 100 according to a first embodiment of the invention. The cluster 100 comprises a cup 101 configured to receive liquid metal, a crown 102, a plurality of molds 103, a grain selector 104, a set of main channels 105, a descender 106 connected to the cup 101, each channel of the set of main channels 105 connecting the descender 106 to a grain selector 104. The plurality of molds 103 comprises molds formed by a lost wax method, and each mold of the plurality of molds 103 has a top, an intermediate portion, and a bottom. The crown 102 connects the cup 101 to each top 103a of each mold of the plurality of molds 103, and each grain selector of the plurality of grain selectors 104 is connected to a bottom 103c of a mold of the plurality of molds 103. Advantageously, the plurality of molds 103 may comprise a plurality of cores, in order to obtain, for example, hollow blades. In the present example, a ceramic upper plug 107 may be provided at the junction between the cup 101 and the descender 106. This plug is impervious to the liquid metal, so that a liquid metal poured into the cup 101 is forced to flow into the crown 102, then into the plurality of molds 103. When a liquid metal follows such a path, this is referred to as falling liquid metal pouring. A first metal alloy 10 is inserted into the descendant 106. The first metal alloy 10 is inserted in the form of a single-piece cylindrical ingot with a circular base. In other examples, the first metal alloy 10 may be inserted into the crown. Furthermore, the first metal alloy 10 may be inserted in the form of shot or in any other solid form making it suitable for insertion into the cluster 100. In the present example, the descender 106 is cylindrical with a circular base. A clearance is provided between the internal wall of the descender 106 and the first metal alloy 10. [Fig. 2] shows the cluster 100 of the first embodiment arranged in a Birdgman furnace 50. The furnace 50 comprises a hot zone 51 and a cold zone 52. Initially, the cluster 100 is placed at the hot zone 51 of the furnace 50. The first metal alloy 10 liquefies. The volume of the liquefied metal alloy 10 is calculated according to the following formula. [Math.1] — THE Vs=7-V, With Vs the volume of the metal alloy in the solid state, V; the volume of the metal alloy in the liquid state, ps the density of the metal alloy in the solid state and p, the density of the metal alloy in the liquid state. Generally, for nickel alloys, the density ratio is of the order of 1.14. Knowing the volume of the plurality of molds 103 to be filled, it is possible to deduce the quantity, or volume, of metal alloy 10 to be provided to fill the plurality of molds 103. The inventors have found that it is necessary to provide a volume of solid metal alloy slightly in addition to the volume necessary for filling the plurality of molds 103, to compensate for a residual volume lost during the solidification of the metal alloy, linked to the contraction of the metal alloy during said solidification. As shown in [Fig. 3], the first molten metal alloy 10 follows the set of channels 105 to fill the plurality of molds 103 through their bottom 103c. For example, this filling can be carried out simply by gravity and / or capillarity. When a liquid metal follows such a path, we speak of casting the metal alloy in source. In the present example, the first metal alloy 10 partially fills the plurality of molds 103. However, in other examples, the first metal alloy 10 may completely fill the plurality of molds 10, provided that the adequate volume has been provided. As shown in [Fig.4], once the first metal alloy 10 is cast into the plurality of molds 103, the cluster is transferred (e.g. by gravity descent of the cluster or under the action of actuating members such as jacks) towards the cold zone 52 of the mold so that the first liquid metal alloy 10 is in the cold zone 52 of the furnace 50. In the present example, only the partially filled part of the plurality of molds 103 is in the cold zone 52 of the furnace 50. Thus, the first metal alloy 10 crystallizes in the plurality of molds 103. In the present example, by means of the plurality of grain selectors 104, the solidification of the first metal alloy 10 is directed. In other words, the first metal alloy 10 crystallizes in the plurality of molds 103 in a plurality of single-crystal alloys. In the present example, after the crystallization of the first metal alloy 10, a terminal metal alloy 20 ([Fig.5]), different from the first metal alloy 10, is poured in the liquid state into the cup 101. Thanks to the upper plug 107, the casting of the terminal metal alloy 20 is falling. The terminal metal alloy 20 flows into the plurality of molds 103 and fills the space left vacant by the first metal alloy 10. An interface 12 between the first metal alloy 10 and the terminal metal alloy 20 is created. At this interface, diffusion of the terminal metal alloy 20 into the first metal alloy 10 can be observed. In addition, during pouring of the terminal metal alloy 20, partial remelting of the first metal alloy 10 at the interface 12 can be observed. Once the terminal metal alloy 20 is poured, as shown in [Fig. 6], the entire cluster 100 is transferred (for example by gravity descent of the cluster or under the action of actuating members such as jacks) into the cold zone 52 of the mold 50. In this way, the terminal metal alloy 20 solidifies. Optionally, the first metal alloy 10 can serve as a seed for directed solidification of the terminal metal alloy 20. Once the terminal metal alloy 20 has solidified, a plurality of parts is obtained in the plurality of molds. Different stages of finishing the plurality of parts may be provided. [Fig. 7] shows a cluster 100 according to a second embodiment, compatible with the first embodiment. In the example of the second embodiment, the cluster 100 comprises a plurality of plugs 107' arranged in the descender 106. Furthermore, the cluster 100 comprises a plurality of sets of secondary channels 105', each channel of each set of secondary channels 105” connecting the descender 106 and the intermediate portion 103b of a mold of the plurality of molds 103. In this way, a plurality of cavities are formed in the descender 106 between each plug of the plurality of plugs 107', The channels of the plurality of secondary channel sets 105' are configured to connect each of these cavities to the different molds of the plurality of molds 103. Thus, a plurality of casting paths are formed in the descendant 106. A plurality of metal alloys 10°, different from one another, is inserted into the plurality of cavities formed between the plugs 107. For example, the plugs 107 can be inserted during assembly of the cluster. Advantageously, the metal alloys of the plurality of metal alloys 10° each have a different melting temperature. Once the cluster 100 is placed in the furnace 50, the metal alloys of the plurality of metal alloys 10° can therefore be liquefied selectively, by appropriate control of the temperature of the hot zone 51 of the furnace 50. When one of the plurality of alloys 10° is liquefied, it is cast into the molds of the plurality of molds 103 and solidified in a manner analogous to the casting and solidification of the first metal alloy 10. The liquefied first alloy is thus cast from the source. Under these circumstances, by selectively liquefying and then solidifying the metal alloys of the plurality of 10° metal alloys, a multi-material part is obtained. [Fig. 8] represents a cluster 100 according to a third embodiment, compatible with the other embodiments. Apart from the container 200 and the heating system 202 described below, the cluster 100 according to the third embodiment is in all respects identical to the cluster 100 of the first embodiment. Furthermore, with the exception of the pouring of the terminal metal alloy 20, the method for obtaining the part for this third embodiment is identical to the first embodiment. In the third embodiment, the cluster 100 comprises a container 200 and a heating system 202 capable of heating the container 200. For example, the heating system 202 may be a heating resistor. The container 200 may be attached to the cup 101. Alternatively, the container 200 may be attached by other means not shown, and provided above the cup 101, such that a liquid escaping from the container 200 under the effect of gravity falls into the cup 101. A metal membrane 204, typically made of nickel, may be provided at the junction between the container 200 and the cup 101. In this example, the terminal alloy 20 is inserted into the container 200 in the solid state. As shown in [Fig. 9], the first metal alloy 10 is liquefied and then solidified as described in the first embodiment. Subsequent to this solidification, and as shown in [Fig. 10], the heating system 200 liquefies the terminal metal alloy 20. In other examples, the furnace 50 may be capable of liquefying terminal metal alloy 20. As shown in [Fig. 11], once the terminal metal alloy 20 is liquefied, the metal membrane 204 is removed and the liquid terminal metal alloy 20 pours into the cup 101. The terminal metal alloy 20 is then solidified in a manner analogous to the first embodiment. The removal of the metal membrane 204 can be carried out by melting the latter. Indeed, once the terminal metal alloy 20 is liquefied, the terminal metal alloy 20 is capable of liquefying the metal membrane 204. Alternatively, the container 200 may comprise a bottom instead of the metal membrane 204. Furthermore, the bottom comprises an opening which faces the cup 101. The terminal metal alloy may then have a cylindrical shape, the base of which has a characteristic dimension greater than the characteristic dimension of the opening of the container 200. In these circumstances, when the terminal metal alloy 20 is inserted in the solid state into the container 200, the terminal metal alloy 20 is maintained in a fixed vertical position in the container. However, when the terminal metal alloy 20 is liquefied, the latter is able to pour into the cup 101 of the cluster 100, through the opening of the container 200. Optionally, the heating system may be capable of imposing a temperature gradient in the container 200. Under these circumstances, it is possible to partially liquefy the terminal metal alloy 20. This reduces the risk of the appearance of non-liquefied solid grains. Such grains are undesirable because they harm the properties of the part to be formed. These grains are all the more undesirable because they can block, for example, the channels of the cluster 100. Although the present invention has been described with reference to specific exemplary embodiments, it is obvious that modifications and changes may be made to these examples without departing from the general scope of the invention as defined by the claims. In particular, individual features of the various illustrated / mentioned embodiments may be combined in additional embodiments. Therefore, the description and drawings should be considered in an illustrative rather than restrictive sense. It is also obvious that all the characteristics described with reference to a method are transposable, alone or in combination, to a device, and conversely, all the characteristics described with reference to a device are transposable, alone or in combination, to a method.

Claims

Claims

1. A method of forming jack pieces in a cluster (100), the cluster (100) comprising a plurality of molds (103) formed by a lost wax method, each mold of the plurality of molds (103) having a top, a intermediate part and a bottom, a bucket (101) capable of receiving liquid metal, a crown (102) connecting the bucket (101) to each vertex of each mold of the plurality of molds (103), a descendant (106) connected to the bucket, a plurality of grain selectors (104) each connected to a bottom of a mold of the plurality of molds (103), the method comprising, the insertion of a first metal alloy (10) in the solid state into the cluster (100), the liquefaction of the first alloy (10) inserted into the cluster (100), the directed solidification of the first alloy (10) thus liquefied.

2. The method of claim 1, wherein the cluster (100) comprises further a set of main channels (105), each channel of the set of main channels (105) connecting the descendant (106) to a grain selector (104).

3. Method according to one of claims 1 or 2 in which the first metal alloy (10) is, in the solid state, a cylindrical ingot monobloc.

4. Method according to one of claims 1 to 3, further comprising a preliminary step of assembling the cluster (100) in which the plurality of molds (103), the bucket (101), the crown (102), the descending (106) and the plurality of grain selectors (104) are assembled together; and into which the first metal alloy (10) in the solid state is inserted in the cluster (100) during the preliminary assembly step.

5. Method according to one of claims 1 to 4, in which the cluster (100) further comprises a plurality of sets of secondary channels (105”), each channel of each set of secondary channels (105°) connecting the descendant (106) and the intermediate part of a mold (103), a plurality of plugs (107) defining a plurality of paths of casting, and wherein a plurality of metal alloys (10°) in the solid state is inserted into the plurality of casting paths, the process comprising successively, for each metal alloy of the plurality of metal alloys (10°), the selective liquefaction of the metal alloy followed by casting this metal alloy into one of the sets of secondary channels (105”) up to the plurality of molds (103), then solidification of this liquefied metal alloy.

6. Method according to one of claims 1 to 5, in which the cluster (100) includes an upper cap (107) placed at the junction between the bucket (101) and the descendant (106), and wherein the method comprises: the pouring of a terminal metal alloy (20) in the liquid state into the bucket (101), so that the terminal metal alloy (20) pours out in each mold of the plurality of molds (103) through the crown (102), and the solidification of the terminal metal alloy (20).

7. The method of claim 6, wherein the cluster (100) comprises a container (200), the container (200) comprising a system of heating (202); and the method further comprising inserting the terminal metal alloy (20) in the solid state into the container (200), and the liquefaction of the terminal metal alloy (20) by the system of heating (202).

8. The method of claim 7, wherein the container (200) comprises a metal membrane (204) at the junction between the container (200) and the bucket (101).

9. A method according to one of claims 7 or 8, wherein the system of heating imposes a temperature gradient between 10°C and 50°C in the container.

10. Method according to one of claims 1 to 9 in which a plurality of ceramic cores is provided in the plurality of molds.

11. | Turbomachine blade obtained by a method according to one of the re- previous instructions.

12. A blade according to claim 11, comprising at least two parts made from two different metal alloys, and an area of junction (12) between these two parts.