Improved method for manufacturing a laminated product

The use of aqueous epoxy resin in the manufacturing process for peelable shims addresses health and environmental concerns by ensuring safe handling and reducing scrap rates, enhancing the manufacturing process's safety and efficiency.

FR3146833A3Active Publication Date: 2024-09-27GASTEL DANIEL ANDRE
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
FR2023002645
Authority / Receiving Office
FR · FR
Patent Type
Utility models
Current Assignee / Owner
Filing Date
2023-03-21
Publication Date
2024-09-27
Estimated Expiration
2033-03-21

AI Technical Summary

Technical Problem

Existing manufacturing processes for peelable shims using solvent-based resins pose health risks to operators and environmental pollution due to the use of harmful solvents like acetone, leading to quality degradation and high scrap rates.

Method used

A process using an aqueous epoxy resin solution to bond sheets in a laminated product, ensuring the bonding force is weaker than the sheet resistance, allowing sheets to be detached without tearing, and enabling safe handling and reduced environmental impact.

Benefits of technology

The process ensures operator safety, reduces environmental pollution, and minimizes scrap rates by using water-based resins, facilitating tool cleaning and eliminating the need for exhaust ventilation systems.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

Improved method for manufacturing a laminated product The invention relates mainly to a method for manufacturing a laminated product having an adjustable thickness by thinning, comprising steps in which: - a liquid solution of unpolymerized resin is prepared in a solvent; - several sheets are coated with said liquid solution so as to form a resin film on at least one face of the sheet; - the sheets are stacked so as to separate them from each other by said resin film; and - the resin is brought to a state of polymerization which gives the shim a bonding strength between sheets which is weaker than the resistance of the sheets to tearing, resulting in each sheet being able to be detached from the stack without tearing, characterized in that the solvent is water-based, preferably the liquid solution is an aqueous phase epoxy resin solution.
Need to check novelty before this filing date? Find Prior Art

Description

Title of the invention: Improved method for manufacturing a laminated product technical field

[0001] The invention falls within the field of laminated products and more particularly within the field of peelable wedges.

[0002] PRIOR ART AND DISADVANTAGES OF PRIOR ART

[0003] More specifically, the invention relates to a method of manufacturing a laminated product having a thickness adjustable by delamination, this product comprising an alternating stack of sheets and layers of an adhesive material, each sheet having an intrinsic resistance to tearing, and each layer of adhesive material connecting two adjacent sheets of the stack to each other by a bonding force weaker than the resistance of the sheets to tearing, resulting in each sheet being able to be detached from the stack without tearing.

[0004] Products of this type are known from the prior art and are notably used as shims for mechanical assemblies. These assemblies generally exhibit significant clearances at certain points, resulting from the combination of manufacturing tolerances. These clearances are compensated for by inserting shims. The thickness of these shims is adjusted by removing the upper or lower sheets one by one until the desired thickness is achieved.

[0005] The sheets are generally metallic sheets, for example based on aluminium, stainless steel, carbon steel, brass or titanium, or thermoplastic organic polymer sheets.

[0006] In a known manner, a liquid solution of unpolymerized resin is prepared in a solvent. Several sheets are coated with this liquid solution to form a resin film on at least one side of each sheet, and the sheets are stacked so as to separate them from one another by this resin film. The resin is then brought to a state of polymerization that gives the shim a bond strength between sheets that is weaker than the tear resistance of the sheets, with the result that each sheet can be detached from the stack without tearing. The polymerization can be carried out by heating under pressure at a temperature and for a time determined according to the desired properties of the laminated product, particularly in terms of peelability. The laminated product is then machined or cut.

[0007] Also known, the adhesive material is a polymerizable material based on monomers or oligomers of the epoxy, phenolic, vinyl ester, vinyl, acrylic or other type, which allow the obtaining of a thermoplastic or a thermo Curable by crosslinking. A thermosetting resin is preferably chosen for its hardness characteristics during temperature increases, such as, more specifically, an epoxy resin.

[0008] These resins are mixed with powerful and polluting solvents. Acetone is one example.

[0009] Consequently, operators on the production lines are in constant contact, particularly by inhalation, with these solvents, which exposes them to risks of skin irritation and desensitization.

[0010] Furthermore, the operators' contact with these solvents is not limited to the manufacturing process of the laminated products but also extends to the cleaning of tools such as the gluing machine, the press, and the cutting machine. These tools are indeed impregnated with resin, and their cleaning requires the use of solvents, for example, acetone.

[0011] To limit the undesirable effects of these solvents, extraction ventilation systems are installed to remove them in gaseous form. However, these systems create swirling airflows laden with dust, which can degrade the quality of the final laminated product by causing pitting on the surfaces. This can lead to a scrap rate of up to 50% when the sheets used to produce the laminated product are made of aluminum, a metal particularly susceptible to dust contamination.

[0012] OBJECTIVE OF THE INVENTION

[0013] The invention relates to a method for manufacturing laminated products that overcomes the aforementioned drawbacks. Description of the invention

[0014] To this end, the manufacturing process of a laminated product having an adjustable thickness by flaking of the invention comprises steps in which:

[0015] - a liquid solution of unpolymerized resin is prepared in a solvent;

[0016] - several sheets are coated with said liquid solution so as to form a film of resin on at least one side of the sheet;

[0017] - the sheets are stacked so as to separate them from each other by said film of resin; and

[0018] - the resin is brought to a state of polymerization which gives the wedge a force of bond between sheets which is weaker than the resistance of the sheets to tearing, resulting in each sheet being able to be detached from the stack without tearing,

[0019] The process being characterized in that the solvent is water-based.

[0020] Advantageously, the liquid solution is an aqueous phase epoxy resin solution. DETAILED DESCRIPTION OF THE INVENTION

[0021] Other features and advantages of the invention will become clear from the des- description which is given below.

[0022] The present invention relates to a laminated product having a thickness adjustable by flaking, this product comprising an alternating stack of sheets and layers of an adhesive material, each sheet having an intrinsic resistance to tearing, and each layer of adhesive material connecting two adjacent sheets of the stack to each other by a bonding force weaker than the resistance of the sheets to tearing, resulting in each sheet being able to be detached from the stack without tearing.

[0023] In a known manner, the laminated product of the invention forming a peelable adjustment wedge is manufactured in the following way.

[0024] Sheets are prepared, which are generally metallic sheets, for example based on aluminium, stainless steel, carbon steel, brass or titanium, or thermoplastic organic polymer sheets. The sheets are cut to the desired dimensions.

[0025] The sheets are bonded on one side with a thermosetting polymer. The thermosetting polymer is an aqueous epoxy resin, for example marketed under the trade name Sikafloor®-2540 W.

[0026] The gluing operation is carried out by any type of gluing machine, spraying by means of a nozzle or a gun, by application with a manual roller, by printing on an offset type machine, or by soaking the sheet in a bath of adhesive material.

[0027] The aqueous phase epoxy resin, after its polymer monomer crosslinking treatment, constitutes an adhesive material, its quantity and treatment being chosen and adapted so that the bonding force linking two adjacent sheets is weaker than the resistance of these sheets to tearing, with the result that each sheet can be detached from the stack without tearing.

[0028] In some cases, additives are added to the resin. These additives may include hardeners to impart specific characteristics to the laminated product.

[0029] The glued sheets finally undergo a final polymerization operation under pressure. This operation consists of arranging the sheets in a stack between two parallel flat supports, these supports being pressed against each other at ambient temperature or hot in a heated press for a predetermined time so that the resin polymerizes.

[0030] This operation must give the rolled product the desired mechanical qualities of parallelism, flatness, cohesion and peelability.

[0031] The flat supports consist of two calibrated steel plates of significant thickness, for example 50 mm. The plates are traversed around their periphery by threaded rods or screws, on which a clamping force is applied.

[0032] Polymerization is carried out with temperature cycles between 150 and 200 °C, preferably about 200 °C for a duration between 5 and 12 hours depending on the desired peelability.

[0033] Finally, the laminated product is machined or cut if necessary to the appropriate dimensions, so that it has the correct shapes and dimensions in the plane of the sheets.

[0034] The use of water-based epoxy resin helps protect the health of operators. Furthermore, tools can be cleaned very quickly with water. In addition, the various containers used in the manufacturing process can be reused after simple cleaning with water. Finally, the use of extraction ventilation systems is no longer necessary, which reduces the scrap rate.

[0035] The manufacturing process is thus made safer and simpler, and the associated costs are reduced. In addition, the process of the invention respects both the environment and the health of the operators. Examples

[0036] The aqueous epoxy resin used is marketed, in particular, under the trade name Sikafloor®-2540 W.

[0037] The manufacturing process of the laminated product involving the use of this aqueous epoxy resin is as previously described.

[0038] Peelability tests are performed according to ASTM D 903.

[0039] The results are presented in the Table below. Pelatability ++ - Insufficient

[0040] + Correct

[0041] ++ Very good

[0042] Table 1

Claims

Claims

1. A method of manufacturing a laminated product having an adjustable thickness by disintegration, comprising steps in which: - a liquid solution of unpolymerized resin is prepared in a solvent; - several sheets are coated with said liquid solution so as to form a resin film on at least one sheet face; - the sheets are stacked so as to separate them from each other by said resin film; and - the resin is brought to a state of polymerization which gives the shim a bonding force between sheets which is weaker than the tear resistance of the sheets, as a result of which each sheet can be detached from the stack without tearing, characterized in that the solvent is water-based.

2. Manufacturing method according to claim 1, characterized in that the liquid solution is an epoxy resin solution in aqueous phase.