Concrete incorporating at least a portion of biochar in its composition

Incorporating biochar as an aggregate in concrete addresses the high carbon footprint and mechanical resistance issues of conventional concrete, resulting in low-carbon concrete with improved compressive strength for diverse construction applications.

FR3148594A1Active Publication Date: 2024-11-15SPURGIN LEONHART
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
FR2023004712
Authority / Receiving Office
FR · FR
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-12
Publication Date
2024-11-15
Estimated Expiration
2043-05-12

AI Technical Summary

Technical Problem

Conventional concrete production generates a significant carbon footprint and reduces mechanical resistance, limiting its application in construction operations, while wood concrete alternatives restrict usage due to lower compressive strength.

Method used

Incorporating biochar as an aggregate in concrete composition, replacing sand and/or gravel, to create low-carbon concrete with enhanced mechanical resistance suitable for various construction applications.

Benefits of technology

The biochar-based concrete achieves a negative carbon footprint and maintains or exceeds mechanical resistance requirements, making it suitable for diverse construction uses, including structural elements and unreinforced structures.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

Concrete incorporating at least a portion of biochar in its composition. The invention relates to a concrete for the production of low-carbon buildings or building elements, characterized in that the composition incorporates at least a portion of biochar as an aggregate in addition to cement and water. Figure to be published with the abstract: no figure
Need to check novelty before this filing date? Find Prior Art

Description

Title of the invention: Concrete incorporating at least a portion of biochar in its composition

[0001] The present invention relates to the field of low-carbon constructions and construction elements and more particularly to the field of low-carbon concretes for the construction of constructions.

[0002] As part of the fight against global warming, regulatory constraints have emerged to reduce greenhouse gas emissions. While the transport sector is the primary target of these measures, the building sector is also impacted by these constraints. Indeed, it is not only a question of evaluating the reduction of greenhouse gases through the prism of energy consumption alone but through the carbon footprint, i.e. the measurement of the volume of carbon dioxide (CO2) emitted by the combustion of fossil fuels, carbon dioxide being the main greenhouse gas that contributes to global warming.

[0003] In the field of construction, carbon footprint performance is measured over the entire life cycle of the building, from its construction phase to its demolition. This assessment is thus carried out on the basis of various criteria, including the consistency of the construction, the limitation of carbon energy sources for the operation of the building, and even the use of carbon storage.

[0004] In the context of construction, the use of concrete constitutes a significant source of carbon energy. Indeed, the production of a concrete of a conventional type of composition, for example from cement of the CEM IL A 52.5R type, sand, gravel and water, is likely to generate a carbon footprint of the order of 203 kg of CO2 per cubic meter produced. Also, to overcome this type of constraint, the production of mixtures incorporating crushed wood has been developed to obtain new compositions corresponding to wood concretes. Such wood concretes effectively make it possible to obtain concretes with a negative carbon footprint. However, this reduction in the carbon footprint compared to a concrete of a conventional composition is also accompanied by a significant reduction in the mechanical resistance of the wood concrete to compression compared to a concrete of a conventional composition.Also, the solution provided by the introduction of wood into the composition of a concrete constrains a reduction in the scope of application of the latter in the context of construction operations.

[0005] The present invention aims to overcome these drawbacks by proposing a technical solution with a negative carbon footprint that makes it possible to compensate for the lack of decarbonization of other construction operations likely to take place on a site, while responding favorably to the compressive strength requirements encountered in a wide range of construction operations.

[0006] The invention thus relates to a concrete for the production of low-carbon construction or construction elements, characterized in that the composition incorporates at least a portion of biochar as aggregate in addition to cement and water.

[0007] The invention also relates to a structural construction unit intended for filling and / or manufacturing a pre-wall or pre-slab, characterized in that this unit is made from a concrete according to the invention.

[0008] The invention will be better understood, thanks to the following description, which relates to different preferred embodiments, given by way of non-limiting example, and explained, with reference to the appended tables, in which:

[0009] [Fig.l] represents a synthetic table of different characteristics of an example of concrete according to the first particular range of concrete according to the invention.

[0010] [Fig.2] represents a summary table of different characteristics of an example of concrete according to the second particular range of concrete according to the invention.

[0011] [Fig.3] represents a synthetic table of different characteristics of an example of concrete according to the third particular range of concrete according to the invention.

[0012] [Fig.4] represents a synthetic table of different characteristics of an example of concrete according to the fourth particular range of concrete according to the invention.

[0013] The present invention relates to a concrete for the production of low-carbon construction or construction elements, characterized in that the composition incorporates at least a portion of biochar as aggregate in addition to cement and water. Biochar, also known as charcoal or charcoal of plant origin, is a compound obtained by pyrolysis of biomass and which allows carbon retention in the form of an inert product with a high carbon density compared to other products or compounds. This inertia of the biochar ensures storage and retention of carbon without risk of its release, for as long a period as necessary. By its properties, biochar constitutes a total or partial substitute for aggregates which, mixed with cement, participate in the composition and production of concrete.Thus, while a composition of a conventional type of concrete comprises, in addition to cement, sand and gravel, the composition of a concrete according to the invention also comprises biochar as a replacement for all or part of the sand and gravel. In a complementary manner, the biochar integrated into the mixture for the production of a concrete is likely to also be associated with one or more fines or fillers which correspond in particular to aggregates, for example, of the stone powder type or lime carbonates or even silica fume, and the fineness of which is, for example. example, of the order of 0 to 125 pm.

[0014] According to an exemplary embodiment which corresponds to a variant of the concrete of the invention, the biochar comprises a particle size of between 0 and 5 mm, preferably of the order of 0 to 2 mm. This particle size of the biochar is chosen so that the biochar optimally replaces the aggregates, sand and / or gravel, which it replaces.

[0015] According to another example which corresponds to an alternative embodiment of a first particular range of concrete according to the invention and whose characteristics are capable of being combined with those of the examples detailed above, the concrete has a composition free of gravel and comprising, in mass percentage, between 25% and 50% of biochar and at most 20% of cement. Preferably, the mass percentage of biochar is between 30% and 50% and ideally between 40% and 50%. As an example of embodiment, the composition is capable of comprising, in mass percentage, 9.59% of cement, for example a cement of type CEM II / B 52.5 N with 31.19% of filler, 41.19% of biochar and 18% of water. The production of concrete with such a composition has a negative carbon footprint of around -1455 kg of CO2 / m3, as well as a density of around 1283.5 kg / m3.In addition to a more attractive carbon footprint, concrete with such a composition also has a lighter density than that of conventional concrete, which is around 2338 kg / m3.

[0016] According to another example of producing a concrete with such a composition, it is likely not to require any baking operation as part of its production.

[0017] According to another example which corresponds to a particular variant of the embodiment of this first range of concrete according to the invention, seven days after pouring a concrete of this composition, this concrete has a mechanical compressive strength of at least 0.5 MPa or 0.5 x 106 Pascals, or even, preferably, a mechanical compressive strength of at least 3.4 MPa or 3.4 x 106 Pascals. Also, a concrete according to this first particular range is likely to be used as a particularly relevant reservation material as an alternative to the polystyrene blocks usually integrated into the thickness of slabs, paving elements or pre-walls. Similarly, a concrete according to this first particular range constitutes an interesting material for the production of elements forming structural units, for example in the form of cakes, intended for filling pre-walls or pre-slabs.For example, when producing cakes with an individual volume of around 10.5 litres, each cake produced has a negative carbon footprint of around -15.5 kg of CO2.

[0018] It should also be noted that the invention also relates to a unit structural construction intended for filling and / or manufacturing pre-walls or pre-slabs, characterized in that this unit is made from a concrete according to the invention, that is to say incorporating biochar, and more particularly a concrete whose composition corresponds to that of this first range of concrete according to the invention.

[0019] According to another example which corresponds to an alternative embodiment of a second particular range of concrete according to the invention and whose characteristics are capable of being combined with those of some of the examples detailed previously, the concrete has a composition free of gravel comprising, in mass percentage, between 35% and 60% of biochar and at most 60% of cement. Preferably, the mass percentage of biochar is between 40% and 60% and ideally between 45% and 60%. Such a composition has a higher proportion of biochar than in the context of the first particular range but also makes it possible to achieve higher levels of mechanical resistance. Similarly, this composition is also capable of being completely free of fine or filler. As an example of embodiment, the composition is capable of comprising, in mass percentage, 37% of cement, for example a cement of type CEM II / A 52.5R, 47% biochar and 16% water. The production of concrete with such a composition has a negative carbon balance of around -1434 kg of CO2 / m3, as well as a density of around 1261.7 kg / m3.

[0020] It should be noted that, during the first eighteen hours after pouring / molding, concrete according to this second particular range is likely to require a steaming operation at 35°Celsius.

[0021] According to another example which corresponds to a particular variant of realization of this second range of concrete according to the invention, twenty-eight days after pouring, the concrete has a mechanical resistance to compression of at least 14 MPa or 14xl06 Pascals. According to a more specific example of implementation likely to be obtained in particular in the context of a concrete whose composition is detailed previously, the concrete has a mechanical resistance to compression of the order of 14.3 MPa or 14.3xl06 Pascals at seven days and of the order of 17.8 MPa or 17.8xl06 Pascals at twenty-eight days. Also, a concrete according to this second particular range is likely to be used as a construction material for the realization of non-reinforced structures, as well as an alternative material to concretes of the wood concrete type.

[0022] According to another example which corresponds to an alternative embodiment of a third particular range of concrete according to the invention and the characteristics of which are capable of being combined with those of some of the examples detailed previously, the concrete has a composition comprising gravel and, in mass percentage, between 5% and 12% of biochar and at most 30% of cement, or even 25% of cement. Such a composition incorporates biochar while allowing higher levels of mechanical resistance to be achieved than in the first and second ranges of concrete. Thus, the concrete has a composition in which part of the sand of a conventional concrete is substituted by biochar, for example so that the biochar and the sand are present in similar or even identical volumes. As an example of an embodiment, the composition is free of filaments and may comprise, in mass percentage, 14.43% of cement, for example a cement of type CEM II / A 52.5 R with 6.2% of biochar, 19.24% of sand, 52.91% of gravel and 7.22% of water. The production of a concrete with this composition has a negative carbon balance of the order of -181 kg of CO2 / m3, as well as a density of the order of 2158 kg / m3.Also, concrete with such a composition has a lighter density than that of conventional concrete while having a negative carbon footprint.

[0023] It should be noted that, during the first sixteen hours after pouring / molding, concrete according to this third particular range is likely to require a steaming operation at 35°Celsius.

[0024] According to another example which corresponds to a particular variant of embodiment of this third range of concrete according to the invention, twenty-eight days after pouring, the concrete has a mechanical compressive strength of at least 30 MPa or 30 x 106 Pascals. According to a more specific example of implementation likely to be obtained in particular in the context of a concrete whose composition is detailed previously, the concrete has a mechanical compressive strength of the order of 35.1 MPa or 35.1 x 106 Pascals at seven days and of the order of 40.7 MPa or 40.7 x 106 Pascals at twenty-eight days.

[0025] According to another example which corresponds to an alternative embodiment of a fourth particular range of concrete according to the invention and whose characteristics are capable of being combined with those of some of the examples detailed above, the concrete has a composition comprising gravel and biochar as the only aggregates and, in mass percentage, between 12% and 30% of biochar and at most 30% of cement. Preferably, the mass percentage of biochar is at least 15%. Thus, the concrete has a composition in which the biochar completely replaces the sand of a conventional concrete. As an example of embodiment, the composition is free of filaments and sand and is capable of comprising, in mass percentage, 16.59% of cement, for example a cement of type CEM II / A 52.5 R with 14.27% of biochar, 60.84% ​​of gravel and 8.30% of water.The production of concrete with this composition has a negative carbon footprint of around -586 kg of CO2 / m3, as well as a density of around 1916 kg / m3. Also, concrete with such a composition has a lighter density than that of a . classic concrete while also having a negative carbon footprint.

[0026] It should be noted that, during the first sixteen hours after pouring / molding, concrete according to this fourth particular range is likely to require a steaming operation at 35°Celsius.

[0027] According to another example which corresponds to a particular variant of embodiment of this fourth range of concrete according to the invention, twenty-eight days after pouring, the concrete has a mechanical compressive strength of at least 20 MPa or 20x106 Pascals. According to a more specific example of implementation likely to be obtained in particular in the context of a concrete whose composition is detailed previously, the concrete has a mechanical compressive strength of the order of 21 MPa or 21x106 Pascals at seven days and of the order of 25.9 MPa or 25.9x106 Pascals at twenty-eight days.

[0028] It should be noted that, given their respective mechanical resistances to compression, the concretes produced according to these third and fourth particular ranges are capable of being used as construction material for reinforced or non-reinforced load-bearing structures suitable for application in pre-walls, pre-slabs and / or solid walls. Similarly, these third and fourth particular ranges are capable of being used as construction material for solid slabs.

[0029] In the context of the invention, the mechanical strength of each of these different types of concrete can be adjusted by modifying the quantity of cement in the proportions specific to each of the particular ranges of concrete detailed above. Indeed, the compressive mechanical strength of the concrete can be improved by increasing the quantity of cement in the corresponding concrete composition. Such an increase in cement impacts the carbon footprint of the concrete produced. However, it should be noted that the release of additional CO2 by this additional supply of cement is amply offset by the importance of the negative carbon weight of the biochar. Indeed, it is recalled that if the carbon footprint of the cement is positive and of the order of 680 kgCO2 per tonne, the carbon footprint of the biochar is negative of the order of -2934 kgCO2 / tonne.Also, an addition of cement in the composition of the concrete only slightly affects the significant carbon deficit provided by the biochar.

[0030] The invention also relates to a construction or portion of construction without reinforcement, characterized in that it incorporates a concrete according to the invention or incorporating a composition as detailed above for the second, third and fourth particular ranges of concrete.

[0031] Likewise, the invention also relates to a construction or portion of construction provided with reinforcement characterized in that it incorporates a concrete according to the invention or incorporating a composition as detailed previously for the third and fourth particular ranges of concrete.

[0032] Of course, the invention is not limited to the embodiment described and shown in the attached drawings. Modifications remain possible, in particular from the point of view of the constitution of the various elements or by substitution of technical equivalents, without departing from the scope of protection of the invention.

Claims

Claims

1. Concrete for the production of low-carbon construction or construction elements, characterized in that the composition incorporates at least a portion of biochar as aggregate in addition to cement and water.

2. Concrete according to claim 1, characterized in that the biochar comprises a particle size of between 0 and 5 mm.

3. Concrete according to one of claims 1 to 2, characterized in that the concrete has a composition free of gravel and comprising, in mass percentage, between 25% and 50% of biochar and at most 20% of cement.

4. Concrete according to claim 3, characterized in that, seven days after pouring, the concrete has a mechanical compressive strength of at least 0.5 MPa (106 Pascals).

5. Concrete according to one of claims 1 to 2, characterized in that the concrete has a composition free of gravel comprising, in mass percentage, between 35% and 60% of biochar and at most 60% of cement.

6. Concrete according to claim 5, characterized in that, twenty-eight days after pouring, the concrete has a mechanical compressive strength of at least 14 MPa (106 Pascals).

7. Concrete according to one of claims 1 to 2, characterized in that the concrete has a composition comprising gravel and, in mass percentage, between 5% and 12% of biochar and at most 30% of cement.

8. Concrete according to claim 7, characterized in that, twenty-eight days after pouring, the concrete has a mechanical compressive strength of at least 30 MPa (106 Pascals).

9. Concrete according to one of claims 1 to 2, characterized in that the concrete has a composition comprising gravel and biochar as the only aggregates and, in mass percentage, between 12% and 30% of biochar and at most 30% of cement.

10. Concrete according to claim 9, characterized in that, twenty-eight days after pouring, the concrete has a mechanical compressive strength of at least 20 MPa (106 Pascals).

11. Structural construction unit intended for filling and / or manufacturing a pre-wall or pre-slab, characterized in that this unit is made of concrete according to one of claims 1 to 4.

12. Construction or portion of construction devoid of reinforcement ca- characterized in that it incorporates a concrete according to one of claims 1, 2, 5 to 10.

13. Construction or portion of construction provided with reinforcement characterized in that it incorporates a concrete according to one of claims 1, 2, 7 to 10.

Citation Information

Patent Citations

  • Method for resource utilization of sludge biochar

    CN114394800A

  • A building material mixture of biochar and concrete for the production of blocks or slabs with the additional function of insulation and carbon storage for use in construction, etc.

    DE102021001327A1

  • Swine-waste biochar as a sustainable cement replacement material

    US20190345061A1