Thin, flexible, and luminous electroluminescent film capable of emitting red light

A flexible electroluminescent film with a refractive index adaptation element addresses the limitations of LED lighting by offering high brightness, low power consumption, and shape conformity, meeting brake light standards with reduced thickness and cost.

FR3148676A1Pending Publication Date: 2024-11-15VALEO VISION SA
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
FR2023004685
Authority / Receiving Office
FR · FR
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-11
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

Existing LED-based lighting solutions for vehicles are expensive, generate heat, require cooling devices, are not energy-efficient, and lack flexibility to conform to complex shapes, making them unsuitable for concave and convex surfaces.

Method used

A thin, flexible electroluminescent film comprising a flexible support layer, conductive electrodes, a dielectric insulating layer, a luminophore layer emitting red light, and a transparent protective layer, with a refractive index adaptation element to enhance light transmission, using a phosphor mixture of zinc sulfide, cadmium sulfide, and zinc selenide doped with copper.

Benefits of technology

The film provides high brightness, low power consumption, and flexibility to conform to complex shapes, meeting red light wavelength standards for brake lights with reduced thickness and cost, while being transparent or discreet.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

Thin, flexible, luminous electroluminescent film capable of emitting red light. The film (1) comprises successively: a flexible support layer (2); a first flexible electrode layer (3) made of conductive material; a flexible electrically insulating layer (4) made of dielectric material; a flexible electroluminescent layer (5), comprising a phosphor layer (6) emitting red light having a wavelength approximately equal to 630 nm when excited by an electrostatic field, and comprising a mixture of particles having the following composition: (Znx,Cd1-x)(Sy,Se1-y):Cu, with 0 < x < 1 and 0 < y < 1, preferably such that 0.8 < x < 1 and 0 < y < 0.2, and more preferably such that x = 0.9 and y = 0.1; a second flexible and transparent electrode layer (8) made of conductive material having a refractive index; and a flexible and transparent protective layer (9). Figure to be published with the abbreviation: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

Title of the invention: Thin, flexible and luminous electroluminescent film capable of emitting red light TECHNICAL FIELD OF THE INVENTION

[0001] The technical field of the invention is that of electroluminescent films emitting red light.

[0002] The present invention relates to an electroluminescent film, preferably transparent, capable of emitting red light, which is both very flexible and very luminous when supplied with alternating electric current. TECHNOLOGICAL BACKGROUND OF THE INVENTION

[0003] In the automotive field, certain lighting devices are designed to emit a red light, particularly for rear brake lights, also known as stop lights. For many years, stop lights included an incandescent bulb positioned behind a transparent plastic tinted red.

[0004] Nowadays, in lighting, manufacturers usually replace incandescent bulbs with LEDs. These LEDs are also used to add decorative and / or signaling elements to the interior and / or exterior of vehicles. They advantageously make it possible to emit a red light whose wavelength can be chosen precisely, for example with a wavelength substantially equal to 630 nm and with a width at half-maximum less than 20 nm, in particular in order to comply with the standards in force with regard to the red color authorized for brake lights.

[0005] These LED-based elements, however, have many disadvantages.

[0006] First of all, LEDs are expensive, and present a significant cost when an entire surface must be illuminated.

[0007] In addition, LEDs tend to heat up. Their use in large numbers therefore requires the use of a cooling device, which generates additional bulk and thickness in the LED surfaces. As a result, surfaces with a high density of LEDs are not thin, nor sufficiently flexible to be able to fit complex concave and / or convex shapes. It is therefore not possible to arrange them on any surface, since the latter must be substantially flat.

[0008] Finally, with an efficiency of around 1%, LEDs are not very energy efficient, so they consume a lot of electricity.

[0009] As a result, LED-based lighting does not always represent a financially advantageous solution, either for its manufacture or for its use, and that it is unlikely to be flexible enough to form complex concave and / or convex shapes.

[0010] There is thus a need for a light device which is thin, supple, flexible and uses little electricity, capable of covering concave and / or convex passenger compartment and bodywork parts, and which can emit a red light whose wavelength corresponds to the standards in force with regard to the red color authorized for brake lights. Summary of the invention

[0011] The invention offers a solution to the problems mentioned above, by providing a thin, flexible and luminous electroluminescent film capable of emitting a red light whose wavelength corresponds to the standards in force with regard to the red color authorized for brake lights.

[0012] The thin, flexible and luminous electroluminescent film used in the invention is notably described in detail in patent application FR2304675 in the name of the same applicant as the present application.

[0013] One aspect of the invention relates to a flexible electroluminescent film comprising successively: • a flexible support layer; • a first flexible electrode layer made of conductive material; • a flexible electrically insulating layer of dielectric material; • a flexible electroluminescent layer, comprising a layer of lu minophore having a refractive index of nium and emitting red light when excited by an electrostatic field; • a second flexible and transparent electrode layer made of conductive material having a neiec refractive index; and • a flexible and transparent protective layer.

[0014] Thanks to the invention, an electroluminescent film is provided which is advantageously thin, light, flexible, very bright and which can provide a red lighting color. This film has a high brightness allowing it to contrast with ambient light and to meet the brightness standards in force for rear lights, while having a much lower power consumption than LEDs. It is also sufficiently thin and flexible to be able to be applied to complex concave and / or convex surfaces. Advantageously, the nature and the low thickness of each of the layers of the electroluminescent film allow it in particular to be thin and flexible, but they can also allow it to be entirely transparent.

[0015] According to one aspect of the invention, the electroluminescent layer also comprises at least one refractive index matching element having a refractive index nng such that nium > nng > néiec. Thus, since light preferentially travels in the neighboring material having the nearest lower refractive index, the light emitted by the phosphor layer passes primarily through the material of the refractive index matching element, then passes through the second electrode layer to be emitted towards the top of the film. The refractive index of the matching element being intermediate between that of the adjacent layers for which it serves as an interface, its presence advantageously reduces any effect of refraction and / or reflection of light coming from the phosphor layer towards the second electrode layer.

[0016] According to another aspect of the invention, the phosphor layer comprises a mixture of particles of zinc sulfide, cadmium sulfide, zinc selenide and cadmium selenide, which particles are doped with copper. Indeed, this type of phosphor is advantageously very bright and can in particular provide a red lighting color.

[0017] According to a further aspect of the invention, the mixture has the following composition: (Znx,Cdi_x)(Sy,Seiy):Cu, with 0 <x< letO<y< 1.

[0018] According to one aspect of the invention, 0.8 <x<let0<y< 0,2.

[0019] According to another aspect of the invention, x = 0.9 and y = 0.1.

[0020] Indeed, numerous studies and tests carried out by the applicant have revealed that these compositions make it possible to provide a red lighting color that meets the standards currently in force, particularly for brake lights. These compositions advantageously make it possible to provide a red color with a wavelength between 625 and 635 nm, preferably substantially equal to 630 nm, and with a width at half-maximum of less than 20 nm.

[0021] According to an additional aspect of the invention, the phosphor layer emits a red color having a wavelength of between 625 and 635 nm, preferably substantially equal to 630 nm, and with a width at half-maximum of less than 20 nm, which makes it possible to meet the standards currently in force with regard to the color emitted by brake lights.

[0022] According to one aspect of the invention, the particles of the phosphor layer have a diameter of less than 29 qm, which in particular makes it possible to provide said layer with an extremely low thickness.

[0023] According to another aspect of the invention, the particles of the phosphor layer are incorporated into an epoxy resin, which in particular makes it possible to deposit the phosphor layer by screen printing.

[0024] According to one aspect of the invention, the protective layer comprises a transparent anti-UV material, an anti-UV additive or a transparent anti-UV coating. Thus, In addition to its role of protection against the environment, the protective layer also protects the film against the effects of ultraviolet radiation.

[0025] According to another aspect of the invention, the protective layer comprises a layer of transparent anti-UV material chosen from an acrylic resin, a mixture of high density polyethylene and zinc oxide, polycarbonate, polyamide-imide and poly(vinylidene fluoride). These materials have a very effective anti-UV protection effect, and they can therefore be provided in a very thin layer contributing to the flexibility and transparency of the film.

[0026] Another aspect of the invention relates to a vehicle element, which is at least partially covered by a film as described above. Thus, this vehicle element, even in the case where it has complex concave and / or convex shapes, can advantageously be associated with a film according to the invention in order to emit an intense red light. In the case where the film is advantageously transparent, its presence therefore remains extremely discreet as long as it is not luminous, which represents a major aesthetic advantage, particularly in the automotive field, where manufacturers generally seek to conceal the optics, which are considered unattractive.

[0027] According to one aspect of the invention, said vehicle element is a bodywork part, a dashboard, a decorative part, a grille, a logo or an optical element. Indeed, the film according to the invention can advantageously be used in a very wide range of applications, and not only in the automotive field.

[0028] A further aspect of the invention relates to a method of manufacturing a film as described above, which method comprises the following successive steps: • provision of a flexible support layer; • deposition of a first flexible electrode layer made of conductive material on the flexible support layer; • depositing a flexible electrically insulating layer of dielectric material on the first electrode layer; • depositing a flexible electroluminescent layer on the electrically insulating layer, said electroluminescent layer comprising a phosphor layer emitting red light when excited by an electrostatic field; • deposition of a second layer of flexible and transparent electrode made of conductive material on the electroluminescent layer; • deposition of a flexible and transparent protective layer on the second electrode layer.

[0029] According to one aspect of the invention, the deposition of the phosphor layer is carried out by screen printing, by atomic thin film deposition or by a sol-gel process. Screen printing is particularly advantageous in that it allows any type of phosphor to be deposited on rigid or flexible supports, in a controlled and inexpensive manner, while atomic layer deposition advantageously allows the deposit of an extremely thin and transparent layer controlled at the atomic level which provides very high light extraction. Sol-gel deposition is advantageous in particular in the case where the electroluminescent layer comprises refractive index adaptation elements embedded in a phosphor layer. BRIEF DESCRIPTION OF THE FIGURES

[0030] The present invention will be better understood and other characteristics and advantages will become apparent upon reading the detailed description which follows, comprising embodiments given by way of illustration with reference to the appended figures, presented as non-limiting examples, which may serve to complete the understanding of the present invention and the description of its embodiment and, where appropriate, contribute to its definition, in which:

[0031] [Fig.l] is an example of a schematic representation of an electroluminescent film according to a first variant of the invention where the electroluminescent layer comprises two successive layers.

[0032] [Fig.2] is an example of a schematic representation of an electroluminescent film according to a second variant of the invention where the electroluminescent layer comprises refractive index adaptation elements embedded in a phosphor layer.

[0033] [Fig.3] is a detail view of the part circled in [Fig.l].

[0034] [Fig.4] is a detail view of the part circled in [Fig.2]. DETAILED DESCRIPTION

[0035] Unless otherwise specified, the same element appearing in different figures has a single reference.

[0036] By convention, in the present application, the terms "lower" and "upper", and "inner" and "outer" are defined with respect to the position of the electroluminescent film as shown in [Fig.l] and [Fig.2]. Thus, an outer layer such as the protective layer is shown in the upper portion of the film in [Fig.l] and [Fig.2] while an inner layer, such as the support layer, is shown in the lower portion of the film, even if the film can be used in another orientation.

[0037] In the context of the invention, a material or a layer of material is said to be flexible if the mechanical and electrical properties of the film remain unchanged even under a significant stress of 2.5% with a concave and convex radius of curvature of 0.5 mm. In other words, it can in particular be considered that an electrode layer on the The support layer is flexible if, after a deformation of 2.5%, this deformation has no impact on the variation of the electrical resistance of the electrode film deposited on the support layer. The deformation (flexibility) can be evaluated using the following equation:

[0038] Deformation = ( ts - tp - tf ) / 2 x rc, where: • ts is the thickness of the support layer; • tp is the total thickness of the working layers (luminescent layer + layers electrically insulating) • tf is the total thickness of the electrode layers • rc is the radius of curvature.

[0039] Finally, the term “transparent” means an optically transparent material, i.e. one having a transmittance greater than 75% in the visible spectrum.

[0040] The film 1 according to the invention is a flexible electroluminescent film 1 comprising at least six flexible and superimposed layers, where each layer is in contact with the adjacent layer(s), namely a support layer 2, a first electrode layer 3, an electrically insulating layer 4, an electroluminescent layer 5, a second electrode layer 8 and a protective layer 9.

[0041] The film 1 according to the invention comprises a first layer, preferably lower, which is a flexible support layer 2, on which the other layers are deposited. This support layer 2 is preferably provided in the form of a roll film. It has for example a thickness of between 0.5 and 2.0 mm, preferably of between 0.8 and 1.5 mm and more preferably equal to 1.1 mm.

[0042] The support layer 2 may be transparent, in particular when it is desired that the entire film 1 be transparent. It may also be opaque, for example when the film 1 is intended to be applied to a surface which is also opaque.

[0043] In particular in the case where this layer is transparent, the support layer 2 is preferably made of PET (polyethylene terephthalate), Plasil (siloxane based on polymerized silicon monoxide), PMMA (polymethyl methacrylate), PCL (polycaprolactone), PC (polycarbonate), COP (cycloolefin polymer) or a mixture of at least two of these products.

[0044] The film 1 according to the invention comprises a second layer, deposited on the support layer 2, namely a first flexible electrode layer 3 made of conductive material.

[0045] This first electrode layer 3 is preferably provided in the form of a nanonet (or nanomesh in English), a metal lattice (or electrode mesh in English) or a homogeneous flat layer.

[0046] By nanonet is meant a net-shaped nanostructure, formed of nanowires in mutual contact and forming a mesh, whether these wires are for example intertwined, superimposed, welded or in one piece. A nanowire is a wire-shaped nanostructure, the diameter of which is on the nanometric scale, for example less than 100 nm, and the length of which is significantly greater.

[0047] By wire mesh is meant a net-shaped structure, formed of interlaced, superimposed, welded or single-piece wires, these wires having a diameter of the order of a micron.

[0048] The unitary patterns of the mesh of such a nanonet or metal lattice may for example be squares, rectangles, triangles, diamonds, hexagons or any other shapes and combinations thereof.

[0049] By homogeneous flat layer is meant a layer of material that is substantially flat, without significant unevenness in level, the composition and structure of which are substantially the same at all points, and which extends over a surface capable of forming an electrode of the desired surface area, for example substantially equal to the surface area of ​​the support layer 2 where it is desired to form a luminescent film 1.

[0050] The first electrode layer 3, when provided in the form of a nanonet or a metal mesh, preferably comprises silver nanowires (or AgNWs for Ag nanowires) or copper nanowires (or CuNWs for Cu nanowires).

[0051] It should be noted that wide band-gap nanowires composed of gallium nitride (GaN) or zinc oxide (ZnO) are materials that can also be used for nanowires.

[0052] When provided in the form of a planar layer, the first electrode layer 3 preferably comprises carbon nanotubes, graphene, a metal oxide-based material, a PEDOT [poly(3,4-ethylenedioxythiophene)]-based material, a PEDOT:PSS [poly(3,4-ethylenedioxythiophene) mixed with sodium poly(styrene sulfonate)]-based material or a PEDOT:TOS [poly(3,4-ethylenedioxythiophene) mixed with tosylate]-based material. Such a planar layer is as homogeneous as possible and usually unstructured.

[0053] The metal oxide-based materials for the first electrode layer 3 preferably comprise ITO (indium-tin oxide), ZnO (zinc oxide), ZnO:Al (aluminum-doped zinc oxide), TiO2 (titanium dioxide) and SnO2:F (fluorine-doped tin dioxide, or FTO for English Fluorine-doped Tin Oxide).

[0054] The first electrode layer 3 may be transparent or opaque.

[0055] The film 1 according to the invention comprises a third layer, deposited on the first electrode layer 3, namely a first flexible electrically insulating layer 4 in dielectric material.

[0056] This electrically insulating layer 4 has, for example, a thickness of between 1 and 50 qm. It preferably has a thickness of between 5 and 30 qm, more preferably of between 8 and 15 qm, for example substantially equal to 10 qm.

[0057] The dielectric material of the electrically insulating layer 4 preferably comprises an epoxy resin matrix loaded with particles of alkaline earth metal titanate, which alkaline earth metal is chosen from calcium titanate (CaTiO3), barium titanate (BaTiO3), strontium titanate (SrTiO3), mixed perovskites of barium and strontium titanate type (BaxSr(ix)TiO3, with 0 < x < 1) and a mixture of these products. Preferably x is such that 0 < x < 1.

[0058] The electrically insulating layer 4 may be transparent or opaque.

[0059] The film 1 according to the invention comprises a fourth layer, deposited on the electrically insulating layer 4, namely a flexible electroluminescent layer 5.

[0060] This electroluminescent layer 5 preferably comprises both a luminophoric material capable of generating red-colored light, and a refractive index adaptation material capable of directing the light emitted by the luminophoric material towards the following upper layers, namely the second electrode layer 8 and the protective layer 9.

[0061] By luminophore is meant here a material comprising electroluminescent pigments emitting light, here red in color, after having received energy supplied by an electric field.

[0062] Thus, the electroluminescent layer 5 comprises a phosphor layer 6 having a refractive index nium and preferably at least one refractive index matching element 7 having a refractive index nng so that nium > nng > néiec where néiec is the refractive index of the second electrode layer 8.

[0063] Since the refractive index of the refractive index matching element 7 is intermediate between that of the adjacent layers for which it serves as an interface, its presence reduces the effects of refraction and / or reflection of light coming from the phosphor layer 6 towards the second electrode layer 8.

[0064] Laboratory tests have proven that the addition of the refractive index adaptation element 7 in a conventional electroluminescent film multiplies the luminance of the latter by a value between 1.8 and 2. Thus, for a film 1 according to the invention, for which the luminance is optimized, a luminance greater than 1600 cd / m2 is obtained, which may even be greater than 2000 cd / m2, values ​​which have never been achieved to date for an electroluminescent film.

[0065] According to a first variant of the invention shown in [Fig.l] and [Fig.3], the electroluminescent layer 5 comprises two successive layers, namely a phosphor layer 6 located on the electrically insulating layer 4, and a refractive index matching element layer 7 located on the phosphor layer 6.

[0066] According to a second variant of the invention shown in [Fig.2] and [Fig.4], the electroluminescent layer 5 comprises a heterogeneous layer comprising refractive index adaptation elements 7 located on the electrically insulating layer 4 and embedded in a phosphor layer 6. According to this second variant of the invention, a refractive index adaptation element layer 7 may also be located on said heterogeneous layer.

[0067] The phosphor layer 6 has a refractive index nium whose value is for example approximately equal to 4. In the context of the invention, each refractive index is measured by method A of standard NF EN ISO 489 of March 2022.

[0068] The phosphor layer 6 comprises in particular a mixture of particles of zinc sulfide, cadmium sulfide, zinc selenide and cadmium selenide, which particles are doped with copper.

[0069] By metallic composition doped with a material, we mean here a metallic composition integrating small quantities (generally of the order of ppm) of a material which is introduced into its matrix in order to modify its properties.

[0070] The mixture of particles of the phosphor layer 6 preferably has the following composition: (Znx,Cdi_x)(Sy,Sei y):Cu.

[0071] Preferably, the values ​​of x and y are chosen such that 0 <x< leto<y< 1, plus préférentiellement telles que 0,8 <x<let0<y< 0,2, et encore x="0,9" y="0,1."

[0072] In order to meet current standards, the phosphor layer 6 emits a red color having a wavelength between 625 and 635 nm, preferably substantially equal to 630 nm, and with a width at half-height of less than 20 nm.

[0073] The phosphor layer 6 has, for example, a thickness of between 1 and 50 qm, preferably between 25 and 35 qm, and more preferably equal to 29 qm.

[0074] The deposition of the phosphor layer 6 is preferably carried out by screen printing, by atomic thin layer deposition (or ALD, for Atomic Layer Deposition) or by a sol-gel process.

[0075] Deposition by screen printing or by ALD is preferred in the case of the first variant of the invention, where the electroluminescent layer 5 comprises two successive layers, while deposition by sol-gel process is preferred in the case of the second variant of the invention, where the electroluminescent layer 5 comprises elements 7 adaptation of the refractive index embedded in a layer of phosphor 6.

[0076] Screen printing deposition generally makes it possible to provide a layer of luminophore 6 having, for example, a thickness of between 25 and 30 μm because the particles of the layer of luminophore 6 usually have a diameter less than or equal to 29 μm.

[0077] In the case where the deposition of the phosphor layer 6 is carried out by screen printing, the electroluminescent pigments are preferentially bound in an epoxy resin matrix.

[0078] The ALD technique consists of successively exposing a surface to different chemical precursors in order to obtain ultra-thin layers. In particular, it makes it possible to deposit a layer of phosphor 6 with a thickness of less than 1 μm, which considerably improves the luminous intensity of the film. Indeed, if the distance separating the electrodes is small, the electric field generated can be confined in a smaller space and the light emitted by electroluminescence is therefore stronger.

[0079] In the case where the deposition of the phosphor layer 6 is carried out by ALD, the phosphor layer 6 does not comprise a matrix and is composed solely of electroluminescent pigments.

[0080] The sol-gel process is for example associated with a dip-coating technique, which is a process that consists of immersing the substrate in a suitable coating composition, then removing it and partially drying it by dripping. Once the excess coating has drained off, the substrate is then dried completely, for example by baking, although many other techniques exist. This process is advantageous in that it guarantees a particularly smooth surface condition with reduced roughness.

[0081] It will be noted that the deposition technique for the phosphor layer 6 varies depending on the nature of the refractive index adaptation elements 7 and their shape (for example in layers or in islands / lines, see below). Indeed, if the refractive index adaptation element 7 comprises nano-antennas in the form of colloidal nanoparticles, the phosphor layer 6 is preferentially deposited without immersion and is composed solely of electroluminescent pigments, whereas if the refractive index adaptation element 7 comprises nano-antennas in the form of nanowires or the like, the phosphor layer 6 is preferentially deposited by a sol-gel process, for example associated with a dip-coating technique. In the latter case, the dip-coating process is used to deposit phosphor pigments around the nanowires to ensure a particularly smooth surface condition with reduced roughness.

[0082] The refractive index matching element 7 is transparent and, when in the form of a layer, the latter is flexible.

[0083] The refractive index matching element 7 has the role of directing the light emitted towards the phosphor layer 6 towards the second electrode layer 8 located above it, so that a greater part of the light emitted by the phosphor layer 6 passes through the second electrode layer 8, for greater brightness of the film 1.

[0084] Thus, the refractive index matching element 7 has a refractive index nng whose value is chosen so as to be between that of the two adjacent layers, namely the phosphor layer 6 and the second electrode layer 8, so as to form an intermediate layer reducing the effects of refraction and / or reflection of the light. The refractive index nng of the refractive index matching element is for example between 2 and 3.5.

[0085] The refractive index adaptation element 7 preferably comprises nano-antennas 10, also known as nano-light sensors, or nano-antennas in English.

[0086] These nano-antennas 10 preferably comprise nano-objects, preferably metallic, which promote the displacement of light from the phosphor layer 6 towards the second electrode layer 8, at a scale lower than the wavelength, so that the refractive index adaptation element 7 is also very thin and transparent.

[0087] According to a variant of the invention, the nano-objects may be colloidal nanoparticles, preferably nano-cubes. They may also be three-dimensional elements with a round, oval, triangular, square, rectangular, diamond-shaped, polygonal, etc. section or other polygonal three-dimensional elements, such as tetrahedra, octahedra, dodecahedra, icosahedra, etc.

[0088] A nanoparticle is a nano-object whose three dimensions are on the nanometric scale, that is to say a particle whose nominal diameter is less than approximately 100 nm.

[0089] The colloidal nanoparticles are preferably based on silver, gold, platinum or their mixture.

[0090] In the case of the second variant of the invention, where the electroluminescent layer 5 comprises refractive index adaptation elements 7 embedded in a phosphor layer 6, the nanoparticles are preferably deposited on the electrically insulating layer 4 by a drop deposition process, for example randomly, but so that the nanoparticles are well dispersed, without aggregates and with the most homogeneous density possible on the phosphor layer 6.

[0091] In the case of the first variant of the invention, where the electroluminescent layer 5 comprises two successive layers, the colloidal nanoparticles are preferably embedded in a matrix, for example in polyvinylpyrrolidone (PVP), or covered with a layer of PVP. This matrix or this layer of PVP has, for example, a thickness of approximately 1 to 10 nm, preferably approximately 3 nm.

[0092] According to another variant of the invention, the nano-objects may be nanofibers, nanotubes, nanofilaments, nanowires, nanorods, nanorods or a mixture of these nano-objects.

[0093] Nanofibers, nanotubes, nanofilaments, nanorods and nanorods are nanoobjects whose two similar external dimensions are on the nanometric scale, less than about 100 nm, and whose third dimension is significantly greater.

[0094] These nano-objects are preferably based on zinc oxide. They are grown, for example, by hydrothermal synthesis from a layer of ZnO seeds directly deposited on the phosphor layer 6 (first variant of the invention) or on the electrically insulating layer 4 (second variant of the invention).

[0095] These nano-objects are preferably arranged in the form of a very dense network of nanowires (NWs), nanofibers, nanotubes, nanofilaments, nanorods and / or nanorods aligned vertically. They preferably have a diameter of between 30 and 50 nm and a length of between 400 and 500 nm.

[0096] In the case of the second variant of the invention, where the electroluminescent layer 5 comprises refractive index adaptation elements 7 embedded in a phosphor layer 6, the nanoparticles and nano-objects can for example be deposited in the form of islands, that is to say in the form of small groups of nanoparticles and nano-objects isolated from one another, or in the form of lines, in particular parallel and / or which cross to form a network.

[0097] The refractive index adaptation elements 7, whether embedded in the phosphor layer 6 or in the form of a separate layer, may have a very low height (or thickness in the case of a layer), in particular less than 1 μm.

[0098] In particular depending on its thickness, the phosphor layer 6 can be transparent, translucent or opaque.

[0099] The film 1 according to the invention comprises a fifth layer, deposited on the electroluminescent layer 5, namely a second flexible and transparent electrode layer 8 made of conductive material.

[0100] This second electrode layer 8 may have the same characteristics as the first electrode layer 3.

[0101] It has a neiec refractive index whose value is for example approximately equal to 1.5.

[0102] Within the same film 1 according to the invention, the first electrode layer 3 and the second electrode layer 8 may be identical, for example by their nature, their composition, their thickness and / or their deposition method, but they can also be different. However, it is more practical and less expensive for the manufacture of the film 1 if the first layer and the second electrode layer 3, 8 are identical.

[0103] The first layer and the second electrode layer 3, 8 are provided to be connected to an alternating current source in order to form an electrostatic field between them, capable of exciting the phosphor layer 6 provided between these two layers 3, 8.

[0104] Finally, the film 1 according to the invention comprises a sixth layer, preferably upper, deposited on the second electrode layer 8, namely a flexible and transparent protective layer 9.

[0105] This protective layer 9 has, for example, a thickness of between 0.5 and 2.0 mm, preferably between 0.8 and 1.5 mm and more preferably equal to 1.1 mm.

[0106] It is preferably deposited by printing.

[0107] The protective layer 9 is preferably made of PET (polyethylene terephthalate), Plasil (polymerized silicon monoxide-based siloxane), PMMA (polymethyl methacrylate), PCL (polycaprolactone), PC (polycarbonate), COP (cycloolefin polymer) or a mixture of at least two of these products.

[0108] The protective layer 9 preferably comprises a transparent anti-UV material, an anti-UV additive or a transparent anti-UV coating in order to protect the film 1 from the harmful effects of ultraviolet radiation.

[0109] Indeed, the UV protection can be embedded in the mass of the material constituting the protective layer 9, or be in the form of a coating deposited on the lower and / or upper layer of said protective layer 9.

[0110] Similarly, the material constituting the protective layer 9 may naturally have an anti-UV effect, or be modified so as to have such an effect without this negatively affecting its flexibility and transparency in a significant manner.

[0111] Thus, the protective layer 9 comprises, for example, a layer of transparent anti-UV material chosen from an acrylic resin, a mixture of high-density polyethylene and zinc oxide, polycarbonate, polyamide-imide and poly(vinylidene fluoride).

[0112] The following materials are known to have anti-UV action: Plasil anti-UV, PC, PCL, PMMA, PET and COP.

[0113] Finally, the invention also relates to a method for manufacturing a film 1 as described previously and comprising the following successive steps: • provision of a flexible support layer 2; • deposition of a first flexible electrode layer 3 made of conductive material on the flexible support layer 2; depositing a flexible electrically insulating layer 4 of dielectric material on the first electrode layer 3; depositing a flexible electroluminescent layer 5 on the electrically insulating layer 4, said electroluminescent layer 5 comprising a phosphor layer 6 emitting red light when excited by an electrostatic field; depositing a second flexible and transparent electrode layer 8 made of conductive material on the electroluminescent layer 5; and depositing a flexible and transparent protective layer 9 on the second electrode layer 8.

Claims

Claims

1. Flexible electroluminescent film (1), characterized in that it successively comprises: - a flexible support layer (2); - a first flexible electrode layer (3) made of conductive material; - a flexible electrically insulating layer (4) made of dielectric material; - a flexible electroluminescent layer (5), comprising a phosphor layer (6) having a refractive index n ium and emitting red light when excited by an electrostatic field; - a second flexible and transparent electrode layer (8) made of conductive material having a refractive index neiec; and - a flexible and transparent protective layer (9).

2. Film (1) according to claim 1, characterized in that the electroluminescent layer (5) also comprises at least one refractive index matching element (7) having a refractive index nng such that nium > nng > néiec.

3. Film (1) according to claim 1 or 2, characterized in that the phosphor layer (6) comprises a mixture of particles of zinc sulfide, cadmium sulfide, zinc selenide and cadmium selenide, which particles are doped with copper.

4. Film (1) according to the preceding claim, characterized in that the mixture has the following composition: (Znx,Cdi_x)(Sy,Seiy):Cu, with 0 <x<let0<y<l.

5. Film (1) according to the preceding claim, characterized in that 0.8 <x<let0<y< 0,2.

6. Film (1) according to the preceding claim, characterized in that x = 0.9 and y = 0.

1.

7. Film (1) according to any one of the preceding claims, characterized in that the phosphor layer (6) emits a red color having a wavelength between 625 and 635 nm, preferably substantially equal to 630 nm, and with a width at half-height of less than 20 nm.

8. Film (1) according to any one of the preceding claims, characterized in that the particles of the phosphor layer (6) have a diameter of less than 29 qm.

9. Film (1) according to any one of the preceding claims, characterized in that the particles of the phosphor layer (6) are incorporated in an epoxy resin.

10. Film (1) according to any one of the preceding claims, characterized in that the protective layer (9) comprises a transparent anti-UV material, an anti-UV additive or a transparent anti-UV coating.

11. Film (1) according to any one of the preceding claims, characterized in that the protective layer (9) comprises a layer of transparent anti-UV material chosen from an acrylic resin, a mixture of high density polyethylene and zinc oxide, polycarbonate, polyamide-imide and poly(vinylidene fluoride).

12. Vehicle element, characterized in that it is at least partially covered by a film (1) according to any one of claims 1 to 11.

13. 11. Vehicle element according to the preceding claim, characterized in that said vehicle element is a bodywork part, a dashboard, a decorative part, a grille, a logo or an optical element.

14. A method of manufacturing a Film (1) according to any one of Claims 1 to 11, characterized in that it comprises the following successive steps: - providing a flexible support layer (2); - depositing a first flexible electrode layer (3) made of conductive material on the flexible support layer (2); - depositing a flexible electrically insulating layer (4) made of dielectric material on the first electrode layer (3); - depositing a flexible electroluminescent layer (5) on the electrically insulating layer (4), said electroluminescent layer (5) comprising a phosphor layer (6) emitting red light when excited by an electrostatic field; - depositing a second flexible and transparent electrode layer (8) made of conductive material on the electroluminescent layer nescent (5); - depositing a flexible and transparent protective layer (9) on the second electrode layer (8).

15. Method according to the preceding claim, characterized in that the deposition of the phosphor layer (6) is carried out by screen printing, by deposition of atomic thin layers or by a sol-gel process.

Citation Information

Patent Citations

  • Procede de production de levulose a partir d'amidon granulaire

    FR2304675A1

  • Electroluminescent light strip

    EP0611040A1