Method for preparing zirconia composite adsorbent based on droplet-confined space, and fluorine removal use of zirconia composite adsorbent
Patent Information
- Application Number
- GB2022017736
- Authority / Receiving Office
- GB · GB
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2021-09-02
- Filing Date
- 2022-02-10
- Publication Date
- 2024-10-16
- Estimated Expiration
- 2042-02-10
AI Technical Summary
Nano-zirconia adsorbents face challenges in collection and separation efficiency due to instability and uneven growth, leading to high column pressure and low separation efficiency during dynamic separation, necessitating improved interfacial stability and controlled growth.
A method involving lipase-immobilized poly(styrene-co-glycidyl methacrylate) nanosphere particles and high internal phase emulsions creates a droplet-confined space for the controlled preparation of zirconia composite adsorbents, enhancing stability and uniform growth, and utilizing this adsorbent for efficient fluoride removal.
The method achieves stable and uniform zirconia composite adsorbents with improved fluoride removal efficiency, demonstrating potential for deep fluorine removal in water samples with enhanced separation efficiency and reusability.
Smart Images

Figure 00000001_0000 
Figure 00000001_0001 
Figure 00000002_0000
Abstract
Description
METHOD FOR PREPARING ZIRCONIA COMPOSITE ADSORBENT BASED ON DROPLET-CONFINED SPACE, AND FLUORINE REMOVAL USE OF ZIRCONIA COMPOSITE ADSORBENT TECHNICAL FIELD The present disclosure belongs to the technical field of preparation of adsorption separation functional materials; and the present disclosure relates to the preparation of a zirconia composite adsorbent, and in particular to a method for preparing a zirconia composite adsorbent based on a high internal phase droplet-confined space, and an efficient fluorine removal use of the zirconia composite adsorbent. BACKGROUND As a serious worldwide problem, fluorine pollution is a potential threat to human health. Although low-concentration fluorides are important components for human health, the excessive intake of fluorides may cause irreversible damage, resulting in typical diseases such as dental fluorosis / skeletal fluorosis, nerve damage, and thyroid disease. Therefore, it is necessary to develop an effective technology to remove excessive fluorides in polluted water (including surface water, groundwater, and industrial wastewater), which can make a fluoride content in the polluted water lower than a limit fluoride content in drinking water required by the World Health Organization (WHO). The adsorption method is recognized as one of the effective fluorine removal technologies due to its advantages such as simple operation, low cost, and little secondary pollution. Currently, adsorbents used for the adsorption method to treat fluorine-containing wastewater include metal oxides, hydroxides, rare-earth metal composites, or the like. Zirconia- based materials developed based on the lewis acid-base theory can form a stable metal-ligand interaction with a fluoride, and exhibit a significant affinity for fluoride ions. Compared with the expensive rare earth metals, the zirconia-based materials are insoluble in a wide pH range and have significant cost advantages. Furthermore, a high specific surface area (SSA) of small-sized zirconia nanoparticles can improve the purification efficiency and selectivity by several orders of magnitude. However, small-sized zirconia nanoparticles are not easy to collect in practical applications, and thus it is easy to cause a large column pressure and a low separation efficiency during dynamic separation. The above problems can be effectively solved by loading zirconia nanoparticles on a porous microcarrier or allowing zirconia nanoparticles to in situ grow on a surface of a micromatrix. However, how to further enhance the interfacial stability between zirconia nanoparticles and microcarriers and how to control the homogeneous growth of zirconia nanoparticles are two new problems. Lipase is a biomacromolecule with strong tolerance to conditions such as pH and temperature and high operational stability. The immobilization of lipase can be achieved through covalent bonding between side-chain groups of a lipase protein molecule and functional groups on a surface of a carrier. In addition, the abundant and uniformly-distributed groups on a surface of lipase can provide an excellent platform for the homogeneous growth of nanoparticles. Confined space synthesis is one of the common strategies to achieve the controlled growth of functional nanoparticles. A confined space can enhance the ordered collision and rapid and thorough mixing of reactants, thereby achieving the purpose of synthesizing functional nanoparticles with an adjustable size and structure. The typical "flexible confined space" constructed by continuous phase films of high internal phase emulsions (HIPEs) has the advantages of simple preparation and reusability, and also has promising application prospects in the field of preparation of functional nanomaterials (catalysts, adsorbents, and the like). SUMMARY In order to solve the problems that the nano-zirconia adsorbents in the prior art are not easy to collect and it is easy to cause a large column pressure and a low separation efficiency during dynamic separation of the nano-zirconia adsorbents and in order to improve the interfacial stability of a zirconia-based composite and achieve the controlled homogeneous growth of nanoparticles, the present disclosure establishes a method for preparing a zirconia composite adsorbent based on a droplet-confined space. In the present disclosure, lipase-immobilized poly(styrene-co-glycidyl methacrylate) (P(St-co-GMA)) nanosphere particles are first prepared, namely enzyme-linked particles (ELPs), then oil-in-water (O / W) HIPEs are constructed, and a stable confined space is obtained in a continuous emulsion phase by adjusting an internal-phase ratio; the ELP and a zirconia precursor solution are added to the confined space to realize the controlled preparation of a zirconia composite adsorbent at room temperature; and a fluorine removal use of the adsorbent is explored. A method for preparing a zirconia composite adsorbent based on a droplet-confined space is provided, including the following steps: step 1. preparation of P(St-co-GMA) nanosphere particles: adding glycidyl methacrylate (GMA), styrene (St), and potassium persulfate (KPS) successively to deionized water under high-speed stirring to allow polymerization, cooling a resulting system to room temperature, subjecting a resulting emulsion to dialysis with deionized water, and lyophilizing to obtain the P(St-co-GMA) nanosphere particles; step 2. preparation of an ELP: adding porcine pancreatic lipase (PPL) to deionized water to prepare a PPL aqueous solution; adding the P(St-co-GMA) nanosphere particles prepared in the step 1 to a conical flask in which the PPL aqueous solution and phosphate buffered saline (PBS) are filled, subjecting a resulting mixed solution to stirring at room temperature and then to centrifugation, washing a resulting precipitate with PBS and deionized water successively, and lyophilizing the precipitate to obtain the ELP; step 3. preparation of HIPEs-ELP: dispersing the ELP prepared in the step 2, zirconium oxychloride octahydrate (ZrOCl,-8H20), and a surfactant in deionized water to obtain a water phase, adding an alkane as an oil phase dropwise to the water phase, and stirring a resulting mixture at a rotational speed of 5,000 rpm to 8,000 rpm for 10 min to 30 min to obtain O / W HIPEs, which is the HIPEs-ELP; step 4. preparation of HIPEs-sodium hydroxide (HIPEs-NaOH): adding an alkane as an oil phase dropwise to a NaOH solution, adding a surfactant as an emulsifier, and stirring a resulting mixture at a rotational speed of 5,000 rpm to 8,000 rpm for 10 min to 30 min to obtain O / W HIPEs with the same internal-phase ratio as the HIPEs-ELP, which is the HIPEs-NaOH; and step 5. preparation of the zirconia composite adsorbent (E-ELP-Zr): mixing the HIPEs-ELP prepared in the step 3 and the HIPEs-NaOH prepared in the step 4, and stirring a resulting mixture at a rotational speed of 3,000 rpm to 5,000 rpm for 0 min to 15 min to obtain a new HIPEs system; and placing the new HIPEs system at room temperature for 1.0 h to 10 h, adding ethanol for demulsification, and repeatedly washing with ethanol and deionized water to obtain the zirconia composite adsorbent E-ELP-Zr, which is lyophilized and stored in a sealed container In a preferred embodiment of the present disclosure, in the step 1, the P(St-co-GMA) nanosphere particles are synthesized according to the prior art (M. Wang, M.J Wang, S.M. Zhang, J.D. Chen, Pickering gel emulsion stabilized by enzyme immobilized polymeric nanoparticles: A robust and recyclable biocatalyst system for biphasic catalysis, React. Chem. Eng. 4 (2019) 1459- 1465. https: / / doi.org / 10.1039 / c9re00158a.). The synthesis method adopted by the present disclosure is disclosed here as follows* 200 mL of deionized water is added to a 250 mL three-necked flask, then the deionized water is stirred with a high-speed stirrer at a rotational speed of 250 rpm, and GMA, styrene, and KPS are added under the stirring; and a resulting mixture is stirred at 70°C for 12 h to allow polymerization and then cooled to room temperature, and a resulting emulsion is subjected to dialysis with deionized water for 48 h and then to lyophilization for later use, where GMA, styrene, and KPS are in amass ratio of 40g: 4.0g: 0.16 g. In step 2, in the PPL aqueous solution, a mass ratio of the PPL to the deionized water is (0.2- 0.5) g : (3.0-6.0) g; in the resulting mixed solution, the P(St-co-GMA), the PPL aqueous solution, and the PBS is in a ratio of (3.0-6.0) g : (3.0-6.0) g : (30-50) mL; and the stirring at room temperature is conducted for 3.0 hto 6.0 h. Preferably, the mass ratio of the PPL to the deionized wateris 0.3 g : 5.0 g; the P(St-co-GMA), the PPL aqueous solution, and the PBS is in a ratio of 5.0 g : 5.0 g : 40 mL, and the PBS has a concentration of 50 mM and a pH of 8; and the stirring at room temperature is conducted for 5.0 h. In step 3, the ELP, the ZrOCl,-8H:O0, and the surfactant are in a mass ratio of (100-500) mg : (200-1,000) mg : (200-800) mg; a volume ratio of the water phase to the oil phase alkane is (1.0- 6.0) mL : (15-50) mL; the alkane is n-decane, dodecane, or n-tridecane; and the surfactant is sodium dodecylbenzenesulfonate (SDBS), cetyl trimithyl ammonium bromide (CTAB), or Tween 80. Preferably, the ELP, the ZrOCl,-8H:O, and the surfactant are in a mass ratio of 100 mg : 500 mg : 200 mg; a volume ratio of the water phase to the oil phase alkane is 5 mL : 45 mL; the alkane is dodecane; and the surfactant is CTAB. In step 4, the oil phase alkane, the surfactant, and the NaOH is in a ratio of (5.0-30) mL : (200- 800) mg : (1.0-6.0) mL; the alkane is n-decane, dodecane, or n-tridecane; the surfactant is SDBS, CTAB, or Tween 80; and the NaOH solution has a concentration of 1.0 M. Preferably, the oil phase alkane, the surfactant, and the NaOH (1.0 M) are in a ratio of 27 mL : 200 mg : 3.0 mL; the alkane is dodecane; and the surfactant is CTAB. Preferably, in steps 3 and 4, the stirring is conducted at a rotational speed of 6,800 rpm for 5.0 min. Preferably, in the step 5, a volume ratio of the HIPEs-ELP to the HIPEs-NaOH is 5:3; and the stirring is conducted at a rotational speed of 3,000 rpm for 5.0 min. The present disclosure also discloses a use of the zirconia composite adsorbent prepared based on a droplet-confined space in the deep adsorption separation of fluoride ions. In an environment at 25°C, 5.0 mg of the prepared adsorbent (E-ELP-Zr) is placed in 8.0 mL of a 40 mg / L fluoride ion solution to allow adsorption for 1.0 h and then taken out, and a concentration of the fluoride ion solution is tested. An adsorption capacity is calculated through the following formula:Q, = Lote where Co(mg LL?) and Ce(mg / L) represent an initial concentration and an equilibrium concentration of fluoride ions, respectively; / (mL) represents a volume of the test solution; and m(g) represents a mass of the adsorbent. An integral area of a breakthrough curve is a total mass of fluoride ions adsorbed by the adsorbent, gotai(mg) Coq dt u i total = 1000 I. where Cag represents a change of an adsorption concentration of fluoride ions over time, Cag=Co-Ct, mg / L; Co represents the initial concentration of fluoride ions, mg / L; Ct represents a concentration of fluoride ions flowing out from a fixed bed at time t, mg / L; and t represents a time for fluoride ions to flow through the fixed bed, min. A contact time 7 of the adsorbent with the fluoride ion solution is set as an X-axis and a ratio of the concentration of fluoride ions flowing out from the fixed bed to the initial concentration (Cy / Co) is set as a Y-axis to plot a curve, which is the breakthrough curve. A time when an outlet concentration of the fixed bed is 10% of the initial concentration is set as a breakthrough time (start point) 7p of the breakthrough curve; and a time when the outlet concentration of the fixed bed is 95% of the initial concentration is set as a saturation time (decay point) 7. of the breakthrough curve. When the contact time of the adsorbent with the fluoride ion solution reaches the decay point, it means that the fixed bed is completely broken through, at which point active sites on a surface of the adsorbent are completely occupied and the adsorption saturation is achieved. The adsorption performance evaluation of the present disclosure is conducted as follows: Static adsorption test: 5.0 mg of the adsorbent (E-ELP-Zr) prepared according to the method of the present disclosure is added to 8.0 mL of each of test solutions with an initial pH of 3 to 12 (concentration: 40 mg / L) for adsorption, then a content of residual fluoride ions is determined with a fluorine electrode, and an adsorption capacity is calculated according to a determination result. After the adsorption saturation is achieved, an adsorption effect of the E-ELP-Zr is investigated based on adsorption capacities at different concentrations and temperatures. The recycling ability of the adsorbent is determined by an adsorption-desorption test. Dynamic adsorption test: 500 mg of the adsorbent (E-ELP-Zr) prepared according to the method of the present disclosure is mixed with 5.0 g of quartz sand (2.0 mm to 7.0 mm), a resulting mixture is filled into a cylindrical quartz tube, and two ends of the tube are sealed with filter paper to prevent the E-ELP-Zr from being flushed out of the filter column by a solution; and a fluoride ion solution is allowed to flow in from a bottom of a bed layer of a fixed bed through a peristaltic pump, and then to pass through a bed layer filled with the E-ELP-Zr adsorbent of the fixed bed such that fluoride ions are adsorbed by the E-ELP-Zr, during which a solution sample is collected from a water outlet pipe at a top of the cylindrical quartz tube at a specified interval and a concentration of fluoride ions is determined with a fluorine electrode. The influence of different flow rates on the adsorption effect of the E-ELP-Zr is explored. An adsorption effect of the E-ELP- Zr in an actual environment 1s investigated through adsorption tests on actual water samples. The present disclosure has the following beneficial effects: In the present disclosure, the controlled growth of a zirconia composite adsorbent is achieved in a "flexible confined space" constructed with a continuous phase film of HIPEs as a boundary. The most stable emulsion system is explored out by adjusting an internal-phase ratio and a reaction time and using different surfactants to prepare a zirconia composite adsorbent with uniform particle distribution and uniform size. The adsorbent can be used to efficiently adsorb fluoride ions, and an adsorption effect of the adsorbent shows that the adsorbent has a promising application prospect in the deep fluorine removal of actual water samples in the environment. BRIEF DESCRIPTION OF THE DRAWINGS FIG. 1 shows a scanning electron microscopy (SEM) image (a) of P(St-co-GMA) prepared in Example 1, a transmission electron microscopy (TEM) image (b) of ELP prepared in Example 2, a TEM image (d) of W-ELP-Zr prepared in Comparative Example, and a TEM image (c) of E- ELP-Zr prepared in Example 3; FIG. 2 is a picture of emulsions prepared in Example 3 (a), Example 4 (b), and Example 5 (¢); FIG. 3 shows the thermogravimetric analysis (TGA) curves for Example 10; FIG. 4 shows the influence of pH on the adsorption capacities of E-ELP-Zr and ELP; FIG. 5 shows the comparison of adsorption effect between W-ELP-Zr and E-ELP-Zr prepared in confined spaces with different internal-phase ratios; FIG. 6 shows the adsorption kinetics and model fitting curves of E-ELP-Zr; FIG. 7 shows the adsorption thermodynamics and model fitting curves of E-ELP-Zr; FIG. 8 shows the verification results of the regeneration ability of E-ELP-Zr; and FIG. 9 shows the influence of different flow rates on the adsorption of E-ELP-Zr to fluoride ions. DETAILED DESCRIPTION OF THE EMBODIMENTS The present disclosure is described in detail below with reference to the accompanying drawings and specific examples of the specification, such that those skilled in the art can better understand the present disclosure, but the present disclosure is not limited to the following examples. Comparative Example Synthesis of a zirconia composite adsorbent (ELP-Zr) in an aqueous solution (W-ELP-Zr) 100 mg of ELP and 500 mg of ZrOCl, 8H,0 were added to 5.0 mL of deionized water, and 3.0 mL of NaOH (1.0 M) was added dropwise under magnetic stirring, where the magnetic stirring was continuously conducted for 3.0 h; and the resulting product was washed with deionized water several times until a washing solution had a pH of 7, and then lyophilized for later use. FIG. 1d is a TEM image of W-ELP-Zr. Example 1 Polymerization to prepare P(St-co-GMA) particles with a size of 200 nm 200 mL of deionized water was added to a 250 mL three-necked flask, then the deionized water was stirred with a high-speed stirrer at a rotational speed of 250 rpm, and GMA (4.0 g), styrene (4.0 g), and KPS (0.16 g) were added under the stirring; and the resulting mixture was stirred at 70°C for 12 h to allow polymerization and then cooled to room temperature, and the resulting emulsion was subjected to dialysis with deionized water for 48 h and then to lyophilization for later use. FIG. 1a is an SEM image of the P(St-co-GMA) particles, and it can be seen from the figure that the particles are uniformly distributed and have a uniform size, indicating the successful preparation of the P(St-co-GMA) particles. Example 2 Preparation of ELP 0.3 g of PPL was taken and added to 5.0 g of water to prepare a 6.0 wt% PPL aqueous solution. PPL was immobilized on P(St-co-GMA) nanosphere particles through chemical coupling. 5.0 g of P(St-co-GMA) nanosphere particles were taken and added to a 150 mL conical flask in which 5.0 g of the PPL aqueous solution and 40 mL of PBS were filled; and the resulting mixed solution was stirred at room temperature for 5.0 h and then centrifuged, and the resulting precipitate was washed with PBS and deionized water and then lyophilized for later use. FIG. 1b is a TEM image of the ELP, and it can be seen from the figure that the PPL is successfully immobilized on the P(St-co-GMA) nanosphere particles. Example 3 (1) Preparation of P(St-co-GMA) particles: Preparation steps were the same as those in Example 1. (2) Preparation of ELP: Preparation steps were the same as those in Example 2. (3) ELP (100 mg), ZrOCl,-8H20 (500 mg), and CTAB (200 mg) were dispersed in deionized water (5.0 mL) to obtain a water phase, dodecane (45 mL) was added as an oil phase dropwise to the water phase, and the resulting mixture was stirred at a rotational speed of 6,800 rpm for 5.0 min to obtain O / W HIPEs, which was the HIPEs-ELP. (4) Dodecane (27 mL) was added as an oil phase dropwise to a NaOH solution (1.0 M) (3.0 mL) (to which CTAB (200 mg) was added as an emulsifier), and the resulting mixture was stirred at a rotational speed of 6,800 rpm for 5.0 min to obtain HIPEs-NaOH. (5) The HIPEs-ELP and HIPEs-NaOH prepared above were mixed and stirred at a rotational speed of 3,000 rpm for 5.0 min to obtain a new HIPEs system; and the new HIPEs system was placed at room temperature for 3.0 h, ethanol was added for demulsification, the resulting mixture was centrifuged, and the resulting precipitate was repeatedly washed with ethanol and deionized water to obtain the product E-ELP-Zr, which was lyophilized and stored in a sealed container. FIG. 1c is a TEM image of E-ELP-Zr, and it can be seen from the TEM image that zirconia grows more uniformly on a surface of the ELP compared with that in FIG. 1d. FIG. 2c is a picture of the emulsion, and it can be seen from the picture that the emulsion with CTAB as an emulsifier is stable. It can be seen from Table 1 that, when CTAB is used as an emulsifier, a surface tension at an interface between water and dodecane is small, which is conducive to the stabilization of the emulsion, corresponding to FIG. 2c. Example 4 (1) Preparation of P(St-co-GMA) particles: Preparation steps were the same as those in Example 1. (2) Preparation of ELP: Preparation steps were the same as those in Example 2. (3) ELP (100 mg), ZrOCl,-8H,0O (500 mg), and Tween 80 (200 mg) were dispersed in deionized water (5.0 mL) to obtain a water phase, dodecane (45 mL) was added as an oil phase dropwise to the water phase, and the resulting mixture was stirred at a rotational speed of 6,800 rpm for 5.0 min to obtain O / W HIPEs, which was the HIPEs-ELP. (4) Dodecane (27 mL) was added as an oil phase dropwise to a NaOH solution (1.0 M) (3.0 mL) (to which Tween 80 (200 mg) was added as an emulsifier), and the resulting mixture was stirred at a rotational speed of 6,800 rpm for 5.0 min to obtain HIPEs-NaOH. (5) The HIPEs-ELP and HIPEs-NaOH prepared above were mixed and stirred at a rotational speed of 3,000 rpm for 5.0 min to obtain a new HIPEs system; and the new HIPEs system was placed at room temperature for 3.0 h, ethanol was added for demulsification, the resulting mixture was centrifuged, and the resulting precipitate was repeatedly washed with ethanol and deionized water to obtain the product E-ELP-Zr, which was lyophilized and stored in a sealed container. FIG. 2a is a picture of the emulsion, and it can be seen from the picture that the emulsion with Tween 80 as an emulsifier is unstable Example § (1) Preparation of P(St-co-GMA) particles: Preparation steps were the same as those in Example 1. (2) Preparation of ELP: Preparation steps were the same as those in Example 2. (3) ELP (100 mg), ZrOCl, 8H,0 (500 mg), and SDBS (200 mg) were dispersed in deionized water (5.0 mL) to obtain a water phase, dodecane (45 mL) was added as an oil phase dropwise to the water phase, and the resulting mixture was stirred at a rotational speed of 6,800 rpm for 5.0 min to obtain O / W HIPEs, which was the HIPEs-ELP. (4) Dodecane (27 mL) was added as an oil phase dropwise to a NaOH solution (1.0 M) (3.0 mL) (to which SDBS (200 mg) was added as an emulsifier), and the resulting mixture was stirred at a rotational speed of 6,800 rpm for 5.0 min to obtain HIPEs-NaOH. (5) The HIPEs-ELP and HIPEs-NaOH prepared above were mixed and stirred at a rotational speed of 3,000 rpm for 5.0 min to obtain a new HIPEs system; and the new HIPEs system was placed at room temperature for 3.0 h, ethanol was added for demulsification, the resulting mixture was centrifuged, and the resulting precipitate was repeatedly washed with ethanol and deionized water to obtain the product E-ELP-Zr, which was lyophilized and stored in a sealed container. FIG. 2b is a picture of the emulsion, and it can be seen from the picture that the emulsion with SDBS as an emulsifier is unstable. Table 1 Surface tensions of different surfactants in Examples 3, 4, and 5 at an interface between water and dodecane | Surfactant | Mass p | Volume (water / dodecane) (mL) | Surface tension (mN / m) None 0 25 / 25 45 60.03 | Tweenso | 0.2 25 / 25 6.3£0.01 SDBS 0.3 as128 53+001 CTAB 023 25 / 25 310.01 Example 6 (1) Preparation of P(St-co-GMA) particles: Preparation steps were the same as those in Example 1. (2) Preparation of ELP: Preparation steps were the same as those in Example 2. (3) ELP (100 mg), ZrOCl,-8H20 (500 mg), and CTAB (200 mg) were dispersed in deionized water (5.0 mL) to obtain a water phase, dodecane (15 mL) was added as an oil phase dropwise to the water phase, and the resulting mixture was stirred at a rotational speed of 6,800 rpm for 5.0 min to obtain O / W HIPEs, which was the HIPEs-ELP. (4) Dodecane (9.0 mL) was added as an oil phase dropwise to a NaOH solution (1.0 M) (3.0 mL) (to which CTAB (200 mg) was added as an emulsifier), and the resulting mixture was stirred at a rotational speed of 6,800 rpm for 5.0 min to obtain HIPEs-NaOH. (5) The HIPEs-ELP and HIPEs-NaOH prepared above were mixed and stirred at a rotational speed of 3,000 rpm for 5.0 min to obtain a new HIPEs system; and the new HIPEs system was placed at room temperature for 3.0 h, ethanol was added for demulsification, the resulting mixture was centrifuged, and the resulting precipitate was repeatedly washed with ethanol and deionized water to obtain the product E-ELP-Zr, which was lyophilized and stored in a sealed container. Example 7 (1) Preparation of P(St-co-GMA) particles: Preparation steps were the same as those in Example 1. (2) Preparation of ELP: Preparation steps were the same as those in Example 2. (3) ELP (100 mg), ZrOCl,-8H,0 (500 mg), and CTAB (200 mg) were dispersed in deionized water (5.0 mL) to obtain a water phase, dodecane (20 mL) was added as an oil phase dropwise to the water phase, and the resulting mixture was stirred at a rotational speed of 6,800 rpm for 5.0 min to obtain O / W HIPEs, which was the HIPEs-ELP. (4) Dodecane (12 mL) was added as an oil phase dropwise to a NaOH solution (1.0 M) (3.0 mL) (to which CTAB (200 mg) was added as an emulsifier), and the resulting mixture was stirred at a rotational speed of 6,800 rpm for 5.0 min to obtain HIPEs-NaOH. (5) The HIPEs-ELP and HIPEs-NaOH prepared above were mixed and stirred at a rotational speed of 3,000 rpm for 5.0 min to obtain a new HIPEs system; and the new HIPEs system was placed at room temperature for 3.0 h, ethanol was added for demulsification, the resulting mixture was centrifuged, and the resulting precipitate was repeatedly washed with ethanol and deionized water to obtain the product E-ELP-Zr, which was lyophilized and stored in a sealed container. Example 8 (1) Preparation of P(St-co-GMA) particles: Preparation steps were the same as those in Example 1. (2) Preparation of ELP: Preparation steps were the same as those in Example 2. (3) ELP (100 mg), ZrOCl,-8H,0 (500 mg), and CTAB (200 mg) were dispersed in deionized water (5.0 mL) to obtain a water phase, dodecane (25 mL) was added as an oil phase dropwise to the water phase, and the resulting mixture was stirred at a rotational speed of 6,800 rpm for 5.0 min to obtain O / W HIPEs, which was the HIPEs-ELP. (4) Dodecane (17 mL) was added as an oil phase dropwise to a NaOH solution (1.0 M) (3.0 mL) (to which CTAB (200 mg) was added as an emulsifier), and the resulting mixture was stirred at a rotational speed of 6,800 rpm for 5.0 min to obtain HIPEs-NaOH. (5) The HIPEs-ELP and HIPEs-NaOH prepared above were mixed and stirred at a rotational speed of 3,000 rpm for 5.0 min to obtain a new HIPEs system; and the new HIPEs system was placed at room temperature for 3.0 h, ethanol was added for demulsification, the resulting mixture was centrifuged, and the resulting precipitate was repeatedly washed with ethanol and deionized water to obtain the product E-ELP-Zr, which was lyophilized and stored in a sealed container. Example 9 (1) Preparation of P(St-co-GMA) particles: Preparation steps were the same as those in Example 1. (2) Preparation of ELP: Preparation steps were the same as those in Example 2. (3) ELP (100 mg), ZrOCl,-8H20 (500 mg), and CTAB (200 mg) were dispersed in deionized water (5.0 mL) to obtain a water phase, n-tridecane (45 mL) was added as an oil phase dropwise to the water phase, and the resulting mixture was stirred at a rotational speed of 6,800 rpm for 5 min to obtain O / W HIPEs, which was the HIPEs-ELP. (4) n-Tridecane (27 mL) was added as an oil phase dropwise to a NaOH solution (1.0 M) (3.0 mL) (to which CTAB (200 mg) was added as an emulsifier), and the resulting mixture was stirred at a rotational speed of 6,800 rpm for 5.0 min to obtain HIPEs-NaOH. (5) The HIPEs-ELP and HIPEs-NaOH prepared above were mixed and stirred at a rotational speed of 3,000 rpm for 5.0 min to obtain a new HIPEs system; and the new HIPEs system was placed at room temperature for 3.0 h, ethanol was added for demulsification, the resulting mixture was centrifuged, and the resulting precipitate was repeatedly washed with ethanol and deionized water to obtain the product E-ELP-Zr, which was lyophilized and stored in a sealed container. Example 10 (1) Preparation of P(St-co-GMA) particles: Preparation steps were the same as those in Example 1. (2) Preparation of ELP: Preparation steps were the same as those in Example 2. (3) ELP (100 mg), ZrOCl,-8H20 (500 mg), and CTAB (200 mg) were dispersed in deionized water (5.0 mL) to obtain a water phase, n-decane (45 mL) was added as an oil phase dropwise to the water phase, and the resulting mixture was stirred at a rotational speed of 6,800 rpm for 5.0 min to obtain O / W HIPEs, which was the HIPEs-ELP. (4) n-Decane (27 mL) was added as an oil phase dropwise to a NaOH solution (1.0 M) (3.0 mL) (to which CTAB (200 mg) was added as an emulsifier), and the resulting mixture was stirred at a rotational speed of 6,800 rpm for 5.0 min to obtain HIPEs-NaOH. (5) The HIPEs-ELP and HIPEs-NaOH prepared above were mixed and stirred at a rotational speed of 3,000 rpm for 5.0 min to obtain a new HIPEs system; and the new HIPEs system was placed at room temperature for 3.0 h, ethanol was added for demulsification, the resulting mixture was centrifuged, and the resulting precipitate was repeatedly washed with ethanol and deionized water to obtain the product E-ELP-Zr, which was lyophilized and stored in a sealed container. FIG. 3 shows TGA curves of zirconia growing on the ELP in the aqueous solution and emulsion (with different internal-phase ratios) at the same dosage and the same reaction time. It can be seen from the figure that a mass loss is divided into three stages: a first stage (20°C to 305°C): a mass decreases from 100% to 85.26%, and a mass loss at this stage is caused by the evaporation of water in a sample; a second stage (305°C to 390°C): a mass decreases from 85.26% t0 63.80%, and a mass loss at this stage is caused by the breakage of a terminal strand of p(St-co- GMA); and a third stage (390°C to 500°C): a mass loss at this stage is caused by the decomposition of lipase. Starting from 500°C, a mass of the remaining zirconia is obtained, and the masses of the five samples are different, where the remaining zirconia content of W-ELP-Zr is the lowest, while the remaining zirconia content of E-ELP-Zr is higher than the remaining zirconia content of W- ELP-Zr, especially the remaining zirconia content of E-ELP-Zr prepared by the method in Example 3 is the highest. It indicates that the preparation of ELP-Zr in the confined space leads to the growth of more zirconia; and the higher the internal-phase ratio, the smaller the constructed confined space, which is conducive to the growth of zirconia on a surface of ELP. Performance test: 5.0 mg of the zirconia composite adsorbent (E-ELP-Zr) prepared by the method in Example 3 was added to 8.0 mL of each of prepared fluoride ion test solutions with a pH of 3 to 12 (concentration: 40 mg / L), and a final residual fluoride ion concentration was determined with a fluorine electrode. The experiment was conducted three times to equilibrate an adsorption capacity. The adsorption of the adsorbent to the solutions with a pH of 3 to 12 was investigated. Results were shown in FIG. 4. In a relatively wide pH range (4 to 7), the material exhibits a specified fluorine removal efficiency (average: 80.79%), and the adsorption performance is prominent at a pH of 6. However, in the pH range studied, the fluorine removal efficiency of ELP is very low (less than 10%). According to the hard and soft acids and bases (HSAB) theory, zirconium is a hard base and fluorine is a hard acid. Therefore, zirconia has a strong affinity for fluoride ions. This means that zirconia growing on a surface of the ELP plays a major role in the fluoride adsorption through an electrostatic interaction. Through the comparison of adsorption experiments, it can be seen from FIG. 5 that the E- ELP-Zr (Example 3) prepared in the droplet-confined space constructed by HIPEs exhibits the optimal adsorption effect, which is also consistent with the TGA curve in FIG. 3, indicating that zirconia plays a major role in the fluoride adsorption. Adsorption capacities of E-ELP-Zr at different time points were investigated, and the data were fitted by pseudo-first-order (PFO) and pseudo-second-order (PSO) kinetic models to obtain a kinetic curve and a fitting curve thereof (as shown in FIG. 6). An adsorption process of E-ELP- Zr can be divided into three steps. The kinetic and adsorption model fitting curve results of E-ELP- Zr were shown in FIG. 6. It can be seen from the figure that an adsorption rate of fluoride ions in the material was high. During the first 30 min, due to the electrostatic interaction of zirconia, the rapid adsorption was started and the adsorption capacity increased sharply; from 30 min to 50 min, the adsorption rate decreased, but was still high; and the adsorption equilibrium was reached about one h later, and zirconia particles on the surface of ELPs reacted with fluoride ions to produce a strong complex. FIG. 7 shows the thermodynamics and adsorption model fitting curve results at 288 K, 298 K, and 308 K. The adsorption capacity of E-ELP-Zr increased with the increase of fluoride ion concentration, and the adsorption process was an endothermic process. FIG. 8 shows the adsorption capacities of E-ELP-Zr in five adsorption and desorption cycles. After the five cycles, the adsorption capacity of E-ELP-Zr decreased slightly compared with the original value (decreased to 88.55% of the first adsorption capacity), indicating prominent reusability. 500 mg of the adsorbent (E-ELP-Zr) prepared according to the method of the present disclosure was mixed with 5.0 g of quartz sand (2.0 mm to 7.0 mm), the resulting mixture was filled into a cylindrical quartz tube, and two ends of the tube were sealed with filter paper to prevent the E-ELP-Zr from being flushed out of the filter column by a solution; and a fluoride ion solution (8.0 mg L'!) was allowed to flow in from a bottom of a bed layer of a fixed bed through a peristaltic pump and to pass through a bed layer filled with the E-ELP-Zr adsorbent of the fixed bed. A flow rate of the peristaltic pump was adjusted to make the fluoride ion solution flow in from the bottom of the bed layer of the adsorption column at 1 mL / min, 2 mL / min, and 3 mL / min. During the above process, fluoride ions in the solution were trapped by the E-ELP-Zr adsorbent in the fixed bed, and 20 mL of a fluoride ion solution was collected from a water outlet pipe at a specified interval and tested with a fluorine electrode to obtain a fluoride ion concentration. The influence of different flow rates of the peristaltic pump on the adsorption of E-ELP-Zr to fluoride ions was shown in FIG. 9, and it can be seen that, when the flow rate of the peristaltic pump increased from 1.0 mL / min to 3.0 mL / min, the breakthrough time decreased from 250 min to 72 min and the adsorption equilibrium time decreased from 511 min to 154 min. As the flow rate increased, a slope of a breakthrough curve increased, and the time to reach adsorption equilibrium was shortened. The earliest breakthrough and depletion of the bed layer was observed at the highest flow rate, and a plausible explanation for this phenomenon may be that a residence time of the solute fluoride ions in the packed bed column was insufficient, resulting in the limited diffusion of fluoride ions in the solution at a high flow rate to the adsorbent E-ELP-Zr. The adsorption capacity of E-ELP-Zr at the lowest flow rate may be improved because the residence time was sufficient, such that the contact between the fluoride ion solution and the adsorbent E- ELP-Zr was prolonged and active adsorption sites were fully utilized. A dynamic adsorption test was also conducted on an actual sample at a flow rate of 1.0 mL / min, and the actual sample had a fluoride ion concentration of 7.15 mg L™. The adsorbent E-ELP-Zr has a prominent adsorption capacity for fluoride ions. The above are merely some examples of the present disclosure, and are not intended to limit the scope of the present disclosure. Any equivalent structure or equivalent process transformation made with the description of the present disclosure, or direct or indirect application thereof in other related technical fields, shall still fall in the protection scope of the present disclosure.
Claims
1. A method for preparing a zirconia composite adsorbent based on a flexible confined space, characterized by comprising the following steps:step 1. preparation of poly(styrene-co-glycidyl methacrylate) (P(St-co-GMA)) nanosphere particles for later use;step 2. preparation of an enzyme-linked particle (ELP) for later use:adding porcine pancreatic lipase (PPL) to deionized water to prepare a porcine pancreatic lipase aqueous solution;adding the P(St-co-GMA) nanosphere particles prepared in the step 1 to a conical flask in which the PPL aqueous solution and phosphate buffered saline are filled, subjecting a resulting mixed solution to stirring at room temperature and then to centrifugation, washing a resulting precipitate with phosphate buffered saline and deionized water successively, and lyophilizing the precipitate to obtain the ELP;step 3. preparation of high internal phase emulsions (HIPEs)-ELP:dispersing the ELP prepared in the step 2, zirconium oxychloride octahydrate ZrOCh 8H2O, and a surfactant in deionized water to obtain a water phase, adding an alkane as an oil phase dropwise to the water phase, and stirring a resulting mixture at a rotational speed of 5,000 rpm to 8,000 rpm for 10 min to 30 min to obtain oil-in-water (O / W) HIPEs, which is the HIPEs-ELP;step 4. preparation of HIPEs-sodium hydroxide (HIPEs-NaOH):adding an alkane as an oil phase dropwise to a NaOH solution, adding a surfactant as an emulsifier, and stirring a resulting mixture at a rotational speed of 5,000 rpm to 8,000 rpm for 10 min to 30 min to obtain O / W HIPEs with the same internal-phase ratio as the HIPEs-ELP, which is the HIPEs-NaOH; andstep 5. preparation of the zirconia composite adsorbent E-ELP-Zr:mixing the HIPEs-ELP prepared in the step 3 and the HIPEs-NaOH prepared in the step 4, and stirring a resulting mixture at a rotational speed of 3,000 rpm to 5,000 rpm for 1 min to 15 min to obtain a new HIPEs system; and placing the new HIPEs system at room temperature for 1.0 h to 10 h, adding ethanol for demulsification, and repeatedly washing with ethanol and deionized water to obtain the zirconia composite adsorbent E-ELP-Zr, which is lyophilized and stored in a sealed container.
2. The method for preparing the zirconia composite adsorbent based on the flexible confined space according to claim 1, characterized in that in the step 2, in the porcine pancreatic lipase aqueous solution, a mass ratio of the PPL to the deionized water is (0.2-0.5) g : (3.0-6.0) g; in the resulting mixed solution, the P(St-co-GMA), the porcine pancreatic lipase aqueous solution, and01 08 23the phosphate buffered saline are in a ratio of (3.0-6.0) g : (3.0-6.0) g : (30-50) mL; and the stirring at room temperature is conducted for 3.0 h to 6.0 h.
3. The method for preparing the zirconia composite adsorbent based on the flexible confined space according to claim 2, characterized in that in the porcine pancreatic lipase aqueous solution, the mass ratio of the PPL to the deionized water is 0.3 g : 5.0 g; in the resulting mixed solution, the P(St-co-GMA), the porcine pancreatic lipase aqueous solution, and the phosphate buffered saline are in a ratio of 5.0 g : 5.0 g : 40 mL, and the phosphate buffered saline has a concentration of 50 mM and a pH of 8; and the stirring at room temperature is conducted for 5.0 h.
4. The method for preparing the zirconia composite adsorbent based on the flexible confined space according to claim 1, characterized in that in the step 3, the ELP, the ZrOCh 8H2O, and the surfactant are in a mass ratio of (100-500) mg : (200-1,000) mg : (200-800) mg; a volume ratio of the water phase to the oil phase alkane is (1.0-6.0) mL : (15-50) mL; the alkane is w-decane, dodecane, or w-tridecane; and the surfactant is sodium dodecylbenzenesulfonate, cetyl trimithyl ammonium bromide, or Tween 80.
5. The method for preparing the zirconia composite adsorbent based on the flexible confined space according to claim 4, characterized in that the ELP, the ZrOCh 8H2O, and the surfactant are in a mass ratio of 100 mg : 500 mg : 200 mg; a volume ratio of the water phase to the oil phase alkane is 5.0 mL : 45 mL; the alkane is dodecane; and the surfactant is cetyl trimithyl ammonium bromide.
6. The method for preparing the zirconia composite adsorbent based on the flexible confined space according to claim 1, characterized in that in the step 4, the oil phase alkane, the surfactant, and the NaOH solution are in a ratio of (5.0-30) mL : (200-800) mg : (1.0-6.0) mL; the alkane is w-decane, dodecane, or w-tridecane; the surfactant is sodium dodecylbenzenesulfonate, cetyl trimithyl ammonium bromide, or Tween 80; and the NaOH solution has a concentration of 1.0 M.
7. The method for preparing the zirconia composite adsorbent based on the flexible confined space according to claim 6, characterized in that in the step 4, the oil phase alkane, the surfactant, and the NaOH are in a ratio of 27 mL : 200 mg : 3.0 mL; the alkane is dodecane; and the surfactant is cetyl trimithyl ammonium bromide.
8. The method for preparing the zirconia composite adsorbent based on the flexible confined space according to claim 1, characterized in that in steps 3 and 4, the stirring is conducted at a rotational speed of 6,800 rpm for 5.0 min.
9. The method for preparing the zirconia composite adsorbent based on the flexible confined space according to claim 1, characterized in that in the step 5, a volume ratio of the HIPEs-ELP to the HIPEs-NaOH is 5:3; and the stirring is conducted at a rotational speed of 3,000 rpm for 5.0 min.
10. A use of a zirconia composite adsorbent prepared by the method according to any one of claims 1 to 9 in the adsorption separation of fluoride ions.01 08 23
Citation Information
Patent Citations
Method for preparing zirconium oxide composite adsorbent based on liquid drop confinement space and defluorination application of zirconium oxide composite adsorbent
CN113893830A