Method for preparing refractory material from waste battery residues, and use of refractory material

The method transforms waste battery residues into refractory materials for safe packaging and storage by processing them with wet clay and potassium carbonate, addressing secondary pollution and enhancing safety performance.

GB2618499BActive Publication Date: 2024-11-06GUANGDONG BRUNP RECYCLING TECH CO LTD +2
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
GB2023013009
Authority / Receiving Office
GB · GB
Patent Type
Patents
Current Assignee / Owner
Priority Date
2021-11-17
Filing Date
2022-08-11
Publication Date
2024-11-06
Estimated Expiration
2042-08-11

AI Technical Summary

Technical Problem

Existing waste battery recycling methods generate impure residues like iron-aluminum slags, which are often landfilled, causing secondary environmental pollution and resource waste, as they are not effectively recycled into valuable materials.

Method used

A method involving dismantling waste lithium-ion batteries, sorting and processing powders to obtain graphite and iron-aluminum slags, mixing with wet clay, and then pre-sintering, calcining, and washing to produce refractory materials, which can be used for packaging and storage of waste batteries, utilizing potassium carbonate to enhance porosity and absorption capacity.

Benefits of technology

This method effectively recycles waste residues into refractory materials that provide heat insulation, shockproofing, and electrolyte absorption, reducing fire risks and environmental pollution, while being cost-effective and environmentally friendly, with high commercial application value.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000001_0000
    Figure 00000001_0000
  • Figure 00000002_0000
    Figure 00000002_0000
  • Figure 00000002_0001
    Figure 00000002_0001
Patent Text Reader

Abstract

A method for preparing a refractory material from waste battery residues. The method comprises the following steps: (1) disassembling waste batteries, then sorting same to obtain positive and negative electrode powders, leaching the positive and negative electrode powders with an acid, filtering same to obtain a graphite slag, and then subjecting the filtrate to copper removal, followed by the addition of an alkali for a precipitation reaction, wherein the resulting precipitate is an iron-aluminum slag; (2) wrapping the graphite slag obtained in step (1) with wet clay to form an inner core material, then mixing wet clay with the iron-aluminum slag, wrapping the inner core material with same, and aging the wrapped inner core material to obtain a blank; (3) pre-sintering, calcining and cooling the blank prepared in step (2) to obtain a fired product; and (4) washing and drying the fired product to obtain the refractory material. By means of the present method, waste residues generated during the recovery process of waste batteries can be further recycled, thereby preventing same from causing secondary pollution to the environment.
Need to check novelty before this filing date? Find Prior Art

Description

TECHNICAL FIELD The present disclosure belongs to the technical field of waste battery recycling, and more 5 particularly, to a method for preparing refractory materials with waste battery residues, and an application of the refractory materials. BACKGROUND With the increasing degree of electrification in China, batteries have been used in various 10 fields of people's lives, so there are a large number of waste batteries. Therefore, recycling of waste batteries is of great practical significance, which is beneficial to environmental protection while recycling resources. In the existing recycling process of waste batteries, some waste residues such as iron-aluminum slags are often produced while recycling useful metals. Because the components of these waste residues are impure, the waste residues are often treated by direct landfill, which still causes secondary pollution to the environment. Therefore, the existing recycling methods of waste batteries still need to be further upgraded. SUMMARY The present disclosure aims at solving at least one of the technical problems in the prior art. 20 Therefore, the present disclosure provides a method for preparing refractory materials with waste battery residues and an application of the refractory materials. By this method, the waste residues generated in the recycling process of the waste batteries can be further recycled to avoid secondary pollution to the environment. The above-mentioned technical objects of the present disclosure are achieved by the following 25 technical solutions. A method for preparing refractory materials with waste lithium ion battery residues comprises the following steps of (1) dismantling a waste lithium ion battery and sorting to a mixture of obtain positive and negative electrode powders, performing acid leaching on the mixture of positive and negative powders, filtering to obtain a graphite slag, then removing copper from a filtrate by adding 26 06 24 iron, and adding an alkali for a precipitation reaction to obtain an iron-aluminum slag; (2) wrapping the graphite slag obtained in step (1) with wet clay into an inner core material, mixing further wet clay with the iron-aluminum slag and then wrapping the inner core material, and aging to obtain a blank; (3) pre-sintering, calcining and cooling the blank prepared in step (2) to obtain a sintered 5 product; and (4) washing and drying the sintered product to obtain the refractory materials; wherein the wet clay in step (2) is prepared by mixing clay with a potassium carbonate solution; wherein a mass ratio of the clay to the potassium carbonate solution in the wet clay is (55 to 79): (21 to 45). Further preferably, the mass ratio of the clay to the potassium carbonate solution in the wet clay is 67: 33. 10 Preferably, the potassium carbonate solution is prepared by potassium carbonate and water, wherein a mass ratio of the potassium carbonate to the water is (1 to 5): (20 to 40). Further preferably, the potassium carbonate solution is prepared by potassium carbonate and water, wherein the mass ratio of the potassium carbonate to the water is 3: 30. Preferably, in step (2), a mass ratio of the iron-aluminum slag to the graphite slag and the wet clay is (5 to 7): (2 to 4): 1. Further preferably, in step (2), the mass ratio of the iron-aluminum slag to the graphite slag and the wet clay is 6: 3: 1. Preferably, in step (2), the aging is performed at a temperature of 25°C to 35°C, and lasts for 12 hours to 36 hours. 20 Further preferably, in step (2), the aging is performed at a temperature of 25°C, and lasts for 24 hours. Preferably, in step (3), the pre-sintering is performed at a temperature of 300°C to 500°C, and lasts for 1 hour to 3 hours. Further preferably, in step (3), the pre-sintering is performed at a temperature of 400°C, and 25 lasts for 1 hour. Preferably, in step (3), the calcining is performed at a temperature of 900°C to l,100°C and lasts for 1 hour to 3 hours, and a heating rate from pre-sintering to calcining is 3°C / min to 10°C / min. Preferably, in step (3), the calcining is performed at a temperature of l,100°C and lasts for 1 30 hour, and the heating rate from pre-sintering to calcining is 5°C / min. Preferably, the washing in step (4) is to wash the sintered product with a hydrochloric acid first and then with water. Preferably, the drying in step (4) is performed at a temperature of 80°C and lasts for 6 hours. Specifically, in the process of packaging, transportation and storage of the waste battery, the refractory materials are placed between a packaging box and the waste battery. The present disclosure has the beneficial effects that: (1) The preparation method provided by the present disclosure is simple in operation, mild in reaction conditions, pollution-free to the environment, suitable for industrial production, and can effectively recycle the industrial waste residues generated in the battery recycling process to synthesize new refractories, thereby turning waste into wealth, avoiding secondary pollution, reducing the manufacturing cost and optimizing the recycling process. (2) In the preparation method provided by the present disclosure, an activation ability of the potassium carbonate is utilized for the first time. When the calcining temperature is higher than 750°C, K2CO3 is decomposed into CO2 and K2O (K2CO3 = K2O + CO2 T), and a part of K2O is reduced by carbon atoms at high temperature to generate metal potassium, which consumes carbon and increases the specific surface area; and when, when the temperature is higher than a boiling point (774°C) of the metal potassium, the metal potassium enters the refractory materials structure in the form of potassium vapor, which increases the distance between the refractories, thus increasing the pore volume. In addition, the produced CO2 is a good physical activator and porogen, which can further increase the pore volume of the refractory materials, further improve the absorption capacity of the refractory materials and further improve the safety performance of the refractory materials. (3) Waste batteries, such as discarded lithium ion batteries, may be short-circuited due to improper packaging during packaging, transportation and storage due to high-risk factors such as flammability and explosiveness, resulting in high-risk accidents. The present disclosure first proposes to use the waste battery residues as the raw materials to prepare the refractory materials, and apply the refractory materials in the packaging, transportation and storage process of the waste batteries. The refractory materials prepared by the present disclosure can be placed between the packaging box and the waste battery, thus achieving the functions of heat insulation, shockproof, absorbing leaked electrolyte, isolating the contact between the waste battery and the air when the waste battery is burning, reducing the fire and preventing the battery from exploding. Moreover, when the waste battery catches fire in the package, the refractory materials can quickly absorb heat, isolate oxygen, weaken the fire, and finally extinguish the fire. Meanwhile, the refractory materials can protect the package from damage and gas and liquid leakage, and realize the safe packaging, transportation and storage of the waste battery. According to the present disclosure, through the high-temperature test of the refractory materials and the test of the electrolyte absorption capacity, it is proved that the refractory materials can effectively improve the safety performance of the waste battery in the recycling process. (4) The present disclosure designs a multi-layer porous refractory, wherein the graphite slag in the inner layer expands after calcining to form a porous graphite structure, the middle layer is clay, and the outer layer is iron-aluminum slag and clay. With the multilayer structure, the electrolyte and heat can be respectively absorbed layer by layer. Due to pore-forming and activating abilities of the potassium carbonate, the porous refractory with inner, middle and outer layers is formed, wherein the iron-aluminum slag and the clay layer have strong heat resistance and absorb heat quickly, thus ensuring that the heat will not be emitted to the environment. The porous graphite layer has strong absorption capacity, and the leaked electrolyte permeates through the middle and outer layers, and is finally absorbed into the porous graphite layer for storage, thus ensuring that the electrolyte will not leak out of the refractory materials and cause dangerous accidents. (5) The porous refractory prepared by the present disclosure has the characteristic of recycling, effectively controls the cost, shows the characteristic of environmental protection, has no metal pollution, avoids resource waste, prolongs the service life, and keeps the ability thereof unchanged after repeated use for many times, which indicates that the refractory materials has excellent stability and high commercial application value. BRIEF DESCRIPTION OF DRAWINGS FIG. 1 is an SEM graph of Embodiment 1; FIG. 2 is an isothermal adsorption-desorption curve of Embodiment 1; FIG. 3 is a thermogravimetric curve of Embodiment 1; FIG. 4 is a diagram showing absorption capacities of Embodiments 1, 3, 5 and Comparative Example 1 on an organic electrolyte of a lithium ion battery; FIG. 5 is a diagram showing a repeated adsorption performance of Embodiment 1; and FIG. 6 is an SEM graph of Comparative Example 1. DETAILED DESCRIPTION The present disclosure is further illustrated hereinafter with reference to the specific 26 06 24 embodiments, wherein the room temperature and normal temperature are about 25°C in the experimental operations of the embodiments. Waste batteries are purchased from Guangdong Brunp Recycling Technology Co., Ltd., potassium carbonate, sodium hydroxide, sodium carbonate and sodium chlorate are purchased from Shanghai Macklin Biochemical Co., Ltd., and sulfuric acid and 5 hydrochloric acid are purchased from Shanghai Aladdin Bio-Chem Technology Co., Ltd. Embodiment 1: A method for preparing refractory materials with waste battery residues comprises the following steps of: (1) dismantling a waste battery with a dismantling machine, then pyrolyzing, crushing and 10 mechanically sorting to obtain positive and negative powders, performing acid leaching on the positive and negative powders with a sulfuric acid, and filtering to obtain a graphite slag, then adding iron to a filtrate to remove copper, and then adding sodium hydroxide, sodium carbonate and sodium chlorate for a precipitation reaction to obtain an iron-aluminum slag; (2) wrapping the graphite slag obtained in step (1) with wet clay into an inner core material, then mixing a small amount of wet clay with the iron-aluminum slag and then wrapping the inner core material to form a globularity, and aging at 25°C for 12 hours to obtain a blank, wherein a mass ratio of the sum of the iron-aluminum slag to the graphite slag and the wet clay used in the inner and outer layers was 5: 4: 1, and the wet clay was obtained by mixing clay and a potassium carbonate solution; a mass ratio of the clay to the potassium carbonate solution was 79: 21, and the 20 potassium carbonate solution was prepared by potassium carbonate and water, wherein a mass ratio of the potassium carbonate to the water was 1: 20; (3) calcining the blank prepared in step (3) in a muffle furnace, pre-sintering at 300°C for 1 hour, then heating to 900°C for 1 hour at a heating rate of 5°C / min, and cooling with the furnace to obtain a sintered product; and 25        (4) washing the sintered product with IM hydrochloric acid solution first and then with distilled water, and drying at 80°C for 6 hours to obtain the refractory materials. Refractory materials prepared by the preparation method above. An application of the refractory materials above in packaging, transportation and storage of a waste battery. 30 Embodiment 2: A method for preparing refractory materials with waste battery residues comprises the following steps of: (1) dismantling a waste battery with a dismantling machine, then pyrolyzing, crushing and mechanically sorting to obtain positive and negative powders, performing acid leaching on the positive and negative powders with a sulfuric acid, and filtering to obtain a graphite slag, then adding iron to a filtrate to remove copper, and then adding sodium hydroxide, sodium carbonate and sodium chlorate for a precipitation reaction to obtain an iron-aluminum slag; (2) wrapping the graphite slag obtained in step (1) with wet clay into an inner core material, then mixing a small amount of wet clay with the iron-aluminum slag and then wrapping the inner core material to form a globularity, and aging at 25°C for 36 hours to obtain a blank, wherein a mass ratio of the sum of the iron-aluminum slag to the graphite slag and the wet clay used in the inner and outer layers was 5: 4: 1, and the wet clay was obtained by mixing clay and a potassium carbonate solution; a mass ratio of the clay to the potassium carbonate solution was 55: 45, and the potassium carbonate solution was prepared by potassium carbonate and water, wherein a mass ratio of the potassium carbonate to the water was 5: 40; (3) calcining the blank prepared in step (3) in a muffle furnace, pre-sintering at 500°C for 3 hours, then heating to l,100°C for 3 hours at a heating rate of 5°C / min, and cooling with the furnace to obtain a sintered product; and (4) washing the sintered product with IM hydrochloric acid solution first and then with distilled water, and drying at 80°C for 6 hours to obtain the refractory materials. Refractory materials prepared by the preparation method above. An application of the refractory materials above in packaging, transportation and storage of a waste battery. Embodiment 3: A method for preparing refractory materials with waste battery residues comprises the following steps of: (1) dismantling a waste battery with a dismantling machine, then pyrolyzing, crushing and mechanically sorting to obtain positive and negative powders, performing acid leaching on the positive and negative powders with a sulfuric acid, and filtering to obtain a graphite slag, then adding iron to a filtrate to remove copper, and then adding sodium hydroxide, sodium carbonate and sodium chlorate for a precipitation reaction to obtain an iron-aluminum slag; (2) wrapping the graphite slag obtained in step (1) with wet clay into an inner core material, then mixing a small amount of wet clay with the iron-aluminum slag and then wrapping the inner core material to form a globularity, and aging at 25°C for 24 hours to obtain a blank, wherein a mass ratio of the sum of the iron-aluminum slag to the graphite slag and the wet clay used in the inner and outer layers was 6: 3: 1, and the wet clay was obtained by mixing clay and a potassium carbonate solution; a mass ratio of the clay to the potassium carbonate solution was 67: 33, and the potassium carbonate solution was prepared by potassium carbonate and water, wherein a mass ratio of the potassium carbonate to the water was 3:30; (3) calcining the blank prepared in step (3) in a muffle furnace, pre-sintering at 400°C for 1 hour, then heating to l,100°C for 1 hour at a heating rate of 5°C / min, and cooling with the furnace to obtain a sintered product; and (4) washing the sintered product with IM hydrochloric acid solution first and then with distilled water, and drying at 80°C for 6 hours to obtain the refractory materials. Refractory materials prepared by the preparation method above. An application of the refractory materials above in packaging, transportation and storage of a waste battery. Embodiment 4: A method for preparing refractory materials with waste battery residues comprises the following steps of: (1) dismantling a waste battery with a dismantling machine, then pyrolyzing, crushing and mechanically sorting to obtain positive and negative powders, performing acid leaching on the positive and negative powders with a sulfuric acid, and filtering to obtain a graphite slag, then adding iron to a filtrate to remove copper, and then adding sodium hydroxide, sodium carbonate and sodium chlorate for a precipitation reaction to obtain an iron-aluminum slag; (2) wrapping the graphite slag obtained in step (1) with wet clay into an inner core material, then mixing a small amount of wet clay with the iron-aluminum slag and then wrapping the inner core material to form a globularity, and aging at 25°C for 12 hours to obtain a blank, wherein a mass ratio of the sum of the iron-aluminum slag to the graphite slag and the wet clay used in the inner and outer layers was 6: 3: 1, and the wet clay was obtained by mixing clay and a potassium carbonate solution; a mass ratio of the clay to the potassium carbonate solution was 55: 45, and the potassium carbonate solution was prepared by potassium carbonate and water, wherein a mass ratio of the potassium carbonate to the water was 5: 40; (3) calcining the blank prepared in step (3) in a muffle furnace, pre-sintering at 500°C for 3 hours, then heating to l,100°C for 3 hours at a heating rate of 5°C / min, and cooling with the furnace to obtain a sintered product; and (4) washing the sintered product with IM hydrochloric acid solution first and then with distilled water, and drying at 80°C for 6 hours to obtain the refractory materials. Refractory materials prepared by the preparation method above. An application of the refractory materials above in packaging, transportation and storage of a waste battery. Embodiment 5: A method for preparing refractory materials with waste battery residues comprises the following steps of (1) dismantling a waste battery with a dismantling machine, then pyrolyzing, crushing and mechanically sorting to obtain positive and negative powders, performing acid leaching on the positive and negative powders with a sulfuric acid, and filtering to obtain a graphite slag, then adding iron to a filtrate to remove copper, and then adding sodium hydroxide, sodium carbonate and sodium chlorate for a precipitation reaction to obtain an iron-aluminum slag; (2) wrapping the graphite slag obtained in step (1) with wet clay into an inner core material, then mixing a small amount of wet clay with the iron-aluminum slag and then wrapping the inner core material to form a globularity, and aging at 25°C for 12 hours to obtain a blank, wherein a mass ratio of the sum of the iron-aluminum slag to the graphite slag and the wet clay used in the inner and outer layers was 7: 2: 1, and the wet clay was obtained by mixing clay and a potassium carbonate solution; a mass ratio of the clay to the potassium carbonate solution was 79: 21, and the potassium carbonate solution was prepared by potassium carbonate and water, wherein a mass ratio of the potassium carbonate to the water was 1: 20; (3) calcining the blank prepared in step (3) in a muffle furnace, pre-sintering at 300°C for 1 hour, then heating to 900°C for 1 hour at a heating rate of 5°C / min, and cooling with the furnace to obtain a sintered product; and (4) washing the sintered product with IM hydrochloric acid solution first and then with distilled water, and drying at 80°C for 6 hours to obtain the refractory materials. Refractory materials prepared by the preparation method above. An application of the refractory materials above in packaging, transportation and storage of a waste battery. Embodiment 6: A method for preparing refractory materials with waste battery residues comprises the foilowing steps of: (1) dismantling a waste battery with a dismantling machine, then pyrolyzing, crushing and mechanically sorting to obtain positive and negative powders, performing acid leaching on the positive and negative powders with a sulfuric acid, and filtering to obtain a graphite slag, then adding iron to a filtrate to remove copper, and then adding sodium hydroxide, sodium carbonate and sodium chlorate for a precipitation reaction to obtain an iron-aluminum slag; (2) wrapping the graphite slag obtained in step (1) with wet clay into an inner core material, then mixing a small amount of wet clay with the iron-aluminum slag and then wrapping the inner core material to form a globularity, and aging at 25°C for 12 hours to obtain a blank, wherein a mass ratio of the sum of the iron-aluminum slag to the graphite slag and the wet clay used in the inner and outer layers was 7: 2: 1, and the wet clay was obtained by mixing clay and a potassium carbonate solution; a mass ratio of the clay to the potassium carbonate solution was 55: 45, and the potassium carbonate solution was prepared by potassium carbonate and water, wherein a mass ratio of the potassium carbonate to the water was 5: 40; (3) calcining the blank prepared in step (3) in a muffle furnace, pre-sintering at 500°C for 3 hours, then heating to l,100°C for 3 hours at a heating rate of 5°C / min, and cooling with the furnace to obtain a sintered product; and (4) washing the sintered product with IM hydrochloric acid solution first and then with distilled water, and drying at 80°C for 6 hours to obtain the refractory materials. Refractory materials prepared by the preparation method above. An application of the refractory materials above in packaging, transportation and storage of a waste battery. Comparative Example 1: A method for preparing refractory materials with waste battery residues comprises the following steps of: (1) dismantling a waste battery with a dismantling machine, then pyrolyzing, crushing and mechanically sorting to obtain positive and negative powders, performing acid leaching on the positive and negative powders with a sulfuric acid, and filtering to obtain a graphite slag, then adding iron to a filtrate to remove copper, and then adding sodium hydroxide, sodium carbonate and sodium chlorate for a precipitation reaction to obtain an iron-aluminum slag; (2) wrapping the graphite slag obtained in step (1) with wet clay into an inner core material, then mixing a small amount of wet clay with the iron-aluminum slag and then wrapping the inner core material to form a globularity, and aging at 25°C for 12 hours to obtain a blank, wherein a mass ratio of the sum of the iron-aluminum slag to the graphite slag and the wet clay used in the inner and outer layers was 5: 4: 1, and the wet clay was obtained by mixing clay and distilled water; a mass ratio of the clay to the distilled water was 79: 21; (3) calcining the blank prepared in step (3) in a muffle furnace, pre-sintering at 300°C for 1 hour, then heating to 900°C for 1 hour at a heating rate of 5°C / min, and cooling with the furnace to obtain a sintered product; and (4) washing the sintered product with IM hydrochloric acid solution first and then with distilled water, and drying at 80°C for 6 hours to obtain the refractory materials. Refractory materials prepared by the preparation method above. Experimental Example: 1. Morphologies of the refractories of Embodiment 1 and Comparative Example 1 were observed by a scanning electron microscope. The results were shown in FIG. 1 and FIG. 6. Comparing FIG. 1 with FIG. 6, it could be seen that the interior of the refractory materials of Embodiment 1 had multi-layer structure and were more loose and porous in comparison to Comparative Example 1. The porous structure of the refractory materials of Embodiment 1 were tested by an automatic specific surface area analyzer and inductively coupled plasma emission spectrometer, and the results were shown in FIG. 2. The refractory materials of Embodiment 1 were subjected to a heat resistance test by a synchronous integrated thermal analyzer, and the results were shown in FIG. 3. Appropriate amounts of refractories of Embodiments 1, 3 and 5 and Comparative Example 1 were taken respectively. The refractories were soaked in an organic electrolyte of a lithium ion battery for 5 minutes, and then the electrolyte absorption was calculated by the following formula, P = mi m° X 100%, where P(%) was an absorption rate of the refractory m0 materials; mo and mi(g) were masses of the refractories before and after adsorption respectively. The results were shown in FIG. 4. For recycling the refractory materials of Embodiment 3 after absorbing the electrolyte, the refractory materials of Embodiment 3 were first sintered at 500°C for 2 hours, then washed with IM hydrochloric acid for 3 times, then washed with water until neutrality, then put in the lithium ion electrolyte again and soaked for 5 minutes, and then the absorption rate was calculated. The experiment was repeated for 6 times. The results were shown in FIG. 5. 2. An inductively coupled plasma emission spectrometer was used to test metal contents in the refractory materials prepared in Embodiment 1 and the iron-aluminum slag obtained in step (1) of Embodiment 1 respectively. The results were shown in Table 1. Table 1 Metallic element contents of refractory Sample Ni Co Al Fe Ca Cu mg / L Iron-aluminum slag 0.01 0.01 1.44 0.08 2.58 0.02 Embodiment 1 0.005 0.005 0.86 0.05 2.58 0.006 26 06 24 It can be seen from FIG. 2 that the isothermal adsorption-desorption curve of the refractory 5 materials of the present disclosure shows obvious hysteresis loop, which indicates that the refractory materials of Embodiment 1 are mainly mesoporous material, and the adsorbed volume of Embodiment 1 is 125 cm3 / g STP when P / Po is less than 0.01, that is, the refractory materials have more micropores, which indicates that the refractory materials have excellent adsorption capacity, i.e., good moisture absorption capacity. It can be seen from FIG. 3 that the refractory materials of the present disclosure has strong high-temperature resistance, and a TG curve shows that when the temperature is less than 200°C, a weight of the refractory materials decreases by 5.8%, and a water volatilization reaction occurs at this stage. The weight of the refractory materials does not change between 200°C and 800°C, which indicates that the refractory materials have excellent high-temperature resistance. 15 It can be seen from FIG. 4 that the refractory materials of the present disclosure have excellent adsorption capacity for the organic electrolyte of the lithium ion battery, and meanwhile, it can be seen by comparing Embodiment 1 with Comparative Example 1 that when potassium carbonate is used in the preparation process of the refractory materials of the present disclosure, the final refractory has better adsorption capacity for the organic electrolyte of the lithium ion battery. 20 It can be seen from FIG. 5 that when the refractory materials of the present disclosure are used repeatedly, the absorption rate thereof to the organic electrolyte of the lithium ion battery remains unchanged, so the refractory materials of the present disclosure can be reused and the cost can be effectively controlled. It can be seen from Table 1 that the refractory materials of Embodiment 1 of the present 25 disclosure have a lower heavy metal content in comparison to the iron-aluminum slag, which indicates that the transition metal content of the refractory materials can be effectively reduced through simple process treatment, which meets the requirements of national standards, is nontoxic, 26 06 24 harmless and pollution-free, and achieves the effect of being harmless to the environment.

Claims

1. A method for preparing refractory materials with waste lithium ion battery residues, comprising the following steps of:(1) dismantling a waste lithium ion battery and sorting to obtain a mixture of positive and negative electrode powders, performing acid leaching on the mixture of positive and negative powders, filtering to obtain a graphite slag, then removing copper from a filtrate by adding iron, and adding an alkali for a precipitation reaction to obtain an iron-aluminum slag;(2) wrapping the graphite slag obtained in step (1) with wet clay into an inner core material, mixing further wet clay with the iron-aluminum slag and then wrapping the inner core material, and aging to obtain a blank;(3) pre-sintering, calcining and cooling the blank prepared in step (2) to obtain a sintered product; and(4) washing and drying the sintered product to obtain the refractory materials; wherein the wet clay in step (2) is prepared by mixing clay with a potassium carbonate solution; wherein a mass ratio of the clay to the potassium carbonate solution in the wet clay is (55 to 79): (21 to 45).

2. The method for preparing the refractory materials with waste lithium ion battery residues according to claim 1, wherein the potassium carbonate solution is prepared by potassium carbonate and water, wherein a mass ratio of the potassium carbonate to the water is (1 to 5): (20 to 40).

3. The method for preparing the refractory materials with waste battery lithium ion residues according to claim 1, wherein in step (2), a mass ratio of the iron-aluminum slag to the graphite slag and the wet clay is (5 to 7): (2 to 4): 1.

4. The method for preparing the refractory materials with waste lithium ion battery residues according to claim 1, wherein in step (2), the aging is performed at a temperature of 25°C to 35°C, and lasts for 12 hours to 36 hours.

5. The method for preparing the refractory materials with waste lithium ion battery residues according to claim 1, wherein in step (3), the pre-sintering is performed at a temperature of 300°C to 500°C, and lasts for 1 hour to 3 hours.

6. The method for preparing the refractory materials with waste lithium ion battery residues according to claim 7, wherein in step (3), the calcining is performed at a temperature of 900°C to l,100°C and lasts for 1 hour to 3 hours, and a heating rate from pre-sintering to calcining is 3°C / min to 10°C / min

Citation Information

Patent Citations

  • Method for preparing super-porous carbon material through persimmon fruit peels

    CN105174255A

  • Recycling method for valuable metal from waste nickel-cobalt-manganese lithium ion battery

    CN107653378A

  • Method and device of using image patches to track measured deviation, and storage medium

    CN108470351A

  • Ceramic brick and preparation method and application thereof

    CN109665812A

  • Lightweight and environmentally-friendly ceramsite, and preparation method and application thereof

    CN110655385A