Multilayer wiring board manufacturing method
Patent Information
- Application Number
- JP2022074110
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2022-04-28
- Publication Date
- 2024-11-06
- Estimated Expiration
- 2041-11-30
AI Technical Summary
Existing methods for manufacturing multilayer wiring boards with glass substrates face challenges in controlling the modification depth of laser-modified portions, leading to variations in through-hole diameters and potential damage during the manufacturing process.
A method involving the use of supports bonded to glass substrates with laser irradiation to form modified portions, followed by etching, ensuring uniform formation of through holes with high precision.
The method enables precise and uniform formation of through holes by uniformly forming modified portions on both the core material and support, allowing for accurate etching and improved manufacturing consistency.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a method for manufacturing a multilayer wiring board.
Background Art
[0002] In recent years, as electronic devices become more highly functional and miniaturized, there has been a growing demand for higher precision in multilayer wiring boards typified by interposers mounted on electronic devices. In particular, in recent multilayer wiring boards, a glass substrate is adopted, through holes are formed in the glass substrate, and through electrodes are provided. Then, a multilayer wiring board in which conductor layers, insulating resin layers, and conductor layers are sequentially laminated on both sides of the glass substrate is adopted. However, when the glass thickness of the glass substrate reaches about 100 μm, it is easy for obstacles such as cracks to occur in the glass substrate during the manufacturing process of the multilayer wiring board.
[0003] Therefore, in Patent Document 1, in order to prevent such cracks, a process of adhering a support to the glass substrate via a release layer and peeling off and removing the support after forming the wiring is adopted. Specifically, a process of forming a first wiring on the first surface of a glass substrate, a process of supporting the first wiring side of the glass substrate on which the first wiring is formed with a support, a process of forming a laser modification part serving as a starting point for through hole formation on the glass substrate with a laser irradiated from the surface opposite to the first surface, a through hole formation process of performing etching using a hydrofluoric acid etching solution from the surface opposite to the first surface of the glass substrate toward the first surface to thin the glass substrate while forming through holes, after the through hole formation process, forming a through electrode inside the through holes and forming a second wiring on the surface opposite to the first surface of the glass substrate to connect the first wiring and the second wiring via the through electrode, and a process of removing the support from the glass substrate after forming the second wiring are adopted.
Prior Art Documents
Patent Documents
[0004] [Patent Document 1] International Publication No. 2019 / 235617 [Overview of the project] [Problems that the invention aims to solve]
[0005] However, while it is possible to form a laser-modified area on a glass substrate by laser irradiation, controlling the modification depth is difficult when forming a modified layer partially within the glass substrate. As a result, variations in the depth of the modified area may occur. As a result, variations in the diameter of through-holes may occur during the formation of through-holes by etching.
[0006] The present invention has been made in view of the above problems, and aims to provide a technique for forming through holes with high precision in a method for manufacturing a multilayer wiring board, in which a laser-modified portion is formed in the core material of the multilayer wiring board, and then through holes are formed by etching. [Means for solving the problem]
[0007] One of the representative methods for manufacturing a glass multilayer wiring substrate of the present invention is: In a method for manufacturing multilayer wiring in which through holes are formed in a glass substrate having a first surface and a second surface, A first step of bonding a support to the second surface of the glass substrate, A second step involves forming modified areas on both the glass substrate and the support by laser irradiation. A third step of peeling off the support. A fourth step involves forming through holes in the glass substrate by etching. It has. [Effects of the Invention]
[0008] According to the present invention, by forming modified portions on both the core material and the first support, modified portions can be uniformly formed on the glass substrate. Subsequently, by performing an etching process, through holes can be formed with high precision. Issues, structures, and effects other than those mentioned above will be clarified by the following explanation of the implementation methods. [Brief explanation of the drawing]
[0009] [Figure 1] Figure 1 is a cross-sectional view illustrating the process of bonding the first support to the glass substrate. [Figure 2] Figure 2 is a cross-sectional view illustrating the laser modification process. [Figure 3] Figure 3 is a cross-sectional view illustrating the process of forming the first wiring layer. [Figure 4] Figure 4 is a cross-sectional view illustrating the bonding process of the second support. [Figure 5] Figure 5 is a cross-sectional view illustrating the peeling process of the first support. [Figure 6] Figure 6 is a cross-sectional view illustrating the process of forming through holes by etching. [Figure 7] Figure 7 is a cross-sectional view illustrating the process of forming the second wiring layer. [Figure 8] Figure 8 is a cross-sectional view illustrating the peeling process of the second support. [Figure 9] Figure 9 is a cross-sectional view of a glass substrate with wiring layers formed on both sides. [Figure 10] Figure 10 is a cross-sectional view illustrating the build-up layer formation process. [Figure 11] Figure 11 is a completed cross-sectional view of a multilayer wiring board. [Figure 12] Figure 12 is a cross-sectional view illustrating the wiring layer formation process in the second embodiment. [Figure 13] Figure 13 is a cross-sectional view illustrating the laser modification process in the second embodiment. [Figure 14] Figure 14 is a cross-sectional view illustrating the bonding process of the second support in the third embodiment. [Figure 15] Figure 15 is a cross-sectional view illustrating the laser modification process in the third embodiment. [Figure 16] FIG. 16 is a cross-sectional view of a multilayer wiring board manufactured according to the first to third embodiments. [Figure 17] FIG. 17 is a cross-sectional view of a multilayer wiring board manufactured according to the first to third embodiments. [Figure 18] FIG. 18 is a cross-sectional view for explaining the shape of a through-hole manufactured according to the first to third embodiments. [Figure 19] FIG. 19 is a cross-sectional view of a glass multilayer wiring board for a passive component incorporating a capacitor structure. [Figure 20] FIG. 20 is a cross-sectional view of a structure in which an interposer having a plurality of semiconductor elements mounted thereon is mounted on a BGA substrate.
MODE FOR CARRYING OUT THE INVENTION
[0010] Hereinafter, embodiments of the present invention will be described with reference to the drawings. The following description relates to an example of the present invention, and the present invention is not limited thereto. Also, in the description of the drawings, the same reference numerals are used for the same parts. In the drawings, the positions, sizes, shapes, ranges, etc. of the respective components shown may not represent the actual positions, sizes, shapes, ranges, etc. in order to facilitate understanding of the invention. Therefore, the present invention is not necessarily limited to the positions, sizes, shapes, ranges, etc. disclosed in the drawings.
[0011] In the present disclosure, the term "surface" may refer not only to the surface of a plate-like member but also to the interface of a layer substantially parallel to the surface of the plate-like member in the layers included in the plate-like member. Also, the "upper surface" and "lower surface" mean the surfaces shown above or below in the drawing when the plate-like member or the layers included in the plate-like member are illustrated. The "upper surface" and "lower surface" may also be referred to as the "first surface" and "second surface".
[0012] The "side surface" means the surface or the thickness portion of the layer in the plate-like member or the layers included in the plate-like member. Further, a part of the surface and the side surface may be collectively referred to as an "end portion". Furthermore, "upward" refers to the vertically upward direction when a plate-like member or layer is placed horizontally. In addition, "upward" and its opposite, "downward," may be referred to as the "positive Z-axis direction" and the "negative Z-axis direction," respectively, while the horizontal direction may be referred to as the "X-axis direction" and the "Y-axis direction."
[0013] Furthermore, "planar shape" and "planar view" refer to the shape of a surface or layer as viewed from above. In addition, "cross-sectional shape" and "cross-sectional view" refer to the shape of a plate-like member or layer as viewed from the horizontal when it is cut in a specific direction. Furthermore, "center" refers to the central part of a surface or layer, not its periphery. And "center direction" refers to the direction from the periphery of a surface or layer toward the center of the planar shape of the surface or layer.
[0014] <First Embodiment> The method for manufacturing a multilayer wiring layer in the first embodiment will be described below with reference to Figures 1 to 11. (Adhesion of the first support) First, with reference to Figure 1, the process of bonding the first support 61 to the glass substrate 60 will be explained. As shown in Figure 1, the first adhesive layer 62 is used to bond the first support 61 to the glass substrate 60, forming a laminated structure 63 consisting of the glass substrate 60, the first adhesive layer 62, and the first support 61.
[0015] The aforementioned first adhesive layer 62 for temporary fixing is an adhesive layer for temporarily fixing the first support 61 to the glass substrate 60. For this reason, the material of the first adhesive layer 62 can be appropriately selected from resins that can be peeled off by absorbing light such as UV light, generating heat, sublimation, or altering, resins that can be peeled off by foaming due to heat, or functional groups, etc. To bond the first support to the glass substrate 60, for example, a laminator, a vacuum pressure press, a reduced pressure bonding machine, etc., can be used.
[0016] The first support 61 is preferably made of the same material as the glass substrate 60. If the glass substrate 60 is alkali-free glass, it is preferable that the first support 61 is also alkali-free glass. The thickness of the first support can be set appropriately according to the thickness of the glass substrate 60. However, it is preferable that the thickness be such that it can be transported during the manufacturing process, and the range is 300 to 1,500 μm.
[0017] (Formation of laser-modified area) Next, the process of forming the laser-modified portion will be described with reference to Figure 2. As shown in Figure 2, a laser is irradiated onto the laminated structure 63 to form a laser-modified portion 65 that serves as the starting point for the through-hole. The laser-modified portion 65 extends, for example, perpendicularly to the glass substrate 60 and can be formed over almost the entire surface of the glass substrate 60. In this case, the laser-modified portion 65 may also be formed on the first adhesive layer 62 and the first support 61. In this embodiment, by irradiating the glass substrate 60 with the first support 61 stacked on top of it with a laser, it becomes possible to widen the laser irradiation processing conditions (process window) and to reliably form the desired laser-modified portion on the glass substrate 60.
[0018] (Formation of the first wiring layer) Next, the process for forming the first wiring layer 21 will be described with reference to Figure 3. As shown in Figure 3, the first wiring layer 21, consisting of a conductive layer and an insulating resin layer, is formed on the first surface 20, which is the upper surface on the glass substrate 60 of the laminated structure 63. At this time, a seed layer containing a hydrofluoric acid-resistant metal layer 15 is formed on the glass substrate 60, then through-electrode connection parts 41 and wiring 16 between through-electrodes are formed on the first surface 20 using the semi-additive (SAP) method, and after removing the unnecessary seed layer, the insulating resin layer 25 is formed.
[0019] The hydrofluoric acid-resistant metal layer 15 on the glass substrate 60 is an alloy layer consisting of chromium, nickel, or both, and can be formed in the range of 10 to 1,000 nm by sputtering. Subsequently, a conductive metal film is formed on the hydrofluoric acid-resistant metal to a desired thickness. The conductive metal film can be appropriately selected from, for example, Cu, Ni, Al, Ti, Cr, Mo, W, Ta, Au, Ir, Ru, Pd, Pt, AlSi, AlSiCu, AlCu, NiFe, ITO, IZO, AZO, ZnO, PZT, TiN, and Cu3N4.
[0020] For the formation of the first wiring layer using the semi-additive method, a photoresist can be used to form the desired pattern. Generally, a dry film resist is used, but a liquid resist may also be used. After exposing and developing the desired pattern to form the pattern, a plating film of 2 μm to 20 μm in thickness can be formed by electroplating. The unnecessary resist pattern is then removed, and the seed layer is etched to form the wiring.
[0021] The insulating resin layer 25 is a material containing at least one of the following: epoxy resin, polyimide resin, or polyamide resin, and containing fillers such as silica, titanium dioxide, or urethane. It is preferably a liquid or film-like material. In the case of liquid resin, it can be formed by spin coating, and in the case of film-like resin, it can be formed by heating and pressurizing under vacuum using a vacuum laminator. The material of the insulating resin layer 25 can be appropriately selected as needed.
[0022] (Adhesion of the second support) Next, the bonding process for the second support will be described with reference to Figure 4. As shown in Figure 4, the second adhesive layer 71 and the second support 70 are formed on the first wiring layer 21 of the laminated structure 63.
[0023] The second adhesive layer 71 can be appropriately selected from a resin that absorbs light such as UV light and becomes peelable by generating heat, sublimation, or alteration, a resin that becomes peelable by foaming due to heat, or functional groups that temporarily fix the glass substrate 60 and the first support 61, similar to the first adhesive layer 62, but it is desirable that it be made of a different material from the first adhesive layer 62.
[0024] The second support 70 is made of glass, and preferably of the same material as the glass substrate 60. If the glass substrate 60 is alkali-free glass, it is desirable that the first support 61 is also alkali-free glass. The thickness of the second support can be set appropriately according to the thickness of the glass substrate 60. However, it is preferable that the thickness be transportable, and the range is 300 to 1,500 μm.
[0025] (Peeling of the first support) Next, the peeling process of the first support will be described with reference to Figure 5. As shown in Figure 5, the first adhesive layer 62 and the first support 61 are peeled off from the interface between the glass substrate 60 and the first adhesive layer 62.
[0026] When peeling the first support 61 from the interface between the glass substrate 60 and the first adhesive layer 62, an appropriate peeling method will be selected from UV light irradiation, heat treatment, physical peeling, etc., depending on the material used for the first adhesive layer. Furthermore, if residual material of the first adhesive layer 62 remains at the bonding surface between the glass substrate 60 and the first adhesive layer 62, plasma cleaning, ultrasonic cleaning, water washing, or solvent cleaning using alcohol may be performed.
[0027] (Through-hole formation by etching) Next, the process of forming through holes by etching will be described with reference to Figure 6. As shown in Figure 6, the laser-modified portion 65 of the glass substrate 60 is selectively removed by etching, and through holes 12 are formed from the lower surface in the figure. Wet etching using an aqueous hydrofluoric acid solution is suitable for this process. The amount of etching with the aqueous hydrofluoric acid solution will be set appropriately according to the thickness of the glass multilayer wiring substrate. For example, if the thickness T1 of the glass substrate 60 is 200 μm, it is desirable that the etching amount be in the range of 50 μm or more and 175 μm or less. The thickness T2 of the glass substrate 60 after etching is preferably 25 μm or more and 150 μm or less.
[0028] (Formation of the second wiring layer) Next, the process of forming the second wiring layer will be described with reference to Figure 7. As shown in Figure 7, a second wiring layer 22 consisting of a conductive layer and an insulating resin layer is formed on the second surface 30 below the glass substrate 60. For the formation of the through-hole 12 and the second wiring layer on the second surface side of the glass substrate 60, a seed layer for power supply is formed, a pattern is formed with resist, a plating treatment of 2 μm or more and 20 μm or less is performed, the unnecessary resist pattern is peeled off, the seed layer is removed, and the insulating resin is formed. In the second wiring layer 22, since there is no etching treatment with hydrofluoric acid aqueous solution in subsequent processes, a material different from the hydrofluoric acid-resistant metal can be used. In this case, a metal layer made of a material different from the hydrofluoric acid-resistant metal is formed on the side surface of the through hole 12. Examples of materials different from the hydrofluoric acid-resistant metal include Ti and Cu, and at least one metal layer made of these materials is formed on the side surface of the through hole 12 and on the second surface 30 of the glass substrate 60. The materials, number of layers, etc., are not limited to those described herein and can be set as appropriate as needed.
[0029] (Detachment of the second support) Next, the peeling process of the second support will be described with reference to Figure 8. As shown in Figure 8, the second adhesive layer 71 and the second support 70, which are formed above the first wiring layer 21 on the first surface 20 side of the glass substrate 60, are peeled off from the interface between the first wiring layer 21 and the second adhesive layer 71 on the first surface side. As a result, as shown in Figure 9, a glass substrate 60 is obtained in which the first wiring layer 21 is formed on the first surface 20 side and the second wiring layer 22 is formed on the second surface 30 side. When peeling the second support 70 from the second wiring layer 22, an appropriate peeling method can be selected from UV light irradiation, heat treatment, physical peeling, etc., depending on the material used for the second adhesive layer 71. Furthermore, if residual material of the second adhesive layer 71 remains at the joint surface between the first wiring layer 21 and the second adhesive layer 71, plasma cleaning, ultrasonic cleaning, water washing, solvent cleaning using alcohol, etc., may be performed.
[0030] (Formation of the build-up layer) Next, the process of forming the build-up layer will be explained with reference to Figure 10. As shown in Figure 10, a conductive electrode 31 for connecting the first wiring layer on the first surface 20 and a conductive electrode 32 for connecting the second wiring layer on the second surface 30 are formed on the first wiring layer 21 on the first surface 20 and the second wiring layer 22 on the second surface 30 of the glass substrate 60. The conductive electrodes 31 and 32 are formed by first forming vias in the insulating resin layer 25 with a laser, then forming a seed layer on the vias, and then using a semi-additive process (resist pattern formation, plating, resist stripping, seed layer removal, insulating resin layer 25). Furthermore, the first wiring layer 21 and the second wiring layer 22 are stacked in layers of at least one, and the number of layers can be set as appropriate if necessary.
[0031] The laser used to form the conductive electrodes 31 and 32 is different from the laser used to form the laser-modified portion 65. For example, it is preferable to use a pulsed laser such as a carbon dioxide laser or a UV-YAG laser, and a laser with a pulse width of μs is suitable.
[0032] Next, as shown in Figure 11, after forming an outer protective film such as solder resist 55 on the first wiring layer 21 and the second wiring layer 22, surface treatments such as Ni / Au, Ni / Pd / Au, IT, OSP (water-soluble preflux) are applied to the semiconductor element bonding pad 51 and the substrate bonding pad 53, and solder 52 for semiconductor element bonding and solder 54 for substrate bonding are formed as needed to complete the multilayer wiring board.
[0033] <Second Embodiment> Next, a second embodiment will be described with reference to Figures 1, 12, 13, 4 through 11. The second embodiment differs from the first embodiment in that the laser modification process is performed after the formation of the first wiring layer. In the following description, components identical or equivalent to those in the first embodiment described above will be denoted by the same reference numerals, and their descriptions will be simplified or omitted.
[0034] (Adhesion of the first support) In the method for manufacturing a multilayer wiring board according to the second embodiment, the first step, the bonding step of the first support, is the same as that of the first embodiment described with reference to Figure 1, so its description will be omitted.
[0035] (Formation of the first wiring layer) Next, with reference to Figure 12, the process for forming the wiring layer in the second embodiment will be described.
[0036] In the second embodiment, as shown in Figure 12, following the bonding step of the first support, the first wiring layer 21 is formed on the glass substrate 60 of the laminated structure 63. At this time, a seed layer containing a hydrofluoric acid-resistant metal layer 15 is formed on the glass substrate 60, then the through-electrode connection portion 41 and the wiring 16 between the through-electrodes are formed using the semi-additive (SAP) method, the unnecessary seed layer is removed, and then the insulating resin layer 25 is formed. The materials and film formation methods for the hydrofluoric acid-resistant metal layer and the conductive metal film are the same as in the first embodiment.
[0037] (Formation of laser-modified area) Next, with reference to Figure 13, the process for forming the laser-modified portion in the second embodiment will be described. As shown in Figure 13, a laser is irradiated onto the laminated structure 63 from the surface of the first support 61 to form a laser-modified portion 65 that serves as the starting point for the through-hole. The laser-modified portion 65 extends, for example, perpendicularly to the glass substrate 60 and is formed over the entire surface. At this time, the laser-modified portion 65 may be formed on the first adhesive layer 62 and the first support 61.
[0038] (Process after bonding the second support) In the second embodiment, the steps from the bonding step of the second support onward—peeling of the first support, formation of through holes by etching, formation of the second wiring layer, peeling of the second support, and formation of the build-up layer—are the same as in the first embodiment described with reference to Figures 4 to 11, so a detailed explanation is omitted.
[0039] <Third Embodiment> Next, a third embodiment will be described with reference to Figures 1, 12, 14, 15, and 5 through 11. The third embodiment differs from the second embodiment in that the laser modification process is performed after the bonding process of the second support. In the following description, components that are the same as or equivalent to those in the first and second embodiments described above will be denoted by the same reference numerals, and their descriptions will be simplified or omitted.
[0040] (Adhesion of the first support and formation of the first wiring layer) In the method for manufacturing a glass multilayer wiring substrate according to the third embodiment, the first steps, the bonding step of the first support and the formation step of the first wiring layer, are the same as those described in the second embodiment with reference to Figures 1 and 12, so their description will be omitted.
[0041] (Adhesion of the second support) Next, with reference to Figure 14, the bonding process of the second support in the third embodiment will be described. In the third embodiment, as shown in Figure 14, a second adhesive layer 71 and a second support 70 are formed on the first wiring layer 21 of the laminated structure 63.
[0042] (Formation of laser-modified area) Subsequently, as shown in Figure 15, a laser is irradiated onto the laminated structure 63 to form laser-modified portions 65 that serve as the starting points for through-holes. The laser-modified portions 65 extend, for example, perpendicularly to the glass substrate 60 and are formed over the entire surface. At this time, the laser-modified portions 65 may also be formed on the first adhesive layer 62 and the first support 61.
[0043] (Process after peeling off the first support) In the third embodiment, the processes from the first support peeling step onward—through-hole formation by etching, formation of the second wiring layer, peeling of the second support, and formation of the build-up layer—are the same as in the first embodiment described with reference to Figures 5 to 11, so a detailed explanation is omitted.
[0044] <Effects and Actions> According to the manufacturing method described in the first to third embodiments above, when forming the laser-modified portion, the laser irradiation target is not only the glass substrate 60, but also the support made of the same material as the glass substrate 60 at the same time. Therefore, the laser-modified portion can be reliably formed along the entire thickness direction (z-axis direction) of the glass substrate 60. In other words, the end portions of the laser modification, where laser modification may not be sufficiently performed, are located within the support. Such unstable laser-modified portions are then peeled off along with the support in a later process. As a result, the laser-modified portion formed on the glass substrate 60 is highly homogeneous and formed with high precision, making it possible to uniformly form through-holes even after subsequent etching. Conventionally, since only the glass substrate 60 was targeted for laser irradiation, the laser-modified areas were not always formed uniformly near the surface of the glass substrate, resulting in variations in the shape of the through-holes. However, the multilayer wiring formation method of this disclosure can significantly improve this issue.
[0045] <Regarding a glass multilayer wiring board according to an embodiment of the present invention> The structure of the multilayer wiring board manufactured according to the first, second, and third embodiments will be explained with reference to Figures 16, 17, and 18. In the multilayer wiring boards manufactured according to the first to third embodiments of the present invention, as shown in Figures 16, 17, and 18, the first wiring layer 21 on the first surface 20 side and the second wiring layer 22 on the second surface 30 side are electrically connected to the glass substrate 60 by a frustoconical through-electrode 11.
[0046] The first wiring layer 21 and the through electrode 11 on the first surface 20 side are sealed by the through electrode connection portion 41 of the first wiring layer 21 on the first surface 20 side, and the through electrode connection portion 41 and the through electrode 11 are sandwiched between the hydrofluoric acid-resistant metal layer 15.
[0047] The conductive electrode 31 connecting the first wiring layer 21 on the first surface 20 side is formed on the through-electrode connection portion 41 of the first wiring layer on the first surface 20 side. The conductive electrode 32 connecting the second wiring layer 22 on the second surface 30 side is formed at a position away from the through-electrode 11. The conductive electrode 31 connecting the first wiring layer 21 on the first surface 20 side can be formed on the through-electrode 11 by forming a through-hole 12 by etching after forming the first wiring layer 21 on the first surface 20 side on the glass substrate 60, and in the first wiring layer on the first surface side, it is possible to form wiring 16 between the through-electrodes 11. In the first wiring layer on the first surface side, the degree of freedom in wiring design is improved compared to the second wiring layer 22 on the second surface side.
[0048] Furthermore, according to the present invention, the opening diameter D2 of the second wiring layer 22 on the second surface 30 can be stably formed, and problems such as the opening diameter D2 being blocked can be suppressed. For this reason, as shown in Figure 18, the relationship between the opening diameter D1 of the first wiring layer 21 on the first surface 20 of the glass substrate 60 and the opening diameter D2 of the second wiring layer 22 on the second surface 30 is D2 > D1, and the opening diameter D1 on the first surface 20 side / opening D2 on the second surface side becomes approximately 0.3 to 0.8, which ensures that the seed layer adheres to the sides and bottom of the through electrode 11. This ensures good adhesion between the sides and bottom of the through electrode 11, and high bonding reliability can be obtained.
[0049] The manufacturing method for glass multilayer wiring boards using thin glass with a thickness of 150 μm or less, as described above, can be used for devices such as glass multilayer wiring boards for passive components incorporating a capacitor structure as shown in Figure 19, and interposers equipped with multiple semiconductor elements as shown in Figure 20. This embodiment facilitates the use of thin glass with a thickness of 150 μm or less and enables the simple formation of through-holes and through-electrodes, making it applicable to various devices using glass multilayer wiring boards equipped with through-electrodes.
[0050] The scope of the present invention is not limited to the illustrative embodiments shown and described, but includes various modifications. For example, the embodiments described above are described in detail for the purpose of illustrating the present invention and are not necessarily limited to those having all the configurations described. Furthermore, it is possible to replace parts of the configuration of one embodiment with the configuration of another embodiment, and it is also possible to add configurations from other embodiments to the configuration of one embodiment. In addition, it is possible to add, delete, or replace parts of the configuration of each embodiment with other configurations. Furthermore, this invention also includes all embodiments that produce effects equivalent to those targeted by the present invention. [Explanation of symbols]
[0051] 1: Glass multilayer wiring board 11:Through electrode 12: Through hole 15: Hydrofluoric acid-resistant metal layer 16: Wiring 21: 1st wiring layer 22: 2nd wiring layer 25: Insulating resin layer 31: Conduction electrode 32: Conduction electrode 41: Through electrode connection 42: Through electrode connection 51: Bonding pads for semiconductor devices 52: Solder for semiconductor device bonding 53: Bonding pads for circuit boards 54: Solder for PCB bonding 55: Solder Resist 60: Glass substrate 61: First support 62: 1st adhesive layer 63: Laminated Structures 65: Laser modification section 70:Second support 71:Second adhesive layer 80: Capacitor structure 90: BGA board 100: Semiconductor devices D1: Through-hole first side opening diameter D2: Through-hole second side opening diameter
Claims
1. a first wiring layer is formed on a first surface of a glass substrate having a first surface and a second surface; A removable first support made of glass is adhered to the second surface, A multilayer wiring board in which modified portions are formed on both the glass substrate and the first support by laser irradiation, and through holes can be formed in the glass substrate by etching.
2. 2. The multilayer wiring board according to claim 1, A removable second support is attached above the first wiring layer. A multilayer wiring board comprising:
3. The multilayer wiring board according to claim 2, The first support is peeled off, and a modified portion by laser irradiation is exposed on the second surface of the glass substrate. A multilayer wiring board comprising:
4. The multilayer wiring board according to claim 3, Through holes are formed in the glass substrate by etching. A multilayer wiring board comprising:
5. The multilayer wiring board according to claim 4, a second wiring layer is provided on the second surface of the glass substrate; A portion of the second wiring layer is connected to a through electrode formed on a side surface of the through hole. A multilayer wiring board comprising:
6. The multilayer wiring board according to claim 5, 2. A multilayer wiring board, comprising: at least one of the second wiring layer and the through electrode, the second wiring layer and the through electrode being formed of a metal material different from a hydrofluoric acid resistant metal.
7. The multilayer wiring board according to claim 5 or 6, The second support is peeled off, and build-up layers can be formed above the first wiring layer and below the second wiring layer. A multilayer wiring board comprising: