Crystal pulling system having a fluid-filled exhaust tube extending through the housing
The fluid-cooled exhaust pipe in the crystal pulling system effectively prevents deposit formation by quenching exhaust gases, enhancing system uptime and throughput by transforming deposits into a powdery structure that does not adhere to the pipe walls.
Patent Information
- Application Number
- JP2023527033
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2020-11-04
- Filing Date
- 2021-11-04
- Publication Date
- 2024-11-06
- Estimated Expiration
- 2041-11-04
AI Technical Summary
Existing crystal pulling systems face issues with significant deposit formation on the exhaust system, leading to reduced operating time and increased processing costs due to the need for frequent system shutdowns to remove these deposits.
A crystal pulling system with a fluid-cooled exhaust pipe that extends into the reaction chamber, utilizing an inner and outer wall with a baffle to create a cooling fluid channel, rapidly quenching exhaust gases and preventing the formation of large deposits by changing their morphology to a powdery structure.
This design significantly extends the operating time of the crystal growth process by reducing deposit accumulation, allowing for increased uptime and throughput without the need for frequent system shutdowns.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
[Technical field]
[0001] (CROSS REFERENCE TO RELATED APPLICATIONS) This application claims the benefit of U.S. Provisional Patent Application No. 63 / 109,669, filed November 4, 2020, which is incorporated by reference in its entirety.
[0002] The field of the disclosure relates to crystal pulling systems for growing silicon ingots, and in particular to systems that include one or more exhaust tubes extending through a housing of the crystal pulling system for rapidly quenching exhaust gases. [Background technology]
[0003] Monocrystalline silicon ingots may be prepared by the so-called Czochralski process, in which a monocrystalline silicon seed is brought into contact with a silicon melt held in a crucible. The monocrystalline silicon seed is withdrawn from the melt to pull a monocrystalline silicon ingot from the melt. The ingots may be prepared in a batch system, in which a charge of polycrystalline silicon is first melted in a crucible, and the silicon ingot is withdrawn from the melt until the molten silicon in the crucible is depleted. Alternatively, the ingots may be withdrawn in a continuous Czochralski process, in which polysilicon is intermittently or continuously added to the melt to replenish the silicon melt during ingot growth.
[0004] Crystal pulling may be carried out in the presence of an atmosphere within the puller housing. In both batch and continuous Czochralski processes, a process gas inert to silicon, such as argon, is continuously introduced into the housing and drawn through the exhaust system of the puller. As the process gas is drawn off, compounds can deposit on the exhaust system tubing, which is at a low temperature compared to the puller chamber (e.g., arsenic oxide, silicon carbide, and silicon oxide compounds). Such deposits are removed from the system, which requires the puller to be taken out of operation, which can increase processing costs.
[0005] In the continuous Czochralski process, the crystal pulling system operates for longer periods of time, which causes larger and more obstructive deposits to form in the exhaust line, limiting the system's operating time.
[0006] What is needed is a crystal pulling system that is characterized by reduced deposit formation on the exhaust system of the puller.
[0007] This section is intended to introduce the reader to various aspects of art that may be related to various aspects of the present disclosure, which are described and / or claimed below. This discussion is believed to be helpful in providing the reader with background information to facilitate a better understanding of the various aspects of the present disclosure. As such, it should be understood that these statements are to be read in this light, and not as admissions of prior art. Summary of the Invention
[0008] One aspect of the present disclosure is directed to a crystal pulling system for growing a single crystal ingot from a silicon melt. The system includes a housing defining a growth chamber. The housing has a bottom and a sidewall extending from the bottom. A crucible is disposed within the growth chamber for containing the silicon melt. An exhaust tube extends outwardly through the bottom of the crucible. The exhaust tube defines an exhaust passage for exhausting exhaust gases from the growth chamber. The exhaust tube includes an inner wall, an outer wall, and a fluid passage defined between the inner wall and the outer wall for circulating a cooling fluid to cool the exhaust gases in the exhaust passage.
[0009] There are various refinements of the features described in relation to the above-mentioned aspects of the present disclosure. Further features may also be incorporated into the above-mentioned aspects of the present disclosure. These refinements and additional features may exist individually or in any combination. For example, the various features discussed below in relation to any of the illustrated embodiments of the present disclosure may be incorporated alone or in any combination into any of the above-mentioned aspects of the present disclosure. [Brief description of the drawings]
[0010] [Figure 1] FIG. 2 is a cross-sectional view of a growth chamber of a crystal pulling system. [Diagram 2] FIG. 2 is a detailed cross-sectional view of the crystal pulling system showing the exhaust tube. [Diagram 3] FIG. [Figure 4] FIG. 2 is a perspective view of the inner wall and baffle of the exhaust pipe. [Diagram 5] 1 is a photographic reproduction of an exhaust tube that was not fluid-cooled and did not extend into the reaction chamber of a crystal pulling system. [Figure 6] 1 is a photographic reproduction of a fluid-cooled exhaust tube extending into the reaction chamber of a crystal pulling system. [Figure 7] 1 is a graph of run times between a crystal pulling system that was not fluid-cooled and had an exhaust that did not extend into the reaction chamber, and a crystal pulling system that was fluid-cooled and had an exhaust that extended into the reaction chamber.
[0011] Corresponding reference characters indicate corresponding parts throughout the drawings. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] Referring to Figure 1, a crystal pulling system is shown generally at 10. Figure 1 shows a lower portion of the crystal pulling system 10 where exhaust gases are removed from the system 10. The system 10 includes an upper portion (not shown) that includes a pull chamber in which the crystal is pulled, and includes a pulling mechanism 47 for pulling an ingot 48 from a melt 46.
[0013] The crystal pulling system 10 is used to produce single crystal (i.e., monocrystalline) silicon ingots (e.g., semiconductor or solar grade material) by the Czochralski (CZ) process from a silicon melt 46. Although the illustrated crystal pulling system 10 is configured to grow ingots by the continuous CZ process, the systems and methods disclosed herein may also be used to grow single crystal ingots by the batch or recharge CZ process.
[0014] The illustrated crystal pulling system 10 includes a housing 12 defining a growth chamber 14 and an ingot pull chamber (not shown) connected to and disposed above the growth chamber 14. A graphite support or susceptor 18 is supported by a rotatable shaft 45 within the growth chamber 14. A crucible 44 containing a melt 46 of silicon (e.g., semiconductor or solar grade material) from which a single crystal ingot 48 is pulled by a pulling mechanism 47 is supported within the growth chamber 14 by the susceptor 18. A side heater 19 surrounds the susceptor 18 and the crucible 44 for providing thermal energy to the system 10. The system also includes an outer bottom heater 62 and an inner bottom heater 65.
[0015] During the crystal growth process, the seed crystal 37 is lowered by a pulling mechanism 47 into contact with the melt 46 and then slowly lifted out of the melt 46. As the seed crystal 37 is slowly lifted out of the melt 46, atoms from the melt 46 align with and adhere to the seed crystal 37 to form an ingot 48. The system 10 also includes a heat shield (not shown) configured to shield the ingot 48 from radiant heat from the melt 46 to solidify the ingot 48.
[0016] The system includes a feed tube 43 for adding polysilicon to the crucible 44 (i.e., for replenishing the melt 46 with polysilicon), similar to a continuous Czochralski process. The crystal pulling system 10 also includes a gas inlet (not shown) for introducing an inert gas into the growth chamber 14, and an exhaust port 28 for exhausting the inert gas and other gaseous and airborne particles from the growth chamber 14. A fluid-cooled exhaust tube 52 extends through the bottom 30 of the housing 12 at the exhaust port 28 and into the housing 12. The fluid-cooled exhaust tube 52 is configured to rapidly cool exhaust gases exhausted from the growth chamber 14 during the Czochralski growth process. As described in more detail herein, the fluid-cooled exhaust tube 52 reduces or prevents the accumulation of deposits and precipitates in the exhaust tube 52, thereby facilitating extended run times and increased throughput.
[0017] The housing 12 includes a lower portion 40 including an annular sidewall 42, an upper dome (not shown) connected to the lower portion 40, and an elongated tubular portion (i.e., pull chamber) extending generally upwardly from the upper dome. The lower portion 40 of the housing 12 includes a bottom portion 30, and the annular sidewall 42 extends upwardly from the bottom portion 30. The bottom portion 30 may be rounded, as shown, or may be straight. The housing 12 may be made of stainless steel or other suitable material. In some embodiments, a portion of the housing 12 includes a fluid-cooled (e.g., water-cooled) stainless steel wall.
[0018] The crucible 44 is positioned within the growth chamber 14 such that an ingot 48 can be pulled from a melt 46 within the crucible 44 by a crystal pulling mechanism 47. The crucible 44 may be made of, for example, quartz, or any other suitable material that enables the crystal pulling system 10 to function as described herein. Furthermore, the crucible 44 can have any suitable size that enables the crystal pulling system 10 to function as described herein. The system 10 may include a reflector (not shown) positioned to separate the melt 46 from an upper portion of the system 10.
[0019] The heaters 19, 62, 65 (e.g., resistive heaters) operate to melt an initial charge of solid polycrystalline silicon feedstock and to maintain the melt 46 in a liquefied state after the initial charge has melted. The heaters 19, 62, 65 also operate to melt solid polycrystalline silicon added through the feed tube 43 during the growth of the ingot 48. The heaters are positioned at suitable locations around the crucible 44. In the illustrated embodiment, the bottom heaters 62, 65 are positioned below the susceptor 18 and crucible 44, and the side heater 19 is positioned radially outward from and extends around the susceptor 18 and crucible 44. In the illustrated embodiment, each heater 19, 62, 65 has a generally annular shape, although the heaters can have any suitable shape that enables the crystal pulling system 10 to function as described herein. In the exemplary embodiment, heaters 19, 62, 65 are resistive heaters, however, heaters 19, 62, 65 may be any suitable heating device that enables system 10 to function as described herein. Additionally, system 10 may include any suitable number of heaters that enables system 10 to function as described herein. Crystal pulling system 10 may also include insulation disposed radially outward from and extending around side heaters 19 to prevent heat loss from within growth chamber 14.
[0020] Crystal pulling system 10 may also include a controller communicatively connected to various components of system 10, such as rotatable shaft 45 (or a motor connected to shaft 45), pulling mechanism 47, and heaters 19, 62, 65, to control the operation of such components.
[0021] The gas inlet is fluidly connected to a gas supply. Suitable source gases include, for example, but not limited to, inert gases such as argon, helium, nitrogen, and mixtures thereof. The gas flows generally downward through the growth chamber 14, across the surface of the melt 46, through the exhaust 52, through the ingot puller exhaust 28, and through an exhaust outlet 60 external to the housing 12.
[0022] The crystal pulling system 10 includes an inner shell 55 (sometimes referred to in the art as a "heat pack") within the housing 12 in which the heaters 19, 62, 65 and other components of the system 10 may be disposed. The inner shell 55 includes a bottom heat shield 50 and a side heat shield 57 extending upwardly from the bottom heat shield 50. The bottom heat shield 50 and the side heat shield 57 are disposed within the crystal puller system housing 12 (i.e., the bottom heat shield is axially inward relative to the housing bottom 30 and the side heat shield 57 is radially inward relative to the housing sidewall 42). The bottom heat shield 50 includes a bottom heat shield exhaust opening 58 through the bottom heat shield 50. The bottom heat shield exhaust opening 58 faces generally radially outward relative to the side heat shields 57 of the inner shell.
[0023] 2, the crystal pulling system 10 includes an exhaust gas plenum 33 through which exhaust gases are drawn from inside the inner shell 55 into the exhaust tube 52. The exhaust gas plenum 33 is defined by a plenum housing 71 having a floor 73, a top 76, and a sidewall 75 extending between the floor 73 and the top 76. The plenum housing 71 has an inlet 80 through which exhaust gases enter the plenum 33. The inlet 80 is radially inward of the side heat shield 57 and radially outward of the side heater 19 (FIG. 1). As shown in FIG. 2, the exhaust tube 52 extends into the plenum housing floor 73. The plenum 33 directs gases from within the inner shell 55 radially outward. The plenum 33 extends around the entire circumference of the crystal pulling system 10.
[0024] The plenum housing 71 may be made of an insulating material to keep the exhaust gases at an elevated temperature before they reach the fluid-cooled exhaust 52. Suitable materials from which the plenum housing 71 may be constructed include, for example, without limitation, carbon compounds such as graphite.
[0025] The exhaust pipe 52 extends through the bottom heat shield 50 (e.g., through the entire thickness of the bottom heat shield 50) and through the bottom 30 of the pulling system 10. The plenum inlet 80, the plenum 33, the bottom heat shield exhaust opening 58, the exhaust pipe 52, the ingot puller exhaust port 28 of the housing 12, and the exhaust pipe outlet 60 form an exhaust flow path 70 through which the exhaust gas travels as it is exhausted from the system 10. The exhaust pipe outlet 60 is fluidly connected to a vacuum pump (not shown). The vacuum pump is configured to create a low pressure or suction at the exhaust pipe outlet 60 to remove inert gases, airborne contaminants, and other gaseous products (e.g., SiO, CO) from the growth chamber 14.
[0026] In the illustrated embodiment, the system 10 includes a rotatable auger 49 within the exhaust pipe 52 to remove deposits from the interior surface of the exhaust pipe 52. In another embodiment, the system 10 does not include an auger 49 within the exhaust pipe 52.
[0027] The exhaust pipe 52 extends into the bottom 30 of the housing 12 through a port 56 that extends through the bottom 30. The port 56 may be cooled (e.g., fluid cooled). The port 56 may have an electrical connection 61 for connecting wires to a component (e.g., a heater) within the housing 12. The tube 52 may be removably disposed within the port 56. The tube 52 may be connected to the port 56, such as by clamping a flange portion 78 of the tube 52 between a flange (not shown) of the port 56 and a puller exhaust tubing, or may be connected to the port 56 by other suitable methods. In another embodiment, the tube 52 is fixedly connected to the bottom 30 of the system 10. In some embodiments, the system 10 does not include felt insulation surrounding the exhaust pipe 52.
[0028] The exhaust tube 52 includes a first end 63 that is flush with the floor 73 of the gas plenum housing 71. The exhaust tube 52 is connected to the bottom 30 of the ingot puller housing 12. The exhaust tube 52 includes a second distal end 67 that includes a flange portion 78 for connection to a vacuum system.
[0029] 3-4, the exhaust pipe 52 includes a radially inner wall 82 and a radially outer wall 84 each extending from the first end 63 to the second end 67. The exhaust pipe 52 includes a baffle 91 between the inner wall 82 and the outer wall 84. The inner wall 82, the outer wall 84, and the baffle 91 define a flow channel 88. The flow channel 88 defines a flow path 92 through which a fluid circulates within the exhaust pipe 52. The fluid channel 88 is configured to receive a fluid, such as water, for cooling the exhaust gases within the exhaust flow path 70. The cooling fluid generally travels upward toward the first end 63 of the pipe 52 and returns downward toward the second end 67. The fluid circulating within the fluid channel 88 may be water, which may be at a significantly lower temperature than the hot zone of the puller (e.g., 30°C to 40°C compared to about 1700°C or higher).
[0030] Exhaust pipe 52 The inner wall 82 of the exhaust passage 70 is constructed of a suitable thermally conductive material to facilitate heat exchange between the cooling fluid and the exhaust gases within the exhaust passage 70. Suitable materials from which the inner wall 82 may be constructed include, for example, without limitation, stainless steel. In some embodiments, the inner wall 82 is constructed of the same material as the housing 12. The outer wall 84 and / or the baffle 91 may be constructed of the same material as the inner wall 82 or may be constructed of a different material than the inner wall 82.
[0031] The fluid channel 88 is fluidly connected to a fluid supply 90 at a fluid supply inlet 86 for supplying a cooling fluid to the fluid channel 88. The cooling fluid may be any suitable fluid that enables the system 10 to function as described herein, including, for example, without limitation, water and any cooling fluid (e.g., refrigerated water or ethylene glycol). The flow rate of the cooling fluid through the fluid channel 88 may be controlled to increase or decrease the cooling rate of the exhaust gas in the exhaust flow path. In some embodiments, the flow rate of the cooling fluid through the first fluid channel 88 is between about 5 liters per minute (L / min) and about 60 L / min, and more suitably about 40 L / min. The fluid supply 90 may be connected to suitable flow control components, such as a pump and flow controller (not shown), to control the flow rate of the fluid in the fluid channel 88.
[0032] From a fluid source 90, cooling fluid travels through an inlet 86 and into a fluid channel 88. The cooling fluid travels along a flow path 92 around a baffle 91. The cooling fluid travels within the fluid channel toward the first end 63 of the tube 52 and then toward the second end 64 of the tube 52. 67 and back down the tube towards the fluid supply outlet 93. The cooling fluid travels through the fluid supply outlet 93 and enters the cooling fluid treatment system 96 (e.g., cooled and disposed of or recycled).
[0033] In the illustrated embodiment, the cooling fluid inlet 86 and outlet 93 are fluidly connected to the exhaust pipe 52 at the flange portion 78 of the exhaust pipe 52. The inlet 86 and outlet 93 may be located at other locations along the pipe 52 that enable the exhaust pipe 52 to function as described herein.
[0034] 2, the exhaust pipe 52 extends a length L below the bottom 30 of the housing 12. In the illustrated embodiment, the exhaust pipe 52 is fluid cooled along the entire length L, however, in alternative embodiments, the exhaust pipe 52 may be fluid cooled along only a portion of the length L.
[0035] 1, the crystal pulling system 10 includes a single exhaust tube 52 and port 56. In alternative embodiments, the system may include two, three, or more exhaust tubes 52 and ports. 56 (eg, three exhaust tubes 52 and ports 56 spaced symmetrically around the crystal pulling system bottom 30).
[0036] The crystal pulling system 10 is suitably used to grow a single crystal ingot from a melt 46 according to the Czochralski process. More specifically, the melt 46 is prepared in a crucible 44 by charging the crucible 44 with polycrystalline silicon raw material. The raw material is melted in the crucible 44 using heaters 19, 62, 65 to form a melt 46 of semiconductor or solar grade material. Once the raw material is sufficiently melted, a seed crystal 37 is lowered by a pulling mechanism 47 into contact with the melt 46 to initiate crystal growth, and a single crystal ingot 48 is subsequently grown from the melt 46 by pulling the seed crystal 37 out of the melt 46. Polysilicon is added continuously or intermittently to the crucible 44 via a feed tube 43 to allow the ingot 48 to grow continuously.
[0037] During the growth process, an inert gas, such as argon, is introduced into the growth chamber 14 through the gas inlet and directed generally downward along the surface of the melt 46 to an inlet 80 of the plenum 33. Exhaust gas travels through the plenum 33, the bottom heat shield exhaust opening 58, the exhaust 52, the ingot puller exhaust 28, and through an exhaust outlet 60. A vacuum system establishes a negative or reduced pressure at the exhaust outlet 60 to draw exhaust gases (e.g., inert gases and gas species generated by the melt 46 and / or other components of the system 10) from the growth chamber 14 through an exhaust passage 70.
[0038] The fluid-cooled exhaust pipe 52 cools the exhaust gases relatively rapidly as they flow through the exhaust flowpath 70. In particular, the cooling fluid is directed through fluid channels 88 defined by inner wall 82, outer wall 84, and baffle 91 of the exhaust pipe 52 to effect heat exchange between the exhaust gases and the cooling fluid.
[0039] Without being bound by any particular theory, it is believed that rapidly cooling the exhaust gas, as opposed to maintaining the exhaust gas at an elevated temperature, results in the formation of precipitates (e.g., oxides of silicon (Si) oxide, silicon carbide, and silicon oxide (Si) oxides) having powder-like structures or morphologies that do not adhere to the interior surface of the exhaust pipe 52 as strongly as precipitates formed at higher temperatures (e.g., near the condensation or precipitation temperatures). x O y As a result, precipitates formed within the fluid-cooled exhaust 52 are less likely to agglomerate or accumulate within the exhaust passage 70, allowing the crystal growth process to run for longer periods of time.
[0040] The crystal pulling system described herein offers several advantages over conventional crystal pulling systems. By extending the water-cooled exhaust pipe into the reaction chamber (e.g., through the bottom of the puller, through the bottom heat shield, and / or through the exhaust gas plenum housing), gases near the hot zone of the puller are quench-cooled. This creates a relatively high temperature gradient as gases are removed from the hot zone and gaseous compounds condense in the gas stream to form fewer deposits on the tube walls. Quench cooling also changes the morphology of the condensed particles from a hard solid layer to a powder-like structure that is less likely to adhere to the exhaust tube inner walls. As a result, precipitates that form in the fluid-cooled exhaust pipe of the present disclosure are less prone to agglomerate or accumulate in the exhaust flowpath, allowing the crystal growth process to run for longer. In embodiments where exhaust gases are pulled radially inward from the side heat shields (e.g., through the exhaust gas plenum) and travel radially outward from the side heat shields through the exhaust pipe, the gases may be maintained at a higher temperature (e.g., the flowpath distance to quench cooling is reduced) prior to quench cooling. EXAMPLES
[0041] The processes of the present disclosure are further illustrated by the following examples, which should not be viewed in a limiting sense.
[0042] Example 1: Effect of using a fluid-cooled exhaust tube extending into the reaction chamber Figure 5 shows the conventional Exhaust pipe 52 (i.e., non-fluid cooling that does not extend into the reaction chamber (e.g., through the bottom of the housing) Exhaust pipe 5 shows a blockage of the auger 49 in the exhaust pipe 52. The ingot puller system was operated in a continuous Czochralski pulling process where polycrystalline silicon was added to the melt during ingot growth. The exhaust pipe was constructed of stainless steel and had no cooling fluid channels formed therein. As shown in FIG. 5, the exhaust pipe 52 was completely blocked with deposit D and exhaust gases could not pass through the pipe 52. The auger 49 in the exhaust pipe 52 was energized but was unable to remove the deposit. The reactor was shut down to remove the deposit.
[0043] Figure 6 shows an exhaust pipe 52 that was water cooled and extended into the reaction chamber to the extent shown in Figure 1. Deposit D was more powdery and white-orange in color. The system of Figure 6 did not include an auger. As can be seen, the use of a fluid-cooled exhaust pipe that extended into the reactor chamber closer to the hot zone significantly reduced exhaust pipe deposits.
[0044] Example 2: Effect of using a fluid-cooled exhaust tube extending into the reaction chamber FIG. 7 shows the run time before the exhaust clogged for a crystal puller system where the exhaust was not fluid-cooled and did not extend into the reaction chamber. FIG. 7 also shows the run time before the exhaust clogged for a crystal puller system (circled batches) as shown in FIG. 1 with an exhaust that was fluid-cooled and extended into the reaction chamber. As shown in FIG. 7, the run time increased by over 150% for these batches. This was even with a more highly doped process that would have traditionally increased exhaust tube deposits. This allows more ingots to grow in the puller before pressure buildup occurs.
[0045] As used herein, the terms "about," "substantially," "essentially," and "approximately," when used in conjunction with a range of dimensions, concentrations, temperatures, or other physical or chemical properties or characteristics, are meant to encompass variations that may exist at the upper and / or lower limits of the range of the property or characteristic, including, for example, variations that result from rounding, measurement methods, or other statistical variations.
[0046] When introducing elements of the present disclosure or embodiments thereof, the articles "a," "an," "the," and "said" are intended to mean that there are one or more of the element. The terms "comprising," "including," "containing," and "having" are intended to be inclusive and mean that there may be additional elements other than the listed elements. The use of terms indicating a particular orientation (e.g., "top," "bottom," "side," etc.) is for convenience of description and does not require a particular orientation of the items being described.
[0047] Since various changes can be made in the above structures and methods without departing from the scope of the disclosure, it is intended that all matter contained in the above description and shown in the accompanying drawings shall be interpreted as illustrative and not in a limiting sense.
Claims
1. 1. A crystal pulling system for growing a single crystal ingot from a silicon melt, comprising: a crystal pulling system housing defining a growth chamber, the crystal pulling system housing having a bottom and a sidewall extending from the bottom; a bottom heat shield disposed above a bottom of the crystal pulling system housing, the bottom of the crystal pulling system housing and the bottom heat shield being separated by a gap; a crucible disposed within the growth chamber for containing the silicon melt; an exhaust tube extending outwardly through the bottom of the crystal pulling system housing, the exhaust tube defining an exhaust flow path for exhausting exhaust gases from the growth chamber; Equipped with The exhaust pipe is The inner wall and The exterior wall and a fluid channel defined between the inner wall and the outer wall for circulating a cooling fluid to cool the exhaust gas in the exhaust flow passage, the fluid channel extending through the bottom of the crystal pulling system housing to at least the bottom heat shield; Including, Crystal pulling system.
2. an exhaust gas plenum including a plenum housing including a floor, a top, and a sidewall extending between the floor and the top, the exhaust pipe extending into the floor of the plenum housing; 2. A crystal pulling system as claimed in claim 1.
3. The plenum housing is made of a thermally insulating material.
3. A crystal pulling system according to claim 2.
4. the exhaust gas plenum has an inlet, the inlet being radially inward relative to a side heat shield disposed above the bottom heat shield, the side heat shield being radially inward relative to a side wall of the plenum housing; 3. A crystal pulling system according to claim 2.
5. A side heater surrounding the crucible, the inlet of the exhaust gas plenum being disposed radially outward relative to the side heater.
5. A crystal pulling system according to claim 4.
6. a vacuum pump fluidly connected to the exhaust line to draw the exhaust gas through the exhaust passage.
2. A crystal pulling system as claimed in claim 1.
7. a portion of the exhaust tube extends downwardly from the bottom of the crystal pulling system housing, the portion being fluid cooled; 2. A crystal pulling system as claimed in claim 1.
8. a rotatable auger disposed within the exhaust pipe for removing deposits from an inner surface of the exhaust pipe; 2. A crystal pulling system as claimed in claim 1.
9. further comprising a supply tube for adding polysilicon to the crucible.
2. A crystal pulling system as claimed in claim 1.
10. the exhaust pipe comprises a baffle disposed between the inner wall and the outer wall, the fluid channel being defined between the inner wall, the outer wall, and the baffle.
2. A crystal pulling system as claimed in claim 1.