Template for imprinting, imprinting device, and method for manufacturing semiconductor device

The imprint template with a surrounding wall structure addresses bubble-related defects in nanoimprint technology by ensuring uniform resist application, improving semiconductor device production efficiency and quality.

JP2024132584APending Publication Date: 2024-10-01KIOXIA CORP
View PDF 18 Cites 0 Cited by

Patent Information

Application Number
JP2023043418
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-17
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

The generation of air bubbles during the imprint process in nanoimprint technology leads to defects in the transferred uneven patterns on semiconductor devices, particularly when using templates with multi-stage uneven patterns, causing inefficiencies in mass production.

Method used

The use of an imprint template with a substrate and surrounding wall structure that supports a pattern portion with varying heights, where the surrounding wall has a height greater than the tallest pillar, allowing resist to be supplied and held effectively, suppressing bubble formation and ensuring uniform filling.

Benefits of technology

This approach reduces defects in the transferred pattern on wafers, enhancing the efficiency and quality of semiconductor device production by preventing air bubbles and ensuring consistent resist application.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024132584000001_ABST
    Figure 2024132584000001_ABST
Patent Text Reader

Abstract

To provide a template for imprinting that can suppress the occurrence of defects in a transferred concavo-convex pattern.SOLUTION: A template has a substrate, a patterned section that has a height less than or equal to the first height and is erected from the substrate, and an encircling wall that has a height more than or equal to the first height, is erected from the substrate and surrounds the patterned section, and a resist pattern based on the shape of the patterned section can be formed on a wafer by pressing the wafer against the resist held in the area surrounded by the encircling wall and curing the resist while the wafer is pressed against the resist.SELECTED DRAWING: Figure 1B
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present embodiment relates to an imprint template, an imprint apparatus, and a method for manufacturing a semiconductor device. [Background technology]

[0002] In recent years, nanoimprint technology, known as a microfabrication technology, has been proposed. Nanoimprint technology is a pattern formation technology in which a concave-convex pattern is transferred to a transfer target such as an imprint resin by using an imprint template on which the concave-convex pattern is formed, and has been used, for example, in mass production of semiconductor devices. In a transfer process using the imprint technology, air bubbles may be generated in the resin that penetrates the concave-convex pattern of the template, which may cause defects in the concave-convex pattern transferred to the transfer target. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2010-076300 A [Patent Document 2] International Publication No. 2011 / 040466 Summary of the Invention [Problem to be solved by the invention]

[0004] According to this embodiment, there is provided an imprint template that can suppress the occurrence of defects in the transferred concave-convex pattern. [Means for solving the problem]

[0005] One aspect of an embodiment of the present disclosure provides a template comprising a substrate, a pattern portion standing from the substrate with a height equal to or less than a first height, and a surrounding wall standing from the substrate with a height equal to or greater than the first height and surrounding the pattern portion, the template being configured to be capable of forming a resist pattern on the wafer based on the shape of the pattern portion by pressing a wafer against a resist held in an area surrounded by the surrounding wall and hardening the resist while the wafer is pressed against the resist.

[0006] Another aspect of an embodiment of the present disclosure provides an imprint apparatus including: a template having a substrate, a pattern portion standing from the substrate with a height equal to or less than a first height, and a surrounding wall standing from the substrate with a height equal to or greater than the first height and surrounding the pattern portion; a resist supply unit that supplies resist to an area surrounded by the surrounding wall of the template; a resist pattern forming unit that presses a wafer against the resist held in the area surrounded by the surrounding wall and hardens the resist while the wafer is pressed against the resist, thereby forming a resist pattern on the wafer based on a shape of the pattern portion; and a light source unit that irradiates light from the side of the template opposite to the side against which the wafer is pressed.

[0007] Yet another aspect of an embodiment of the present disclosure provides a method for manufacturing a semiconductor device, the method comprising: supplying resist to an area surrounded by a surrounding wall of a template having a substrate, a pattern portion standing from the substrate with a height equal to or less than a first height, and a surrounding wall standing from the substrate with a height equal to or greater than the first height and surrounding the pattern portion; pressing a wafer against the resist held in the area surrounded by the surrounding wall; and hardening the resist while the wafer is pressed against the resist, thereby forming a resist pattern on the wafer based on the shape of the pattern portion. [Brief description of the drawings]

[0008] [Figure 1A] FIG. 1A is a plan view showing a schematic configuration of an imprint template 100 according to an embodiment of the present disclosure. [Figure 1B]FIG. 1B is a schematic cross-sectional view of the imprint template 100 shown in FIG. 1A. [Diagram 2] FIG. 2 is a schematic diagram showing the overall configuration of the imprint apparatus 300. As shown in FIG. [Diagram 3] FIG. 3 is a flowchart of the imprint method according to this embodiment. [Figure 4A] FIG. 4A is a schematic cross-sectional view showing one step of the imprint process according to this embodiment. [Figure 4B] FIG. 4B is a schematic cross-sectional view showing one step of the imprint process according to this embodiment. [Figure 4C] FIG. 4C is a schematic cross-sectional view showing one step of the imprint process according to this embodiment. [Figure 5A] FIG. 5A is a schematic cross-sectional view showing one step of the imprint process according to this embodiment. [Figure 5B] FIG. 5B is a schematic cross-sectional view showing one step of the imprint process according to this embodiment. [Figure 5C] FIG. 5C is a schematic cross-sectional view showing one step of the imprint process according to this embodiment. [Figure 6A] FIG. 6A is a schematic perspective view of a wafer 200 according to this embodiment. [Figure 6B] FIG. 6B is a schematic perspective view of chip 210 according to this embodiment. [Figure 7A] FIG. 7A is a schematic perspective view of the template 100 according to the present embodiment. [Figure 7B] FIG. 7B is a schematic cross-sectional view of the template 100. [Figure 8A] FIG. 8A is a schematic perspective view of the pattern portion 140. FIG. [Figure 8B] FIG. 8B is an enlarged perspective view of a portion of the pattern portion 140 shown in FIG. 8A. [Figure 8C] FIG. 8C is an enlarged perspective view of a portion of pattern portion 140 shown in FIG. 8B. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] Hereinafter, the present embodiment will be described with reference to the accompanying drawings. In order to facilitate understanding of the description, the same components in each drawing are denoted by the same reference numerals as much as possible, and duplicated description will be omitted.

[0010] [Imprint template] Fig. 1A is a plan view showing a schematic configuration of an imprint template 100 according to an embodiment of the present disclosure, and Fig. 1B is a schematic cross-sectional view showing a BB cross section of the imprint template 100 shown in Fig. 1A. Note that a template on which a pattern to be transferred in an imprint process is formed, such as the imprint template 100 according to this embodiment, may also be called, for example, a mold, stamper, or model, but in the following embodiments, it will be mainly referred to as a template.

[0011] 1A, the imprint template 100 according to the embodiment of the present disclosure includes a substrate 120, a pattern portion 140 having a height equal to or less than a first height H1 and standing from the substrate 120, and a surrounding wall 160 having a height equal to or greater than the first height H1 and standing from the substrate 120 to surround the pattern portion 140. As will be described later, the imprint template 100 according to the embodiment is configured to be capable of forming a resist pattern based on the shape of the pattern portion 140 on the wafer 200 by pressing a wafer 200, which is an object to be transferred, against a resist held in an area surrounded by the surrounding wall 160 in an imprint process, and curing the resist R while the wafer 200 is pressed against the resist R.

[0012] The substrate 120 has a first surface 122 and a second surface 124 opposite to the first surface 122. The pattern portion 140 is formed on the first surface 122.

[0013] The pattern portion 140 includes a plurality of pillars 142 having different heights. The plurality of pillars 142 include a first pillar group 142a, a second pillar group 142b, a third pillar group 142c, and a fourth pillar group 142d. The first pillar group 142a includes first pillars 142a11, 142a12, 142a13, 142a21, 142a22, 142a23, 142a31, 142a32, 142a33, 142a41, 142a42, and 142a43. Similarly, the second pillar group 142b includes second pillars 142b11, 142b12, 142b13, 142b21, 142b22, 142b23, 142b31, 142b32, 142b33, 142b41, 142b42, and 142b43, and the third pillar group 142c includes third pillars 142c11, 142c12, 142c13, 142c21, 142c22, and 142b43. , 142c23, 142c31, 142c32, 142c33, 142c41, 142c42, and 142c43, and the fourth pillar group 142d includes fourth pillars 142d11, 142d12, 142d13, 142d21, 142d22, 142d23, 142d31, 142d32, 142d33, 142d41, 142d42, and 142d43. The heights of first pillars 142a11, 142a12, 142a13, 142a21, 142a22, 142a23, 142a31, 142a32, 142a33, 142a41, 142a42, and 142a43 included in first pillar group 142a are all a first height H1.Similarly, the heights of the second pillars 142b11, 142b12, 142b13, 142b21, 142b22, 142b23, 142b31, 142b32, 142b33, 142b41, 142b42, and 142b43 included in the second pillar group 142b are all the second height H2. 1B, the heights of the fourth pillars 142d11, 142d12, 142d13, 142d21, 142d22, 142d23, 142d31, 142d32, 142d33, 142d41, 142d42, and 142d43 included in the fourth pillar group 142d are all the third height H3. As shown in FIG. 1B, the first height H1, the second height H2, the third height H3, and the fourth height H4 satisfy the relationship H1>H2>H3>H4. As described below, in an embodiment of the present disclosure, a template 100 including a plurality of pillars 142 in multiple stages with different heights is used to transfer a multi-stage concave-convex pattern onto a wafer 200 that is a transfer target.

[0014] The surrounding wall 160 has a first wall portion 162a and a second wall portion 162b spaced apart from each other in the X direction. The surrounding wall 160 further has a third wall portion 162c and a fourth wall portion 162d spaced apart from each other in the Y direction perpendicular to the X direction. In the template 100, the surrounding wall 160 is configured such that the first wall portion 162a, the second wall portion 162b, the third wall portion 162c, and the fourth wall portion 162d surround a region of the first surface 122 of the substrate 120 where the pattern portion 140 is to be formed. Therefore, in the imprinting process described later, the resist R used as an imprinting resin can be stored in the template 100. In this embodiment, the first wall portion 162a, the second wall portion 162b, the third wall portion 162c, and the fourth wall portion 162d constituting the surrounding wall 160 all have a height equal to or greater than the first height H1, which is the height of the first pillar group 142a having the maximum height among the plurality of pillars 142. Therefore, the resist R can be stored (held) inside the surrounding wall 160 so that all the pillars 142 are immersed in the resist R. Therefore, the imprint template 100 according to this embodiment can be effectively used in an imprint process in which the pattern portion 140 having a concave-convex pattern formed therein faces upward (upward in the Z direction in this embodiment), the pattern portion 140 is coated with the resist R, and the resist R is transferred to the lowered wafer 200.

[0015] In the imprint process using an imprint template, when resist is applied to the concave-convex pattern formed on the template, air bubbles may enter the concave-convex pattern without penetrating the concave-convex pattern. In this case, the desired concave-convex pattern is not formed on the transfer target such as a wafer, which may result in a defect. The present inventors have found that defects caused by air bubbles may be easily generated when an imprint process is performed using an imprint template in a semiconductor device manufacturing process. In the semiconductor device manufacturing process, a multi-stage concave-convex pattern is transferred to a wafer by an imprint process using a template having a multi-stage concave-convex pattern, for example, in which a plurality of pillars having different heights are provided. By transferring the multi-stage concave-convex pattern, for example, a columnar electrode may be provided on the wafer as described later. The present inventors have found that when such a multi-stage concave-convex pattern is transferred to a wafer, air bubbles are easily generated in the concave-convex pattern on the template, particularly near the pillars having a low height. In the imprint process using a template having a multi-stage uneven pattern, a resist layer to which the uneven pattern is transferred can be formed by applying resist onto a wafer and then pressing the template onto the resist, but it is considered that bubbles are likely to occur, particularly near relatively low pillars, because some of the air that existed before being pressed against the resist does not escape and remains as air bubbles in the resist layer. Alternatively, when using a template having a multi-stage uneven pattern, it is difficult to fill the resist uniformly compared to using a template with pillars of the same height, and it is considered that in areas where low pillars are formed, the volume that can be filled with resist is relatively large compared to areas where high pillars are formed, and therefore air bubbles are likely to occur due to the fact that the resist to be filled is likely to be insufficient.

[0016] As a result of intensive research, the present inventors have found that by providing a surrounding wall on the imprint template, it is possible to suppress the generation of bubbles in the resist filled in the template in the imprint process, as described below. The imprint template 100 according to this embodiment is arranged so that the surface on which the pattern portion 140 is formed faces upward, the inside of the surrounding wall 160 of the template 100 is filled with the resist R, the wafer 200 is pressed from above the filled resist R, and the resist R is hardened to form a resist layer on the wafer 200 to which the shape of the pattern portion 140 is transferred. That is, since the imprint template 100 according to this embodiment has the surrounding wall 160, it can be effectively used in the imprint process in which the pattern portion 140 of the template 100 is arranged on the upper side, and at this time, the resist R can be filled from above the pattern portion 140, so that the resist R can be supplied along the uneven shape of the pattern portion 140, for example. Therefore, in the case where the pattern portion 140 includes a plurality of pillars 142 having different heights as described above, even in the portion where low pillars (for example, the third pillar group 142c and the fourth pillar group 142d) are formed, the resist R can be supplied along the shape of the pillars 142, so that the resist R can be supplied while suppressing the generation of bubbles. In this embodiment, the surrounding wall 160 is provided on the template 100, so that the outflow of the resist R held (stored) by the surrounding wall 160 can be suppressed. Therefore, even in the case where the imprint process is performed with the pattern portion 140 of the template 100 arranged to be on the upper side, it is possible to efficiently supply the resist R and hold the supplied resist R. In this embodiment, the surrounding wall 160 has a height equal to or greater than the highest pillar 142 (first pillar group 142a) having a height of the first height H1 among the plurality of pillars 142, so that the imprint resin R does not flow out even if the imprint resin (resist R) is supplied in an amount that immerses the highest pillar 142. Therefore, even if the template 100 has relatively high pillars, the geometric pattern can be transferred onto the wafer 200 while suppressing the occurrence of defects.Furthermore, since the surrounding wall 160 is provided, it is possible to use, for example, a resist R having a relatively low viscosity. By using the resist R having a low viscosity, it is possible to efficiently supply the resist R along the uneven shape.

[0017] In recent years, in the manufacturing process of semiconductor devices, imprint technology has been used in the step of forming a fine pattern structure on a wafer, and the improvement of mass production efficiency has been considered. The pattern structure formed has uneven shapes such as pillar shapes of different heights, and defects in the pattern structure may occur due to bubbles generated in the resist that penetrates the template. By using the imprint template 100 according to this embodiment, it is possible to suppress the occurrence of defects in the uneven shape transferred onto the wafer 200, thereby improving the mass production efficiency of semiconductor devices.

[0018] [Imprint device] An imprint apparatus 300 according to this embodiment will be described with reference to Fig. 2. Fig. 2 is a schematic diagram showing the overall configuration of the imprint apparatus 300. The imprint apparatus 300 according to this embodiment is an apparatus that transfers a pattern of a template 100 onto a wafer 200, and forms a pattern on the wafer 200 with a resist R using an imprint method such as optical nanoimprint lithography.

[0019] The imprint apparatus 300 includes the template 100 having the substrate 120, the pattern portion 140 having a height equal to or less than a first height H1 and standing from the substrate 120, and a surrounding wall 160 having a height equal to or greater than the first height H1 and standing from the substrate 120, surrounding the pattern portion 140, as described above with reference to Figures 1A and 1B, a resist supply unit 320 that supplies resist R to the area surrounded by the surrounding wall 160 of the template 100, a resist pattern forming unit 340 that presses the wafer 200 against the resist R held in the area surrounded by the surrounding wall 160, and hardens the resist R while the wafer 200 is pressed against the resist R, thereby forming a resist pattern on the wafer 200 based on the shape of the pattern portion 140, and a light source unit 360 that irradiates light from the side of the substrate 120 of the template 100 opposite the side against which the wafer 200 is pressed.

[0020] The resist supply unit 320 includes a resist tank 322 and a resist nozzle 324. The resist tank 322 holds the resist R before curing (i.e., before irradiation with a resin curing light such as ultraviolet light). The resist nozzle 324 drops the resist R in the resist tank 322 onto the template 100, and supplies the resist R to the region surrounded by the surrounding wall 160 of the template 100. The amount of resist R to be dropped and the location to which the resist nozzle 324 drops may be controlled by a control unit, a driving mechanism, etc. (not shown). For example, the resist nozzle 324 may be an inkjet type resist dropping mechanism, and the amount of resist R to be dropped may be controlled by controlling the voltage applied to the inkjet type resist nozzle 324, the time for applying the voltage, etc. For example, the resist nozzle 324 may be controlled so that a larger amount of resist R is dropped into a region of the template 100 where a pattern portion 140 with a small height is formed, compared to a region where a pattern portion 140 with a large height is formed.

[0021] In the example shown in FIG. 2, the imprint apparatus 300 is provided with one resist nozzle 324, and the one resist nozzle 324 moves and scans on the template 100 in the X direction and the Y direction (directions perpendicular to the paper surface in FIG. 2) to supply the resist R to the template 100, but is not limited to this. The imprint apparatus 300 may be configured to have, for example, a plurality of resist nozzles 324, and the plurality of resist nozzles 324 move in the X direction and the Y direction, respectively, to supply the resist R. Alternatively, the imprint apparatus 300 may be configured to have a plurality of resist nozzles 324 arranged in an array to supply the resist R to the template 100. In this case, for example, the plurality of resist nozzles 324 may be arranged in one row, a plurality of rows, or a staggered pattern. In addition, for example, the plurality of resist nozzles 324 may be arranged in an array over the width of the template 100 in the X direction or the Y direction or more, and thus the resist R can be supplied to the template 100 by at least one scan in a direction (for example, the X direction or the Y direction) intersecting the arrangement direction of the resist nozzles 324. At this time, as in the case where one resist nozzle 324 is used, the amount of resist R discharged from each of the multiple resist nozzles 324 arranged in an array may be controlled depending on the shape of the pattern portion 140 of the template 100, etc.

[0022] The resist pattern forming unit 340 includes a wafer chuck 342, a wafer stage 344, and a pressurizing mechanism 346. The wafer chuck 342 is configured to hold the wafer 200. For example, a vacuum suction mechanism may be used as the wafer chuck 342, and the wafer 200 held by the wafer chuck 342 is configured to be movable by driving the wafer stage 344 by a driving mechanism (not shown). The pressurizing mechanism 346 is configured to be able to pressurize the wafer 200 from above via the wafer stage 344 and the wafer chuck 342, and presses the wafer 200 against the template 100 by applying pressure in the vertical direction (Z direction) as will be described later regarding the imprint process.

[0023] The light source unit 360 includes an exposure light source 362, an optical mechanism 364, and a template chuck 366. For example, an ultraviolet ray irradiation lamp such as a halogen lamp that irradiates ultraviolet rays or the like capable of curing the resist R is used as the exposure light source 362. When a photocurable resin that uses light rays other than ultraviolet rays is used as the resist R, an irradiation lamp that irradiates light rays other than ultraviolet rays is used as the exposure light source 362. The optical mechanism 364 includes a lens, an aperture, a shutter, and the like that exposes the resist R and adjusts the irradiation light that hardens it. The template chuck 366 is configured to hold the template 100. The template chuck 366 may be formed of, for example, a light-transmitting material, and the light rays from the exposure light source 362 are adjusted by the optical mechanism 364 and are irradiated to the template 100 side through the template chuck 366. In this embodiment, the template 100 is also formed of a light-transmitting material, and the irradiation light from the exposure light source 362 also passes through the template 100 and is irradiated onto the resist R stored in the template 100, hardening the resist R. In this way, the resist R is hardened on the wafer 200 pressed vertically against the template 100, and a resist pattern corresponding to the pattern portion 140 formed on the template 100 is transferred.

[0024] 2, the imprint apparatus 300 may further include a base plate 382 that supports the entire imprint apparatus 300. The imprint apparatus 300 may also include mechanisms for positioning the template 100 and the wafer 200 that is the transfer target, such as an alignment scope 384 and a reference mark 386, and the alignment scope 384 may be configured to detect the position of the reference mark 386 and supply information for positioning the wafer 200 held and driven by the above-mentioned wafer chuck 342 to a control unit (not shown). The imprint apparatus 300 may also include a wafer stage support frame 388 that can form a plane that serves as a reference for the movement of the wafer stage 344. The imprint apparatus 300 may also include, for example, a resist recovery mechanism (not shown) that recovers the resist R that has fallen from the template 100. The imprinting apparatus 300 may further include a vibration mechanism configured to apply vibration to the template 100. The vibration mechanism vibrates the template 100 in the vertical and / or horizontal directions, and can promote penetration of the resist R supplied to the template 100 into the fine pattern shape of the pattern portion 140. The imprinting apparatus 300 may also be provided with a pressure control mechanism, and the pressure control mechanism can reduce the pressure in the space in which the template 100 is placed, thereby more effectively promoting penetration of the resist R supplied to the template 100 into the pattern portion 140. At this time, for example, the template 100 may be formed of a porous layer in which a large number of minute cavities are formed, and thus the pressure inside the minute cavities of the porous layer formed in the template 100 is reduced, and a force is applied to the resist R to draw it into the cavities, promoting penetration of the resist R. Note that the cavities of the porous layer formed here preferably have a size (diameter of the cavities) such that the resist R does not penetrate into the inside of the cavities of the porous layer due to the surface tension of the interface of the resist R.

[0025] [Method of manufacturing semiconductor device] Next, a method for manufacturing a semiconductor device according to an embodiment of the present disclosure will be described. The method for manufacturing a semiconductor device according to an embodiment of the present disclosure includes a substrate 120, a pattern portion 140 having a height equal to or less than a first height H1 and standing from the substrate 120, and a surrounding wall 160 having a height equal to or more than the first height H1 and standing from the substrate 120 to surround the pattern portion 140. The method supplies resist R to an area surrounded by the surrounding wall 160 of a template 100, presses a wafer 200 against the resist R held in the area surrounded by the surrounding wall 160, and hardens the resist while the wafer is pressed against the resist, thereby forming a resist pattern based on the shape of the pattern portion 140 on the wafer 200.

[0026] Hereinafter, an imprint method according to an embodiment of the present disclosure will be described with reference to Fig. 3. The imprint method according to the present embodiment shown in Fig. 3 is performed as at least a part of a method for manufacturing a semiconductor device, and for example, as described above, the imprint method according to the present embodiment may be implemented in the step of forming a columnar electrode in the method for manufacturing a semiconductor device.

[0027] As shown in FIG. 3, first, a resist R is supplied to the area surrounded by the surrounding wall 160 of the template 100 (S302).

[0028] Next, the wafer 200 is pressed against the resist R (S304).

[0029] Next, with the wafer 200 pressed against the resist R, the resist R is hardened to form a resist pattern on the wafer 200 (S306).

[0030] In this manner, a resist pattern to which the shape of the pattern portion 140 is transferred can be formed on the wafer 200.

[0031] Next, an imprint process using the imprint template 100 according to an embodiment of the present disclosure will be described. Figures 4A, 4B, 4C, 5A, 5B, and 5C are schematic cross-sectional views showing each step of the imprint process according to this embodiment.

[0032] First, as shown in FIG. 4A, an imprint template 100 is prepared.

[0033] Next, as shown in FIG. 4B, the imprint resin R is supplied to the template 100. As the imprint resin R (resist R), for example, a photo-curable resin such as an ultraviolet-curable resin may be used. In the imprint process according to this embodiment, the imprint resin R may be supplied to the region of the template 100 surrounded by the surrounding wall 160, for example, by an inkjet method. By supplying the imprint resin R by an inkjet method, it is easy to adjust the supply amount to the region of the template 100 surrounded by the surrounding wall 160. For example, it is possible to adjust the amount of imprint resin supplied to a region where a relatively high pillar 142 (for example, the first pillar group 142a) is provided, compared to a region where a relatively low pillar 142 (for example, the fourth pillar group 142d) is provided. Therefore, in the imprint process using a template provided with a plurality of pillars 142 having different heights from each other, such as the imprint template 100 according to the embodiment of the present disclosure, the imprint resin can be efficiently supplied by the inkjet method. Furthermore, the amount of the imprinting resin supplied can be easily adjusted, which makes it easier to prevent the generation of air bubbles.

[0034] Fig. 4C shows a state in which the template 100 is filled with the imprinting resin R. As shown typically in Fig. 4C, in this embodiment, the template 100 is used to supply the imprinting resin R from above, whereby the template 100 can be filled with the imprinting resin R while suppressing the generation of air bubbles.

[0035] Next, as shown in FIG. 5A, the wafer 200 is pressed against the resist R held in the area surrounded by the surrounding wall 160.

[0036] In this embodiment, an adhesion layer may be formed on the wafer 200. That is, the wafer 200 has a main surface 200a on which a resist pattern is formed, and an adhesion layer may be formed on the main surface before the wafer 200 is pressed against the resist R held in the area surrounded by the surrounding wall 160. The adhesion layer may be formed on the main surface 200a of the wafer 200 by a spin coating method using a known adhesion composition for imprints, so as to have a thickness of several nanometers (e.g., 3 nanometers). By forming the adhesion layer, the adhesion between the resin for imprints R and the wafer 200 can be improved.

[0037] In addition, in this embodiment, before the wafer 200 is pressed against the resist R held in the region surrounded by the surrounding wall 160, a film may be formed on the main surface 200a of the wafer 200 using the same material as the resist R. The film formed by the resist R corresponds to a film called a resist residual film formed on the surface of the wafer 200 when a pattern structure is formed by pressing the template 100 from above the wafer 200 after the resist R is supplied onto the wafer 200 in an imprint process. The thickness of the resist residual film is also called RLT (Residual Layer Thickness) and may be, for example, 20 nm. The film (thin film) formed by the resist R may be formed by a spin coating method, or may be formed by, for example, exposing the main surface 200a to light and curing the resist R after the resist R is supplied to the main surface 200a of the wafer 200. That is, prior to exposure (main exposure) for forming a pattern structure on the main surface 200a of the wafer 200, a thin film of resist R may be formed by pre-exposing the resist R applied in a thin film form on the main surface 200a of the wafer 200.

[0038] 5B, the resist R is hardened by exposing the substrate 120 of the template 100 from the side opposite to the side against which the wafer 200 is pressed (the lower side in the Z direction in FIG. 5B). That is, the resist R is hardened in a state in which the wafer 200 is pressed against the resist R. Therefore, the thin film provided in advance on the main surface 200a of the wafer 200 described above using the resist R may be temporarily exposed during the thin film formation, and then hardened by main exposure that hardens the resist R held by the template 100.

[0039] In this way, the template 100 according to this embodiment can be used in an imprint process for forming a concave-convex pattern by using a photocurable resin such as a UV curable resin as the resist R. At this time, in the process of curing the resist R shown in Fig. 5B, the substrate 120 of the template 100 may be light-transmitting so that the light beam used for curing can be transmitted from the lower side of the template 100 in the Z direction in Fig. 5B.

[0040] 5C, the template 100 is separated from the wafer 200. In this manner, a resist pattern to which the pattern structure of the pattern portion 140 of the template 100 is transferred is formed on the main surface 200a of the wafer 200.

[0041] In this embodiment, a release layer may be formed on the inner surface of the template 100. That is, a release layer may be formed on the pattern portion 140 of the template 100, the region of the substrate 120 other than the portion where the pattern portion 140 is in contact, and the inside of the surrounding wall 160. By forming the release layer, when separating the wafer 200, which is the transfer target, from the template 100 after exposure, it is possible to perform the release while suppressing the occurrence of damage to the transferred resist pattern. Note that, as the release agent, for example, a known release material used in imprint processing may be used and provided to have a thickness in the range of 1 nm to 1 μm.

[0042] Next, a specific example of a semiconductor device having a resist pattern produced using the imprint template 100 according to this embodiment will be described. FIG. 6A is a schematic diagram of a wafer 200 according to this embodiment, and FIG. 6B is a schematic diagram of an enlarged portion of the wafer 200. In the example shown in FIG. 6A, a plurality of chips 210 on which a resist pattern is formed are present on the main surface 200a of the wafer 200. As shown in FIG. 6A and FIG. 6B, in this embodiment, 16 chips 210 are arranged in a 4x4 arrangement (4 in the x direction and 4 in the y direction).

[0043] Fig. 6B shows a schematic diagram of 16 chips out of the plurality of chips 210. In the example shown in Fig. 6B, eight resist patterns 212 are formed for each chip 210.

[0044] Here, as shown in FIG. 6A, gaps 220 are formed between each of chip groups 210-1, ..., 210-n, each of which is a set of 16 chips 210. In this embodiment, a resist pattern can be transferred to 16 chips in a 4x4 arrangement as shown in FIG. 6B by one imprint process, and by repeating the transfer to the 16 chips, transfer to a plurality of chips 210 arranged across the entire wafer 200 via gaps 220 as shown in FIG. 6A is advanced. The repeated imprint process is also called a step-and-repeat method, in which the wafer 200 is moved step by step for each batch transfer of a shot of the wafer 200, and moved to the transfer area of ​​the next shot. The gaps 220 between the areas where transfer is performed in one shot are also called streets. In addition, as shown in Figures 6A and 6B, when wafer 200 is circular in a planar view, chip group 210 existing on the circumference may include 16 or less chips; for example, chip group 210-6 shown in Figure 6A includes 11 chips 210.

[0045] With reference to FIG. 7A and FIG. 7B, the template 100 used for the one-shot imprinting to the 16 chips 210 will be described. FIG. 7A is a schematic perspective view of the template 100 according to this embodiment, and FIG. 7B is a schematic cross-sectional view of the template 100. As shown in FIG. 7A and FIG. 7B, the template 100 has 16 pattern portions 144 provided to correspond to the 16 chips 210, and a surrounding wall 160 provided to surround the 16 pattern portions 144. Each pattern portion 144 includes eight pattern structures 146 for transferring eight resist patterns 212 for one chip 210. Note that, for ease of understanding, FIG. 7B shows only the pattern structures 146 of some of the pattern portions 144 among the eight pattern structures 146 included in each of the 16 pattern portions 144. By using the template 100 shown in FIG. 7A and FIG. 7B, one-shot imprinting can be performed for 16 chips. For example, as in the chip group 210-6 shown in FIG. 6A, 16 or less chips 210 are provided in a peripheral region of the wafer 200, but imprinting can be performed in a similar manner using the template 100 even in a peripheral region such as the region in which the chip group 210-6 is provided. Thus, in the template 100 according to this embodiment, the pattern portion 140 may have a plurality of pillars 142 periodically arranged in a first direction (X direction) and / or a second direction (Y direction) intersecting the first direction. In the example shown in FIG. 7A, the X direction and the Y direction are orthogonal to each other.

[0046] In the imprint process of this embodiment, after imprinting of one shot is completed, when imprinting of the next shot is performed, the template 100 is moved so that the surrounding wall 160 of the template 100 is on the street 220 between the current shot and the next shot, or between the previous shot and the next shot, and the imprint process for multiple chips 210 on the wafer 200 is carried out.

[0047] That is, in this embodiment, the main surface 200a of the wafer 200 includes a first transferred region (for example, the chip group 210-1 shown in FIG. 6A) in which a resist pattern is formed, and a second transferred region (chip group 210-2) in which a resist pattern is formed and which is adjacent to the first transferred region (chip group 210-1) via a gap portion (street 220), and the surrounding wall 160 of the template 100 has a first wall portion 162a and a second wall portion 162b that are provided to be spaced apart in the first direction (x direction). In the imprint process according to this embodiment, the template 100 transfers the first transferred region (chip group 210- When the template 100 is positioned at a first position facing the first transfer region (chip group 210-1) where the first wall portion 162a is positioned at a gap portion facing position facing the gap portion (street 220), a resist pattern is formed in the first transferred region (chip group 210-1), and by moving the template 100 relative to the wafer 200 in the first direction (X direction) from the first position to a second position facing the second transfer region (chip group 210-2) where the second wall portion is positioned at a gap portion facing position, a resist pattern is formed in the second transferred region (chip group 210-2).

[0048] In other words, in the template 100 according to this embodiment, the surrounding wall 160 may be formed to correspond to the gap portion 220 (streets 220) on the wafer 200. That is, in this embodiment, the wafer 200 includes a first transferred region (e.g., chip group 210-1) in which the shape of the pattern portion 140 is formed, and a second transferred region (chip group 210-2) in which a resist pattern is formed and which is adjacent to the first transferred region (chip group 210-1) via a gap portion (streets 220), and the surrounding wall 160 has a first wall portion 162a and a second wall portion 162b that are spaced apart in a first direction (X direction in FIG. 6A ), and the first wall portion The wall portion 162a and the second wall portion 162b may be provided such that when the pattern portion 140 is disposed so as to face the first transferred region (chip group 210-1), the first wall portion 162a faces the gap portion (street 220) of the wafer 200, and when the template 100 is moved in the first direction (X direction) and the pattern portion 140 is disposed so as to face the second transferred region (chip group 210-2), the second wall portion 162b faces the gap portion (street 220). At this time, the width of the first wall portion 162a and / or the width of the second wall portion 162b may be equal to or smaller than the width of the gap portion (street 220). By forming the surrounding wall 160 so that the width of the first wall portion 162a and / or the width of the second wall portion 162b is equal to or less than the width of the gap portion (the street 220), when a resist pattern is transferred to a wafer 200 having a plurality of chips 210 provided thereon as shown in Fig. 6A, for example, it is possible to suppress contact of the surrounding wall 160 with the surface of the chip 210. Therefore, damage to the chip 210 and damage to the resist pattern caused by the surrounding wall 160 of the template 100 can be suppressed.

[0049] In this embodiment, the width of the first wall portion 162a in the first direction (X direction) and the width of the second wall portion 162b in the first direction (X direction) may be not less than 1 μm and not more than 10 μm.

[0050] Another example of the template 100 according to the present embodiment will be described with reference to FIG. 8A, FIG. 8B, and FIG. 8C. FIG. 8A is a schematic perspective view of a pattern portion 140 formed on the template 100. The pattern portion 140 corresponds to one of the pattern structures 146 shown in FIG. 7A, which is configured to form, for example, eight resist patterns 212 formed on one chip 210 shown in FIG. 6A. The pattern portion 140 is used to form, by transfer, a resist pattern 212 that can be used to form a columnar electrode in a semiconductor device (e.g., a three-dimensional Nand Flash Memory) that is a semiconductor memory having a three-dimensional structure. The resist pattern 212 is used, for example, in a semiconductor memory having a three-dimensional structure, when forming contact electrodes formed in a columnar shape with different heights so as to be wired to each layer of a step-like pattern of a memory layer having a step-like structure formed by stacking multiple layers. FIG. 8A illustrates 96×21 pillars 142 formed on the pattern portion 140 on the template 100. FIG. 8B is a perspective view showing an enlarged portion of the pattern portion 140 shown in FIG. 8A. Fig. 8B shows an enlarged view of 24x21 pillars 142 of pattern portion 140 shown in Fig. 8A. Fig. 8C shows a further enlarged perspective view of a portion of pattern portion 140 shown in Fig. 8B. As shown in Fig. 8C, pattern portion 140 shown with reference to Figs. 8A and 8B has 16 types of pillars 142-1, 142-2, 142-3, 142-4, 142-5, 142-6, 142-7, 142-8, 142-9, 142-10, 142-11, 142-12, 142-13, 142-14, 142-15, and 142-16 having different heights. Pillars 142-1, 142-2, 142-3, 142-4, 142-5, 142-6, 142-7, 142-8, 142-9, 142-10, 142-11, 142-12, 142-13, 142-14, 142-15, and 142-16 are formed in order of height, with pillar 142-1 being the lowest and pillar 142-16 being the highest.

[0051] As shown in Fig. 8B, the pattern unit 140 according to this embodiment has a pattern in which 16 types of pillars shown in Fig. 8C are periodically arranged in a first direction (X direction) and a second direction (Y direction). For example, in the pattern unit 140 shown in Fig. 8B, if the X direction is the row direction of a periodic pattern formed by a plurality of pillars 142, pillars 142-1, 142-2, and 142-3 are periodically arranged in this order in one row. Also, for example, pillars 142-13, 142-14, and 142-15 are periodically arranged in this order in another row.

[0052] The template 100 according to this embodiment can be effectively used to form columnar electrodes of different heights in a semiconductor device such as a three-dimensional memory by the imprint process described above with reference to Figures 4A, 4B, 4C, 5A, 5B, and 5C. At this time, the template 100 is formed with a pattern portion 140 including a plurality of pillar groups 142 of different heights periodically arranged in a first direction (X direction) and / or a second direction (Y direction) intersecting the first direction, as shown in Figures 8A, 8B, and 8C, and by performing an imprint process using such a template 100, a resist pattern 212 can be formed that can be used to form columnar electrodes having different heights by transferring the pillar groups 142.

[0053] In a semiconductor device used as a three-dimensional semiconductor memory, many more pillar electrodes of different heights may be used. In that case, too, the imprint template 100 according to this embodiment can be used to form three-dimensional structures such as pillar electrodes by the above-described imprint process.

[0054] In the example described above with reference to Figures 1A and 1B, the template 100 has pattern portions 140 of four different heights formed therein, but the template 100 of this embodiment may have pattern portions 140 of less than four or five or more different heights formed therein. For example, as described with reference to Figures 8A, 8B, and 8C, the template 100 may have pattern portions 140 of 16 different heights so that resist patterns 240 of 16 different heights are formed, or pattern portions 140 of a number other than 16 different heights may be formed therein.

[0055] The template 100 according to the present embodiment is formed, for example, using a light-transmitting material as described above. The template 100 may be formed, for example, using a glass material such as quartz glass, soda glass, fluorite, calcium fluoride, magnesium fluoride, acrylic glass, or borosilicate glass, or a resin such as polycarbonate, polypropylene, polyethylene, polymethyl methacrylate, or polyethylene terephthalate. The template 100 according to the present embodiment is capable of transmitting light having a wavelength capable of curing the imprint resin (resist R), and, for example, when an ultraviolet curable resin is used as the resist R, it is preferable that the template 100 is capable of transmitting 60% or more of light in a relatively long wavelength region, for example, in the range of 320 nm to 400 nm. From the viewpoint of the curing efficiency of the resist R, a high transmittance is preferable, and it is more preferable that the template 100 has a transmittance of 90% or more of light in the effective wavelength region of the resin to be cured, for example.

[0056] The template 100 according to the present embodiment can be produced by, for example, an imprint method using a master template. The template 100 may be produced by forming a pattern in which the concave-convex pattern of the pattern portion 140 and the shape of the surrounding wall 160 are inverted in the master template, and transferring the master template onto the substrate 120 formed of the above-mentioned light-transmitting material. Alternatively, the master template does not have an inverted shape of the surrounding wall 160, but only has an inverted shape of the concave-convex pattern of the pattern portion 140, and the template 100 may be produced by forming the surrounding wall 160 on a template produced by transferring the master template to a transparent substrate. In this case, for example, the template 100 according to the present embodiment may be produced by adding the structure of the surrounding wall 160 to a conventional imprint template. The surrounding wall 160 may be formed by, for example, a lithography method using the same light-transmitting material as above.

[0057] (Appendix 1) A substrate; a pattern portion having a height equal to or less than a first height and standing on the substrate; a surrounding wall having a height equal to or greater than the first height, standing from the substrate, and surrounding the pattern portion; a resist pattern based on the shape of the pattern portion can be formed on the wafer by pressing the wafer against the resist held in the area surrounded by the surrounding wall and curing the resist while the wafer is pressed against the resist; Template.

[0058] (Appendix 2) The pattern portion includes a plurality of pillars having different heights. The template described in Appendix 1.

[0059] (Appendix 3) the wafer includes a first transfer region in which the shape of the pattern portion is formed, and a second transfer region in which the resist pattern is formed and which is adjacent to the first transfer region with a gap therebetween; The surrounding wall has a first wall portion and a second wall portion spaced apart in a first direction, the first wall portion and the second wall portion are provided such that, when the pattern portion is disposed so as to face the first transferred region, the first wall portion faces the gap portion of the wafer, and, when the template is moved in the first direction and the pattern portion is disposed so as to face the second transferred region, the second wall portion faces the gap portion; The width of the first wall portion is equal to or smaller than the width of the gap portion, The width of the second wall portion is equal to or less than the width of the gap portion. A template as described in Appendix 1 or 2.

[0060] (Appendix 4) The width of the first wall portion in the first direction and the width of the second wall portion in the first direction are 1 μm or more and 10 μm or less. The template described in Appendix 3.

[0061] (Appendix 5) The substrate is optically transparent. 5. A template according to any one of appendices 1 to 4.

[0062] (Appendix 6) the pattern portion includes a shape obtained by inverting a group of pillars in which the plurality of pillars are periodically arranged in a first direction and / or a second direction intersecting the first direction, The template described in Appendix 2.

[0063] (Appendix 7) a template including a substrate, a pattern portion standing on the substrate with a height equal to or less than a first height, and a surrounding wall standing on the substrate with a height equal to or greater than the first height and surrounding the pattern portion; a resist supply unit that supplies a resist to a region of the template that is surrounded by the surrounding wall; a resist pattern forming unit that presses a wafer against the resist held in the area surrounded by the surrounding wall, and hardens the resist while the wafer is pressed against the resist, thereby forming a resist pattern on the wafer based on the shape of the pattern portion; a light source unit that irradiates light from the template opposite to the side against which the wafer is pressed; An imprint apparatus comprising:

[0064] (Appendix 8) a template including a substrate, a pattern portion having a height equal to or less than a first height and standing on the substrate, and a surrounding wall having a height equal to or greater than the first height and standing on the substrate to surround the pattern portion, supplying a resist to an area surrounded by the surrounding wall; pressing the wafer against the resist stored in the region surrounded by the surrounding wall; hardening the resist while the wafer is pressed against the resist, thereby forming a resist pattern on the wafer based on the shape of the pattern portion; A method for manufacturing a semiconductor device.

[0065] (Appendix 9) hardening the resist by exposing the template to light from the side opposite to the side against which the wafer is pressed; The method described in Appendix 8.

[0066] (Appendix 10) the wafer has a main surface on which the resist pattern is to be formed, and an adhesive layer is formed on the main surface before the wafer is pressed against the resist. 10. The method according to claim 8 or 9.

[0067] (Appendix 11) the wafer has a main surface on which the resist pattern is formed, and the resist is applied to the main surface before the wafer is pressed against the resist; exposing the major surface to light; 11. The method according to any one of claims 8 to 10.

[0068] (Appendix 12) the resist is supplied to the region of the template surrounded by the surrounding wall by an inkjet method; 12. The method according to any one of claims 8 to 11.

[0069] (Appendix 13) forming a release layer on the pattern portion, on a region of the substrate other than the pattern portion, and on an inner side of the surrounding wall; 13. The method of any one of claims 8 to 12.

[0070] (Appendix 14) the wafer has a main surface on which the resist pattern is formed, the main surface includes a first transferred region in which the resist pattern is formed, and a second transferred region in which the resist pattern is formed and adjacent to the first transferred region via a gap portion; The surrounding wall of the template has a first wall portion and a second wall portion spaced apart in a first direction, The method comprises: forming the resist pattern in the first transferred region when the template is disposed at a first position that is a position facing the first transferred region of the wafer, and the first wall portion is disposed at a gap portion facing position facing the gap portion; moving the template from the first position in the first direction relative to the wafer to a second position facing the second transferred region, where the second wall portion is disposed at a position facing the gap portion; forming the resist pattern in the second transfer region; 14. The method according to any one of claims 8 to 13.

[0071] The present embodiment has been described above with reference to specific examples. However, the present disclosure is not limited to these specific examples. Any design modifications made by a person skilled in the art to these specific examples are also included within the scope of the present disclosure as long as they have the features of the present disclosure. The elements of each of the above-mentioned specific examples and their arrangements, conditions, shapes, etc. are not limited to those exemplified and can be changed as appropriate. The combination of each of the elements of each of the above-mentioned specific examples can be changed as appropriate as long as no technical contradiction occurs. [Explanation of symbols]

[0072] 100 Imprint Templates 120 Substrate 140 Pattern section 160 Siege Wall 200 wafers 300 Imprinting device 320 Resist Supply Unit 340 Resist Pattern Formation Division 360 Light source section R Resist (imprint resin)

Claims

1. A substrate; a pattern portion having a height equal to or less than a first height and standing on the substrate; a surrounding wall having a height equal to or greater than the first height, standing from the substrate, and surrounding the pattern portion; a resist pattern based on the shape of the pattern portion can be formed on the wafer by pressing the wafer against the resist held in the area surrounded by the surrounding wall and curing the resist while the wafer is pressed against the resist; Template.

2. The pattern portion includes a plurality of pillars having different heights. The template of claim 1 .

3. the wafer includes a first transfer region in which a shape of the pattern portion is formed, and a second transfer region in which the resist pattern is formed and which is adjacent to the first transfer region with a gap therebetween; The surrounding wall has a first wall portion and a second wall portion spaced apart in a first direction, the first wall portion and the second wall portion are provided such that, when the pattern portion is disposed so as to face the first transferred region, the first wall portion faces the gap portion of the wafer, and, when the template is moved in the first direction and the pattern portion is disposed so as to face the second transferred region, the second wall portion faces the gap portion; The width of the first wall portion is equal to or smaller than the width of the gap portion, The width of the second wall portion is equal to or less than the width of the gap portion. The template of claim 1 .

4. a width of the first wall portion in the first direction and a width of the second wall portion in the first direction are 1 μm or more and 10 μm or less; The template of claim 3.

5. The substrate is optically transparent. The template of claim 1 .

6. the pattern portion includes a shape obtained by inverting a group of pillars in which the plurality of pillars are periodically arranged in a first direction and / or a second direction intersecting the first direction, The template of claim 2.

7. a template including a substrate, a pattern portion standing on the substrate with a height equal to or less than a first height, and a surrounding wall standing on the substrate with a height equal to or greater than the first height and surrounding the pattern portion; a resist supply unit that supplies a resist to a region of the template that is surrounded by the surrounding wall; a resist pattern forming unit that presses a wafer against the resist held in the region surrounded by the surrounding wall, and hardens the resist while the wafer is pressed against the resist, thereby forming a resist pattern on the wafer based on the shape of the pattern portion; a light source unit that irradiates light from the template opposite to the side against which the wafer is pressed; An imprint apparatus comprising:

8. a template including a substrate, a pattern portion having a height equal to or less than a first height and standing on the substrate, and a surrounding wall having a height equal to or greater than the first height and standing on the substrate to surround the pattern portion, supplying a resist to an area surrounded by the surrounding wall; pressing a wafer against the resist held in the area surrounded by the surrounding wall; hardening the resist while the wafer is pressed against the resist, thereby forming a resist pattern on the wafer based on the shape of the pattern portion; A method for manufacturing a semiconductor device.

9. hardening the resist by exposing the template to light from the side opposite to the side against which the wafer is pressed; The method according to claim 8.

10. the wafer has a main surface on which the resist pattern is to be formed, and an adhesive layer is formed on the main surface before the wafer is pressed against the resist; The method according to claim 8.

11. the wafer has a main surface on which the resist pattern is formed, and the resist is applied to the main surface before the wafer is pressed against the resist; exposing the major surface to light; The method according to claim 8.

12. the resist is supplied to the region of the template surrounded by the surrounding wall by an inkjet method; The method according to claim 8.

13. forming a release layer on the pattern portion, on a region of the substrate other than the pattern portion, and on an inner side of the surrounding wall; The method according to claim 8.

14. the wafer has a main surface on which the resist pattern is formed, the main surface includes a first transferred region in which the resist pattern is formed, and a second transferred region in which the resist pattern is formed and adjacent to the first transferred region via a gap portion; The surrounding wall of the template has a first wall portion and a second wall portion spaced apart in a first direction, The method comprises: forming the resist pattern in the first transferred region when the template is disposed at a first position that is a position facing the first transferred region of the wafer and where the first wall portion is disposed at a gap portion facing position facing the gap portion; moving the template from the first position in the first direction relative to the wafer to a second position facing the second transferred region, where the second wall portion is disposed at a position facing the gap portion; forming the resist pattern in the second transfer region; The method according to claim 8.

Citation Information

Patent Citations

  • Liquid embossing fabrication of devices with microfeatures

    JP2003509228A

  • Mold and release method of mold

    JP2007320037A

  • Manufacturing method of mold for imprinting

    JP2008238502A

  • Method and apparatus for imprinting substrates

    JP2008509555A

  • Resin pattern formation method

    JP2009034926A