Additional manufacturing condition determination device, additional manufacturing condition determination method, and additional product manufacturing method
By evaluating and optimizing manufacturing conditions for shape and density across intermediate stages of additive manufacturing using machine learning, the apparatus and method ensure the production of structures with desired final shape and density, addressing the limitations of existing techniques.
Patent Information
- Application Number
- JP2023045194
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-22
- Publication Date
- 2024-10-04
- Estimated Expiration
- 2043-03-22
AI Technical Summary
Existing additive manufacturing techniques, such as those described in Patent Document 1, do not adequately consider the shape and density of intermediate structures during the manufacturing process, leading to challenges in achieving desired final product shape and density.
An apparatus and method that determine additive manufacturing conditions by evaluating the shape and density of intermediate structures through lamination, resin curing, degreasing, and sintering stages, using machine learning to optimize manufacturing conditions for both stages, thereby ensuring the final product achieves the desired shape and density.
The solution allows for the efficient and accurate manufacturing of structures with desired shape and density by optimizing manufacturing conditions, reducing the time and cost associated with determining suitable control factors across multiple additive manufacturing steps.
Smart Images

Figure 2024134811000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to an apparatus for determining additive manufacturing conditions, a method for determining additive manufacturing conditions, and a method for manufacturing an additive product. [Background technology]
[0002] Additive manufacturing (layered manufacturing) is known to include, for example, powder bed fusion and directed energy deposition. In powder bed fusion, additive manufacturing is performed by irradiating a light beam (laser beam, electron beam, etc.) onto a flatly spread powder material (e.g., metal powder). Powder bed fusion methods include selective laser melting (SLM) and electron beam melting (EBM). In directed energy deposition, additive manufacturing is performed by controlling the position of a head that irradiates a light beam and ejects powder material. Directed energy deposition methods include laser metal deposition (LMD) and direct metal deposition (DMP).
[0003] Another method is the binder jetting method. In the powder bed fusion method and the directed energy deposition method, an additive manufacturing product (laminated object) is formed by directly melting and solidifying the powder material using a beam as a heat source. On the other hand, in the binder jetting method, a binder is applied to the powder material (e.g., metal powder) according to the shape of the object, which bonds the powder material together. Next, the binder is removed (debinding heat treatment) and then sintering heat treatment is performed to produce a three-dimensional part.
[0004] Metal Injection Molding (MIM) is a manufacturing method similar to the binder injection method. In MIM, metal powder and binder (binding material, plasticizer, lubricant) are pressurized and mixed to produce pellets (compounds). The pellets are then placed in an injection molding machine where they are plasticized by heating, and the MIM material is injection molded into the cavity of the mold. The molded body is called a green part, and the molded body that has been solvent degreased and heated and degreased is called a brown part. Sintering the brown part produces a sintered product called a silver part.
[0005] For additive manufacturing, it is preferable to set manufacturing conditions (recipe) for additive manufacturing appropriate for the conditions of materials, manufacturing equipment, etc. As a technology for determining manufacturing conditions, claim 1 of Patent Document 1 describes "a machine learning device, comprising: a data acquisition unit that acquires first data including shape data representing a target shape of a three-dimensional object and additional shape data representing a target shape of an additional part to be added to the three-dimensional object to suppress deformation of the three-dimensional object during manufacturing; second data regarding deformation of the three-dimensional object; a storage unit that stores a learning dataset including a plurality of the first data and a plurality of the second data; and a learning unit that learns a relationship between the first data and the second data by executing machine learning using the learning dataset." [Prior art documents] [Patent documents]
[0006] [Patent Document 1] Patent Publication No. 2022-021956 Summary of the Invention [Problem to be solved by the invention]
[0007] In the technology described in Patent Document 1, the target shape of the part to be added to the three-dimensional structure is corrected by predicting the manufacturing error of the finally obtained three-dimensional object (paragraph 0051). Therefore, in the technology described in Patent Document 1, the shape and density of the structure (e.g., intermediate structure) in the manufacturing process of the finally obtained three-dimensional structure are not taken into consideration. The problem to be solved by the present disclosure is to provide an apparatus for determining additive manufacturing conditions, a method for determining additive manufacturing conditions, and a method for manufacturing additive manufactured products that are capable of producing structures having desired shapes and density. [Means for solving the problem]
[0008] The additive manufacturing condition determination device of the present disclosure includes a first condition determination unit that determines a first manufacturing condition for lamination and resin hardening to manufacture a first structure having a desired shape and density from the shape and density of a first structure manufactured by lamination and resin hardening performed during additive manufacturing using a binder jetting method, and a second condition determination unit that determines a second manufacturing condition for debinding and sintering to manufacture a second structure having a desired shape and density using the manufactured desired first structure from the shape and density of a second structure manufactured by debinding and sintering performed during additive manufacturing. Other solutions will be described later in the description of the embodiment of the invention. Effect of the Invention
[0009] According to the present disclosure, it is possible to provide an apparatus for determining additive manufacturing conditions, a method for determining additive manufacturing conditions, and a method for manufacturing additive manufactured products that are capable of producing structures having desired shapes and density. [Brief description of the drawings]
[0010] [Figure 1] FIG. 1 is a block diagram of an additive manufacturing condition determination apparatus of the present disclosure. [Diagram 2] FIG. 2 is a perspective view showing the shape of a green part used for evaluation. [Diagram 3] FIG. 2 is a perspective view showing the shape of a silver part used for evaluation. [Figure 4]1 is a flowchart illustrating an additive manufacturing method of the present disclosure. [Diagram 5] FIG. 2 is a block diagram showing the hardware configuration of the additive manufacturing condition determination device of the present disclosure. [Figure 6] 1 is a flowchart showing the first stage of the additive manufacturing condition determination method of the present disclosure. [Figure 7] 1 is a flowchart showing the latter stage of the additive manufacturing condition determination method of the present disclosure. [Figure 8A] FIG. 1 is a schematic diagram of an additive manufacturing apparatus of the present disclosure viewed from the side. [Figure 8B] FIG. 1 is a schematic diagram of an additive manufacturing apparatus of the present disclosure viewed from above. [Figure 9A] FIG. 13 is a schematic diagram showing an example of a powder-laying operation. [Figure 9B] FIG. 13 is a schematic diagram showing an example of a powder-laying operation. [Figure 9C] FIG. 13 is a schematic diagram showing an example of a powder-laying operation. [Figure 9D] FIG. 13 is a schematic diagram showing an example of a powder-laying operation. [Figure 10A] FIG. 4 is a schematic diagram showing an example of a coating operation. [Figure 10B] FIG. 4 is a schematic diagram showing an example of a coating operation. [Figure 11] FIG. 11 is a diagram illustrating an example of a drying operation. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] Hereinafter, a form for carrying out the present disclosure (referred to as an embodiment) will be described with reference to the drawings. In the following description of one embodiment, other embodiments applicable to the one embodiment will also be described as appropriate. The present disclosure is not limited to the following one embodiment, and different embodiments can be combined with each other or modified as desired without significantly impairing the effects of the present disclosure. In addition, the same symbols will be used for the same members, and duplicate descriptions will be omitted. Furthermore, the same names will be used for members having the same functions. The contents shown are merely schematic, and for the sake of illustration, changes may be made from the actual configuration within a range that does not significantly impair the effects of the present disclosure, and some members may be omitted or modified between drawings. In addition, the same embodiment does not necessarily need to have all the configurations.
[0012] 1 is a block diagram of an additive manufacturing condition determination apparatus 100 of the present disclosure. Also shown in FIG. 1 are an additive manufacturing apparatus 200, an input device 300, and an output device 400.
[0013] Additive manufacturing using binder jetting involves four main processes: lamination (powder laying, binder application and drying), resin curing, degreasing and sintering. The green part, which is an intermediate structure, is produced by lamination and resin curing. The silver part, which is the final structure, is produced by degreasing and sintering the intermediate structure.
[0014] To optimize each of these processes, it is preferable to evaluate the quality of the product (obtained structure) in each process. However, evaluation of the product itself may be difficult due to circumstances such as the state of the product and the convenience of the process. Therefore, in the example of the present disclosure, the dimensions, mass, density, etc. of the green part (intermediate structure), which is the molded product after the resin has hardened and before degreasing, are measured. Furthermore, the dimensions, weight, density, etc. of the silver part (final structure), which is the molded product after the sintering process, are also measured.
[0015] For example, debinding of the green part reduces the density of the green part by about 55% to 65%, and the bond becomes loose. Note that a density of 100% is defined as a state in which the powder material (e.g., metal powder) used in additive manufacturing is densely packed. The final density of the silver part is improved to about 95% to 99% compared to the green part after debinding. Thus, during additive manufacturing, a large shrinkage deformation occurs, for example, in the powder metallurgy bonding process. For this reason, the shrinkage rate, anisotropy, and density change caused by, for example, sintering the green part affect the accuracy of the final shape of the silver part. Therefore, as disclosed herein, it is preferable to evaluate the shape and density of the green part manufactured during the manufacturing process of the silver part.
[0016] The determination device 100 determines the manufacturing conditions during additive manufacturing in an additive manufacturing device 200 that performs additive manufacturing by a binder jetting method. The manufacturing conditions include first manufacturing conditions during lamination and resin hardening, and second manufacturing conditions during degreasing and sintering. The manufacturing conditions include a large number of parameters (control factors described later). The parameters may also vary depending on the metal material used, the specifications of the additive manufacturing device 200, and the shape and density of the desired final structure (silver part). For this reason, it is not easy to consider appropriate parameters and determine manufacturing conditions each time manufacturing is performed. Therefore, by using the determination device 100, it is possible to search for appropriate manufacturing conditions and determine the manufacturing conditions.
[0017] The determination device 100 includes a first condition determination unit 101, a first learning unit 102, a second condition determination unit 103, and a second learning unit 104.
[0018] The first condition determination unit 101 determines the first manufacturing conditions from the shape and density of the first structure manufactured by lamination and resin curing performed during additive manufacturing using the binder jetting method. The first manufacturing conditions are manufacturing conditions during lamination and resin curing for manufacturing a first structure having a desired shape and density, as described above. The first structure is a structure (intermediate structure) obtained in the manufacturing process of a second structure described below. By providing the first condition determination unit 101, it is possible to determine the manufacturing conditions for the first structure having a desired shape and density.
[0019] The first condition determination unit 101 determines, as the first manufacturing conditions, the manufacturing conditions when manufacturing a first structure in which the dimensional difference and density difference from the desired shape are both within a predetermined range. The shape and density of the actually manufactured first structure are compared with the desired shape and density, and if the difference is within a predetermined range, it can be determined that the manufactured first structure is close to the desired first structure. The difference here is the dimensional difference between corresponding sides in the case of shape, and the density difference in the case of density. Therefore, the first condition determination unit 101 can determine the manufacturing conditions when such a first structure can be manufactured as the first manufacturing conditions when manufacturing a first structure having a desired shape and density.
[0020] The predetermined range here refers to an allowable difference in size and density that is expected due to lamination and resin curing. Specific values of the predetermined range can be determined, for example, by experiment.
[0021] Fig. 2 is a perspective view showing the shape of the green part 30 used in the evaluation. The green part 30 is manufactured as a first structure under, for example, initially set first manufacturing conditions, and the first condition determination unit 101 determines the first manufacturing conditions using the manufacturing conditions, the shape and density of the green part 30, etc. Therefore, the green part 30 shown in Fig. 2 is a structure manufactured for determining the first manufacturing conditions.
[0022] The green part 30 (first structure) includes a plurality of unit structures 31, 32, and 33 that are different in volume but have the same shape. Therefore, the unit structures 31, 32, and 33 have a similar relationship. The unit structures 31, 32, and 33 each have three types of block shapes: large, medium, and small. The block shapes have sides that are formed by straight lines. The block shapes make it easier to measure the length of each side, and make it easier to calculate the dimensional difference. In the illustrated example, the unit structures 31, 32, and 33 are all cubes. By using cubes, the dimensions in each direction of the x, y, and z axes can be measured, and the shrinkage in each direction due to lamination, etc. can be evaluated. In addition, the effects of temperature distribution due to differences in volume, thermal stress due to temperature distribution, and the effects of uneven processing can be evaluated. However, the shapes are not limited to cubes.
[0023] The green part 30 further includes a unit structure 34. The unit structure 34 includes a support portion 341 and a pin-shaped portion 342 standing upright from the support portion 341. Thus, the green part 30 includes the pin-shaped portion 342. As described above, the green part 30 is manufactured by stacking powder material and curing the resin. Therefore, if the powder material has an elongated shape like the pin-shaped portion 342, it is difficult to stack the powder material. Even if the powder material can be stacked, it is brittle and easily crumbles, and is therefore easily damaged. Therefore, the pin-shaped portion 342 is included in order to determine and eliminate the first manufacturing condition that causes such a phenomenon.
[0024] The shape of the pin-shaped portion 342 (columnar portion) is not limited, but for example, it can be a columnar shape with a length (width) of, for example, 1 mm to 2 mm in the direction in which the powder material is laid (direction perpendicular to the stacking direction). The column may be a circular cylinder, an elliptical cylinder, or a rectangular cylinder.
[0025] Returning to FIG. 1, the first condition determination unit 101 further determines, as the first manufacturing condition, the manufacturing condition under which the density differences in the unit structures 31, 32, and 33 (FIG. 2) are all within a predetermined range. For example, when the unit structures 31, 32, and 33 are laminated and resin cured, the density of each of the unit structures 31, 32, and 33 decreases below the density when the structure in which the powder material is densely present is taken as 100%. However, the degree of decrease may differ for each of the unit structures 31, 32, and 33 because the shapes are the same but the volumes are different as described above. Therefore, by determining, as the first manufacturing condition, the manufacturing condition under which the density differences in the unit structures 31, 32, and 33 are all within a predetermined range, it is possible to determine the first manufacturing condition under which the density change is the same regardless of the volume. This makes it possible to suppress the density change regardless of the volume of the first structure and the second structure.
[0026] The predetermined range here is an allowable density difference that is assumed to occur due to lamination and resin hardening. The specific numerical value of the predetermined range can be determined, for example, by experiment. In addition, it is preferable that the density differences of the unit structures 31, 32, and 33 are approximately the same for the reasons described above.
[0027] The first learning unit 102 performs machine learning using the first manufacturing conditions, the shape of the intermediate structure, and the density of the intermediate structure as feature quantities. By providing the first learning unit 102, the evaluation results of the first structure linked to lamination and resin curing can be constructed as a database of learning conditions. The shape here refers to, for example, the dimensions of the sides forming the first structure. The machine learning can perform, for example, supervised learning using the first manufacturing conditions as the objective variable and the shape and density of the first structure as the explanatory variables. However, the machine learning is not limited to supervised learning, and can be either unsupervised learning or reinforcement learning. For example, Bayesian optimization, kernel ridge regression analysis, etc. can be used as the machine learning algorithm.
[0028] The second condition determination unit 103 determines the second manufacturing conditions from the shape and density of the second structure manufactured by debinding and sintering performed during additive manufacturing. The second manufacturing conditions are manufacturing conditions during debinding and sintering for manufacturing a second structure having a desired shape and density using the manufactured desired first structure. The second condition determination unit 103 can determine the manufacturing conditions for manufacturing a second structure (final structure, final product) having a desired shape and density from a first structure having a desired shape and density.
[0029] The second condition determination unit 103, like the first condition determination unit 101, determines the manufacturing conditions when manufacturing a second structure in which the dimensional difference and density difference from the desired shape are both within a predetermined range as the second manufacturing conditions. The shape and density of the actually manufactured second structure are compared with the desired shape and density, and if the difference is within a predetermined range, it can be determined that the shape and density of the manufactured second structure are close to the desired second structure. The difference here is the dimensional difference between corresponding sides in the case of shape, and the density difference in the case of density. Therefore, the second condition determination unit 103 can determine the manufacturing conditions when such a second structure can be manufactured as the second manufacturing conditions when manufacturing a second structure having a desired shape and density.
[0030] The predetermined range here refers to an allowable difference in size and density that is expected to occur due to debinding and sintering. Specific values of the predetermined range can be determined, for example, by experiment.
[0031] Fig. 3 is a perspective view showing the shape of the silver parts 40 used in the evaluation. The silver parts 40 are manufactured as a second structure under, for example, initially set second manufacturing conditions, and the second condition determination unit 103 determines the second manufacturing conditions using the manufacturing conditions, the shape and density of the silver parts 40, etc. Therefore, the silver parts 40 shown in Fig. 3 are structures manufactured for determining the second manufacturing conditions.
[0032] The silver part 40 (second structure) includes a plurality of unit structures 41, 42, 43 that are different in volume but have the same shape. Therefore, the unit structures 41, 42, 43 have a similar relationship. The unit structures 41, 42, 43 each have three types of block shapes, large, medium, and small. Therefore, the above-mentioned green part 30 and silver part 40 have a block shape. The block shape has sides formed by straight lines. The block shape makes it easy to measure the length of each side, and makes it easy to calculate the dimensional difference. In the illustrated example, the unit structures 41, 42, 43 are all cubes. By using a cube, the dimensions in each direction of the x, y, and z axes can be measured, and the shrinkage in each direction due to lamination, etc. can be evaluated. In addition, the effects of temperature distribution due to differences in volume, thermal stress due to temperature distribution, and the effects of uneven processing can be evaluated. However, the shape is not limited to a cube.
[0033] The silver part 40 further includes a unit structure 44. The unit structure 44 includes a main body 441 having an overhanging shape, and a support 442 that supports the lower side (stacking direction) of the main body 441. Therefore, the silver part 40 has an overhanging shape. An overhanging shape is a shape in which there is nothing below in the stacking direction. The bonds of an overhanging shape are weakened by debinding, and the shape is prone to deformation due to its own weight during the process of raising the temperature to the sintering temperature. This can result in a large change in shape. Therefore, by using the unit structure 44, the impact of such changes can be evaluated.
[0034] It is possible that the self-weight deformation of the overhang can be somewhat suppressed by adjusting the heating rate, etc. However, in the example of the present disclosure, it is preferable to consider the case on the premise that the self-weight deformation will occur and to provide supports 442. Therefore, supports 442 are also used in the unit structure 44 used as a prototype.
[0035] Returning to FIG. 1, the second condition determination unit 103 further determines, as the second manufacturing condition, the manufacturing condition under which the density differences in the unit structures 41, 42, and 43 (FIG. 3) are all within a predetermined range. For example, when the unit structures 41, 42, and 43 are stacked and degreased, the density of each of the unit structures 41, 42, and 43 decreases below the density when the structure in which the powder material is densely present is taken as 100%. However, the degree of decrease may differ for each of the unit structures 41, 42, and 43 because the unit structures have the same shape but different volumes as described above. Therefore, by determining, as the second manufacturing condition, the manufacturing condition under which the density differences in the unit structures 41, 42, and 43 are all within a predetermined range, it is possible to determine the second manufacturing condition under which the density change is the same regardless of the volume. This makes it possible to suppress the density change regardless of the volume of the first structure and the second structure.
[0036] The second learning unit 104 performs machine learning using the second manufacturing conditions, the shape of the second structure, and the density of the second structure as feature quantities. By providing the second learning unit 104, the evaluation results of the second structure linked to debinding and sintering can be constructed as a database of learning conditions. The shape here refers to, for example, the dimensions of the sides forming the second structure. The machine learning can perform, for example, supervised learning using the second manufacturing conditions as the objective variable and the shape and density of the final structure as the explanatory variables. However, the machine learning is not limited to supervised learning, and can be either unsupervised learning or reinforcement learning. For example, Bayesian optimization, kernel ridge regression analysis, etc. can be used as the machine learning algorithm.
[0037] The second learning unit 104 performs machine learning by using, as second manufacturing conditions, manufacturing conditions determined by applying a desired shape and density to a thermal deformation analysis model using the thermal properties of the first structure and the shape and density of the second structure. This makes it possible to calculate the shape and density of the second structure using the thermal deformation analysis model and the thermal properties (e.g., linear expansion coefficient, etc.) of the first structure without actually performing debinding and sintering. Then, machine learning can be performed using the calculated shape and density of the second structure, so that learning opportunities in machine learning can be increased.
[0038] Sintering in particular is a time-consuming process. For this reason, it may take a long time to converge if all conditions are evaluated using experimental methods. Therefore, by performing a thermal deformation analysis using the thermal properties of the first structure and the shape and density of the second structure, which are linked to the sintering conditions obtained by initial learning, and fitting them, it is possible to analyze the second manufacturing conditions and increase the learning opportunities.
[0039] The additive manufacturing apparatus 200 performs additive manufacturing by the binder jetting method as described above. Specific details of the additive manufacturing apparatus 200 will be described later with reference to FIG. 8A and subsequent figures. The additive manufacturing apparatus 200 performs additive manufacturing based on the first manufacturing conditions and the second manufacturing conditions determined by the determination apparatus 100, for example.
[0040] Information regarding the shapes and densities of the first and second structures obtained by additive manufacturing, information regarding the thermal property values of the intermediate structure, etc. are input to the determination device 100 via the input device 300, for example, by a user. The input device 300 is, for example, a keyboard, a mouse, etc. The first and second manufacturing conditions determined by the determination device 100 are output to the output device 400 as appropriate. The output device 400 is, for example, a monitor, a display, a printer, etc.
[0041] The determined first and second manufacturing conditions are manufacturing conditions corresponding to, for example, the properties of the powder material, the properties (functions, specifications, etc.) of the additive manufacturing apparatus 200 used, and the shape and density of the final structure that is the desired second structure. Therefore, by performing additive manufacturing using the additive manufacturing apparatus 200 assumed at the time of determining the conditions under the determined first and second manufacturing conditions, a structure having a desired shape and density can be manufactured.
[0042] 4 is a flowchart showing the additive manufacturing method of the present disclosure. The additive manufacturing method of the present disclosure includes a first condition determination step S101, a second condition determination step S102, and an additive manufacturing step S103.
[0043] The first condition determination step S101 is a step of determining the first manufacturing conditions from the shape and density of the first structure manufactured by lamination and resin curing performed during additive manufacturing by the binder jet method. The first manufacturing conditions are manufacturing conditions during lamination and resin curing for manufacturing a first structure having a desired shape and density, as described above. The first condition determination step S101 can be executed by the first condition determination unit 101 (FIG. 1). The second condition determination step S102 is a step of determining the second manufacturing conditions from the shape and density of the second structure manufactured by debinding and sintering performed during additive manufacturing. The second manufacturing conditions are manufacturing conditions during debinding and sintering for manufacturing a second structure having a desired shape and density using the manufactured desired first structure, as described above. The second condition determination step S102 can be executed by the second condition determination unit 103 (FIG. 1). The first learning step by the first learning unit 102 and the second learning step by the second learning unit 104 may be performed as appropriate.
[0044] The additive manufacturing step S103 is a step of manufacturing a structure using the first manufacturing conditions determined in the first condition determination step S101 and the second manufacturing conditions determined in the second condition determination step S102. The structure referred to here is preferably one that has the conditions used when the first manufacturing conditions and the second manufacturing conditions were determined. In addition, it is preferable that the additive manufacturing device 200 (FIG. 1) used for additive manufacturing also has the conditions used when the first manufacturing conditions and the second manufacturing conditions were determined. According to the manufacturing method of the present disclosure, an additive manufactured product (a layered object, a molded object, a structure) having a desired shape and density can be manufactured.
[0045] The determination of the manufacturing conditions and the additive manufacturing may be performed at the same location or at different locations. In the latter case, for example, the manufacturing conditions may be determined at point A, and additive manufacturing may be performed at point B using the determined first and second manufacturing conditions. In this case, it is preferable to determine the manufacturing conditions at point A after obtaining in advance the specifications, characteristics, etc. of the additive manufacturing apparatus 200 to be used at point B. In this way, for example, the first and second manufacturing conditions that match the specifications, characteristics, etc. of the additive manufacturing apparatus 200 installed at the remote point B can be determined by a user at point A and provided to a manufacturer at point B.
[0046] 5 is a block diagram showing a hardware configuration of an additive manufacturing condition determination device 100 according to the present disclosure. The determination device 100 is configured to include, for example, a CPU (Central Processing Unit) 1001, a RAM (Random Access Memory) 1002, and a ROM (Read Only Memory) 1003. The determination device 100 is realized by a predetermined control program (for example, a method for determining additive manufacturing conditions) stored in the ROM 1003 being loaded into the RAM 1002 and executed by the CPU 1001.
[0047] FIG. 6 is a flow chart showing the first stage of the additive manufacturing condition determination method of the present disclosure. The additive manufacturing condition determination method of the present disclosure includes steps S1 to S9. FIG. 6 mainly shows an example of a method for exploring both the lamination and resin curing processes to evaluate the performance of the green part. The performance of the green part can be controlled by a "first control factor" which will be described below with reference to FIG. 6. Therefore, the first manufacturing condition during lamination and resin curing is the first control factor that is appropriately set. The flow shown in FIG. 6 can be executed by the first condition determination unit 101 and the first learning unit 102 (both of which are shown in FIG. 1).
[0048] The first control factors during lamination include the material, particle size, particle size distribution, and binder material of the powder material. However, since these are materials used by end users, it is preferable that these first control factors are fixed factors. Other first control factors include the lamination thickness for each layer, the supply amount of powder material (output, time, etc. of the vibration mechanism 11 described later), the powder spreading speed (movement speed of the powder spreading mechanism 4 described later), leveling settings (roller rotation speed, etc.), the binder application amount (inkjet output from the application mechanism 5 described later, inkjet interval, etc.), drying (output, time, etc. of the heater 13 described later), etc. Among them, the finish of the green part is particularly influenced by these first control factors. Other first control factors may include the supply speed of the powder material, etc.
[0049] The primary control factors during resin curing include the temperature step of the heat treatment (how many steps the temperature is increased), the rate of temperature increase, the treatment temperature, and the holding time.
[0050] In order to optimize both the lamination and resin curing processes, first, in the lamination process, the first control factors are assigned and allocated, and an initial first control factor group (initialized lamination recipe group) is set (step S1). The initial first control factor group is a group of initial conditions for the predetermined first control factors. The initial first control factor group includes, for example, 10 to 20 manufacturing conditions (parameter sets) in total by changing each of the first control factors during the lamination.
[0051] Next, lamination and drying are performed using the initial first control factor group (steps S2 and S3). Furthermore, in the resin curing process, an initial first control factor group (initial setting curing recipe group) is set by allocating and assigning the first control factors (step S4). The initial first control factor group set here also includes, for example, 10 to 20 manufacturing conditions (parameter sets) in total by changing each of the first control factors during the resin curing. The green part is controlled by curing the resin using each initial first control factor group (step S5).
[0052] The total number of first control factors (number of recipes) during lamination and resin hardening is the product of the number of lamination recipes and the number of hardening recipes, and the number of evaluations may be enormous. Here, in the resin hardening process, the processing temperature is roughly determined by the resin material. Therefore, it is preferable to first fix the heating rate and the number of steps, and roughly determine the processing temperature and processing time. The lamination recipe group may be set using an experimental design method, or by determining the range based on other material recipes that use materials similar to the metal material used when determining the conditions.
[0053] In order to evaluate the quality of the green parts, it is preferable to manufacture and evaluate a plurality of green parts using one recipe, as described above. The plurality of green parts used are, for example, the green parts 30 described with reference to FIG.
[0054] The shape, mass, and density of the green part manufactured using the initially set lamination recipe group and curing recipe group are measured (step S6). The density may be calculated instead of measured. For the manufactured green part, manufacturing conditions close to the target shape are extracted as described with reference to FIG. 2 above, and among these recipes, manufacturing conditions with high density and small density difference due to volume difference (large, medium, and small in FIG. 2 above) are determined as first manufacturing conditions.
[0055] If any of the green parts meet the target in the measurement evaluation, the first manufacturing conditions are determined and both the lamination and resin curing processes can be completed (YES in step S7). However, if the target is not met or if there is a need to check for further improvement (NO in step S7), the initial lamination recipe and curing recipe, as well as the evaluation results of the shape and density of the green parts obtained using these recipes, are stored in a database of learning conditions and machine learning can be performed as described above (step S8). This allows an appropriate combination to be derived.
[0056] After the machine learning in step S7, a new stacking recipe and a new curing recipe are proposed by machine learning (step S9). Step S1 and the following steps are performed again according to the newly proposed stacking recipe and the newly proposed curing recipe.
[0057] The above steps S1 to S9 are first condition determination steps for determining the first manufacturing conditions from the shape and density of the first structure manufactured by lamination and resin curing performed during additive manufacturing using the binder jetting method. The first manufacturing conditions are the manufacturing conditions during lamination and resin curing for manufacturing the first structure having the desired shape and density, as described above.
[0058] FIG. 7 is a flow chart showing the latter part of the additive manufacturing condition determination method of the present disclosure. The additive manufacturing condition determination method of the present disclosure includes steps S11 to S19. The flow shown in FIG. 7 is executed following the flow shown in FIG. 6 above. FIG. 7 mainly shows an example of a method for exploring both degreasing and sintering processes to evaluate the performance of the silver parts. The performance of the silver parts can be controlled by a "second control factor" described below with reference to FIG. 7. Therefore, the second manufacturing conditions during degreasing and sintering are the appropriately set second control factors. The flow shown in FIG. 7 can be executed by the second condition determination unit 103 and the second learning unit 104 (both in FIG. 1).
[0059] The second control factors during debinding include the treatment atmosphere, heating rate, treatment temperature, treatment time (holding time), etc. The second control factors during sintering include the treatment atmosphere, temperature step, heating rate, sintering temperature, holding time, etc.
[0060] In order to optimize both the debinding and sintering processes, first, a green part is produced using the first manufacturing conditions determined with reference to FIG. 6 above, and the produced green part is subjected to simultaneous differential thermal analysis (TG / DTA) (step S11). Data analysis of simultaneous differential thermal analysis reveals the temperature range where mass change occurs due to binder loss, and the debinding process temperature (an example of a debinding recipe) can be determined. By maintaining the temperature range where mass change occurs during debinding, it is possible to suppress damage to the green part caused by too high a temperature and insufficient binder removal caused by too low a temperature. This allows the binder to be sufficiently removed, and a brown part can be produced.
[0061] The degreasing process time (an example of a degreasing recipe) can be set, for example, with reference to the binder removal time calculated by a predetermined algorithm based on the record of the thermal mass change. The predetermined algorithm can use, for example, a predetermined formula that associates the process temperature and the rate of change of the temperature (an example of a degreasing recipe) during heating.
[0062] In addition, the thermal property values of the produced green parts, such as the linear expansion coefficient, are measured (step S12). The thermal property values here are physical property values that affect at least one of the shape and density of the sintered silver parts due to the heating caused by debinding and sintering.
[0063] Next, the produced green part is degreased (step S13).
[0064] After debinding, a group of initial second control factors (a group of sintering recipes initially set) is set to optimize sintering (step S14). The group of initial second control factors is a group of initial conditions for predetermined second control factors. The group of initial second control factors includes, for example, 10 to 20 manufacturing conditions (parameter sets) by changing each of the second control factors during sintering. Sintering is performed with the initial second control factors as the second manufacturing conditions (step S15). The shape, mass, and density of each silver part obtained by sintering are measured (step S16). The density may be calculated instead of measured.
[0065] In order to evaluate the quality of the silver parts, it is preferable to manufacture and evaluate a plurality of silver parts according to one recipe, as described above. The plurality of silver parts used are, for example, the silver parts 40 described with reference to FIG.
[0066] The shape, mass, and density of the silver parts manufactured using the initially set debinding recipe group and sintering recipe group are measured (step S16). The density may be calculated instead of measured. For the manufactured silver parts, manufacturing conditions close to the target shape are extracted as described with reference to Fig. 3 above, and among these recipes, manufacturing conditions with high density and small density difference due to volume difference (large, medium, and small in Fig. 3 above) are determined as second manufacturing conditions.
[0067] If any of the silver parts meet the target in the measurement evaluation, the second manufacturing conditions are determined and both the debinding and sintering processes can be completed (YES in step S17). However, if the target is not met or if there is further prospect for improvement (NO in step S17), the initial debinding recipe and sintering recipe, as well as the evaluation results of the shape and density of the silver parts obtained using these, are stored in a database of learning conditions and machine learning is performed as described above (step S18). This makes it possible to derive an appropriate combination. The data used for the machine learning in step S18 may be data obtained by thermal deformation analysis as described above.
[0068] After the machine learning in step S18, new debinding and sintering recipes are proposed by machine learning (step S19). Steps S12 and after are performed again according to the newly proposed debinding and sintering recipes.
[0069] The above steps S11 to S19 are second condition determination steps for determining second manufacturing conditions from the shape and density of the second structure manufactured by debinding and sintering performed during additive manufacturing. The second manufacturing conditions are manufacturing conditions during debinding and sintering for manufacturing a second structure having a desired shape and density using the desired first structure manufactured as described above.
[0070] According to the above-described determination device 100 and determination method, additive manufacturing is performed under the determined first and second manufacturing conditions, thereby making it possible to manufacture a structure (final structure) having a desired shape and density. In particular, additive manufacturing using a binder jetting method involves multiple manufacturing processes and a wide variety of control factors, such as the first control factor and the second control factor. For this reason, it is not easy to determine suitable control factors. In order to determine suitable manufacturing conditions, a large number of molded objects are manufactured and evaluated. For this reason, constructing a recipe, which is the manufacturing conditions for each process, requires huge costs and time.
[0071] In contrast, in the above-mentioned powder bed fusion, there is a method of using machine learning to compare control factors and modeling results, and performing regression analysis to optimize. However, even if this method is applied to the binder jet method, the binder jet method requires processing time to evaluate the recipe through a series of processes of additive manufacturing conditions. For this reason, it still takes a long time to evaluate, and the number of evaluations increases, and the analysis does not converge to the search for appropriate conditions when the results of the previous process are poor. Therefore, according to the determination device 100 and determination method disclosed herein, the manufacturing conditions are determined by dividing them into first and second manufacturing conditions, so that the time and labor required for determination can be reduced and the determination can be made efficiently. In other words, by dividing the search for additive manufacturing conditions in the binder powder method into multiple parts, the efficiency of optimization can be improved.
[0072] FIG. 8A is a schematic diagram of the additive manufacturing apparatus 200 of the present disclosure, viewed from the side. FIG. 8B is a schematic diagram of the additive manufacturing apparatus 200 of the present disclosure, viewed from above. The additive manufacturing apparatus 200 applies a binder to the powder material (powder bed 3) laid in layers and dries it to bind the metal powder. The binder is, for example, a solution containing a resin. The binder may further contain additives such as a surfactant and a viscosity modifier in addition to the resin and organic solvent. The powder material is, for example, a powder of a metal material such as hot work tool steel, copper, a titanium alloy, a nickel alloy, an aluminum alloy, a cobalt chromium alloy, or stainless steel, a powder of a resin material such as polyamide, or a powder of ceramics. The additive manufacturing apparatus 200 forms a three-dimensional structure of the metal powder bound by the binder in the modeling layer 2 by repeating the formation of the powder bed 3, the application of the binder, and the drying in this order.
[0073] The fluidity of metal powder changes depending on the humidity. For this reason, the moisture can be removed and humidity can be controlled by heating the parts that come into contact with the powder material, such as the powder supply mechanism 10, the leveling mechanism 12, the powder spreading mechanism 4, and the modeling layer 2, which will be described later.
[0074] A space that functions as a collection section 20 is formed around the modeling layer 2. Excess powder falls into the collection section 20 as the powder-laying mechanism 4 performs the powder-laying operation. The powder collected in the collection section 20 is reclassified using a sieve and reused for modeling.
[0075] The additive manufacturing apparatus 200 includes a modeling layer 2, a powder-laying mechanism 4, a coating mechanism 5 that applies a binder, a supply mechanism 6 that supplies the binder to the coating mechanism 5, a chamber 7, and a lifting mechanism 8 that raises and lowers the modeling layer 2. The additive manufacturing apparatus 200 further includes a monitoring device 9 that monitors the operation and control of the additive manufacturing apparatus 200. The monitoring device 9 can have the same hardware configuration as the determining device 100 shown in FIG. 7 above, for example. The chamber 7 houses each mechanism of the additive manufacturing apparatus 200 except for the monitoring device 9 and the supply mechanism 6. However, the chamber 7 may also house the monitoring device 9 and the supply mechanism 6.
[0076] The modeling area 21 is composed of a modeling layer 2 and a bottom plate 22. The bottom plate 22 is fixed to a lifting mechanism 8, and the vertical position of the bottom plate 22 changes according to the operation of the lifting mechanism 8.
[0077] The powder-laying mechanism 4, all of which will be described later with reference to Figure 9A etc., comprises a powder supplying mechanism 10, a vibration mechanism 11, a leveling mechanism 12, a heater 13, and a drive mechanism (not shown) that moves the powder-laying mechanism 4. The heater 13 does not necessarily have to be provided.
[0078] The application mechanism 5 includes a binder head 51, which will be described later, and a drive mechanism (not shown) that moves the binder head 51. The binder is supplied from the supply mechanism 6 to the binder head 51 through a pipe (not shown), and the supplied binder is discharged from the binder head 51.
[0079] Figures 9A, 9B, 9C, and 9D are schematic diagrams showing an example of the powder-laying operation. The powder-laying operation is performed in the order of the operations shown in Figures 9A, 9B, 9C, and 9D. The powder-laying operation is a part of the lamination process, and is preferably performed under conditions included in the first manufacturing conditions.
[0080] First, the outline of the powder-laying mechanism 4 will be described. The powder-laying mechanism 4 vibrates the powder supply mechanism 10 with the vibration mechanism 11 to drop the powder onto the modeling layer 2. Furthermore, the powder-laying mechanism 4 moves, and the powder is laid in the modeling layer 2 via the leveling mechanism 12, forming the powder bed 3. Although not shown, the powder supply mechanism 10 may be provided in a concave shape on the inner bottom of the chamber 7 (FIG. 8A) independent of the powder-laying mechanism 4, with the top open and an opening at the top end. In this case, it is preferable that the powder supply mechanism 10 has a stage that can be moved up and down for placing and supplying the powder material. This stage constitutes the bottom wall of the powder supply mechanism 10, and is provided so as to be able to be raised and lowered at a predetermined pitch by an appropriate lifting mechanism (not shown).
[0081] Next, the powder spreading operation using the powder spreading mechanism 4 will be described. The powder spreading operation is started by moving the powder spreading mechanism 4 onto the modeling layer 2, for example, as shown by the thick solid arrow in Figures 9A to 9D. As shown in Figure 9A, the powder spreading mechanism 4 vibrates the powder supply mechanism 10 by the vibration of the vibration mechanism 11 on the modeling layer 2, thereby dropping the powder material to be supplied. As shown in Figure 9B, the powder spreading mechanism 4 drops the powder material while moving, so that the powder is spread onto the modeling layer 2. As shown in Figure 9C, the leveling mechanism 12 acts on the spread powder by the movement of the powder spreading mechanism 4, and the powder bed 3 is formed by leveling the ground. The leveling mechanism 12 is a blade, roller, etc. that adjusts the height level of the powder bed 3. In the case of a roller, the powder bed 3 can be formed by compressing it by moving the powder spreading mechanism 4 while rotating the roller. As shown in Figure 9D, the excess powder material falls from the modeling layer 2.
[0082] 10A and 10B are schematic diagrams showing an example of a coating operation. The coating operation is a part of the lamination process, and is preferably performed under conditions included in the first manufacturing conditions. As shown in FIG. 10A, the binder is applied to the powder bed 3 formed on the modeling layer 2 in accordance with a two-dimensional planar shape corresponding to one layer of the modeled product (green part). The coating is performed continuously by inkjet from a coating mechanism 5 that moves as shown by the thick solid arrow in FIGS. 10A and 10B.
[0083] FIG. 11 is a diagram showing an example of the drying operation. The drying operation is a part of the lamination process, and is preferably performed under conditions included in the first manufacturing conditions. The applied binder can be dried by, for example, heating a heater 13 moving in the direction shown by the thick solid arrow and passing it over the powder bed 3. Alternatively, drying may be performed simultaneously with the application of the binder by continuously heating the modeling layer 2 or the bottom surface of the modeling layer 2 with the heater 13.
[0084] 9A to 11 are repeated to form a three-dimensional shape of an object in the modeling layer 2 (FIG. 8A). The modeling layer 2 is then placed in a thermostatic chamber (not shown) at a temperature range of approximately 100°C to 300°C for several hours to several tens of hours, whereby the binder hardens. This allows a green part to be extracted from the powder in the modeling layer 2.
[0085] The removed green parts are degreased by being held in a constant temperature bath or heat treatment furnace (neither shown) at a temperature range of about 400°C to 600°C for several hours to several tens of hours. This removes the binder and gives brown parts. Degreasing is preferably carried out under conditions included in the second manufacturing conditions. In the brown parts, the bonds between the powder materials have been weakened by the removal of the binder, so the shape is easily distorted and care must be taken when handling them.
[0086] The brown parts are sintered by being held in a vacuum furnace or a heat treatment furnace in a vacuum atmosphere (neither shown) at a temperature range from below the melting point to approximately 80% of the melting point for several hours to several tens of hours. The powder particles of the brown parts are metallically bonded together by sintering, resulting in a sintered body, a silver part. The sintering is preferably performed under conditions included in the second manufacturing conditions. Note that degreasing and sintering may be performed collectively in the same furnace.
[0087] Brown parts may deform under their own weight when exposed to high temperatures during sintering. Therefore, in the parts with the above-mentioned overhanging shapes, supports or other supports are manufactured at the same time, as described above, to suppress deformation during sintering. It is preferable that the supports are installed with a small gap between them and the molded object during sintering, and a release agent is applied to the interface to prevent deformation contact and bonding during sintering. [Explanation of symbols]
[0088] 100 decision device 101 First condition determination unit 102 First Learning Section 103 Second condition determination unit 104 Second Learning Section 200 Additive Manufacturing Equipment 30 Green Parts 300 Input Device 31 Unit Structure 32 Unit Structure 33 Unit Structure 34 Unit Structures 341 Support part 342 Pin-shaped part 40 Silver Parts 400 Output Device 41 Unit Structure 42 Unit Structure 43 Unit Structure 44 Unit Structure 441 Main body 442 Support S101 First condition determination step S102: Second condition determination step S103 Additive Manufacturing Steps
Claims
1. A first condition determination unit that determines a first manufacturing condition for lamination and resin curing for manufacturing a first structure having a desired shape and density from a shape and density of a first structure manufactured by lamination and resin curing performed during additive manufacturing using a binder jetting method; A second condition determination unit that determines second manufacturing conditions for the debinding and sintering from the shape and density of the second structure manufactured by the debinding and sintering performed during the additive manufacturing, in order to manufacture the second structure having a desired shape and density using the desired first structure manufactured. An apparatus for determining additive manufacturing conditions.
2. The first condition determination unit determines, as the first manufacturing conditions, manufacturing conditions for manufacturing the first structure, under which both a dimensional difference and a density difference from a desired shape are within a predetermined range.
2. The apparatus for determining additive manufacturing conditions according to claim 1 .
3. the first structure includes a plurality of unit structures having different volumes but the same shape, The first condition determination unit further determines, as the first manufacturing condition, a manufacturing condition under which each density difference in the unit structures is within a predetermined range.
3. The apparatus for determining additive manufacturing conditions according to claim 2.
4. a first learning unit that performs machine learning using the first manufacturing conditions, the shape of the first structure, and the density of the first structure as feature quantities; 2. The apparatus for determining additive manufacturing conditions according to claim 1 .
5. The first structure and the second structure each have a block shape.
2. The apparatus for determining additive manufacturing conditions according to claim 1 .
6. The first structure includes a pin-shaped portion.
2. The apparatus for determining additive manufacturing conditions according to claim 1 .
7. The second condition determination unit determines, as the second manufacturing conditions, manufacturing conditions for manufacturing the second structure, under which both a dimensional difference and a density difference from a desired shape are within a predetermined range.
2. The apparatus for determining additive manufacturing conditions according to claim 1 .
8. the second structure includes a plurality of unit structures having different volumes but the same shape, The second condition determination unit further determines, as the second manufacturing condition, a manufacturing condition under which each density difference in the unit structures falls within a predetermined range.
8. An apparatus for determining additive manufacturing conditions according to claim 7.
9. a second learning unit that performs machine learning using the second manufacturing conditions, the shape of the second structure, and the density of the second structure as feature quantities; 2. The apparatus for determining additive manufacturing conditions according to claim 1 .
10. The second learning unit performs the machine learning by using, as the second manufacturing conditions, manufacturing conditions determined by applying a desired shape and density to a thermal deformation analysis model using the thermal properties of the first structure and the shape and density of the second structure.
10. The apparatus for determining additive manufacturing conditions according to claim 9.
11. The second structure has an overhang shape.
2. The apparatus for determining additive manufacturing conditions according to claim 1 .
12. A first condition determination step of determining a first manufacturing condition for lamination and resin curing for manufacturing a first structure having a desired shape and density from the shape and density of the first structure manufactured by lamination and resin curing performed during additive manufacturing by a binder jetting method; A second condition determination step of determining second manufacturing conditions for the debinding and sintering from the shape and density of the second structure manufactured by the debinding and sintering performed during the additive manufacturing, in order to manufacture the second structure having a desired shape and density using the desired manufactured first structure; A method for determining additive manufacturing conditions, comprising:
13. A first condition determination step of determining a first manufacturing condition for lamination and resin curing for manufacturing a first structure having a desired shape and density from the shape and density of the first structure manufactured by lamination and resin curing performed during additive manufacturing by a binder jetting method; A second condition determination step of determining second manufacturing conditions for the debinding and sintering from the shape and density of the second structure manufactured by the debinding and sintering performed during the additive manufacturing, in order to manufacture the second structure having a desired shape and density using the desired manufactured first structure; An additive product is manufactured using the first manufacturing conditions determined in the first condition determination step and the second manufacturing conditions determined in the second condition determination step. A method for producing an additive product, comprising:
Citation Information
Patent Citations
Powder for lamination molding, lamination molded object and manufacturing method of lamination molded object
JP2020172674A
System and method for producing printed material
JP2020517824A
Method for making nano-crystal article using additional production
JP2021102814A
Molding liquid, and method for producing molding liquid
JP2022135572A
Stereoscopic molding system, stereoscopic molding method, and program
JP2022187593A
Cited By
Modeling planning support system, learning device, computing device, modeling planning support method, and program
JP7864277B1