Deck slab

The deck slab design addresses crack control by reducing concrete thickness under beams, shortening reinforcing bars, and minimizing material use, achieving efficient crack prevention and lower floor heights.

JP2024135150APending Publication Date: 2024-10-04NIPPON STEEL METAL PROD CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2023045695
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-22
Publication Date
2024-10-04

AI Technical Summary

Technical Problem

Conventional deck slabs experience cracks due to negative bending at the point of beam support, necessitating long reinforcing bars to control cracks, which increases material and installation costs.

Method used

A deck slab design with a reduced thickness portion in the concrete layer under beam support, narrowing the area of negative bending stress, allowing shorter reinforcing bars and reduced steel usage.

Benefits of technology

The design reduces reinforcing bar length by at least 6.9%, decreases steel and spacer requirements, and contributes to lower floor heights while maintaining structural integrity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024135150000001_ABST
    Figure 2024135150000001_ABST
Patent Text Reader

Abstract

To provide a deck slab capable of shortening a reinforcing bar for crack control.SOLUTION: In a concrete 7, in a region E2 including a region supported by a beams 2 and the periphery of the region supported by the beams, a reduced thickness part 12 in which the concrete thickness is reduced as compared with a general part 11 of the other region E1 is formed. As described above, since the thickness of the concrete in the vicinity of the beam 2 can be reduced, the range in which the negative bending stress is generated can be narrowed, whereby the required length of a reinforcing bar 9 for crack control can be reduced. Therefore, this leads to a reduction in the amount of steel of the reinforcing bar 9 and the number of spacers to be installed, and also contributes to a reduction in floor height because the thickness above the beam can be reduced.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a deck slab. [Background technology]

[0002] A conventional deck slab is described in Non-Patent Document 1. This deck slab includes a deck plate and concrete poured on the deck plate. Reinforcement bars are placed in the concrete on the upper side of the beam. [Prior art documents] [Non-patent literature]

[0003] [Non-Patent Document 1] "Deck Plate Floor Structure Design and Construction Standards: 2018 (Supervised by the Building Research Institute, National Research and Development Agency)" Summary of the Invention [Problem to be solved by the invention]

[0004] Here, as material properties, concrete is strong against compression and weak against tension. On the other hand, it is known that steel is weak against compression and strong against tension. A deck slab is a structure in which concrete bears compression and deck plate (steel plate) and reinforcing bars bear tension. Figure 1 shows the moment acting on the deck slab. At the point where the deck slab is supported by the beam from below, a peak MT of the moment occurs on the negative side, so negative bending occurs at that point instead of positive bending, and tension acts on the concrete. This causes cracks CR to occur on the surface layer. To counter this negative bending, cracks are controlled by placing reinforcing bars inside the concrete, but the length of the reinforcing bars is required to be long, and generally, reinforcing bars of 1m or more are required.

[0005] The present invention has been made to solve such problems, and has an object to provide a deck slab in which the reinforcement bars for crack control can be shortened. [Means for solving the problem]

[0006] The deck slab of the present invention is a deck slab having a deck plate and concrete placed on the deck plate, in which reinforcing bars are placed inside the concrete above the beams, and in the area of ​​the concrete supported by the beams, a reduced thickness portion is formed in which the concrete is thinner than the general portion of other areas.

[0007] In the deck slab according to the present invention, in the area of ​​concrete supported by the beams, a reduced thickness portion is formed in which the concrete thickness is thinner than that of the general portion of other areas. In this way, the concrete thickness near the beams can be made thinner, so the area where negative bending stress occurs can be narrowed. This makes it possible to shorten the length of the reinforcement bars required for cracking. This leads to a reduction in the amount of steel material for the reinforcement bars and the number of spacers installed. In addition, the thickness above the beams can be reduced, which contributes to a reduction in the floor height.

[0008] The ratio of the thickness of the general portion to the thickness of the reduced thickness portion may be greater than 1.0 and less than or equal to 2.5. By adopting such a thickness ratio, the range in which negative bending stress occurs can be narrowed.

[0009] A diagonal portion may be provided in the span direction of the deck slab. In this case, the reduced thickness portion can be formed without providing additional steel material.

[0010] A steel material may be used as the support material for the deck plate. In this case, the reduced thickness portion can be easily formed using the steel material.

[0011] By disposing a steel material on the beam, a concrete impermeable area where concrete does not permeate may be provided. In this case, the thickness of the concrete can be reduced by the thickness of the concrete impermeable area to form a reduced thickness portion.

[0012] The live load may be set to 0.92 or more of the allowable load obtained from the results of the study of the negative bending moment or shear force in the thinned portion. In this case, it is possible to obtain a reduction in the required reinforcement length of at least 6.9%.

[0013] Specifically, the reinforcing bar may be shorter than the standardized length. Specifically, the reinforcing bar may be a steel bar or the like.

[0014] The length of the reinforcing bar may be set to be equal to or greater than the dimension in the span direction of the deck slab in the area where the negative bending stress exceeds the allowable strength of the concrete, thereby enabling the reinforcing bar to reinforce an appropriate range. Effect of the Invention

[0015] According to the present invention, a deck slab can be provided that allows the length of reinforcement bars for crack control to be shortened. [Brief description of the drawings]

[0016] [Figure 1] FIG. 2 is a schematic cross-sectional view of a deck slab according to an embodiment of the present invention. [Diagram 2] FIG. 2 is an enlarged cross-sectional view of the deck slab as viewed from the width direction of the deck slab. [Diagram 3] 3A to 3C are cross-sectional views taken along lines IIIa-IIIa, IIIb-IIIb, and IIIc-IIIc shown in FIG. 2. [Figure 4] FIG. 13 is a diagram showing a verification result by simulation. [Diagram 5] FIG. 13 is a diagram showing a verification result by simulation. [Figure 6] 13 is a table showing verification results by simulation. [Figure 7] FIG. 13 is a diagram showing a verification result by simulation. [Figure 8] 13 is a table showing verification results by simulation. [Figure 9] FIG. 11 is a schematic cross-sectional view showing a deck slab according to a modified example. [Figure 10]13 is a table showing verification results by simulation. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0017] Hereinafter, preferred embodiments of the present invention will be described with reference to the drawings.

[0018] Fig. 1 is a schematic cross-sectional view of a deck slab 100 according to an embodiment of the present invention. As shown in Fig. 1, the deck slab 100 is provided as a floor slab in a building. The deck slab 100 is supported at its four edges by beams 2. The beams 2 on the four sides are each supported by a column 3. Also, a beam 2 (two beams in this example) may be provided midway between the beams 2 corresponding to a pair of opposing sides.

[0019] The span direction D1 and width direction D2 of the deck slab 100 will be described. The direction in which the peaks 6a and valleys 6b of the deck plate 6 of the deck slab 100 extend is the span direction D1 of the deck slab 100, and the direction in which the peaks 6a and valleys 6b are aligned is the width direction D2 of the deck slab 100. In the following description, when simply referred to as "span direction" and "width direction", it means the span direction D1 and width direction D2 of the deck slab 100. FIG. 2 is an enlarged cross-sectional view of the deck slab 100 as viewed from the width direction D2. FIGS. 3(a), (b), and (c) are cross-sectional views along the lines IIIa-IIIa, IIIb-IIIb, and IIIc-IIIc shown in FIG. 2. As shown in FIG. 2, the deck slab 100 has a deck plate 6 and concrete 7 provided on the deck plate 6.

[0020] As shown in Figures 3(a) and (b), the deck plate 6 has alternating peaks 6a and valleys 6b in the width direction D2. The peaks 6a are provided so as to protrude upward from the bottom surfaces of the valleys 6b. The peaks 6a extend parallel to each other in the span direction D1 while being spaced apart from each other in the width direction D2. The peaks 6a form both side walls of the valleys 6b.

[0021] The concrete 7 is poured onto the deck plate 6. The concrete 7 is filled inside the valleys 6b of the deck plate 6 up to a position higher than the upper surface of the peaks 6a. As a result, the concrete 7 has an upper surface that extends in the span direction D1 and width direction D2 above the deck plate 6. This upper surface becomes the upper surface 100a of the deck slab 100. The thickness t of the concrete 7 on the peaks 6a of the deck plate 6 is 50 mm to 100 mm. According to the above range of thickness t, the upper limit of the ratio of the thickness of the general portion to the thickness of the reduced thickness portion is 50:125 (=50+75), or 2.5.

[0022] 2 and 3, crack expansion prevention bars 8 are arranged inside the concrete 7. The crack expansion prevention bars 8 are mesh members extending parallel to the span direction D1 and width direction D2. The crack expansion prevention bars 8 are arranged between the peaks 6a and the upper surface 100a.

[0023] As shown in FIG. 2, reinforcing bars 9 are arranged on the upper side of the beam 2 inside the concrete 7. The reinforcing bars 9 are steel bars extending in the span direction D1. The reinforcing bars 9 extend so as to protrude from both sides of the beam 2 in the span direction D1. The length of the reinforcing bars 9 that protrude from the beam 2 is called the anchorage length. The reinforcing bars 9 are arranged between the peaks 6a and the upper surface 100a. The reinforcing bars 9 are arranged at a predetermined pitch in the width direction D2.

[0024] The reinforcing bar may be shorter than the standardized length. The standard may be, for example, a standard that conforms to "Standard Specifications for Building Construction and Commentary JASS5 Reinforced Concrete Construction 2018". For example, the length of the straight anchorage may conform to 40d (d: rebar diameter (mm)).

[0025] In the area of ​​the concrete 7 supported by the beam 2, a reduced thickness portion 12 is formed in which the concrete thickness is thinner than that of the general portion 11 in the other area E1. In this embodiment, in the area of ​​the concrete 7 supported by the beam 2 and the area E2 including the periphery of the area supported by the beam 2, the reduced thickness portion 12 is formed. The deck plate 6 includes an oblique side portion 13 provided in the span direction D1 and a flat portion 14. The oblique side portion 13 is provided on both sides of the beam 2 in the span direction D1. The oblique side portion 13 is inclined upward from the end of the general portion 11 (area E1) on the beam 2 side toward the beam 2 side in the span direction D1. The flat portion 14 is formed between the upper ends of the pair of oblique side portions 13. The flat portion 14 is disposed on the upper surface of the upper flange of the beam 2.

[0026] As shown in FIG. 3(a), the thickness of the concrete 7 in the general portion 11 is "t1". As shown in FIG. 3(b), the valley portion 6b of the oblique side portion 13 is disposed at a higher position than the valley portion 6b of the general portion 11. As a result, the thickness of the concrete 7 in the oblique side portion 13 is thinner than the thickness t1 of the concrete 7 in the general portion 11. As shown in FIG. 3(c), the flat portion 14 is disposed at a higher position than the valley portion 6b of the general portion 11. In this embodiment, the flat portion 14 is disposed at the same height as the peak portion 6a of the general portion 11. As a result, the thickness t2 of the concrete 7 in the flat portion 14 is thinner than the thickness t1 of the concrete 7 in the general portion 11 (see also FIG. 2). The deck slab 100 of this embodiment is called a reverse enclosing type.

[0027] The ratio of the thickness t1 of the general portion 11 to the thickness t2 of the reduced thickness portion 12 may be greater than 1.0 and may be 1.75 or more. The ratio of the thickness t1 of the general portion 11 to the thickness t2 of the reduced thickness portion 12 may be 2.50 or less, 2.25 or less, or 1.94 or less.

[0028] Next, the bending stress difference when a predetermined load is applied to the deck slab 100 will be verified. Here, the thickness of the top of the deck plate 6 is set to 80 mm, and the design load W is set to 6000 (N / m 2The load acts on the entire surface of the deck slab 100. In the following explanation, "H: deck height", "S: concrete thickness on top of the mound", B S: thickness of the reduced thickness portion 12 (above the beam) and D: total thickness of the slab. Here, as a comparative example, a model of a normal deck slab 200 whose entire area is the general portion 11 as shown in the middle part of Fig. 4 is prepared, and as an example, a model of a deck slab 100 as shown in the lower part of Fig. 4 is prepared.

[0029] The top graph in Fig. 4 shows the stress values ​​(D1 direction) of the concrete surface layer plotted in the span direction D1 for Comparative Example 1 and Example 1. The results of the Example are shown in graph GA1, and the results of the Comparative Example are shown in graph GA2. The horizontal axis shows the X coordinate (position in the span direction D1) with the center of the beam 2 set to 0, and the vertical axis shows the stress. In the figure, the range of the width of the beam 2 is colored. As shown in the top graph of Fig. 4, there is a large difference in the stress in the span direction D1 (general part 11 is 4.79 N / mm 2 In contrast, the reduced thickness portion 12 is 8.08N / mm 2 ), the effect of the smaller cross-section resisting negative bending on the girder was confirmed.

[0030] Here, the "Standards for Reinforced Concrete Structural Calculation - Commentary (Architectural Institute of Japan)" states that the tensile strength of concrete is about 1 / 10 of its compressive strength, and in the case of Fc18, the allowable tensile stress of concrete is ft = 1.8 N / mm 2 Here, the negative bending stress is assumed to be 1.8 N / mm2, as shown by the dashed line. 2 In the range above 1.8N / mm, the concrete 7 alone cannot bear the load and cracks will occur, so reinforcement bars 9 must be installed. 2The reinforcing bars 9 are arranged in an area larger than the dashed line. In other words, the length of the reinforcing bars 9 needs to be equal to or greater than the dimension in the span direction D1 of the area where the negative bending stress exceeds the allowable strength of concrete. The positions of the ends of the reinforcing bars 9 in Example 1 and Comparative Example 1 are indicated by lines L1 and L2. It can be seen that the range of the reinforcing bars 9 is wider in the specifications of Comparative Example 1. In other words, when a reduced thickness portion 12 is provided in Example 1, it is possible to reduce the installation range of the reinforcing bars 9 that bear the negative bending stress.

[0031] Next, the thickness of the top of the deck plate 6 is set to 80 mm, and the design load W is set to 2900 N / m 2 In comparison with the above Example 1 and Comparative Example 1 (No. 1), an analysis was additionally carried out without and with partial thickness reduction in the specifications of Example 2 and Comparative Example 2 (No. 2) in which the live load was reduced. Graph GB1 in FIG. 5 shows the results of Example 2, and graph GB2 shows the comparative example. No. 1 and No. 2 were compared as shown in FIG. 6 in terms of the "reduced ratio of required length of reinforcement" calculated by dividing the required length Lr of the reinforcement in Comparative Example 2 without partial thickness reduction by the new required length Lr of the reinforcement in Example 2 with partial thickness reduction. As a result, it was confirmed that the reduction effect was weakened, with No. 1 being able to reduce the length by 43.2%, while No. 2 being able to reduce by 15.2%. This is thought to be because when the live load introduced is small compared to the allowable load in the concrete tensile part, the area exceeding the allowable tensile stress of concrete (dashed line) is small in the first place, and the need for reinforcement is low.

[0032] Next, the thickness of the top of the deck plate 6 is set to 60 mm, and the design load W is set to 1640 N / m 2 In addition to the above Example 2 and Comparative Example 2 (No. 2), an analysis was additionally carried out with and without partial thickness reduction for the specifications of Example 3 and Comparative Example 3 (No. 3) in which the peak thickness was reduced. Graph GC1 in Fig. 7(a) shows the results of Example 3, and graph GC2 shows the comparative example. The peak thickness of the deck plate 6 was set to 100 mm, and the design load W was 4550 N / m 2In addition to the above-mentioned Example 2 and Comparative Example 2 (No. 2), an analysis was conducted with and without partial thickness reduction in the specifications of Example 4 and Comparative Example 4 (No. 4) in which the thickness of the top of the cone was increased. Graph GD1 in FIG. 7(b) shows the results of Example 4, and graph GD4 shows the comparative example. As for the live load, the value was set so that the "live load to the allowable load" in the reduced thickness portion 12 was approximately the same ratio (0.92 to 0.93), and consideration was given to ensure that the margin was approximately the same for each set cross section. In this way, the live load may be set to 0.92 or more with respect to the allowable load in the reduced thickness portion 12 (study of negative bending moment based on "4.3 Study of load at completion" in Non-Patent Document 1 or study of shear force based on "5.4 Design for in-plane shear force" in Non-Patent Document 1). Comparing the "reduced ratio of required length of reinforcement" in FIG. 8, it can be seen that the effect is greater as the thickness of the top of the cone increases, i.e., "top of the cone 60 mm < top of the cone 80 mm < top of the cone 100 mm".

[0033] Next, the action and effect of the deck slab 100 according to the embodiment of the present invention will be described.

[0034] In the deck slab 100 according to this embodiment, in the area E2 of the concrete 7, which includes the area supported by the beam 2 and the periphery of the area supported by the beam 2, a reduced thickness portion 12 is formed in which the concrete thickness is thinner than the general portion 11 of the other area E1. In this way, the concrete thickness near the beam 2 can be made thinner, so that the range where negative bending stress occurs can be narrowed. This allows the length of the reinforcing bars 9 required for crack control to be shortened. This leads to a reduction in the amount of steel material for the reinforcing bars 9 and the number of spacers installed. In addition, the thickness above the beam can be reduced, which contributes to a reduction in the floor height.

[0035] The ratio of the thickness of the general portion 11 to the thickness of the reduced thickness portion 12 may be greater than 1.0 and equal to or less than 2.5. By adopting such a thickness ratio, the range in which negative bending stress occurs can be narrowed.

[0036] The oblique side portion 13 may be provided in the span direction D1 of the deck slab 100. In this case, the reduced thickness portion 12 can be formed without providing additional steel materials or the like.

[0037] The live load may be set to 0.92 or more of the allowable load obtained from the results of the study of the negative bending moment or shear force in the thinned portion. In this case, it is possible to obtain a reduction in the required reinforcement length of at least 6.9%.

[0038] The reinforcing bar 9 may be shorter than the standardized length. For example, as shown in FIG. 10, in the cases of the first to fourth embodiments having the reduced thickness portion 12, the required length of the reinforcing bar is shorter than when the specifications of the conventional technology are used. In addition, in the specifications of the conventional technology, since the beam width is 300 mm, the required length from the beam center is "required anchorage length: 400 + 150 (half the beam width) = 550 mm". This length is the standardized length.

[0039] The length of the reinforcing bar 9 may be set to be equal to or greater than the dimension in the span direction D1 of the deck slab 100 in the region where the negative bending stress exceeds the allowable strength of the concrete. This allows the reinforcing bar 9 to reinforce an appropriate range.

[0040] The present invention is not limited to the above-described embodiments.

[0041] The deck slab 100 shown in FIG. 9(a) has a support material 21 for the deck plate 6 provided on the beam 2 and a drop material 22. The support material 21 extends from the beam 2 in the width direction D2. The support material 21 is made of steel or the like. The drop material 22 is provided at the end of the support material 21, and has a portion extending downward and a portion extending in the width direction D2 at the lower end. The drop material is made of angle steel or the like. The end of the deck plate 6 is supported by the drop material. As a result, the concrete 7 of the general portion 11 reaches a position lower than the upper end of the beam 2, and the concrete 7 of the reduced thickness portion 12 is higher than the upper end of the beam 2. As a result, the thickness of the concrete 7 of the reduced thickness portion 12 becomes thinner. In addition, the reduced thickness portion 12 can be easily formed using steel. Alternatively, the support material 21 and the drop material 22 may be integrally formed from a member such as a Z-shaped steel material.

[0042] In the deck slab 100 shown in FIG. 9(b), a concrete-impermeable region 24 where the concrete 7 does not permeate is provided by placing steel materials 23 on the beams 2. The steel materials 23 are formed of channel steel materials or the like. The concrete-impermeable region 24 is a space surrounded by the walls of the steel materials 23. As a result, in the reduced thickness portion 12, the thickness of the concrete 7 is reduced by the amount of the concrete-impermeable region 24.

[0043] The deck slab 100 shown in Fig. 9(c) is obtained by adding an oblique side portion 26 to the upper side of the deck slab 100 in Fig. 2. The oblique side portion 26 slopes downward from the end of the general portion 11 on the beam 2 side toward the beam 2 side in the span direction D1. This type of deck slab 100 is called an intermediate encro type. [Explanation of symbols]

[0044] 2...beam, 6...deck plate, 7...concrete, 9...reinforcing bar, 11...general part, 12...reduced thickness part, 13...hypothetic part, 100...deck slab.

Claims

1. A deck slab having a deck plate and concrete provided on the deck plate, A reinforcing bar is placed on the upper side of the beam inside the concrete, A deck slab, in which a reduced thickness portion is formed in the area of ​​the concrete supported by the beam, in which the concrete is thinner than the general portion of other areas.

2. The deck slab according to claim 1 , wherein a ratio of a thickness of the general portion to a thickness of the reduced thickness portion is greater than 1.0 and is not greater than 2.

5.

3. The deck slab according to claim 1 , wherein a slanted portion is provided in the span direction of the deck slab.

4. The deck slab according to claim 1, wherein a steel material is used as a support material for the deck plate.

5. 2. The deck slab according to claim 1, wherein a concrete-impermeable area is provided in which the concrete does not penetrate by placing steel material on the beam.

6. 2. The deck slab according to claim 1, wherein the live load is set to 0.92 or more relative to the allowable load determined from the results of an investigation of the negative bending moment or shear force in the reduced thickness portion.

7. 2. The deck slab of claim 1, wherein the reinforcing bars are short compared to a standardized length.

8. 2. The deck slab according to claim 1, wherein the length of the reinforcing bar is set to be equal to or greater than the dimension in the span direction of the deck slab in an area where the negative bending stress exceeds the allowable strength of the concrete.

Citation Information

Patent Citations

  • JP1968004378Y1

  • Execution method of floor block that use deck plate

    JP1977026714A

  • Deck plate and floor block structure that use deck plate

    JP1977036817A

  • PC beam

    JP1987033961A

  • Construction of composite floor slab and deck plate therefor

    JP1993311794A