Joining method for dissimilar materials

By applying electricity to heat the inside of a higher-resistance first member, the method stabilizes temperature and enhances bonding strength in joining dissimilar materials, addressing instability issues in conventional methods.

JP2024135891APending Publication Date: 2024-10-04NISSAN MOTOR CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2023046791
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-23
Publication Date
2024-10-04

AI Technical Summary

Technical Problem

Conventional methods for joining dissimilar materials face instability in heat generation and temperature control due to varying contact resistance between materials.

Method used

The method involves applying electricity to cause the inside of a first member, which has higher electrical resistance, to reach the highest temperature, thereby stabilizing the temperature for effective bonding.

Benefits of technology

This approach ensures stable temperature control and improved bonding strength by effectively discharging oxide films and plating layers, while minimizing thickness loss in the second member with a lower melting point.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024135891000001_ABST
    Figure 2024135891000001_ABST
Patent Text Reader

Abstract

To provide a joining method for dissimilar materials, capable of joining materials to each other at a stable temperature.SOLUTION: A joining method for dissimilar materials includes: a first step of abutting a first component 100 made of a first material on a second component 200 made of a second material different from the first material; a second step of abutting a first electrode 10 on the first component 100 and abutting a second electrode 20 on the second component 200, and then pressurizing the layered first and second components 100, 200 between the first electrode 10 and the second electrode 20; and a third step of applying electric current between the first electrode 10 and the second electrode 20, thereby resistance-spot welding the first component 100 and the second component 200. In the third step, the electric current generates the highest heat inside the first component 100, and thereby joins the first component 100 and the second component 200 to each other.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for joining different types of materials. [Background technology]

[0002] A method for joining dissimilar materials is known in which a first material and a second material of a different type from the first material are overlapped and joined by resistance spot welding (for example, Patent Document 1). In this method for joining dissimilar materials, the first material and the second material are melted and joined by resistance heating at the contact surface between the first material and the second material. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Patent No. 5120864 Summary of the Invention [Problem to be solved by the invention]

[0004] However, since the resistance at the contact surface varies depending on the contact state between the materials, conventional joining methods have the problem that the amount of heat generated at the contact surface becomes unstable, resulting in an unstable temperature.

[0005] An object of the present invention is to provide a method for joining dissimilar materials, which is capable of joining the materials together at a stable temperature. [Means for solving the problem]

[0006] The present invention solves the above-mentioned problems by joining the first member and the second member by heating the inside of the first member to the highest temperature by passing an electric current through the first member. Effect of the Invention

[0007] According to the present invention, the inside of the first member is heated to the highest temperature by passing an electric current through it, so that the first member and the second member can be joined at a stable temperature. [Brief description of the drawings]

[0008] [Figure 1] FIG. 1 is a side view showing one embodiment of the method for joining dissimilar materials of the present invention. [Diagram 2] FIG. 2 is an enlarged view showing the vicinity of the dissimilar materials and electrodes in FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] An embodiment of a power supply system according to the present invention will be described with reference to the drawings. Fig. 1 is a side view showing an example of a method for joining dissimilar materials in the present embodiment. Fig. 2 is an enlarged view showing the vicinity of the dissimilar materials and electrodes in Fig. 1.

[0010] 1, the joining device 1 used in the method for joining dissimilar materials of this embodiment is a joining device that joins a first member 100 made of a first material and a second member 200 made of a second material different from the first material by melting. A part of the first member 100 and a part of the second member 200 are overlapped with each other, and the joining device 1 joins the overlapped parts of the first member 100 and the second member 200 by melting.

[0011] The first material is not particularly limited, but may be steel or the like, and the first member 100 made of this first material may be a steel plate. The steel plate is not particularly limited, but may be a zinc-plated steel plate (GI steel plate), a zinc alloy-plated steel plate (GA steel plate), a bare steel plate, etc. This first member 100 is used, for example, as a vehicle frame.

[0012] On the other hand, the second material is not particularly limited, but an example thereof can be an aluminum alloy, and an example of the second member 200 made of this second material can be an aluminum alloy plate, etc. This second member 200 is used, for example, as a panel of a vehicle.

[0013] In the present embodiment, the first material may have a higher electrical resistance than the second material. For example, when the first material is steel and the second material is an aluminum alloy, the electrical resistance of the first material is higher than the electrical resistance of the second material.

[0014] In this embodiment, the second material may have a lower melting point than the first material. For example, if the first material is steel and the second material is an aluminum alloy, the melting point of the second material is lower than the melting point of the first material.

[0015] The bonding device 1 in this embodiment includes a first electrode 10, a second electrode 20, and a power source 30. Although not particularly shown, the first electrode 10 and the second electrode 20 may be provided at the tip of a multi-joint robot, and may be configured to be movable by the multi-joint robot.

[0016] The first electrode 10 is an electrode tip made of a conductive material such as metal. The first electrode 10, together with the second electrode 20, sandwiches the laminate 300, thereby applying pressure to the laminate 300 from the first member 100 side.

[0017] The shape of the first electrode 10 in this embodiment is not particularly limited, but is a dome radius type (DR type). As shown in Fig. 2, the first electrode 10 includes a first columnar section 11 and a first tip section 12. The first columnar section 11 is a cylindrical portion and includes a cylindrical side surface 11a.

[0018] A first tip portion 12 is connected to the lower end of the first columnar portion 11. The first tip portion 12 of the first electrode 10 includes a dome portion 13 and a radius portion 14. The dome portion 13 is provided at the lower end of the first columnar portion 11, and the dome portion 13 in this embodiment has a dome shape that gradually decreases in diameter downward. This dome portion 13 includes a dome surface 13a as a side surface. The curvature of this dome surface 13a is larger than the curvature of the radius surface 14a of the radius portion 14 described later. The radius of curvature of this dome surface 13a is not particularly limited, but may be 5 mm to 10 mm.

[0019] A first radius portion 14 is disposed at the lower end of this dome portion 13. This first radius portion 14 has a radius shape that slightly protrudes downward. The first radius portion 14 in this embodiment is a portion that contacts the first member 100 and includes a first radius surface 14a as a lower end surface. The curvature of this first radius surface 14a is smaller than the curvature of the dome surface 13a. The radius of curvature of this first radius surface 14a is not particularly limited, but may be 10 mm to 100 mm.

[0020] Also, the diameter d1 of this first radius portion 14 is smaller than the diameter D1 of the first columnar portion 11 described above (d1 < D1). Although not particularly limited, the diameter D1 can be 8 mm to 16 mm, and the diameter d1 can be 6 mm to 8 mm.

[0021] Note that although not particularly limited, depending on the pressing force during joining, not only the first radius surface 14a but also the lower region of the dome surface 13a may contact the first member 100.

[0022] The second electrode 20 is an electrode chip made of a material having conductivity such as metal. By sandwiching the laminate 300 together with the first electrode 10, the laminate 300 is pressed from the second member 200 side.

[0023] The shape of the second electrode 20 in this embodiment is not particularly limited, but it is a radius type (R type). This second electrode 20 includes a second columnar portion 21 and a second tip portion 22. The second columnar portion 21 is a columnar portion and includes a cylindrical side surface 21a.

[0024] The second tip portion 22 includes a second radius portion 24. This second radius portion 24 is disposed at the lower end of the second columnar portion 21. This second radius portion 24 has a radius shape that slightly protrudes upward. The second radius portion 24 in this embodiment is a portion that contacts the second member 200 and includes a second radius surface 24a as an upper end surface. The curvature of this second radius surface 24a is smaller than the curvature of the first radius surface 14a. The radius of curvature of this second radius surface 24a is not particularly limited, but it may be 20 mm to 300 mm.

[0025] Also, the diameter d2 of this second radius portion 24 is the same as the diameter D2 of the above-mentioned second columnar portion 21 (d2 = D2). And the diameter d2 of this second radius portion 24 is larger than the diameter d1 of the above-mentioned first radius portion 14 and the diameter D1 of the first columnar portion 11 (d1 < D1 < d2). The diameters D2 and d2 are not particularly limited, but they may be 19 mm or more.

[0026] In this embodiment, by setting the first electrode 10 as a DR type electrode and the second electrode 20 as an R type electrode, the most pressure can be applied to the center of the joint portion between the first member 100 and the second member 200. For this reason, it becomes easy to discharge an oxide film or a plating layer, which will be described later, from the joint interface during joining, and the joining strength can be improved. Also, the DR type electrode and the R type electrode do not include a corner portion on the tip surface, and since the corner portion is not crushed by repeated use and the electrode is not deformed, it is also possible to suppress deterioration of the joining quality over time.

[0027] The power source 30 is electrically connected to the first electrode 10 and the second electrode 30. The power source 30 applies a voltage between the first electrode 10 and the second electrode 20 in a state in which the first electrode 10 and the second electrode 20 pressurize the first member 100 and the second member 200, and passes a current between the first electrode 10 and the second electrode 20. In FIG. 2, the current c that flows between the first electrode 10 and the second electrode 20 is indicated by a dashed arrow. As shown in FIG. 2, the power source 30 in this embodiment passes a current from the first electrode 10 to the second electrode 20, although this is not particularly limited.

[0028] A description will now be given of a method for joining dissimilar materials using the above-described joining device 1. First, in the first step, the above-described first member 100 and second member 200 are overlapped. For this overlapping operation, a jig capable of holding the first member 100 and the second member 200 in an overlapped state can be used, although not shown in the drawings.

[0029] 1, in the second step, the first electrode 10 is brought into contact with the first member 100 and the second electrode 20 is brought into contact with the second member 200, so that the overlapped first member 100 and second member 200 are sandwiched and pressurized between the first electrode 10 and the second electrode 20. The pressing force at this time is not particularly limited, but can be 4 kN to 8 kN. The squeeze time is also not particularly limited, but can be 50 msec to 200 msec.

[0030] Next, in a third step, the power source 30 applies electricity between the first electrode 10 and the second electrode 20 to resistance spot join the first member 100 and the second member 200. At this time, the inside of the first member 100 is heated to the highest temperature by the application of electricity, thereby joining the first member 100 and the second member 200. The time for which electricity is applied at this time is not particularly limited, but can be 150 msec to 300 msec.

[0031] 2, in this embodiment, the diameter of the first electrode 10 (diameter D1 of the first columnar section 11) is set smaller than the diameter of the second electrode 20 (diameter D2 of the second columnar section 21), and the diameter d1 of the first radius section 14 is set smaller than the diameter d2 of the second radius section 24. As a result, the contact area of ​​the first electrode 10 with the first member 100 can be made smaller than the contact area of ​​the second electrode 20 with the second member 200. For this reason, the density of the current c indicated by the dashed arrow in FIG. 2 is relatively high in the first member 100 in contact with the first electrode 10, and is relatively low in the second member 200 in contact with the second electrode 20.

[0032] At this time, the amount of heat generated inside the first member 100 is greater than the amount of heat generated at the bonding interface between the first member 100 and the second member 200 and the amount of heat generated inside the second member 200. Therefore, compared to the temperatures at the bonding interface between the first member 100 and the second member 200 and the temperature inside the second member 200, the temperature inside the first member 100 is the highest.

[0033] For example, when the first member 10 is a bare steel plate and the second member 20 is an aluminum alloy plate, the temperature of the highest temperature part 101 of the first member 10 in FIG. 2 is about 1500°C. Then, due to heat transfer from the highest temperature part 101, the temperature at the interface between the first member 10 and the second member 20 becomes, for example, about 700°C. At this time, eutectic melting (or diffusion melting) of iron and aluminum occurs at the joining interface due to pressure and temperature rise, and the oxide film of the surface layer is melted and discharged outside the joining interface. Then, the new surface of the steel plate and the new surface of the aluminum alloy plate come into contact with each other and are joined, thereby joining the first member 10 and the second member 20. Note that, when the first member 10 is a GA steel plate or GI steel plate having a plating layer, the plating layer is also melted and discharged outside the joining interface.

[0034] After the current flow is terminated, in the fourth step, the first member 100 and the second member 200 after the welding are held for a predetermined time by the first electrode 10 and the second electrode 20. The hold time is not particularly limited, but may be 200 msec to 400 msec. Thereafter, the first member 100 and the second member 200 are released from the first electrode 10 and the second electrode 20.

[0035] In the method for joining dissimilar materials in this embodiment, the first member 100 and the second member 200 are joined by heating the inside of the first member 10 to the highest temperature by passing electricity through the first member 10. The inside of the first member 100 has a substantially uniform electrical resistance, unlike the joint interface with the second member 200, where dissimilar materials overlap, so that a stable amount of heat can be obtained and the temperature of the joint interface can be stabilized. This makes it possible to effectively remove oxide films and plating layers from the joint interface and to join the first member 10 and the second member 20.

[0036] In this embodiment, the inside of the first member 10, which has a relatively high electrical resistance, is heated to the highest temperature, thereby suppressing the amount of heat generated in the second member 20, which has a relatively low melting point, and melting the outermost layer of the second member 20. This makes it possible to suppress a reduction in the thickness of the second member 20 due to heat generation under pressure, and to suppress a reduction in the strength of the second member 200 after joining.

[0037] In this embodiment, by making the diameter D1 of the first electrode 10 smaller than the diameter D2 of the second electrode 20, the contact area of ​​the first electrode 10 with the first member 100 can be reliably made smaller than the contact area of ​​the second electrode 20 with the second member. This makes it possible to reliably make the current density inside the first member 100 higher than the current density inside the second member 200.

[0038] At the same time, since the diameter D2 of the second electrode 20 is relatively large, the heat capacity of the second electrode 20 is also relatively large. Therefore, by the second electrode 20 being in contact with the second member 200, the cooling performance of the second electrode 20 for the second member 200 can be improved, and a reduction in the thickness of the second member 20 can be suppressed.

[0039] The above-described embodiments are described for the purpose of facilitating understanding of the present invention, and are not described for the purpose of limiting the present invention. Therefore, the elements disclosed in the above embodiments are intended to include all design modifications and equivalents that fall within the technical scope of the present invention.

[0040] For example, in the above embodiment, the first electrode 10 and the second electrode 20 are bonded in a state in which they are arranged opposite each other in the vertical direction, but this is not limited to the above. The first electrode 10 and the second electrode 20 may be arranged opposite each other in a direction other than the vertical direction.

[0041] In the above embodiment, DR-type and R-type electrode tips are used as the electrodes, but the present invention is not limited to this. Any type of electrode tip may be used as long as it can make the inside of the first member 100 the highest temperature. As the first electrode 10 and the second electrode 20, in addition to the DR-type and R-type, a dome-type (D-type), a cone-radius-type (CR-type), a flat-type (F-type), a cone-flat-type (CF-type), or an offset-type (E-type) electrode tip may be used. [Explanation of symbols]

[0042] 1...Joining device 10...1st electrode 11...First columnar part 11a…Cylindrical side 12...First tip 13…Dome section 13a…Dome surface 14…First radius section 14a…First radius surface 20…Second electrode 21…Second columnar part 21a…Cylindrical side 22…Second tip 24…Second radius section 24a…Second radius surface 30...Power supply

Claims

1. A first step of overlapping a first member made of a first material and a second member made of a second material different from the first material; a second step of contacting a first electrode with the first member and a second electrode with the second member, and sandwiching and pressurizing the overlapped first and second members between the first and second electrodes; a third step of resistance spot joining the first member and the second member by passing a current between the first electrode and the second electrode, In the third step, the first member and the second member are joined by heating the inside of the first member to the highest temperature by passing an electric current through the first member.

2. The method for joining dissimilar materials according to claim 1, the electrical resistance of the first material is higher than the electrical resistance of the second material; the melting point of the second material is lower than the melting point of the first material; The third step is a method for joining dissimilar materials that includes melting a surface layer of the second member by heating the inside of the first member to the highest temperature by passing an electric current through the first member.

3. The method for joining dissimilar materials according to claim 1 or 2, A method for joining dissimilar materials, wherein the diameter of the first electrode is made smaller than the diameter of the second electrode, thereby making the current density inside the first member higher than the current density inside the second member in the third step.

4. The method for joining dissimilar materials according to claim 3, A method for joining dissimilar materials, wherein in the third step, a contact area of ​​the first electrode with the first member is made smaller than a contact area of ​​the second electrode with the second member.

Citation Information

Patent Citations

  • Different material joining method of steel and aluminum material

    JP2008200687A

  • Spot welding method

    JP2022063070A

  • Hisetsushokushikisoatsusokuteisochi

    JP1976020864A