The mesa structure with a window region addresses the risk of optical damage on the active layer by expanding the band gap, thereby preventing defects and maintaining semiconductor integrity.

JP2024136554APending Publication Date: 2024-10-04FURUKAWA ELECTRIC CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
JP2023047704
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-24
Publication Date
2024-10-04

AI Technical Summary

Technical Problem

The risk of optical damage on the side surfaces of the active layer in optical semiconductor devices due to defects caused by oxidation or etching, leading to increased light absorption and potential melting of the semiconductor material.

Method used

A novel configuration with a mesa structure and a window region, such as a mixed crystal layer, impurity diffusion layer, or wide bandgap layer, is provided along the side surfaces of the active layer to expand the band gap and suppress light absorption.

Benefits of technology

The configuration effectively suppresses optical damage on the side surfaces of the active layer, preventing defects and maintaining the integrity of the semiconductor material.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024136554000001_ABST
    Figure 2024136554000001_ABST
Patent Text Reader

Abstract

To provide an optical semiconductor element having a novel and improved structure that makes it possible to suppress optical damage on the side surface of an active layer, and a manufacturing method for the optical semiconductor element.SOLUTION: An optical semiconductor element includes, for example, a mesa in which a first cladding layer, an active layer, and a second cladding layer are stacked in a first direction, and which extends in a third direction intersecting the first and second directions with a predetermined width in a second direction intersecting the first direction, and has side surfaces at an end in the second direction and an end in the opposite direction to the second direction, a first electrode electrically connected to the first cladding layer, and a second electrode electrically connected to the second cladding layer, and a window region covering the active layer is provided along the side surface. The mesa may be made of a GaAs-based semiconductor material.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an optical semiconductor element and a method for manufacturing an optical semiconductor element. [Background technology]

[0002] Conventionally, as an optical semiconductor element made of GaAs-based semiconductor material, an optical semiconductor element in which a trench forming a ridge structure extends from the upper cladding layer, beyond the active layer, to the lower cladding layer is known (for example, Non-Patent Document 1). With such a structure, the trench can suppress leakage of current outside the ridge, and it is possible to suppress the occurrence of undesirable phenomena caused by the leakage, such as an increase in energy loss of the supplied power or the occurrence of higher-order transverse modes in light. [Prior art documents] [Non-patent literature]

[0003] [Non-Patent Document 1] Joseph P. Donnelly, Robin K. Huang, James N. Walpole, Leo J. Missaggia, Chris T. Harris, Jason J. Plant, Robert J. Bailey, Daniel E. Mull, William D. Goodhue, and George W. Turner, AlGaAs-InGaAs Slab-Coupled Optical Waveguide Lasers, IEEE JOURNAL OF QUANTUM ELECTRONICS, VOL. 39, NO. 2, FEBRUARY 2003 Summary of the Invention [Problem to be solved by the invention]

[0004] In a configuration in which an active layer faces a trench, there is a risk of defects occurring on the side surface of the active layer facing the trench due to oxidation or the like. In addition, there is a risk of defects occurring on the side surface when forming a trench by etching. When a defect occurs on the side surface of the active layer, electrons and holes combine through the defect, causing the temperature of the side surface to rise, which in turn reduces the band gap of the semiconductor material on the side surface, resulting in increased light absorption. When light absorption increases, the temperature of the side surface further increases, the band gap further reduces, and light absorption further increases, resulting in a cycle that may ultimately lead to the melting of the semiconductor material.

[0005] Therefore, one object of the present invention is to provide an optical semiconductor element having a new and improved configuration that makes it possible to suppress optical damage on the side surface of the active layer, for example, and a method for manufacturing the optical semiconductor element. [Means for solving the problem]

[0006] The optical semiconductor element of the present invention comprises, for example, a mesa in which a first cladding layer, an active layer, and a second cladding layer are stacked in a first direction, extending in a third direction intersecting the first direction and the second direction with a predetermined width in a second direction intersecting the first direction, and having side surfaces at an end in the second direction and an end in the opposite direction to the second direction, a first electrode electrically connected to the first cladding layer, and a second electrode electrically connected to the second cladding layer, and a window region covering the active layer is provided along the side surfaces.

[0007] In the optical semiconductor device, the mesa may have a portion made of a GaAs-based semiconductor material.

[0008] In the optical semiconductor device, the window region may be a mixed crystal layer provided in the mesa.

[0009] In the optical semiconductor element, the window region may be an impurity diffusion layer provided in the mesa.

[0010] In the optical semiconductor element, the window region may be a wide band gap layer provided outside the mesa.

[0011] The optical semiconductor element may include a multilayer portion that is shifted in the second direction with respect to the mesa and has the same multilayer structure as the mesa, and a trench may be provided between the multilayer portion and the mesa.

[0012] In the optical semiconductor element, the mesa may have a portion in which the width changes toward the third direction.

[0013] The optical semiconductor element may be configured as a semiconductor laser element.

[0014] The optical semiconductor device may be configured as a semiconductor optical amplifier.

[0015] A method for manufacturing an optical semiconductor element of the present invention includes, for example, the steps of forming a mesa in which a first cladding layer, an active layer, and a second cladding layer are stacked in a first direction, the mesa extends in a third direction intersecting the first direction and the second direction with a predetermined width in a second direction intersecting the first direction, and the mesa has side surfaces at an end in the second direction and an end in the opposite direction to the second direction; forming a first electrode electrically connected to the first cladding layer; forming a second electrode electrically connected to the second cladding layer; and forming a window region covering the active layer along the side surfaces. Effect of the Invention

[0016] According to the present invention, it is possible to obtain an optical semiconductor element having a more improved novel configuration that makes it possible to suppress optical damage on the side surfaces of an active layer, and a method for manufacturing the optical semiconductor element. [Brief description of the drawings]

[0017] [Figure 1] FIG. 1 is an illustrative schematic cross-sectional view of an optical semiconductor element according to the first embodiment. [Diagram 2]FIG. 2 is an illustrative schematic plan view of a portion of the optical semiconductor element according to the first embodiment. [Diagram 3] FIG. 3 is an illustrative schematic cross-sectional view of a product during the manufacture of the optical semiconductor element of the first embodiment. [Figure 4] FIG. 4 is an illustrative schematic cross-sectional view of a product during the manufacture of the optical semiconductor element of the first embodiment, showing a stage subsequent to that shown in FIG. [Diagram 5] FIG. 5 is an illustrative schematic cross-sectional view of a product during the manufacture of the optical semiconductor element of the first embodiment, showing a stage subsequent to that shown in FIG. [Figure 6] FIG. 6 is an illustrative schematic cross-sectional view of a product during the manufacture of the optical semiconductor element of the first embodiment, showing a stage subsequent to that shown in FIG. [Figure 7] FIG. 7 is an illustrative schematic cross-sectional view of a product during the manufacture of the optical semiconductor element of the first embodiment, showing a stage subsequent to that shown in FIG. [Figure 8] FIG. 8 is an illustrative schematic cross-sectional view of the optical semiconductor element according to the second embodiment. [Figure 9] FIG. 9 is an illustrative schematic cross-sectional view of a product in the middle of manufacturing the optical semiconductor element according to the second embodiment. [Figure 10] FIG. 10 is an illustrative schematic cross-sectional view of a product during the manufacture of the optical semiconductor element of the second embodiment, showing a stage subsequent to that shown in FIG. [Figure 11] FIG. 11 is an illustrative schematic cross-sectional view of an optical semiconductor element according to the third embodiment. [Figure 12] FIG. 12 is an illustrative schematic cross-sectional view of a product in the middle of manufacturing the optical semiconductor element of the third embodiment. [Figure 13] FIG. 13 is an illustrative schematic cross-sectional view of a product during the manufacture of the optical semiconductor element of the third embodiment, showing a stage subsequent to that shown in FIG. [Figure 14] FIG. 14 is an illustrative schematic cross-sectional view of an optical semiconductor element according to the fourth embodiment. [Figure 15]FIG. 15 is an illustrative schematic plan view of a part of the optical semiconductor element according to the fifth embodiment. [Figure 16] FIG. 16 is an illustrative schematic plan view of a part of the optical semiconductor element according to the sixth embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0018] Exemplary embodiments and modifications of the present invention are disclosed below. The configurations of the embodiments and modifications shown below, as well as the actions and results (effects) brought about by the configurations, are merely examples. The present invention can be realized by configurations other than those disclosed in the following embodiments and modifications. Furthermore, according to the present invention, it is possible to obtain at least one of the various effects (including derivative effects) obtained by the configurations.

[0019] The following embodiments and modifications have similar components, and in the following description, the same reference numerals will be used to denote the similar components, and duplicated descriptions may be omitted.

[0020] In this specification, ordinal numbers may be given for convenience to distinguish directions, parts, members, etc. In addition, ordinal numbers do not indicate a priority order or sequence, and do not specify a number.

[0021] In each drawing, the X direction is represented by an arrow X, the Y direction is represented by an arrow Y, and the Z direction is represented by an arrow Z. The X direction, Y direction, and Z direction intersect with each other and are perpendicular to each other.

[0022] [First embodiment] [Configuration of optical semiconductor element] FIG 1 is a cross-sectional view of an optical semiconductor element 100A (100) according to the first embodiment. FIG 2 is a plan view of a portion of the optical semiconductor element 100A (100). In this embodiment, the optical semiconductor element 100A is configured as a semiconductor laser element. The X direction is the direction in which laser light is emitted from the optical semiconductor element 100. The X direction may also be referred to as the longitudinal direction, and the Y direction may also be referred to as the width direction.

[0023] As shown in FIG. 1, the optical semiconductor element 100 includes a first electrode 21, a laminated portion 10, a passivation film 15, a conductive layer 16, and a second electrode 22.

[0024] The laminated portion 10 has a configuration in which a first semiconductor layer 12, a second semiconductor layer 13, and a third semiconductor layer 14 are laminated in this order in the Z direction on a substrate 11. The Z direction is an example of a first direction, and may also be referred to as a lamination direction. The laminated portion 10 is made of a GaAs-based semiconductor material, and may also be referred to as a semiconductor laminated portion.

[0025] The substrate 11 intersects with and is perpendicular to the Z direction. The substrate 11 is made of, for example, GaAs.

[0026] The first semiconductor layer 12 is stacked in the Z direction on the substrate 11. The first semiconductor layer 12 intersects with and is perpendicular to the Z direction. The first semiconductor layer 12 is made of, for example, n-AlGaAs.

[0027] The second semiconductor layer 13 is stacked in the Z direction on the first semiconductor layer 12. The second semiconductor layer 13 intersects with and is perpendicular to the Z direction. The second semiconductor layer 13 is made of, for example, InGaAs.

[0028] The third semiconductor layer 14 is stacked in the Z direction on the second semiconductor layer 13. The third semiconductor layer 14 intersects with and is perpendicular to the Z direction. The third semiconductor layer 14 is made of, for example, p-AlGaAs.

[0029] The stacked portion 10 is provided with a trench 10c recessed in the opposite direction to the Z direction from the end surface 10b in the Z direction. The trench 10c penetrates the third semiconductor layer 14 and the second semiconductor layer 13, and extends to the middle of the first semiconductor layer 12. The trench 10c may further extend in the opposite direction to the Z direction to reach the middle of the substrate 11. As shown in FIG. 2, the trench 10c extends in the X direction with a predetermined width in the Y direction. The trench 10c may also be referred to as a groove or a recess.

[0030] As shown in Fig. 1, the stacked portion 10 has two trenches 10c of substantially the same shape spaced apart in the Y direction. As shown in Fig. 2, these two trenches 10c extend substantially parallel to each other in the X direction. As a result, as shown in Figs. 1 and 2, a mesa 30 is formed between the two trenches 10c, protruding in the Z direction relative to the bottoms of the two trenches 10c. The mesa 30 extends in the X direction with a predetermined width in the Y direction. The Y direction is an example of a second direction, and the X direction is an example of a third direction.

[0031] In this embodiment, the trench 10c is formed after the first semiconductor layer 12, the second semiconductor layer 13, and the third semiconductor layer 14 are stacked on the substrate 11. Therefore, the mesa 30 located between the two trenches 10c and the stacked portion 50 located on the opposite side of the mesa 30 with respect to the trench 10c in the Y direction and the opposite direction to the Y direction have the same stacked structure in which the same semiconductor layers are stacked in the same order.

[0032] The mesa 30 functions as a waveguide. In the mesa 30, the first semiconductor layer 12 is an example of a first cladding layer 31, which may also be referred to as a lower cladding layer. In the mesa 30, the second semiconductor layer 13 is an example of an active layer 32, which may also be referred to as a core layer. In the mesa 30, the third semiconductor layer 14 is an example of a second cladding layer 33, which may also be referred to as an upper cladding layer.

[0033] As shown in FIG. 1, the passivation film 15 covers the end face of the stacked portion 10 in which the trench 10c is formed, on the side opposite to the substrate 11. The passivation film 15 also covers the side face 10c1 and bottom face of the trench 10c. The passivation film 15 has a substantially constant thickness and extends in the X direction. An opening 15a is provided in the passivation film 15 at the end of the mesa 30 in the Z direction. The passivation film 15 is made of, for example, SiN. The passivation film 15 may also be called an insulating layer or a dielectric layer.

[0034] The second electrode 22 covers the passivation film 15 from the side opposite to the substrate 11. The second electrode 22 is a p-electrode. The second electrode 22 penetrates an opening 15a provided in the passivation film 15, and contacts and is electrically connected to the second cladding layer 33 (third semiconductor layer 14) of the mesa 30.

[0035] The conductive layer 16 is laminated in the Z direction on the second electrode 22. The conductive layer 16 is, for example, a plated layer made of Au. The conductive layer 16 also fills the trench 10c.

[0036] The first electrode 21 is laminated in the opposite Z direction to the end surface 10a of the substrate 11. The first electrode 21 is an n-electrode, and is electrically connected to the substrate 11. Note that the first electrode 21 may be provided at a location other than on the end surface 10a of the substrate 11, as long as it is electrically connected to the substrate 11.

[0037] When a current is applied between the first electrode 21 and the second electrode 22, the current flows in the mesa 30 substantially along the opposite direction to the Z direction.

[0038] In such a configuration, the active layer 32 may have defects due to oxidation or the like on the side surface 10c1 facing the trench 10c, or defects may occur during etching of the trench 10c. Such defects are a cause of optical damage to the active layer 32 due to light absorption. Therefore, in this embodiment, a window region 40 that covers the active layer 32 of the mesa 30 is provided along the Y direction of the mesa 30 and two side surfaces 10c1 facing the opposite direction to the Y direction. The window region 40 can expand the band gap near the side surface 10c1, thereby suppressing light absorption and thus optical damage.

[0039] In this embodiment, the window region 40 is configured as a mixed crystal layer 40A. A method for manufacturing an optical semiconductor element 100A including the mixed crystal layer 40A will be described below with reference to Figures 3 to 7. Figures 3 to 7 are cross-sectional views of the optical semiconductor element 100A at various stages during the manufacture of the optical semiconductor element 100A.

[0040] First, as shown in FIG. 3, a substrate 11, a first semiconductor layer 12, a second semiconductor layer 13, and a third semiconductor layer 14 are laminated in this order in the Z direction to form a laminated portion 10.

[0041] 4, a dielectric film 101 is formed on the Z-direction end face 10b of the laminated portion 10. The dielectric film 101 extends in the X-direction with a predetermined thickness in the Z-direction and a predetermined width in the Y-direction. The two dielectric films 101 are spaced apart in the Y-direction and extend parallel to each other in the X-direction.

[0042] 5, the third semiconductor layer 14 and the alloyed layer 40A with an expanded band gap are formed by an impurity free vacancy disordering (IFVD) method. Here, Ga diffused by rapid thermal annealing (RTA) is absorbed into the dielectric film 101, generating vacancies in the portion of the third semiconductor layer 14 that contacts the dielectric film 101, and the vacancies diffuse into the second semiconductor layer 13, which is the active layer, causing limited alloying of the second semiconductor layer 13 below the dielectric film 101.

[0043] Next, as shown in FIG. 6, the stacked portion 10 is selectively etched to form two trenches 10c. The trenches 10c are formed so as to penetrate the third semiconductor layer 14 and the second semiconductor layer 13 from the end face 10b to the first semiconductor layer 12. At this time, the trenches 10c are etched so that the mixed crystallization layer 40A remains on the other trench 10c side. As a result, the mixed crystallization layer 40A is formed in the mesa 30 along the side surface 10c1 facing the trench 10c of the mesa 30 in a state of covering the active layer 32 that has not been mixed. In addition, the mixed crystallization layer 40A is not provided along the entire side surface 10c1 of the trench 10c, but is provided on the active layer 32 and a part of the side surface 10c1 that is the periphery thereof.

[0044] Next, as shown in FIG. 7, a passivation film 15 is formed to cover the end of the stacked portion 10 in the Z direction and the inside of the trench 10c, and an opening 15a is formed in the passivation film 15 at the end of the mesa 30 in the Z direction.

[0045] Thereafter, a conductive layer 16 is laminated so as to cover the passivation film 15, and a second electrode 22 is formed to cover the conductive layer 16, and a first electrode 21 is formed on the end face 10a opposite the Z direction of the laminated portion 10, thereby obtaining the optical semiconductor element 100A shown in FIG. 1.

[0046] As described above, according to this embodiment, by providing the window region 40 that covers the active layer 32 along the side surface 10c1 in the mesa 30, it is possible to suppress deterioration and, in turn, optical damage of the active layer 32. This configuration is effective when the stacked portion 10, i.e., the semiconductor layer, is made of a GaAs-based semiconductor material.

[0047] [Second embodiment] 8 is a cross-sectional view of an optical semiconductor element 100B (100) according to the second embodiment. In this embodiment, the window region 40 is configured as an impurity diffusion layer 40B. Except for this, the optical semiconductor element 100B has the same configuration as the optical semiconductor element 100A according to the first embodiment.

[0048] A manufacturing process for the optical semiconductor element 100B including the impurity diffusion layer 40B will be described below with reference to Figures 9 and 10. Figures 9 and 10 are cross-sectional views of the optical semiconductor element 100B at various stages during the manufacturing process.

[0049] In this embodiment, the laminated portion 10 shown in FIG. 9 is formed, and two trenches 10c similar to those in the first embodiment are formed, and then an impurity diffusion layer 40B is formed as a window region 40. The impurity diffusion layer 40B is formed by injecting, for example, protons as impurities into the active layer 32 on the side surface 10c1 of the mesa 30 and its adjacent region. As a result, the impurity diffusion layer 40B is formed in the mesa 30 along the side surface 10c1 facing the trench 10c of the mesa 30 in a state covering the active layer 32 that has not been impurity diffused. In addition, the impurity diffusion layer 40B is not provided corresponding to the entire side surface 10c1 of the trench 10c, but is provided corresponding to the active layer 32 and a part of the side surface 10c1 that is the periphery thereof.

[0050] Next, as shown in FIG. 10, a passivation film 15 is formed to cover the end of the laminated portion 10 in the Z direction and the inside of the trench 10c, and an opening 15a is formed in the passivation film 15 at the end of the mesa 30 in the Z direction.

[0051] Thereafter, a conductive layer 16 is laminated so as to cover the passivation film 15, and a second electrode 22 is formed to cover the conductive layer 16, and a first electrode 21 is formed on the end face 10a opposite the Z direction of the laminated portion 10, thereby obtaining the optical semiconductor element 100B shown in FIG. 8.

[0052] In this embodiment as well, by providing an impurity diffusion layer 40B as a window region 40 that covers the active layer 32 along the side surface 10c1 within the mesa 30, deterioration of the active layer 32 and therefore optical damage can be suppressed.

[0053] [Third embodiment] 11 is a cross-sectional view of an optical semiconductor element 100C (100) according to the third embodiment. In this embodiment, the window region 40 is configured as a wide band gap layer 40C. Except for this, the optical semiconductor element 100C has a similar configuration to the optical semiconductor element 100A according to the first embodiment.

[0054] A method for manufacturing an optical semiconductor device 100C including a wide band gap layer 40C will now be described with reference to Figures 12 and 13. Figures 12 and 13 are cross-sectional views of optical semiconductor device 100C at various stages during the manufacture thereof.

[0055] In this embodiment, the stacked portion 10 shown in FIG. 12 is formed, and two trenches 10c similar to those in the first embodiment are formed, and then hydrogen cleaning is performed on the inner surfaces of the two trenches 10c. Then, a wide band gap layer 40C is formed as a window region 40 for the two trenches 10c. The wide band gap layer 40C is formed so as to cover the lower part including the bottom of the trench 10c including the active layer 32 on the side surface 10c1 of the mesa 30 and its adjacent region. The wide band gap layer 40C is made of, for example, ZnSe. As a result, the wide band gap layer 40C is formed outside the mesa 30 along the side surface 10c1 facing the trench 10c of the mesa 30 in a state of covering the active layer 32. In addition, the wide band gap layer 40C is not provided corresponding to the entire side surface 10c1 of the trench 10c, but is provided corresponding to the active layer 32 and a part of the side surface 10c1 that is the periphery thereof.

[0056] Next, as shown in FIG. 13, a passivation film 15 is formed so as to cover the end of the laminated portion 10 in the Z direction and the inside of the trench 10c, and an opening 15a is formed in the passivation film 15 at the end of the mesa 30 in the Z direction.

[0057] Thereafter, a conductive layer 16 is laminated so as to cover the passivation film 15, and a second electrode 22 is formed to cover the conductive layer 16, and a first electrode 21 is formed on the end face 10a opposite the Z direction of the laminated portion 10, thereby obtaining the optical semiconductor element 100C shown in FIG. 11.

[0058] According to this embodiment, by providing the wide band gap layer 40C outside the mesa 30 as the window region 40 that covers the active layer 32 along the side surface 10c1, deterioration of the active layer 32 and therefore optical damage can be suppressed.

[0059] [Fourth embodiment] FIG. 14 is a cross-sectional view of an optical semiconductor element 100D (100) of the fourth embodiment. The optical semiconductor element 100D of this embodiment has the same configuration as the first to third embodiments, except that the trench 10c and the stacked portion 50 (see FIG. 1, etc.) on the opposite side of the mesa 30 across the trench 10c are not provided. That is, in this embodiment, too, a window region 40 that covers the active layer 32 along the side surface 10c1 can be provided inside or outside the mesa 30, thereby suppressing deterioration of the active layer 32 and optical damage. The window region 40 may be any one of the mixed crystal layer 40A, the impurity diffusion layer 40B, and the wide band gap layer 40C.

[0060] [Fifth embodiment] FIG. 15 is a plan view of a part of the optical semiconductor device 100E (100) of the fifth embodiment. The optical semiconductor device 100E of this embodiment is configured as a semiconductor optical amplifier. The mesa 30 constituting the waveguide has a straight portion 30s having a substantially constant width in the Y direction and a tapered portion 30t whose width in the Y direction increases as it approaches the X direction. The tapered portion 30t may also be referred to as a widening portion. The straight portion 30s and the tapered portion 30t are provided between two trenches 10c, and both of these two trenches 10c extend from the second cladding layer 33 through the active layer 32 to the first cladding layer 31, and have a substantially constant depth in the opposite direction to the Z direction. A window region 40 is provided not only in the active layer 32 of the straight portion 30s but also in the active layer 32 of the tapered portion 30t.

[0061] In the optical semiconductor device 100E configured as a semiconductor optical amplifier having a tapered portion 30t as in this embodiment, a window region 40 that covers the active layer 32 along the side surface 10c1 (see FIG. 1) is provided inside or outside the mesa 30, thereby making it possible to suppress deterioration of the active layer 32 and, in turn, optical damage. Furthermore, in the tapered portion 30t, a trench 10c having a depth similar to that of the straight portion 30s is not originally required, but in this embodiment, by making the straight portion 30s and the tapered portion 30t have a similar configuration, including the trench 10c, an effect is obtained in that the manufacturing effort and cost can be further reduced.

[0062] [Sixth embodiment] FIG. 16 is a plan view of a part of the optical semiconductor device 100F (100) of the sixth embodiment. The optical semiconductor device 100F of this embodiment is also configured as a semiconductor optical amplifier, and has a similar configuration to the optical semiconductor device 100E of the fifth embodiment. However, in this embodiment, a gap 10d is provided between the straight portion 30s and the tapered portion 30t. The gap 10d has a groove-like shape, similar to the trench 10c. A window region 40 is also provided in the second semiconductor layer 13 adjacent to the gap 10d. In the optical semiconductor device 100F of this embodiment, the window region 40 that covers the active layer 32 is provided inside or outside the mesa 30 along the side surface 10c1 (see FIG. 1) of the trench 10c and the gap 10d, thereby suppressing deterioration of the active layer 32 and optical damage.

[0063] Although the embodiment and the modified examples of the present invention have been illustrated above, the above-mentioned embodiment and the modified examples are merely examples and are not intended to limit the scope of the invention. The above-mentioned embodiment and the modified examples can be implemented in various other forms, and various omissions, substitutions, combinations, and modifications can be made without departing from the gist of the invention. In addition, the specifications of each configuration, shape, and the like (structure, type, direction, model, size, length, width, thickness, height, number, arrangement, position, material, etc.) can be appropriately changed and implemented. [Explanation of symbols]

[0064] 10…Laminated section 10a...end face 10b...end face 10c…Trench 10c1…side 10d…Gap 11...Substrate 12...First semiconductor layer 13...Second semiconductor layer 14...Third semiconductor layer 15...Passivation film 15a…Aperture 16...Conductive layer 21...First electrode 22…Second electrode 30…Mesa 30t…Tapered section 30s…straight part 31…First cladding layer 32…Active layer 33…Second clad layer 40…Window area 40A…Mixed crystal layer 40B: Impurity diffusion layer 40C…Wide band gap layer 50…Laminated section 100A-100D: Optical semiconductor elements (semiconductor laser elements) 100E, 100F...Optical semiconductor element (semiconductor optical amplifier) 101...Dielectric film X…direction (third direction) Y…direction (second direction) Z…direction (first direction)

Claims

1. a mesa in which a first cladding layer, an active layer, and a second cladding layer are laminated in a first direction, the mesa extends in a third direction intersecting the first direction and the second direction with a predetermined width in a second direction intersecting the first direction, and the mesa has side surfaces at an end in the second direction and an end in a direction opposite to the second direction; a first electrode electrically connected to the first cladding layer; a second electrode electrically connected to the second cladding layer; Equipped with An optical semiconductor element, comprising: a window region that covers the active layer along the side surface.

2. 2. The optical semiconductor device according to claim 1, wherein the mesa has a portion made of a GaAs-based semiconductor material.

3. The optical semiconductor device according to claim 1 , wherein the window region is a mixed layer provided within the mesa.

4. The optical semiconductor device according to claim 1 , wherein the window region is an impurity diffusion layer provided within the mesa.

5. The optical semiconductor device according to claim 1 , wherein the window region is a wide band gap layer provided outside the mesa.

6. a laminated portion that is shifted in the second direction with respect to the mesa and has the same laminated structure as the mesa; The optical semiconductor device according to claim 1 , further comprising a trench provided between the stacked portion and the mesa.

7. The optical semiconductor element according to claim 1 , wherein the mesa has a portion in which the width changes in the third direction.

8. 8. The optical semiconductor element according to claim 1, configured as a semiconductor laser element.

9. 8. The optical semiconductor device according to claim 1, configured as a semiconductor optical amplifier.

10. forming a mesa in which a first cladding layer, an active layer, and a second cladding layer are stacked in a first direction, the mesa extends in a third direction intersecting the first direction and the second direction with a predetermined width in a second direction intersecting the first direction, and the mesa has side surfaces at an end in the second direction and an end in a direction opposite to the second direction; forming a first electrode electrically connected to the first cladding layer; forming a second electrode electrically connected to the second cladding layer; forming a window region covering the active layer along the side; The method for manufacturing an optical semiconductor element comprising the steps of: