Heat insulating material for combustion chamber, water heater and boiler
The combustion chamber insulation material with an inorganic cured material layer or ceramic plate addresses wind and water erosion issues, enhancing the durability and efficiency of boilers and water heaters.
Patent Information
- Application Number
- JP2023048126
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-24
- Publication Date
- 2024-10-04
AI Technical Summary
Existing heat-resistant materials used in combustion chambers of boilers and water heaters suffer from wind erosion and erosion caused by water droplets, leading to the peeling off of inorganic fibers and damage to the inorganic coating layer.
A combustion chamber insulation material comprising a plate-shaped molded body with an inorganic cured material layer or ceramic plate on its surface, bonded by a bonding layer, which is resistant to wind erosion and water droplet impact.
Prevents wind erosion and erosion of the insulation material due to combustion gas and water droplets, ensuring long-term durability and efficient operation of boilers and water heaters.
Smart Images

Figure 2024136844000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a combustion chamber insulation material, a water heater, and a boiler. [Background technology]
[0002] The inside of the combustion chamber, where heat treatment is performed in a high-temperature environment, becomes very hot, so refractories and heat insulating materials are placed inside the combustion chamber to prevent thermal damage to surrounding equipment and to reduce energy loss. As the heat insulating material, a plate-shaped heat insulating material formed from inorganic fibers and a binder may be used. In order to prevent the inorganic fibers from falling off, Patent Document 1 describes a heat-resistant material in which an inorganic fiber cloth is arranged on the surface of an inorganic fiber molded body, and further an inorganic coating layer is arranged on the surface of the inorganic fiber cloth. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2000-246821 A Summary of the Invention [Problem to be solved by the invention]
[0004] Devices equipped with a combustion chamber include boilers and oil water heaters, which are devices for heating water (steam). In boilers and oil water heaters, fuel is burned in the combustion chamber, and the combustion gases generated by the combustion are discharged into the flue as exhaust gases through water tubes and heat exchangers. During this time, the combustion gas exchanges heat with the water in each water tube and heat exchanger, heating the water in each water tube. The heated water can be used as a water heater.
[0005] Here, the heat-resistant material described in Patent Document 1 is intended for use in heat treatments used in semiconductor manufacturing processes, and is not intended for use in the combustion chambers of boilers or water heaters. If such heat-resistant materials are used as insulation, the insulation placed inside the combustion chamber of a boiler may be exposed to combustion gases, causing the fibers that make up the insulation to fall off and leading to wind erosion. Furthermore, since the flow of combustion gas in the combustion chamber is complex, the inorganic fiber cloth may peel off or turn up.
[0006] In addition, in the combustion chamber of the water heater, the combustion gas is cooled in a heat exchanger to generate condensed water, and the inorganic fibers constituting the heat-resistant material may be eroded by the impact of the water droplets falling on the bottom surface of the combustion chamber. In addition, the inorganic coating layer described in Patent Document 1 is a hard and brittle layer, and the long-term presence of condensed water droplets may damage and cause the inorganic coating layer to fall off.
[0007] The present invention has been made to solve the above problems, and has an object to provide a combustion chamber insulation material that is less susceptible to wind erosion due to combustion gases and erosion due to water droplets inside the combustion chamber. [Means for solving the problem]
[0008] The combustion chamber insulating material of the present invention comprises a plate-shaped molded body containing inorganic fibers, and an inorganic cured material layer or a ceramic plate arranged on at least one main surface of the plate-shaped molded body, wherein the plate-shaped molded body has a bonding layer containing the inorganic fibers and a binder on the main surface side on which the inorganic cured material layer or the ceramic plate is arranged, the inorganic cured material layer or the ceramic plate is bonded to the plate-shaped molded body by the bonding layer, and the inorganic cured material layer or the ceramic plate is arranged on the indoor side of the combustion chamber.
[0009] The combustion chamber insulating material of the present invention has an inorganic cured material layer or a ceramic plate on the surface disposed on the indoor side of the combustion chamber. By disposing the inorganic cured material layer or the ceramic plate on the surface disposed on the indoor side of the combustion chamber, wind erosion of the plate-shaped molded body by combustion gas can be prevented. In addition, the inorganic cured material layer or the ceramic plate is less likely to be damaged when struck by water droplets, and therefore, the plate-shaped molding can be prevented from being eroded by water droplets. Furthermore, by having the bonding layer on the main surface side on which the inorganic cured material layer or the ceramic plate is disposed, it is possible to prevent the inorganic cured material layer or the ceramic plate from peeling off from the plate-shaped product.
[0010] In the combustion chamber insulating material of the present invention, the inorganic cured material layer or the ceramic plate does not necessarily need to contain inorganic fibers.
[0011] In the combustion chamber insulating material of the present invention, when a drop of water is dropped with a dropper from 5 cm above the surface, it is preferable that the water absorption time of the bonding layer is 1 second or less, and the water absorption time of the inorganic cured material layer or the ceramic plate is 2 seconds or more. When the water absorption time of the bonding layer is within the above range, air is contained between the inorganic fibers constituting the bonding layer, and the heat insulating effect is high. On the other hand, when the water absorption time of the inorganic cured material layer or the ceramic plate is within the above range, the heat insulating material surface is dense and has high strength, water droplets remain on the heat insulating material surface, and the evaporation of the water droplets is promoted because the inside of the combustion chamber is at a high temperature, so that the erosion of the plate-shaped molded body by the water droplets can be prevented.
[0012] In the combustion chamber insulating material of the present invention, the binder is preferably silica sol and / or alumina sol. Silica sol and alumina sol are suitable as binders for use in combustion chamber insulating materials because of their excellent heat resistance.
[0013] It is preferable that the content of silica (SiO2) and / or alumina (Al2O3) in the bonding layer is at least 5 wt % higher than the content of silica and / or alumina in the portion of the plate-shaped body other than the bonding layer. When the bonding layer contains a large amount of the binder, namely, silica sol and / or alumina sol, the effect of preventing the inorganic cured material layer or the ceramic plate from peeling off from the plate-shaped molded article is enhanced.
[0014] The inorganic cured material layer or the ceramic plate preferably has a thickness of 0.2 mm or more. If the inorganic cured material layer or the ceramic plate is too thin, the effect of preventing the plate-shaped body from being eroded by combustion gases and from being eroded by water droplets may not be sufficiently obtained.
[0015] In the combustion chamber insulating material of the present invention, the surface of the combustion chamber inner side of the combustion chamber preferably has a concave shape. The surface of the combustion chamber heat insulating material on the inside of the combustion chamber has a recessed shape, so that water droplets can be collected in the recessed parts. Since the inside of the combustion chamber is at a high temperature, the water droplets collected in the recessed parts will eventually evaporate. Furthermore, if the water droplets can be evaporated, there is no need to remove the water droplets that have accumulated in the combustion chamber, which can improve the efficiency of the operation of the combustion chamber.
[0016] The water heater of the present invention comprises a combustion chamber, a heat exchanger installed in the combustion chamber, and a combustion chamber insulation material of the present invention installed at the bottom of the combustion chamber, and is characterized in that the combustion chamber insulation material is arranged so that the inorganic cured material layer or the ceramic plate is located directly below the heat exchanger.
[0017] The water heater of the present invention is equipped with the combustion chamber insulating material of the present invention, and since the inorganic cured material layer or the ceramic plate is located directly below the heat exchanger, it is possible to prevent the progress of erosion of the plate-shaped body due to water droplets dropping from the heat exchanger. It is also possible to prevent the progress of wind erosion of the plate-shaped body due to contact with combustion gas. Furthermore, since the plate-shaped body has a bonding layer, it is possible to prevent the inorganic cured material layer or the ceramic plate from peeling off from the plate-shaped body, and it can be used for a long period of time.
[0018] The boiler of the present invention is characterized by comprising a combustion chamber and the combustion chamber insulating material of the present invention installed in the bottom and / or ceiling of the combustion chamber.
[0019] The boiler of the present invention is equipped with the combustion chamber insulating material of the present invention and is less susceptible to wind erosion due to contact with combustion gas, so that the progress of wind erosion of the combustion chamber insulating material due to contact with combustion gas inside the boiler can be prevented. Furthermore, since the plate-shaped molded body has a bonding layer, peeling of the inorganic cured material layer or the ceramic plate from the plate-shaped molded body can be prevented, and the plate-shaped molded body can be used for a long period of time. [Brief description of the drawings]
[0020] [Figure 1] FIG. 1 is a perspective view that diagrammatically illustrates an example of a combustion chamber insulating material. [Diagram 2] FIG. 2 is a cross-sectional view taken along line AA of the combustion chamber insulating material shown in FIG. [Diagram 3] FIG. 3 is a cross-sectional view that illustrates an example of a water heater in which the combustion chamber insulating material of the present invention is disposed. [Figure 4] FIG. 4 is a cross-sectional view that illustrates an example of a boiler in which the combustion chamber insulating material of the present invention is disposed. [Diagram 5] FIG. 5 is a perspective view that diagrammatically shows another example of a combustion chamber insulating material. [Figure 6] FIG. 6 is a cross-sectional view of the combustion chamber insulating material shown in FIG. 5 taken along line BB. [Figure 7] FIG. 7 is a perspective view that diagrammatically shows another example of a combustion chamber insulating material. [Figure 8] FIG. 8 is a cross-sectional view taken along line CC of the combustion chamber insulating material shown in FIG. [Figure 9] FIG. 9 is a perspective view showing an example of a combustion chamber insulating material, in which a ceramic plate and a plate-shaped insulating material are separated. [Figure 10] FIG. 10 is a cross-sectional view taken along line DD of a combustion chamber insulating material formed by combining the ceramic plate and the plate-shaped insulating material shown in FIG. [Figure 11] FIG. 11 is a perspective view showing a schematic diagram of another example of a combustion chamber insulating material, in which a ceramic plate and a plate-shaped insulating material are separated. [Figure 12] FIG. 12 is a cross-sectional view taken along line EE of the combustion chamber insulation material formed by combining the ceramic plate and the plate-shaped insulation material shown in FIG.
[0021] Detailed Description of the Invention The combustion chamber insulating material, water heater, and boiler of the present invention will be specifically described below. However, the present invention is not limited to the following configurations, and can be appropriately modified and applied within the scope of the present invention. Note that the present invention also includes a combination of two or more of the individual preferred configurations of the present invention described below.
[0022] The combustion chamber insulating material of the present invention comprises a plate-shaped molded body containing inorganic fibers, and an inorganic cured material layer or a ceramic plate arranged on at least one main surface of the plate-shaped molded body, the plate-shaped molded body having a bonding layer containing the inorganic fibers and a binder on the main surface side on which the inorganic cured material layer or the ceramic plate is arranged, the inorganic cured material layer or the ceramic plate is bonded to the plate-shaped molded body by the bonding layer, and the inorganic cured material layer or the ceramic plate is arranged on the indoor side of the combustion chamber.
[0023] The combustion chamber insulating material of the present invention includes a plate-like molded body having a layer of an inorganic cured material disposed on at least one main surface thereof, and a plate-like molded body having a ceramic plate disposed thereon.
[0024] (Insulating material for combustion chambers with inorganic hardened material layer) First, a combustion chamber insulating material having a plate-like molded body and an inorganic cured material layer disposed on at least one main surface thereof will be described. FIG. 1 is a perspective view that shows a schematic diagram of an example of a combustion chamber insulating material, and FIG. 2 is a cross-sectional view taken along line AA of the combustion chamber insulating material shown in FIG. The combustion chamber insulating material 1 shown in FIG. 1 is formed by disposing an inorganic cured material layer 20 on the main surface of a plate-like molded body 10 . The inorganic cured material layer 20 is disposed on the upper surface (first main surface 11) of the plate-like molded body .
[0025] The shape of the plate-like molded body may be a plate shape, which is a shape having two opposing main surfaces with relatively large areas and a side surface connecting the two main surfaces. A plate-like molded body 10 shown in FIGS. 1 and 2 has a first main surface 11 and a second main surface 12, and has a side surface 13 connecting the first main surface 11 and the second main surface 12. In the plate-like molded body 10 , the area of the second main surface 12 is relatively larger than the area of the first main surface 11 . Moreover, the first main surface 11 and the second main surface 12 are substantially parallel surfaces. The top surface shapes of the first main surface 11 and the second main surface 12 are both circular, but the shape is not limited to circular. In addition, the area relationship between the first main surface and the second main surface may be such that the first main surface is larger, or the area of the first main surface and the area of the second main surface may be the same. The plate-shaped body 10 has an overall shape in which the top of a cone is cut along a plane parallel to the bottom. As shown in Fig. 2, the cross-sectional shape of the plate-shaped body 10 is substantially trapezoidal. For example, the circular diameter of the first main surface can be about 150 to 500 mm, and the circular diameter of the second main surface can be about 180 to 530 mm.
[0026] The thickness of the plate-shaped body is preferably 15 to 60 mm. If the thickness of the plate-shaped body is 15 mm or more, sufficient heat insulation can be ensured. On the other hand, if the thickness of the plate-shaped body is more than 60 mm, it is too large for the volume of the combustion chamber, and the heat insulating material for the combustion chamber becomes heavy, which is not preferable.
[0027] The plate-like molded body is a molded body containing inorganic fibers. Examples of the plate-like molded body include a molded body obtained by pouring a slurry containing inorganic fibers into a mold and suction-dehydrating the slurry, followed by drying, and a molded body obtained by solidifying an amorphous product containing inorganic fibers, molding the product, and drying the product. The plate-like molded product is preferably a molded product obtained by suction dehydration of inorganic fibers, molding the same into a paper molded product, and drying the same, that is, a paper molded product, and the bulk density of the molded product is preferably 0.3 to 0.6 g / cm. 3 The inorganic fibers constituting the papermaking molded product preferably have an average fiber length of 0.05 to 3.0 mm, and more preferably 0.5 to 1.5 mm.
[0028] Also, as the plate-shaped molded body, a molded body formed by needling inorganic fibers, i.e., a needle molded body, can be used. The needle molded body is a molded body in which inorganic fibers having a relatively long fiber length are entangled by needling to maintain their shape, and is cut into various shapes. The bulk density of the needle molded body is 0.05 to 0.2 g / cm. 3 The inorganic fibers constituting the needle-shaped body preferably have an average fiber length of 1 to 150 mm, and more preferably 10 to 80 mm.
[0029] As the inorganic fibers, at least one type of fiber selected from the group consisting of biosoluble fibers, alumina fibers, silica fibers, aluminosilicate fibers, rock wool, and glass fibers can be used. As the biosoluble fiber, alkaline earth silicate fiber can be used.
[0030] The plate-shaped molded body has a bonding layer containing inorganic fibers and a binder on at least one main surface side. The inorganic cured material layer described below is bonded to the plate-shaped molded body by the bonding layer. By having the bonding layer on the plate-shaped molded body, it is possible to prevent the inorganic cured material layer from peeling off from the plate-shaped molded body. Note that it is not prohibited to provide a bonding layer on a surface other than the main surface bonded to the inorganic cured material layer.
[0031] In the combustion chamber insulating material 1 shown in FIGS. 1 and 2, the bonding layer 16 is formed on the first main surface 11 side of the plate-shaped body 10. By forming the bonding layer on the first main surface side of the plate-shaped molded body and disposing the inorganic cured material layer on the first main surface of the plate-shaped molded body, it is possible to prevent the inorganic cured material layer from peeling off from the plate-shaped molded body.
[0032] In the bonding layer, the inorganic fibers are attached to the binder and integrated, and the bonding layer has liquid permeability. As an index of the liquid permeability of the bonding layer, it is preferable that the water absorption time is 1 second or less when one drop of water is dropped from 5 cm above the surface of the bonding layer using a dropper. The water absorption time is more preferably 0.5 seconds or less. When the water absorption time of the bonding layer is within the above range, air is contained between the inorganic fibers constituting the bonding layer, and the heat insulating effect of the combustion chamber insulation material of the present invention is high.
[0033] The thickness of the bonding layer is preferably 0.5 mm or more, more preferably 1 to 10 mm. If the thickness of the bonding layer is too thin, the effect of bonding the inorganic cured material layer may not be sufficiently obtained. On the other hand, if the thickness of the bonding layer is too thick, the binder is used in excess, and a film of the binder is formed, which may impair the heat insulation.
[0034] The bonding layer is preferably formed in a range of 50% or more of the area of the first main surface of the plate-like molded body.More preferably, the bonding layer is formed in a range of 70% or more of the area of the first main surface of the plate-like molded body.The bonding layer is intended to bond the inorganic cured material layer and the plate-like molded body, so it is preferably formed at the position where the inorganic cured material layer is to be disposed.
[0035] As the binder, it is preferable to use an inorganic adhesive. The inorganic adhesive is not particularly limited, and examples thereof include sodium silicate, silica sol, alumina sol, zirconia sol, titania sol, etc. As the inorganic adhesive, it is preferable to use silica sol and / or alumina sol. Silica sol and alumina sol are excellent in heat resistance, and therefore are suitable as binders used in combustion chamber insulation materials.
[0036] The content of silica (SiO2) and / or alumina (Al2O3) in the bonding layer is preferably 5% by weight or more higher than the content of silica and / or alumina in the portion of the plate-shaped molded body other than the bonding layer. If the bonding layer contains a large amount of silica sol and / or alumina sol as a binder, the effect of preventing the inorganic cured material layer from peeling off from the plate-shaped molded body is enhanced. In this specification, the silica and alumina contents are values measured by a fluorescent X-ray analyzer.
[0037] The bonding layer can be formed by applying a binder such as silica sol to the surface of the plate-shaped molded body. A part of the binder penetrates into the plate-shaped molded body from the surface and is integrated with the inorganic fibers.
[0038] In the combustion chamber insulating material, an inorganic cured material layer is disposed on at least one main surface of a plate-shaped molded body. As described above, a bonding layer is formed on the main surface of the plate-shaped molded body on which the inorganic cured material layer is disposed. The inorganic cured material layer is disposed on the interior side of the combustion chamber. Therefore, the inorganic cured material layer is provided on the surface disposed on the interior side of the combustion chamber, taking into account the shape of the combustion chamber insulating material and the shape of the combustion chamber. However, this does not preclude the provision of an inorganic cured material layer on a surface other than the "surface disposed on the interior side of the combustion chamber."
[0039] By disposing the inorganic cured material layer on the surface that is disposed on the interior side of the combustion chamber, it is possible to prevent wind erosion of the plate-shaped molded body due to combustion gas. In addition, the inorganic cured material layer is less likely to be damaged when struck by water droplets, and therefore, the plate-shaped molded article can be prevented from being eroded by water droplets. That is, the plate-shaped molded body is protected by the inorganic cured material layer, and the plate-shaped molded body is less susceptible to wind erosion of the plate-shaped molded body by combustion gas and erosion of the plate-shaped molded body by water droplets, making the heat insulating material for combustion chambers.
[0040] In the combustion chamber insulating material 1 shown in Figures 1 and 2, the inorganic cured material layer 20 is disposed on the first main surface 11 of the plate-shaped molded body 10. In other words, the inorganic cured material layer 20 is disposed on the upper surface of the bonding layer 16 of the plate-shaped molded body 10. By placing an inorganic cured material layer on a first main surface of a plate-shaped molding and positioning the first main surface on the side that comes into contact with combustion gas or on the side that comes into contact with water droplets directly below a heat exchanger, it is possible to prevent wind erosion of the plate-shaped molding due to combustion gas and erosion of the plate-shaped molding due to water droplets.
[0041] The inorganic cured material layer preferably covers 50% or more of the area of the first main surface of the plate-like molded body. When the inorganic cured material layer covers 50% or more of the area of the first main surface of the plate-like molded body, the protective effect of the inorganic cured material layer is more suitably exhibited. In addition, the inorganic cured material layer preferably covers 70% or more of the area of the first main surface of the plate-like molded body. The inorganic cured material layer preferably covers 50% or more of the area of the portion on the first main surface of the plate-like molded product where the bonding layer is formed.
[0042] The inorganic cured material layer is preferably a dense layer having poor liquid permeability. When the inorganic cured material layer is a dense layer, wind erosion of the plate-shaped molded body due to combustion gas and erosion of the plate-shaped molded body due to water droplets can be more suitably prevented.
[0043] As an index of the liquid permeability of the inorganic cured material layer, when one drop of water is dropped from 5 cm above the surface of the inorganic cured material layer using a dropper, the water absorption time is preferably 2 seconds or more. The water absorption time is more preferably 5 seconds or more. When the water absorption time of the inorganic cured material layer is within the above range, erosion of the plate-shaped molded body by the water droplets can be prevented.
[0044] The inorganic cured material layer is preferably a layer of an unshaped refractory material. Examples of the unshaped refractory material include refractory mortar, a castable material which is a refractory material made by mixing a refractory aggregate with a cement material or a chemical binder, and an inorganic binder. It may also be a coating layer containing glass. It may also be a layer containing natural clay or synthetic clay.
[0045] The inorganic cured material layer can be formed by applying an amorphous refractory material or the like to the surface of the plate-shaped molded body, i.e., the surface of the bonding layer of the plate-shaped molded body, and drying it. Furthermore, a part of the inorganic cured material layer may be integrated with the inorganic fibers and binder present in the bonding layer by penetrating into a part of the bonding layer. In this case, a part of the inorganic cured material layer may be a mixture of an inorganic material such as an amorphous refractory material or glass, a binder, and inorganic fibers constituting the plate-shaped molded body. A part of the inorganic cured material layer may not contain inorganic fibers. The entire inorganic cured material layer may not contain inorganic fibers.
[0046] The thickness of the inorganic cured material layer is preferably 0.2 mm or more, more preferably 0.4 to 7 mm. If the thickness of the inorganic cured material layer is less than 0.2 mm, the effect of preventing the plate-shaped molded body from being eroded by combustion gas and the erosion of the plate-shaped molded body from being eroded by water droplets may not be sufficiently obtained. On the other hand, if the thickness of the inorganic cured material layer is too thick, it may become necessary to reduce the thickness of the plate-shaped molded body in order to secure the combustion chamber space. In that case, the heat insulating property of the combustion chamber insulation material may be reduced. In addition, the thickness of the inorganic cured material layer may be uniform or non-uniform, and the surface may be uneven or spotty. In addition, in the case where at least a part of the inorganic cured material layer is a mixture of an inorganic material such as an amorphous refractory material or glass and an inorganic fiber and a binder that constitute the bonding layer, even if inorganic fibers are present, it is regarded as an inorganic cured material layer and is included in the thickness of the inorganic cured material layer.
[0047] The combustion chamber insulation material can be obtained by obtaining a paper molded body or a needle molded body as a plate-shaped molded body, applying a binder to at least one of its main surfaces, and then applying a slurry containing an amorphous refractory material to the main surface to which the binder has been applied, and drying the same. Alternatively, after a paper molded product or needle molded product is obtained as a plate-like molded product, a binder is applied to the product, and then a glass slurry containing a glass material, a binder, etc. is applied to the product, followed by drying. After the binder is applied to the plate-like molded body, the plate-like molded body may be dried and then the slurry or the like may be applied thereto. Alternatively, the plate-like molded body may be coated with the slurry or the like without being dried.
[0048] Although the method of applying the slurry containing the amorphous refractory or the glass slurry is not particularly limited, it is preferable to apply the slurry to the plate-shaped molded body with a trowel or the like, and then add more slurry and apply it using a scraper, etc. By performing the work of adding and applying the slurry, it is possible to reduce uncoated areas, make the thickness of the inorganic cured material layer uniform, and reduce the occurrence of pinholes.
[0049] The combustion chamber insulating material of the present invention can be used by being placed inside the combustion chamber of an apparatus having a combustion chamber. Examples of devices having a combustion chamber include water heaters for supplying hot water and boilers for supplying steam.
[0050] A water heater in which the combustion chamber insulating material of the present invention is disposed is the water heater of the present invention. The water heater of the present invention comprises a combustion chamber, a heat exchanger arranged in the combustion chamber, and the combustion chamber insulation material of the present invention arranged at the bottom of the combustion chamber, and is characterized in that the combustion chamber insulation material is arranged so that the inorganic cured material layer or ceramic plate is located directly below the heat exchanger.
[0051] FIG. 3 is a cross-sectional view that illustrates an example of a water heater in which the combustion chamber insulating material of the present invention is disposed. The water heater 100 has a combustion chamber 110 and a heat exchanger 120 disposed in the combustion chamber 110 . Water flows through heat exchanger 120 , and the water within heat exchanger 120 is heated in combustion chamber 110 to become hot water, which is then supplied to the outside of water heater 100 .
[0052] The combustion chamber insulating material 1 is disposed at the bottom of the combustion chamber 110 such that the inorganic cured material layer 20 is located directly below the heat exchanger 120 . In the combustion chamber, condensed water is generated by cooling the combustion gas in the heat exchanger, and may fall to the bottom of the combustion chamber. Figure 3 shows water droplets 130 falling from the heat exchanger 120 to the bottom of the combustion chamber 110.
[0053] When the inorganic cured material layer 20 is provided directly below the heat exchanger 120, that is, in a position corresponding to the position where the water droplets 130 fall, the water droplets falling from the heat exchanger do not pass through the inorganic cured material layer 20 and do not reach the plate-shaped molded body 10. Therefore, the inorganic cured material layer 20 can prevent the progress of erosion of the plate-shaped molded body 10. In addition, the inorganic cured material layer 20 can also prevent the progress of wind erosion of the plate-shaped molded body 10 due to contact with combustion gas. In addition, since the plate-shaped molded body 10 has the bonding layer 16, the inorganic cured material layer 20 is prevented from peeling off from the plate-shaped molded body 10, and the plate-shaped molded body 10 can be used for a long period of time.
[0054] Moreover, a boiler in which the combustion chamber insulating material of the present invention is disposed is the boiler of the present invention. The boiler of the present invention is characterized by comprising a combustion chamber and the combustion chamber insulating material of the present invention arranged in the bottom and / or ceiling of the combustion chamber.
[0055] FIG. 4 is a cross-sectional view that illustrates an example of a boiler in which the combustion chamber insulating material of the present invention is disposed. The boiler 200 has a combustion chamber 210 and water tubes 220 disposed within the combustion chamber 210 . Water is supplied into the water pipe 220 from the lower part of the combustion chamber 210 , and the water passing through the water pipe 220 is heated in the combustion chamber 210 and turns into steam, which is discharged from the upper part of the combustion chamber 210 . The discharged water vapor is used for power generation, heating, cleaning, cooking, drying, disinfection, sterilization, etc. after separating the liquid water or superheating as necessary.
[0056] The combustion chamber insulating material 1 of the present invention is disposed on the ceiling 210 a and bottom 210 b of the combustion chamber 210 such that the inorganic cured material layer 20 is located on the interior side of the combustion chamber 210 .
[0057] Although the boiler is not structured such that water droplets fall onto the combustion chamber insulation material, the combustion chamber insulation material of the present invention is less susceptible to wind erosion due to contact with combustion gas, and therefore the progress of wind erosion of the plate-shaped molded body due to contact with combustion gas in the boiler is prevented. In addition, the combustion chamber insulation material of the present invention has a bonding layer on the plate-shaped molded body, which prevents the inorganic cured material layer from peeling off from the plate-shaped molded body and allows for long-term use. Since the falling of water droplets is not a consideration, the combustion chamber insulation material of the present invention may be provided on the ceiling of the combustion chamber.
[0058] (Another embodiment of the combustion chamber insulation material) Another embodiment of the thermal insulating material for a combustion chamber will be described below by taking as an example a thermal insulating material for a combustion chamber having an inorganic cured material layer.
[0059] In the combustion chamber insulating material of the present invention, the surface of the combustion chamber insulating material facing the inside of the combustion chamber may have a recessed shape. FIG. 5 is a perspective view that shows a schematic diagram of another example of a combustion chamber insulating material, and FIG. 6 is a cross-sectional view taken along the line BB of the combustion chamber insulating material shown in FIG. The combustion chamber insulating material 2 shown in Figures 5 and 6 is formed by disposing an inorganic cured material layer 20 on the main surface of a plate-shaped molded body 10. A recessed shape 14 is provided on the first main surface 11 of the plate-shaped molded body 10, and the inorganic cured material layer 20 is provided along the recessed shape 14. Therefore, a recessed shape 24 is also provided on the surface of the inorganic cured material layer 20, which is the surface on the inside of the combustion chamber in the combustion chamber insulating material 2. Since the recessed shape 14 is provided on the first main surface 11 of the plate-shaped molded body 10, the bonding layer 16 is also formed along the recessed shape 14.
[0060] The surface of the combustion chamber insulation material on the inside of the combustion chamber has a concave shape, so water droplets can accumulate in the concave shape. Since the temperature inside the combustion chamber is high, the water droplets that accumulate in the concave shape will eventually evaporate. If the water droplets can be evaporated, there is no need to remove the water droplets that have accumulated in the combustion chamber, which makes the operation of the combustion chamber more efficient.
[0061] When the water heater starts operating, the temperature inside the combustion chamber is not very high, but a lot of condensation occurs, so water droplets tend to accumulate in the depressions. As the water heater continues to operate, the temperature inside the combustion chamber rises, the evaporation rate of the water accumulated in the depressions increases, and the amount of water accumulated in the depressions decreases. The depth and width of the recess may be determined to be the size required when the most water droplets accumulate during operation of the water heater. If the recess is too deep, the thickness of the combustion chamber insulation material will be insufficient, and the strength and heat insulating properties of the combustion chamber insulation material will decrease, so it is preferable that the recess is not too deep. For example, it is preferable that the depth of the recessed shape is about 1 / 3 or less of the thickness of the combustion chamber insulating material.
[0062] In the combustion chamber insulation of the present invention, a flow path with an incline may be provided on the surface of the combustion chamber insulation facing the inside of the combustion chamber to allow liquid to flow from the combustion chamber insulation to the outside of the combustion chamber. FIG. 7 is a perspective view that shows a schematic diagram of another example of a combustion chamber insulating material, and FIG. 8 is a cross-sectional view taken along line CC of the combustion chamber insulating material shown in FIG. The combustion chamber insulating material 3 shown in Figures 7 and 8 is formed by disposing an inorganic cured material layer 20 on the main surface of a plate-shaped molded body 10. A flow path 15 with an inclination is provided on the first main surface 11 of the plate-shaped molded body 10, and the inorganic cured material layer 20 is provided along the flow path 15. Therefore, a flow path 25 is also provided on the surface of the inorganic cured material layer 20, which is the surface on the inside of the combustion chamber in the combustion chamber insulating material 3. Since the flow path 15 with an inclination is provided on the first main surface 11 of the plate-shaped molded body 10, the bonding layer 16 is also formed along the flow path 15.
[0063] In Fig. 8, the surface of the plate-shaped molded body has an inclination such that the left side is higher and the right side is lower. Therefore, the flow path 15 (flow path 25) is a flow path through which water flows from left to right in Fig. 8. By connecting another flow path leading to the outside of the combustion chamber to the end of the flow path 15 (flow path 25) of the combustion chamber insulation material 3, the water can be discharged outside the combustion chamber.
[0064] 7, the first main surface 11 of the plate-shaped molded body 10 has a recess 14 (recess 24), so that the periphery of the plate-shaped molded body is higher than the recess 14 (recess 24). Therefore, water droplets collect in the recess 14 (recess 24), and the collected water flows along the flow path 15 (flow path 25). Near the outer periphery of the combustion chamber insulation, the portions other than the flow paths are higher than the flow paths, so that water does not leak out of the combustion chamber insulation from the portions other than the flow paths.
[0065] When a large amount of water droplets fall on the inorganic cured material layer, the water droplets may not be able to evaporate completely on the inorganic cured material layer. If such a case is expected, a flow path is provided in the heat insulating material for the combustion chamber so that the water droplets falling on the inorganic cured material layer flow out of the combustion chamber, thereby preventing the water droplets from eroding other parts of the combustion chamber.
[0066] (Insulation for combustion chamber with ceramic plate) Next, a combustion chamber insulating material having a ceramic plate disposed on at least one main surface of a plate-shaped body will be described. This combustion chamber insulating material is a ceramic plate instead of an inorganic cured material layer on at least one of the main surfaces of a plate-shaped molded body, and can be placed in the combustion chamber of an apparatus having a combustion chamber in the same manner as the combustion chamber insulating material having an inorganic cured material layer described above. Since the configuration is the same except for replacing the inorganic cured material layer with a ceramic plate, detailed description of the configuration other than the ceramic plate will be omitted.
[0067] Figure 9 is a schematic perspective view of an example of a combustion chamber insulation material, showing the ceramic plate and the plate-shaped insulation material separated, and Figure 10 is a cross-sectional view along line DD of a combustion chamber insulation material that combines the ceramic plate and the plate-shaped insulation material shown in Figure 9.
[0068] The combustion chamber insulating material 4 shown in FIGS. 9 and 10 has a ceramic plate 30 disposed on the upper surface (first main surface 11) of a plate-shaped body . As the plate-like molded body 10, the above-mentioned ones can be used.
[0069] The ceramic plate 30 is disposed on the surface of the combustion chamber insulation material that is disposed on the indoor side of the combustion chamber. By disposing the ceramic plate on the surface of the combustion chamber insulation material that is disposed on the indoor side of the combustion chamber, it is possible to prevent wind erosion of the plate-shaped body by combustion gas. Furthermore, the ceramic plate is less likely to be damaged when struck by water droplets, and therefore the plate-shaped body can be prevented from being eroded by water droplets. That is, the plate-shaped body is protected by the ceramic plate, and the plate-shaped body is less susceptible to wind erosion of the plate-shaped body by combustion gas and erosion of the plate-shaped body by water droplets, making the combustion chamber insulating material.
[0070] The ceramic plate is preferably a dense ceramic plate having poor liquid permeability. If the ceramic plate is dense, it is possible to more effectively prevent the plate-shaped body from being eroded by combustion gas and from being eroded by water droplets. The material of the ceramic plate is not particularly limited, but examples thereof include alumina, mullite, zirconia, titania, cordierite, silicon carbide, silicon nitride, forsterite, steatite, sialon, and the like. The ceramic plate preferably does not contain inorganic fibers.
[0071] As an index of the liquid permeability of the ceramic plate, when a drop of water is dropped onto the surface of the ceramic plate from 5 cm above with a dropper, the water absorption time is preferably 2 seconds or more. The water absorption time is more preferably 5 seconds or more. When the water absorption time of the ceramic plate is within the above range, erosion of the plate-shaped molding by the water droplets can be prevented.
[0072] The thickness of the ceramic plate is preferably 0.2 mm or more, and preferably 1 to 7 mm. If the thickness of the ceramic plate is too thin, the strength of the ceramic plate may be insufficient and the ceramic plate may crack. In addition, the effect of preventing the wind erosion of the plate-shaped body by combustion gas and the erosion of the plate-shaped body by water droplets may not be sufficiently obtained. On the other hand, if the thickness of the ceramic plate is thick, it is necessary to reduce the thickness of the plate-shaped body of the combustion chamber insulation material to secure the combustion chamber space, and in that case, the heat insulating property of the combustion chamber insulation material may be reduced. In addition, the thickness of the ceramic plate may be uniform or non-uniform, and the surface may be uneven or spotty.
[0073] The combustion chamber insulation material can be obtained by obtaining a paper molded body or a needle molded body as a plate-shaped molded body, applying the above-mentioned binder to at least one of its main surfaces to form a bonding layer, and then adhering a ceramic plate to it.
[0074] In a combustion chamber insulating material having a ceramic plate disposed on at least one of the main surfaces of a plate-shaped body, the surface of the combustion chamber insulating material facing the combustion chamber may also have a recessed shape or flow paths. In this case, the recesses and the flow paths may be provided in the ceramic plate, and the plate-shaped molded body does not need to have the recesses and the flow paths. An example in which the recesses are provided in the ceramic plate will be described below.
[0075] Figure 11 is a schematic perspective view of another example of a combustion chamber insulation material, showing the ceramic plate and the plate-shaped insulation material separated, and Figure 12 is a cross-sectional view along line EE of a combustion chamber insulation material that combines the ceramic plate and the plate-shaped insulation material shown in Figure 11.
[0076] The combustion chamber insulating material 5 shown in FIGS. 11 and 12 is configured by disposing a ceramic plate 40 having recesses 44 on the upper surface (first main surface 11) of a plate-shaped body 10. A ceramic plate 40 having a recessed shape 44 can be prepared by forming a recessed shape 44 in the ceramic plate by a technique such as machining the main surface of the flat ceramic plate, and the ceramic plate 40 can be bonded to the upper surface of the plate-shaped molded body 10 to obtain the combustion chamber insulation material 5. The combustion chamber insulating material 5, like the combustion chamber insulating material 2 described above, can exhibit an effect due to having a recessed shape on the surface.
[0077] Also, although not shown in the drawings, a ceramic plate having a flow passage can be prepared by forming a flow passage in the ceramic plate by a method such as machining the main surface of the flat ceramic plate, and then the ceramic plate having the flow passage can be bonded to the upper surface of the plate-shaped molded body to obtain a combustion chamber insulating material. The combustion chamber insulating material having the flow passage can exhibit the effects of having the flow passage on the surface, similar to the combustion chamber insulating material 3 described above. [Explanation of symbols]
[0078] 1, 2, 3, 4, 5 Combustion chamber insulation 10 Plate-shaped molded body 11 First main surface 12 Second main surface 13 Side 14 Concave shape 15 Flow Path 16 Bonding layer 20 Inorganic cured material layer 24 Concave shape 25 Flow Path 30, 40 Ceramic plate 44 Concave shape 100 Water heater 110 Combustion chamber 120 Heat exchanger 130 water drops 200 Boiler 210 Combustion chamber 210a Ceiling 210b bottom 220 Water pipe
Claims
1. A plate-shaped molded body containing inorganic fibers; An inorganic cured material layer or a ceramic plate arranged on at least one main surface of the plate-shaped molded body, The plate-shaped molded body has a bonding layer containing the inorganic fibers and a binder on a main surface side on which the inorganic cured material layer or the ceramic plate is disposed, the inorganic cured material layer or the ceramic plate is bonded to the plate-like molded body by the bonding layer, 13. A thermal insulation material for a combustion chamber, characterized in that the inorganic cured material layer or the ceramic plate is disposed on the interior side of a combustion chamber.
2. The insulating material for a combustion chamber according to claim 1 , wherein the inorganic cured material layer or the ceramic plate does not contain inorganic fibers.
3. 2. The combustion chamber insulating material according to claim 1, wherein when a drop of water is dropped from 5 cm above the surface using a dropper, the bonding layer has a water absorption time of 1 second or less, and the inorganic cured material layer or the ceramic plate has a water absorption time of 2 seconds or more.
4. 2. The insulating material for a combustion chamber according to claim 1, wherein the binder is silica sol and / or alumina sol.
5. The silica (SiO 2 ) component and / or alumina (Al 2 O 3 5. The combustion chamber insulating material according to claim 4, wherein the content of the silica component and / or the alumina component in the portion of the plate-like molded body other than the bonding layer is at least 5% by weight higher.
6. 2. The thermal insulating material for a combustion chamber according to claim 1, wherein the inorganic cured material layer or the ceramic plate has a thickness of 0.2 mm or more.
7. 2. The combustion chamber insulating material according to claim 1, wherein the surface of the combustion chamber inner side of the combustion chamber insulating material has a concave shape.
8. A combustion chamber; A heat exchanger installed in the combustion chamber; and a combustion chamber insulating material according to any one of claims 1 to 7, which is installed at the bottom of the combustion chamber; A water heater, characterized in that the combustion chamber insulation material is arranged so that the inorganic cured material layer or the ceramic plate is located directly below the heat exchanger.
9. A combustion chamber; A boiler comprising the combustion chamber insulating material according to any one of claims 1 to 7, which is installed in the bottom and / or ceiling of a combustion chamber.
Citation Information
Patent Citations
Heat resistant material and its manufacture
JP2000246821A