Display device
Patent Information
- Application Number
- JP2024113772
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2017-04-04
- Filing Date
- 2024-07-17
- Publication Date
- 2024-10-07
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
【0032】 運転者などの利用者に対して広い面積の表示領域を提供し、広い面積の表示領域に表示さ れる情報を利用することで運転者の安全運転を確保することができる。
Smart Images

Figure 2024137986000001_ABST
Abstract
Description
[Technical field]
[0001] The technical field of one embodiment of the invention disclosed in this specification and the like relates to an object, a method, or a manufacturing method. Alternatively, one aspect of the present invention is a process, a machine, a manufacture, or , composition of matter. The technical field of one embodiment of the present invention disclosed in this specification is a semiconductor device, a display device, a light-emitting device, device, lighting device, power storage device, storage device, driving method thereof, or manufacturing method thereof, It should be noted that the present invention is not limited to the above-mentioned technical fields. stomach.
[0002] In this specification, a semiconductor device is a device that can function by utilizing semiconductor characteristics. Generally speaking, electro-optical devices, semiconductor circuits, and electronic devices are all semiconductor devices. [Background technology]
[0003] Development is underway to replace some of the instrument displays in automobiles with liquid crystal displays. In addition, more information (such as information about the surroundings of the vehicle, traffic information, and geographic information) will be utilized. To this end, efforts are being made to assist drivers of automobiles and other vehicles by using displays inside the vehicle. There are.
[0004] In the future, a large number of cameras and sensors will be installed inside and outside the vehicle.
[0005] A display panel having a curved surface is disclosed in Patent Document 1. Patent Document 2 discloses a display device having a non-rectangular display area. Such a device is disclosed in Patent Document 3. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] Patent Publication No. 2003-229548 [Patent Document 2] Patent Publication 2014-197179 [Patent Document 3] Patent Publication 2015-180924 Summary of the Invention [Problem to be solved by the invention]
[0007] To display danger warnings to the driver according to the situation obtained from various cameras and sensors In order to achieve this, a display area that corresponds to the number of cameras and sensors is required. However, the interior of the car is a limited space surrounded by windows, and there are few places inside the car where a display unit can be installed. The place has a surface with many irregularities, including curved surfaces.
[0008] In addition, when a display panel with a large flat surface and thickness is installed on the dashboard, , obstructing the driver's view. [Means for solving the problem]
[0009] A plurality of display panels having curved surfaces are arranged in a limited space. The display panel has an overlapping area. At least one of the display panels has a curved surface. Alternatively, the other display panel may be flat.
[0010] Two or more display panels are combined to form a single display area with a T-shaped outer edge. Therefore, a display panel that combines video signals for one T-shaped display area is constructed. In other words, two or more systems are used for each display area as necessary. Therefore, if the driver does not need the entire display, the multiple displays that make up one display area can be switched off. By setting a period during which the power supplied to one of the display panels is zero, It can also be electrified.
[0011] One aspect of the present invention is a display device having a first display panel, a second display panel, and a third display panel. The first display panel has a first region and a second region, and the second display panel has a first region and a second region. The first display panel has a third region and a fourth region, and the second display panel has a fifth region and a sixth region. The first region, the third region, and the fifth region have a function of transmitting visible light, and the second region The first, fourth and sixth regions have a display function, and the first region of the first display panel The first region and the fourth region of the second display panel have a first portion that overlaps with each other, and the third region The fifth region of the display panel and the second region of the first display panel are arranged to overlap each other. a fifth region of the third display panel and a fourth region of the second display panel are mutually a third portion overlapping the second region, a fourth region, and a sixth region; The single display area is a display device having a roughly T-shape.
[0012] Multiple display panels are fixed to the curved surface of the dashboard inside the car, and the It is preferable to overlap the ends of the display panel to form a single display area. In order to overlap the transparent area around the display area with the display area of the adjacent display panel, It is desirable that each display panel be thin. Therefore, the display panel is made of plastic. A display panel using active matrix organic light-emitting elements formed on a film is suitable. .
[0013] In order to overlap the ends of the multiple display panels, in the above configuration, the first display panel of the third display panel The fifth region, the third region of the second display panel, and the first region of the first display panel are mutually a fourth portion overlapping the second portion and the third portion, the fourth portion being disposed between the second portion and the third portion; This is one of its characteristics.
[0014] When displaying one image by overlapping the edges of multiple display panels, the display may not be displayed properly if the image is displayed in full screen. If two or more display panels are combined and The discontinuity of the image at the seam of the display areas of the overlapping display panels is made noticeable to the user. In particular, when the display panel is a high-definition panel, e.g. 2K display panel with 1920 x 1080 pixels, 3840 x 2160 or 4096 x 2160 pixels for 4K display panels and 7680 x 4320 pixels for 8K display panels When combining several images, it is necessary to adjust the image so that the discontinuity is difficult for the user to recognize. Use artificial intelligence (AI) is preferred.
[0015] To address the issue of discontinuity of images at seams, a display panel according to one embodiment of the present invention is used. The display system, which has a display device combined with a It is preferable to provide a correction circuit having a function of correcting the artificial neural signal. Study of Artificial Neural Network (ANN) By learning the technique, the video signal is adjusted so that the discontinuity of the image is reduced, especially at the joints of the display area. A correction circuit capable of correcting the above-mentioned problem is constructed. By using the network to perform inference (cognition), the video signal is corrected and the discontinuity of the image is eliminated. This makes it possible to display a seamless image with no noticeable seams. This allows for improved quality of high-resolution images.
[0016] Artificial intelligence is a computer that mimics human intelligence. A neural network is a circuit that mimics a neural network composed of neurons and synapses, and is an artificial neural network. A neural network is a type of artificial intelligence. " refers specifically to artificial neural networks.
[0017] Use artificial intelligence to efficiently analyze and utilize behavior to determine future actions Repeated actions and information are stored as experience values that serve as a basis for recognizing patterns. From the large amount of data thus accumulated, general rules can be predicted.
[0018] For example, environmental data is used for data integration. Information from various sensors is collected from each area. By collecting and integrating data, more effective predictions can be made than with a single piece of data. For example, digital map data, data obtained from cameras, and location information obtained from radio There are reports etc.
[0019] By using a hierarchical ordered set, when a car driver parks in a parking lot, the data obtained from the camera By using the vehicle's driving data, map data, etc., the vehicle can effectively assist the driver in driving. When the driver switches to autonomous driving mode, the car uses artificial intelligence and data (back monitor) Parking facilities can use automated teller machines (such as parking cameras and lane tracking cameras) to stop vehicles in designated parking spaces.
[0020] In addition, large-area flexible display panels have a yield problem during the glass substrate peeling process. Therefore, it may be possible to reduce manufacturing costs by forming multiple panels of the same size. In other words, when the cost and yield of one high-resolution large-area panel are taken into consideration, The larger the area that is peeled off at one time, the greater the risk of defects. For example, In some cases, it may be cheaper to create a panel of four different sizes. Some factories that manufacture panels may produce displays that are the same size as displays that use a certain size display panel. When combining multiple display panels of different sizes, the same photomask as a display panel of a certain size may be used. Since the photomask can be manufactured using a photomask, the cost of manufacturing the photomask can be reduced.
[0021] In addition, multiple display panels with the same display area but different terminal positions can be combined. In the above configuration, the first display panel may have a first terminal portion on a short side thereof, and the second display panel may have a second terminal portion on a short side thereof. A first outer terminal having a second terminal portion on a long side of the display panel and connected to the first terminal portion. and a connection position of the second external terminal connected to the second terminal portion are different from each other. By changing the position of the terminals, the display panel can be arranged in a variety of ways. can be increased.
[0022] In recent years, there has been a trend to electronically convert side mirrors (also called door mirrors). In addition to the driver's seat, there are attempts to install cameras and sensors and display the captured images on a panel inside the car. It has also been said that side mirrors that protrude outside the vehicle will be eliminated in the future. Conventionally, side mirrors are adjusted to match the driver's line of sight. However, if the side mirrors are not installed and are electronic, it becomes difficult to adjust them. This is because the display panel that displays the image is often fixed, and the image There was a risk that visibility would be reduced, posing a safety issue.
[0023] Therefore, multiple display panels are stacked to form a single screen, and the driver can adjust the display panel as needed. By bending a part of the display panel, it is possible to make the display easier to see. It can be made easier to see. It can also change the design of the interior of the car. If the vehicle detects a vehicle approaching rapidly, the display panel will The system automatically bends a portion of the road surface and displays a video of the vehicle that requires attention to make the driver aware of it. By bending a part of the display panel, the distance from the driver is reduced. This makes it possible to display information in a way that is easy to see even for drivers with poor eyesight.
[0024] According to one aspect of the present invention, in the above-mentioned structure, the first display panel or the second display panel is One of its features is that it is flexible and has a position adjustment function that allows the end to be bent. The position adjustment function for bending the edge of the display panel is a part that changes the edge periphery to a protruding state on the back side of the display panel. In one embodiment of the present invention, a display panel is used. The present invention is not limited to the above, and may be applied to a display panel having an organic light-emitting element on a flexible film and a display panel having an organic light-emitting element on a flexible film. an optical film on the flexible film, and a display panel on the optical film and the flexible film. and a position adjustment jig for bending the end of the display panel. This is a display device in which both the optical film and the flexible film are bent by the structure. Since the film and flexible film are made of different materials, it is better not to fix them with adhesives, etc. This is because the position of the film edge that is being bent is shifted, allowing the entire display panel edge to be bent smoothly. The edge of the display panel is bent and an image equivalent to that of a side mirror is displayed in the bent area. This makes it possible to display information that is easy for the driver to see. For example, when the driver operates the turn signal, When the display is turned on, the position adjustment tool is driven in sync to bend the edge of the display panel to attract attention. It can also assist driving by displaying side mirror images in the bent area.
[0025] In addition, display devices that combine multiple display panels are used in large, medium and small vehicles (automobiles, etc.). In the cockpit area of various types of vehicles, including the driver's seat (including the steering wheel), It can also be applied to the driver's seat of aircraft, ships, and other vehicles. can be done.
[0026] Display devices that combine multiple display panels are not limited to the cockpit area around the driver's seat, but are also used in It can also be incorporated along surfaces, including curved surfaces, in the interior of a vehicle (including seats and ceiling).
[0027] In addition, the driver (pilot or crew member) can switch to the automatic driving mode. This technology can also be applied to autonomous vehicles that can drive autonomous vehicles.
[0028] In the case of self-driving vehicles, sensors will detect whether or not the steering wheel is touching the driver's hand and automatically switch the steering wheel. The switching will be done by the driver or through input operations. For safety reasons, it is preferable to provide a clear difference in the image display so that the driver can accurately understand the difference. For this reason, the display is made over a wide area, so that not only the driver but also everyone in the car can see in which direction they are looking. It is preferable that the display indicating the switch to autonomous driving is visible and understandable even when the vehicle is not in operation.
[0029] In addition, when switching from automated to manual driving, the driver must understand the settings for automated driving. The operation mode is switched by changing the display area. The more information you receive, the easier it is to receive it.
[0030] Also, the display in strong outdoor light during the day is very different from the display at night. The visibility of the display to the driver is also subject to change. Even if the environment outside the vehicle changes, multiple display panels can be displayed. By overlapping the displays, a single screen is formed, and the driver can easily bend parts of the display panel to make it easier to see. That is, a part of the display panel can be bent to make it easier to view.
[0031] Furthermore, one embodiment of the present invention is not limited to installation of a display device inside a vehicle. In some cases, the vehicle may be operated wirelessly from outside the vehicle by a person who is remotely controlling the vehicle. It is also possible to switch between autonomous driving and remote control. In that case, for example, A driver's seat is provided indoors, a display device according to one embodiment of the present invention is arranged around the driver's seat, and a remote control The system displays images captured by cameras installed in vehicles that can be used, and uses the images where necessary. The driver will remotely control the vehicle in certain situations, and the rest of the operation will be automatic. When displaying the scenery through the windshield, a high-definition display using organic EL elements is used. It is preferable that the display panel be a display panel that changes according to the driving speed, especially when driving at high speed. It is necessary to display the external environment and produce clear video that matches the speed. The response speed of is much faster than that of liquid crystal display elements, and it can provide accurate information to the driver. Display devices that combine multiple display panels can provide information in near real time. In order to use video data in a single system, it is necessary to compress the data and transmit it wirelessly. is doing. Effect of the Invention
[0032] It provides a wide display area for users such as drivers, and displays information on the wide display area. By utilizing the information provided, it is possible to ensure safe driving by drivers. [Brief description of the drawings]
[0033] [Figure 1] 1A and 1B are a top view and a cross-sectional view illustrating one embodiment of the present invention. [Diagram 2] 1A and 1B are diagrams illustrating examples of a display device according to one embodiment of the present invention that is mounted on a vehicle. [Diagram 3] FIG. 1 is a top view illustrating one embodiment of the present invention. [Figure 4] FIG. 1 is a top view illustrating one embodiment of the present invention. [Diagram 5] 1A to 1C are cross-sectional views illustrating an example of a method for manufacturing a display panel. [Figure 6] 1A to 1C are cross-sectional views illustrating an example of a method for manufacturing a display panel. [Figure 7] 1A and 1B are a top view and a cross-sectional view illustrating an example of a display panel. [Figure 8] FIG. 1 is a cross-sectional view showing an example of a display device. [Figure 9] FIG. 1 is a cross-sectional view showing an example of a display panel. [Figure 10] 1A to 1C illustrate a display panel and a display device according to a first embodiment. [Figure 11] FIG. 2 is a cross-sectional view illustrating the display device of the first embodiment. [Figure 12] FIG. [Figure 13]FIG. 2 is a perspective view of a position adjustment jig. [Figure 14] FIG. [Figure 15] FIG. 1 is a perspective view showing an example of a display device. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0034] Hereinafter, an embodiment of the present invention will be described in detail with reference to the drawings. The present invention is not limited to the following description, and those skilled in the art will recognize that the present invention may be modified in various ways in form and detail. The present invention is not limited to the description of the following embodiments. It is not something that can be done.
[0035] (Embodiment 1) In this embodiment, a configuration example and an application example of a display device according to one embodiment of the present invention will be described with reference to the drawings. This will be explained in light of the above.
[0036] [Configuration example 1] FIG. 1A is a schematic top view of a display panel 100 included in a display device according to one embodiment of the present invention. do.
[0037] The display panel 100 includes a display area 101 and a region adjacent to the display area 101 that transmits visible light. In FIG. 1A, the display panel 100 includes a display area 110, which is a type of external terminal. The flexible printed circuit (FPC) 112 is installed. Here is an example.
[0038] The display area 101 includes a plurality of pixels arranged in a matrix and is capable of displaying an image. It is possible. Each pixel is provided with one or more display elements. Representative display elements include Typically, a light-emitting element such as an organic EL element, or a liquid crystal element can be used.
[0039] In the region 110, for example, a pair of substrates constituting the display panel 100 and a pair of substrates A sealant for sealing the sandwiched display element may be provided. The material in the region 110 is transparent to visible light. Since the 0 does not have any wiring or elements other than the substrate and the encapsulant, it is transparent to visible light. This is an area where
[0040] Here, the width W of the region 110 shown in FIG. 1(A) is preferably 0.5 mm or more and 150 mm or less. The thickness is preferably 1 mm or more and 100 mm or less, and more preferably 2 mm or more and 50 mm or less. Since the region 110 functions as a sealing region, the larger the width W of the region 110, the Therefore, the distance between the edge of the display panel 100 and the display area 101 can be increased, and the It is possible to effectively prevent impurities such as water from penetrating into the display area 101. In particular, in this configuration example, the area 110 is provided adjacent to the display area 101. It is important to set the width W of the pixel to an appropriate value. For example, if the display element is an organic EL element, When using the EL element, the width W of the region 110 is set to 1 mm or more to effectively prevent deterioration of the EL element. In addition, in other areas other than the area 110, the display area 10 It is preferable to set the distance between the end of the display panel 100 and the end face of the display panel 100 to be within the above range. I wish.
[0041] In the region 120, for example, wiring electrically connected to pixels included in the display region 101 is provided. In addition to these wirings, a driving circuit (scanning line driving circuit) is also used to drive the pixels. In addition, the area 120 may be provided with an FPC 112 and Terminals for electrical connection (also called connection terminals), wiring for electrical connection with the terminals, and I This includes the area where the C chip, etc. are provided.
[0042] The display device 10 of one embodiment of the present invention includes a plurality of the above-described display panels 100. FIG. 1 is a schematic top view of a display device 10 having three display panels 100a, 100b, and 100c. The figure is shown.
[0043] In the following, the display panels, the components included in the display panels, and In order to distinguish between components related to each display panel, an alphabetical character is added after the reference numeral. In addition, unless otherwise specified, the bottom side (opposite side from the display surface side) The display panel or component placed in the upper part of the display panel is marked with "a", and the other components are placed in the upper part of the display panel or component. For one or more display panels and their components, the reference numerals are followed by an alphabet. In addition, unless otherwise specified, the display panel is equipped with multiple Even when describing a configuration that includes multiple display panels, the matters common to each display panel or component are described. In the following explanation, the alphabet will be omitted.
[0044] The display device 10 shown in FIG. 1B includes a display area 101a, a display area 101b, and a display area 101c, and a single optical film (typically a circularly polarizing It is also possible to attach the optical film separately, but in that case, If the optical film overlaps with the adjacent panels, a step will occur and the boundary will be noticeable. If they are attached separately, a maximum of three optical films will overlap. One optical film is used in common, and three display panels are partially overlapped on one optical film. This reduces the overlap of the panels and makes the surface appear flat, which is preferable. In this embodiment, the location where the three display panels overlap is portion 163.
[0045] The display panel 100b is disposed so that a part of it overlaps the upper side (display surface side) of the display panel 100a. Specifically, the display area 101a of the display panel 100a and the display area 101b of the display panel 100b are The visible light transmitting region 110b is disposed so as to overlap with the visible light transmitting region 110a.
[0046] In the portion 161, the region 110a of the display panel 100a provided at the bottom, which transmits visible light, and the display area 101b of the display panel 100b provided on the upper side are provided so as to overlap each other. In the portion 162, a display area 101c of the display panel 100c provided at the bottom and The region 110b of the display panel 100b that transmits visible light is overlapped with the region 110b of the display panel 100b that is provided above. It is provided.
[0047] In addition, the display panel 100c is partly overlapped on the lower side (rear side) of the display panel 100b. Specifically, the display area 101b of the display panel 100b and the display panel 10 The region 110c that transmits visible light of 0c overlaps with the display region 110b of the display panel 100b. The FPC of the display panel 101b and that of the display panel 100c are arranged so as to overlap each other.
[0048] Since the region 110b that transmits visible light is overlapped on the display region 101a, the display region 101 The entire display area 101a can be viewed from the display surface side. Since the areas 110a and 110b overlap each other, the entire display area 101c is visible from the display surface side. The display area 101a, the display area 101b, and the display area 10 The area where the seam of 1c is arranged so as not to be noticeable is regarded as one display area of the display device 10. As shown in FIG. 1B, one display area of the display device 10 is roughly T-shaped. The shape becomes.
[0049] FIG. 1B shows a case where the same display panel 100 is used for all three display panels. do.
[0050] FIG. 1C is a schematic diagram of the display device 10 taken along the dashed line AB shown in FIG. 1B. In FIG. 1C, for ease of understanding, the display area 1 is shown including the substrate film. The display areas are 01a, 101c, 110b, 120b, and 120c.
[0051] The display device 10 has an optical member 166 disposed on the outermost surface.
[0052] The optical member 166 is provided in contact with at least the display region 101b. In this example, the optical member 166 overlaps the entire surface of the display panel. The rod may be at least partially fixed with an adhesive or the like, or may not be fixed at all. For example, the optical member 166 and each display panel may be independently configured as the display device 10 or may be fixed to a housing of the electronic device.
[0053] The optical member 166 may be one or more of a polarizing member, a phase difference member, and an anti-reflection member. The outermost surface of the optical member 166 is not hard-coated. It may be possible.
[0054] Examples of the polarizing member include a polarizing plate, a polarizing film, and a polarizing membrane.
[0055] Examples of the phase difference member include a phase difference plate, a phase difference film, and a phase difference membrane.
[0056] Anti-reflection materials include anti-reflection films (AR (Anti-Reflection) films). Low-Reflection Film (LR (Low-Reflection) Film) Anti-glare film (AG film) Also, the following films are available: An anti-reflection plate or anti-reflection film having a similar function is also an example of the anti-reflection member.
[0057] In this embodiment, an example in which a circular polarizing plate is used as the optical member 166 will be described. The linear polarizing plate has, for example, a linear polarizing layer between a pair of substrates. The retardation plate may be a 1 / 4 λ plate or the like. The linear polarizer and the retardation plate are connected to each other. By using a circular polarizer, the surface and interior of the display panel are This can prevent a user of the display device from visually recognizing the overlapping portion due to reflection of light from the overlapping portion.
[0058] The portion 165 shown in FIG. 1B is a deformed portion. FIG. 1(D) is a schematic diagram of the display device 10 cut along the line 110.
[0059] The end of the display area 101b is pushed out by the position adjustment means 167, so that the display area 101b A part of the display panel is bent and deformed into a protruding part 165. The design of the display device 10 can also be varied.
[0060] When the position adjustment means 167 is moved, the optical member 166 and the display panel are fixed with an adhesive or the like. When the position adjustment means 167 is moved to bend the optical member 166, The display panel can be bent more smoothly if it is not glued. , motors, fixtures, hinges, etc.
[0061] (Embodiment 2) In this embodiment, the display device described in the above embodiment is disposed inside a vehicle. An example is shown below.
[0062] FIG. 2 shows an example of the display device 5002 being mounted on a vehicle with a right-hand drive, but the present invention is not limited thereto. In the case of a 100cc vehicle, the left and right positions are swapped.
[0063] In FIG. 2, a dashboard 5001 and a steering wheel 500 are arranged around the driver's seat and the passenger seat. 3, windshield 5004, etc.
[0064] The display device 5002 is disposed at a predetermined position on the dashboard 5001, specifically, around the driver. The T-shape is placed in front of the driver's seat inside the car. This is preferable because display areas can be provided in front of the passenger seat and between the passenger seat and the driver's seat. In FIG. 2, multiple display panels are assembled on the curved surface of the dashboard 5001. In the example shown, a single display device 5002 is provided by combining the two. The number of display devices is not limited to one, and multiple display devices may be provided at multiple locations. The display devices 5002 are attached to the connection parts of the steering wheel, the display parts of the instruments, the air outlet 5006, etc. The display area is not provided, and the display has a complex shape with multiple openings. Another advantage of using flexible display panels is that they can be made into roughly any shape.
[0065] In addition, a plurality of cameras 5005 for capturing images of the rear and side areas are provided outside the vehicle. In this example, the camera 5005 is installed instead of the side mirror. It is also possible to install both a camera to capture the situation above and a camera to capture the situation below.
[0066] Camera 5005 uses a CCD camera or CMOS camera in combination with an infrared camera. You can use infrared cameras. The higher the temperature of the subject, the higher the output level. It is possible to detect or extract living bodies such as humans and animals.
[0067] The image captured by the camera 5005 is displayed on the screen of the display device 5002 (display area 5002a, 002b, 5002c, 5002d, or any one or more of them) In addition, in the display device 5002, for example, the display area 5002a corresponds to one display panel. It is made up of four main display panels.
[0068] This display device 5002 is mainly used to assist driving of the vehicle. By capturing the situation in the direction of the vehicle from a wide horizontal angle and displaying the image, the system can detect the driver's blind spot. Being able to see the situation helps prevent accidents from occurring.
[0069] In addition, the display areas 5002a, 5002b, 5002c, and 5002d are adjacent display areas. In order to display images with inconspicuous seams between images, artificial intelligence (AI) is used to It is preferable to use a display system that includes a correction circuit capable of correcting the image signal. Specifically, the artificial neural network (ANN) is trained to detect the boundary between regions. A correction circuit capable of correcting a video signal so as to reduce discontinuity in the video Then, the learned artificial neural network is used to perform inference (cognition). By doing this, the video signal is corrected and the discontinuity of the image is compensated for. This makes it possible to display images with no noticeable seams, improving the quality of high-resolution images. Cut.
[0070] In addition, the display area 5002d of the display device 5002 is flexible. By using the position adjustment means to bend the left end portion 5002e, the angle is set to an easy-to-view position for the driver. The angle of the screen, which is part of the display area 5002d, can be changed. The display at the end of d is difficult to distinguish due to the distance from the driver and the viewing angle, but the display area 500 If the left end 5002e of 2d is bent to an angle that is easy for the driver to see, the side mirror will be This is useful because it can be provided at a position suitable for the display area where the image is displayed.
[0071] In addition, a distance image sensor is provided on the roof of the car, and the obtained image is displayed on a display device 5002. The range image sensor may be an image sensor or a LIDAR (Li Uses a wide display area. The device displays both the image obtained by the distance image sensor and the image obtained by the CCD camera. This makes it possible to provide the driver with a wealth of information and assist them in driving.
[0072] The display device 5002 can also display map information, traffic information, television images, DVD images, etc. If so, the number of display panels should be increased to create a larger display area. For example, it is preferable to display map information in the display areas 5002a, 5002b, 5002c, and 5002d. 002d can be displayed large as one display screen.
[0073] The display areas 5002a, 5002b, 5002c, and 5002d are fixed areas for displaying images. The TV is not set in a specific order, but can be freely changed according to the driver's preferences. Video and DVD video are displayed in the left display area 5002d, and map information is displayed in the center display area 5002b. The instrument display is in the right display area 5002c, and the audio display is in the display area near the gear shift. The area 5002a can be placed between the driver's seat and the passenger seat. For example, a multi-panel display can be used as a fail-safe design. Even if one of the display panels in the display area fails for some reason, the display area can be changed. By doing so, it is possible to display the image on a display panel arranged in another area.
[0074] In the case of flat display panels, installation locations are limited and there is dead space between the display panel and the curved surfaces inside the car. This results in a narrower interior space. If the display panel used in the 002d is a flexible display panel, it will be able to fit the curved surface of the interior of the car. This is desirable because it can be easily installed and does not reduce the space inside the vehicle. If the internal space can be made smaller, flat display panels and flexible display panels are For example, the display area 5002a may be a flat display panel. In addition, since the display area 5002a is within reach of the driver, a touch panel Alternatively, the input operation may be performed as follows.
[0075] In this embodiment, an example of application to a dashboard of a car is shown, but the present invention is not limited thereto. For example, an example of a motorcycle such as a scooter is shown in FIG.
[0076] A scooter 8600 shown in FIG. 15 includes a display device 8605, a power storage device 8602, a side mirror 8601, and a turn signal lamp 8603. A power storage device 860 stored in a trunk 8604. 2 can supply electricity to a display device 8605 and a turn signal light 8603.
[0077] The display device 8605 is disposed near the steering wheel in front of the driver, specifically, around the driver, The display device 8605 is configured by combining three display panels. The speedometer display, navigation display, rear monitor display, etc. can be switched appropriately. It is possible to switch between the two and display them.
[0078] The display device of this embodiment can also be used as a display device around the cockpit of an aircraft. The display device of the present embodiment can also be used in a very small mobility vehicle, which is a type of electric vehicle. It can also be provided in the
[0079] In addition, a flat surface for feet is provided between the two wheels, and the vehicle moves by shifting the rider's center of gravity. The display device of the present embodiment may be used in a ride-on type mobility support robot or the like.
[0080] In addition, digital signage (Digital Signage) attached to structures such as cylindrical pillars is also being used. The present embodiment can also be used as a display device for digital signage. The display device of the present invention can also be incorporated along the curved surface of an interior or exterior wall of a house or building. .
[0081] This embodiment mode can be freely combined with the first embodiment mode.
[0082] (Embodiment 3) In FIG. 1B shown in the first embodiment, the three display panels are all the same display panel 100. In this embodiment, an example in which a partially different display panel is used is shown in FIG. Note that there are only some differences, and the same reference numerals are used in FIG. 3 to describe the same parts as in FIG. 1. do.
[0083] FIG. 3A is a schematic top view of a display panel 100d included in a display device according to one embodiment of the present invention. be.
[0084] The display panel 100d has a display area 101d and a transparent layer adjacent to the display area 101d. In FIG. 3A, the region 120d has a The display panel 100d is provided with an FPC 112d, which is a type of external terminal. 101d has approximately the same area as the display area 101 of the display panel 100 shown in FIG. However, the location of area 120 is different, and the location where the FPC is attached is different.
[0085] The display device 11 according to one embodiment of the present invention includes two display panels 100 shown in FIG. In FIG. 3B, three display panels 100d shown in FIG. 1 shows a schematic top view of a display device 11 including display panels 100a, 100c, and 100d.
[0086] The display device 11 shown in FIG. 3B includes a display area 101a, a display area 101c, and a display area 101d are placed with almost no gap between them, forming a single sheet that overlaps all of these display areas. The display has an optical film (typically a circularly polarizing film). The area where the three panels overlap is section 163.
[0087] The display panel 100d is disposed so that a portion of it overlaps the lower side of the display panel 100a. Specifically, the display area 101a of the display panel 100a is disposed on the upper side, and the display panel 10 The area 120d of 0d and the FPC 112d are arranged so as to overlap with the area 110a. The display panel 100a has a region 110a that transmits visible light and the display panel 100b has a region 110c that transmits visible light. The portion where the display panel 100d overlaps with the display panel 100a is shown as a portion 168. A portion 168 of the rule 100d is displayed transparently through the area 110a.
[0088] Compared to the display area 101, the area 120 including the part connected to the FPC is not deformed. However, it may be difficult to repeatedly deform the surface. The portion 165 that becomes deformed by using the display panel 100d instead of the display panel 100b. By increasing the area of the portion 165, more image information can be obtained. The position can be easily seen by the driver, etc., especially in large vehicles such as trucks. In the 2010 model, the bonnet is also wide, making it possible to place the display panel far away from the driver. Therefore, it is useful to deform a part of a display panel in a distant place to make it easier to see.
[0089] FIG. 3C shows a modified example of FIG. 3B. In FIG. 3C, The display device 12 is shown in combination with the panel 100f. The display areas are display area 101a, display area 101d, display area 101c, and display area 10 This is the sum of 1f and 1f. In this specification, the shape of one such display area is also called a T-shape. In FIG. 3C, the display device 12 is provided with deformation portions 165 on both sides. It is possible.
[0090] FIG. 4 shows a modified example of FIG. 3(B). In FIG. 4, three display panels 100 The display device 13 shown in FIG. 1 has two display panels 100e and 100g arranged vertically and two display panels 100d arranged horizontally. In the display device 13, one display area is divided into three display areas 101d and 101e. The shape of such a single display area is also included in the present specification. In this case, it is called a T-shape. A T-shape is a shape that combines a vertical bar and a horizontal bar in the longitudinal direction. It is a shape that is composed of about 90 degrees to each other so that they intersect, and near the center of the horizontal bar The shape is not limited to a contact shape, i.e., a symmetrical shape.
[0091] In addition, in FIG. 4, the three display panels are arranged so as not to overlap each other, and the display device 13 The display panel 1 does not have a portion where three display panels overlap. The FPC of 00e is disposed in a position overlapping with the display panel 100d.
[0092] In addition, the three display panels 100d of the display device 13 are arranged in a row, with the left panel in FIG. 4 being the top panel. The right panel is the bottom panel, and the FPC of the center panel overlaps with the display area of the left display panel. are arranged so that
[0093] In FIG. 4, the display panel 100e has a curved shape, and the display panel 100g has a conventional A liquid crystal display device using a conventional glass substrate may be used. In this case, The display surface of the display panel 100d may be angled at an angle of 60° or more and 120° or less.
[0094] In this way, a display device having a wide display area can be provided by using various combinations. It can be assembled appropriately to fit the cockpit of an automobile, aircraft, ship, etc. that is equipped with a display device. It can be adjusted.
[0095] This embodiment mode can be freely combined with other embodiment modes.
[0096] (Embodiment 4) In this embodiment, a manufacturing method of the display panel shown in FIG. 5 will be used to explain.
[0097] First, as shown in FIG. 5A, a peeling layer 233 is formed on a formation substrate 231. Then, A plasma treatment is performed on the surface of the peeling layer 233 (see the dotted arrow in FIG. 5(A)). In this specification, a layer formed on a release layer may be referred to as a layer to be peeled off.
[0098] The substrate 231 to be prepared is a substrate having at least heat resistance capable of withstanding the processing temperature during the preparation process. The substrate 231 may be, for example, a glass substrate, a quartz substrate, a sapphire substrate, a semiconductor substrate, or the like. A solid substrate, a ceramic substrate, a metal substrate, a plastic substrate, etc. can be used.
[0099] In order to improve mass productivity, a large glass substrate may be used as the production substrate 231. For example, 3rd generation (550mm x 650mm) or higher and 10th generation (2950mm) A glass substrate of 3400 mm or less or a larger size may be used. preferable.
[0100] When a glass substrate is used as the preparation substrate 231, a lower layer is provided between the preparation substrate 231 and the peeling layer 233. Forming a base film is preferable because it can prevent contamination from the glass substrate. For example, a silicon oxide film, a silicon oxynitride film, a silicon nitride film, a silicon nitride oxide film, etc. Examples of the insulating film include the following.
[0101] The peeling layer 233 can be made of an inorganic material. Examples of the inorganic material include tungsten, Molybdenum, titanium, tantalum, niobium, nickel, cobalt, zirconium, zinc, An element selected from the group consisting of ruthenium, rhodium, palladium, osmium, iridium, and silicon. Examples of the silicon include metals containing the element, alloys containing the element, and compounds containing the element. The crystal structure of the layer containing the tantalum may be amorphous, microcrystalline, or polycrystalline. When high melting point metal materials such as tungsten, titanium, and molybdenum are used, the process of forming the peeled layer is This is preferable because it increases the degree of freedom.
[0102] When the peeling layer 233 has a single-layer structure, it is a tungsten layer, a molybdenum layer, or a tungsten and molybdenum layer. It is preferable to form a layer containing a mixture of tungsten and molybdenum. A mixture of tungsten and molybdenum corresponds, for example, to an alloy of tungsten and molybdenum.
[0103] The peeling layer 233 is formed by, for example, a sputtering method or a CVD (Chemical Vapor Deposition) method. deposition method (plasma CVD method, thermal CVD method, MOCVD (Metal O rganic CVD method), ALD (Atomic Layer Deposit ion method, coating method (including spin coating method, droplet ejection method, dispense method, etc.), It can be formed by a printing method, a vapor deposition method, or the like.
[0104] The thickness of the peeling layer 233 is 1 nm or more and 1000 nm or less, preferably 1 nm or more and 200 nm or less. More preferably, the thickness is set to 10 nm or more and 100 nm or less.
[0105] The peeling layer 233 may be a multilayer of a layer containing tungsten and a layer containing an oxide of tungsten. When forming a layer structure, a layer containing tungsten is formed, and an oxide insulating film is formed thereon. By this, a layer containing a tungsten oxide is formed at the interface between the tungsten layer and the insulating film. It may be useful to take advantage of this.
[0106] In addition, the surface of the layer containing tungsten is treated by thermal oxidation, oxygen plasma treatment, and nitrous oxide (N 2) Plasma treatment, treatment with highly oxidizing solutions such as ozone water, etc., are used to remove tungsten. A layer containing an oxide may be formed. The plasma treatment or heat treatment may be performed using oxygen, nitrogen, suboxide, or the like. The treatment can be carried out in an atmosphere of nitrogen alone or a mixture of nitrogen gas with other gases.
[0107] The surface state of the peeling layer 233 is changed by plasma treatment or heat treatment, so that the peeling layer 2 It is possible to control the adhesion between the insulating film 33 and the insulating film to be formed later. An example of a plasma treatment will be described below.
[0108] The plasma treatment is preferably carried out in an atmosphere containing nitrous oxide. It is more preferable to carry out the treatment under an atmosphere containing fluorine. It is possible to form an oxide layer of the material that constitutes layer 233. In particular, the silane-containing atmosphere If the oxide layer is very thin, it can be formed. In some cases, it is difficult to confirm this from cross-sectional observation images.
[0109] The oxide layer is a layer that contains an oxide of the material contained in the release layer. In this case, the oxide layer is a layer containing an oxide of a metal contained in the peeling layer 233. It is preferable that the oxide contains tungsten oxide, titanium oxide, or molybdenum oxide.
[0110] Next, as shown in FIG. 5B, a first insulating layer 205 is formed on the peeling layer 233. A second insulating layer 207 is formed on the insulating layer 205 .
[0111] In this embodiment mode, a stacked structure of a layer containing tungsten and a layer containing an oxide of tungsten is used. Although an example of using the peeling layer 233 has been shown, there is no particular limitation, and an organic resin such as polyimide may be used. Using this, an organic resin and a first insulating layer 205 are laminated on the fabrication substrate, and a part of the organic resin is laser-treated. The starting point of peeling is formed by locally heating the substrate with light or the like, and the first insulating layer is separated from the substrate. Peeling may occur at the interface 205 .
[0112] The first insulating layer 205 and the second insulating layer 207 are made of a silicon nitride film and a silicon oxynitride film, respectively. It is formed in a single layer or multiple layers using silicon film, silicon oxide film, silicon oxynitride film, etc. It can be achieved.
[0113] In this specification, "silicon oxynitride" refers to a material having a composition containing more oxygen than nitrogen. In this specification, the term "silicon oxynitride" refers to a material having a high content of The composition of the material contains more nitrogen than oxygen.
[0114] The first insulating layer 205 preferably contains oxygen and silicon. A single layer structure of a silicon oxide film or a silicon oxynitride film is preferable.
[0115] The first insulating layer 205 preferably further contains hydrogen. The function of the heat treatment is to release hydrogen from the first insulating layer 205. Hydrogen is released, and hydrogen is supplied to the oxide layer. In a subsequent heating step, the catalyst may have a function of releasing hydrogen and nitrogen. Nitrogen is released from the first insulating layer 205, and is supplied to the oxide layer.
[0116] The first insulating layer 205 is formed by secondary ion mass spectrometry (SIMS). The hydrogen concentration detected by mass spectrometry was 1.0×10 20 atoms / cm 3 Above 1.0×10 22 atoms / cm 3 Less than or equal to 5.0x 10 20 atoms / cm 3 Above 5.0×10 21 atoms / cm 3 The region where It is preferred that it includes
[0117] The first insulating layer 205 has a nitrogen concentration of 5.0×10 20 atom s / cm 3 Above 1.0×10 23 atoms / cm 3 Less than or equal to 1.0×10 21 atoms / cm 3 Above 5.0×10 22 atoms / cm3 Contains an area that is is preferred.
[0118] As the first insulating layer 205, a silicon oxide film or a silicon oxynitride film is formed by evaporating silane gas and By forming a film using the plasma CVD method with a film formation gas containing nitrous oxide gas, a large amount of This is preferable because it is possible to incorporate hydrogen and nitrogen into the film. The higher the ratio of hydrogen gas, the greater the amount of hydrogen released in the subsequent heating step, which is preferable. It is.
[0119] The second insulating layer 207 preferably contains nitrogen and silicon. A single layer structure of a silicon nitride film or a silicon oxynitride film, or a silicon nitride film or a nitride It is preferable that the second insulating layer 207 has a stacked structure including a silicon oxide film. In this case, the second insulating layer 207 is further made of at least a silicon oxide film and a silicon oxynitride film. It is preferable to have one as well.
[0120] The second insulating layer 207 is formed by absorbing hydrogen released from the first insulating layer 205 in a subsequent heating process. The second insulating layer 207 has a function of blocking hydrogen and nitrogen. The second insulating layer 207 may be a layer that can separate the element layer from the first insulating layer 205. It is possible to suppress the supply of hydrogen (and nitrogen) to the oxide layer, and to prevent hydrogen from being introduced into the oxide layer. (and nitrogen) can be efficiently supplied. There may be other layers between layers 207.
[0121] The silicon nitride film included in the second insulating layer 207 is etched by ionizing the silicon nitride film with silane gas, nitrogen gas, and ammonia gas. It is preferable to form the film by a plasma CVD method using a film forming gas containing the gas.
[0122] The first insulating layer 205 and the second insulating layer 207 are formed by a sputtering method and a plasma It can be formed by using a CVD method, a coating method, a printing method, etc. For example, plasma CVD By using the D method and setting the film formation temperature at 250℃ to 400℃, a dense and very The first insulating layer 205 and the second insulating layer 207 can be formed as a film having high moisture resistance. The thicknesses are 10 nm to 3000 nm, and 200 nm to 1500 nm, respectively. m or less is preferable.
[0123] Next, the peeling layer 233, the first insulating layer 205, and the second insulating layer 207 are heated. The heat treatment may be performed after forming at least a part of the element layer 209 described later. For example, after forming the transistor, heat treatment may be performed before forming the display element. When the manufacturing process of the child layer 209 includes a heating step, the heating step may also serve as the heat treatment. good.
[0124] By carrying out the heat treatment, hydrogen (and nitrogen) is released from the first insulating layer 205, and the first insulating layer 205 is oxidized. At this time, the second insulating layer 207 absorbs the released hydrogen (and nitrogen). This allows hydrogen (and nitrogen) to be efficiently supplied to the oxide layer.
[0125] The hydrogen supplied to the oxide layer reduces the oxides in the oxide layer, and oxygen is introduced into the oxide layer. For example, if the peeling layer contains tungsten, In the case of the plasma treatment, the WO3 formed by the plasma treatment is reduced, and the composition of oxygen is higher than that of WO3. Low-temperature tungsten oxide (WO)x (2 < x < 3) and WO2 are generated and a state in which they are mixed occurs. Since such a mixed metal oxide exhibits different crystal structures depending on the oxygen composition , the mechanical strength within the oxide layer is weakened. As a result, a state in which it is likely to collapse inside the oxide layer is realized, and the peelability in the subsequent peeling process can be improved.
[0126] Furthermore, due to the nitrogen supplied to the oxide layer, a compound containing the material included in the release layer and nitrogen is also generated. The presence of such a compound can further weaken the mechanical strength of the oxide layer and can enhance the peelability. When the release layer contains a metal, a compound containing the metal and nitrogen (metal nitride) is generated in the oxide layer. For example, when the release layer contains tungsten , tungsten nitride is generated in the oxide layer.
[0127] The more hydrogen supplied into the oxide layer, the easier it is for WO3 to be reduced, and it is likely to become a state in which a plurality of oxides with different oxygen compositions are mixed in the oxide layer. Therefore, the force required for peeling can be reduced . The more nitrogen supplied into the oxide layer, the more the mechanical strength of the oxide layer can be weakened , and the force required for peeling can be reduced. The thicker the first insulating layer 205 , the more hydrogen (and nitrogen) can be released, which is preferable. On the other hand, the thinner the first insulating layer 205, the higher the productivity, which is preferable.
[0128] The heat treatment may be performed at a temperature equal to or higher than the temperature at which hydrogen (and nitrogen) desorbs from the first insulating layer 205 and equal to or lower than the softening point of the production substrate 2 31. Also, it is preferable to perform heating at a temperature equal to or higher than the temperature at which the reduction reaction of the metal oxide in the oxide layer by hydrogen occurs. The higher the temperature of the heat treatment, the more the first insulating layer The amount of hydrogen (and nitrogen) desorbed from 205 is increased, improving the subsequent stripping properties. Depending on the heating time and temperature, peelability may become too high, resulting in unintended peeling. Therefore, the use of tungsten for the peeling layer 233 may cause peeling. In this case, the temperature is 300° C. or higher and lower than 700° C., preferably 400° C. or higher and lower than 650° C., and more preferably Alternatively, the material is heated at a temperature of 400°C or higher and 500°C or lower.
[0129] The atmosphere in which the heat treatment is performed is not particularly limited. The heat treatment may be performed in an air atmosphere, but it is also possible to use nitrogen or a rare gas. It is preferable to carry out the reaction under an inert gas atmosphere such as ethyl acetate or the like.
[0130] Next, as shown in FIG. 5C, the second insulating layer 20 in the region 110 that transmits visible light is The second insulating layer 207 can be removed by dry etching, wet etching, or the like. In addition, a method such as a bonding method can be used for the subsequent manufacturing process of the element layer 209. Any of the etching steps may also serve as a step of removing the second insulating layer 207.
[0131] In one embodiment of the present invention, the second insulating layer 2 is formed on the entire surface of the release layer 233 until the heat treatment is performed. After the heat treatment, the second 110 in the region that transmits visible light is The insulating layer 207 is removed. This allows the peelability of the visible light transmitting region 110 to be improved. Therefore, the peelability of the entire display panel can be made uniform. The structure of the region 110 that transmits visible light can improve the yield of the manufacturing process of the display panel. The impact on the
[0132] Next, as shown in FIG. 5D, an element layer 209 and a connection terminal The element layer 209 includes a display element. It is preferable that the insulating layer is not included in the region 110 that transmits visible light.
[0133] Next, a substrate 235 to be bonded to the fabrication substrate 231 in a later step is prepared. A release layer 237 is formed. Then, a plasma treatment is performed on the surface of the release layer 237 (FIG. 5(E) ) (see dotted arrow).
[0134] Next, as shown in FIG. 5(F), a third insulating layer 215 is formed on the peeling layer 237. A fourth insulating layer 217 is formed on the insulating layer 215, and a functional layer 219 is formed on the fourth insulating layer 217. Form.
[0135] The heat treatment is performed after the fourth insulating layer 217 is formed and after a part of the fourth insulating layer 217 is removed. Before forming the functional layer 219, the release layer 237 and the third insulating layer 215 are removed. The heat treatment may be performed to heat at least part of the functional layer 219. In the case where the manufacturing process of the functional layer 219 includes a heating step, the heating step may be performed after at least a part of the functional layer 219 is formed. The heating step may also serve as the heat treatment.
[0136] By carrying out the heat treatment, the peelability in the subsequent peeling step can be improved.
[0137] Next, as shown in FIG. 5(G), the fourth insulating layer 21 in the region 110 that transmits visible light is The fourth insulating layer 217 can be removed by dry etching or wet etching. In addition, the etching process included in the manufacturing process of the functional layer 219 may be performed by using a method such as etching. Any one of the above steps may also serve as a step for removing the fourth insulating layer 217.
[0138] In one embodiment of the present invention, the fourth insulating layer 2 is formed on the entire surface of the release layer 237 until the heat treatment is performed. After the heat treatment, the fourth region 110 that transmits visible light is provided. The insulating layer 217 is removed. This allows the peeling property of the entire display panel to be uniform. The structure of the region 110 that transmits visible light affects the yield of the manufacturing process of the display panel. This can suppress the noise.
[0139] Next, the preparation substrate 231 and the substrate 235 are bonded together with an adhesive layer 221. (FIG. 6(A) ))
[0140] The adhesive layer 221 may be a photo-curable adhesive such as an ultraviolet-curable adhesive, a reaction-curable adhesive, or a heat-curable adhesive. Various curing adhesives such as adhesives, anaerobic adhesives, etc. can be used. 1. Water-soluble resin, organic solvent-soluble resin, plasticized by exposure to ultraviolet light, etc. The substrate 235 and the first insulating layer 205 can be separated from each other when necessary, for example, from a resin that can be easily removed. A suitable adhesive may be used.
[0141] Then, the release layer 233 and the first insulating layer 205 are separated.
[0142] As a method of peeling, for example, the preparation substrate 231 or the substrate 235 is fixed to an adsorption stage, A peeling starting point is formed between the peeling layer 233 and the first insulating layer 205. For example, The starting point for peeling may be formed by inserting a sharp tool such as a blade. Alternatively, the peeling layer 233 may be irradiated with X-rays to dissolve a part of the peeling layer 233, thereby forming a peeling starting point. A liquid (e.g., alcohol, water, water containing carbon dioxide, etc.) is applied to the release layer 233 or the first The liquid is dropped onto the end of the insulating layer 205, and the liquid is transferred to the peeling layer 233 and the first insulating layer 205 by utilizing the capillary phenomenon. The initiation of delamination may be achieved by penetrating the edge layer 205 boundary.
[0143] Next, in the portion where the peeling starting point was formed, the adhesive layer was gently pulled in a direction approximately perpendicular to the adhesive surface. Applying physical force to the film (pulling it off with a human hand or a tool, or rolling it with a roller) By using a process that separates the layer from the substrate, the layer to be peeled off can be peeled off without damaging it. For example, a tape or the like is attached to the preparation substrate 231 or the substrate 235, and the tape is pulled in the above direction. Alternatively, a hook-shaped member may be attached to the edge of the preparation substrate 231 or substrate 235. It is also possible to peel off the adhesive by hooking it onto the surface of the adhesive. The peeling may be performed by adsorbing the substrate to the back surface of the substrate 231 or 235 and pulling the substrate. stomach.
[0144] Here, during peeling, a liquid containing water, such as water or an aqueous solution, is added to the peeling interface, and the liquid By performing peeling so that the adhesive penetrates the surface, peelability can be improved. The static electricity generated in the peeled layer adversely affects the functional elements contained in the peeled layer (semiconductor elements are It can suppress damage caused by electricity.
[0145] By the above method, the layer to be peeled off can be peeled off from the formation substrate 231 with a high yield.
[0146] Thereafter, the substrate 201 is attached to the first insulating layer 205 via the adhesive layer 203 (FIG. 6(B) The adhesive layer 203 may be made of a material that can be used for the adhesive layer 221. For 01, a material that can be used for the substrate 211 described later can be used.
[0147] The release layer 237 and the substrate 235 are then separated.
[0148] Thereafter, the substrate 211 is attached to the first insulating layer 215 via the adhesive layer 213 (FIG. 6(C) ))
[0149] As the substrate 211, various substrates that can be used for the fabrication substrate 231 can be used. Alternatively, a flexible substrate may be used as the substrate 211. Conductive elements, light-emitting elements such as organic EL elements, liquid crystal elements, detector elements, and other functional elements and color filters A substrate on which a filter or the like is formed in advance may be used. Materials that can be used for the above can be applied.
[0150] By using flexible substrates for the substrate 201 and the substrate 211, In addition, when the substrate 211 functions as a temporary support substrate, In this case, the substrate 211 and the layer to be peeled are separated, and the layer to be peeled is placed on another substrate (for example, a substrate having flexibility). ) may be pasted together.
[0151] As described above, in the method for manufacturing a display panel according to one embodiment of the present invention, the first insulating layer 205 and The second insulating layer 207 is formed on the entire surface of the peeling layer 233, and then a heat treatment is performed to form the surface. The peelability of the entire display panel can be improved uniformly. By removing the second insulating layer 207 in the region 110 that transmits visible light, The reflectance of 110 can be reduced.
[0152] In addition, in a method for manufacturing a display panel according to one embodiment of the present invention, after forming a functional element over a formation substrate, The functional element is then peeled off from the substrate and transferred to another substrate. There are almost no restrictions on the heat that can be applied to the device. Functional elements can be fabricated with good yield on flexible substrates with poor heat resistance. This makes it possible to realize a highly reliable and flexible display panel.
[0153] In this embodiment, a display panel in which EL elements are used as display elements will be described as an example.
[0154] The display panel is structured so that one color is expressed by three sub-pixels of R (red), G (green), and B (blue). A configuration in which four sub-pixels of R, G, B, and W (white) are used to express one color, or a configuration in which R, G, and B A configuration in which one color is expressed by four sub-pixels of Y (yellow), Y (yellow), etc. can be applied. Colors other than RGBWY (for example, cyan or magenta) may be used. 7(A) and (B) show top views of the display panel 370. FIG.
[0155] The display panels 370 shown in FIGS. 7A and 7B each have a region 110 that transmits visible light. 7A, the display portion 381 and the driver circuit portion 382 are arranged in a region that transmits visible light. 1 shows an example in which the area 110 is adjacent to the display unit 381 and arranged along two sides of the display unit 381. In FIG. 7B, the region 110 that transmits visible light is adjacent to the display portion 381. An example is shown here, arranged along three sides of 81.
[0156] FIG. 7C shows a top-emission display panel 3 using a color filter method. 7(A) and (B) is a cross-sectional view of the dashed line A1-A2 in FIG. and corresponds to the cross-sectional view between A3 and A4.
[0157] The display panel 370 includes a substrate 201, an adhesive layer 203, a first insulating layer 205, a second insulating layer 206, and a 07, a plurality of transistors, a capacitor element 305, a conductive layer 307, an insulating layer 312, and an insulating layer 31 3, insulating layer 314, insulating layer 315, light emitting element 304, conductive layer 355, spacer 316, The adhesive layer 317, the colored layer 325, the light-shielding layer 326, the substrate 211, the adhesive layer 213, the third insulating layer 2 15, and a fourth insulating layer 217. The layers included in the region 110 that transmits visible light are , and transmits visible light.
[0158] The driver circuit portion 382 includes a transistor 301. The display portion 381 includes a transistor 302. and a transistor 303.
[0159] Each transistor has a gate, a gate insulating layer 311, a semiconductor layer, a source, and a drain. The gate and the semiconductor layer overlap with a gate insulating layer 311. A part of the transistor 302 functions as a dielectric of the capacitor 305. The conductive layer functioning as a drain or a gate also serves as one electrode of the capacitor 305 .
[0160] In FIG. 7C, a transistor having a bottom gate structure is shown. The transistor structure may be different between the driving circuit section 382 and the display section 38. 1 may each have multiple types of transistors.
[0161] The capacitor 305 has a pair of electrodes and a dielectric between them. The conductive layer is made of the same material and formed in the same process as the gate of the transistor. The source and drain have a conductive layer formed of the same material and in the same process.
[0162] The insulating layer 312, the insulating layer 313, and the insulating layer 314 each cover the transistors and the like. The number of insulating layers covering the transistors and the like is not particularly limited. The insulating layer 314 is a flat Among the insulating layers 312, 313, and 314, At least one layer is preferably made of a material that is difficult for impurities such as water or hydrogen to diffuse into. It is possible to effectively suppress the diffusion of impurities from the outside into the transistor. This makes it possible to improve the reliability of the display panel.
[0163] The display panel 370 has a structure in which reflection of light in the region 110 that transmits visible light is suppressed. The visible light transmitting region 110 is made up of the substrate 201, the adhesive layer 203, the first insulating layer 205, and the like. Then, the adhesive layer 317, the third insulating layer 215, the adhesive layer 213, and the substrate 211 are laminated in this order. It has.
[0164] The second insulating layer 207, the fourth insulating layer 217, the gate insulating layer 311, the insulating layer 312, the insulating layer The insulating layer 313, the insulating layer 314, and the insulating layer 315 are provided in the display unit 381 and transmit visible light. The insulating layers are not provided in the transparent region 110. It is preferable that the insulating layer 110 is located near the boundary between the insulating layer 110 and the region 110 that transmits visible light. The edge of the edge layer preferably overlaps with the light-shielding layer 326. This reduces the area that transmits visible light. This can reduce variations in reflectance and transmittance within the surface of the region 110.
[0165] The first insulating layer 205 and the substrate 201 are bonded together by an adhesive layer 203. The insulating layer 215 and the substrate 211 are bonded together by an adhesive layer 213. In the method for manufacturing the display panel of the embodiment, the first insulating layer 205 and the third insulating layer 215 are Each of these layers is located at the peeling interface with the production substrate, and covers the entire surface of the display panel 370. Therefore, the display panel 370 can be manufactured with a high yield.
[0166] In the display section 381, a light emitting element 304 is disposed between the second insulating layer 207 and the fourth insulating layer 217. Impurities may enter the light emitting element 304 from the thickness direction of the display panel 370. Similarly, in the display unit 381, a plurality of insulating layers are provided to cover the transistors. This prevents impurities from entering the transistor.
[0167] By disposing the light emitting element 304 and the transistor between a pair of highly moisture-proof insulating films, This makes it possible to prevent impurities such as water from entering these elements, thereby increasing the reliability of the display panel. Therefore, it is preferable.
[0168] Highly moisture-proof insulating films include those containing nitrogen and silicon, such as silicon nitride film and silicon oxide nitride film. and films containing nitrogen and aluminum, such as an aluminum nitride film. A silicon oxide film, a silicon oxynitride film, an aluminum oxide film, or the like may be used.
[0169] For example, the water vapor permeability of a highly moisture-resistant insulating film is 1×10 -5 [g / (m 2 ·day)] Less than or equal to 1×10 -6 [g / (m 2 ·day)] or less, preferably 1×10 -7 [g / (m 2 ·day)] or less, and more preferably 1×10 -8 [g / (m 2 ·da y)] or less.
[0170] When an organic material is used for the insulating layer 314, the insulating layer 314 exposed at the edge of the display panel is There is a risk that impurities such as moisture may enter the light emitting elements 304 and the like from the outside of the display panel through the insulating film. If the light emitting element 304 is deteriorated due to the intrusion of impurities, it will lead to deterioration of the display panel. Therefore, as shown in the vicinity of the connection portion 306 in FIG. 7(C), an inorganic film (insulating film in this case) is formed on the insulating layer 314. An opening is provided that reaches the edge layer 313, so that even if impurities such as moisture enter the display panel from the outside, It is preferable to have a structure that makes it difficult for the light to reach the light emitting element 304 .
[0171] The light-emitting element 304 includes an electrode 321, an EL layer 322, and an electrode 323. The light emitting element 304 may have an optical adjustment layer 324. The light emitting element 304 emits light toward the colored layer 325. Inject.
[0172] The transistor, the capacitor, the wiring, etc. are arranged so as to overlap with the light emitting region of the light emitting element 304. As a result, the aperture ratio of the display portion 381 can be increased.
[0173] One of the electrodes 321 and 323 functions as an anode, and the other functions as a cathode. A voltage higher than the threshold voltage of the light emitting element 304 is applied between the electrodes 321 and 323. Then, holes are injected into the EL layer 322 from the anode side, and electrons are injected from the cathode side. The electrons and holes are recombined in the EL layer 322, and the light-emitting material contained in the EL layer 322 It glows.
[0174] The electrode 321 is electrically connected to the source or drain of the transistor 303. The electrodes 321 are connected directly or through other conductive layers. The electrodes 321 function as a light-emitting element and are provided for each light-emitting element 304. It is electrically insulated by 315.
[0175] The EL layer 322 is a layer containing a light-emitting material. An organic EL element using the compound can be suitably used.
[0176] The EL layer 322 has at least one light-emitting layer.
[0177] Quantum dots can also be used as light-emitting materials. Quantum dots are semiconductors with a size of a few nm. The nanocrystals are 1×10 3 1×10 6 It is composed of about atoms. Since the dots have a size-dependent energy shift, quantum dots made of the same material Even if the quantum dot is a single crystal, the emission wavelength varies depending on the size, so it is necessary to change the size of the quantum dot used. This makes it possible to easily adjust the emission wavelength.
[0178] Quantum dots have a narrow emission spectrum peak width, making it possible to obtain emission with good color purity. Furthermore, the theoretical internal quantum efficiency of quantum dots is said to be nearly 100%. By using quantum dots as a light-emitting material, it is possible to obtain a light-emitting device with high light-emitting efficiency. Moreover, quantum dots, which are inorganic compounds, are inherently stable. In this way, a light-emitting element that is also favorable in terms of life can be obtained.
[0179] The materials that make up quantum dots are elements in Group 14 of the periodic table, elements in Group 15 of the periodic table, Group 16 elements, compounds consisting of multiple Group 14 elements, Groups 4 to 1 Compounds of Group 4 elements and Group 16 elements of the periodic table, Compounds of Group 2 elements and Group 16 elements of the periodic table Compounds with elements, compounds with elements in group 13 and group 15, compounds with elements in group 13 Compounds of elements and elements of group 17 of the periodic table, compounds of elements of group 14 of the periodic table and elements of group 15 of the periodic table compounds of elements in Group 11 and Group 17 of the periodic table; iron oxides; titanium oxides; Examples include chalcogenide spinels and various semiconductor clusters.
[0180] Examples of materials that make up quantum dots include cadmium selenide, cadmium sulfide, and tetrahydrofuran. Cadmium sulphide, zinc sulphide, indium phosphide, lead selenide, lead sulphide, selenium and zinc Cadmium compounds, cadmium, selenium and sulfur compounds, etc. In addition, so-called alloy type quantum dots, in which the ratios of cadmium and cadmium are arbitrary, may be used. The alloy quantum dots of selenium, selenium and sulfur can change the emission wavelength by changing the content ratio of the elements. Since the emission can be changed, this is an effective means for obtaining blue light emission.
[0181] Quantum dot structures include core type, core-shell type, and core-multishell type. Since the quantum efficiency of light emission is greatly improved, the core-shell type or It is preferable to use a core-multishell type quantum dot. Examples of the shell material are Examples include zinc sulfide and zinc oxide.
[0182] Quantum dots have a high proportion of surface atoms, making them highly reactive and prone to aggregation. Therefore, a protective agent or a protective group is attached to the surface of the quantum dot. This is preferable because it is possible to prevent the quantum dots from agglomerating and increase their solubility in a solvent. It can also reduce reactivity and improve electrical stability.
[0183] The size (diameter) of the quantum dots is 0.5 nm or more and 20 nm or less, preferably 1 nm or more and 10 nm or less. Quantum dots in the sub-nm range are usually used. The size distribution of quantum dots is narrow. The narrower the emission spectrum, the more excellent the color purity of the light emitted. The shape of the quantum dots is not particularly limited, and may be spherical, rod-like, disk-like, or other shapes. .
[0184] Quantum dots maintain their luminous efficiency even when the light-emitting layer is composed of only quantum dots without using a host material. Therefore, in this respect, a light emitting element that is preferable in terms of life can be obtained. When the light-emitting layer is formed only from quantum dots, the quantum dots have a core-shell structure (core- It is preferable that the structure is a multi-shell structure.
[0185] The electrode 323 functions as a common electrode and is provided across the multiple light emitting elements 304. The electrode 323 is supplied with a constant potential.
[0186] The light emitting element 304 overlaps the colored layer 325 via the adhesive layer 317. 7C, the light emitting element 304 and the light shielding layer 326 are overlapped with each other through the adhesive layer 317. 7(C) shows a case where there is a gap between the 26 and the 27, but they may be in contact with each other. 2 shows a configuration in which the spacer 316 is provided on the substrate 201 side, Alternatively, the insulating layer 325 may be provided on the substrate 201 side of the layer 326 .
[0187] A combination of a color filter (colored layer 325) and a microcavity structure (optical adjustment layer 324) By combining these two, light with high color purity can be extracted from the display panel. The thickness of layer 324 varies depending on the color of each pixel.
[0188] The colored layer is a colored layer that transmits light of a specific wavelength band. For example, red, green, blue, or A color filter that transmits light in the yellow wavelength range can be used for the colored layer. Materials that can be used include metal materials, resin materials, or pigments or dyes. Examples of such materials include resin materials.
[0189] Note that one embodiment of the present invention is not limited to the color filter type, but may be a color-coded type, a color conversion type, Alternatively, a quantum dot method or the like may be applied.
[0190] The light-shielding layer is provided between adjacent colored layers. The light-shielding layer blocks light from the adjacent light-emitting element. The colored layer is formed on the edge of the light-shielding layer to prevent color mixing between adjacent light-emitting elements. By providing the layers so as to overlap, it is possible to suppress light leakage. A material that blocks light from the element can be used, for example a metallic material or a pigment or dye. The black matrix can be formed by using a resin material containing the above. If the driver circuit is provided in an area other than the pixel area, unintended light leakage due to guided light can be suppressed. This is preferable because it can be controlled.
[0191] The connection portion 306 includes a conductive layer 307 and a conductive layer 355. The conductive layer 307 is the same as the source and drain of the transistor. The conductive layer 355 can be formed of the same material and in the same process. The external input terminal is electrically connected to the external input terminal, which transmits signals and potentials from the outside. In this example, an FPC 373 is provided as an input terminal. and the conductive layer 355 are electrically connected.
[0192] The connector 319 may be made of various anisotropic conductive films (ACFs). Conductive Film and Anisotropic Conductive Paste (ACP) pic Conductive Paste) can be used.
[0193] The transistors 301, 302, and 303 shown in FIG. 9A each have two gates, a gate insulating layer, and a 311, a semiconductor layer, a source, and a drain. This figure shows an example in which a semiconductor layer is sandwiched between two gates. Compared to other transistors, the field-effect mobility of the transistor can be increased, and the on-current can be increased. As a result, a circuit capable of high speed operation can be fabricated. By applying a transistor with a large on-current, the circuit area can be reduced. By doing so, even if the display panel becomes larger or more precise and the number of wirings increases, the signal quality of each wiring can be maintained. This can reduce the signal delay and reduce the variation in the brightness of the display. ) shows an example in which one gate is formed between the insulating layer 313 and the insulating layer 314.
[0194] As shown in FIG. 9(A), the display panel preferably has an overcoat 329. The overcoat 329 prevents impurities contained in the colored layer 325 from diffusing into the light emitting element 304. The overcoat 329 is a material that transmits the light of the light emitting element 304. For example, the insulating film may be an inorganic insulating film such as a silicon nitride film or a silicon oxide film, or Organic insulating films such as acrylic films and polyimide films can be used. In FIG. 9A, an overcoat 329 is provided on one surface of the display panel. The overcoat 329 is provided in the region 110 that transmits visible light. It does not have to be done.
[0195] In addition, when the material of the adhesive layer 317 is applied onto the colored layer 325 and the light-shielding layer 326, The material of the coat 329 may be a material having high wettability with respect to the material of the adhesive layer 317. For example, the overcoat 329 is preferably made of indium tin oxide (ITO). A conductive oxide film such as a tin oxide (TiO2) film or a thin film having a light transmitting property It is preferable to use a metal film such as an Ag film.
[0196] By using a material having high wettability with respect to the material of the adhesive layer 317 for the overcoat 329, This allows the material of the adhesive layer 317 to be applied uniformly. This can prevent air bubbles from being mixed in when the liquid crystal display is joined, thereby preventing display defects.
[0197] It is preferable to use a flexible substrate as the substrate 201 and the substrate 211. For example, materials such as glass, quartz, resin, metal, alloy, and semiconductors that are thick enough to be flexible are used. The substrate on the side from which light is extracted from the light-emitting element is made of a material that transmits the light. For example, the thickness of the substrate is preferably 1 μm or more and 200 μm or less, and more preferably 1 μm or more and 100 μm or less. More preferably, the thickness is 10 μm or less and 50 μm or less, and even more preferably, the thickness is 10 μm or more and 20 μm or less. The thickness and hardness of the flexible substrate are determined based on the mechanical strength and the flexibility. The substrate with flexibility can be either a single-layer structure or a multi-layer structure. This is also fine.
[0198] Since resin has a smaller specific gravity than glass, using resin as a flexible substrate This is preferable because it allows the display panel to be made lighter than when glass is used.
[0199] It is preferable to use a highly tough material for the substrate. This makes it possible to improve impact resistance and prevent breakage. For example, a display panel that is less susceptible to cracks can be realized using a resin substrate or a thin metal substrate. By using an alloy substrate, it is lighter and less susceptible to breakage than when using a glass substrate. It is possible to realize a simple display panel.
[0200] Metal and alloy materials have high thermal conductivity and can easily conduct heat across the entire substrate, making it possible to It is preferable to use a metal material or an alloy material because it can suppress a local temperature rise of the panel. The thickness of the substrate is preferably 10 μm or more and 200 μm or less, and more preferably 20 μm or more and 50 μm or less. It is more preferable that:
[0201] The material constituting the metal substrate or alloy substrate is not particularly limited. For example, aluminum Aluminum, copper, nickel, or alloys of metals such as aluminum alloys or stainless steel Examples of materials that can be used for the semiconductor substrate include silicon. can be.
[0202] In addition, if a material with high thermal emissivity is used for the substrate, the surface temperature of the display panel can be prevented from becoming too high. Therefore, damage to the display panel and deterioration of its reliability can be suppressed. A layer with high thermal emissivity (for example, a metal oxide or ceramic material can be used) A laminated structure may also be used.
[0203] Examples of materials having flexibility and light transmission include polyester resins such as PET and PEN. , polyacrylonitrile resin, acrylic resin, polyimide resin, polymethyl methacrylate Resin, PC resin, PES resin, polyamide resin (nylon, aramid, etc.), polysiloxane San resin, cycloolefin resin, polystyrene resin, polyamide-imide resin, polyurethane Tan resin, polyvinyl chloride resin, polyvinylidene chloride resin, polypropylene resin, PTF E resin, ABS resin, etc. In particular, it is preferable to use a material with a low linear expansion coefficient. For example, polyamide-imide resin, polyimide resin, polyamide resin, PET, etc. are preferable. In addition, a substrate in which a fiber body is impregnated with a resin and a substrate in which an inorganic filler is impregnated with a resin can be used. It is also possible to use a substrate having a lower linear expansion coefficient by mixing with a material such as a polyimide.
[0204] As for the flexible substrate, the layer using the above-mentioned material protects the surface of the device from scratches, etc. A hard coat layer (e.g., a silicon nitride layer), a layer of a material capable of dispersing pressure (e.g., The protective layer may be laminated with at least one of the protective layers. Any substrate that can be used as the substrate 132 may be used.
[0205] When the flexible substrate has a glass layer, the substrate has a barrier property against water and oxygen. This improves the display quality and makes it possible to provide a highly reliable display panel.
[0206] The adhesive layer may be a photo-curable adhesive such as an ultraviolet curable adhesive, a reactive curable adhesive, a heat curable adhesive, or an antibacterial adhesive. Various curing adhesives such as vapor-curing adhesives can be used. Also, adhesive sheets, etc. can be used. Good too.
[0207] The adhesive layer may also contain a desiccant. For example, an oxide of an alkaline earth metal (oxide Use substances that adsorb moisture by chemical adsorption, such as calcium oxide and barium oxide. Or, it can be used to absorb moisture by physical adsorption, such as with zeolites or silica gels. If a desiccant is included, impurities such as moisture may be absorbed into the functional element. This is preferable because it can suppress the intrusion of the ultraviolet ray into the display panel and improve the reliability of the display panel.
[0208] In addition, by including a filler having a high refractive index or a light scattering material in the adhesive layer, the light emitted from the light emitting element can be For example, titanium oxide, barium oxide, zeolite, etc. can improve the light extraction efficiency. Light, zirconium, etc. can be used.
[0209] The light-emitting element may be a self-emitting element that is illuminated by a current or a voltage. The category includes devices whose light intensity can be controlled. For example, light-emitting diodes (LEDs), organic An EL element, an inorganic EL element, or the like can be used. Various display elements can be used. For example, liquid crystal elements, electrophoretic elements, MEMS A display element using the above may be applied.
[0210] The light-emitting elements are top emission type, bottom emission type, and dual emission type. For the electrode from which light is extracted, a conductive film that transmits visible light is used. In addition, it is preferable to use a conductive film that reflects visible light for the electrode on the side from which light is not extracted. .
[0211] The conductive film that transmits visible light is, for example, indium oxide, ITO, indium zinc oxide, It can be formed using zinc oxide (ZnO), ZnO doped with gallium, etc. Gold, silver, platinum, magnesium, nickel, tungsten, chromium, molybdenum, iron, Metallic materials such as cobalt, copper, palladium, or titanium, and alloys containing these metallic materials; Alternatively, nitrides of these metal materials (for example, titanium nitride) may be thin enough to have light transmission properties. In addition, a laminated film of the above materials can be used as a conductive film. For example, by using a laminated film of an alloy of silver and magnesium and ITO, it is possible to obtain a conductive film. In addition, graphene or the like may be used.
[0212] The conductive film that reflects visible light is made of, for example, aluminum, gold, platinum, silver, nickel, tungsten, etc. Metallic materials such as zinc, chromium, molybdenum, iron, cobalt, copper, or palladium, In addition, the above-mentioned metal material or alloy may include Lanthanum, neodymium, germanium, or the like may be added. Aluminum and titanium alloys, aluminum and nickel alloys, aluminum and neodymium alloys, Aluminum-containing alloys such as aluminum, nickel, and lanthanum alloys (Al-Ni-La) Silver-palladium-copper alloys (Ag-Pd- Cu, APC), and alloys containing silver, such as alloys of silver and magnesium, may also be used. The alloy containing copper and aluminum is preferable because of its high heat resistance. By laminating a metal film or a metal oxide film, the oxidation of the aluminum alloy film can be suppressed. Examples of materials for the metal film and metal oxide film include titanium and titanium oxide. In addition, the conductive film that transmits visible light and a film made of a metal material may be laminated. For example, A laminated film of silver and ITO, a laminated film of an alloy of silver and magnesium and ITO, etc. can be used. Cut.
[0213] The electrodes can be formed by vapor deposition or sputtering. Other methods include ejection methods such as the inkjet method, printing methods such as screen printing, and plating methods. The electrode can be formed using:
[0214] The EL layer 322 has at least a light-emitting layer. The EL layer 322 has a plurality of light-emitting layers. The EL layer 322 may be formed of a material having a high hole injection property, a material having a high hole transport property, or a layer other than the light emitting layer. high electron transporting material, high electron injecting material, or The semiconductor device further includes a layer containing a bipolar substance (a substance having high electron transport and hole transport properties). This is also fine.
[0215] The EL layer 322 may be made of either a low molecular weight compound or a high molecular weight compound. The layers constituting the EL layer 322 may each be formed by deposition (vacuum deposition). The method may include a transfer method, a printing method, an ink-jet method, a coating method, etc. do.
[0216] The light emitting element 304 may contain two or more types of luminescent materials. For example, it is possible to realize a light-emitting element that emits light of two or more different types of luminescent materials. White light emission can be obtained by selecting luminescent materials that have complementary colors. For example, R (red), G (green), B (blue), Y (yellow), or O (orange) light emission. A substance or a luminescent substance that emits light containing two or more of the R, G, and B spectral components. It can be used.
[0217] The light-emitting element 304 may be a single element having one EL layer, or a charge generating It may also be a tandem element having a plurality of EL layers stacked with an intervening layer.
[0218] <Example of light-emitting panel configuration> Figures 9(A) and 9(B) show the top emission structure with the color-coded method applied. 9A and 9B show cross-sectional views of panels 370A and 370B, respectively. If not necessary, a configuration without color filters may be used as shown in FIG. In this case, it is preferable that the light-emitting layers of the light-emitting elements of the respective colors are separate from each other. Since such a display device is formed using multiple display panels, the size of one display panel is Therefore, it is possible to improve the alignment accuracy of the metal mask. This makes it possible to improve the yield of the different color coating. This is advantageous in terms of adopting a child.
[0219] The structure of the transistor in the display panel is not particularly limited. For example, The transistor may be a staggered type transistor, or an inverse staggered type transistor. The transistor may be either a top gate type or a bottom gate type. Alternatively, gate electrodes may be provided above and below the channel.
[0220] The crystallinity of the semiconductor material used in the transistor is not particularly limited. A semiconductor having crystallinity (microcrystalline semiconductor, polycrystalline semiconductor, single crystal semiconductor, or semiconductor with partially crystalline regions) If a semiconductor having crystallinity is used, the This is preferable because it is possible to suppress deterioration of the resistor characteristics.
[0221] The semiconductor material used for the transistor is not particularly limited, and may be, for example, a Group 14 element, a compound semiconductor, or the like. A conductor or an oxide semiconductor can be used for the semiconductor layer. Typically, a semiconductor containing silicon Semiconductors, semiconductors containing gallium arsenide, or oxide semiconductors containing indium can be used. Cut.
[0222] In particular, it is preferable to use an oxide semiconductor as a semiconductor in which a channel of a transistor is formed. In particular, it is preferable to use an oxide semiconductor having a larger band gap than silicon. It is desirable to use a semiconductor material with a wider band gap and lower carrier density than silicon. This is preferable because it can reduce the current in the off state of the transistor.
[0223] For example, the oxide semiconductor may contain at least indium (In) or zinc (Zn). More preferably, the oxide contains In-M-Zn (wherein M is Al, Ti, Ga , Ge, Y, Zr, Sn, La, Ce, Hf or Nd (metals such as include.
[0224] As a semiconductor material for transistors, CAAC-OS (C Axis Aligne d. Using Crystalline Oxide Semiconductor CAAC-OS is preferable because it has fewer defect levels and is more reliable in transistors than amorphous materials. In addition, CAAC-OS has the advantage that no grain boundaries are visible. Since it has a high molecular weight, it is possible to form a stable and uniform film over a large area, and it is also possible to form a flexible surface. The CAAC-OS film is less likely to crack due to stress caused when the display panel is curved.
[0225] CAAC-OS is a crystalline oxide semiconductor whose c-axis is aligned approximately perpendicular to the film surface. Another crystal structure of oxide semiconductors is nanoscale microcrystal aggregates called nano-structures. There are various structures that are different from single crystals, such as nanocrystals (nc). It has been confirmed that CAAC-OS has lower crystallinity than single crystals and has a higher crystallinity than nc. High crystallinity.
[0226] In addition, the CAAC-OS has a c-axis orientation and multiple pellets are arranged in the ab-plane direction. The CAAC-OS is a distorted crystal structure. , CAA crystal(c-axis-aligned ab-plane-an The oxide semiconductor may also be referred to as an oxide semiconductor having a chord crystal.
[0227] The insulating layer of the display panel can be made of an organic insulating material or an inorganic insulating material. Examples of the resin include acrylic resin, epoxy resin, polyimide resin, and polyamide resin. Resin, polyimide amide resin, siloxane resin, benzocyclobutene resin, phenol resin Examples of the inorganic insulating film include a silicon oxide film, a silicon oxynitride film, and a silicon nitride film. silicon oxide film, silicon nitride film, aluminum oxide film, hafnium oxide film, yttrium oxide film tantalum oxide film, zirconium oxide film, gallium oxide film, tantalum oxide film, magnesium oxide film, Examples of the film include a lanthanum oxide film, a cerium oxide film, and a neodymium oxide film.
[0228] The conductive layers of the display panel are made of aluminum, titanium, chromium, nickel, Copper, yttrium, zirconium, molybdenum, silver, tantalum, or tungsten Any metal or alloy containing this metal as the main component can be used as a single layer or laminate structure. Alternatively, indium oxide, ITO, indium oxide with tungsten, tungsten Indium zinc oxide containing titanium, Indium oxide containing titanium TO, indium zinc oxide, ZnO, gallium doped ZnO, or silicon-containing A light-transmitting conductive material such as indium tin oxide containing impurity elements may be used. A semiconductor such as polycrystalline silicon or an oxide semiconductor that has been made low-resistance by, for example, containing Alternatively, a silicide such as nickel silicide may be used. The graphene-containing film can be prepared by, for example, reducing a film containing graphene oxide. In addition, a semiconductor such as an oxide semiconductor containing an impurity element can be used. Alternatively, a conductive paste such as silver, carbon, or copper, or a polythiophene Alternatively, the conductive layer may be formed using a conductive polymer such as polyvinyl chloride. The conductive paste is inexpensive and is therefore preferred. Conductive polymers are preferred because they are easy to apply.
[0229] FIG. 8 is a cross-sectional view of a display device having two display panels 370 shown in FIG. 7(C) stacked on top of each other. As shown in.
[0230] In FIG. 8, a display area 101a of the lower display panel (corresponding to the display unit 381 shown in FIG. 7(C)) is ) and a region 120a that blocks visible light (corresponding to the driving circuit section 382 shown in FIG. 7C), and 7C) of the display area 101b of the upper display panel; and Region 110b that transmits visible light (corresponding to region 110 that transmits visible light shown in FIG. 7(C)) Shows.
[0231] In the display device shown in FIG. 8, the display panel located on the display surface side (upper side) transmits visible light. The display area 110b of the lower display panel is adjacent to the display area 101b. The region 01a overlaps with the region 110b of the upper display panel that transmits visible light. This allows the non-display area between the display areas of two overlapping display panels to be reduced, or even eliminated. This allows for a large display where the seams of the display panel are less noticeable to the user. A display device can be realized.
[0232] In addition, the display device shown in FIG. 8 has a transparent region 110b between the display region 101a and the region 110b that transmits visible light. The display has a transparent layer 103 that has a higher refractive index than air and transmits visible light. It is possible to prevent air from entering between the region 101a and the region 110b that transmits visible light, and the refractive index This can reduce reflections at the interface due to the difference in the thickness of the substrate. Furthermore, it is possible to suppress uneven brightness.
[0233] The light-transmitting layer 103 is formed on the substrate 211 of the lower display panel or the substrate 201 of the upper display panel. The display area 101a and the visible light transmitting area 110b may overlap the entire surface. The transparent layer 103 may overlap only the region 120a that blocks visible light. It may be possible.
[0234] For example, the light-transmitting layer 103 may be an adhesive film having an adhesive layer on both sides of the substrate. This can be done.
[0235] The region 110b that transmits visible light is configured to suppress reflection of light. The overlapping portion between the two display panels is difficult for a user of the device to see. In addition, the display in the display area 101a is visually recognized through the area 110b that transmits visible light. This can reduce the difference in luminance between the portion that is seen through the region and the portion that is not seen through the region.
[0236] This embodiment mode can be freely combined with other embodiment modes. EXAMPLES
[0237] In this example, the results of manufacturing a display device according to one embodiment of the present invention will be described. The display device we fabricated is a kawara-type multidisplay.
[0238] <Display panel> First, the details of the display panel used in the display device of this embodiment will be shown.
[0239] FIG. 10A shows a schematic diagram of a display panel of this embodiment. The display panel shown in FIG. The size of the light-emitting part 250 is 13.5 inches diagonally, the number of effective pixels is 1280 x 720, and the resolution is It is an active matrix organic EL display with a resolution of 108ppi and an aperture ratio of 41.3%. The display panel has a built-in DeMUX 253. The display panel also includes a scan driver 255. Two sides of the light-emitting portion 250 are in contact with the area 251 that transmits visible light. Around the two sides, wiring 257 is provided.
[0240] The transistor is a channel-etched type transistor using CAAC-OS. For the oxide semiconductor, an In-Ga-Zn oxide was used.
[0241] The light-emitting elements are made of three types of organic EL elements, RGB. The light-emitting element is a top-emission structure. It is made of.
[0242] FIG. 10(B) shows a schematic diagram of a display device in which three display panels are stacked in a T-shape. FIG. 10C is a schematic diagram of a dashed-dotted line XY cross section of the display device shown in FIG. 10B.
[0243] The display device of this embodiment has a plurality of display panels, and the non-display areas between the display areas are small. Specifically, the visible light in the upper display panel is A light-transmitting layer 10 is provided between the light-transmitting region 251 and the light-emitting portion 250 of the lower display panel. 3 is provided.
[0244] On two sides of the display panel, wiring is provided from the end of the light-emitting unit 250 to the end of the display panel. However, there are no structures that block visible light, such as wiring or drivers, and the visible light transmitting area 25 The width of the region 251 of the display panel through which visible light passes is set to about 5 mm. The thickness T of the light transmitting region 251 (which can also be said to be the thickness of one display panel) is approximately 110 μm. Therefore, in the display device of this embodiment, the maximum number of overlapping display panels is three. However, the difference in height on the display surface is very small, making the seams less noticeable. do.
[0245] The three display panels are flexible. For example, as shown in FIG. 10(C), the lower display panel The vicinity of FPC373a of the panel is curved, and the upper display panel adjacent to FPC373a is A part of the lower display panel and a part of the FPC 373a are disposed below the light emitting unit 250. As a result, the FPC373a does not physically interfere with the rear surface of the upper display panel. This allows other display panels to be placed on all four sides of the display panel. This makes it easier to increase the area.
[0246] In this embodiment, an adhesive film having an adhesive layer on both sides of a substrate was used as the light-transmitting layer 103 . By using this adhesive film, the two display panels that make up the display device can be attached and detached freely. The adsorption layer on one side of the light-transmitting layer 103 is adsorbed to the substrate 211a. The adsorption layer on the other surface of the light-transmitting layer 103 is adsorbed to the substrate 201b.
[0247] In FIG. 10B, the light transmitting layer 103 is formed only in a portion overlapping with the region 251 that transmits visible light. 10C, the light-transmitting layer 103 is not limited to the substrate 101, but has a portion overlapping with the light-emitting portion 250. The end of 201b overlaps the entire region 251 that transmits visible light, and further includes a display element. It also overlaps a part of the region 155b. The light-transmitting layer 103 is not provided in the curved portion of the display panel near the curved portion. However, depending on the thickness of the light-transmitting layer 103 and the thickness of the flexible substrate, That's fine.
[0248] Each display panel was fabricated by bonding a substrate and an element layer with an adhesive layer. For example, Figure 10 As shown in (C), the substrate 201a and the element layer 153a, the substrate 211a and the element layer 153a, The substrate 201b and the element layer 153b, and the substrate 211b and the element layer 153b are bonded to each other. The element layer 153a is bonded to the display element region 155a via a bonding layer 157. The element layer 153 also includes a region 156a including wirings electrically connected to the display element. b is a region 155b including a display element and a region 155b including wiring electrically connected to the display element. 6b.
[0249] FIG. 11 shows a cross-sectional view of a display device including an overlapping portion of two display panels.
[0250] 11, the light-emitting portion 250 and the visible light transmitting area of the display panel used in this embodiment are shown. The configuration of the light-emitting unit 250a and the light-emitting unit 250b is similar to each other. The light emitting section 250 and the region 251 that transmits visible light are described below. The first insulating layer 205, the second insulating layer 207, the gate insulating layer 311, the insulating layer 312, the third The insulating layer 215 and the fourth insulating layer 217 are formed on the insulating layer 313, the insulating layer 314 and the insulating layer 315. The edge layer 315 is provided on the light-emitting portion 250 and is not provided on the region 251 that transmits visible light. The display panel of this embodiment is not implemented except for the configuration of the region 251 that transmits visible light. This has the same configuration as the display panel 370A shown in FIG. 9(A) described in the fourth embodiment.
[0251] A photograph of the panel that was actually produced is shown in Figure 12(A). The edge of the panel is pushed from the back of the display panel by the position adjustment function and bent, and the circular area is The image shown in Fig. 12(A) is a side-mirror image. The image shown is a conceptual image. When actually installing the camera in a car, the camera will be fitted to a circular area. The image captured by the camera (side mirror image) will be displayed. Of course, the position adjustment function is also available. It is also possible to return the bent parts to their original state. A photo of the returned panel is shown in Figure 12 ( The image displayed on the display device in FIG. 12(B) is a car navigation system. The video is displayed.
[0252] FIG. 13 shows an example of a position adjustment jig 21 for pushing out a part of the right display panel. 1, the display panel 100 is pushed out so that its periphery is positioned as shown by the dotted line. The motor 22 rotates the rotary shaft 23 shown by the chain line, and the position adjustment jig 21 moves. One edge of the display panel moves. The area with a radius of about 14.5 cm is centered on one edge of the display panel. The area is pushed up, and the edge of the pushed-up display panel is approximately 5 cm above the plane of the display panel. cm lifted.
[0253] Figure 14(A) shows a side view of the display panel with part of it pressed. A side view of the jig 21 in its original state is shown in FIG. 14(B). The side mirror image is displayed in a circular area as shown in the figure. It is data. [Explanation of symbols]
[0254] 10 Display device 11 Display device 12 Display device 13 Display device 21 Position adjustment jig 22 Motor 23 Rotation axis 100 Display Panel 101 Display area 103 Translucent layer 110 areas 112 FPC 120 areas 132 Protection Board 153a Element layer 153b Element layer 155a area 155b area 156a area 156b area 157 Adhesive layer 161 parts 162 parts 163 parts 165 parts 166 Optical Components 167 Position adjustment means 168 parts 201 Substrate 201a Substrate 201b Substrate 203 Adhesive layer 205 Insulating layer 207 Insulating Layer 209 Element Layer 211 Substrate 211a Substrate 211b board 213 Adhesive layer 215 Insulating Layer 217 Insulating Layer 221 Adhesive layer 223 Connection terminal 231 Preparation Substrate 233 Peeling layer 250 Light emitting part 250a Light emitting part 250b Light emitting part 251 areas 255 scan driver 257 Wiring 301 Transistor 302 Transistor 303 Transistor 304 Light emitting element 305 Capacitive element 306 Connection 307 Conductive Layer 311 Gate insulating layer 312 Insulating layer 313 Insulating Layer 314 Insulating layer 315 Insulating Layer 316 Spacer 317 Adhesive layer 319 Connectors 321 Electrode 322 EL layer 323 Electrode 324 Optical adjustment layer 325 Colored layer 326 Light blocking layer 329 Overcoat 355 Conductive Layer 370 Display Panel 370A Display Panel 370B Display Panel 373 FPC 373a FPC 381 Display section 382 Drive circuit section 5001 Dashboard 5002 Display device 5002a Display area 5002b Display area 5002c display area 5002d Display area 5002e Left end 5003 Handle 5004 Windshield 5005 Camera 5006 Ventilator
Claims
[Claim 1] A first display panel, a second display panel, and a third display panel, the first display panel has a first region and a second region; the second display panel has a third region and a fourth region; the third display panel has a fifth region and a sixth region; the first region, the third region, and the fifth region have a function of transmitting visible light; the second area, the fourth area, and the sixth area have a display function; the first region of the first display panel and the fourth region of the second display panel have a first portion that overlaps with each other; the fifth region of the third display panel and the second region of the first display panel have a second portion that overlaps with each other; the fifth region of the third display panel and the fourth region of the second display panel have a third portion that overlaps with each other, A display device in which one display area formed by the second area, the fourth area, and the sixth area has a substantially T-shape.
Citation Information
Patent Citations
Display panel, electronic instrument and wearable type electronic instrument
JP2002014366A
Combined display device
JP2004251981A
Display device, and driving method of display device
JP2010107551A
Organic electroluminescent panel, organic electroluminescent device, and method of manufacturing organic electroluminescent panel
JP2012028638A
Tile-type display using overlapping flexible substrates
JP2013504092A