Display device

The display device addresses threshold voltage variations in transistors by using a dual-gate configuration with capacitors and oxide semiconductors, achieving higher definition and improved aperture ratios through stabilized brightness and increased current flow.

JP2024138319AActive Publication Date: 2024-10-08SEMICON ENERGY LAB CO LTD
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
JP2024105174
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2015-05-05
Filing Date
2024-06-28
Publication Date
2024-10-08
Estimated Expiration
2036-05-03

AI Technical Summary

Technical Problem

Active matrix display devices using light emitting elements face challenges in achieving high definition due to variations in threshold voltage of driving transistors, leading to brightness inconsistencies between pixels and reduced aperture ratios, especially in bottom emission structures.

Method used

The display device incorporates a transistor with a first and second gate, connected through capacitors to stabilize the threshold voltage, utilizing an oxide semiconductor for reduced variations and enabling dual-gate drive to enhance current flow and reduce pixel brightness variations.

Benefits of technology

This configuration reduces brightness variations between pixels, allows for higher definition displays with increased aperture ratios, and improves overall display quality by stabilizing threshold voltages and enhancing current flow.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024138319000001_ABST
    Figure 2024138319000001_ABST
Patent Text Reader

Abstract

To provide a display device with reduced variations in luminance among pixels.SOLUTION: The display device includes a transistor, first to fourth switches, first and second capacitors, a light-emitting element, and first to fifth wirings. The transistor comprises a first gate and a second gate. A first terminal of the transistor is connected to the third wiring. The first switch controls a conduction state between the first wiring and the first gate, the second switch controls a conduction state between the second wiring and the second gate, the third switch controls a conduction state between the first gate and a second terminal of the transistor, and the fourth switch controls a conduction state between the fifth wiring and the second terminal of the transistor. The first capacitor retains a potential difference between the first gate and the second terminal of the transistor, and the second capacitor retains a potential difference between the first gate and the second gate. The first terminal of the light-emitting element is connected to the second terminal of the transistor, and the second terminal of the light-emitting element is connected to the fourth wiring.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] One embodiment of the present invention relates to a display device.

[0002] The present invention relates to an article, a method, or a manufacturing method. The present invention also relates to a composition of matter. One embodiment is a semiconductor device, a light-emitting device, a power storage device, a memory device, a driving method thereof, or a method for driving the same. In particular, one embodiment of the present invention relates to a semiconductor device including an oxide semiconductor, a display device including an oxide semiconductor, and a manufacturing method thereof. or a light emitting device.

[0003] In this specification and the like, a semiconductor device is a device that can function by utilizing semiconductor characteristics. The display device, the electro-optical device, the semiconductor circuit, and the electronic device all have a semiconductor device. There are cases. [Background technology]

[0004] The specific configuration of an active matrix display device using a light emitting element is as follows: Although it varies by manufacturer, it usually consists of at least a light-emitting element and a video signal input to the pixel. The transistor to be controlled (switching transistor) and the current value to be supplied to the light emitting element A transistor (drive transistor) for controlling the above is provided in each pixel.

[0005] By making all the transistors in the pixel have the same polarity, In the manufacturing process, a process such as adding an impurity element that gives one conductivity to the semiconductor film is performed. In the following Patent Document 1, a pixel is formed by only n-channel transistors. A constructed light emitting device display is described.

[0006] In an active matrix display device using light emitting elements, light is supplied to the light emitting elements according to an image signal. Variation in the threshold voltage of the transistor (drive transistor) that controls the current supplied However, the above-mentioned variation in threshold voltage is easily reflected in the luminance of the light-emitting element. A circuit configuration for preventing this effect is described in Patent Document 2 listed below. [Prior art documents] [Patent documents]

[0007] [Patent Document 1] JP 2003-195810 A [Patent Document 2] JP 2013-137498 A Summary of the Invention [Problem to be solved by the invention]

[0008] A pixel capable of correcting the threshold voltage of a driving transistor is Therefore, it is difficult to achieve high resolution, and the bottom emission structure (transistor In the case of a structure in which light is extracted through a substrate on which a transistor is provided, the light from the light-emitting element is This causes the aperture ratio to become smaller.

[0009] In light of the above technical background, one aspect of the present invention is to provide a method for improving a threshold voltage of a driving transistor. One of the objectives is to provide a display device that can suppress the luminance variation between pixels caused by the temperature fluctuation. Another object of one embodiment of the present invention is to provide a high-definition display device. An object of one embodiment is to provide a display device with a high aperture ratio.

[0010] Another embodiment of the present invention is to provide a novel display device or a novel semiconductor device. One of our goals is to provide

[0011] In addition, the description of a plurality of problems does not preclude the existence of each problem. The embodiments do not necessarily solve all of these problems. Problems other than those listed may be solved by the present specification. These problems will become apparent from the description of the present invention, drawings, claims, etc. This could be a form of challenge for the Ming. [Means for solving the problem]

[0012] One embodiment of the present invention is a display device having a transistor, first and second capacitors, and a light-emitting element. The transistor has a first gate and a second gate. The term "transistor" refers to a region that overlaps with another transistor, with the channel formation region of the transistor in between. Preferably, the first terminal of the transistor is applied with a first potential. The second terminal of the first capacitance element is electrically connected to the first gate of the transistor. The first terminal of the second capacitance element is electrically connected to the first gate. The second terminal of the second capacitance element is electrically connected to the second gate. The second terminal of the light-emitting element is electrically connected to the second terminal of the transistor. can be obtained.

[0013] In the above embodiment, the transistor is preferably an n-channel type.

[0014] In the above embodiment, the first potential is preferably higher than the second potential.

[0015] In the above embodiment, the channel formation region preferably contains an oxide semiconductor.

[0016] One embodiment of the present invention is a semiconductor device including a transistor, first to fourth switches, and first and second capacitors. The display device has a first gate electrode, a second gate electrode, a light emitting element, and first to fifth wirings. and a second gate. The first gate and the second gate are disposed in a channel forming region of the transistor. The first terminal of the transistor is preferably a first terminal having a first region therebetween. , and the third wiring. The first switch is in a conductive state between the first wiring and the first gate. The second switch has a function of controlling the conduction state between the second wiring and the second gate. The third switch controls the conduction state between the first gate and the second terminal of the transistor. The fourth switch has a function of controlling the conduction state between the fifth wiring and the second terminal of the transistor. The first terminal of the first capacitance element is electrically connected to the first gate. The second terminal of the first capacitance element is electrically connected to the second terminal of the transistor. A first terminal of the capacitive element is electrically connected to the first gate. A second terminal of the second capacitive element is electrically connected to the first gate. The first terminal of the light emitting element is electrically connected to the second terminal of the transistor. The second terminal of the light emitting element is electrically connected to the fourth wire.

[0017] In the above embodiment, the transistor is preferably an n-channel type.

[0018] In the above embodiment, the channel formation region preferably contains an oxide semiconductor.

[0019] In the above embodiment, the first to fourth switches each have an oxide semiconductor layer in a channel forming region. It is preferable that the transistor has a conductor.

[0020] One embodiment of the present invention is a semiconductor device including a transistor, first to third switches, and first and second capacitors. The display device has a light emitting element and first to fifth wirings. The first gate and the second gate form a channel of the transistor. The first terminal of the transistor is preferably a first terminal of the first semiconductor layer. The first switch is electrically connected to the third wiring. The second switch has a function of controlling the conduction state between the second wiring and the second gate. The third switch controls the electrical continuity between the fifth wiring and the second terminal of the transistor. The first terminal of the first capacitance element is electrically connected to the first gate. The second terminal of the first capacitance element is electrically connected to the second terminal of the transistor. A first terminal of the second capacitance element is electrically connected to the first gate. A second terminal of the second capacitance element is electrically connected to the second gate. The first terminal of the light emitting element is electrically connected to the second terminal of the transistor. The second terminal of the light emitting element is electrically connected to the fourth wiring.

[0021] In the above embodiment, the transistor is preferably an n-channel type.

[0022] In the above embodiment, the channel formation region preferably contains an oxide semiconductor.

[0023] In the above embodiment, the first to third switches each have an oxide semiconductor layer in a channel forming region. It is preferable that the transistor has a conductor.

[0024] One embodiment of the present invention is a semiconductor device including a transistor, first to third switches, and first and second capacitors. The display device has a light emitting element and first to fourth wirings. The first gate and the second gate form a channel of the transistor. The first terminal of the transistor is preferably a first terminal of the first semiconductor layer. The first switch is electrically connected to the third wiring. The second switch has a function of controlling the conduction state between the second wiring and the second gate. The third switch has a function of switching the conduction state between the first gate and the second terminal of the transistor. The first terminal of the first capacitance element is electrically connected to the first gate. The second terminal of the first capacitance element is electrically connected to the second terminal of the transistor. A first terminal of the element is electrically connected to the first gate. A second terminal of the second capacitive element is electrically connected to the second gate. The first terminal of the light-emitting element is electrically connected to the second terminal of the transistor. The second terminal of the light emitting element is electrically connected to the fourth wire.

[0025] In the above embodiment, the transistor is preferably an n-channel type.

[0026] In the above embodiment, the channel formation region preferably contains an oxide semiconductor.

[0027] In the above embodiment, the first to third switches each have an oxide semiconductor layer in a channel forming region. It is preferable that the transistor has a conductor.

[0028] One aspect of the present invention is a semiconductor device including a transistor, first and second switches, and first and second capacitance elements. The display device has a light emitting element and first to fourth wirings. The first gate and the second gate form a channel of the transistor. The first terminal of the transistor is preferably a first terminal of the first semiconductor layer. The first switch is electrically connected to the third wiring. The second switch has a function of controlling the conduction state between the second wiring and the second gate. The first terminal of the first capacitance element is electrically connected to the first gate. The second terminal of the capacitive element is electrically connected to the second terminal of the transistor. The first terminal is electrically connected to the first gate. The second terminal of the second capacitance element is electrically connected to the second gate. The first terminal of the light-emitting element is electrically connected to the second terminal of the transistor. The second terminal of the light emitting element is electrically connected to the fourth wire.

[0029] In the above embodiment, the transistor is preferably an n-channel type.

[0030] In the above embodiment, the channel formation region preferably contains an oxide semiconductor.

[0031] In the above embodiment, the first and second switches each have an oxide semiconductor in a channel forming region. It is preferable that the transistor has a conductor.

[0032] One aspect of the present invention is a display device according to the above aspect, a microphone, a speaker, and an operation and at least one of the keys. Effect of the Invention

[0033] According to one embodiment of the present invention, the brightness between pixels caused by the variation in the threshold voltage of the driving transistor is It is possible to provide a display device in which the variation in the degree of reflection can be suppressed. According to one embodiment of the present invention, a display device with high aperture ratio can be provided. It will be possible to provide.

[0034] According to one embodiment of the present invention, a novel display device or a novel semiconductor device is provided. It will be possible to provide

[0035] The description of these effects does not preclude the existence of other effects. An embodiment does not necessarily have all of these effects. Effects other than these may be included in the description, This is self-evident from the description in the drawings, claims, etc. It is possible to extract other effects from any of the descriptions. [Brief description of the drawings]

[0036] [Figure 1] FIG. 2 is a circuit diagram showing an example of the configuration of a pixel. [Diagram 2] FIG. 2 is a circuit diagram showing an example of the configuration of a pixel. [Diagram 3] 4 is a timing chart showing an example of the operation of a pixel. [Figure 4] FIG. 4 is a circuit diagram showing an example of the operation of a pixel. [Diagram 5] FIG. 1 is a diagram showing the relationship between VBGS and Vth. [Figure 6] FIG. 2 is a circuit diagram showing an example of the configuration of a pixel. [Figure 7] 4 is a timing chart showing an example of the operation of a pixel. [Figure 8] FIG. 4 is a circuit diagram showing an example of the operation of a pixel. [Figure 9] FIG. 2 is a circuit diagram showing an example of the configuration of a pixel. [Figure 10] 4 is a timing chart showing an example of the operation of a pixel. [Figure 11] FIG. 4 is a circuit diagram showing an example of the operation of a pixel. [Figure 12] FIG. 2 is a circuit diagram showing an example of the configuration of a pixel. [Figure 13] 4 is a timing chart showing an example of the operation of a pixel. [Figure 14] FIG. 4 is a circuit diagram showing an example of the operation of a pixel. [Figure 15] FIG. 2 is a circuit diagram showing an example of the configuration of a pixel. [Figure 16] FIG. 2 is a circuit diagram showing an example of the configuration of a pixel. [Figure 17] FIG. 2 is a circuit diagram showing an example of the configuration of a pixel. [Figure 18] FIG. 2 is a circuit diagram showing an example of the configuration of a pixel. [Figure 19] FIG. 2 is a circuit diagram showing an example of the configuration of a pixel. [Figure 20] FIG. 2 is a circuit diagram showing an example of the configuration of a pixel. [Figure 21] FIG. 2 is a circuit diagram showing an example of the configuration of a pixel. [Figure 22] FIG. 2 is a circuit diagram showing an example of the configuration of a pixel. [Diagram 23] FIG. 2 is a circuit diagram showing an example of the configuration of a pixel. [Figure 24] FIG. 2 is a circuit diagram showing an example of the configuration of a pixel. [Diagram 25] FIG. 2 is a circuit diagram showing an example of the configuration of a pixel. [Figure 26] FIG. 2 is a circuit block diagram showing a configuration example of a pixel portion. [Figure 27] FIG. [Figure 28] FIG. 1 is a cross-sectional view of a transistor. [Figure 29] FIG. [Diagram 30] FIG. 1 is a cross-sectional view of a transistor. [Diagram 31] FIG. [Diagram 32] FIG. 1 is a cross-sectional view of a transistor. [Diagram 33] FIG. 1 is a cross-sectional view of a transistor. [Diagram 34] 1A and 1B are a top view and a cross-sectional view of a transistor. [Diagram 35] 1A and 1B are a top view and a cross-sectional view of a transistor. [Diagram 36] 1A and 1B are a top view and a cross-sectional view of a transistor. [Figure 37] 1A to 1C are cross-sectional views illustrating a manufacturing process of a transistor. [Figure 38] 1A to 1C are cross-sectional views illustrating a manufacturing process of a transistor. [Figure 39] 1A to 1C are cross-sectional views illustrating a manufacturing process of a transistor. [Diagram 40] 1A to 1C are cross-sectional views illustrating a method for manufacturing a display device. [Diagram 41] 1A to 1C are cross-sectional views illustrating a method for manufacturing a display device. [Diagram 42] 1A to 1C are cross-sectional views illustrating a method for manufacturing a display device. [Diagram 43] FIG. 2 is a perspective view of a display device and an input device. [Diagram 44] FIG. 2 is a cross-sectional view of a display device and an input device. [Diagram 45] FIG. [Figure 46] FIG. 2 is a cross-sectional view of a display device and an input device. [Figure 47] 1A and 1B are a block diagram showing a configuration example of a touch sensor and a timing chart showing an operation example of the touch sensor. [Figure 48] FIG. 4 is a circuit diagram showing an example of a sensor circuit. [Figure 49] FIG. 1 is a perspective view showing an example of a display device. [Figure 50] FIG. 1 is a perspective view showing an example of an electronic device. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0037] Hereinafter, an embodiment will be described with reference to the drawings. However, the embodiment may be different from the embodiment. The present invention can be implemented in any manner without departing from the spirit and scope of the present invention. It will be readily understood by those skilled in the art that various modifications may be made to the embodiments and details of the present invention. The present invention should not be construed as being limited to the description of the following embodiments.

[0038] In addition, the present specification can be appropriately combined with the following embodiments and examples. In addition, when a plurality of configuration examples are shown in one embodiment or example, the configuration examples are mutually exclusive. can be appropriately combined.

[0039] Also, in the drawings, sizes, layer thicknesses, or areas are exaggerated for clarity. Therefore, the scale is not necessarily limited to that shown in the drawings. The drawings are merely schematic illustrations and are not limited to the shapes or values ​​shown in the drawings.

[0040] In the present specification and the like, when describing the connection relationship of a transistor, is expressed as "one of the source and drain" (or the first electrode, or the first terminal), and the source The other of the source and drain is called the "other of the source or drain" (or the second electrode, or the second terminal). This is because the source and drain of a transistor are This is because it changes depending on the operating conditions. In this case, the term source (drain) terminal, source (drain) electrode, etc. should be used appropriately depending on the situation. It can be replaced.

[0041] In this specification, unless otherwise specified, the on-current is the current when a transistor is in the on-state. The drain current when the transistor is in the on state is an n-channel transistor unless otherwise specified. In a transistor, the voltage difference between the gate and source (V GS ) is the transistor threshold voltage (V t h ) above, for p-channel transistors, V GS V th This refers to the following state. Examples For example, the on-current of an n-channel transistor is V GS V th Slave at the above time The on-current of a transistor is the voltage between the drain and source. Pressure (V DS ) may be dependent on

[0042] In this specification, unless otherwise specified, the off-state current refers to the current flowing when a transistor is in an off state. The off state refers to the drain current when the transistor is in the off state unless otherwise specified. At the stadium, V GS V th For p-channel transistors, V GS V th For example, the off-state current of an n-channel transistor is higher than V G S V th The off-state current of a transistor is the drain current when the transistor is off. , V GS Therefore, the off-state current of the transistor may depend on -21 Less than A This means that the off-state current of the transistor is 10 -21 V less than A GS The value exists. It is sometimes said that...

[0043] The off-state current of the transistor is V DS In this specification, Unless otherwise specified, the V DS The absolute value of is 0.1V, 0.8V, 1V, 1.2V , 1.8V, 2.5V, 3V, 3.3V, 10V, 12V, 16V, or 20V Alternatively, in a semiconductor device or the like including the transistor, V used in DS The term "off-state current" may also refer to the off-state current at

[0044] In this specification, the high power supply voltage is referred to as the H level (or V DD ), low power supply voltage L level This is sometimes called the ground (or GND).

[0045] (Embodiment 1) In this embodiment, a configuration example of a display device according to one embodiment of the present invention will be described.

[0046] <Basic configuration> FIG. 1 shows a basic structure of a pixel included in a display device according to one embodiment of the present invention. 0 includes a transistor M1, a capacitance element C1, a capacitance element C2, and a light-emitting element EL1. do.

[0047] The transistor M1 has a first gate and a second gate. The transistors M1 and M2 have an overlapping region with the channel forming region of the transistor M1 therebetween. The transistor M1 has a first terminal which functions as either a source or a drain, and The second terminal functions as the other of the drain and the source terminal.

[0048] The transistor M1 has a channel forming region made of amorphous silicon, polycrystalline silicon, or crystalline silicon. Semiconductors, oxide semiconductors (OS), organic semiconductors, etc. In particular, a transistor having an OS in a channel formation region (hereinafter , OS transistors) are preferable because there is little variation between elements during the manufacturing process.

[0049] The light-emitting element EL1 is an LED (Light Emitting Diode) or an OLED ( Organic Light Emitting Diode), etc. The category includes elements whose brightness is controlled by an EL (Electroluminescent) light emitting diode (OLED). The organic electroluminescence (EL) layer includes an anode and a cathode. The EL layer is composed of a single layer or multiple layers between the anode and cathode. The EL layer is located between the cathode and the anode. When the potential difference between the first and second electrodes becomes equal to or greater than the threshold voltage of the light-emitting element EL1, Electroluminescence is obtained. Hereinafter, the threshold voltage of the light-emitting element EL1 is defined as V E L Electroluminescence is the phenomenon that occurs when the electron returns from the singlet excited state to the ground state. This includes luminescence (fluorescence) and luminescence upon returning from the triplet excited state to the ground state (phosphorescence).

[0050] In addition, one of the anode and cathode of the light-emitting element EL1 functions as a pixel electrode, The other electrode functions as a common electrode. In FIG. 1, the anode of the light-emitting element EL1 is used as a pixel electrode. 1, a configuration in which the cathode of the light-emitting element EL1 is used as a common electrode is illustrated.

[0051] The first terminal of transistor M1 is connected to a potential V ANO The first terminal of the capacitance element C1 is , and a second terminal of the capacitive element C1 is electrically connected to the second gate of the transistor M1. The first terminal of the capacitance element C2 is electrically connected to the first gate. The second terminal of the capacitive element C2 is electrically connected to the second gate of the light-emitting element EL1. The terminal (anode) is electrically connected to the second terminal of the transistor M1, and the first terminal of the light-emitting element EL1 The two terminals (cathode) have a potential of V CAT is given.

[0052] In FIG. 1, the transistor M1 is an n-channel type. ANO is V C AT In particular, the threshold voltage of the transistor M1 is preferably set to a potential higher than V t hThen, V ANO V CAT To, V EL and V th The voltage is higher than the sum of is preferred.

[0053] V at the first terminal of transistor M1 ANO is applied to the second terminal of the light-emitting element EL1, and V CA T When the first gate of the transistor M1 is turned on, the drain of the transistor M1 is turned on in accordance with the image signal applied to the first gate of the transistor M1. The drain current is supplied to the light emitting element EL1, and thus the value of the drain current is determined. EL1 is in a light emitting state.

[0054] The capacitance element C1 has the function of maintaining the potential difference between the first gate and the second terminal of the transistor M1. That is, the capacitance element C1 is a potential difference between the first gate and the source of the transistor M1. The capacitance element C2 has a function of storing the potential difference between the first gate and the second gate. It has the function of holding.

[0055] In one embodiment of the present invention, before determining the value of the drain current of the transistor M1 according to an image signal, In addition, the threshold voltage of the transistor M1 is corrected to eliminate the variation in threshold voltage between different pixels. In addition, a potential corresponding to the image signal is also applied to the second gate, preventing the transistor from Transistor M1 performs dual-gate drive, making it possible to increase the on-current.

[0056] In this specification, Dual-Gate driving refers to driving a first gate and a second gate. This refers to a state in which a high potential (or a low potential) is applied simultaneously.

[0057] Hereinafter, a switch or the like will be added to the pixel 10, and a more specific configuration of the display device according to one embodiment of the present invention will be described. We will explain some examples.

[0058] <Configuration Example of Pixel 20a> FIG. 2A illustrates a configuration example of a pixel 20a included in a display device according to one embodiment of the present invention. The pixel 20a shown in FIG. 1A includes a transistor M1, a switch S1, a switch S2, and a a switch S3, a switch S4, a capacitance element C1, a capacitance element C2, and a light-emitting element EL1. The pixel 20a is the pixel 10 with the addition of switches S1 to S4. The pixel 20a is electrically connected to the wiring L1, the wiring L2, the wiring L3, the wiring L4, and the wiring L5. This is being continued.

[0059] The switches S1 to S4 are each configured using a single transistor or a plurality of transistors. Alternatively, the switches S1 to S4 may each include, in addition to one or more transistors, A capacitive element may also be used.

[0060] A first terminal of the transistor M1 is electrically connected to a line L3.

[0061] The switch S1 has a function of controlling the electrical connection between the line L1 and the first gate. The switch S2 has a function of controlling the electrical connection between the line L2 and the second gate. The switch has a function of controlling the conduction state between the first gate and the second terminal of the transistor M1. The switch S4 has a function of controlling the electrical continuity between the wiring L5 and the second terminal of the transistor M1. .

[0062] The first terminal of the light-emitting element EL1 is electrically connected to the second terminal of the transistor M1. A second terminal of the child EL1 is electrically connected to the wiring L4.

[0063] The line L1 has a function of supplying an image signal to the pixel 20a.

[0064] FIG. 2B shows a more specific example of the configuration of the pixel 20a. 1 shows a circuit diagram in which switches S1 to S4 are replaced with n-channel transistors. The gate of the switch S1 is electrically connected to the wiring GL1, and the gate of the switch S2 is The gate of the switch S3 is electrically connected to the wiring GL2. The gate of the switch S4 is electrically connected to the wiring GL3. When a H level is applied to each, the switch connected to it turns on, and the wiring GL When an L level is applied to GL1 to GL3, the switches connected to each are turned off. do.

[0065] For the switches S1 to S4, it is preferable to use transistors with low off-state current, for example. Here, a low off-state current means that the off-state current is , the normalized off-current per 1 μm of channel width is 10 × 10 -21 A or lower By using transistors with low off-state current for the switches S1 to S4, This allows the image information to be retained in the pixels for as long as the still image is displayed. This reduces the frequency with which image information needs to be rewritten, making it possible to reduce the power consumption of the display device.

[0066] Transistors with low off-state current include OS transistors and transistors with a wide channel formation region. Band gap semiconductors (semiconductors with a band gap of 2.2 eV or more, e.g., silicon carbide) Examples of transistors using silicon dioxide (SiO2), gallium nitride, diamond, etc.

[0067] For details regarding other configurations of the pixel 20a, the description of the pixel 10 may be referred to.

[0068] <Operation Example of Pixel 20a> Next, an example of the operation of the pixel 20a will be described with reference to FIGS.

[0069] In FIG. 3, the potential V DATA and are given to the wiring GL1 to wiring GL3. The timing chart of the potential applied to the wiring L2 and the potential applied to the wiring L3 is shown in FIG. The timing chart has periods P1 to P4. FIG. 4A shows pixel 2 in period P1. FIG. 4(B) shows the state of pixel 20a during period P2, and FIG. 4(C) shows the state of pixel 20a during period P 4(A) to (C) show the states of the pixel 20a in FIG. In order to clearly show the operation of the pixel 20a, the switches S1 to S4 are respectively This is illustrated as a switch.

[0070] The period P1 is a period for initializing the pixel 20a. The period P2 is a period for The threshold voltage is fixed to 0 V during the period P3. Period P4 is a period during which the pixel 20a emits light.

[0071] 4A to 4C, the first gate of the transistor M1 and the first gate of the capacitance element C1 The node between the first terminal and the second gate of the transistor M1 is indicated as a node N1, and the second gate of the transistor M1 and the capacitance element C2 are indicated as a node N2. The node between the second terminal of the transistor M1 and the second terminal of the capacitance element C is indicated as node N2. The node between the second terminal of light-emitting element EL1 and the first terminal of light-emitting element EL1 is designated as node N3.

[0072] In the following description, the potential difference between the first gate and the second terminal of the transistor M1 (node ​​N 1 and node N3) is V GS and the second gate and second terminal of the transistor M1 are The potential difference between the nodes N2 and N3 is V BGS This is expressed as:

[0073] Throughout the periods P1 to P4, V DATA is applied to the wiring L2, and a potential V 0 Given The potential V ANO is applied to the wiring L4, and the potential V CAT is given, and wiring Voltage V at L5 1 is given.

[0074] First, in a period P1, the pixel 20a is initialized. The line GL1 is given an L level. An H level is applied to the wiring GL2, and an H level is applied to the wiring GL3. Switch S4 is turned on and switch S1 is turned off (FIG. 4(A)).

[0075] At this time, node N1 and node N3 are at the same potential, and V GS becomes 0V. Also, the node N1 and N3 are V 1 is applied to node N2, and V 0 Also, during period P1, In order to prevent the light emitting element EL1 from emitting light, V 1 is preferably sufficiently small. To, V 1 -V CAT V EL (the threshold voltage of the light-emitting element EL1) I wish.

[0076] Here, V BGS and V th (threshold voltage of transistor M1) The explanation will be given using the V th V BGS This shows the dependency. BGS The larger , V th It can be seen that V shifts negatively during period P1. BGS =V 0 -V 1 In RuV th V th1 Let us assume that V th1 To make V negative, 0 -V 1 is large enough It is preferable. th1 When V becomes negative, transistor M1 GS =0V The on state is set.

[0077] Next, in period P2, pixel 20a detects the V th Fix the voltage at 0V. An L level is applied to the lines GL1 and GL3, and an H level is applied to the line GL2. Switches S1 and S4 are turned off, and switches S2 and S3 are turned on (FIG. 4(B)).

[0078] A current flows through the transistor M1, and the potential of the node N3 rises. As it rises, V BGS becomes smaller, and from Figure 5, the V th is V th 1 The capacitance element C1 shifts the V GS is kept at 0V, so V t h When V = 0V, GS =V th As a result, the transistor M1 is turned off, and the node N The potential rise of 3 stops.

[0079] In Figure 5, V BGS V when = 0Vth V th0 Then, the following relation holds: stand.

[0080] V th =V th0 -αV BGS (1)

[0081] In formula (1), α is a constant determined by the capacitance value of the gate insulating film, etc. V th If =0, V BGS =V th0 / α (Figure 5).

[0082] In the period P2, it is preferable that no current flows through the light-emitting element EL1. 0 - V CAT V th0 / α+V EL It is preferable that the value is smaller than

[0083] Next, in the period P3, data is written to the pixel 20a. A high level is applied to the line GL1, and a low level is applied to the line GL2. The switches S1 and S4 are on. Switches S2 and S3 are turned off. Node N1 is connected to V DATA is applied, and node N3 is again connected to V 1 is given (Figure 4 (C)). V GS =V DATA -V 1 It becomes.

[0084] At this time, the potential of node N2 is V DATA +V th0 / αto Therefore, V BGS =V DATA +V th0 / α-V 1 The transistor M1 is as follows: The first and second gates are connected to V DATA A potential that depends on the Transistor M1 is now driven by Dual-Gate. The transistor driven by the gate is more efficient than the transistor driven by the single gate. The on current is large.

[0085] Next, in a period P4, the pixel 20a receives the V DATA Depending on Light is emitted. The wirings GL1 to GL3 are given an L level, and the switches S1 to S4 are turned off. become.

[0086] During the period P2, the V th is corrected to 0V, so light emission Element EL1 is the V th It is possible to obtain light emission that is independent of the In addition, the transistor M1 is capable of passing a larger current because it is driven by dual gate. It becomes possible.

[0087] If the transistor M1 is driven by Dual-Gate, the transistor M1 can be made smaller. This allows a large current to flow through the channel width, reducing the area occupied by transistor M1. If the area occupied by the transistor M1 can be reduced, the pixel 20 This makes it possible to reduce the area occupied by a, thereby enabling the provision of a higher-definition display device. It becomes Noh.

[0088] In addition, when the light of the light emitting element EL1 is blocked by the transistor M1 (when the display device is bottom In the case of a MOS emission structure, the area occupied by the transistor M1 is reduced, To provide a display device having a higher display quality by increasing the aperture ratio of the device. This will be possible.

[0089] In the pixel 20a, a current I flows through the transistor M1 via the switch S4 and the line L5. PIX may be supplied to an external circuit. The external circuit provides a current I PIX Depending on the value of By using the above configuration, the pixel 20a can be Zista M1 V th In addition, the mobility of the transistor M1 is compensated for. It will be possible to do this.

[0090] By using the above-described pixel 20a in a display device, a display device in which the luminance variation between pixels is suppressed can be obtained. It is also possible to provide a display device with higher resolution. In addition, it is possible to provide a display device with a higher aperture ratio. It becomes possible to provide a high-quality display device.

[0091] <Configuration example of pixel 21a> The pixel 20a shown in FIG. 2A may omit the switch S3. 6(A).

[0092] A configuration example of a pixel 21a included in a display device according to one embodiment of the present invention is shown in FIG. The pixel 21a shown in A) includes a transistor M1, a switch S1, a switch S2, and a The pixel has a capacitance element C1, a capacitance element C2, and a light-emitting element EL1. 21a is electrically connected to the wiring L1, the wiring L2, the wiring L3, the wiring L4, and the wiring L5. The transistor M1 has a first gate and a second gate. The gates are overlapping regions with the channel forming region of the transistor M1 in between. do.

[0093] FIG. 6B shows a more specific example of the configuration of the pixel 21a. The circuit diagram shows the case where the switches S1, S2, and S4 are replaced with n-channel transistors. The gate of the switch S1 is electrically connected to the wiring GL1, and the gate of the switch S2 is The gate of the switch S4 is electrically connected to the wiring GL3. can be.

[0094] Pixel 21a does not have switch S3 and the V th below 0V The pixel 20a shown in FIG. 2 differs from the pixel 20a shown in FIG. 2 in that the pixel 20a can be set outside the pixel 20a. The other configurations are the same as those of the pixel 20a. The description of pixel 20a should be taken into consideration.

[0095] <Operation Example of Pixel 21a> Next, an example of the operation of the pixel 21a will be described with reference to FIGS. By using the same symbols as in Figure 4 for the potential (or potential difference), Let us use the term "difference" to represent the difference between the two.

[0096] In FIG. 7, a potential applied to the wiring L1, a potential applied to the wirings GL1 to GL3, and a potential applied to the wirings 7 shows a timing diagram of the potential applied to L3. The period includes periods P1 to P4. FIG. 8A shows the state of the pixel 21a in the period P1. FIG. 8B shows the state of pixel 21a during period P2, and FIG. 8C shows the state of pixel 21a during period P3. 8(A) to 8(C) show the states of the pixel 21a. In order to easily understand the operation, the switches S1, S2, and S4 are each The figure shows the

[0097] The period P1 is a period for initializing the pixel 21a. The period P2 is a period for The threshold voltage is V 2 -V 1 In the period P3, data is written to the pixel 21a. Period P4 is a period during which the pixel 21a emits light.

[0098] 8A to 8C, the first gate of the transistor M1 and the first gate of the capacitance element C1 The node between the first terminal of the transistor M1 and the first terminal of the capacitance element C2 is referred to as a node N1. The node between the second gate and the second terminal of the capacitance element C2 is designated as node N2. A node between the second terminal of the capacitance element C1 and the first terminal of the light emitting element EL1 is connected to a node. The code is shown as N3.

[0099] Throughout the periods P1 to P4, V 0 is applied to the wiring L3, ANO is given , V to wire L4 CAT is applied to the wiring L5. 1 is given.

[0100] First, in a period P1, the pixel 21a is initialized. A high level is applied to the line GL1. An H level is applied to the wiring GL2, and an H level is applied to the wiring GL3. and S4 is turned on (FIG. 8(A)).

[0101] At this time, an arbitrary fixed potential (potential V 2 ) is given. V 2 Given The node N2 is connected to V 0 is applied to node N3, and V 1 In this case, V G S =V2 -V 1 , V BGS =V 0 -V 1 The threshold voltage of transistor M1 is V t h1 become.

[0102] Next, in a period P2, the pixel 21a th V 2 -V 1 Fixed to An L level is applied to the wires GL1 and GL3, and an H level is applied to the wire GL2. Switches S1 and S4 are turned off and switch S2 is turned on. Node N2 is V 0 Given (Figure 8(B)).

[0103] At this time, a current flows through the transistor M1, and the potential of the node N3 rises. 1, V GS is V 2 -V 1 Since it is kept at V th =V 2 -V 1 When V GS =V th This causes the transistor M1 to be turned off, and the potential rise at the node N3 stops. At this time, V BGS (V th0 -V 2 +V 1 ) / α (Figures 5 and 8(B)).

[0104] Next, in the period P3, data is written to the pixel 21a. A high level is applied to the line GL1, and a low level is applied to the line GL2. The switches S1 and S4 are turned on. Switch S2 is turned on and switch S2 is turned off. Node N1 is connected to V DATA is applied, and node N3 is again connected to V1 In this case, V GS =V DATA -V 1 , V BGS =V DATA -V 2 +(V th0 -V 2 +V 1 ) / α (Figure 8(C)).

[0105] The transistor M1 has a first gate and a second gate connected to V DATA A potential dependent on That is, the transistor M1 is driven by a dual gate.

[0106] During the period P2, the V th is V 2 -V 1 Since it has been corrected to the state of , the light-emitting element EL1 is V th It is now possible to obtain light emission that is independent of In addition, the transistor M1 is driven as a dual gate, so it can pass a larger current. This makes it possible.

[0107] If the transistor M1 is driven by Dual-Gate, the transistor M1 can be made smaller. This allows a large current to flow through the channel width, reducing the area occupied by transistor M1. If the area occupied by the transistor M1 can be reduced, the pixel 21 This makes it possible to reduce the area occupied by a, thereby enabling the provision of a higher-definition display device. It becomes Noh.

[0108] In addition, when the light of the light emitting element EL1 is blocked by the transistor M1, By reducing the area occupied by the display device 1, it is possible to increase the aperture ratio of the display device. It is therefore possible to provide a display device with high display quality.

[0109] In the pixel 21a, a current I flows through the transistor M1 via the switch S4 and the line L5. PIX may be supplied to an external circuit. The external circuit provides a current I PIX Depending on the value of By using the above configuration, the pixel 21a can be Zista M1 V th In addition, the mobility of the transistor M1 is compensated for. It will be possible to do this.

[0110] By using the above-described pixel 21a in a display device, a display device in which the luminance variation between pixels is suppressed can be obtained. It is also possible to provide a display device with higher resolution. In addition, it is possible to provide a display device with a higher aperture ratio. It becomes possible to provide a high-quality display device.

[0111] <Configuration example of pixel 22a> The pixel 20a shown in FIG. 2A may omit the switch S4 and the line L5. In that case, An example of the configuration is shown in FIG.

[0112] FIG 9A illustrates a configuration example of a pixel 22a included in a display device according to one embodiment of the present invention. The pixel 22a shown in FIG. 1A includes a transistor M1, a switch S1, a switch S2, and a The pixel includes a pixel electrode S3, a capacitance element C1, a capacitance element C2, and a light-emitting element EL1. The element 22a is electrically connected to the wiring L1, the wiring L2, the wiring L3, and the wiring L4. The transistor M1 has a first gate and a second gate. , and have an overlapping region with the channel formation region of the transistor M1 therebetween.

[0113] FIG. 9B shows a more specific example of the configuration of the pixel 22a. 1 shows a circuit diagram in which switches S1 to S3 are replaced with n-channel transistors. The gate of switch S1 is electrically connected to wiring GL1, and the gate of switch S2 is The gate of the switch S3 is electrically connected to the wiring GL3.

[0114] The pixel 22a differs from the pixel 20a shown in FIG. 2 in that it does not have the switch S4 and the line L5. The other configurations are the same as those of the pixel 20a, and the description of the pixel 20a may be referred to.

[0115] <Operation Example of Pixel 22a> Next, an example of the operation of the pixel 22a will be described with reference to FIGS. 10 and 11. In FIG. 11, the potential (or potential difference) is indicated by the same reference numerals as in FIG. 4 or FIG. 8. This represents the electric potential (or potential difference).

[0116] In FIG. 10, a potential applied to the wiring L1, a potential applied to the wirings GL1 to GL3, and a 10 shows a timing chart of the potential applied to the line L3. The period includes periods P1 to P4. FIG. 11A shows the state of the pixel 22a in the period P1. 11(B) shows the state of pixel 22a in period P2, and FIG. 11(C) shows the state of pixel 22a in period P3. 11(A) to 11(C) respectively show the states of the pixel 22a in the following cases: To clearly illustrate the operation of pixel 22a, switches S1 to S3 are This is illustrated as Chi.

[0117] The period P1 is a period for initializing the pixel 22a. The period P2 is a period for The threshold voltage is fixed to 0 V during the period P3. Period P4 is a period during which the pixel 22a emits light.

[0118] 11A to 11C, the first gate of the transistor M1 and the first gate of the capacitance element C1 The node with the first terminal is indicated as node N1, and the second gate of the transistor M1 and the capacitance element C The node between the second terminal of the transistor M1 and the second terminal of the capacitor element The node between the second terminal of C1 and the first terminal of the light-emitting element EL1 is designated as node N3.

[0119] Throughout the periods P1 to P4, V DATA is applied to wiring L2, and V 0 Given And V is connected to wire L4. CAT is given.

[0120] First, in a period P1, the pixel 22a is initialized. The line GL1 is given an L level. A high level is applied to GL2 and GL3. Switch S1 is turned off, and switches S2 and Then, S3 is turned on (FIG. 11(A)).

[0121] A low potential (potential V L ) is applied to node N2, and V 0 is given. Node N1 At this time, the potentials of the nodes N1 and N3 are equal to the potential V 3 So, , V GS = 0V, V BGS =V 0 -V 3 In addition, the threshold voltage of the transistor M1 is V th2 During the period P1, V LBy providing In addition, it prevents a current from flowing to the light-emitting element EL1.

[0122] Next, in period P2, pixel 22a detects the V th Fix the voltage at 0V. An L level is applied to the lines GL1 and GL3, and an H level is applied to the line GL2. Switches S1 and S3 are turned off and switch S2 is turned on. Node N2 is V 0 is given In addition, wiring L3 is connected to V ANO is given (Figure 11(B)).

[0123] At this time, a current flows through the transistor M1, and the potential of the node N3 rises. 1, V GS is kept at 0V, so V th When V = 0V, GS =V th And This turns off the transistor M1, and the potential rise of the node N3 stops. BGS is V th0 / α.

[0124] Next, in a period P3, data is written to the pixel 22a. is applied, and the L level is applied to the wirings GL2 and GL3. The switch S1 is turned on. , switches S2 and S3 are turned off. Node N1 is connected to V DATA At this time, the potential of node N3 is V 4 Then, V GS =V DATA -V 4 , V BGS =V DATA +V th0 / α-V 4 (Figure 11(C)).

[0125] The transistor M1 has a first gate and a second gate connected to V DATA A potential dependent on That is, the transistor M1 is driven by a dual gate.

[0126] During the period P2, the V th is corrected to 0V, so light emission Element EL1 is the V th It is possible to obtain light emission that is independent of the In addition, the transistor M1 is capable of passing a larger current because it is driven by dual gate. It becomes possible.

[0127] If the transistor M1 is driven by Dual-Gate, the transistor M1 can be made smaller. This allows a large current to flow through the channel width, reducing the area occupied by transistor M1. If the area occupied by the transistor M1 can be reduced, the pixel 22 This makes it possible to reduce the area occupied by a, thereby enabling the provision of a higher-definition display device. It becomes Noh.

[0128] In addition, when the light of the light emitting element EL1 is blocked by the transistor M1, By reducing the area occupied by the display device 1, it is possible to increase the aperture ratio of the display device. It is therefore possible to provide a display device with high display quality.

[0129] By using the above-mentioned pixel 22a in a display device, a display device in which the luminance variation between pixels is suppressed can be obtained. It is also possible to provide a display device with higher resolution. In addition, it is possible to provide a display device with a higher aperture ratio. It becomes possible to provide a high-quality display device.

[0130] <Configuration example of pixel 23a> The pixel 20a shown in FIG. 2A can be used without the switches S3 and S4 and the line L5. The circuit diagram for this case is shown in Figure 12(A).

[0131] FIG. 12A illustrates a configuration example of a pixel 23a included in a display device according to one embodiment of the present invention. The pixel 23a shown in FIG. 12(A) includes a transistor M1, a switch S1, and a switch S2. The pixel 23a includes a capacitive element C1, a capacitive element C2, and a light-emitting element EL1. The transistor is electrically connected to the wiring L1, the wiring L2, the wiring L3, and the wiring L4. The transistor M1 has a first gate and a second gate. The first gate and the second gate are The first and second electrodes have an overlapping region with the channel formation region of the second electrode M1 therebetween.

[0132] FIG. 12B shows a more specific example of the configuration of the pixel 23a. ) Switch S1 and switch S2 are replaced with n-channel transistors. The gate of the switch S1 is electrically connected to the wiring GL1, and the gate of the switch S2 is electrically connected to the wiring GL1. The gate of is electrically connected to the wiring GL2.

[0133] The pixel 23a is different from the pixel shown in FIG. 2 in that it does not have the switch S3, the switch S4, and the line L5. The other configurations are the same as those of the pixel 20a, and the description of the pixel 20a should be referred to. Just do that.

[0134] <Operation Example of Pixel 23a> Next, an example of the operation of the pixel 23a will be described with reference to FIGS. 13 and 14. FIG. 14 uses the same symbols as FIG. 4, FIG. 8, or FIG. 11 for potentials (or potential differences). , represent the same potential (or potential difference).

[0135] In FIG. 13, a potential applied to the wiring L1, a potential applied to the wirings GL1 to GL3, and a 13 shows a timing chart of the potential applied to the line L3. The period includes periods P1 to P4. FIG. 14A shows the state of the pixel 23a in the period P1. 14(B) shows the state of pixel 23a in period P2, and FIG. 14(C) shows the state of pixel 23a in period P3. 14(A) to 14(C) respectively show the states of the pixel 23a in the above-mentioned cases. In order to clearly illustrate the operation of the pixel 23a, the switches S1 and S2 are This is illustrated as Chi.

[0136] The period P1 is a period for initializing the pixel 23a. The period P2 is a period for The threshold voltage is V 2 -V 5 In the period P3, data is written to the pixel 23a. Period P4 is a period during which the pixel 23a emits light.

[0137] 14A to 14C, the first gate of the transistor M1 and the first gate of the capacitance element C1 The node between the first terminal and the first terminal of the capacitance element C2 is referred to as node N1. The node between the second gate of the transistor A node between the second terminal of M1, the second terminal of the capacitance element C1, and the first terminal of the light-emitting element EL1 is It is designated as node N3.

[0138] Throughout the periods P1 to P4, V 0 is applied to wire L4, and V CAT is given do.

[0139] First, in a period P1, the pixel 23a is initialized. An H level is applied to the wirings GL1 and GL2. The switches S1 and S2 are turned on (FIG. 14(A)).

[0140] An arbitrary fixed potential (potential V 2 ) is applied to the wiring L3, and a low potential (potential V L ) is given Node N1 is V 2 is applied to node N2, and V 0 At this time, The potential of node N3 is V 5 Then, V GS =V 2 -V 5 , V BGS =V 0 -V 5 It becomes Also, the threshold voltage of transistor M1 is V th3 In the period P1, the wiring L3 V L By providing this, a current is prevented from flowing through the transistor M1 and the light-emitting element EL1.

[0141] Next, in a period P2, the pixel 23a th V 2 -V 5 Fixed to The L level is applied to the wiring GL1, and the H level is applied to the wiring GL2. 1 is turned off and switch S2 is turned on. Node N2 is V 0 Also, the distribution Line L3 has V ANO is given (Figure 14(B)).

[0142] At this time, a current flows through the transistor M1, and the potential of the node N3 rises. 1, V GS is V 2 -V 5 Since it is kept at V th =V 2 -V5 When V GS =V th This causes the transistor M1 to be turned off, and the potential rise at the node N3 stops. At this time, V BGS (V th0 -V 2 +V 5 ) / α.

[0143] Next, in the period P3, data is written to the pixel 23a. is applied, and the L level is applied to the wiring GL2. The switch S1 is turned on, and the switch S2 is turned off. Node N1 is connected to V through switch S1. DATA is given. When the potential of node N3 is V 6 Then, V GS =V DATA -V 6 , V BGS =V DA TA -V 2 +V 5 +(V th0 -V 2 +V 5 ) / α-V 6 (Figure 14(C)).

[0144] The transistor M1 has a first gate and a second gate connected to V DATA A potential dependent on That is, the transistor M1 is driven by a dual gate.

[0145] During the period P2, the V th is V 2 -V 5 Since it has been corrected to the state of , the light-emitting element EL1 is V th It is now possible to obtain light emission that is independent of In addition, the transistor M1 is driven as a dual gate, so it can pass a larger current. This makes it possible.

[0146] If the transistor M1 is driven by Dual-Gate, the transistor M1 can be made smaller. This allows a large current to flow through the channel width, reducing the area occupied by transistor M1. If the area occupied by the transistor M1 can be reduced, the pixel 23 This makes it possible to reduce the area occupied by a, thereby enabling the provision of a higher-definition display device. It becomes Noh.

[0147] In addition, when the light of the light emitting element EL1 is blocked by the transistor M1, By reducing the area occupied by the display device 1, it is possible to increase the aperture ratio of the display device. It is therefore possible to provide a display device with high display quality.

[0148] By using the above-described pixel 23a in a display device, a display device in which the luminance variation between pixels is suppressed can be obtained. It is also possible to provide a display device with higher resolution. In addition, it is possible to provide a display device with a higher aperture ratio. It becomes possible to provide a high-quality display device.

[0149] Other pixel configuration examples The above-mentioned pixels 20a to 23a have a first gate and a second gate of the transistor M1. The circuit diagrams in this case are shown in Figures 15(A) to (D). 15(B) corresponds to pixel 21a. 15(C) corresponds to pixel 22a, and pixel 23 shown in FIG. 15(D) corresponds to pixel 22b. b corresponds to pixel 23a.

[0150] The above-mentioned pixels 20a to 23a have a capacitance element C1 connected to the first gate of the transistor M1. The circuit diagrams for this case are shown in Figures 16(A) to 16(D). Pixel 20c shown in FIG. 16(A) corresponds to pixel 20a, and pixel 21c shown in FIG. corresponds to pixel 21a, pixel 22c shown in FIG. 16(C) corresponds to pixel 22a, and The pixel 23c shown in D) corresponds to the pixel 23a.

[0151] The above-mentioned pixels 20a to 23a have first and second gates connected to the switches S1 to S4. A transistor having the above structure may be used. Circuit diagrams in this case are shown in FIGS. The pixel 20d shown in FIG. 17(A) corresponds to the pixel 20a, and the pixel 21 shown in FIG. 17(C) corresponds to pixel 22a, and pixel 22d shown in FIG. 17(D) corresponds to pixel 22a. The pixel 23d shown in (D) corresponds to the pixel 23a. The gates are connected to a common potential V 7 By adopting the above configuration, The threshold voltages of switches S1 to S4 can be controlled.

[0152] In addition, the switches S1 to S4 shown in FIGS. 17(A) to 17(D) have first and second gates. The circuit diagrams in this case are shown in Figures 18(A) to 18(D). The pixel 20e shown in FIG. 18(A) corresponds to the pixel 20d, and the pixel 21e shown in FIG. 18(C) corresponds to pixel 22d, and the pixel 22e shown in FIG. 18(D) corresponds to pixel 22e. The pixel 23e corresponds to the pixel 23d. It is possible to improve the on-current of the transistor.

[0153] In the above-mentioned pixels 20a to 23a, the transistor M1 is a p-channel transistor. The positions of the anode and cathode of the photoelement EL1 may be interchanged. The circuit diagram in this case is shown in FIG. The pixel 20f shown in FIG. 19(A) corresponds to the pixel 20a, and the pixel 20f shown in FIG. 19(B) corresponds to the pixel 20a. The pixel 21f shown in FIG. 19(C) corresponds to the pixel 21a, and the pixel 22f shown in FIG. 19(C) corresponds to the pixel 22a. 19(D) corresponds to the pixel 23a. By swapping the positions of the cathode and cathode, the wiring L3 has V CAT is given, and V A NO is preferably given.

[0154] The above-mentioned pixels 20a to 23a each include a second terminal of the capacitance element C1 and a first terminal of the light-emitting element EL1. A switch S5 may be provided between the input and the output. Circuit diagrams in this case are shown in Figures 20(A) to 20(D). The pixel 20g shown in FIG. 20A corresponds to the pixel 20a, and the pixel 20g shown in FIG. 1g corresponds to pixel 21a, pixel 22g shown in FIG. 20(C) corresponds to pixel 22a, and Pixel 23g shown in FIG. 20(D) corresponds to pixel 23a. The switch S5 is an n-channel transistor. The gate is electrically connected to the wiring GL4. By providing the light emitting element EL1, it becomes possible to control the current flowing through the light emitting element EL1.

[0155] The above-mentioned pixels 20a to 23a each have a switch between the first terminal of the transistor M1 and the line L3. A switch S5 may be provided. Circuit diagrams in this case are shown in Figures 21(A) to (D). 21(B) corresponds to pixel 21a. 21(C) corresponds to pixel 22a, and the pixel 22h shown in FIG. 21(D) corresponds to pixel 22a. Pixel 23h corresponds to pixel 23a. The gate of the switch S5 is connected to the wiring G By using the above configuration, the pixels 20h to 23h are electrically connected to the transistors L1 and L2. It is possible to control the current flowing through the transistor M1 and the light-emitting element EL1.

[0156] The above-mentioned pixels 20a to 23a each include a second terminal of the transistor M1 and a second terminal of the capacitance element C1. A switch S5 may be provided between the MOSFET and the power supply. Circuit diagrams in this case are shown in Figures 22(A) to 22(D). The pixel 20i shown in FIG. 22(A) corresponds to the pixel 20a, and the pixel 21 shown in FIG. 22(B) corresponds to the pixel 21. i corresponds to pixel 21a, pixel 22i shown in FIG. 22(C) corresponds to pixel 22a, and The pixel 23i shown in (D) corresponds to the pixel 23a. The gate of switch S5 is an n-channel transistor. The gate is electrically connected to the wiring GL4. 23i can control the current flowing through the transistor M1 and the light-emitting element EL1. do.

[0157] In the above-described pixels 20a to 23a, a capacitive element C3 may be connected in parallel to the light-emitting element EL1. Circuit diagrams in this case are shown in FIGS. 23(A) to (D). The pixel 20j shown in FIG. 23(A) is 23(C) corresponds to pixel 20a, pixel 21j shown in FIG. 23(B) corresponds to pixel 21a, 23(D) corresponds to pixel 23a. By adopting the above configuration, the pixels 20j to 23j each have a first terminal of the light-emitting element EL1. This makes it possible to stabilize the potential of the electron.

[0158] In the above-described pixels 20a to 23a, the positions of the anode and cathode of the light-emitting element EL1 may be interchanged. Circuit diagrams in this case are shown in FIGS. 24(A) to (D). The pixel 20k shown in FIG. 24(C) corresponds to pixel 20a, pixel 21k shown in FIG. 24(B) corresponds to pixel 21a, 24(D) corresponds to pixel 23a. In pixels 20k and 22k, the switch S3 has a first gate and a transistor The pixel 20k to the pixel 23k have a function of controlling the conduction state between the first terminal of the pixel M1 and the first terminal of the pixel M2. In the capacitance element C1, a first terminal is electrically connected to a first gate, and a first The second terminal is electrically connected to the first terminal of the transistor M1. By swapping the cathode positions, V CAT is given, and V AN O is preferably given.

[0159] The above-described pixels 20a to 23a may also be configured with the transistor M1 as a p-channel transistor. Circuit diagrams in this case are shown in FIGS. 25(A) to 25(D). 25(B) corresponds to pixel 21a, and pixel 21l shown in FIG. 25(B) corresponds to pixel 21a. The pixel 22l shown in FIG. 25(C) corresponds to the pixel 22a, and the pixel 23l shown in FIG. 25(D) corresponds to the pixel 23a. In pixels 20l and 22l, the switch S3 is connected to the first gate and the transistor The pixel 201 has a function of controlling the conduction state between the first terminal of the transistor M1 and the pixel 202. In l, the first terminal of the capacitance element C1 is electrically connected to the first gate, and the capacitance element C1 The second terminal of the transistor M1 is electrically connected to the first terminal of the transistor M2.

[0160] Example of pixel section and selection circuit configuration Next, FIG. 26 shows an example of a structure of a pixel portion of a display device according to one embodiment of the present invention.

[0161] In FIG. 26, the pixel section 40 has a plurality of pixels 20a arranged in a matrix. The pixel section 40 includes wirings GL1 to GL3 connected to the drive circuit 110 and a 20, wiring L1 to L3, wiring L4 (not shown), and wiring L5. In addition, in FIG. 26, the wirings GL1 to GL3 are represented as one wiring GL. Each of the pixels 20a is connected to at least one of the wirings GL1 and at least one of the wirings GL2. At least one of the wirings GL3, at least one of the wirings L1, and at least one of the wirings L2 one of the wirings L1, at least one of the wirings L2, at least one of the wirings L3, at least one of the wirings L4, and at least one of the wirings L5. Each of the two is electrically connected to the other.

[0162] The type and number of the wirings are determined based on the configuration, number and arrangement of the pixels 20a. Specifically, in the case of the pixel section 40 shown in FIG. 26, the pixels 20a in m rows and n columns are arranged in a matrix. The wirings GL[1] to GL[m] are electrically connected to each other in a grid shape. A line GL, a plurality of wirings L1 indicated by wirings L1[1] to L1[n], and wirings L2[1] to A plurality of wirings L2 indicated by L2[n] and a plurality of wirings L3[1] to L3[n] 3 and a plurality of wirings L5 indicated by wirings L5[1] to L5[n] are disposed in the pixel section 40. This shows an example of a case where

[0163] Although FIG. 26 shows an example of the configuration of a pixel section having the pixel 20a, the present invention is not limited to this. can be applied to all the pixels exemplified in this embodiment.

[0164] (Embodiment 2) In this embodiment, a channel transistor applicable to the pixel transistor described in the above embodiment will be described. a transistor in which a gate formation region is formed using an oxide semiconductor film (OS transistor); and and a transistor in which the channel formation region is formed of silicon (Si transistor). An example will be given.

[0165] <Transistor configuration example 1> First, the OS transistor will be described.

[0166] Figures 27(A), 27(B), and 27(C) show three transistors with different device structures. The top view (layout diagram) of the resistors (TA1, TA2, TB1) and their respective circuit symbols are shown below. FIG. 28 is a cross-sectional view of the transistors (TA1, TA2, and TB1). TA1 is a cross-sectional view taken along the lines a1-a2 and b1-b2. Cross-sectional views taken along lines a4 and b3-b4, and lines a5-a6 of transistor TB1; The cross-sectional views taken along the line b5-b6 are shown in FIG. 28(A) and FIG. 28(B). The cross-sectional structure in the channel length direction is shown in FIG. 28(A), and the cross-sectional structure in the channel width direction is shown in FIG. Shown in Figure 28(B).

[0167] As shown in FIG. 28(A) and (B), the transistors (TA1, TA2, TB1) are the same. These transistors are integrated on an insulating surface and can be fabricated in the same fabrication process. In order to clarify the device structure, the gate of each transistor is shown in FIG. (G), source (S), and drain (D) are connected to the wiring for supplying potential and power. Electrical connections are omitted.

[0168] The transistor TA1 (FIG. 27(A)) and the transistor TA2 (FIG. 27(B)) have gates The gate electrode is a first gate electrode (G) and a back gate electrode (BG). The gate electrode corresponds to the first gate electrode, and the back gate electrode corresponds to the second gate electrode. The back gate electrode of transistor TA1 and transistor TA2 are connected to the gate electrode. The transistor TB1 (FIG. 27(C)) is a transistor that does not have a back gate electrode. As shown in FIG. 28, these transistors (TA1, TA2, TB1) are 30. The configuration of these transistors will be described below with reference to FIGS. 27 and 28. Explain.

[0169] [Transistor TA1] The transistor TA1 includes a gate electrode GE1, a source electrode SE1, a drain electrode DE1, and a The gate electrode BGE1 and the oxide semiconductor film OS1 are provided.

[0170] In this embodiment, the channel length of the OS transistor is determined by dividing the length of the source electrode and the drain electrode by the distance between the source electrode and the drain electrode. The channel width of the OS transistor is the distance between the oxide semiconductor film and the gate electrode. The width of the source electrode or drain electrode in the overlapping region is defined as the width of the The channel length is La1 and the channel width is Wa1.

[0171] The oxide semiconductor film OS1 overlaps with the gate electrode GE1 via the insulating film 34. A pair of electrodes (SE1, DE1) are formed in contact with the top and side surfaces of the semiconductor film OS1. As shown in FIG. 27A, the oxide semiconductor film OS1 is provided with a gate electrode GE1 and a pair of The oxide semiconductor film OS1 has a portion that does not overlap with the electrodes (SE1, DE1). The length in the channel length direction is longer than the channel length La1, and the length in the channel width direction is It is longer than the width Wa1.

[0172] An oxide semiconductor film OS1, a gate electrode GE1, a source electrode SE1, and a drain electrode DE1 An insulating film 35 is formed to cover the back gate electrode BGE1. The back gate electrode BGE1 is formed by the oxide semiconductor film OS1 and the gate electrode G Here, as an example, the gate electrode GE1 is formed to overlap with the gate electrode E1. The back gate electrodes BGE1 are arranged in the same position. The gate electrode BGE1 is provided at an opening CG1 penetrating the insulating film 34, the insulating film 35, and the insulating film 36. This structure allows the gate electrode of the transistor TA1 to be in contact with the gate electrode GE1. and the back gate electrode are electrically connected.

[0173] By connecting the back gate electrode BGE1 to the gate electrode GE1, The on-current can be increased. The strength of the resistor TA1 can be improved. The gate electrode BGE1 acts as a reinforcing member to make the transistor TA1 less likely to break. Cut.

[0174] The oxide semiconductor film OS1 including the channel formation region has a multi-layer structure. The oxide semiconductor film OS has a three-layer structure consisting of three oxide semiconductor films 31, 32, and 33. The oxide semiconductor film constituting 1 is a metal oxide film containing at least one identical metal element. It is preferable that the semiconductor film of the transistor contains In, and it is particularly preferable that the semiconductor film contains In. Examples of metal oxides containing In that can be used include In-Ga oxide films and In-M-Zn oxide films. The typical example is a film (where M is Al, Ga, Y, Zr, La, Ce, or Nd). It is also possible to use a film in which other elements or materials are added to such a metal oxide film.

[0175] The oxide semiconductor film 32 is a film that constitutes a channel formation region of the transistor TA1. The oxide semiconductor film 33 is a transistor for transistors TA2 and TB1, which will be described later. The oxide semiconductor film 33 is also a film that constitutes a channel forming region. The electrical characteristics required for the transistor TA2 and the transistor TB1 (e.g., field effect mobility, An oxide semiconductor film having an appropriate composition may be used depending on the characteristics of the semiconductor device (eg, threshold voltage).

[0176] In the transistor TA1, a channel is formed in the oxide semiconductor film 32. In this way, the channel forming region can be prevented from contacting the insulating films 34 and 35. The oxide semiconductor films 31 to 33 are metal oxide films containing at least one of the same metal elements. As a result, the interface between the oxide semiconductor film 32 and the oxide semiconductor film 31 and the interface between the oxide semiconductor film 32 and the oxide semiconductor film 31 are This makes it possible to make it difficult for interface scattering to occur at the interface of the compound semiconductor film 33. Therefore, the field effect mobility of the transistor TA1 is set to be higher than that of the transistor TA2 and the transistor TB1. It is also possible to increase the drain current (on-state current) in the on-state. It is possible.

[0177] [Transistor TA2] The transistor TA2 includes a gate electrode GE2, a source electrode SE2, a drain electrode DE2, and a The back gate electrode BGE2 and the oxide semiconductor film OS2 are E2 is connected to the gate electrode GE2 at an opening CG2 penetrating the insulating films 34 to 36. The transistor TA2 is a modified example of the transistor TA1, and has an oxide semiconductor film The transistor OS2 is different from the transistor TA1 in that it has a single-layer structure made of an oxide semiconductor film 33. The other parts are the same. Here, the channel length La2 of the transistor TA2, the channel The channel width Wa2 is equal to the channel length La1 and the channel width Wa1 of the transistor TA1. I try to do so.

[0178] [Transistor TB1] The transistor TB1 has a gate electrode GE3, a source electrode SE3, a drain electrode DE3 and a The transistor TB1 is a modified example of the transistor TA2. As in the transistor TA2, the oxide semiconductor film OS3 is not the oxide semiconductor film 33. It has a single-layer structure. It differs from the transistor TA2 in that it does not have a back gate electrode. In addition, the layout of the oxide semiconductor film OS3 and the electrodes (GE3, SE3, DE3) is As shown in FIG. 27C, the oxide semiconductor film OS3 overlaps with the gate electrode GE3. The non-existent region overlaps with either the source electrode SE3 or the drain electrode DE3. Therefore, the channel width Wb1 of the transistor TB1 is determined by the width of the oxide semiconductor film OS3. The channel length Lb1 is set to be the length between the source electrode SE3 and the drain electrode SE4, as in the transistor TA2. The distance between the drain electrodes DE3 is determined by the channel length La of the transistor TA2. It is longer than 2.

[0179] [Insulating film] The insulating film 34, the insulating film 35, and the insulating film 36 are formed on the transistors TA1, TA2, The insulating film 34, the insulating film 35, and the insulating film 36 are formed on the entire area where the TB1 is formed. The insulating film 36 is formed of a single layer or multiple layers of insulating film. The insulating film 35 and the insulating film 36 are also included in the gate insulating film of A1, TA2, and TB1. The film 36 constitutes the gate insulating film on the back channel side of the transistors TA1, TA2, and TB1. The insulating film 36 on the top surface serves as a protection film for the transistors formed on the substrate 30. It is preferable to form the insulating film 36 from a material that functions as a protective film. In order to insulate the third layer electrode (BGE1) from the second layer electrodes (SE1, DE1), At least one insulating film needs to be present between them.

[0180] The insulating films 34 to 36 may be formed of a single layer insulating film or a multilayer insulating film having two or more layers. The insulating films 34 to 36 can be made of aluminum oxide. Aluminum, magnesium oxide, silicon oxide, silicon oxynitride, silicon nitride oxide, nitrogen silicon oxide, gallium oxide, germanium oxide, yttrium oxide, zirconium oxide, Examples of the film include films made of lanthanum oxide, neodymium oxide, hafnium oxide, and tantalum oxide. These insulating films can be formed by sputtering, CVD, MBE, ALD, or It can be formed by using a PLD method.

[0181] [Oxide semiconductor film] Here, an oxide semiconductor film which is a semiconductor film of an OS transistor will be described. When a semiconductor film has a multi-layer structure like the oxide semiconductor film OS1, the oxide semiconductors that compose it are The conductive film is preferably a metal oxide film containing at least one of the same metal elements, and In It is preferred that the compound contains

[0182] For example, when the oxide semiconductor film 31 is an In-Ga oxide film, the atomic ratio of In is set to the atomic ratio of Ga. The ratio should be smaller than the numerical ratio. In-M-Zn oxide film (M is Al, Ga, Y, Zr, La, C In the case of (e) or (d), the atomic ratio of In is made smaller than the atomic ratio of M. In this case, It is possible to make the atomic ratio of Zn the largest.

[0183] For example, when the oxide semiconductor film 32 is an In-Ga oxide film, the atomic ratio of In is set to the atomic ratio of Ga. In the case of an In-M-Zn oxide film, the atomic ratio of In is set to be larger than the atomic ratio of M. In the In-M-Zn oxide film, the atomic ratio of In is larger than that of M and Zn. It is preferable to make it larger than the numerical ratio.

[0184] For example, when the oxide semiconductor film 33 is an In-Ga oxide film, the atomic ratio of In is set to the atomic ratio of Ga. In the case of In-M-Zn oxide film, the atomic ratio of In is set to be equal to or smaller than the atomic ratio of In. The atomic ratio of Zn is set to be the same as that of M. In this case, the atomic ratio of Zn is larger than that of In and M. Here, the oxide semiconductor film 33 is a transistor TA2. It is also the membrane that constitutes the channel-forming region of TAB1.

[0185] The atomic ratio of the oxide semiconductor films 31 to 33 is set to 1 / 1000 when the oxide semiconductor films are formed by a sputtering method. This is possible by adjusting the atomic ratio of the constituent materials of the CVD method. In this case, it is possible to adjust the flow rate ratio of the raw material gases. As an example of forming an In-M-Zn oxide film by sputtering, The targets used for depositing these films are In-M-Zn A target made of an oxide is used.

[0186] The atomic ratio of the metal elements in the target of the oxide semiconductor film 31 is In:M:Zn=x1:y1: If z1 is used, 、 It is preferable that x1 / y1 is equal to or greater than 1 / 6 and less than 1. It is preferable that 1 is ⅓ or more and 6 or less, and more preferably 1 or more and 6 or less.

[0187] Representative examples of the atomic ratio of the target metal elements are In:M:Zn=1:3:2, In :M:Zn=1:3:4, In:M:Zn=1:3:6, In:M:Zn=1:3:8, In:M:Zn=1:4:4, In:M:Zn=1:4:5, In:M:Zn=1:4: 6, In:M:Zn=1:4:7, In:M:Zn=1:4:8, In:M:Zn=1: 5:5, In:M:Zn=1:5:6, In:M:Zn=1:5:7, In:M:Zn= 1:5:8, In:M:Zn=1:6:8, etc.

[0188] The atomic ratio of the metal elements in the target of the oxide semiconductor film 32 is In:M:Zn=x2:y2: If we set it to z2, 、 It is preferable that x2 / y2 is greater than 1 and equal to or less than 6. It is preferable that y2 is greater than 1 and less than 6. Examples of the table are In:M:Zn=2:1:1.5, In:M:Zn=2:1:2.3, I n:M:Zn=2:1:3, In:M:Zn=3:1:2, In:M:Zn=3:1:3 , In:M:Zn=3:1:4, etc.

[0189] The atomic ratio of the metal elements in the target of the oxide semiconductor film 33 is In:M:Zn=x3:y3: If we say z3, 、 It is preferable that x3 / y3 is 1 / 6 or more and 1 or less. The number 3 is preferably 1 / 3 or more and 6 or less, and more preferably 1 or more and 6 or less. Representative examples of atomic ratios of group elements are In:M:Zn=1:1:1 and In:M:Zn=1 :1:1.2, In:M:Zn=1:3:2, In:M:Zn=1:3:4, In:M: Zn=1:3:6, In:M:Zn=1:3:8, In:M:Zn=1:4:4, In: M:Zn=1:4:5, In:M:Zn=1:4:6, In:M:Zn=1:4:7, I n:M:Zn=1:4:8, In:M:Zn=1:5:5, In:M:Zn=1:5:6 , In:M:Zn=1:5:7, In:M:Zn=1:5:8, In:M:Zn=1:6 :8 etc.

[0190] In the deposition target for the In-M-Zn oxide film, the atomic ratio of metal elements is In:M: When Zn=x:y:z, by setting 1≦z / y≦6, the In-M-Zn oxide film can be obtained. This is preferable because it is easy to form a CAAC-OS film. More details will be given later.

[0191] As the oxide semiconductor films 31 to 33, oxide semiconductor films with low carrier density are used. For example, the oxide semiconductor films 31 to 33 each have a carrier density of 1×10 17 pieces / cm 3 below , preferably 1 x 10 15 pieces / cm 3 Less than 1×10, more preferably 13 pieces / cm 3 Below In particular, the oxide semiconductor films 31 to 33 are formed using the oxide semiconductor films having a carrier density But 8×10 11 pieces / cm 3 less than 1×10 11 pieces / cm 3 Less than, more Preferably 1 x 10 10 pieces / cm 3 Less than or equal to 1×10 -9 pieces / cm 3 More than 100% acid It is preferable to use a nitride semiconductor film.

[0192] The oxide semiconductor films 31 to 33 are formed of oxide semiconductors having a low impurity concentration and a low density of defect states. By using a thin film, it is possible to fabricate transistors with even better electrical characteristics. Here, the low impurity concentration and low defect level density (low oxygen vacancies) are the main factors. It is called pure or substantially high purity. Pure or substantially high purity Since oxide semiconductors have few carrier generation sources, the carrier density can be reduced in some cases. Therefore, a transistor in which a channel region is formed in the oxide semiconductor film may have a problem. The threshold voltage rarely becomes negative (also called normally on). In addition, a highly-purified intrinsic or substantially highly-purified intrinsic oxide semiconductor film has a low density of defect states. Since the concentration is low, the trap density may also be low. The intrinsic oxide semiconductor film has a significantly small off-state current and a channel width of 1×10 6 μ Even if the device has a channel length of 10 μm and a The off-state current is measured at a voltage between 1V and 10V. below the measurement limit, i.e. 1×10 -13 A characteristic of less than A can be obtained. In the transistor in which the channel region is formed in the oxide semiconductor film, the electrical characteristics are less likely to change. This results in a small and highly reliable transistor. Impurities include hydrogen, nitrogen, and alkali metals. , or alkaline earth metals, etc.

[0193] Hydrogen contained in the oxide semiconductor film reacts with oxygen that is bonded to metal atoms to form water and an acid. Oxygen vacancies are formed in the lattice from which the atoms are desorbed (or in the part from which oxygen is desorbed). When hydrogen enters the electron carrier, it can generate electrons. When it bonds with oxygen, which bonds with a metal atom, it may generate electrons, which act as carriers. Therefore, a transistor using an oxide semiconductor containing hydrogen has normally-on characteristics. Easy to use.

[0194] For this reason, in the oxide semiconductor films 31 to 33, oxygen vacancies and hydrogen are reduced as much as possible. Specifically, in the oxide semiconductor films 31 to 33, it is preferable that the secondary ion species Secondary Ion Mass Spectrometer (SIMS) The hydrogen concentration obtained by y) is 5×10 19 atoms / cm 3 More preferably, 1×10 19 atoms / cm 3 Less than or equal to 5×10 18 atoms / cm 3 less than 1×10 18 atoms / cm 3 Less than or equal to 5×10 1 7 atoms / cm 3 Less than 1×10, more preferably 16 atoms / cm 3 The following do.

[0195] When the oxide semiconductor films 31 to 33 contain silicon or carbon, which is one of Group 14 elements, The oxygen vacancies in the film increase, and the film becomes n-type. Silicon and carbon concentrations in 1 to 33 (concentrations obtained by secondary ion mass spectrometry) 2 × 10 18 atoms / cm 3 Less than or equal to 2 x 10 17 atoms / cm 3 The following applies.

[0196] In addition, in the oxide semiconductor films 31 to 33, Al was measured by secondary ion mass spectrometry. The concentration of potassium metal or alkaline earth metal is 1×10 18 atoms / cm 3 The following are the preferred Or 2×10 16 atoms / cm 3 The following are alkali metals and alkaline earth metals: When a metal is bonded to an oxide semiconductor, it may generate carriers, which may cause the off-state current of a transistor to decrease. Therefore, the alkali metal current in the oxide semiconductor films 31 to 33 may increase. Alternatively, it is preferable to reduce the concentration of alkaline earth metals.

[0197] When nitrogen is contained in the oxide semiconductor films 31 to 33, electrons that serve as carriers are generated. The rear density increases and it is easy to make it n-type. Therefore, an oxide semiconductor containing nitrogen is used. Since the transistor tends to have normally-on characteristics, the nitrogen in the oxide semiconductor films 31 to 33 is It is preferable that the content is as low as possible. For example, it is preferable that the content is as low as possible by secondary ion mass spectrometry. The resulting nitrogen concentration is 5 x 10 18 atoms / cm 3 It is preferable to do the following:

[0198] Although the oxide semiconductor films 31 to 33 have been described above, the present invention is not limited to these. Depending on the semiconductor characteristics and electrical characteristics of the transistor (field effect mobility, threshold voltage, etc.) An oxide semiconductor film having an appropriate composition may be used. In order to obtain desired properties and electrical characteristics, the carrier density and impurity concentration of the oxide semiconductor films 31 to 33 are By appropriately adjusting the concentration, defect density, atomic ratio of metal elements to oxygen, interatomic distance, density, etc. is preferred.

[0199] The transistor TA1 is a Ga or M (M is Al, Ga, Y, Zr, La, Ce, or A channel is formed in the oxide semiconductor film 32 in which the atomic ratio of In is larger than the atomic ratio of Nd. This allows the field effect mobility to be increased. Typically, the field effect mobility is , 10cm 2 / Vs > 60cm 2 / Vs, preferably less than 15cm 2 / Vs or more 50cm 2 / Vs. Therefore, there is no possibility of causing a disturbance in the circuit of the active matrix display device. When the transistor TA1 is used, it is suitable for a drive circuit that requires high speed operation.

[0200] It is also preferable to provide the transistor TA1 in a light-shielded area. By providing a transistor TA1 having a high mobility in the drive circuit, the drive frequency can be increased. Therefore, a display device with higher resolution can be realized.

[0201] The transistors TA2 and TB1, in which the channel formation region is formed of the oxide semiconductor film 33, It has a lower field effect mobility than the transistor TA1 and its size is 3 cm 2 / Vs or more 10 cm 2 The transistors TA2 and TB1 have an oxide semiconductor film 32. Since it is not exposed to light, it is less susceptible to deterioration by light than the transistor TA1. The increase in current is small. Therefore, the channel formation region is formed in the oxide semiconductor film 33. The transistors TA2 and TB1 are suitable for a pixel portion that is irradiated with light.

[0202] The transistor TA1 has a lower resistance than the transistors TA2 and TB1 that do not have the oxide semiconductor film 32. In comparison, when light is irradiated, the current in the off state tends to increase. This is one of the reasons why it is suitable for peripheral driving circuits, which are less affected by light than the pixel area, which cannot be sufficiently shielded from light. Of course, transistors with configurations like transistors TA2 and TB1 can also be used. It can be provided in the drive circuit.

[0203] The transistors TA1, TA2, and TB1 and the oxide semiconductor films 31 to 33 have been described above. However, the present invention is not limited to these, and may be applied depending on the semiconductor characteristics and electrical characteristics of the required transistor. For example, the presence or absence of a back gate electrode, the oxide semiconductor The laminated structure of the conductor film, the oxide semiconductor film, the gate electrode, the source electrode, and the drain electrode The arrangement, etc., of the components can be changed as appropriate.

[0204] [Structure of oxide semiconductor] Next, the structure of the oxide semiconductor will be described.

[0205] In this specification, "parallel" means that two straight lines are arranged at an angle of -10° or more and 10° or less. Therefore, it includes the case where the angle is between -5° and 5°. "Approximately parallel" refers to a state in which two straight lines are arranged at an angle of -30° or more and 30° or less. Also, "perpendicular" means that two straight lines are arranged at an angle of 80° to 100°. Therefore, it also includes the case where the angle is between 85° and 95°. This refers to a state in which two straight lines are arranged at an angle of 60° or more and 120° or less.

[0206] In addition, in this specification, when the crystal is a trigonal or rhombohedral crystal, it is represented as a hexagonal crystal system. .

[0207] Oxide semiconductor films are classified into non-single-crystal oxide semiconductor films and single-crystal oxide semiconductor films. Alternatively, oxide semiconductors are divided into, for example, crystalline oxide semiconductors and amorphous oxide semiconductors. do.

[0208] As the non-single-crystal oxide semiconductor, CAAC-OS (C Axis Aligned Crystalline Oxide Semiconductor, polycrystalline oxide Semiconductors made of crystalline oxides include semiconductors made of microcrystalline oxides and amorphous oxides. The materials include single-crystal oxide semiconductors, CAAC-OS, polycrystalline oxide semiconductors, and microcrystalline oxides. Semiconductors, etc.

[0209] First, we will explain the CAAC-OS film.

[0210] The CAAC-OS film is one of oxide semiconductor films having a plurality of crystal parts aligned along the c-axis.

[0211] Transmission Electron Microscope (TEM) A bright-field image and a combined diffraction pattern of the CAAC-OS film were obtained by using a microscope. By observing the TEM image, multiple crystalline regions can be confirmed. On the other hand, the high-resolution TEM image also shows clear boundaries between crystals, i.e., grain boundaries. Therefore, the CAAC-OS film is It can be said that the decrease in electron mobility caused by grain boundaries is unlikely to occur.

[0212] When a high-resolution TEM image of the cross section of the CAAC-OS film was observed from a direction approximately parallel to the sample surface, It can be seen that the metal atoms are arranged in layers in the crystal part. Each layer of metal atoms is The CAAC-OS film is formed on the surface (also called the surface on which the film is formed) or on the upper surface. The CAAC-OS film has a shape similar to that of the crystalline silicon film, and is aligned parallel to the surface on which the CAAC-OS film is formed or the upper surface.

[0213] On the other hand, a high-resolution TEM image of the plane of the CAAC-OS film was observed from a direction approximately perpendicular to the sample surface. It was confirmed that the metal atoms in the crystals were arranged in triangular or hexagonal shapes. However, there is no regularity in the arrangement of metal atoms between different crystal parts.

[0214] X-ray diffraction (XRD) was performed on the CAAC-OS film. For example, InGaZnO 4 CAAC-OS film with crystals In the out-of-plane analysis, a peak was observed at a diffraction angle (2θ) of approximately 31°. This peak may appear in InGaZnO 4 It is assigned to the (009) plane of the crystal of From this, it can be seen that the crystals of the CAAC-OS film have a c-axis orientation, and the c-axis is approximately aligned on the surface on which the film is formed or on the upper surface. You can see that it is oriented vertically.

[0215] In addition, InGaZnO 4 Out-of-plane synthesis of CAAC-OS films with crystallites In the analysis by , in addition to the peak at 2θ near 31°, a peak also appeared at 2θ near 36°. The peak at 2θ of around 36° may be due to the c-axis orientation in some parts of the CAAC-OS film. The CAAC-OS film contains crystals that do not have a 2θ of around 31°. It is preferred that the spectrum exhibits a peak and does not exhibit a peak at 2θ of around 36°.

[0216] The CAAC-OS film is an oxide semiconductor film with a low concentration of impurities. The impurities include hydrogen, carbon, and The elements are other than the main components of the oxide semiconductor film, such as silicon and transition metal elements. The elements that bond to oxygen more strongly than the metal elements that form the oxide semiconductor film, such as arsenic, are oxidized. By removing oxygen from the oxide semiconductor film, the atomic arrangement of the oxide semiconductor film is disrupted, reducing its crystallinity. In addition, heavy metals such as iron and nickel, argon, and carbon dioxide have an atomic radius of Since the molecular radius is large, when the cation is contained in the oxide semiconductor film, the The impurities in the oxide semiconductor film may cause the atomic arrangement to be disturbed, which may result in a decrease in crystallinity. Objects can act as carrier traps or carrier generation sources.

[0217] The CAAC-OS film is an oxide semiconductor film having a low density of defect states. Oxygen vacancies in the semiconductor film can become carrier traps or trap hydrogen, It can be a carrier source.

[0218] A material with a low impurity concentration and a low defect level density (few oxygen vacancies) is called a high-purity intrinsic or The term "substantially high-purity intrinsic" refers to a highly-purified intrinsic oxide semiconductor film. Since there are fewer carrier generation sources, the carrier density can be reduced. The transistor including the oxide semiconductor film has electrical characteristics in which the threshold voltage is negative ( Also called normally on.) It is rare for the product to be intrinsically or substantially pure. The intrinsic oxide semiconductor film has few carrier traps. Transistors using the film have little fluctuation in electrical characteristics and are highly reliable. Note that it takes a certain time for charges trapped in the carrier traps in the oxide semiconductor film to be released. The time is long and the charge may behave as if it were a fixed charge. In addition, a transistor using an oxide semiconductor film having a high density of defect states has unstable electrical characteristics. There may be cases where this occurs.

[0219] In addition, the electrical characteristics of transistors using CAAC-OS films were improved by irradiation with visible light or ultraviolet light. The fluctuation is small.

[0220] Next, a microcrystalline oxide semiconductor film will be described.

[0221] The microcrystalline oxide semiconductor film has a region where crystals can be confirmed in a high-resolution TEM image. The microcrystalline oxide semiconductor film has a crystal structure including a region where a crystal part is not clearly observed and a region where a crystal part is not clearly observed. The crystal part contained in the crystal has a size of 1 nm to 100 nm or 1 nm to 10 nm. In particular, the fineness is often between 1 nm and 10 nm, or between 1 nm and 3 nm. The oxide semiconductor film having nanocrystals (nc) is called nc -OS(nanocrystalline oxide semiconductor) In the nc-OS film, for example, the grain boundaries are clearly identified in high-resolution TEM images. It may not be possible to recognize

[0222] The nc-OS film is a microscopic region (e.g., a region of 1 nm to 10 nm, especially a region of 1 nm or more). The atomic arrangement has periodicity in the region of 3 nm or less. There is no regularity in the crystal orientation between the crystal parts. Therefore, no orientation is observed throughout the film. Therefore, the nc-OS film cannot be distinguished from an amorphous oxide semiconductor film depending on the analysis method. For example, X-ray diffraction (XR) is used to measure the nc-OS film using X-rays with a diameter larger than that of the crystals. When structural analysis was performed using the D instrument, the crystal plane In addition, the peaks indicating the probe size were not detected in the nc-OS film. Electron diffraction (also called selected area electron diffraction) using an electron beam with a diameter (for example, 50 nm or more) When the diffraction pattern is changed to 0.05μm, a halo-like diffraction pattern is observed. Nano-beam electrons are used, which use an electron beam with a probe diameter close to or smaller than the size of the crystal part. When diffraction is performed, spots are observed. When this is done, a circular (ring-shaped) area of ​​high brightness may be observed. Nanobeam electron diffraction of the nc-OS film revealed multiple spots within the ring-shaped region. It may be observed.

[0223] The nc-OS film is an oxide semiconductor film that has higher order than an amorphous oxide semiconductor film. Therefore, the nc-OS film has a lower density of defect states than the amorphous oxide semiconductor film. In the nc-OS film, there is no regularity in the crystal orientation between different crystal parts. The S film has a higher density of defect states than the CAAC-OS film.

[0224] Next, the amorphous oxide semiconductor film will be described.

[0225] The amorphous oxide semiconductor film is an oxide semiconductor film in which the atomic arrangement in the film is irregular and does not have a crystal part. An example is an oxide semiconductor film that has an amorphous state, such as quartz.

[0226] In the amorphous oxide semiconductor film, no crystalline parts can be confirmed in a high-resolution TEM image.

[0227] When the structure of the amorphous oxide semiconductor film is analyzed using an XRD device, out-of-p In the lane analysis, no peaks indicating crystal planes were detected. When electron diffraction is performed on a conductive film, a halo pattern is observed. When nanobeam electron diffraction is performed on a conductive film, no spots are observed, and a halo pattern is observed. Observed.

[0228] Note that the oxide semiconductor film has a structure that exhibits physical properties between the nc-OS film and the amorphous oxide semiconductor film. An oxide semiconductor film having such a structure may have a structure such as the following. Amorphous-like Oxide Semiconductor (a-like OS) The conductor membrane is called the endothelium.

[0229] In the a-like OS film, voids are observed in the high-resolution TEM image. In addition, crystals may be clearly visible in high-resolution TEM images. The a-like OS film has a region in which a crystal part is not observed and a region in which a crystal part is not observed. Crystallization occurs due to the small amount of electron irradiation, which is the level observed in TEM observations, and the growth of the crystals can be seen. On the other hand, if the nc-OS film is of good quality, the small amount of charge observed by TEM can be observed. Almost no crystallization due to electron irradiation was observed.

[0230] The size of the crystals in the a-like OS film and the nc-OS film was measured using a high-resolution T This can be done using EM images. For example, InGaZnO 4 The crystals have a layered structure, There are two Ga-Zn-O layers between the In-O layers. 4 Crystal unit cell of The layer has three In-O layers and six Ga-Zn-O layers, for a total of nine layers aligned in the c-axis direction. The spacing between adjacent layers is therefore the (009) plane. This is approximately the same as the lattice spacing (also called the d value), and crystal structure analysis has determined that this value is 0.29 nm Therefore, we focused on the lattice fringes in high-resolution TEM images and In the region where the distance is between 0.28 nm and 0.30 nm, the lattice fringes are InG aZnO 4 This corresponds to the ab plane of the crystal.

[0231] In addition, the density of an oxide semiconductor film may differ depending on the structure. If the composition of the membrane is known, the density can be determined by comparing it with that of a single crystal of the same composition. The structure of the oxide semiconductor film can be estimated. The density of the OS-like film is 78.6% or more and less than 92.3%. The density of the nc-OS film and the CAAC-OS film was 92.3% or more. Note that an oxide semiconductor film having a density of less than 78% of the density of a single crystal is The film formation itself is difficult.

[0232] The above will be explained using a specific example. For example, In:Ga:Zn=1:1:1 [atomic In the oxide semiconductor film that satisfies the [number ratio], single crystal InGaZnO having a rhombohedral crystal structure 4 The density of is 6.357g / cm 3 Therefore, for example, In:Ga:Zn=1:1:1 In the oxide semiconductor film that satisfies the atomic ratio, the density of the a-like OS film is 5.0 g / cm 3 More than 5.9g / cm 3 For example, In:Ga:Zn=1:1: In the oxide semiconductor film that satisfies the atomic ratio of 1, the density of the nc-OS film and the CAAC- The density of the OS film is 5.9 g / cm 3 More than 6.3g / cm 3 It will be less than.

[0233] In addition, there are cases where single crystals with the same composition do not exist. In such cases, the composition may differ in any ratio. By combining single crystals, it is possible to calculate the density equivalent to a single crystal of the desired composition. The density of a single crystal of a desired composition can be determined by the ratio of the single crystals of different compositions. However, the density should be calculated using as few types of single crystals as possible. It is preferable to perform the calculation in combination.

[0234] Note that the oxide semiconductor film may be, for example, an amorphous oxide semiconductor film, an a-like OS film, or a microcrystalline oxide semiconductor film. The semiconductor layer may be a stacked film including two or more of a crystalline oxide semiconductor film and a CAAC-OS film.

[0235] As described above, the OS transistor can achieve extremely excellent off-state current characteristics.

[0236] [Substrate 30] The substrate 30 may be any of a variety of substrates and is not limited to any particular one. Examples of the substrate 30 include a semiconductor substrate (e.g., a single crystal substrate or a silicon substrate), a SO I substrate, glass substrate, quartz substrate, plastic substrate, metal substrate, stainless steel substrate , Substrate with Stainless Steel Foil, Tungsten Substrate, Tungsten Foil A substrate having a fibrous material, a flexible substrate, a laminated film, a paper containing a fibrous material, or a base film Examples of glass substrates include barium borosilicate glass and aluminophore. silicate glass, or soda lime glass. Flexible substrates, lamination films Examples of the materials and base films are as follows: Polyethylene terephthalate (PET), polyethylene naphthalate (PEN), polyethersulf For example, there are plastics such as polyether ether sulphate (PES). Synthetic resins, etc. Examples include polypropylene, polyester, and polyfluorine. Examples of such materials include polyvinyl chloride, polyvinyl chloride, and polyamide. Imide, aramid, epoxy, inorganic deposition film, paper, etc. In particular, semiconductor By manufacturing transistors using substrates, single crystal substrates, or SOI substrates, etc. , small variation in characteristics, size, or shape, high current capability, small size It is possible to manufacture transistors. Circuits are constructed using such transistors. As a result, it is possible to reduce the power consumption of the circuit or to increase the degree of integration of the circuit.

[0237] Before forming the gate electrodes GE1 to GE3, a base insulating film may be formed on the substrate 30. The base insulating film may be silicon oxide, silicon oxynitride, silicon nitride, or silicon nitride oxide. Con, gallium oxide, hafnium oxide, yttrium oxide, aluminum oxide, oxynitride Aluminum, etc. Silicon nitride, gallium oxide, halide, etc. are used as the base insulating film. By using fluorine, yttrium oxide, aluminum oxide, etc., impurities can be removed from the substrate 30. The diffusion of oxygen (typically, alkali metal, water, hydrogen, or the like) into the oxide semiconductor films OS1 to OS3 It can be suppressed.

[0238] [Gate electrodes GE1, GE2, GE3] The gate electrodes GE1 to GE3 are each formed of a single layer conductive film or a multilayer structure in which two or more conductive films are laminated. The conductive film formed as the gate electrodes GE1 to GE3 is made of aluminum. A metal element selected from the group consisting of aluminum, chromium, copper, tantalum, titanium, molybdenum, and tungsten; Or an alloy containing the above-mentioned metal elements or an alloy combining the above-mentioned metal elements. It can be formed by using one or more of manganese and zirconium. Alternatively, a metal element selected from the group consisting of aluminum, titanium, tantalum, and tantalum may be used. A combination of one or more selected from the group consisting of tin, molybdenum, chromium, neodymium, and scandium. Alternatively, an alloy film made of indium tin oxide or a nitride film may be used. Indium oxide containing tungsten, indium zinc oxide containing tungsten oxide, Indium oxide containing titanium oxide, indium tin oxide containing titanium oxide, indium zinc Uses conductive materials with translucency such as lead oxide and indium tin oxide containing silicon oxide It is also possible.

[0239] For example, an aluminum film containing silicon is formed as the gate electrodes GE1 to GE3. When the gate electrodes GE1 to GE3 have a two-layer structure, for example, aluminum forming a titanium film on a titanium nitride film; forming a titanium film on a titanium nitride film; forming a tungsten film on a tantalum nitride film or a tungsten nitride film; In addition, when the gate electrodes GE1 to GE3 have a three-layer structure, for example, For example, a titanium film is laminated on top of an aluminum film, and a titanium film is further laminated on top of that. It is sufficient to form the following.

[0240] By sputtering, vacuum deposition, pulsed laser deposition (PLD), thermal CVD, etc. The gate electrodes GE1 to GE3 are formed.

[0241] The tungsten film can be formed using a film forming apparatus that uses ALD. In this case, WF 6 Gas and B 2 H 6 The gas is introduced repeatedly in sequence to form the initial tungsten film. , then W.F. 6 Gas and H 2 A tungsten film is formed using gas. 2 H 6 G Instead of silicon 4 A gas may also be used.

[0242] The gate electrodes GE1 to GE3 can be formed by the above-mentioned method, as well as by electrolytic plating, printing, inkjet printing, etc. This can be done by the ink jet method or the like.

[0243] [Insulating film 34 (gate insulating film)] An insulating film 34 is formed to cover the gate electrodes GE1 to GE3. The insulating film 34 is a single-layer insulating film. The insulating film formed as the insulating film 34 is an insulating film having a multi-layer structure of two or more layers. , an oxide insulating film, a nitride insulating film, an oxynitride insulating film, a nitride oxide insulating film, and the like. In this specification, an oxynitride is a material that contains more oxygen than nitrogen. Nitrided oxide is a material that contains more nitrogen than oxygen.

[0244] The insulating film formed as the insulating film 34 may be, for example, silicon oxide or silicon oxynitride. , silicon oxide nitride, silicon nitride, aluminum oxide, hafnium oxide, gallium oxide Alternatively, an insulating film made of Ga-Zn-based metal oxide or the like can be formed. Hafnium silicate (HfSiO x ), nitrogen-added Hafniu HfSi x O y N z ), nitrogen-doped hafnium aluminate (Hf Al x O y N z ), hafnium oxide, yttrium oxide, and other high-k materials By using high-k materials, the gate leakage of transistors can be reduced. can be reduced.

[0245] The insulating film 34 functions as a gate insulating film. In order to improve the interface characteristics with the gate insulating film, the oxide semiconductor film OS1 is The region in contact with OS3 is preferably formed of an oxide insulating film or an oxynitride insulating film. For example, the top layer of the insulating film 34 is a silicon oxide film or a silicon oxynitride film. That's good.

[0246] The thickness of the insulating film 34 may be, for example, 5 nm to 400 nm. Alternatively, it is 10 nm or more and 300 nm or less, and more preferably, it is 50 nm or more and 250 nm or less. It is.

[0247] When the oxide semiconductor films OS1 to OS3 are formed by a sputtering method, plasma is generated. The power supply for the operation of the device should be an RF power supply, an AC power supply, a DC power supply, etc. can be done.

[0248] The sputtering gas is a rare gas (typically argon), oxygen, or a mixture of a rare gas and oxygen. In the case of a mixture of rare gas and oxygen, the ratio of oxygen to rare gas is It is preferable to increase the ratio.

[0249] The target is appropriately selected depending on the composition of the oxide semiconductor films OS1 to OS3 to be formed. Just choose.

[0250] Note that in the case where a sputtering method is used to form the oxide semiconductor films OS1 to OS3, The temperature is 150° C. or higher and 750° C. or lower, preferably 150° C. or higher and 450° C. or lower, and more preferably The oxide semiconductor films 31 to 33 can be formed by the CAA A C-OS film can be formed.

[0251] In addition, the following conditions are preferably applied to form the CAAC-OS film.

[0252] By suppressing the inclusion of impurities during film formation, it is possible to prevent the crystal state from being destroyed by impurities. For example, the concentration of impurities (hydrogen, water, carbon dioxide, nitrogen, etc.) present in the film formation chamber is In addition, the impurity concentration in the deposition gas may be reduced. A deposition gas having a temperature of -80°C or lower, preferably -100°C or lower, is used.

[0253] In addition, by increasing the oxygen ratio in the deposition gas and optimizing the power, plasma damage during deposition is reduced. The oxygen ratio in the deposition gas is preferably 30% by volume or more, and 100% by volume or more is preferably 100% by volume or more. Product % is more preferred.

[0254] The oxide semiconductor film is formed while being heated, or after the oxide semiconductor film is formed, By the heat treatment, the hydrogen concentration in the oxide semiconductor film was increased to 2 × 10 20 atoms / cm 3 Below Lower, preferably 5 x 10 19 atoms / cm 3 Less than or equal to 1×10 19 at oms / cm 3 Less than or equal to 5×10 18 atoms / cm 3 Less than, more preferred 1×10 18 atoms / cm 3 Less than or equal to 5×10 17 atoms / c m 3 Less than 1×10, more preferably 16 atoms / cm 3 It can be as follows:

[0255] The heat treatment is carried out at a temperature higher than 350°C and lower than 650°C, preferably at a temperature higher than 450°C and lower than 600°C. By carrying out the above steps, the CAAC conversion rate described below is 70% or more but less than 100%, preferably 80%. More preferably, the ratio is 90% or more and less than 100%, more preferably 95% or more and less than 98%. % or less. In addition, the content of hydrogen, water, and the like is reduced. That is, it is possible to obtain an oxide semiconductor film having a low impurity concentration and a low defect state density. In this way, an oxide semiconductor film with low thermal conductivity can be formed.

[0256] An oxide semiconductor film can be formed using a deposition system that uses ALD. For example, InG aZnO X When forming a (X>0) film, In(CH 3 ) 3 Gas and O 3 Gas is sequentially Repeatedly introducing InO 2 layer, and then Ga(CH 3 ) 3 Gas and O 3 Using gas A GaO layer is then formed, followed by Zn(CH 3 ) 2 Gas and O 3 Forming ZnO layer using gas The order of these layers is not limited to this example. aO 2 Layer and InZnO 2 Layers, GaInO layers, ZnInO layers, GaZnO layers, etc. A material layer may be formed. 3 H bubbled with inert gas such as Ar instead of gas 2 O gas may be used, but it should be O gas that does not contain H. 3 It is preferable to use gas. CH 3 ) 3 Instead of gas, In(C 2 H 5 ) 3 Gas may also be used. 3 ) 3 Instead of gas, Ga(C 2 H 5 ) 3 Gas may also be used. Zn(CH 3 ) 2 G A suction cup may also be used.

[0257] The oxide semiconductor film 32 and the oxide semiconductor film 33 are used as a gate insulating film. The thickness of the film can be 3 nm or more and 200 nm or less. , preferably 3 nm to 100 nm, and more preferably 30 nm to 50 nm. The thickness of the oxide semiconductor film 31 is, for example, 3 nm to 100 nm. It is preferably 3 nm or more and 30 nm or less, and more preferably 3 nm or more and 15 nm or less. The oxide semiconductor film 31 is thinner than the oxide semiconductor film 32 and the oxide semiconductor film 33. It is preferable to form the

[0258] Here, as the oxide semiconductor films 31 to 33, In-Ga-Zn films are formed by sputtering. The atomic ratio of the metal elements in the targets used for these films (In:Ga: For example, the oxide semiconductor film 31 has a ratio of 1:3:6, and the oxide semiconductor film 32 has a ratio of 3: The oxide semiconductor film 33 can have a thickness of 1:1:1.2 or 1:1:1. The oxide semiconductor films 31, 32, and 33 have thicknesses of 5 nm, 35 nm, and It can be 35 nm.

[0259] [Source electrode, drain electrode] The source and drain electrodes (SE1, DE1, SE2, DE2, SE3, DE3) are The gate electrodes GE1 to GE3 can be formed in the same manner.

[0260] For example, a copper-manganese alloy film having a thickness of 50 nm, a copper film having a thickness of 400 nm, and a copper film having a thickness of 100 nm thick copper-manganese alloy film was laminated by sputtering. In this way, a source electrode and a drain electrode having a three-layer structure can be formed.

[0261] [Insulating film 35, 36] The insulating film 35 may have a two-layer structure. The first film layer is called insulating film 35a, and the second film layer is called insulating film 35b.

[0262] The insulating film 35a may be, for example, an oxide insulating film made of silicon oxide or the like, or a film containing nitrogen. It is possible to form an oxide insulating film containing nitrogen and having few defects. Typical examples of oxide insulating films with low oxidation resistance include a silicon oxynitride film and an aluminum oxynitride film. etc.

[0263] The oxide insulating film with few defects shows a high ESR spectrum below 100K. The first signal has a g value between 2.037 and 2.039, and the second signal has a g value between 2.001 and 2. A second signal with a g value of 0.003 or less, and a third signal with a g value of 1.964 to 1.966 or less. A null is observed. Note that the split width of the first signal and the second signal, The split width of the second and third signals is The g value is about 5 mT. The first signal has a g value of 2.037 to 2.039. A second signal between 2.001 and 2.003, and a g value between 1.964 and 1.96 The sum of the spin densities of the third signals that are 6 or less is 1 × 10 18 spins / cm 3 Not yet is typically 1×10 17 spins / cm 3 More than 1×10 18 spins / c m 3 is less than.

[0264] In addition, in the ESR spectrum below 100K, the g value is 2.037 to 2.039. The first signal, the second signal with a g value between 2.001 and 2.003, and the g value between 1 The third signal, between .964 and 1.966, is nitrogen oxides (NOx, where x is greater than 0). Representative examples of nitrogen oxides are: Examples include nitrogen monoxide and nitrogen dioxide. That is, the g value is between 2.037 and 2.039. the first signal with a g-value between 2.001 and 2.003, and the second signal with a g-value between 2.001 and 2.003. The smaller the sum of the spin densities of the third signals, which are between 1.964 and 1.966, the Therefore, it can be said that the content of nitrogen oxide in the oxide insulating film is small.

[0265] Since the insulating film 35a is a film containing a small amount of nitrogen oxides, the insulating film 35a and the oxide semiconductor It is possible to reduce carrier traps at the interfaces with the conductive films OS1 to OS3. As a result, it is possible to reduce the shift in the threshold voltage of the transistor. The fluctuation in the electrical characteristics of the transistor can be reduced.

[0266] In order to improve the reliability of the transistor, the insulating film 35a is formed by SIMS (Secondary The nitrogen concentration measured by y Ion Mass Spectrometry is 6×10 2 0 / cm 3 This is because the insulating film 35 is This is because nitrogen oxides are less likely to be produced in a.

[0267] As an example of the insulating film 35a, an oxide insulating film containing nitrogen and having a small amount of defects is CV A silicon oxynitride film can be formed by the method D. In this case, the source gas is It is preferable to use a silicon-containing deposition gas and an oxidizing gas. Representative examples of reactive gases include silane, disilane, trisilane, and fluorinated silane. Chemical gases include nitrous oxide, nitrogen dioxide, and the like.

[0268] In addition, the flow rate of the oxidizing gas is preferably more than 20 times and less than 100 times the flow rate of the deposition gas. The pressure in the treatment chamber is preferably less than 100 Pa, more preferably less than 50 By using a CVD method at a temperature of 0.1 Pa or less, the insulating film 35a contains nitrogen and has a low defect amount. In this way, an oxide insulating film with little damage can be formed.

[0269] For example, the insulating film 35b may be formed by using a material containing more oxygen than the oxygen that satisfies the stoichiometric composition (excess oxygen). The oxide insulating film containing excess oxygen can be used as the insulating film. The oxide insulating film containing the excess oxygen is desorbed by heating. The amount of oxygen released is 1.0×10 18 atoms / cm 3 That's all, Preferably 3.0 x 10 20 atoms / cm 3 That's all. In addition, during the above TDS analysis, The surface temperature of the film is 100°C to 700°C or 100°C to 500°C. The lower range is preferred.

[0270] The insulating film 35b has a thickness of 30 nm to 500 nm, preferably 50 nm to 400 nm. The insulating film 35 may be made of silicon oxide, silicon oxynitride, or the like having a thickness of 00 nm or less. When a silicon oxynitride film containing excess oxygen is used as b, it is preferable to form it by using a CVD method. This can be done.

[0271] When a silicon oxide film or a silicon oxynitride film is formed as the insulating film 35b, the following is performed. The deposition can be performed under the following conditions. The substrate is heated to a temperature of 180° C. or higher and 280° C. or lower, more preferably 200° C. or higher and 240° C. or lower. The pressure in the processing chamber is maintained at 100 Pa or more and 250 Pa or less by introducing the raw material gas into the processing chamber. a or less, more preferably 100 Pa or more and 200 Pa or less, and 0.17W / cm at pole 2 More than 0.5W / cm 2 Less than or equal to 0.25 W / cm 2 More than 0.35W / cm 2 The following high frequency power is supplied:

[0272] The insulating film 36 is made of a film having at least a blocking effect against hydrogen and oxygen. Furthermore, it is preferable to use a blocker such as oxygen, hydrogen, water, an alkali metal, or an alkaline earth metal. Typically, a nitride insulating film such as silicon nitride may be formed. In addition to silicon nitride films, silicon oxynitride films, aluminum nitride films, and aluminum oxynitride films are also available. Membranes and the like can also be used.

[0273] In addition, the insulating film 36 is made of a material having a blocking effect against oxygen, hydrogen, water, etc. Such an oxide insulating film may be formed using an aluminum oxide or Aluminum oxynitride, gallium oxide, gallium oxynitride, yttrium oxide, oxynitride Examples include yttrium, hafnium oxide, and hafnium oxynitride.

[0274] The thickness of the insulating film 36 may be set to 50 nm or more and 300 nm or less, and preferably 100 The insulating film has a blocking effect against oxygen, hydrogen, water, etc. The insulating film 36 is formed to prevent oxygen from diffusing from the oxide semiconductor films 31 to 33 to the outside. In addition, entry of hydrogen, water, and the like from the outside into the oxide semiconductor films 31 to 33 can be prevented.

[0275] When a silicon nitride film is formed as the insulating film 36 by the plasma CVD method, the silicon-containing It is preferable to use deposition gases such as nitrogen and ammonia as source gases. By using this source gas, ammonia dissociates in the plasma and active species are generated. The active species is a bond between silicon and hydrogen contained in the silicon-containing deposition gas, and nitrogen. This breaks the triple bond between silicon and nitrogen, promoting the bonding of silicon and nitrogen. Therefore, a dense silicon nitride film having few hydrogen bonds and few defects can be formed. On the other hand, if the amount of ammonia relative to nitrogen in the source gas is high, the deposition properties including silicon are deteriorated. The decomposition of gas and nitrogen does not proceed, and silicon and hydrogen bonds remain, resulting in defects. The silicon nitride film formed is rough and has large defects. In the above, the flow rate ratio of nitrogen to ammonia is set to 5 or more and 50 or less, preferably 10 or more and 50 or less. It is preferable to set it to lower.

[0276] After the insulating film 35 is formed, heat treatment may be performed. The temperature of the heat treatment is typically 150°C or higher and lower than the substrate distortion point, preferably 200°C or higher and 450°C or lower, more preferably 3 The temperature is set to 00° C. or higher and 450° C. or lower. By this heat treatment, the oxide constituting the second layer of the insulating film 35 is The oxygen contained in the oxide semiconductor insulating film is transferred to the oxide semiconductor films 31 to 33. The heat treatment can reduce oxygen vacancies that occur in the alloy. The heating temperature is 350°C in a gas atmosphere for one hour.

[0277] After the insulating film 36 is formed, hydrogen and the like are released from the oxide semiconductor films 31 to 33. For this purpose, a heat treatment may be carried out. The heating temperature is 350° C. and the heating time is 1 hour in a mixed gas atmosphere containing the metal.

[0278] [Backgate electrode] The back gate electrodes BGE1 and BGE2 are formed in the same manner as the gate electrodes GE1 to GE3. This can be done.

[0279] Below, some other examples of transistor configurations are shown.

[0280] (Transistors TA3 and TA4) 29(A) and (B) are top views of the transistor TA3 and the transistor TA4, respectively. (Layout diagram) and its circuit symbol are shown in Fig. 30(A) and (B). 3, and a sectional view taken along lines a7-a8 and b7-b8 of transistor TA4. Cross-sectional views taken along lines a10 and b9-b10 are shown.

[0281] The transistor TA3 includes a gate electrode GE4, an oxide semiconductor film OS4, a source electrode SE4, The transistor TA3 has a drain electrode DE4 and a back gate electrode BGE4. , a variant of the transistor TA1, in which the back gate electrode BGE4 has two openings CG4 , CG5 is different from the transistor TA1 in that it is in contact with the gate electrode GE4. As shown in FIG. 30B, the oxide The oxide semiconductor film OS4 is surrounded by a gate electrode GE4 and a back gate electrode BGE4. The strength of the transistor TA3 can be further improved.

[0282] The transistor TA4 includes a gate electrode GE5, an oxide semiconductor film OS5, a source electrode SE5, The transistor TA4 has a drain electrode DE5 and a back gate electrode BGE5. This is a modified example of the transistor TA2, in which the back gate electrode BGE5 is connected to the gate electrode GE5. Without connecting, different signals or potentials can be input to the back gate electrode BGE5 and gate electrode GE5. For example, a signal that controls the conductive state of the transistor TA4 is applied to the gate electrode GE5. is input to the back gate electrode BGE5 to correct the threshold voltage of the transistor TA4. Such signals and potentials can be input.

[0283] (Transistors TC1, TB2, TD1) 31A to 31C show transistors TC1, TB2, and FIG. 32(A) shows a top view (layout diagram) of the transistor TD1 and its circuit symbol. ,(B) shows cross sections of the transistor TC1 taken along lines a11-a12 and b11-b12. FIG. 1 is a cross-sectional view of the transistor TB2 taken along lines a13-a14 and b13-b14, and 1 shows a cross-sectional view of the transistor TD1 taken along lines a15-a16 and b15-b16.

[0284] The transistor TC1 includes a gate electrode GE6, an oxide semiconductor film OS6, a source electrode SE6, The drain electrode DE6 and the back gate electrode BGE6 are provided. The gate electrode E6 is in contact with the gate electrode GE6 at an opening CG6. This is a modified example of the transistor TA1, in which the oxide semiconductor film OS6 has a two-layer structure. The conductive film OS6 is composed of an oxide semiconductor film 32 and an oxide semiconductor film 33. Similarly to the transistor TA1, the channel formation region of the transistor TA1 is formed of an oxide semiconductor film 32. Therefore, the transistor TC1 is also as sensitive as the transistor TA1. A high field effect mobility transistor, typically with a field effect mobility of 10 cm 2 / V Larger than s, 60cm 2 / Vs, preferably less than 15cm 2 / Vs or more 50cm 2 / Vs Therefore, the transistor TC1 is also a transistor with a capacitance of 1.5 V. This is suitable for transistors that operate at high speed, such as in driving circuits.

[0285] The transistor TB2 includes a gate electrode GE7, an oxide semiconductor film OS7, a source electrode SE7, The drain electrode DE7 and the back gate electrode BGE7 are provided. The gate electrode E7 is in contact with the gate electrode GE7 at an opening CG7. This is a modification of the transistor TB1, and is similar to the transistor T The transistor TB2 is different from the transistor B1 in that the back gate electrode GE7 is connected to the back gate electrode GE7. Since it has BGE7, it has a higher on-state current than transistor TB1 and is mechanically strong. The degree has been improved.

[0286] The transistor TD1 includes a gate electrode GE8, an oxide semiconductor film OS8, a source electrode SE8, and a drain electrode DE8. The transistor TD1 is a variant of the transistor TB1. In this example, the oxide semiconductor film OS8 is entirely overlapped with the gate electrode GE8. Thus, the transistor TD1 has no part outside the end of E8. Since the semiconductor film OS8 is less exposed to light than the transistor TB1, This is suitable for use in transistors in pixel sections.

[0287] In addition, like transistors TA1, TA2, TA3, TC1, and TB2, In the cross-sectional view of FIG. 1, the channel formation region (active layer region) is electrically insulated from the electric field of the upper and lower gate electrodes. The structure surrounded by the surroundings is called the s-channel (surrounded channel). The s-channel structure allows a large current to flow between the source and drain of a transistor. can flow, and the on-state current of the transistor can be increased.

[0288] In addition, an s-channel transistor having an oxide semiconductor in a channel formation region is The threshold voltage variation for each transistor is small. egative gate bias temperature) stress and PGBT ( Positive Gate Bias Temperature) In addition, the transistor is a DIBL (Drain Induced Barrier r Lowering) is suppressed, and the short channel effect is less likely to be affected. The transistor has a high drain withstand voltage and Id (drain current) - Vd (drain voltage) characteristics In addition, the transistor has good switching characteristics. and has a small subthreshold coefficient in the Id-Vg (gate voltage) characteristics.

[0289] Transistors that operate at high speed, such as those used in the driver circuits of light-emitting devices, The transistors TA1 and TA2, or the transistors TA3, TA4, and TC1 It is preferable to shorten the channel length as shown in FIG. It is preferable that the thickness is less than 2.5 μm. For example, it may be 2.2 μm or less. In the transistor of the embodiment, the channel length is determined by the distance between the source electrode and the drain electrode. Therefore, the minimum value of the channel length is determined by processing the conductive film that will become the source electrode and the drain electrode. In the transistor of this embodiment, for example, the channel length is 0.5 μm. or more, or 1.0 μm or more.

[0290] <Transistor configuration example 2> The transistor used in the display device according to one embodiment of the present invention may be an amorphous, microcrystalline, or polycrystalline or a semiconductor film or substrate of single crystal silicon or germanium, The transistor may have a channel formation region. In this case, the thin film is formed by a vapor phase growth method such as a plasma CVD method or a sputtering method. The amorphous silicon produced is crystallized by processes such as laser annealing. Hydrogen ions were injected into the polycrystalline silicon and single crystal silicon wafers to remove the surface layer. Single crystal silicon or the like can be used.

[0291] 33A and 33B show a thin film that can be used in a display device according to one embodiment of the present invention. 33A and 33B are cross-sectional views of a transistor using a silicon film of n 2, a n-channel transistor 70 and a p-channel transistor 71 are shown.

[0292] The transistor 70 is formed by forming a conductive film serving as a gate electrode on a substrate 72 having an insulating surface. 73, an insulating film 74 on the conductive film 73, and a semiconductor layer overlapping the conductive film 73 with the insulating film 74 interposed therebetween. A conductor film 75, an insulating film 76 on the semiconductor film 75, and a semiconductor film 75 with the insulating film 76 interposed therebetween. A conductive film 77a and a conductive film 77b overlap each other and function as a gate electrode, and a conductive film 77a and an insulating film 78 on the conductive film 77b; an insulating film 79 on the insulating film 78; and electrically connected to the semiconductor film 75 through an opening provided in the insulating film 79; and The conductive film 80 and the conductive film 81 function as a source and a drain.

[0293] The conductive film 77b has a width in the channel length direction shorter than that of the conductive film 77a. The conductive film 77b is laminated in this order from the insulating film 76 side. A channel forming region 82 is disposed at a position where the channel forming region 82 overlaps the conductive film 77b. A pair of LDD (Light Doped Drain) regions 83 and A pair of impurity regions 84 are disposed so as to sandwich an LDD region 83 therebetween. The pair of impurity regions 84 function as a source region or a drain region. The LDD region 83 and the impurity region 84 are impurities that impart n-type conductivity to the semiconductor film 75. The alloy is doped with elements such as boron (B), aluminum (Al), and gallium (Ga). is.

[0294] In addition, the transistor 71 has a gate electrode formed on a substrate 72 having an insulating surface. A conductive film 85, an insulating film 74 on the conductive film 85, and a conductive film 85 overlapping the insulating film 74 therebetween. A semiconductor film 86 is formed on the semiconductor film 86, an insulating film 76 is formed on the semiconductor film 86, and the insulating film 76 is formed on the semiconductor film 86. A conductive film 87a and a conductive film 87b overlapping with the gate electrode 86 and functioning as a gate electrode; An insulating film 78 on the conductive film 87a and the conductive film 87b, and an insulating film 79 on the insulating film 78, The semiconductor film 86 is electrically connected to the insulating film 78 through an opening provided in the insulating film 79. In addition, the conductive film 88 and the conductive film 89 function as a source and a drain.

[0295] The conductive film 87b has a width in the channel length direction that is shorter than that of the conductive film 87a. The conductive film 87b is laminated in this order from the insulating film 76 side. A channel forming region 90 is sandwiched between the conductive film 87b and the channel forming region 90. The pair of impurity regions 91 are arranged so as to face the source region. The impurity region 91 functions as a p-type conductivity region or a drain region. Impurity elements such as phosphorus (P) and arsenic (As) are added to the silicon substrate 6.

[0296] The semiconductor film 75 or the semiconductor film 86 may be crystallized by various techniques. Crystallization methods include laser crystallization using laser light and crystallization using catalytic elements. Alternatively, the crystallization method using a catalytic element and the laser crystallization method can be used in combination. In addition, when a substrate having excellent heat resistance such as quartz is used as the substrate 72, the substrate can be heated in an electric furnace. The thermal crystallization method using a thermal annealing method using infrared light, the lamp annealing crystallization method using a catalytic element, A crystallization method in which a high-temperature annealing at about 950° C. is combined with the crystallization method may be used.

[0297] In FIG. 33A, conductive films 77a and 77b functioning as gate electrodes and a back gate Although the configuration having the conductive film 73 functioning as the electrode is shown, other configurations may be used. For example, as shown in FIG. 33(B), the conductive film 73 functioning as the back gate electrode may be omitted. In FIG. 33A, conductive films 87a and 87b functioning as gate electrodes may be formed. 1 and a conductive film 85 functioning as a back gate electrode. For example, as shown in FIG. 33(B), a conductive layer functioning as a back gate electrode may be used. The conductive film 85 may be omitted. The structure of FIG. 33B is applicable to an OS transistor. be.

[0298] FIG. 34A shows a transistor corresponding to the n-channel transistor 70 shown in FIG. FIG. 34(B) shows a top view of the transistor 70A. FIG. 34C is a cross-sectional view taken along line L1-L2, which shows the length direction of the transistor 70A. 1 is a cross-sectional view taken along line W1-W2, which represents the channel width direction.

[0299] In FIG. 34A, a conductive film 77, a conductive film 73, a semiconductor film 75, a conductive film 80, a conductive film 81, The conductive film 77 is a gate electrode. The conductive film 73 functions as a back gate electrode. In the figure, the details of the components denoted by the same reference numerals are the same as those described in FIG. 33(A). The openings 93 and 94 are formed by the semiconductor film 75, the conductive film 80, and the conductive film 81. The openings 95 and 96 are openings for electrically connecting the conductive film 77 and the conductive film 73. This is an opening for connecting to the

[0300] In FIG. 34B, a conductive film 73, an insulating film 74, and a semiconductor device having a semiconductor device with the insulating film 74 interposed therebetween are provided on a substrate 72. A semiconductor film 75 overlapping with the conductive film 73, an insulating film 76 on the semiconductor film 75, and the insulating film 76 are A conductive film 77a and a conductive film 77b overlap the semiconductor film 75 and function as a gate electrode. and a conductive film 77b; an insulating film 78 on the conductive film 77a and the conductive film 77b; The insulating film 79 and the insulating film 78 are provided with openings 93 and 94, respectively. A conductive film 80 electrically connected to the film 75 and functioning as a source or drain; and a conductive film 81. In the description of FIG. 34(B), the details of the components with the same reference numerals are The details are the same as those explained in FIG. 33(A), so they will be omitted here.

[0301] In FIG. 34B, a conductive film 73, an insulating film 74, and a semiconductor device having a semiconductor device with the insulating film 74 interposed therebetween are provided on a substrate 72. A semiconductor film 75 overlapping with the conductive film 73, an insulating film 76 on the semiconductor film 75, and the insulating film 76 are A conductive film 77a and a conductive film 77b overlap the semiconductor film 75 and function as a gate electrode. and a conductive film 77b; an insulating film 78 on the conductive film 77a and the conductive film 77b; The insulating film 79 and the insulating film 78 are provided with openings 93 and 94, respectively. A conductive film 80 electrically connected to the film 75 and functioning as a source or drain; and a conductive film 81. The semiconductor film 75 has a channel forming region 82 and a pair of LDD regions. The pair of impurity regions 84 are a source region or It functions as a drain region. In the explanation of FIG. 34(B), the same reference numerals are used to denote the same components. Details are the same as those explained in FIG. 33(A), so they will be omitted here.

[0302] In FIG. 34C, a conductive film 73, an insulating film 74, and a channel forming region 82 are formed on a substrate 72. , an insulating film 76, and a conductive film 77 electrically connected to the conductive film 73 in the openings 95 and 96. a and a conductive film 77b, an insulating film 78 on the conductive film 77a and the conductive film 77b, and an insulating film 7 34(C), the same reference numerals are used to denote the same components. The details are the same as those described in FIG. 33(A), and therefore will be omitted here.

[0303] The top view and cross-sectional views shown in FIGS. 34A to 34C are the conductive film 77 and the conductive film 77. The electrically connected conductive film 73 forms a channel in the channel forming region 82 of the semiconductor film 75. The s-channel structure electrically surrounds the width of the transistor. The structure is a structure that encloses the channel formation region from the top, bottom, and sides of the channel formation region. Therefore, the on-current can be increased and the size in the channel width direction can be reduced. In addition, since the channel formation region is surrounded by a conductive film, The channel formation region can be easily shielded from light, preventing unintended light from reaching the channel formation region. It is possible to suppress photoexcitation caused by the photoinduced reaction.

[0304] In the top view and cross-sectional view shown in FIGS. 34A to 34C, the semiconductor film 75 To suppress a conductive state due to an unintended increase in conductivity at the side end in the W1-W2 direction In addition, the influence of the distribution variation of the impurity element added in the semiconductor film 75 can be reduced. It is possible.

[0305] In the top view and cross-sectional view shown in FIGS. 34A to 34C, the gate electrode and the backgate However, a configuration in which they are supplied with different voltages is also effective. This structure is particularly effective for circuits that are composed of only n-channel types. The threshold voltage of the transistor can be controlled by applying a voltage to It is possible to configure logic circuits such as inverter circuits using different ED-MOS transistors. By applying such a logic circuit to a driving circuit for driving pixels, This reduces the area occupied by the operating circuitry, making it possible to realize a narrower frame for the display device. In addition, the back gate voltage can be set to a voltage that turns off the transistor. As a result, the off-state current of the transistor can be reduced when the transistor is turned off. Therefore, even if the display device is refreshed less frequently, the written voltage can still be maintained. Therefore, the power consumption of the display device can be reduced by reducing the number of times writing is performed. It is expected that this will lead to a shift in the

[0306] Note that the top views and cross-sectional views shown in FIGS. 34(A) to 34(C) are merely examples and may be of other configurations. For example, FIGS. 35(A) to (C) show top views different from those in FIGS. and a cross-sectional view.

[0307] The configurations shown in FIGS. 35(A) to 35(C) differ from the configurations shown in FIGS. 34(A) to 34(C) in the following points. The point is that the conductive film 77 which becomes the gate electrode is formed as a single layer. The point is that the position of the channel forming region 82 is closer to the channel forming region 82. This makes it easier to apply an electric field from the top, bottom and side of the hole formation region toward the channel formation region. This configuration also has the same effects as those shown in FIGS. It is possible.

[0308] As another configuration, FIGS. 36(A) to 36(C) show the configurations shown in FIGS. 34(A) to 34(C) and 35( 1A) to 1C) show different top views and cross-sectional views.

[0309] The configuration shown in Figs. 36(A) to (C) is the same as that shown in Figs. 34(A) to (C) and Figs. The difference from the configuration shown in FIG. 1C is that the conductive film 73 serving as the back gate electrode is replaced with a conductive film 73a. The conductive film 73b is surrounded by the conductive film 73a. This configuration can also provide the same effects as those in Figures 34(A) to (C).

[0310] In addition, in the configurations of FIGS. 36(A) to 36(C), the conductive film 73b contains a mobile element (e.g., copper ( Even when Cu) is used, mobile elements penetrate the semiconductor film and cause the semiconductor film to deteriorate. This can prevent this.

[0311] The conductive film 73a on the surface on which the wiring is to be formed and functions as a barrier film is made of a material having a high melting point. The point materials are tungsten (W), molybdenum (Mo), chromium (Cr), and titanium (Ti ), tantalum (Ta), or their alloys (e.g., W-Mo, Mo-Cr, Ta-Mo), or its nitrides (e.g., tungsten nitride, titanium nitride, tungsten The material used for the formation of the insulating layer is a material such as TiNx or TiSiNx. The method for forming the insulating layer is sputtering or CVD. The conductive film 73b is preferably made of copper (Cu), but There are no particular limitations as long as the material is low resistance. For example, silver (Ag), aluminum (Al), gold ( Au) and alloys thereof may also be used. The sputtering method is preferable, but by selecting conditions that do not damage the resist mask, Alternatively, a CVD method may be used.

[0312] The transistors shown in FIGS. 34 to 36 have an s-channel structure. The s-channel transistor, which has silicon in the region, has a high on-current and The threshold voltage variation for each transistor is small. In addition, the transistor has suppressed DIBL. The transistor is less susceptible to short channel effects. It is less susceptible to the effects of MOSFETs and has a high drain withstand voltage. Therefore, it has good saturation characteristics in terms of Id-Vd. The transistor also has good switching characteristics and Id-Vg In terms of gate voltage characteristics, the subthreshold coefficient is small.

[0313] <About the transistor manufacturing process> Next, the above-mentioned transistor, particularly the back gate transistor described in FIGS. 1 shows a cross-sectional view of a transistor having an electrode and a light-emitting element provided on the transistor. An example of a manufacturing process will be described.

[0314] First, as shown in FIG. 37(A), a layer functioning as a back gate electrode is formed on the insulating surface of a substrate 501. The conductive film 502 is selected from Al, W, Mo, Ti, and Ta. The conductive material may be one or more of the above materials. The conductive film 502 was made by laminating tungsten on tantalum nitride. Also, the layer may be configured not as a single layer but as a plurality of layers.

[0315] The substrate 501 is made of, for example, barium borosilicate glass or aluminoborosilicate glass. A glass substrate, a quartz substrate, a ceramic substrate, or the like can be used. Also, a metal substrate or A silicon substrate with an insulating film formed on its surface may also be used. Generally, substrates made of synthetic resins tend to have a lower heat resistance than the above-mentioned substrates. However, it can be used as long as it can withstand the processing temperatures in the manufacturing process.

[0316] Next, an insulating film 503 is provided so as to cover the conductive film 502. The insulating film 503a is, for example, a silicon oxynitride film. The insulating film 503b is, for example, a silicon oxide film or a silicon oxynitride film. The insulating film 503 is not limited to this configuration, and may be formed of a single insulating film or three or more insulating films. The insulating film may be made of any of the above materials.

[0317] The surface of the insulating film 503 (here, the surface of the insulating film 503b) is connected to the conductive film 502 formed earlier. In this case, a process for flattening the unevenness may be provided. In this embodiment, CMP (Chemical-Mechanical Polishing) is used. The surface is flattened using a polishing tool.

[0318] Next, an amorphous semiconductor film 504 is formed on the insulating film 503 by plasma CVD. The semiconductor film 504 is heated at a temperature of 400 to 550° C. for several hours, depending on the amount of hydrogen contained. The hydrogen content is reduced to 5 atomic % or less, and then the crystallization process is carried out. It is also desirable to form an amorphous semiconductor film by other manufacturing methods such as sputtering or deposition. However, it is necessary to sufficiently reduce the impurity elements such as oxygen and nitrogen contained in the film. is desirable.

[0319] The semiconductor used is not limited to silicon, but may be, for example, silicon germanium. When silicon germanium is used, the concentration of germanium is 0.01 to 4.5 at. It is preferable that the concentration is about omic%.

[0320] In addition, when both the insulating film 503 and the amorphous semiconductor film 504 are formed by the plasma CVD method, Alternatively, these two films may be formed in succession without being exposed to the atmosphere. Therefore, surface contamination by the atmosphere is minimized, and the characteristics of the manufactured transistors are minimized. It is possible to reduce the

[0321] Next, a catalyst is added to the amorphous semiconductor film 504. In this embodiment, A nickel acetate solution containing nickel of 100 ppm or less was applied by a spinner. In order to improve the compatibility of the nickel solution, the surface of the amorphous semiconductor film 504 is immersed in an ozone-containing aqueous solution. By treating it with a liquid, an extremely thin oxide film is formed, and the oxide film is then washed with a mixture of hydrofluoric acid and hydrogen peroxide. After etching to form a clean surface, it is treated again with an ozone-containing aqueous solution to form a very thin oxide film. The surface of the semiconductor film is inherently hydrophobic, so forming an oxide film in this way By preparing the nickel acetate solution in advance, it is possible to apply the nickel acetate solution evenly. This is an explanation of (A).

[0322] Of course, the method of adding the catalyst to the amorphous semiconductor film is not limited to the above method, and sputtering, deposition, and plating may be used. It may be added by using plasma treatment or the like.

[0323] Next, heat treatment is performed at 500 to 650° C. for 4 to 24 hours, for example, at 570° C. for 14 hours. By carrying out the heat treatment, the crystallization of the nickel-containing layer 505 progresses, and the crystallinity is improved. A crystalline semiconductor film is formed.

[0324] Heat treatment methods include furnace annealing using an electric furnace, halogen lamps, and Tal halide lamps, xenon arc lamps, carbon arc lamps, high pressure sodium lamps The RTA method using a high-pressure mercury lamp or a heated It is also possible to use a gas heating type RTA that uses an active gas.

[0325] When the RTA method is used, the heating lamp light source is turned on for 1 to 60 seconds, preferably 30 to 6 0 seconds, and repeat this 1 to 10 times, preferably 2 to 6 times. The strength is arbitrary, but the amorphous semiconductor film 504 is instantaneously heated to 600 to 1000° C. Preferably, the temperature is increased to about 650 to 750° C. Even if the semiconductor film is heated, it is only heated momentarily, and the substrate 501 itself is distorted. It will not deform.

[0326] When using the furnace annealing method as another method, the substrate is heated for 500 The amorphous semiconductor film 504 is heated at 50° C. for about 1 hour to release hydrogen contained therein. Then, the mixture is heated in an electric furnace at 550° C. to 600° C., preferably in a nitrogen atmosphere. Heat treatment is performed at 580° C. for four hours to crystallize the amorphous semiconductor film 504 .

[0327] In this embodiment, nickel (Ni) is used as the catalytic element. , Germanium (Ge), Iron (Fe), Palladium (Pd), Tin (Sn), Lead (Pb) Alternatively, elements such as cobalt (Co), platinum (Pt), copper (Cu), and gold (Au) may be used. stomach.

[0328] Next, gettering of the catalytic element present in the crystalline semiconductor film 506 will be described. By crystallization using a catalyst element, a catalyst element (nickel in this example) is introduced into the crystalline semiconductor film 506. The average concentration of 19 / cm 3 It is believed that the amount of If catalytic elements remain, they may adversely affect the characteristics of the transistor. Therefore, it is necessary to provide a process for reducing the concentration of the catalytic element.

[0329] There are various gettering methods. In this embodiment, the crystalline semiconductor film 506 is patterned. An example of gettering performed before the etching will be described. First, as shown in FIG. As shown in FIG. 1, a barrier layer 507 is formed on the surface of the crystalline semiconductor film 506. The barrier layer 507 is Prevents the crystalline semiconductor film 506 from being etched when removing the gettering sites. This is provided for.

[0330] The thickness of the barrier layer 507 is about 1 to 10 nm. It is formed by processing with ozone water. Chemical oxides that are suitable for use as a barrier layer may also be used. It was also found that chemical oxides were formed when the material was treated with an aqueous solution of hydrogen peroxide. Other methods include plasma treatment in an oxidizing atmosphere and plasma treatment in an oxygen-containing atmosphere. A method of generating ozone by irradiating ultraviolet rays to perform oxidation treatment may also be used. A thin oxide film is formed by heating the surface to about 200 to 350°C in a lean oven. Alternatively, a thickness of about 1 to 5 nm may be used by plasma CVD, sputtering, deposition, etc. Alternatively, an oxide film of the same material may be deposited as a barrier layer. The catalyst element can move to the gettering site side, and during the gettering site removal process, A film that is impermeable to etching liquid (protects the crystalline semiconductor film 506 from the etching liquid), e.g. For example, chemical oxide films and silicon oxide films formed by processing with ozone water. (SiOx), or a porous film may be used.

[0331] Next, rare gas is deposited on the barrier layer 507 by sputtering to form gettering sites 508 in the film. 1×10 20 / cm 3 A semiconductor film for gettering containing the above concentration (typically A gettering layer (amorphous silicon film) is formed to a thickness of 25 to 250 nm. The etching site 508 is formed at a high density in order to increase the etching selectivity with respect to the crystalline semiconductor film 506. It is preferable to form a film having a low

[0332] Since the rare gas element itself is inactive in the semiconductor film, it is not necessary to add the rare gas element to the crystalline semiconductor film 506. There is no adverse effect. Also, rare gas elements include helium (He), neon (Ne ), argon (Ar), krypton (Kr), xenon (Xe) or Use multiple types.

[0333] Next, gettering is performed by applying heat treatment (Figure 37(B)). The furnace annealing method is used. In the case of furnace annealing, the nitrogen atmosphere is used. Heat treatment is carried out in air at 450 to 600°C for 0.5 to 12 hours. When using the heating lamp, the heating lamp is turned on for 1 to 60 seconds, preferably 30 to 60 seconds. This is repeated 1 to 10 times, preferably 2 to 6 times. The light emission intensity of the lamp light source is arbitrary. It is optional, but the semiconductor film is instantaneously heated to 600 to 1000° C., preferably 700 to Heat it up to about 750°C.

[0334] By the heat treatment, the catalytic element in the crystalline semiconductor film 506 is released by thermal energy, As shown by the arrows, the gettering site 508 is moved by diffusion. The gettering process depends on the processing temperature, and the higher the temperature, the shorter the gettering time.

[0335] After the gettering process is completed, the gettering sites 508 are selectively etched away. The etching method is ClF 3 Dry etching without plasma using Or hydrazine, tetramethylammonium hydroxide (chemical formula (CH 3 ) 4 This can be done by wet etching using an alkaline solution such as an aqueous solution containing NOH. At this time, the barrier layer 507 functions as an etching stopper. 507 is then removed with hydrofluoric acid (FIG. 37(C)).

[0336] Next, the crystalline semiconductor film 506 after removing the barrier layer 507 is patterned to form an island-shaped semiconductor film. The semiconductor films 509 and 510 are formed (FIG. 37(D)). The thickness is set to 100 nm (preferably 30 to 60 nm). Next, the semiconductor films 509 and 510 are covered. The insulating film 511 is formed as an electrode that will later function as a gate electrode. In the dry etching performed to form the film, the film thickness is reduced by about 10 to 40 nm. Therefore, it is desirable to set the film thickness taking this reduction into consideration. An insulating film 511 is formed to a thickness of about 150 nm (more preferably, 60 to 120 nm). do.

[0337] The insulating film 511 may be made of, for example, silicon oxide, silicon nitride, silicon nitride oxide, or the like. In this embodiment, the insulating film 511 is made of a single insulating layer. The insulating film may be formed by a method such as plasma CVD or sputtering. For example, the insulating film 511 can be formed of silicon oxide by using a plasma CVD method. When forming a membrane, TEOS (Tetraethyl Orthosilicate) and O 2 of Using a mixed gas, the reaction pressure was 40 Pa, the substrate temperature was 300 to 400°C, and high frequency (13. 56MHz) power density 0.5 to 0.8W / cm 2 Then, a film is formed.

[0338] Aluminum nitride can also be used as the insulating film 511. Aluminum nitride is a thermal It has a relatively high conductivity and can efficiently dissipate heat generated by transistors. After forming silicon oxide or silicon oxynitride that does not contain aluminum, aluminum nitride is A laminate of these may be used as the insulating film 511.

[0339] Next, a conductive film is formed on the insulating film 511 (FIG. 37(E)). The conductive film 512a made of tungsten is then formed with a thickness of 20 to 100 nm. The conductive film 512b is formed to a thickness of 100 to 400 nm. The tantalum nitride used is a target with a purity of 99.99%. The temperature in the chamber is Room temperature, Ar flow rate 50 ml / min, N 2 The flow rate of the chamber was set at 10 ml / min. The pressure was 0.6 Pa, the power was 1 kW, and the deposition rate was about 40 nm / min. The tungsten used for the conductive film 512b is 99.99% pure tungsten. The temperature in the chamber was 230°C, the flow rate of Ar was 100 ml / min, The pressure was 1.5 Pa, the deposition power was 6 kW, and the deposition rate was about 390 nm / min.

[0340] In this embodiment mode, an electrode that functions as a gate electrode is formed using a two-layer conductive film. An example will be described, but the conductive film may be a single layer, or may be formed of three or more layers. The materials of the conductive layers are not limited to those described in this embodiment.

[0341] Specifically, each conductive film contains an element selected from Ta, W, Ti, Mo, Al, and Cu, or a precursor. It can be made of an alloy or compound whose main components are the above elements. For example, the first layer is titanium. tantalum nitride with tungsten as the second layer, or tantalum nitride with aluminum as the first layer and aluminum as the second layer. A combination of tantalum nitride for the first layer and copper for the second layer is also possible. An alloy of silver, palladium and copper may be used for either one of the above. Alternatively, a three-layer structure may be used in which an alloy of aluminum and silicon (Al-Si) and titanium nitride are laminated in that order. Instead of tungsten, tungsten nitride may be used, or aluminium and silicon An alloy film of aluminum and titanium (Al-Ti) may be used instead of the alloy (Al-Si). Alternatively, titanium may be used in place of titanium nitride. However, when forming multiple conductive films, If it is desired to make the width of each conductive film in the channel length direction different after etching, Materials that have a mutual etching selectivity are used.

[0342] It is important to select an appropriate etching gas depending on the material of the conductive film.

[0343] Next, a mask 514 is formed, and the conductive film 512a and the conductive film 512 are formed as shown in FIG. b is etched (first etching process). In this embodiment, an ICP (Inductively Coupled Plasma) Inductively Coupled Plasma (ICP) etching method was used. The etching gas was Cl. 2 and CF 4 and O 2 A gas mixture of The pressure of the etching gas in the bar is set to 1.0 Pa. Then, a coil-shaped electrode is connected to the Then, 13.56MHz radio frequency (RF) power is applied to generate plasma. A radio frequency (RF) power of 150 W and 13.56 MHz was applied to the stage (lower electrode) placed on the Then, the etching gas is changed to Cl. 2 and CF 4 The total pressure was changed to 1.0 Pa. The coil-type electrode was also changed to 500 A high-frequency power (13.56 MHz) of 20 W was applied to the substrate side (sample stage). High frequency (13.56MHz) power was supplied.

[0344] CF 4 and Cl 2When the etching gas is used, the conductive film 512a, which is tantalum nitride, The etching rates of the tungsten conductive film 512b are approximately equal. The etching is repeated.

[0345] This first etching process produces a first shape consisting of a lower layer 515a and an upper layer 515b. The first shape conductive film 515 is composed of a lower layer 516a and an upper layer 516b. In this first etching process, the lower layers 515a and 516a are formed. In addition, the side surfaces of the upper layers 515b and 516b are slightly tapered. When the insulating film 5 is etched in this manner, the insulating film 5 that is not covered with the first shape conductive films 515 and 516 is The surface of 11 may be etched on the order of 5-10 nm or more.

[0346] Next, as shown in FIG. 38(B), the surface is etched in a first etching process to reduce the width. Using the reduced mask 514, the conductive films 515 and 516 in the first shape are etched (second The second etching process is the same as the first etching process. The P etching method is used. The etching gas is SF 6 , Cl 2 , O 2 Using a gas mixture of The pressure of the etching gas in the chamber is set to 1.3 Pa. Then, the coil-shaped electrode is A high-frequency power of 700 W and 13.56 MHz is applied to generate plasma. A high-frequency power of 10 W and 13.56 MHz was applied to the stage (lower electrode) placed on the A self-bias voltage is applied to the substrate.

[0347] science fiction 6 and Cl 2 Add O to the mixed gas2 By adding 6, the etching rate of tungsten increases, and the etching rate of tantalum nitride also increases. Since the rate is extremely decreased, a selection ratio can be obtained.

[0348] The second etching process forms a second shape of the conductive film 517 (lower layer 517a, upper layer 517 b) and a second shape conductive film 518 (lower layer 518a, upper layer 518b) are formed. The width of 517b and 518b in the channel length direction is smaller than the width of the lower layers 517a and 518a. The second shape of the conductive films 517 and 51 The surface of the insulating film 511 that is not covered with 8 is etched by about 5 to 10 nm or more. It will be done.

[0349] Next, as shown in FIG. 38(C), the second shape conductive films 517 and 518 are used as a mask. Then, an impurity that imparts n-type conductivity to the semiconductor films 509 and 510 is added (first doping Doping is performed by ion implantation. The dose is 1×10 13 ~5×10 14 atoms / cm 2 The acceleration voltage is set to 40 to 80 kV. The impurity elements that give the valence are group 5 atoms such as P, As, and Sb, which function as donors, and S and Te. In the first doping process, a group 6 atom such as Se is used, but in this embodiment, P is used. As a result, impurity regions 520 and 521 are formed in a self-aligned manner. is 1×10 18 〜1×10 20 atoms / cm 3 Impurities that give n-type conductivity in the concentration range Elements are added.

[0350] Next, a second doping process is performed to obtain the state shown in FIG. The treatment was performed with an acceleration voltage of 50 to 100 kV and a dose of 1×10 15 〜1×10 17 atoms / cm 2 By the first doping process and the second doping process, Impurity regions 522 and 523 overlapping the lower layers 517a and 518a, and impurity regions 524 and 52 The impurity regions 522 and 523 are formed at a concentration of 1×10 18 ~5×10 19 ato ms / cm 3 The impurity element that gives n-type is added in a concentration range of 25 is 1 x 10 19 ~5×10 21 atoms / cm 3 Give n-type in the concentration range An impurity element is added.

[0351] The impurity regions 522 and 523 are formed inside the impurity regions 524 and 525. Regions 522 and 523 are LDD regions, and impurity regions 524 and 525 are source / drain regions. It functions as such.

[0352] Of course, by setting an appropriate acceleration voltage, the first doping process and the second doping process can be performed. The process is completed with a single doping process, forming low-concentration impurity regions and high-concentration impurity regions. It is also possible to do so.

[0353] Through the above steps, impurity regions are formed in each island-shaped semiconductor film.

[0354] Next, island-shaped semiconductor films 509 and 510, an insulating film 511, a second shape conductive film 517, An interlayer insulating film 530 is formed to cover the insulating film 518 (FIG. 39(A)). The interlayer insulating film 530 is An insulating film containing silicon, such as silicon oxide, silicon nitride, or silicon oxynitride, can be used. The thickness is about 100 to 200 nm.

[0355] Next, in order to activate the impurity elements added to the island-shaped semiconductor films 509 and 510, a heat treatment is performed. This process involves the use of a thermal annealing furnace and laser annealing. The thermal annealing method or the rapid thermal annealing method (RTA method) can be used. When activation is performed by the Neal method, the oxygen concentration is 1 ppm or less, preferably 0.1 ppm or less. The heating is carried out in a nitrogen atmosphere at 400 to 700°C (preferably 500 to 600°C). Furthermore, in an atmosphere containing 3 to 100% hydrogen, at 300 to 450° C. for 1 to 12 hours A heat treatment is performed to hydrogenate the island-shaped semiconductor film. The purpose of hydrogenation is to terminate dangling bonds with hydrogen atoms. Alternatively, plasma hydrogenation (using hydrogen excited by plasma) may be performed. The activation process may be performed before the interlayer insulating film 530 is formed.

[0356] Through the above series of steps, the transistor 531 and the transistor 532 are formed. In this embodiment, the transistors 531 and 532 are Although it is treated as an n-channel transistor, transistor 531 or transistor 53 2 may be treated as a p-channel transistor. In that case, the first doping process and in the second doping process, p-type impurities may be doped. The first doping process and the second doping process are performed by a single p-type impurity doping process. The impurity element that gives the p-type conductivity may be B. Impurity region 5 22, 523 is 1 x 10 18 ~5×10 19 atoms / cm 3 In the concentration range of The impurity elements are added to the impurity regions 524 and 525, and the impurity elements are doped at a concentration of 1×10 19 ~5×1 0 21 atoms / cm 3 It is sufficient that an impurity element that imparts p-type conductivity is added in a concentration range of 100 ppm or more.

[0357] In addition, a first doping process is performed between the first etching process and the second etching process. After the first doping step, a second etching step may be performed to remove the upper layer along the channel length. The second doping process is then performed to shorten the impurity region. 522, 523 and impurity regions 524, 525 may be formed.

[0358] The above plasma etching is not limited to the ICP etching method. For example, Electron Cyclotron Resonance Etching method, RIE etching method, Helicon wave etching method, Helical resonance etching Alternatively, plasma etching, pulse modulated etching or other plasma etching techniques may be used.

[0359] In this embodiment, an example in which only the crystallization method using a catalyst element is used has been shown, but the present invention is not limited to this. After crystallization using a catalytic element, pulsed irradiation is performed to further increase the crystallinity. In addition, the above-mentioned gettering process may be performed in this embodiment. The method is not limited to the above-mentioned embodiment. Other methods may be used to reduce the catalytic element in the semiconductor film. It may be possible to do so.

[0360] Next, interlayer insulating films 533 and 534 are formed so as to cover the interlayer insulating film 530. In this embodiment, the interlayer insulating film 533 is made of an organic resin, for example, a non-photosensitive acrylic. The interlayer insulating film 534 is formed to prevent moisture, oxygen, and other factors that accelerate the deterioration of the OLED. A film that is less permeable to substances than other insulating films is used. A typical example is DLC. It is preferable to use a silicon nitride film formed by a film, a carbon nitride film, an RF sputtering method, or the like.

[0361] Next, the insulating film 511, the interlayer insulating film 530, the interlayer insulating film 533, and the interlayer insulating film 534 are etched. Then, the island-shaped semiconductor films 509 and 510 and contacts are formed. Then, wirings 535 to 538 are formed.

[0362] Next, a transparent conductive film is formed to cover the interlayer insulating film 534 and the wirings 535 to 538. By this, the wiring 5 connected to the island-shaped semiconductor film 510 of the transistor 532 A pixel electrode (anode) 540 is formed, which is connected to the substrate 38 (FIG. 39(B)). The transparent conductive film used in this project is not only ITO (indium tin oxide), but also indium oxide. A transparent conductive film containing 20% ​​to 20% zinc oxide (ZnO) may be used. In order to flatten the surface, the CMP method and a polyvinyl alcohol-based porous material are used. After polishing using the CMP method, the surface of the pixel electrode 540 may be polished with a purple polishing agent. External radiation exposure, oxygen plasma treatment, etc. may also be performed.

[0363] Then, an organic resin film 541 to be used as a partition is formed on the interlayer insulating film 534. The oil film 541 has an opening in the area where it overlaps with the pixel electrode 540. Organic resin The film 541 is then heated to remove adsorbed moisture, oxygen, etc. before the electroluminescent layer is formed. Heat in an empty atmosphere. Specifically, heat at 100°C to 200°C for about 0.5 to 1 hour. The heat treatment is carried out in a vacuum atmosphere. -7 Torr or less, if possible. If yes, 3×10 -8 It is most desirable to set the pressure to less than Torr. When forming an electroluminescent layer after subjecting 1 to a heat treatment in a vacuum atmosphere, the vacuum is maintained until immediately before the film formation. By keeping the device under atmospheric conditions, reliability can be further improved.

[0364] The end of the opening of the organic resin film 541 is in contact with an electroluminescent layer to be formed later. It is desirable to make the opening rounded to prevent holes. The radius of curvature of the cross section of the resin film 541 is about 0.2 to 2 μm. is desirable.

[0365] FIG. 39C shows an example in which a positive photosensitive acrylic resin is used as the organic resin film 541. Photosensitive organic resins are exposed to energy rays such as light, electrons, and ions. There are positive types in which the exposed areas are removed, and negative types in which the exposed areas remain. Alternatively, the organic resin film 541 may be formed using photosensitive polyimide. You can do that.

[0366] When the organic resin film 541 is formed using negative acrylic, the edge of the opening is S The cross-sectional shape of the opening is a square. The radius of curvature at the top and bottom of the opening is 0.2 It is preferable that the thickness is in the range of 1 to 2 μm.

[0367] The above-mentioned configuration makes it possible to improve the coverage of the electroluminescent layer and the cathode to be formed later. Prevent the pixel electrode 540 and the cathode from shorting out at the hole formed in the electroluminescent layer. In addition, by relaxing the stress in the electroluminescent layer, shrinkage in the light-emitting area and the like can be prevented. This can reduce the number of defects and improve reliability.

[0368] Next, the light-emitting layer 542 is formed on the pixel electrode 540. The light-emitting layer 542 may include one or more The layer may include not only organic but also inorganic layers.

[0369] Next, a cathode 543 is formed to cover the light-emitting layer 542. The cathode 543 is made of a material having a small work function. Other known conductive materials can be used. For example, Ca, Al, MgAg, AlLi etc. are preferable.

[0370] The pixel electrode 540, the light-emitting layer 542, and the cathode 543 overlap each other in the opening of the organic resin film 541. The overlapping portion corresponds to the light emitting element 544 .

[0371] Next, a protective film 545 is formed on the organic resin film 541 and the cathode 543. The insulating film 45, like the interlayer insulating film 534, is a cause of accelerating the deterioration of the light-emitting element, such as moisture and oxygen. A film that is less permeable to substances such as DL compared to other insulating films is used. It is preferable to use a C film, a carbon nitride film, a silicon nitride film formed by RF sputtering, etc. The above-mentioned membrane is difficult to permeate substances such as moisture and oxygen, and the membrane is more resistant to moisture, oxygen, etc. than the membrane. It is also possible to use the film as a protective film by laminating it with a film that is easily permeable to substances.

[0372] In addition, FIG. 39C shows a configuration in which light emitted from a light emitting element is irradiated to the substrate 501 side. However, the light emitting element may be structured so that light is directed toward the opposite side to the substrate.

[0373] In addition, once the construction is completed up to Figure 39(C), the structure is made more airtight to prevent exposure to the outside air. Protective films with little outgassing (laminate films, UV-curable resin films, etc.) It is preferable to package (enclose) the product in a light-transmitting covering material. When the part is placed in an inert atmosphere or a hygroscopic material (e.g. barium oxide) is placed inside, it emits light. The reliability of a display device having the element is improved.

[0374] By using the above-described manufacturing method, a transistor having a back gate electrode and The light emitting element provided on the transistor can be formed on the same substrate.

[0375] (Embodiment 3) In this embodiment mode, an example of a manufacturing method of a display device will be described with reference to FIGS. In particular, in this embodiment mode, a manufacturing method of a flexible display device will be described.

[0376] <Display device manufacturing method 1> First, an insulating film 420 is formed on a substrate 462, and a first element layer 410 is formed on the insulating film 420. (See FIG. 40A). The first element layer 410 is provided with a semiconductor element. Alternatively, the first element layer 410 may include a display element or a pixel electrode in addition to the semiconductor element. A part of the display element may be provided.

[0377] The substrate 462 must have at least sufficient heat resistance to withstand subsequent heat treatment. For example, a glass substrate, a ceramic substrate, a quartz substrate, a sapphire substrate, etc. may be used as the substrate 4. It may also be used as 62.

[0378] When a glass substrate is used as the substrate 462, a silicon oxide film is formed between the substrate 462 and the insulating film 420. When an insulating film such as a silicon oxide nitride film, a silicon nitride film, or a silicon nitride oxide film is formed, the glass This is preferable because it can prevent contamination from the substrate.

[0379] The insulating film 420 may be made of, for example, epoxy resin, aramid resin, acrylic resin, or polyimide resin. An organic resin film such as a resin, a polyamide resin, or a polyamide-imide resin can be used. In particular, it is preferable to use a polyimide resin because of its high heat resistance. When a polyimide resin is used, the thickness of the polyimide resin is preferably 3 nm or more and 20 μm or less. The thickness is preferably 500 nm or more and 2 μm or less. In this case, the coating method may be a spin coating method, a dip coating method, a doctor blade method, or the like. For example, when a polyimide resin is used as the insulating film 420, By removing a portion of the film using the polyimide resin by the method, a film having a desired thickness can be obtained. An insulating film 420 can be obtained.

[0380] The first element layer 410 is fabricated at a temperature of room temperature or higher and 300° C. or lower. For example, the insulating film or conductive film using an inorganic material included in the first element layer 410 is preferably The conductive film is formed at a film formation temperature of 150°C to 300°C, and more preferably 200°C to 270°C. In addition, the organic resin material contained in the first element layer 410 is preferably used. The insulating film or the like is preferably formed at a film formation temperature of from room temperature to 100° C. or less.

[0381] In addition, the oxide semiconductor film of the transistor included in the first element layer 410 is It is preferable to use AC-OS for the oxide semiconductor film of the transistor. When S is used, for example, when a display device is bent, cracks or the like are generated in the channel formation region. This makes it possible to improve the bending resistance.

[0382] The conductive film included in the first element layer 410 is made of indium tin oxide to which silicon oxide is added. When tin oxide is used, cracks are less likely to occur in the conductive film when the display device is bent. This is preferable because

[0383] Next, the first element layer 410 and a temporary support substrate 466 are bonded together using a peeling adhesive 464. Then, the insulating film 420 and the first element layer 410 are peeled off from the substrate 462. The first element layer 420 and the first element layer 410 are provided on the temporary support substrate 466 side (see FIG. 40(B)). .

[0384] The temporary support substrate 466 may be a glass substrate, a quartz substrate, a sapphire substrate, a ceramic substrate, A metal substrate or the like can be used. In addition, a substrate having heat resistance capable of withstanding the processing temperature of this embodiment is also suitable. A plastic substrate having a thickness of 100 nm or a flexible substrate such as a film may be used. .

[0385] The peeling adhesive 464 may be soluble in water or solvent, or plasticized by exposure to ultraviolet light, etc. The temporary support substrate 466 and the first element layer 410 can be removed as needed. An adhesive that can chemically or physically separate the adhesive from the adhesive is used.

[0386] In addition, the transfer step onto the temporary support substrate 466 can be performed by using various methods as appropriate. For example, , the side of the substrate 462 on which the insulating film 420 is not formed, that is, the lower side shown in FIG. By irradiating the insulating film 420 with the laser light 468, the insulating film 420 is weakened. The substrate 462 and the insulating film 420 can be peeled off by the laser beam 468. By adjusting the energy density, it is possible to obtain a region where the substrate 462 and the insulating film 420 have high adhesion and a region where the substrate 462 and the insulating film 420 have high adhesion. Alternatively, regions where the plate 462 and the insulating film 420 have low adhesion may be created and then peeled off.

[0387] In this embodiment, the method of peeling off the substrate 462 and the insulating film 420 at the interface is as follows. However, the present invention is not limited to this. For example, the boundary between the insulating film 420 and the first element layer 410 may be It may be peeled off at the surface.

[0388] In addition, a liquid is permeated into the interface between the substrate 462 and the insulating film 420 to remove the insulating film 420 from the substrate 462. Alternatively, a liquid may be permeated into the interface between the insulating film 420 and the first element layer 410. The first element layer 410 may be peeled off from the insulating film 420 by removing the liquid. For example, water, a polar solvent, or the like can be used. The liquid is formed at the interface between the plate 462 and the insulating film 420 or at the interface between the insulating film 420 and the first element layer 410. The electrostatic charge generated by the peeling applied to the first element layer 410 by penetrating the body The effects of heat and other factors can be suppressed.

[0389] Next, the first substrate 401 is bonded to the insulating film 420 using the adhesive layer 418 (FIG. 40( See C).

[0390] The release adhesive 464 is then dissolved or plasticized to remove the release adhesive from the first element layer 410. The adhesive 464 and the temporary support substrate 466 are removed (see FIG. 40(D)).

[0391] The peeling adhesive 464 is removed by removing water or a solvent so that the surface of the first element layer 410 is exposed. It is preferable to remove it.

[0392] Through the above steps, the first element layer 410 can be manufactured over the first substrate 401 .

[0393] Next, the second substrate 4 is formed by the same method as the steps shown in FIG. 40(A) to FIG. 40(D). 05, an adhesive layer 412 on the second substrate 405, an insulating film 440 on the adhesive layer 412, and The second element layer 411 is formed using a semiconductor Alternatively, the second element layer 411 may include a display element in addition to a semiconductor element. Alternatively, a part of a display element such as a pixel electrode may be provided.

[0394] The insulating film 440 of the second element layer 411 is made of the same material as the insulating film 420. can be formed using an organic resin.

[0395] Next, a sealing layer 432 is filled between the first element layer 410 and the second element layer 411. The element layer 410 and the second element layer 411 are bonded to each other (see FIG. 41B).

[0396] The sealing layer 432 can provide, for example, solid sealing. The sealing layer 432 is preferably made of, for example, glass frit. Glass materials such as these, two-part resins that harden at room temperature, and photocurable resins For example, a resin material such as a thermosetting resin can be used.

[0397] In this manner, a display device can be manufactured.

[0398] <Display device manufacturing method 2> Next, another method for manufacturing a display device will be described with reference to FIG. A structure in which an inorganic insulating film is used as the insulating film 420 will be described.

[0399] First, a separation layer 463 is formed over a substrate 462. Next, an insulating film 420 is formed over the separation layer 463. A first element layer 410 is formed over the insulating film 420 (see FIG. 42A).

[0400] The peeling layer 463 may be made of, for example, tungsten, molybdenum, titanium, tantalum, or niobium. , Nickel, Cobalt, Zirconium, Zinc, Ruthenium, Rhodium, Palladium, Os An element selected from the group consisting of tungsten, iridium, and silicon, an alloy material containing the element, or The material may be a compound material containing silicon, and may be a single layer or a laminated structure. In the case of a layer containing silicon, the crystal structure of the layer containing silicon may be amorphous, microcrystalline, polycrystalline, or the like. The crystal may be either a single crystal or a single crystal.

[0401] The release layer 463 can be formed by a sputtering method, a PECVD method, a coating method, a printing method, or the like. The coating method includes a spin coating method, a droplet ejection method, and a dispense method.

[0402] When the release layer 463 has a single layer structure, it is made of tungsten, molybdenum, or tungsten and molybdenum. It is preferable to form a layer containing a mixture of tungsten and butenone. a layer containing an oxynitride, a layer containing an oxide or oxynitride of molybdenum, or a layer containing tungsten A layer containing an oxide or oxynitride of a mixture of stainless steel and molybdenum may be formed. A mixture of tungsten and molybdenum is, for example, an alloy of tungsten and molybdenum. is equivalent to.

[0403] The peeling layer 463 may be a stack of a layer containing tungsten and a layer containing an oxide of tungsten. When forming a layered structure, a layer containing tungsten is formed, and an upper layer made of oxide is formed. By forming an insulating layer, tungsten oxide is formed at the interface between the tungsten layer and the insulating layer. In addition, the surface of the layer containing tungsten may be treated with a thermal acid. Chemical treatment, oxygen plasma treatment, nitrous oxide (N 2 O) Oxidation power of plasma treatment, ozone water, etc. A layer containing tungsten oxide may be formed by treatment with a strong solution or the like. Zuma treatment and heat treatment can be performed using oxygen, nitrogen, or nitrous oxide alone or in combination with other gases. The above-mentioned plasma treatment or heat treatment may be performed under a mixed gas atmosphere. By changing the surface condition of the peeling layer 463, the adhesion between the peeling layer 463 and the insulating film 420 to be formed later can be improved. It is possible to control the

[0404] The insulating film 420 may be, for example, a silicon oxide film, a silicon nitride film, a silicon oxynitride film, or a silicon nitride oxide film. Inorganic insulating films with low moisture permeability, such as silicon films and aluminum oxide films, can be used. The inorganic insulating film can be formed by using, for example, a sputtering method, a PECVD method, or the like. Cut.

[0405] Next, the first element layer 410 and a temporary support substrate 466 are bonded together using a peeling adhesive 464. Then, the insulating film 420 and the first element layer 410 are peeled off from the peeling layer 463. The film 420 and the first element layer 410 are provided on the temporary support substrate 466 side (see FIG. 42(B)). ).

[0406] In addition, the transfer step onto the temporary support substrate 466 can be performed by using various methods as appropriate. For example, When a layer including a metal oxide film is formed at the interface between the peeling layer 463 and the insulating film 420, the metal The oxide film is weakened by crystallization, and the insulating film 420 can be peeled off from the peeling layer 463. In addition, when the peeling layer 463 is formed using a tungsten film, ammonia water and hydrogen peroxide are used. The tungsten film may be removed while being etched with a mixed solution of water.

[0407] In addition, a liquid is permeated into the interface between the peeling layer 463 and the insulating film 420 to remove the insulating film from the peeling layer 463. The liquid may be, for example, water, a polar solvent, or the like. At the interface where the insulating film 420 is peeled off, specifically, at the interface between the peeling layer 463 and the insulating film 420, By infiltrating the liquid, the static electricity generated by the peeling applied to the first element layer 410 is reduced. The effects of electricity, etc. can be suppressed.

[0408] Next, the first substrate 401 is bonded to the insulating film 420 using the adhesive layer 418 (FIG. 42(C) reference).

[0409] The release adhesive 464 is then dissolved or plasticized to remove the release adhesive from the first element layer 410. The adhesive 464 and the temporary support substrate 466 are removed (see FIG. 42(D)).

[0410] The peeling adhesive 464 is removed by removing water or a solvent so that the surface of the first element layer 410 is exposed. It is preferable to remove it.

[0411] Through the above steps, the first element layer 410 can be manufactured over the first substrate 401 .

[0412] In this manner, a display device can be manufactured.

[0413] (Embodiment 4) In this embodiment, a display device according to one embodiment of the present invention and an input device attached to the display device will be described. The attached electronic device will be described with reference to FIGS.

[0414] <Touch panel explanation> In the present embodiment, an electronic device that combines a display device and an input device is used as an example of the electronic device. The touch panel 2000 will be described. In addition, as an example of an input device, a touch sensor The case where the above formula is used will be described.

[0415] 43(A) and (B) are perspective views of the touch panel 2000. 2, representative components of touch panel 2000 are shown for clarity.

[0416] The touch panel 2000 includes a display device 2501 and a touch sensor 2595 (see FIG. 43). The touch panel 2000 also includes a substrate 2510, a substrate 2570, and a substrate The substrate 2510, the substrate 2570, and the substrate 2590 are all However, any of the substrates 2510, 2570, and 2590 is flexible. Alternatively, one or all of the components may be configured to have no flexibility.

[0417] The display device 2501 includes a plurality of pixels on a substrate 2510 and a display device that can supply signals to the pixels. The plurality of wirings 2511 are arranged around the periphery of the substrate 2510. The wire is routed through a wire loop, part of which constitutes the terminal 2519. The terminal 2519 is an FPC 2509 (1) and electrically connect it.

[0418] The substrate 2590 includes a touch sensor 2595 and a plurality of electrodes electrically connected to the touch sensor 2595. The plurality of wirings 2598 are routed around the periphery of the substrate 2590. A part of the terminal is electrically connected to the FPC2509(2). In FIG. 43(B), for the sake of clarity, the back side of the substrate 2590 (the substrate 2510) is shown. Electrodes and wiring of a touch sensor 2595 provided on the opposing surface are indicated by solid lines.

[0419] As the touch sensor 2595, for example, a capacitive touch sensor can be used. The capacitance type includes a surface type capacitance type and a projected type capacitance type.

[0420] Projected capacitive touch panels are classified into self-capacitance and mutual capacitance types, which differ mainly in their drive systems. The mutual capacitance method is preferable because it enables simultaneous multi-point detection.

[0421] The touch sensor 2595 shown in FIG. 43(B) is a projected capacitive touch sensor. This is a configuration in which the above is applied.

[0422] The touch sensor 2595 can detect the proximity or contact of a detection target such as a finger. Various sensors can be applied.

[0423] The projected capacitive touch sensor 2595 has an electrode 2591 and an electrode 2592. The electrode 2591 is electrically connected to one of a plurality of wirings 2598, and the electrode 2592 is 2598 .

[0424] As shown in FIG. 43(A)(B), the electrode 2592 is a plurality of electrodes repeatedly arranged in one direction. It has a shape in which quadrilaterals are connected at the corners.

[0425] The electrode 2591 is quadrilateral and is repeatedly arranged in a direction intersecting the direction in which the electrodes 2592 extend. It is placed there.

[0426] The wiring 2594 is electrically connected to the two electrodes 2591 that sandwich the electrode 2592. Preferably, the shape is such that the area of ​​the intersection between the electrode 2592 and the wiring 2594 is as small as possible. This makes it possible to reduce the area of ​​the region where no electrodes are provided, and thus reduce variations in transmittance. As a result, it is possible to reduce the variation in the brightness of the light passing through the touch sensor 2595. can.

[0427] The shapes of the electrodes 2591 and 2592 are not limited to these, and may take various shapes. For example, multiple electrodes 2591 are arranged with as few gaps as possible, and are A plurality of electrodes 2592 are provided at intervals so that there is an area where the electrodes 2592 do not overlap with the electrodes 2591. In this case, a wire may be provided between two adjacent electrodes 2592, which is electrically isolated from the two adjacent electrodes 2592. Providing an insulated dummy electrode is preferable because it can reduce the area of ​​the region with different transmittance. .

[0428] In addition, the conductive films such as the electrodes 2591, the electrodes 2592, and the wiring 2598, that is, the touch panel Materials that can be used for the wiring and electrodes that make up the device include indium oxide, tin oxide, and Examples of such conductive films include transparent conductive films containing zinc, etc. (e.g., ITO, etc.). As a material that can be used for the wiring and electrodes, for example, a material with a low resistance value is preferable. Examples include silver, copper, aluminum, carbon nanotubes, graphene, and halogens. Metal halide (silver halide, etc.) may also be used. Metal nanowires having a diameter of several nanometers and composed of multiple conductors may be used. Alternatively, a metal mesh made of a conductor may be used. Nanowires, Cu nanowires, Al nanowires, Ag mesh, Cu mesh, Al mesh For example, Ag nanowires may be used for the wiring and electrodes that make up the touch panel. When used, the transmittance in visible light is 89% or more, and the sheet resistance is 40 Ω / cm 2 1 more 00Ω / cm 2 The wiring and the like constituting the above-mentioned touch panel can be Examples of materials that can be used for the electrodes include metal nanowires, metal mesh, and carbon. Nanotubes and graphene have high transmittance in visible light, so they are used in display elements. It may be used as an electrode (eg, a pixel electrode or a common electrode).

[0429] <Explanation about the display device> Next, the display device 2501 will be described in detail with reference to FIGS. 44(A) and 44(B). 4(A) and (B) correspond to cross-sectional views taken along dashed line X1-X2 shown in FIG. 43(B).

[0430] The display device 2501 has a plurality of pixels arranged in a matrix. and a pixel circuit for driving the display element.

[0431] In the cross-sectional view shown in FIG. 44(A), an EL element that emits white light is used as a display element. However, the EL element is not limited to this. As shown in Figure 2B, adjacent pixels emit different colors of light. In the following explanation, the EL element that emits white light can be painted differently for each pixel. An example in which an emitting EL element is used as a display element will be described.

[0432] The substrate 2510 and the substrate 2570 are, for example, a substrate having a water vapor permeability of 10 -5 g / (m 2 ·day) or less, preferably 10 -6 g / (m 2 -Flexibility of less than 1000msec Alternatively, the thermal expansion coefficient of the substrate 2510 and the thermal expansion coefficient of the substrate 2570 may be set to be equal to or larger than the thermal expansion coefficient of the substrate 2570. It is preferable to use a material with a linear expansion coefficient approximately equal to that of the material. For example, a material with a linear expansion coefficient of 1×10 - 3 / K or less, preferably 5×10 -5 / K or less, more preferably 1×10 -5 / K or less Certain materials may be used advantageously.

[0433] The substrate 2510 is made up of an insulating layer 2510a for preventing impurities from diffusing into the EL element, and a flexible substrate. The plate 2510b is bonded to the insulating layer 2510a and the flexible substrate 2510b by an adhesive layer 2 510c. The substrate 2570 is a laminate having a structure for preventing diffusion of impurities into the EL element. and a flexible substrate 2570b. and an adhesive layer 2570c for bonding the plates 2570b together.

[0434] The adhesive layer 2510c and the adhesive layer 2570c may be made of, for example, polyester or polyolefin. Polyimide, polycarbonate, polyurethane, polyamide (nylon, aramid, etc.) Materials containing tan, acrylic resin, epoxy resin, or resin with siloxane bonds It can be used in the adhesive layer.

[0435] In addition, a sealing layer 2560 is provided between the substrate 2510 and the substrate 2570. The sealing layer 2560 is It is preferable that the refractive index of the sealing layer is larger than that of air. When light is extracted to the 2560 side, the sealing layer 2560 can also serve as an optical element.

[0436] A sealant may be formed on the outer periphery of the sealing layer 2560. As a result, the area surrounded by the substrate 2510, the substrate 2570, the sealing layer 2560, and the sealant The sealing layer 2560 may have a structure in which the EL element 2550 is disposed in the insulating layer 2560. It is also possible to fill the container with an inactive gas (such as nitrogen or argon). In addition, a desiccant may be placed in the inactive gas. In addition, the above-mentioned sealing material may be, for example, It is preferable to use epoxy resin or glass frit. It is preferable to use a material that is not permeable to moisture or oxygen.

[0437] The display device 2501 shown in FIG. 44A includes a pixel 2505. 05 includes a light emitting module 2580, an EL element 2550, and a power supply for the EL element 2550. The transistor 2502t can supply a t functions as a part of the pixel circuit.

[0438] The light emitting module 2580 also includes an EL element 2550 and a coloring layer 2567. The EL element 2550 includes a lower electrode, an upper electrode, and an EL layer between the lower electrode and the upper electrode. and

[0439] In addition, when the sealing layer 2560 is provided on the side from which light is extracted, the sealing layer 2560 is an EL The element 2550 is in contact with a colored layer 2567. The colored layer 2567 is made of EL elements having different luminescent colors. If the child is painted pixel by pixel, it is possible to omit it as shown in FIG. .

[0440] The colored layer 2567 is located so as to overlap the EL element 2550. A part of the light emitted by the light emitting module 2560 passes through the colored layer 2567 and travels in the direction of the arrow shown in the figure. It is ejected from the exterior of Lu2580.

[0441] The display device 2501 is also provided with a light-shielding layer 2568 in the light-emitting direction. 2568 is provided to surround the colored layer 2567 .

[0442] The colored layer 2567 may have a function of transmitting light of a specific wavelength band. For example, For example, a color filter that transmits light in the red wavelength range and a color filter that transmits light in the green wavelength range are used. -filter, a color filter that transmits light in the blue wavelength band, and a color filter that transmits light in the yellow wavelength band Each color filter can be made of various materials. Printing, inkjet printing, photolithography etching, etc. It can be formed.

[0443] The display device 2501 is also provided with an insulating layer 2521. The insulating layer 2521 is provided to flatten the unevenness caused by the pixel circuit. In addition, the insulating layer 2521 has a function of suppressing diffusion of impurities. This prevents the reliability of the transistors 2502t and the like from being reduced due to the diffusion of impurities. It can be suppressed.

[0444] The EL element 2550 is formed above the insulating layer 2521. A partition wall 2528 is provided on the lower electrode of the semiconductor device 250 so as to overlap an edge of the lower electrode. A spacer for controlling the distance between the substrate 2510 and the substrate 2570 is formed on the partition wall 2528. This is also fine.

[0445] The gate line driver circuit 2504 includes a transistor 2503t and a capacitor 2503c. Note that the driver circuit and the pixel circuit can be formed on the same substrate in the same process. .

[0446] In addition, wiring 2511 capable of supplying signals is provided on the substrate 2510. In addition, a terminal 2519 is provided on the wiring 2511. FPC2509(1) is electrically connected to the FPC2509(1). It has the function of supplying lock signals, start signals, reset signals, etc. A printed wiring board (PWB) may be attached to 09(1).

[0447] In addition, either one or both of the transistors 2502t and 2503t The transistor described in the above embodiment may be used for the transistor. The transistor has a highly purified oxide semiconductor film with high crystallinity. Therefore, the current value (off-state current value) at the time of the image signal or other electric signal can be reduced. The retention time of the data can be extended, and the write interval can also be set longer when the power is on. This reduces the frequency of refresh operations, resulting in reduced power consumption. The refresh operation will be described in detail later.

[0448] In addition, the transistor used in this embodiment has a relatively high field-effect mobility. For example, a transistor capable of high speed driving is used in a display device. By using 2501, the switching transistor of the pixel circuit and the driving circuit The driver transistor can be formed on the same substrate. In addition, since it is not necessary to use a semiconductor device formed from a silicon wafer or the like, This allows the number of components in the device to be reduced. By using a transistor, it is possible to provide a high quality image.

[0449] <Explanation about touch sensor> Next, the touch sensor 2595 will be described in detail with reference to FIG. 3(B) along dashed line X3-X4.

[0450] The touch sensor 2595 includes electrodes 2591 and electrodes 2592 arranged in a staggered pattern on a substrate 2590. 2592, an insulating layer 2593 covering the electrodes 2591 and 2592, and adjacent electrodes 2593. 591 and a wiring 2594 that electrically connects them.

[0451] The electrode 2591 and the electrode 2592 are formed using a light-transmitting conductive material. Examples of conductive materials having the above structure include indium oxide, indium tin oxide, and indium zinc oxide. Conductive oxides such as zinc oxide, zinc oxide doped with gallium can be used. A film containing graphene may also be used. The film containing graphene may be, for example, a film-like The graphene oxide-containing film formed on the substrate can be reduced to form the graphene oxide-containing film. An example of such a method is the application of heat.

[0452] For example, a light-transmitting conductive material is formed on the substrate 2590 by a sputtering method. After that, various patterning techniques such as photolithography are used to remove unnecessary parts, An electrode 2591 and an electrode 2592 can be formed.

[0453] The material used for the insulating layer 2593 may be, for example, a resin such as acrylic or epoxy. In addition to resins with siloxane bonds, silicon oxide, silicon oxynitride, and aluminum oxide It is also possible to use inorganic insulating materials such as the above.

[0454] In addition, an opening reaching the electrode 2591 is provided in the insulating layer 2593, and a wiring 2594 is adjacent The transparent conductive material is electrically connected to the electrode 2591. Therefore, it can be suitably used for the wiring 2594. A material having a higher electrical conductivity than the electrode 2592 is preferable for the wiring 2594 because it can reduce electrical resistance. It can be used appropriately.

[0455] The electrodes 2592 extend in one direction, and a plurality of electrodes 2592 are provided in a stripe pattern. Moreover, the wiring 2594 is provided so as to intersect with the electrode 2592 .

[0456] A pair of electrodes 2591 are provided with one electrode 2592 in between. The pair of electrodes 2591 are electrically connected.

[0457] The multiple electrodes 2591 are arranged in a direction that is not necessarily perpendicular to one electrode 2592. This is not necessary, and they may be arranged to form an angle greater than 0 degrees but less than 90 degrees.

[0458] The wiring 2598 is electrically connected to the electrode 2591 or the electrode 2592. A part of the wiring 2598 functions as a terminal. The wiring 2598 is, for example, an aluminum Aluminum, gold, platinum, silver, nickel, titanium, tungsten, chromium, molybdenum, iron, Metal materials such as zinc, copper, palladium, etc., and alloy materials containing such metal materials can be used. can.

[0459] An insulating layer is provided to cover the insulating layer 2593 and the wiring 2594, and the touch sensor 2595 may be protected.

[0460] Furthermore, the connection layer 2599 electrically connects the wiring 2598 and the FPC 2509(2).

[0461] The connection layer 2599 is made of an anisotropic conductive film (ACF). Conductive Film) and Anisotropic Conductive Paste (ACP) c Conductive Paste) can be used.

[0462] <Touch panel explanation> Next, the touch panel 2000 will be described in detail with reference to FIG. 43A) corresponds to a cross-sectional view taken along dashed line X5-X6 shown in FIG. 43A.

[0463] The touch panel 2000 shown in FIG. 46A includes the display device 2501 described in FIG. The touch sensor 2595 described in FIG. 45 is bonded to the touch sensor 2595.

[0464] The touch panel 2000 shown in FIG. 46(A) is similar to the touch panel 2000 described in FIG. 44(A) and FIG. In addition to this configuration, it has an adhesive layer 2597 and an anti-reflective layer 2569.

[0465] The adhesive layer 2597 is provided in contact with the wiring 2594. The substrate 2590 is attached to the substrate 2570 so that the sensor 2595 overlaps the display device 2501. In addition, it is preferable that the adhesive layer 2597 is transparent. The material 97 can be a thermosetting resin or an ultraviolet curing resin. Use acrylic resin, urethane resin, epoxy resin, or siloxane resin. can be done.

[0466] The anti-reflection layer 2569 is provided at a position overlapping the pixel. For example, a circular polarizing plate can be used.

[0467] Next, for a touch panel having a different configuration from that shown in FIG. 46(A), FIG. 46(B) is used. I will explain it below.

[0468] FIG. 46(B) is a cross-sectional view of the touch panel 2001. The control unit 2001 corresponds to the touch panel 2000 shown in FIG. The location of the touch sensor 2595 is different. The different configurations are described in detail here, and The description of touch panel 2000 is cited for the parts in which this configuration can be used.

[0469] The colored layer 2567 is located below the EL element 2550. The element 2550 emits light to the side where the transistor 2502t is provided. A part of the light emitted by the EL element 2550 is transmitted through the colored layer 2567 and is reflected by the light emitting diode 2566 shown in FIG. The light is emitted to the outside of the light emitting module 2580 in the direction of the arrow.

[0470] In addition, the touch sensor 2595 is provided on the substrate 2510 side of the display device 2501.

[0471] The adhesive layer 2597 is between the substrate 2510 and the substrate 2590 and is connected to the display device 2501 and the touch panel 2520. Attach the sensor 2595.

[0472] As shown in FIGS. 46(A) and 46(B), the light emitted from the light emitting element passes through the substrate 2510 and the substrate 2570. It may be injected through either or both of the 2570.

[0473] <Explanation of how to drive the touch panel> Next, an example of a method for driving a touch panel will be described with reference to FIG.

[0474] FIG. 47(A) is a block diagram showing the configuration of a mutual capacitance type touch sensor. In A), a pulse voltage output circuit 2601 and a current detection circuit 2602 are shown. In 47(A), the electrodes 2621 to which the pulse voltage is applied are designated as X1-X6, and the change in current is The electrodes 2622 for detecting the voltage are designated Y1-Y6, and are illustrated with six wires each. FIG. 47(A) shows a capacitance 2 formed by overlapping an electrode 2621 and an electrode 2622. 603. The electrodes 2621 and 2622 have functions interchangeably. This is also fine.

[0475] The pulse voltage output circuit 2601 is a circuit for applying a pulse voltage to the wirings X1-X6 in sequence. When a pulse voltage is applied to the wiring of X1-X6, a capacitance 2603 is formed. An electric field is generated between the electrodes 2621 and 2622. The electric field generated between these electrodes may cause shielding or the like. This generates a change in the mutual capacitance of the capacitor 2603, and is used to detect the proximity of the object to be detected, or can detect contact.

[0476] The current detection circuit 2602 detects the change in mutual capacitance of the capacitor 2603 between the wirings Y1 to Y6. This is a circuit for detecting changes in current at the If there is no contact, the detected current value will not change, but the proximity of the object to be detected or When the mutual capacitance decreases due to contact, the current value decreases. The detection may be performed using an integrating circuit or the like.

[0477] Next, FIG. 47(B) shows the input / output of the mutual capacitance type touch sensor shown in FIG. 47(A). FIG. 47(B) shows the timing chart of the output waveform for each row and column in one frame period. In FIG. 47(B), the case where the object to be detected is not detected (non-detection) is shown. The two cases shown are when a touch is detected and when a detected object is detected. For the wiring Y1-Y6, the waveform is shown as a voltage value corresponding to the detected current value. do.

[0478] A pulse voltage is applied to the wires X1-X6 in sequence, and the wires Y1-Y The waveform in wire 6 changes. When there is no proximity or contact of the object to be sensed, the waveform in wire X1-X6 The waveforms of Y1-Y6 change uniformly according to the change in the voltage of the wiring. At the points where the current flows or comes into contact, the current value decreases, and the corresponding voltage waveform also changes. .

[0479] In this way, the proximity or contact of a sensing object can be detected by detecting the change in mutual capacitance. It is possible.

[0480] <Sensor circuit explanation> In FIG. 47A, only a capacitor 2603 is provided at the intersection of the wiring as a touch sensor. The configuration of a passive matrix touch sensor has been shown, but The touch sensor may be an active matrix type. An example of a sensor circuit included in the sensor is shown in FIG.

[0481] The sensor circuit shown in FIG. 48 includes a capacitor 2603, a transistor 2611, and a transistor 2612. 612 and a transistor 2613.

[0482] A signal G2 is applied to the gate of the transistor 2613, and a voltage is applied to either the source or the drain. A voltage VRES is applied, and the other is connected to one electrode of the capacitor 2603 and the The transistor 2611 has a source and a drain that are electrically connected to each other. It is electrically connected to either the source or drain of the transistor 2612, and the other is connected to the voltage VSS A signal G1 is applied to the gate of the transistor 2612, and a signal G2 is applied to the source or drain of the transistor 2612. The other electrode of the capacitor 2603 is electrically connected to the wiring ML. is given.

[0483] Next, the operation of the sensor circuit shown in FIG. 48 will be described. First, a transistor is used as the signal G2. When a potential is applied to turn on the transistor 2613, the gate of the transistor 2611 A potential corresponding to the voltage VRES is applied to the node n to which the signal G2 is connected. By applying a potential that turns off the transistor 2613, the potential of the node n is maintained. It will be held.

[0484] Next, the mutual capacitance of the capacitance 2603 changes due to the proximity or contact of a detection object such as a finger. Accordingly, the potential of the node n changes from VRES.

[0485] The read operation applies a potential to the signal G1 to turn on the transistor 2612. A current flows through the transistor 2611 in response to the potential of the node n, that is, a current flows through the wiring ML. By detecting this current, the proximity or contact of the object to be detected can be detected. can be done.

[0486] The transistors 2611, 2612, and 2613 are In particular, the transistor 2613 may be a transistor having the above-mentioned structure. By using the transistor described in the embodiment, the potential of the node n can be maintained for a long period of time. It becomes possible to hold the voltage, and the operation of supplying VRES to node n again (refresh operation) ) can be reduced.

[0487] (Embodiment 5) In this embodiment mode, the appearance and display of a display device having the pixels described in the above embodiment mode will be described. An example of an electronic device equipped with the device will be described.

[0488] <Appearance of the display device> FIG. 49(A) is a perspective view showing an example of the appearance of a display device. The device is composed of a panel 1601, a controller, a power supply circuit, an image processing circuit, an image memory, and a CP. The panel 160 includes a circuit board 1602 on which a U or the like is provided, and a connection portion 1603. 1 is a pixel portion 1604 having a plurality of pixels and a driver circuit for selecting the plurality of pixels for each row. 1605, and a driver circuit 1606 for controlling the input of data voltages to the pixels in a selected row. has.

[0489] Various signals and a power supply potential are transmitted from the circuit board 1602 to the panel via the connection portion 1603. The connection part 1603 is connected to an FPC (Flexible Printer The FPC with the chip mounted on it is called CO This is called F tape, and the use of COF tape allows for higher density mounting in a smaller area. In addition, when a COF tape is used for the connection portion 1603, A part of the circuit, or a part of the driver circuit 1605 or the driver circuit 1606 of the panel 1601 The above is formed on a separately prepared chip and then the COF (Chip On Film) method is used. The chip may be connected to the COF tape in advance.

[0490] FIG. 49(B) is a perspective view showing an example of the appearance of a display device using the COF tape 1607. As shown in.

[0491] The chip 1608 is a semiconductor bare chip (such as an IC or LSI) having terminals such as bumps on its surface. In addition, CR components can also be mounted on the COF tape 1607, and the circuit board 1602 The wiring pattern of the flexible board corresponds to the terminals of the chip to be mounted. The chip 1608 is bonded to a substrate having a wiring pattern by a bonder device or the like. The chip is positioned and placed on a flexible substrate and then mounted by thermocompression bonding.

[0492] FIG. 49(B) shows an example of one COF tape 1607 on which one chip 1608 is mounted. However, it is not particularly limited. A single COF tape 1607 may have multiple rows of chips on one or both sides. However, to reduce costs, it is necessary to reduce the number of chips to be mounted. It is preferable to have a single row, and more preferably, to have only one.

[0493] <Examples of electronic device configurations> Next, an electronic device equipped with a display device will be described.

[0494] A display device according to one aspect of the present invention is a display device, a notebook personal computer, a recording medium, Image playback devices equipped with a DVD player (typically DVD: Digital Versatile Digital Used for devices that play recording media such as ISC and have a display that can display the images. In addition, an electronic device in which the display device according to one embodiment of the present invention can be used As devices, mobile phones, portable game consoles, personal digital assistants, e-book terminals, video cameras, Digital still cameras and other cameras, goggle-type displays (head-mounted displays) (car audio, digital audio player), navigation systems, audio playback devices Layers, etc.), copiers, facsimiles, printers, multifunction printers, ATM machines Examples of electronic devices include ATMs and vending machines. show.

[0495] FIG. 50A shows a display device, which includes a housing 5001, a display unit 5002, a support stand 5003, etc. The display device according to one embodiment of the present invention can be used for the display portion 5002. Display devices include all information displays, such as those for personal computers, TV broadcast reception, and advertisement displays. A display device for displaying information is included.

[0496] FIG. 50B shows a portable information terminal, which includes a housing 5101, a display unit 5102, and operation keys 5103. The display device according to one embodiment of the present invention can be used for the display portion 5102.

[0497] FIG. 50C shows a display device having a curved housing 5701, a display portion 5702, etc. By using a flexible substrate in the display device according to one embodiment of the present invention, a curved case can be easily formed. The display device can be used for a display portion 5702 supported by a body 5701. It is therefore possible to provide a display device that is compact, lightweight, and easy to use.

[0498] FIG. 50D shows a portable game machine. The portable game machine includes a housing 5301, a housing 5302, a display portion 5303, A display unit 5304, a microphone 5305, a speaker 5306, an operation key 5307, a star The display device according to one embodiment of the present invention includes the display portion 5303 or the display The display portion 5303 or the display portion 5304 may be used as one of the display devices of the present invention. By using the display device according to the embodiment, the user experience is excellent and deterioration of quality is unlikely to occur. It is possible to provide a portable game machine that can be used with a portable game machine shown in FIG. The display device has two display areas 5303 and 5304. The number of display units is not limited to this.

[0499] FIG. 50E shows an electronic book terminal, which includes a housing 5601, a display portion 5602, and the like. The display device according to one embodiment can be used for the display portion 5602. By using a substrate that can be used for display devices, the display device can be made flexible. Moreover, it is possible to provide an electronic book terminal that is light and easy to use.

[0500] FIG. 50F shows a mobile phone. A housing 5901 includes a display unit 5902, a microphone 5907, and a speaker. Speaker 5904, camera 5903, external connection part 5906, and operation button 5905 are provided. The display device according to one embodiment of the present invention can be used for the display portion 5902. In addition, when the display device according to one embodiment of the present invention is formed on a flexible substrate, The display device can be applied to a display unit 5902 having a curved surface as shown in FIG. do.

[0501] In this specification, the terms "above" and "below" that indicate the position of components are used. The positional relationship is used for convenience in describing the configuration with reference to the drawings. The orientation of each component changes accordingly. The present invention is not limited to the above description, and may be rephrased appropriately depending on the situation.

[0502] In the present specification and the like, in the block diagrams, components are classified by function and are independent of each other. However, in actual circuits, the components are divided into blocks according to their functions. In some cases, it is difficult to separate the circuits, and multiple functions are involved in one circuit, or multiple circuits are involved. Therefore, the blocks in the block diagram may be different from those described in the specification. The present invention is not limited to the above-described components, and may be rephrased appropriately depending on the situation.

[0503] In addition, the terms "electrode" and "wiring" used in this specification and the like do not limit the functionality of these components. For example, an "electrode" may be used as part of a "wire." In addition, the term "electrode" or "wiring" may be used to refer to the plural "electrodes" or "wirings". This also includes cases where the "line" is formed as a single unit.

[0504] In this specification and the like, the terms voltage and potential can be interchanged as appropriate. For example, the reference potential is the ground potential (earth potential). If we define the potential as the ground potential, the voltage can be expressed as the potential. Note that the potential is relative, and the arrangement may differ depending on the reference potential. The potential applied to the wires may be changed.

[0505] In this specification, the terms "film" and "layer" may be used depending on the circumstances. For example, the term "conductive layer" can be used interchangeably with "conductive layer" depending on the application. Alternatively, for example, the term "insulating film" may be used. In some cases, it may be possible to change the term "insulating layer" to the term "insulating layer."

[0506] In this specification, a switch refers to a device that is in a conductive state (on state) or a non-conductive state (off state). A switch that is in a "switchable state" and has the function of controlling whether or not current flows. A switch is a device that has the function of selecting and switching the path through which a current flows.

[0507] As an example, an electrical switch or a mechanical switch can be used. The switch is not limited to a specific one as long as it can control the current.

[0508] An example of an electrical switch is a transistor (e.g., a bipolar transistor, M OS transistors, etc.), diodes (e.g., PN diodes, PIN diodes, Schottky diode, MIM (Metal Insulator Metal) diode , MIS (Metal Insulator Semiconductor) diode diode-connected transistors, or logic circuits that combine these. be.

[0509] When a transistor is used as a switch, the "conduction state" of the transistor is This refers to a state in which the source and drain of a transistor can be considered to be electrically shorted. The "non-conducting state" of a transistor is when the source and drain of the transistor are electrically isolated. In addition, when a transistor is operated simply as a switch, In this case, the polarity (conductivity type) of the transistor is not particularly limited.

[0510] An example of a mechanical switch is a digital micromirror device (DMD). There are switches that use MEMS (microelectromechanical systems) technology. The switch has an electrode that can be mechanically moved, and the movement of the electrode causes Thus, the device operates by controlling conduction and non-conduction.

[0511] For example, in the present specification, when it is explicitly stated that X and Y are connected, In this case, X and Y are electrically connected, and X and Y are functionally connected. The case where X and Y are directly connected is also considered to be disclosed in the present specification. Therefore, the present invention is not limited to a specific connection relationship, for example, a connection relationship shown in a drawing or a sentence. Any connections other than those shown in the drawings or text shall be deemed to be included in the drawings or text. do.

[0512] Here, X and Y are objects (e.g., devices, elements, circuits, wiring, electrodes, terminals, conductive films, layers, etc.). , etc.).

[0513] An example of a direct connection between X and Y is a circuit that allows electrical connection between X and Y. The elements to be considered (e.g., switches, transistors, capacitance elements, inductors, resistance elements, When a resistor (such as an electrode, display element, light-emitting element, or load) is not connected between X and Y, The elements that allow electrical connection between X and Y (e.g., switches, transistors, capacitors, etc.) elements, inductors, resistors, diodes, display elements, light-emitting elements, loads, etc.) , X and Y are connected.

[0514] An example of a case where X and Y are electrically connected is The elements to be considered (e.g., switches, transistors, capacitance elements, inductors, resistance elements, One or more elements (such as an electrode, a display element, a light-emitting element, or a load) can be connected between X and Y. It is possible. The switch has a function that can be controlled by turning it on and off. A switch can be in a conductive state (on) or a non-conductive state (off) to allow current to flow. The switch has the function of controlling whether or not current flows. When X and Y are electrically connected, X This also includes the case where and Y are directly connected.

[0515] An example of a case where X and Y are functionally connected is a case where a functional connection between X and Y is possible. Circuits that perform the above functions (for example, logic circuits (inverters, NAND circuits, NOR circuits, etc.), signal conversion conversion circuits (DA conversion circuits, AD conversion circuits, gamma correction circuits, etc.), potential level conversion circuits ( power supply circuits (voltage boost circuits, voltage drop circuits, etc.), level shifter circuits that change the potential level of signals, etc.) , voltage sources, current sources, switching circuits, amplifier circuits (which can increase the signal amplitude or current amount, etc.) circuits, operational amplifiers, differential amplifier circuits, source follower circuits, buffer circuits, etc.), signal generation One or more devices (such as a memory circuit, a control circuit, etc.) can be connected between X and Y. For example, even if another circuit is inserted between X and Y, the signal output from X If X is transmitted to Y, then X and Y are considered to be functionally connected. When X and Y are functionally connected, there are cases where X and Y are directly connected and cases where X and Y are functionally connected. and the case where they are electrically connected to each other.

[0516] In addition, if it is explicitly stated that X and Y are electrically connected, are electrically connected (i.e., there is another element or circuit between X and Y) When X and Y are functionally connected (i.e., when X and Y are connected), (When there is a functional connection between X and Y via another circuit in between) and when X and Y are directly connected (i.e., when X and Y are connected without any other element or circuit between them) is deemed to be disclosed in the present specification. If it is explicitly stated that it is connected, The same contents are deemed to be disclosed in the present specification and the like.

[0517] For example, if the source (or the first terminal, etc.) of the transistor is connected via Z1 (or The drain (or second terminal, etc.) of the transistor is electrically connected to X. It may be electrically connected to Y through (or without) a transistor source (or is the first terminal, etc.) is directly connected to a part of Z1, and another part of Z1 is directly connected to X. The drain (or second terminal, etc.) of the transistor is directly connected to a part of Z2. If another part of Z2 is directly connected to Y, it can be expressed as follows: is possible.

[0518] For example, "X and Y and the source (or first terminal, etc.) and drain (or second terminal, etc.) of a transistor The transistors (e.g., the first terminal, etc.) are electrically connected to each other, and X is the source (or first terminal) of the transistor. The transistor drain (or second terminal, etc.) is electrically connected in the order of Y. Or, it can be expressed as "the source (or first terminal) of the transistor." The transistor drain (or second terminal, etc.) is electrically connected to X, and the transistor drain (or second terminal, etc.) is electrically connected to Y. The transistor drain is electrically connected to X. The input (or second terminal, etc.), Y, and the Or, "X is the source (or first terminal, etc.) and drain (or is electrically connected to Y via the second terminal, and X is the source (or The first terminal, the drain of the transistor, and Y are connected in this order. Using the same expression as these examples, the circuit By specifying the order of connections in the configuration, the source (or first The technical scope is determined by distinguishing between the first terminal (or the first terminal, etc.) and the drain (or the second terminal, etc.). This can be done.

[0519] Or, as another way of expressing it, for example, "The source (or first terminal, etc.) of a transistor is , electrically connected to X through at least a first connection path, the first connection path being The second connection path is a path through a transistor. The source (or first terminal, etc.) of the resistor and the drain (or second terminal, etc.) of the transistor The first connection path is a path through Z1, and the second connection path is a path between the drain of the transistor The drain (or the second terminal, etc.) is electrically connected to Y through at least a third connection path. The third connection path does not include the second connection path, and the third connection path is a path through Z2. The source (or the first terminal, etc.) is connected to X through Z1 by at least the first connection path. electrically connected, the first connection path does not have a second connection path, and the second The connection path has a connection path through a transistor, and the connection path is connected to the drain (or the second terminal, etc.) is electrically connected to Y through Z2 by at least a third connection path. The third connection path does not include the second connection path. Alternatively, the source (or the first terminal, etc.) of the transistor may be The first electrical path is electrically connected to X through Z1, and the first electrical path is The second electrical path does not include the source of the transistor (or the first 1 terminal) to the drain (or second terminal) of the transistor, The drain (or second terminal, etc.) of the transistor is connected to the , Z2, and Y, and the third electrical path is electrically connected to the fourth electrical path and the fourth electrical path is a drain (or a second terminal, etc.) of the transistor. The term "electrical path" refers to the electrical path from the input terminal to the source (or first terminal, etc.) of the transistor. Using the same expression method as these examples, the connection paths in the circuit configuration can be expressed as follows: By this definition, the source (or first terminal, etc.) and drain (or third terminal, etc.) of a transistor are The technical scope can be determined by distinguishing between devices with two terminals and devices with two terminals.

[0520] Note that these expression methods are merely examples, and the present invention is not limited to these expression methods. , Y, Z1, and Z2 are objects (e.g., devices, elements, circuits, wiring, electrodes, terminals, conductive films, layer, etc.).

[0521] In addition, the circuit diagram shows independent components as if they are electrically connected to each other. Even if the components are the same, one component may have the functions of multiple components. For example, when a part of the wiring also functions as an electrode, one conductive film has the function of the wiring and The electrode functions as both components. The term "electrochemically connected" refers to a case where one conductive film has the functions of multiple components. This also falls within the scope of the above. [Explanation of symbols]

[0522] BGE1 Back gate electrode BGE2 Back gate electrode BGE4‐BGE7 Backgate electrode C1‐C3 Capacitive element CG1 opening CG2 opening CG4-CG7 Aperture DE1-DE8 drain electrode EL1 light emitting element G1 signal G2 signal GE1‐GE8 Gate electrodes GL wiring GL1‐GL4 wiring L1‐L5 wiring La1 Channel length La2 Channel Length Lb1 Channel Length M1 Transistor ML wiring N1‐N3 nodes OS1‐OS8 Oxide semiconductor film P1-P4 period S1‐S5 Switches SE1‐SE8 source electrodes TA1-TA4 transistors TB1 Transistor TB2 Transistor TC1 Transistor TD1 Transistor Wa1 Channel width Wa2 Channel width Wb1 Channel width 10 pixels 20a‐20l pixels 21a‐21l pixels 22a-22l pixels 23a‐23l pixels 30 Substrate 31-33 Oxide semiconductor film 34 Insulating film 35 Insulating film 35a Insulating film 35b Insulating film 36 Insulating Film 40 Pixel section 70 Transistor 70A Transistor 71 Transistor 72 Substrate 73 Conductive Film 73a Conductive film 73b Conductive film 74 Insulating Film 75 Semiconductor Film 76 Insulating Film 77 Conductive Film 77a Conductive film 77b Conductive film 78 Insulating Film 79 Insulating Film 80 Conductive Film 81 Conductive Film 82 Channel formation region 83 LDD area 84 Impurity region 85 Conductive Film 86 Semiconductor Film 87a Conductive film 87b Conductive film 88 Conductive Film 89 Conductive Film 90 Channel formation region 91 Impurity region 93-96 Aperture 110 Drive circuit 120 Drive circuit 401 Substrate 405 Substrate 410 Element Layer 411 Element Layer 412 Adhesive layer 418 Adhesive layer 420 Insulating film 432 Sealing layer 440 Insulating film 462 Substrate 463 Peeling layer 464 Peeling adhesive 466 Temporary Support Substrate 468 Laser Light 501 Substrate 502 Conductive film 503 Insulating film 503a Insulating film 503b Insulating film 504 Amorphous semiconductor film 505 Nickel-containing layer 506 Crystalline Semiconductor Film 507 Barrier Layer 508 Gettering Site 509 Semiconductor Film 510 Semiconductor Film 511 Insulating film 512a Conductive film 512b Conductive film 514 Mask 515 Conductive Film 515a lower layer 515b upper layer 516 Conductive Film 516a lower layer 516b Upper layer 517 Conductive Film 517a Lower layer 517b upper layer 518 Conductive Film 518a Lower layer 518b Upper layer 520-525 Impurity region 530 Interlayer insulating film 531 Transistor 532 Transistor 533 Interlayer insulating film 534 Interlayer insulating film 535 Wiring 538 Wiring 540 Pixel electrode 541 Organic resin film 542 Light-emitting layer 543 Cathode 544 Light emitting element 545 Protective film 1601 Panel 1602 Circuit Board 1603 Connection 1604 Pixel section 1605 Drive circuit 1606 Drive circuit 1607 COF Tape 1608 Chip 2000 Touch Panel 2001 Touch Panel 2501 Display device 2502t transistor 2503c Capacitive element 2503t Transistor 2504 Gate line driver circuit 2505 pixels 2509 FPC 2510 Board 2510a Insulating layer 2510b flexible substrate 2510c adhesive layer 2511 Wiring 2519 Terminal 2521 Insulating layer 2528 Bulkhead 2550 EL element 2560 Sealing layer 2567 Colored layer 2568 Light blocking layer 2569 Anti-reflection layer 2570 PCB 2570a Insulating layer 2570b flexible substrate 2570c adhesive layer 2580 Light Emitting Module 2590 Board 2591 Electrode 2592 Electrode 2593 Insulation layer 2594 Wiring 2595 Touch Sensor 2597 Adhesive layer 2598 Wiring 2599 Connection Layer 2601 Pulse voltage output circuit 2602 Current detection circuit 2603 Capacity 2611-2613 Transistor 2621 Electrode 2622 Electrode 5001 Case 5002 Display section 5003 Support stand 5101 Case 5102 Display section 5103 Operation key 5301 Case 5302 Case 5303 Display section 5304 Display section 5305 Microphone 5306 Speaker 5307 Operation key 5308 Stylus 5601 Case 5602 Display section 5701 Case 5702 Display section 5901 Case 5902 Display section 5903 Camera 5904 Speaker 5905 Button 5906 External connection part 5907 Mike

Claims

[Claim 1] a transistor, a first capacitance element, a second capacitance element, and a light emitting element; the transistor has a first gate and a second gate; the first gate and the second gate have an overlapping region with a channel formation region of the transistor therebetween, a first terminal of the transistor is applied with a first potential; a first terminal of the first capacitance element electrically connected to the first gate; a second terminal of the first capacitance element electrically connected to a second terminal of the transistor; a first terminal of the second capacitance element electrically connected to the first gate; a second terminal of the second capacitive element electrically connected to the second gate; a first terminal of the light-emitting element electrically connected to the second terminal of the transistor; A display device according to claim 1, wherein a second terminal of said light-emitting element is given a second potential.

Citation Information

Patent Citations

  • Dual gate field-effect transistor

    JP2004296795A

  • Semiconductor device, light-emitting device, and electronic apparatus

    JP2013077814A

  • Semiconductor device

    JP2015073088A

  • Organic light emitting display device and driving method thereof

    JP2015129934A

  • Indication device

    JP6727909B2