Protective structure for protection from rock falling

The protective structure enhances impact resistance against falling rocks using ultra-high strength fiber-reinforced concrete and buffer materials, addressing space constraints and facilitating component replacement.

JP2024138677APending Publication Date: 2024-10-09TAIHEIYO CEMENT CORP
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2023049273
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-27
Publication Date
2024-10-09

AI Technical Summary

Technical Problem

Existing protective walls against falling rocks face challenges in improving impact resistance without increasing size, which is necessary due to space constraints in mountainous areas.

Method used

A protective structure featuring an impact structure with a front panel made of ultra-high strength fiber-reinforced concrete and a buffer material, such as foam or honeycomb structures, installed on the retaining wall to enhance impact resistance without increasing the wall's size.

Benefits of technology

The structure provides improved impact resistance, allows for easier replacement of damaged components, and prevents localized damage to the retaining wall while maintaining a compact design.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024138677000001_ABST
    Figure 2024138677000001_ABST
Patent Text Reader

Abstract

To provide a rock falling protection structure that has improved impact resistance without increasing dimensions.SOLUTION: A rock falling protection structure 10 has an impact structure 6 attached to a protective surface 2 of a retaining wall 1. The impact structure 6 has a front panel 7 made of ultra-high strength fiber-reinforced concrete, which is a cementitious hardened body with a compressive strength of 150 N / mm2 or more, and a buffer material 8 provided between the front panel 7 and the protective surface 2, and the buffer material 8 is a foam body, or a rubber-shaped body, or a honeycomb structure.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a protective structure for preventing falling rocks, which is installed along mountain roads or the like. [Background technology]

[0002] Traditionally, protective walls have been installed along mountain roads and coastlines as a disaster prevention measure against falling rocks. Most of the protective walls are made of unreinforced concrete, and there is a possibility of localized damage when a falling rock strikes them, so improving the impact resistance of the protective walls has become an issue. In particular, in recent years, the scale of falling rocks has tended to increase due to not only the deterioration of mountain slopes over time but also climate change associated with global warming, making it urgent to find a solution to this problem.

[0003] For example, the protective wall described in Patent Document 1 below (hereinafter referred to as the "Publication 1 Invention") has foam blocks such as polystyrene foam and metal cages filled with soil and sand layered on the mountain side to absorb the impact energy of falling rocks. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2011-84918 A Summary of the Invention [Problem to be solved by the invention]

[0005] If one were to try to improve the impact resistance of the invention described in the first prior art, it would be possible to increase the thickness of the foam block or to strengthen the cage, but if the volume increases, a large space would be required to install the protective wall. In other words, since the place where the wall is to be installed is a narrow place in a mountainous region, it is not possible to install a large wall, and a large wall would also hinder the securing of the space required for installation work.

[0006] The present invention has been proposed in view of the above circumstances, and has an object to provide a rockfall protection structure which has improved impact resistance without being large in size. [Means for solving the problem]

[0007] In order to achieve the above object, the present invention provides a rockfall protection structure, in which an impact structure is installed on a protective surface of a retaining wall against which a colliding object collides, and the impact structure has a resistance to impact of 150N / mm 2 The present invention is characterized by having a front panel made of ultra-high strength fiber reinforced concrete, which is a cementitious hardened body having a compressive strength of at least 1000 g / m2, and a cushioning material installed between the front panel and the protective surface.

[0008] In the rockfall protection structure according to the present invention, the cushioning material is a foam selected from polystyrene foam, urethane foam, polyethylene foam, sponge rubber, silicone foam, and vinyl chloride foam, a rubber-like body selected from chloroprene rubber, butyl rubber, styrene rubber, nitrile rubber, ethylene-propylene rubber, acrylic rubber, urethane rubber, silicone rubber, and natural rubber, or a honeycomb structure made of a material selected from kraft paper, aluminum, and aramid fiber, and the compressive elastic modulus of the cushioning material is 200 to 2000 N / cm 2 The present invention is characterized in that:

[0009] The rockfall protection protective structure according to the present invention is characterized in that the impact structure is located at an upper part of the protection surface.

[0010] The present invention is characterized in that a top panel made of the ultra-high strength fiber reinforced concrete is installed on the top of the retaining wall. Effect of the Invention

[0011] In the rockfall protection structure according to the present invention, an impact structure is provided on the protective surface of the retaining wall against which a colliding object collides, and the impact structure has a resistance to impact of 150N / mm 2The structure has a front panel made of ultra-high-strength fiber-reinforced concrete, a cementitious hardened body with a compressive strength of 10 ...

[0012] The rockfall protection structure according to the present invention has a cushioning material which is a foam selected from polystyrene foam, urethane foam, polyethylene foam, sponge rubber, silicone foam and polyvinyl chloride foam, a rubber-like body selected from chloroprene rubber, butyl rubber, styrene rubber, nitrile rubber, ethylene-propylene rubber, acrylic rubber, urethane rubber, silicone rubber and natural rubber, or a honeycomb structure made of a material selected from kraft paper, aluminum and aramid fiber, and the compressive elastic modulus of the cushioning material is 200 to 2000 N / cm 2 , more preferably 400 to 1000N / cm 2 When the compressive elastic modulus of the cushioning material is within a predetermined range, excellent load dispersion is achieved in the front panel.

[0013] In the rockfall protection structure according to the present invention, the impact structure is located at the upper part of the protection surface. Therefore, it is easier to replace the impact structure compared to when the impact structure is installed on the entire surface of the protection surface. Also, since it is the lower part of the protection surface that is buried in soil and sand, the impact structure located at the upper part of the protection surface can perform its function.

[0014] In the rockfall protection structure of the present invention, a top panel made of ultra-high strength fiber reinforced concrete is installed on the top of the retaining wall. Even if the impact of a colliding object is applied to the protective surface of the retaining wall and cracks reach the top of the retaining wall, localized damage to the top is suppressed by the top panel made of ultra-high strength fiber reinforced concrete. [Brief description of the drawings]

[0015] [Figure 1] 1 is a schematic diagram of a rockfall protection structure according to a first embodiment of the present invention, in which (a) is a cross-section along line II of (b), which is a side cross-sectional view of the rockfall protection structure, and (b) is a front view of the rockfall protection structure. [Diagram 2] FIG. 2 is a schematic cross-sectional side view of a rockfall protection structure according to a second embodiment of the present invention. [Diagram 3] 3 is a schematic diagram of a rockfall protection structure according to a third embodiment of the present invention, in which (a) is a cross-sectional side view of the rockfall protection structure taken along line III-III in (b), and (b) is a front view of the rockfall protection structure. [Figure 4] FIG. 4 is a schematic side cross-sectional view of a rockfall protection structure according to a fourth embodiment of the present invention. [Diagram 5] FIG. 5 is a schematic side cross-sectional view of a rockfall protection structure according to a fifth embodiment of the present invention. [Figure 6] FIG. 6 is a schematic cross-sectional side view of a rockfall protection structure according to a sixth embodiment of the present invention. [Figure 7] FIG. 7 is a schematic side cross-sectional view of a rockfall protection structure according to a seventh embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0016] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS A rockfall protection structure according to an embodiment of the present invention will now be described with reference to the drawings. Fig. 1 shows a rockfall protection structure 10 according to a first embodiment of the present invention.

[0017] As shown in FIG. 1, a rockfall protection structure 10 according to the first embodiment is installed along mountain roads, coastlines, etc. as a disaster prevention measure against rockfalls, and has an impact structure 6 attached to the front of a retaining wall 1. The retaining wall 1 is constructed by cast-in-place concrete or manufactured as precast concrete. The retaining wall 1 is of a gravity type, and is thicker toward the bottom than the top, and is generally trapezoidal in side view (see FIG. 1(a)). The front of the retaining wall 1 is a protection surface 2 against which a falling rock or other impact object is expected to collide, and the back surface of the retaining wall 1 is an opposite surface 3 that slopes toward the back surface toward the bottom. The top surface of the retaining wall 1 is a top surface 4, and the bottom surface of the retaining wall 1 is a foundation surface 5. An impact structure 6 is installed on the protection surface 2.

[0018] The impact structure 6 has a front panel 7 made of ultra-high strength fiber reinforced concrete, and a buffer material 8 installed between the front panel 7 and the protective surface 2. The impact structure 6 is installed over the entire surface of the protective surface 2, and is fixed with anchors 11, anchor plates 12, etc. The thickness of the front panel 7 is 20 to 100 mm, and preferably 30 to 80 mm. The thickness of the buffer material 8 is 100 to 1000 mm, and preferably 200 to 500 mm.

[0019] The cushioning material 8 is a foam, a rubber-like material, or a honeycomb structure. The foam is selected from, for example, polystyrene foam, urethane foam, polyethylene foam, sponge rubber foam, silicone foam, and polyvinyl chloride foam. The rubber is selected from chloroprene rubber, butyl rubber, styrene rubber, nitrile rubber, ethylene-propylene rubber, acrylic rubber, urethane rubber, silicone rubber, and natural rubber. The honeycomb structure is selected from kraft paper, aluminum, and aramid fiber. The compression elastic modulus of the cushioning material 8 is 200 to 2000 N / cm 2 , more preferably 400 to 1000N / cm 2 , and more preferably 450 to 600 N / cm 2 It is.

[0020] Ultra-high strength fiber reinforced concrete is 150N / mm 2The cementitious hardened body has a compressive strength of 15 to 25 m. Specifically, the cement composition used in the cementitious hardened body is cement, a BET specific surface area of ​​15 to 25 m. 2 / g silica fume (hereinafter may be abbreviated as "silica fume"), inorganic powder (hereinafter may be abbreviated as "inorganic powder") having a 50% cumulative particle size of 0.8 to 5 μm, aggregate A having a maximum particle size of 1.2 mm or less, a high-performance water-reducing agent, an antifoaming agent and water, wherein the total amount of cement, silica fume and inorganic powder is 100% by volume, and the proportion of cement is 55 to 65% by volume, the proportion of silica fume is 5 to 25% by volume, and the proportion of inorganic powder is 15 to 35% by volume.

[0021] The type of cement is not particularly limited, and various types of Portland cement can be used, such as ordinary Portland cement, early strength Portland cement, extra early strength Portland cement, moderate heat Portland cement, sulfate resistant Portland cement, low heat Portland cement, etc. Among them, it is preferable to use moderate heat Portland cement or low heat Portland cement from the viewpoint of improving the fluidity of the cement composition.

[0022] The BET specific surface area of ​​silica fume is 15 to 25 m 2 / g, preferably 17 to 23 m 2 / g, particularly preferably 18 to 22m 2 / g. The specific surface area is 15 m 2 If the specific surface area is less than 25 m / g, the strength development of the cement composition is reduced. 2 If it exceeds 1 / g, the fluidity of the cement composition before hardening decreases.

[0023] Examples of inorganic powders having a 50% cumulative particle size of 0.8 to 5 μm include quartz powder (silica powder), volcanic ash, fly ash (classified or crushed), slag powder, limestone powder, feldspar powder, mullite powder, alumina powder, silica sol, carbide powder, nitride powder, crushed emery sand (artificial or natural), etc. These may be used alone or in combination of two or more. Among them, it is preferable to use quartz powder or fly ash from the viewpoint of improving the fluidity and strength development of the cement composition. In this specification, the inorganic powder having a 50% cumulative particle size of 0.8 to 5 μm does not include cement.

[0024] The 50% cumulative particle size of the inorganic powder is 0.8 to 5 μm, preferably 1 to 4 μm, more preferably 1.1 to 3.5 μm, and particularly preferably 1.2 μm or more and less than 3 μm. When the particle size is less than 0.8 μm, the flowability of the cement composition decreases. When the particle size is more than 5 μm, the strength development of the cement composition decreases. In this specification, the 50% cumulative particle size of the inorganic powder is based on volume. The 50% cumulative particle size of the inorganic powder can be determined using a commercially available particle size distribution measuring device (for example, Nikkiso Co., Ltd., product name "Microtrac HRA Model 9320-X100"). Specifically, a cumulative particle size curve is created using the particle size distribution measuring device, and the 50% cumulative particle size can be determined from the cumulative particle size curve. In this case, 20 cm of ethanol, which is a solvent for dispersing the sample, is added to the sample. 3 0.06 g of a sample is added to each of the samples, and the mixture is ultrasonically dispersed for 90 seconds using an ultrasonic dispersing device (for example, product name "US300" manufactured by Nippon Seiki Seisakusho Co., Ltd.), and then the measurement is performed.

[0025] The maximum particle size of the inorganic powder is preferably 15 μm or less, more preferably 14 μm or less, and particularly preferably 13 μm or less, from the viewpoint of improving the strength development of the cement composition. The 95% cumulative particle size of the inorganic powder is preferably 8 μm or less, more preferably 7 μm or less, and particularly preferably 6 μm or less, from the viewpoint of improving the strength development of the cement composition.

[0026] The inorganic powder is preferably one containing SiO2 as a main component. If the content of SiO2 in the inorganic powder is preferably 50 mass% or more, more preferably 60 mass% or more, and particularly preferably 70 mass% or more, the strength development of the cement composition can be further improved.

[0027] In the cement composition, the proportion of cement is 55-65 volume % (preferably 57-63 volume %), the proportion of silica fume is 5-25 volume % (preferably 7-23 volume %), and the proportion of the inorganic powder is 15-35 volume % (preferably 17-33 volume %) in the total amount of cement, silica fume, and the inorganic powder, which is 100 volume %. When the proportion of cement is less than 55 volume %, the strength development of the cement composition is reduced. When the proportion of cement is more than 65 volume %, the fluidity of the cement composition is reduced. When the proportion of silica fume is less than 5 volume %, the strength development of the cement composition is reduced. When the proportion of silica fume is more than 25 volume %, the fluidity of the cement composition is reduced. When the proportion of the inorganic powder is less than 15 volume %, the strength development of the cement composition is reduced. When the proportion of the inorganic powder is more than 35 volume %, the fluidity of the cement composition is reduced.

[0028] Examples of aggregate A include river sand, mountain sand, land sand, sea sand, crushed sand, silica sand, natural emery sand, artificial fine aggregate (for example, slag fine aggregate, burned fine aggregate obtained by burning fly ash, etc., artificial emery sand, coarsely crushed alumina or carbide (for example, silicon carbide, boron carbide), etc.), recycled fine aggregate, and mixtures thereof. The maximum particle size of aggregate A is 1.2 mm or less, preferably 1.1 mm or less, and more preferably 1.0 mm or less. If the maximum particle size is 1.2 mm or less, the strength development of the cement composition can be further improved, and the strength development of the cement composition can be improved to 300 N / mm 2 or more (preferably 400N / mm 2In some cases, the aggregate A can exhibit a compressive strength of 0.6 mm or less (or more). From the viewpoint of improving the fluidity and strength development of the cement composition, the particle size distribution of the aggregate A is preferably such that the ratio of aggregates having a particle size of 0.6 mm or less is 95% by mass or more, the ratio of aggregates having a particle size of 0.3 mm or less is 40 to 50% by mass, and the ratio of aggregates having a particle size of 0.15 mm or less is 6% by mass or less. The ratio of the aggregate A in the cement composition is preferably 20 to 40% by volume, more preferably 22 to 39% by volume, even more preferably 25 to 38% by volume, even more preferably 30 to 37% by volume, and particularly preferably 32 to 36% by volume. If the ratio is 20% by volume or more, the fluidity of the cement composition can be improved, the heat generation amount of the cement composition can be reduced, and the shrinkage amount of the cementitious hardened body can be reduced. If the ratio is 40% by volume or less, the strength development of the cement composition can be improved.

[0029] As the high-performance water reducing agent, a naphthalenesulfonic acid-based, melamine-based, polycarboxylic acid-based, or other high-performance water reducing agent can be used. Among them, a polycarboxylic acid-based high-performance water reducing agent is preferred from the viewpoint of improving the fluidity and strength development of the cement composition. The amount of the high-performance water reducing agent is preferably 0.2 to 1.5 parts by mass, more preferably 0.4 to 1.2 parts by mass, calculated as solid content, relative to 100 parts by mass of the total amount of cement, silica fume, and inorganic powder. If the amount is 0.2 parts by mass or more, the water reducing performance is improved and the fluidity of the cement composition is improved. If the amount is 1.5 parts by mass or less, the strength development of the cement composition is improved.

[0030] As the defoaming agent, a commercially available product can be used. The amount of the defoaming agent is preferably 0.001 to 0.1 parts by mass, more preferably 0.01 to 0.07 parts by mass, and particularly preferably 0.01 to 0.05 parts by mass, relative to 100 parts by mass of the total amount of cement, silica fume, and inorganic powder. If the amount is 0.001 parts by mass or more, the strength development of the cement composition is improved. If the amount exceeds 0.1 parts by mass, the effect of improving the strength development of the cement composition reaches a plateau.

[0031] The cement composition does not usually contain glass fibers from the viewpoint of avoiding a decrease in long-term strength. The cement composition may contain one or more fibers selected from the group consisting of metal fibers, organic fibers, and carbon fibers from the viewpoint of improving the bending strength, fracture energy, etc. of a hardened body (cementitious hardened body) obtained by hardening the cement composition. The ratio of fibers in the cement composition is preferably 3 volume % or less, more preferably 0.3 to 2.5 volume %, further preferably 0.4 to 2.3 volume %, and particularly preferably 0.5 to 2.0 volume %. When the ratio is 3 volume % or less, the bending strength, fracture energy, etc. of the hardened body can be improved without decreasing the fluidity and workability of the cement composition.

[0032] Examples of metal fibers include steel fibers, stainless steel fibers, and amorphous fibers. Among them, steel fibers are preferred in terms of excellent strength, cost, and availability. The dimensions of the metal fibers are preferably 0.01 to 1.0 mm in diameter and 2 to 30 mm in length, more preferably 0.05 to 0.5 mm in diameter and 5 to 25 mm in length, from the viewpoints of preventing material separation of the metal fibers in the cement composition and improving the bending strength of the hardened body. The aspect ratio of the metal fibers (fiber length / fiber diameter) is preferably 20 to 200, more preferably 40 to 150. Furthermore, the shape of the metal fibers is preferably a shape that imparts some kind of physical adhesion (for example, a spiral or wavy shape) rather than a straight shape. If the shape is a spiral shape, the metal fibers and the matrix secure stress while being pulled out, improving the bending strength of the hardened body.

[0033] The organic fibers may be any fibers that can withstand heating in the manufacturing method of the cementitious hardened body described below, and examples thereof include aramid fibers, polyparaphenylene benzobisoxazole fibers, polyethylene fibers, polyallylate fibers, polypropylene fibers, etc. Examples of carbon fibers include PAN-based carbon fibers and pitch-based carbon fibers. The dimensions of the organic fibers and carbon fibers are preferably 0.005 to 1.0 mm in diameter and 2 to 30 mm in length, more preferably 0.01 to 0.5 mm in diameter and 5 to 25 mm in length, from the viewpoints of preventing material separation of these fibers in the cement composition and improving the fracture energy of the hardened body. The aspect ratio (fiber length / fiber diameter) of the organic fibers and carbon fibers is preferably 20 to 200, more preferably 30 to 150.

[0034] As the water, tap water or the like can be used. The amount of water is preferably 10 to 20 parts by mass, more preferably 12 to 18 parts by mass, and particularly preferably 14 to 16 parts by mass, relative to 100 parts by mass of the total amount of cement, silica fume, and inorganic powder. When the amount is 10 parts by mass or more, the fluidity of the cement composition is improved. When the amount is 20 parts by mass or less, the strength development of the cement composition is improved.

[0035] The flow value before hardening of the mortar made of the above cement composition (not containing aggregate B described later) is preferably 200 mm or more, more preferably 210 mm or more, and particularly preferably 220 mm or more, as measured without performing the 15 drop motions in the method described in "JIS R 5201 (Physical Testing Methods for Cement) 11. Flow Test" (hereinafter also referred to as "zero drop flow value"). In addition, the compressive strength of the cementitious hardened body obtained by hardening the mortar made of the above cement composition (not containing aggregate B described later) is preferably 320 N / mm 2 More preferably, 350N / mm 2 More preferably, 400N / mm 2 More than 450N / mm 2In addition, in the case of a mortar (not including aggregate B described later) made of a cement composition using aggregate A having a modified Mohs hardness of 9 or more (preferably 9 to 14, more preferably 9 to 13, even more preferably 10 to 13, and particularly preferably 11 to 13) (for example, natural or artificial (man-made) emery sand, coarsely crushed alumina or carbide, etc.), the hardness of the mortar is 450 N / mm 2 or more (especially when using emery sand, 500N / mm 2 It is possible to achieve a compressive strength of 100% or more.

[0036] The cement composition may contain aggregate B having a maximum particle size of more than 1.2 mm and not more than 13 mm. Examples of aggregate B include river sand, mountain sand, land sand, sea sand, crushed sand, silica sand, natural emery sand, artificial fine aggregate (e.g., artificial emery sand, slag fine aggregate, and burned fine aggregate obtained by burning fly ash, etc.), recycled fine aggregate, river gravel, mountain gravel, land gravel, crushed stone, artificial coarse aggregate (e.g., burned coarse aggregate obtained by burning slag coarse aggregate, and fly ash, etc.), recycled coarse aggregate, and mixtures thereof. The maximum particle size of aggregate B is 13 mm or less, preferably 12 mm or less, more preferably 11 mm or less, and particularly preferably 10 mm or less. If the maximum particle size is 13 mm or less, the strength development of the cement composition is improved, and the strength development of the cement composition is improved, for example, to 300 N / mm 2 or more. From the viewpoint of cost reduction and the like, the maximum particle size of aggregate B is a value exceeding 1.2 mm, and is preferably 3 mm or more, more preferably 5 mm or more, and particularly preferably 7 mm or more. In this specification, the "maximum particle size" in the case where aggregate B has a maximum particle size of 5 mm or more means the particle size of aggregate B indicated by the nominal size of the smallest sieve among sieves through which 90% by mass or more of the entire aggregate B passes (generally known as the definition of the maximum particle size of coarse aggregate).

[0037] The minimum particle size of aggregate B is preferably a value exceeding the maximum particle size of aggregate A, more preferably 2 mm or more, even more preferably 3 mm or more, even more preferably 4 mm or more, and particularly preferably 5 mm or more (in this case, it corresponds to coarse aggregate). In this specification, the minimum particle size of aggregate B refers to the particle size of aggregate B when it reaches 15% by mass of the entire aggregate B when accumulating from the smallest particle size to the larger particle sizes in aggregate B.

[0038] The ratio of the total amount of aggregate A and aggregate B in the cement composition is preferably 25 to 40 volume %, more preferably 30 to 38 volume %, and particularly preferably 32 to 36 volume %. When the ratio is 25 volume % or more, the heat generation amount of the cement composition is small, and the shrinkage amount of the cementitious hardened body is small. When the ratio is 40 volume % or less, the strength development of the cement composition can be improved. The ratio of aggregate B to the total amount of aggregate A and aggregate B is preferably 40 volume % or less, more preferably 30 volume % or less. When the ratio is 40 volume % or less, the strength development (e.g., compressive strength) of the cement composition can be improved. The compressive strength of the cementitious hardened body obtained by hardening the cement composition (e.g., concrete) containing aggregate B is preferably 300 N / mm 2 More preferably, 320N / mm 2 More preferably, 340N / mm 2 That's all.

[0039] A method for producing a cementitious hardened body obtained by hardening a cement composition will be described in detail below. An example of the method for producing a cementitious hardened body includes a molding step of casting the above-mentioned cement composition into a formwork to obtain an unhardened molded body, a room temperature curing step of subjecting the unhardened molded body to sealed curing or air curing at 10 to 40°C for 24 hours or more, and then removing it from the formwork to obtain a hardened molded body, a heat curing step of subjecting the hardened molded body to steam curing or hot water curing at 70°C or more and less than 100°C for 1 hour or more, and / or autoclave curing at 100 to 200°C for 1 hour or more to obtain a hardened body after heat curing, and a high temperature heating step of heating the hardened body after heat curing at 150 to 200°C for 24 hours or more (excluding heating by autoclave curing) to obtain a cementitious hardened body.

[0040] [Molding process] This step is a step of casting the cement composition into a formwork to obtain an unhardened molded body. The method of kneading the cement composition of the present invention before casting is not particularly limited. The device used for kneading is also not particularly limited, and a conventional mixer such as an omni mixer, a pan mixer, a biaxial mixer, or a tilting mixer can be used. Furthermore, the casting (molding) method is also not particularly limited. The unhardened molded body in this step may be made of a cement composition in which air bubbles in the cement composition have been reduced or removed. By reducing or removing air bubbles in the cement composition, the strength development of the cement composition can be further improved. Examples of the method of reducing or removing air bubbles in the cement composition include (1) a method of kneading the cement composition under reduced pressure, (2) a method of degassing the kneaded cement composition by reducing the pressure before casting it into a formwork, and (3) a method of degassing the cement composition by reducing the pressure after casting it into a formwork.

[0041] [Room temperature curing process] This step involves subjecting the unhardened molded body to sealed curing or air curing at 10 to 40°C (preferably 15 to 30°C) for 24 hours or more (preferably 24 to 72 hours, more preferably 24 to 48 hours), and then removing it from the formwork to obtain a hardened molded body. If the curing temperature is 10°C or higher, the curing time can be shortened. If the curing temperature is 40°C or lower, the compressive strength of the cementitious hardened body can be improved. If the curing time is 24 hours or longer, defects such as chips and cracks are less likely to occur in the hardened molded body when it is removed from the form. Furthermore, in this step, the hardened molded body preferably has a compressive strength of 20 to 100 N / mm 2 , more preferably 30 to 80N / mm 2 When the compressive strength reaches 20 N / mm, the cured molded body is preferably removed from the mold. 2 If the compressive strength is 100 N / mm or more, defects such as chipping or cracking are unlikely to occur in the hardened molded body when it is demolded. 2 If the above condition is met, the hardened molded body can absorb water with little effort in the water absorption step described below.

[0042] [Heat curing process] This step is a step of subjecting the cured molded body obtained in the previous step to steam curing or hot water curing at 70°C or higher but lower than 100°C (preferably 75 to 95°C, more preferably 80 to 92°C) for 1 hour or more, and autoclave curing at 100 to 200°C (preferably 160 to 190°C) for 1 hour or more, or both, to obtain a cured body after heat curing. When only steam curing or hot water curing is performed in this step, the curing time is preferably 12 hours or more, more preferably 24 to 96 hours, and particularly preferably 36 to 72 hours. When only autoclave curing is performed, the curing time is preferably 2 hours or more, more preferably 3 to 60 hours, and particularly preferably 4 to 48 hours. When both steam curing or hot water curing and autoclave curing are performed (for example, when steam curing or hot water curing is performed and then autoclave curing is performed), the curing time in steam curing or hot water curing is preferably 1 to 72 hours, more preferably 2 to 48 hours, and the curing time in autoclave curing is preferably 1 to 24 hours, more preferably 2 to 18 hours. In this step, if the curing temperature is within the above range, the curing time can be shortened and the compressive strength of the cementitious hardened body can be improved. In addition, in this step, if the curing time is within the above range, the compressive strength of the cementitious hardened body can be improved.

[0043] [High temperature heating process] This step is a step of heating (excluding heating by autoclave curing) the hardened body after heat curing at 150 to 200°C (preferably 170 to 190°C) for 24 hours or more (preferably 24 to 72 hours, more preferably 36 to 48 hours) to obtain a cementitious hardened body. The heating in this step is usually performed in a dry atmosphere (in other words, in a state where water or water vapor is not artificially supplied). When the heating temperature is 150°C or higher, the heating time can be shortened. When the heating temperature is 200°C or lower, the compressive strength of the cementitious hardened body can be improved. When the heating time is 24 hours or more, the compressive strength of the cementitious hardened body can be improved.

[0044] [Water absorption process] Between the room temperature curing step and the heat curing step, a water absorbing step may be included in which the hardened molded body obtained in the room temperature curing step is made to absorb water. As a method for making the hardened molded body absorb water, a method of immersing the molded body in water may be mentioned. In addition, in the method of immersing the molded body in water, from the viewpoint of increasing the amount of water absorption in a short time and increasing the compressive strength of the cementitious hardened body, the following method is preferable: (1) a method of immersing the molded body in water under reduced pressure, (2) a method of immersing the molded body in boiling water, and then lowering the water temperature to 40°C or less while the molded body is immersed, (3) a method of immersing the molded body in boiling water, and then removing the molded body from the boiling water and then immersing the molded body in water at 40°C or less, (4) a method of immersing the molded body in water under pressure, or (5) a method of immersing the molded body in an aqueous solution in which an agent for improving the water permeability of the molded body is dissolved.

[0045] The above-mentioned molded body can be immersed in water under reduced pressure using equipment such as a vacuum pump or a large reduced pressure vessel. The above-mentioned molded body can be immersed in boiling water using equipment such as a high-temperature high-pressure vessel or a hot water tank. The time for which the hardened molded body is immersed in water under reduced pressure or boiling water is preferably 3 minutes or more, more preferably 8 minutes or more, and particularly preferably 20 minutes or more, from the viewpoint of increasing the water absorption rate. The upper limit of the time is preferably 60 minutes, more preferably 45 minutes, from the viewpoint of increasing the compressive strength of the cementitious hardened body.

[0046] The water absorption rate in the water absorption step is preferably 0.2% by volume or more, more preferably 0.3 to 2.0% by volume, and particularly preferably 0.35 to 1.7% by volume, as a ratio of water to 100% by volume of a hardened molded body of φ50×100 mm, when the cement composition does not contain a coarse aggregate (when the cement composition does not contain aggregate B, or when aggregate B in the cement composition does not correspond to a coarse aggregate), and is preferably 0.2% by volume or more, more preferably 0.3 to 2.0% by volume, and particularly preferably 0.35 to 1.7% by volume, as a ratio of water to 100% by volume of a hardened molded body of φ100×200 mm, when the cement composition contains a coarse aggregate (when aggregate B in the cement composition corresponds to a coarse aggregate). If these water absorption rates are 0.2% by volume or more, the compressive strength of the cementitious hardened body can be further increased.

[0047] As described above, the front panel 7 of the impact structure 6 has higher strength characteristics than general concrete, improving the impact resistance of the rockfall protection structure 10. In addition, the high strength characteristics allow the thickness to be reduced, eliminating the need for excessive surface layer material. When the front panel 7 is damaged, it can be replaced. In addition, the compressive elastic modulus of the buffer material 8 is within a predetermined numerical range (200 to 2000 N / cm 2 , more preferably 400 to 1000N / cm 2 , and more preferably 450 to 600 N / cm 2 ) provides excellent load distribution in the front panel 7 and prevents damage to the concrete portion of the retaining wall 1.

[0048] Next, other embodiments of the present invention will be described with reference to the drawings. Fig. 2 shows a rockfall protection structure 20 according to a second embodiment, Fig. 3 shows a rockfall protection structure 30 according to a third embodiment, Fig. 4 shows a rockfall protection structure 40 according to a fourth embodiment, Fig. 5 shows a rockfall protection structure 50 according to a fifth embodiment, Fig. 6 shows a rockfall protection structure 60 according to a sixth embodiment, and Fig. 7 shows a rockfall protection structure 70 according to a seventh embodiment. In the following, mainly the configurations different from the first embodiment will be described, and the description of the same configurations as the first embodiment will be omitted as appropriate.

[0049] 2, the rockfall protection structure 20 according to the second embodiment differs from the rockfall protection structure 10 according to the first embodiment in that it has piles 13 driven into the supporting layer. This embodiment also has the same effects as the rockfall protection structure 10, and the shape of the retaining wall 21 can be a rectangular parallelepiped.

[0050] As shown in Figure 3, the rockfall protection protective structure 30 of the third embodiment differs from the rockfall protection protective structure 10 of the first embodiment in that the impact structure 36 is installed only on the upper part of the protective surface 32 of the retaining wall 31, and not on the lower part, so that the protective surface 32 is exposed on the lower part.

[0051] The impact structure 36 is approximately the size of the upper half of the protective surface 32, and is installed, for example, via a steel jig 14. In this case, anchors or the like for fixing the impact structure 36 to the protective surface 32 are not required. The steel jig 14 is made of shaped steel or the like, and has a side frame 15 extending along the side edge of the impact structure 36 and a lower frame 16 extending along the lower edge of the impact structure 36. Even in this embodiment, the same effect as the rockfall protection structure 10 is achieved, and the impact structure 36 is easier to replace than the rockfall protection structure 10 in which the impact structure 6 is installed over the entire surface of the protective surface 2. In addition, since the lower part of the protective surface 32 is buried by soil and sand, the impact structure 36 located at the upper part of the protective surface 32 can function against falling rocks.

[0052] As shown in Fig. 4, the rockfall protection structure 40 according to the fourth embodiment differs from the rockfall protection structure 10 according to the first embodiment in that a top panel 49 made of ultra-high strength fiber reinforced concrete is installed on the top surface 44 of the retaining wall 41. The top panel 49 is fixed to the top surface 44 by anchors or adhesives, and no buffer material 48 is installed between the top panel 49 and the top surface 44. This embodiment also has the same effect as the rockfall protection structure 10, and even if the impact of a colliding object is applied to the protection surface 42 and cracks reach the top surface 44, localized damage to the top surface 44 is suppressed by the top panel 49.

[0053] As shown in FIG. 5, the rockfall protection structure 50 according to the fifth embodiment differs from the rockfall protection structure 10 according to the first embodiment in that a top panel 59 made of ultra-high strength fiber reinforced concrete is installed on the top surface 54 of the retaining wall 51 and the upper surface of the impact structure 56. As with the rockfall protection structure 40 according to the fourth embodiment, the top panel 59 is fixed to the top surface 54 by anchors or adhesives, and no buffer material 58 is installed between the top panel 59 and the top surface 54. This embodiment also has the same effect as the rockfall protection structure 10, and as with the rockfall protection structure 40, even if the impact of the colliding object is applied to the protection surface 52 and cracks reach the top surface 54, the top panel 59 suppresses local damage to the top surface 54, and the front panel 57 and the buffer material 58 are also suppressed from protruding from the top surface 54 side. In a modification of this embodiment, if the top panel 59 is firmly fixed to the top surface 54 with anchors or the like, the front panel 57 may be fixed with an adhesive or the like without requiring anchors or the like. If the top panel 59 and the front panel 57 are integrated with each other by adhesion or the like and firmly fixed to the top surface 54 with anchors or the like, the number of anchors or the like required will be reduced and replacement of the impact structure 56 will be easier.

[0054] 6, the rockfall protection structure 60 according to the sixth embodiment differs from the rockfall protection structure 10 according to the first embodiment in that, like the rockfall protection structure 30 according to the third embodiment, the impact structure 66 is installed only on the upper part of the protection surface 62 of the retaining wall 61, not on the lower part, so that the protection surface 62 is exposed on the lower part, and in that, like the rockfall protection structure 40 according to the fourth embodiment, a top panel 69 made of ultra-high strength fiber reinforced concrete is installed on the top surface 64 of the retaining wall 61. The impact structure 66 is installed via a steel jig 14.

[0055] This embodiment also has the same effect as the rockfall protection structure 10, and compared to the rockfall protection structure 10 in which the impact structure 6 is installed over the entire surface of the protection surface 2, like the rockfall protection structure 30, the impact structure 66 can be easily replaced. Also, like the rockfall protection structure 30, it is the lower part of the protection surface 62 that is buried in soil and sand, so the impact structure 66 on the upper part of the protection surface 62 can function against falling rocks. Also, like the rockfall protection structure 40, even if the impact of a colliding object is applied to the protection surface 62 and cracks reach the top surface 64, local destruction of the top surface 64 is suppressed by the top panel 69.

[0056] In the modified rockfall protection structure 60, a top panel 69 is installed on the top surface 64 of the retaining wall 61 and the upper surface of the impact structure 66, as in the rockfall protection structure 50 according to the fifth embodiment. In this case, the top panel 69 and the front panel 67 may be integrated together. In this case, if the top panel 69 is firmly fixed to the top surface 64 with anchors or the like, the front panel 67 may be fixed with an adhesive or the like without requiring anchors or the like.

[0057] As shown in Fig. 7, the rockfall protection structure 70 according to the seventh embodiment differs from the rockfall protection structure 10 according to the first embodiment in that it has piles 13 driven into the support layer, like the rockfall protection structure 20 according to the second embodiment, and that a top panel 79 made of ultra-high strength fiber reinforced concrete is installed on the top surface 74 of the retaining wall 71, like the rockfall protection structure 40 according to the fourth embodiment. This embodiment also has the same effects as the rockfall protection structure 10, and like the rockfall protection structure 20, it is possible to make the shape of the retaining wall 71 a rectangular parallelepiped, and like the rockfall protection structure 40, even if the impact of a colliding object is applied to the protection surface 72 and cracks reach the top surface 74, local damage to the top surface 74 is suppressed by the top panel 79.

[0058] In the modified rockfall protection structure 70, a top panel 79 is installed on the top surface 74 of the retaining wall 71 and the upper surface of the impact structure 76, as in the rockfall protection structure 50 according to the fifth embodiment. In this case, the top panel 79 and the front panel 77 may be integrated together. In this case, if the top panel 79 is firmly fixed to the top surface 74 with anchors or the like, the front panel 77 may be fixed with an adhesive or the like without requiring anchors or the like.

[0059] Next, an embodiment of the present invention will be described.

[0060] In the ultra-high strength fiber reinforced concrete of the embodiment, the cement composition had a water-binder ratio (W / B) of 14%, and the steel fiber mixing ratio was 3.0% by volume. The compressive strength was 311 N / mm 2 The compressive elastic modulus of the examples was 200 N / cm 2 , 500N / cm 2 , 850N / cm 2 , 2000N / cm 2The retaining wall had a width of 3000 mm, a height of 2000 mm, and a depth of 1300 mm. The thicknesses of the front panel were 20 mm, 50 mm, and 100 mm, and the thicknesses of the cushioning material were 100 mm, 250 mm, and 1000 mm. The front panel was installed on the protection surface and the top surface. The cushioning material was installed only on the protection surface. When installed on the protection surface, it was fixed with a steel jig (sixth embodiment, see Figure 6). The comparative example did not have an impact structure and was only a retaining wall.

[0061] [Table 1]

[0062] A weight was collided with the protective surfaces (impact structures) of the retaining walls of Examples 1 to 9 and the protective surface of the comparative example. The weight was made of steel with a mass of 890 kg, and was cylindrical with a diameter of 500 mm and a total length of 690 mm. The weight was collided with the retaining wall by a pendulum motion using two cranes, and the drop height was 10 m. As a result of the experiment, the comparative example, which was not reinforced, was damaged by the action of the collision load, and cracks developed up, down, left and right from the collision position, and cracks occurred beyond the center of half of the retaining wall, resulting in a destroyed state. On the other hand, in the examples, the destruction of the retaining wall could be prevented by reinforcing the protective surface with the impact structure.

[0063] Although the embodiment of the present invention has been described in detail above, the present invention is not limited to the above embodiment, and various design modifications can be made to the present invention without departing from the scope of the claims. [Explanation of symbols]

[0064] 1, 21, 31, 41, 51, 61, 71 Retaining wall 2, 22, 32, 42, 52, 62, 72 Protective surface 3, 23, 33, 43, 53, 63, 73 Opposite side 4, 24, 34, 44, 54, 64, 74 Top surface 5, 25, 35, 45, 55, 65, 75 Foundation surface 6, 26, 36, 46, 56, 66, 76 Impact Structure 7, 27, 37, 47, 57, 67, 77 Front Panel 8, 28, 38, 48, 58, 68, 78 buffer material 10, 20, 30, 40, 50, 60, 70 Protective structures for rockfall protection 11. Anchor 12 Anchor plate 13 stake 14 Steel Jig 15 Side frame 16 Lower frame 49, 59, 69, 79 Top panel

Claims

1. An impact structure is installed on the protective surface of the retaining wall where the colliding object will collide. The impact structure, 150N / mm 2 A front panel of ultra-high strength fiber reinforced concrete, which is a cementitious hardened body having a compressive strength of at least 1000 mm; A cushioning material is provided between the front panel and the protective surface. A rockfall protection structure characterized by the above.

2. The cushioning material is a foam selected from the group consisting of polystyrene foam, urethane foam, polyethylene foam, sponge rubber foam, silicone foam, and vinyl chloride foam; A rubber-like material selected from chloroprene rubber, butyl rubber, styrene rubber, nitrile rubber, ethylene-propylene rubber, acrylic rubber, urethane rubber, silicone rubber, and natural rubber, or A honeycomb structure made of one material selected from kraft paper, aluminum, and aramid fiber; The compressive elastic modulus of the buffer material is 200 to 2000 N / cm 2 That is, 2. A rockfall protection structure according to claim 1.

3. The impact structure is located at an upper portion of the protective surface.

3. A rockfall protection structure according to claim 1 or 2.

4. The top panel of the ultra-high strength fiber reinforced concrete was installed on the top of the retaining wall.

3. A rockfall protection structure according to claim 1 or 2.

Citation Information

Patent Citations

  • Styrofoam protective structure for rockfall prevention protective structure

    JP1991093815U

  • Member for protection work of road or railroad, and method for producing the same

    JP2017226547A

  • Rockfall preventive guard structure

    JP2011084918A