Wafer grinding method
The wafer grinding method uses surfactant-containing grinding water to prevent debris adhesion by utilizing a mixed fluid of water and air, addressing contamination issues and maintaining a cost-effective, uncomplicated device structure.
Patent Information
- Application Number
- JP2023049859
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-27
- Publication Date
- 2024-10-09
AI Technical Summary
Existing wafer grinding methods result in grinding debris adhering to the non-grinding surface due to the entry of grinding waste into the chuck table, leading to contamination, and require complex cleaning units that increase cost and inefficiency.
A wafer grinding method that involves holding one side of the wafer on a chuck table, supplying grinding water containing a surfactant to the wafer and grinding wheel, and using a mixed fluid of water and air to separate the wafer, effectively preventing debris adhesion by incorporating a surfactant into the grinding process.
The method effectively prevents debris adhesion to the wafer surface without the need for a dedicated cleaning unit, maintaining a simple device structure and avoiding cost increases.
Smart Images

Figure 2024139067000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a wafer grinding method for grinding a wafer held on a chuck table. [Background technology]
[0002] For example, wafers used in the manufacture of semiconductor devices such as ICs and LSIs used in electronic devices are obtained by flattening both sides of as-sliced wafers cut from single crystal ingots of silicon or the like by a cutting device such as a blade saw or a wire saw using a grinding device or a polishing device. Devices such as ICs and LSIs are then formed on the front surface of the wafer thus flattened on both sides, the back surface of the wafer on which these devices are formed is ground to thin the wafer to a predetermined thickness, and the thinned wafer is cut by a dicing saw or the like to separate it into individual devices.
[0003] Incidentally, an as-sliced wafer cut from an ingot has warpage due to differences in the magnitude of processing strain that occurs on both sides during cutting processing using a cutting device such as a blade saw, and undulations that occur on the surface layers of both sides. For this reason, Patent Document 1 proposes a processing method in which a protective member such as an ultraviolet curing resin is formed on one side of the as-sliced wafer to flatten the surface, one flat side of the protective member is held by a holding surface of a chuck table while the other side of the as-sliced wafer is ground to flatten the other side, and then the protective member is peeled off from the as-sliced wafer, and one side of the as-sliced wafer is ground to flatten the other side while the other flat side is held by a holding surface of a chuck table.
[0004] However, the grinding process of as-sliced wafers (hereinafter simply referred to as "wafers") by the above-mentioned processing method is performed while supplying grinding water to the grinding area, but grinding debris generated by grinding one side of the wafer enters the chuck table together with the grinding water through a gap between the other side of the wafer and the holding surface of the chuck table. When a mixed fluid of water and air is sprayed from the chuck table to remove the wafer from the chuck table after grinding, the grinding water that has entered the chuck table and the grinding debris contained therein are sprayed out together with the mixed fluid, and the sprayed grinding debris adheres to the other side of the wafer, causing a problem of contaminating the other side.
[0005] Therefore, Patent Document 2 proposes a processing apparatus that cleans the lower surface of a workpiece such as a wafer by using a cleaning unit that includes a roll sponge that rotates while receiving a supply of cleaning water. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] JP 2011-249652 A [Patent Document 2] JP 2020-145256 A Summary of the Invention [Problem to be solved by the invention]
[0007] However, providing a separate cleaning unit as proposed in Patent Document 2 complicates the structure of the processing apparatus, leading to increased costs, and also poses the problem of reduced efficiency as cleaning takes a long time.
[0008] The present invention has been made in consideration of the above problems, and an object of the present invention is to provide a wafer grinding method that does not require a dedicated cleaning unit, does not complicate the structure, and does not increase costs, and can prevent adhesion of grinding debris to the wafer. [Means for solving the problem]
[0009] In order to solve the above-mentioned problems, the present invention is a wafer grinding method for grinding a wafer, comprising: a holding step of holding one side of the wafer on a chuck table; a grinding step of supplying grinding water containing a surfactant to the wafer and a grinding wheel and grinding the other side of the wafer with the grinding wheel; and a separating step of spraying a mixed fluid of water and air from the chuck table to separate the wafer from the chuck table. Effect of the Invention
[0010] According to the present invention, when one side of the wafer held on the chuck table in the holding step is ground in the next grinding step, grinding water containing a surfactant is supplied to the wafer and the grinding wheel, so that the grinding water containing the grinding chips generated by grinding the other side of the wafer is sucked into the chuck table. Then, when a mixed fluid of water and air is ejected from the chuck table in the next separating step, the grinding chips and the grinding water sucked into the chuck table during grinding are ejected from the chuck table together with the mixed fluid, but since the grinding water contains a surfactant, adhesion of the grinding chips to the one side of the wafer can be suppressed. And, since such an effect can be obtained by simply adding a surfactant to the grinding water, a dedicated cleaning unit is not required, and the structure of the grinding device is not complicated and the cost is not increased. [Brief description of the drawings]
[0011] [Figure 1] 1 is a perspective view showing, in a partially cutaway form, a grinding apparatus for carrying out a wafer grinding method according to the present invention; [Diagram 2] 1 is a block diagram showing the steps of a wafer grinding method according to the present invention in order. [Diagram 3] 3(a) to 3(e) are side cross-sectional views sequentially showing protective member forming steps in the wafer grinding method according to the present invention. [Figure 4] 2 is a side cross-sectional view showing a first grinding step in the wafer grinding method according to the present invention. FIG. [Diagram 5] 5(a) and 5(b) are side cross-sectional views showing a separating step of separating a first ground wafer from a chuck table in the wafer grinding method according to the present invention. [Figure 6] 5(a) to 5(c) are side cross-sectional views showing a peeling step in the wafer grinding method according to the present invention. [Figure 7] 5(a) and 5(b) are side cross-sectional views showing a reversing step in the wafer grinding method according to the present invention. [Figure 8] 2 is a side cross-sectional view showing a first grinding step in the wafer grinding method according to the present invention. FIG. [Figure 9] 5(a) and 5(b) are side cross-sectional views showing a separating step of separating the second ground wafer from the chuck table in the wafer grinding method according to the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] Hereinafter, an embodiment of the present invention will be described with reference to the accompanying drawings.
[0013] [Grinding equipment configuration] First, the configuration of a grinding device for carrying out a grinding method according to the present invention will be described with reference to Fig. 1. In the following description, the directions of the arrows shown in Fig. 1 are the X-axis direction (left-right direction), the Y-axis direction (front-back direction), and the Z-axis direction (up-down direction), respectively.
[0014] The grinding apparatus 1 shown in Fig. 1 is an apparatus for grinding disk-shaped wafers (see Figs. 3 to 9) that are workpieces, and includes, as main components, three chuck tables 10 arranged on a rotatable disk-shaped turntable 2, a rough grinding unit (first grinding unit) 20 and a finish grinding unit (second grinding unit) 30 that are grinding units for grinding the wafers W held on the chuck tables 10, and a grinding water supply unit 40 that supplies grinding water to the grinding area of the wafers W held on the chuck tables 10. Here, the wafers W are as-sliced wafers cut from a cylindrical ingot, and have warpage due to differences in the magnitude of processing strain generated on both sides and waviness generated on the surface layers of both sides.
[0015] Other components of the grinding apparatus 1 include thickness gauges 51, 52 for measuring the thickness of the wafer W during grinding, a cleaning unit 50 for cleaning the ground wafer W, a peeling device 70 for peeling off the protective material P from the first ground wafer W, a cassette 81 for storing a plurality of wafers W before grinding, a cassette 82 for storing the wafers W after grinding, an alignment table 83 for aligning the wafers W removed from the cassette 81, and a wafer holder 84 for holding the wafers W relative to the cassettes 81, 82. The system is equipped with a loading / unloading robot 84 which loads and unloads the wafer W and transports the wafer W removed from the cassette 81 to the alignment table 83, a first transport means 85 which transports the wafer W aligned on the alignment table 83 to the chuck table 10 located in the wafer loading / unloading area R1, and a second transport means 90 which removes the wafer W that has been finish ground in the finish grinding area R3 from the chuck table 10 and transports it to the peeling device 70, but detailed explanations of these will be omitted.
[0016] Here, the configurations of the chuck table 10, the rough grinding unit 20, the finish grinding unit 30, and the grinding water supply unit 40, which are the main components of the grinding apparatus 1, will be described.
[0017] (Chuck table) The three chuck tables 10 are disk-shaped members arranged at equal angular pitches (120° pitches) in the circumferential direction on the turntable 2, which rotates intermittently about a central axis perpendicular to the Z-axis direction. These chuck tables 10 revolve around the axis of the turntable 2 perpendicular to the Z-axis direction by an angle of 120° each time the turntable 2 intermittently rotates, and move sequentially between the wafer loading / unloading region R1, the rough grinding region R2, and the finish grinding region R3, and also rotate (spin) around the axis at a predetermined speed by a rotation mechanism (not shown).
[0018] 4, a disk-shaped porous member 10A made of porous ceramic or the like is incorporated in the center of each chuck table 10, and the upper surface of each porous member 10A forms a holding surface 10a that suction-holds a disk-shaped wafer W. The porous member 10A of each chuck table 10 is selectively connected to a suction source 13 (see FIG. 5), such as a vacuum pump, as will be described later.
[0019] (Rough grinding unit and finish grinding unit) The grinding device 1 according to this embodiment includes a rough grinding unit 20 as a first grinding unit and a finish grinding unit 30 as a second grinding unit. As shown in FIG. 1, the rough grinding unit 20 and the finish grinding unit 30 are vertically arranged in a state of being arranged side by side in the X-axis direction (left and right direction) at the +Y-axis direction end (rear end) of a rectangular box-shaped base 200 that is long in the Y-axis direction (front and back direction). Here, the rough grinding unit 20 is a unit that roughly grinds both sides of a wafer W held on the holding surface 10a of the chuck table 10 located in the rough grinding region R2, and the finish grinding unit 30 is a unit that finish grinds both sides of a wafer W held on the holding surface 10a of the chuck table 10 located in the finish grinding region R3, and the basic configurations of both units are the same.
[0020] That is, the rough grinding unit 20 includes a spindle motor 22 fixed to a holder 21, a vertical spindle 23 rotated by the spindle motor 22, a disk-shaped mount 24 attached to the lower end of the spindle 23, and a grinding wheel 25 detachably mounted on the lower surface of the mount 24. Here, the grinding wheel 25 is composed of a disk-shaped base 25a and a plurality of grinding stones 25b attached in an annular shape to the lower surface of the base 25a.
[0021] Similarly to the rough grinding unit 20, the finish grinding unit 30 also includes a spindle motor 32 fixed to a holder 31, a vertical spindle 33 rotated by the spindle motor 32, a disk-shaped mount 34 attached to the lower end of the spindle 33, and a grinding wheel 35 detachably attached to the lower surface of the mount 34. Here, the grinding wheel 35 is composed of a disk-shaped base 35a and a plurality of grinding wheels 35b attached in an annular shape to the lower surface of the base 35a, and these grinding wheels 35b are composed of finer abrasive grains than the grinding wheels 25b of the rough grinding unit 20.
[0022] The rough grinding unit 20 and the finish grinding unit 30 are supported so as to be able to rise and fall by lifting mechanisms 3 provided on the -Y axis direction end faces (front faces) of a pair of block-shaped columns 101 that are erected vertically along the X axis direction (left and right direction) at the +Y axis direction end (rear end) of the base 200. Here, since both lifting mechanisms 3 have the same configuration, corresponding components will be described below with the same reference numerals.
[0023] Each lifting mechanism 3 lifts and lowers the rough grinding unit 20 and the finish grinding unit 30 independently along the Z-axis direction (up and down direction), and includes a rectangular plate-shaped lifting plate 4 and a guide rail 5 for guiding the lifting and lowering movement of the lifting plate 4. Here, the rough grinding unit 20 and the finish grinding unit 30 are respectively attached to each lifting plate 4. The guide rail 5 is disposed vertically on the front surface of the column 101.
[0024] A rotatable ball screw 6 is provided vertically along the Z-axis direction (up and down direction) beside each guide rail 5, and the upper end of the ball screw 6 is connected to a servo motor 7, which serves as a drive source and can rotate forward and backward. The lower end of the ball screw 6 is rotatably supported on a column 101 by a bearing (not shown), and a nut member (not shown) that is provided on the back surface of the lift plate 4 and protrudes horizontally toward the rear (+Y-axis direction) is screwed into the ball screw 6.
[0025] Therefore, when the servo motor 7 of each lifting mechanism 3 configured as described above is started to rotate each ball screw 6 forward and backward, each lifting plate 4, on which a nut member (not shown) that screws into each ball screw 6 is protruding, moves up and down along the guide rail 5, and the rough grinding unit 20 and the finish grinding unit 30 attached to the lifting plate 4 also move up and down independently of each other along the Z-axis direction (up and down direction).
[0026] (Grinding water supply unit) 1, the grinding water supply unit 40 supplies grinding water containing a surfactant to the contact area (grinding area) between the grinding wheel 25b of the rough grinding unit 20 and the wafer W during grinding, and includes a grinding water supply source 41. A pipe 42 extends from the grinding water supply source 41, and two branch pipes 42a, 42b branch out from the pipe 42. The branch pipes 42a, 42b are connected to supply paths (not shown) formed in the axial centers of the spindle motors 22, 32 of the rough grinding unit 20 and the finish grinding unit 30, respectively, and opening / closing valves V1, V2 are provided midway through the branch pipes 42a, 42b, respectively. Although not shown, a supply path (not shown) formed in the shaft center of each spindle motor 22, 32 of the rough grinding unit 20 and the finish grinding unit 30 communicates with a supply path (not shown) formed in each spindle 23, 33, mount 24, 34, and grinding wheel 25, 35 of the rough grinding unit 20 and the finish grinding unit 30, and by switching the opening and closing of the opening and closing valves V1, V2, grinding water containing a surfactant is selectively supplied to the contact area (grinding area) between the grinding wheels 25b, 35b of the rough grinding unit 20 or the finish grinding unit 30 and the wafer W during grinding processing. Here, pure water is preferably used as the grinding water.
[0027] [Wafer grinding method] Next, a method for grinding the wafer W according to the present invention, which is carried out in the grinding apparatus 1 configured as above, will be described.
[0028] As shown in FIG. 2, the method for grinding a wafer W according to the present invention includes the following steps: 1) Protective material forming process 2) Holding process 3) First grinding process 4) Separation process 5) Peeling process 6) Reversal process 7) Second grinding process 8) Separation process This is a method for grinding both sides of a wafer (as-sliced wafer) W through the steps. Each step will be described below.
[0029] 1) Protective member formation process: The protective member forming step is a step of forming a protective member P on one surface (the lower surface in FIG. 3) of the wafer W, and as shown in FIGS. 2 and 3, 1-1) Sheet supply process 1-2) Liquid resin supply process 1-3) Wafer holding process 1-4) Spreading process 1-5) Curing process This is a process for forming a protective member P on one surface of the wafer W through the above steps. Each of the above steps will be described below.
[0030] 1-1) Sheet supply process: 3(a), the sheet supplying step is a step of supplying a thin, disk-shaped transparent sheet S toward the upper surface of a case 60. Here, the case 60 is configured such that the upper surface of a cylindrical side wall 61 is covered with a light-transmitting transparent top plate 62, the lower surface of the side wall 61 is covered with a bottom plate 63, and a space is formed by accommodating a plurality of UV lamps 64 that emit ultraviolet (UV) rays upward.
[0031] In this sheet supplying step, the sheet S having one end gripped by the gripper 65 is supplied and set on the flat top plate 62 of the case 60 .
[0032] 1-2) Liquid resin supply process: 3(b), the liquid resin supplying step is a step of dripping liquid resin r from a nozzle 66 installed above the case 60 toward the center of the sheet S. Note that, although an ultraviolet curing resin is used as the liquid resin r in this embodiment, other resins such as a thermosetting resin may also be used.
[0033] 1-3) Wafer holding process: The wafer holding step is a step of suction-holding the wafer W by the transport pad 67, as shown in Fig. 3(c). The transport pad 67 is configured by incorporating a disk-shaped porous member 67A made of porous ceramic or the like in the center of its lower surface, and by connecting the porous member 67A to a suction source (not shown), negative pressure is generated in the porous member 67A, and the other surface of the wafer W (the upper surface in Fig. 3(c)) is sucked by this negative pressure, and the wafer W is held on the lower surface of the transport pad 67. The transport pad 67 can be raised and lowered by a lifting mechanism 68.
[0034] 1-4) Spreading process: As shown in FIG. 3(d), the spreading process is a process of spreading out the liquid resin (ultraviolet-curable resin) r dropped onto the sheet S in the liquid resin supply process. In this spreading process, the transport pad 67 is lowered by the lifting mechanism 68, and the wafer W held by the transport pad 67 is pressed against the liquid resin r on the sheet S, spreading out the liquid resin r to a uniform thickness.
[0035] 1-5) Curing process: In the curing step, as shown in FIG. 3(e), the lifting mechanism 68 raises the conveying pad 67 and separates it from the wafer W, leaving the sheet S, the liquid resin r, and the wafer W on the case 60 side. Then, from this state, the UV lamps 64 in the case 60 are turned on. Then, ultraviolet light (UV) emitted upward from each UV lamp 64 passes through the transparent top plate 62 and the sheet S and is irradiated onto the liquid resin r, and the liquid resin r is cured. As a result of the liquid resin r being cured in this way, a protective member P is formed on one surface of the wafer W. The cured protective member P and the surface of the sheet S that is in close contact with the protective member P (the lower surface in FIG. 3(e)) are flat surfaces that follow the flat upper surface of the top plate 62 of the case 60.
[0036] 2) Holding process: The holding process is a process in which a wafer W having a protective member P formed on one side by the protective member forming process is held on the holding surface 10a of the chuck table 10 with the sheet S facing down, as shown in FIG. 4. In this holding process, the porous member 10A of the chuck table 10 is connected to a suction source 13 shown in FIG. 5.
[0037] 5, a communication passage 10b communicating with the porous member 10A is formed vertically in the center of the chuck table 10, and a pipe 11 extending from the communication passage 10b branches into four branch pipes 11a, 11b, 11c, and 11d. The branch pipe 11a is connected to a suction source 13 via a flow control valve (throttle valve) 12 and a suction valve V3, and the branch pipe 11b is connected to an air supply source 15 via a flow control valve 14 and an air ejection valve V4. The branch pipe 11c is connected to a water supply source 17 via a flow control valve 16 and a water ejection valve V5, and the branch pipe 11d is connected to a surfactant supply source 19 via a flow control valve 18 and a surfactant ejection valve V6.
[0038] Therefore, in the holding step, when the suction valve V3 is opened to connect the porous member 10A of the chuck table 10 to the suction source 13 with the air jet valve V4, water jet valve V5, and surfactant jet valve V6 closed, the porous member 10A is suctioned by the suction source 13. Then, a negative pressure is generated in the porous member 10A, and the wafer W is sucked and held by the holding surface 10a of the chuck table 10 together with the protective member P and the sheet S by being attracted by this negative pressure, as shown in FIG.
[0039] 3) First grinding process: 4, the first grinding step is a step of grinding the other surface (upper surface in FIG. 4) of the wafer W held on the holding surface 10a of the chuck table 10, and the grinding step includes rough grinding by the rough grinding unit 20 and finish grinding by the finish grinding unit 30, and the other surface of the wafer W is rough ground and finish ground. Note that while FIG. 4 shows a state in which the wafer W is roughly ground by the grinding wheel 25b of the rough grinding unit 20, the finish grinding of the wafer W by the finish grinding unit 30 is also performed in the same manner.
[0040] 4, the holding surface 10a of the chuck table 10 is configured as a conical surface that slopes downward radially outward with the center as the apex, and the chuck table 10 is rotated in the direction of the arrow shown in the figure about an axis CL1 that passes through the center. In contrast, the spindle 23 and grinding wheel 25 of the rough grinding unit 20 are rotated in the direction of the arrow shown in the figure about a vertical axis CL2 that passes through the center.
[0041] To roughly grind the other surface (upper surface) of the wafer W by the rough grinding unit 20, the inclination of the chuck table 10 is adjusted by the inclination adjustment mechanism 8 so that the holding surface 10a (radial area) of the chuck table 10 is parallel to the lower surface (grinding surface) of the grinding wheel 25b. Specifically, the axis CL1 of the chuck table 10 is inclined by the angle α shown in the figure with respect to the vertical. In addition, the chuck table 10 is moved in the +Y axis direction (rightward in FIG. 4) by a horizontal movement mechanism (not shown) and is positioned so that the circumscribed circle of the grinding wheel 25b passes through the center of the wafer W held on the holding surface 10a.
[0042] 1 moves the grinding wheel 25b downward in the -Z-axis direction from the above state, the lower surface (grinding surface) of the grinding wheel 25b rotates while contacting the other surface (upper surface in FIG. 4) of the wafer W, thereby roughly grinding the other surface of the wafer W. During rough grinding of the wafer W, grinding water containing a surfactant is supplied from the grinding water supply source 41 of the grinding water supply unit 40 shown in FIG. 1 to the contact area (grinding area) between the grinding wheel 25b of the rough grinding unit 20 and the wafer W. That is, when one of the on-off valves V2 is closed and the other on-off valve V1 is opened, grinding water containing a surfactant is supplied from the grinding water supply source 41 through the piping 42, the branch pipe 42a, and a supply path (not shown) formed at the center of the axis of the spindle motor 22 and the spindle 23 of the rough grinding unit 20 to the contact area (grinding area) between the grinding wheel 25b and the wafer W, and is used to cool and clean the contact area.
[0043] During rough grinding of the wafer W by the grinding wheel 25b of the rough grinding unit 20, the thickness of the wafer W is measured by a thickness gauge 51 shown in Fig. 1, and rough grinding of the wafer W is continued until the thickness of the wafer W measured by the thickness gauge 51 reaches a target thickness. Then, when rough grinding of the wafer W is completed, the turntable 2 shown in Fig. 1 rotates by an angle of 120° in the direction of the arrow, so that the chuck table 10 also revolves by the same angle and moves from the rough grinding region R2 to the finish grinding region R3. Then, the wafer W held by the chuck table 10 that has moved to the finish grinding region R3 is subjected to the same rough grinding by the finish grinding unit 30.
[0044] Therefore, although illustration and description of the finish grinding of the wafer W are omitted, in this finish grinding as well, grinding water containing a surfactant is supplied from the grinding water supply source 41 of the grinding water supply unit 40 shown in Fig. 1 to the contact area (grinding area) between the grinding wheel 35b of the finish grinding unit 30 and the wafer W. That is, when one on-off valve V1 is closed and the other on-off valve V2 is opened, grinding water containing a surfactant is supplied from the grinding water supply source 41 through the pipe 42, the branch pipe 42b, and a supply path (not shown) formed at the center of the axis of the spindle motor 32, the spindle 33, etc. of the finish grinding unit 30 to the contact area (grinding area) between the grinding wheel 35b and the wafer W, and is used for cooling and cleaning the contact area.
[0045] Depending on the conditions, the rough grinding step may be omitted in the first grinding step, and only the finish grinding step may be performed.
[0046] 4) Separation process: The separating process is a process of separating the wafer W ground in the first grinding process from the chuck table 10, and the separated wafer W is held by the second transport means 90 shown in FIG. 1 and transported to the peeling device 70.
[0047] That is, in the separation step, as shown in FIG. 5(a), in a state where the second conveying means 90 is pressed against the upper surface of the wafer W to hold the wafer W, the suction valve V3 is closed, and the air ejection valve V4, the water ejection valve V5, and the surfactant ejection valve V6 are opened. Then, air from the air supply source 15 flows into the pipe 11 through the branch pipe 11b, water from the water supply source 17 flows into the pipe 11 through the branch pipe 11c, and the surfactant (concentrated liquid) from the surfactant supply source 19 flows into the pipe 11 through the branch pipe 11d. Therefore, in the pipe 11, a mixed fluid (two fluids) of water containing a surfactant and air is formed, and this mixed fluid is supplied to the porous member 10A of the chuck table 10 through the communication passage 10b formed in the center of the chuck table 10, and the mixed fluid containing the surfactant is ejected from the holding surface 10a of the chuck table 10. In this way, the mixed fluid containing the surfactant is ejected from the holding surface 10a, whereby the holding surface 10a can be cleaned. Moreover, while the wafer W is being held by suction using the second conveying means 90, the lower surface of the sheet S of the wafer W is cleaned with the mixed fluid containing a surfactant that is sprayed from the holding surface 10a.
[0048] Then, the wafer W receives pressure on its lower surface, and as shown in Fig. 5(b), the wafer W, together with the protective member P and the sheet S, is separated from the holding surface 10a of the chuck table 10. Therefore, the second conveying means 90 can suction-hold the wafer W together with the protective member P and the sheet S, and convey them to the peeling device 70 shown in Fig. 1.
[0049] 5) Peeling process: The peeling step is a step of peeling off the protective material P and the sheet S from one side of the wafer W that has been transported to the peeling device 70 by the second transport means 90, and in this peeling step, the protective material P and the sheet S are peeled off from one side of the wafer W according to the procedure shown in Figs. 6(a) to (c). Here, the details of the configuration of the second transport means 90 are shown in Fig. 6, and the second transport means 90 is provided with a disk-shaped suction pad 94 that is supported horizontally at the tip of an arm 91 via a connecting member 92 and a support member 93. Here, the arm 91 and the suction pad 94 supported thereby can be moved horizontally by a horizontal movement mechanism 95, and can be raised and lowered by a lifting mechanism 96.
[0050] Here, the suction pad 94 is configured by incorporating a disk-shaped porous suction member 94B in the center of the lower surface of a frame body 94A, and is supported by a support member 93 with a plurality of pins 97 (only two are shown in FIG. 6). The suction member 94B of the suction pad 94 is selectively connected to a suction source 98 or an air supply source 99 through a communication passage 9A formed in the arm 91, the connecting member 92, and the support member 93. That is, a pipe 9 is connected to the communication passage 9A formed in the arm 91, the connecting member 92, and the support member 93, and two branch pipes 9a and 9b are branched from this pipe 9. One branch pipe 9a is connected to the suction source 98 through an on-off valve V7, and the other branch pipe 9b is connected to the air supply source 99 through an on-off valve V8.
[0051] Thus, in a state in which the wafer W, together with the protective member P and the sheet S, is sucked and held by the suction pad 94 of the second conveying means 90, one on-off valve V7 is opened and the other on-off valve V8 is closed, so that air in the suction member 94B of the suction pad 94 is sucked by the suction source 98 through the communication passage 9A, the piping 9 and the branch pipe 9a. Therefore, a negative pressure is generated in the suction member 94B, and the wafer W, together with the protective member P and the sheet S, is sucked and held by the suction member 94B of the suction pad 94 due to the negative pressure.
[0052] In the peeling step, as shown in Fig. 6(a), one end of the sheet S that is in close contact with a protective member P formed on one surface (the lower surface in Fig. 6) of the wafer W held by the suction pad 94 of the second conveying means 90 is gripped by a gripper 71. The gripper 71 is supported by a shaft 72 so as to be rotatable in the vertical direction, and a roller 73 that is long in the direction perpendicular to the paper surface of Fig. 6 is disposed near the gripper 71.
[0053] 6(b), when gripper 71 gripping one end of sheet S rotates about shaft 72 by an angle of 90° in the direction of the arrow and moves downward, protective member P and a part of sheet S gripped by gripper 71 are pulled downward about roller 73 and peeled off from one side of wafer W. After that, from the state shown in FIG. 6(b), as shown in FIG. 6(c), suction pad 94 moves horizontally together with wafer W in the direction of the arrow (to the right) by horizontal movement mechanism 95, and gripper 71 moves in the direction of the arrow (to the left) while gripping one end of sheet S, and protective member P and sheet S are peeled off and removed from one side (lower surface) of wafer W.
[0054] 6) Reversal process: The inversion step is a step of inverting the wafer W from which the protective material P and the sheet S have been peeled off from one surface (lower surface) in the peeling step, and as shown in Fig. 7(a), the wafer W sucked and held by the suction pad 94 of the second transport means 90 is separated from the suction pad 94 and transferred onto the disk-shaped holding pad 76 of the inversion mechanism 75. When the wafer W is separated from the suction pad 94, the on-off valve V7 is closed and the on-off valve V8 is opened, and air is supplied to the suction member 94B of the suction pad 94. Then, air is ejected from the suction member 94B of the suction pad 94, so that the wafer W, which receives the pressure of this air on the other surface (the upper surface in Fig. 7(a)), is easily separated from the suction member 94B of the suction pad 94.
[0055] As described above, the wafer W transferred onto the holding pad 76 of the inversion mechanism 75 rotates the holding pad 76 half a turn (180°), so that the other flat surface ground in the first grinding step becomes the lower surface, and the surface on which the protective member P was formed becomes the upper surface, as shown in Fig. 7(b). Note that a peeling step may be performed after the inversion step.
[0056] 7) Second grinding process: In the second grinding process, one surface (the surface on which the protective member P was formed) of the wafer W that has been inverted in the inversion process is roughly ground by the rough grinding unit 20 and finish ground by the finish grinding unit 30.
[0057] Here, the state in which one side of the wafer W is roughly ground by the rough grinding unit 20 is shown in FIG. 8. In this rough grinding, the wafer W is sucked and held on the holding surface 10a of the chuck table 10 with the other side (flat surface ground in the first grinding step) facing down. The rough grinding and finish grinding of one side of the wafer W are performed in the same manner as the rough grinding and finish grinding of the other side of the wafer W in the first grinding step, so the description of these is omitted. In this second grinding step, grinding water containing a surfactant is also supplied toward the contact area (grinding area) between the grinding wheels 25b, 35b and the wafer W. The finish grinding of one side of the wafer W by the finish grinding unit 30 is not shown, but depending on the conditions, there are cases in which the rough grinding is omitted and only the finish grinding is performed on one side of the wafer W.
[0058] 8) Separation process: The separating process is a process of separating the wafer W, one side of which has been ground in the second grinding process, from the chuck table 10, and the separated wafer W is held by the second transport means 90 shown in FIG. 1 and transported to the cleaning unit 50.
[0059] That is, in the separation step, as shown in FIG. 9(a), in a state where the second conveying means 90 is pressed against the upper surface of the wafer W to hold the wafer W, the suction valve V3 is closed, and the air ejection valve V4, the water ejection valve V5, and the surfactant ejection valve V6 are opened. Then, air from the air supply source 15 flows into the pipe 11 through the branch pipe 11b, water from the water supply source 17 flows into the pipe 11 through the branch pipe 11c, and the surfactant (concentrated liquid) from the surfactant supply source 19 flows into the pipe 11 through the branch pipe 11d. Therefore, in the pipe 11, a mixed fluid (two fluids) of water containing a surfactant and air is formed, and this mixed fluid is supplied to the porous member 10A of the chuck table 10 through the communication passage 10b formed in the center of the chuck table 10, and the mixed fluid containing the surfactant is ejected from the holding surface 10a of the chuck table 10. In this way, the mixed fluid containing the surfactant is ejected from the holding surface 10a, whereby the holding surface 10a can be cleaned. Moreover, while the wafer W is being suction-held by the second conveying means 90, the lower surface of the wafer W is cleaned with the mixed fluid containing a surfactant that is sprayed from the holding surface 10a.
[0060] Then, the wafer W receives pressure on its lower surface, and the wafer W is separated from the holding surface 10a of the chuck table 10 as shown in FIG. 9(b). Therefore, the second transport means 90 can suction-hold the wafer W and transport it to the cleaning unit 50 shown in FIG. 1. The wafer W transported to the cleaning unit 50 is cleaned by spraying cleaning water in the cleaning unit 50, and the cleaned wafer W is held by the carry-in / out robot 84 and transported to the cassette 82, where it is stored in the cassette 82, completing a series of grinding processes for the wafer W. The cleaning unit 50 sprays cleaning water onto the wafer W to remove the surfactant. Before the spinner table of the cleaning unit 50 holds the wafer W, an operation of spraying water from the spinner table to remove the surfactant from the lower surface of the wafer W may be performed.
[0061] As described above, in the method for grinding the wafer W according to the present invention, when the other surface of the wafer W, one of which is held on the chuck table 10 in the holding step, is ground in the next grinding step, grinding water containing a surfactant is supplied to the wafer W and the grinding wheels 25b, 35b, so that the grinding water containing the grinding chips generated by grinding the other surface of the wafer W is sucked into the chuck table 10. Then, when the mixed fluid of water and air is ejected from the chuck table 10 in the next separating step, the grinding chips and the grinding water sucked into the chuck table 10 during grinding are ejected from the chuck table 10 together with the mixed fluid, but since the grinding water contains a surfactant, adhesion of the grinding chips to the one surface of the wafer W can be suppressed. And, since such an effect can be obtained simply by adding a surfactant to the grinding water, a dedicated cleaning unit is not required, and the structure of the grinding device 1 is not complicated and the cost is not increased.
[0062] It should be noted that the present invention is not limited to the above-described embodiments, and various modifications are possible within the scope of the claims and the technical ideas described in the specification and drawings. [Explanation of symbols]
[0063] 1: grinding device, 2: turntable, 3: lifting mechanism, 4: lifting plate, 5: guide rail, 6: ball screw, 7: servo motor, 8: tilt adjustment mechanism, 9: piping, 9A: communication passage, 9a, 9b: branch pipes, 10: chuck table, 10A: porous member, 10a: holding surface, 10b: communication passage, 11: piping, 11a, 11b, 11c, 11d: branch pipes, 12: flow rate control valve, 13: suction source, 14: flow rate control valve, 15: air supply source, 16: flow control valve, 17: water supply source, 18: flow control valve, 19: surfactant supply source, 20: rough grinding unit, 21: holder, 22: spindle motor, 23: spindle, 24: mount, 25: grinding wheel, 25a: base, 25b: grinding stone, 30: finish grinding unit, 31: holder, 32: spindle motor, 33: spindle, 34: mount, 35: grinding wheel, 35a: base, 35b: grinding stone, 40: grinding water supply unit, 41: grinding water supply source, 42: piping, 42a, 42b: branch pipes, 50: cleaning unit, 51, 52: thickness measuring device, 60: case, 61: side wall, 62: top plate, 63: bottom plate, 64: UV lamp, 65: gripper, 66: nozzle, 67: transport pad, 67A: porous member, 68: lifting mechanism, 70: peeling device, 71: gripper, 72: shaft, 73: roller, 75: inversion mechanism, 76: holding pad, 81, 82: cassette, 83: alignment table, 84: carry-in / out robot, 85: first conveying means, 90: second conveying means, 91: arm, 92: connecting member, 93: supporting member, 94: suction pad, 94A: frame body, 94B: suction member, 95: horizontal movement mechanism, 96: lifting mechanism, 97: pin, 98: suction source, 99: air supply source, 101: column, 200: Base, CL1: Chuck table axis, CL2: Spindle axis, P: Protective material, R1: Wafer loading / unloading area, R2: Rough grinding area, R3: Finish grinding area, r: Liquid resin, S: Sheet, V1, V2: Opening / closing valve, V3: Suction valve, V4: Air injection valve, V5: Water injection spring, V6: Surfactant supply valve, V7, V8: Open / Close Valve, W: Wafer, α: Tilt Angle of Chuck Table
Claims
1. A method for grinding a wafer, comprising the steps of: a holding step of holding one surface of the wafer on a chuck table; a grinding step of supplying a grinding water containing a surfactant to the wafer and the grinding wheel and grinding the other surface of the wafer with the grinding wheel; a separating step of ejecting a mixed fluid of water and air from the chuck table to separate the wafer from the chuck table; A method for grinding a wafer comprising the steps of:
2. 2. The method for grinding a wafer according to claim 1, wherein in the separating step, a mixed fluid containing a surfactant is ejected from the chuck table.
3. 2. The method for grinding a wafer according to claim 1, wherein in said holding step, a protective member is placed on the entire one surface of said wafer, and said wafer is held on said chuck table via said protective member.
4. 2. The method for grinding a wafer according to claim 1, wherein the wafer is an as-sliced wafer sliced from an ingot.
Citation Information
Patent Citations
Manufacturing method for mirror-polished wafer
JP2003062740A
Grinding machine for semiconductor wafer, and grinding method thereof
JP2006100644A
Holding mechanism for workpiece in grinding device
JP2009125900A
Method for grinding semiconductor wafer
JP2011082520A
Planarization method of wafer
JP2011249652A