Method for producing ammonium nitrate using nitrogen dioxide in cement exhaust gas
The method efficiently converts nitrogen dioxide in cement factory exhaust gas into ammonium nitrate using a multi-step process with magnetite catalysts, addressing inefficiencies in existing denitrification methods and creating an environmentally friendly recycling system.
Patent Information
- Application Number
- JP2023050759
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-28
- Publication Date
- 2024-10-10
- Estimated Expiration
- 2043-03-28
AI Technical Summary
Existing methods for denitrifying nitrogen dioxide in cement factory exhaust gas are inefficient, limited to specific temperature ranges, and complicate the process, making it difficult to effectively reuse the recovered NOx.
A method involving nitrogen dioxide recovery, reduction, ammonia recovery, solid-liquid separation, neutralization, and catalyst production steps, utilizing waste heat gas and magnetite as a reducing catalyst to convert NOx into ammonium nitrate, reducing environmental impact and enabling effective reuse of residues.
Highly efficient denitrification of nitrogen dioxide in cement factory exhaust gas, reducing environmental burden and enabling the production of ammonium nitrate suitable for use in cement production, with a closed-loop recycling system.
Smart Images

Figure 2024139840000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for producing ammonium nitrate using nitrogen dioxide in cement exhaust gas, and in particular to a method for producing ammonium nitrate using nitrogen dioxide in cement exhaust gas, which can easily and effectively reduce the environmental load by highly efficiently recovering nitrogen dioxide generated in cement factories, and which can also suppress the environmental load in the preparation of a catalyst used in the process of preparing the ammonium nitrate. [Background technology]
[0002] In general, in cement production, exhaust gas generated by burning coal, heavy oil, and recycled fuel is used to dry the cement raw materials, and then the contained dust is recovered in a dust collection process and discharged outside the system. In addition to carbon dioxide and trace amounts of chlorides, the exhaust gas discharged from the system also contains large amounts of nitrogen oxides (hereinafter referred to as "NOx") resulting from fuel combustion, etc. NOx is an environmental load, such as acid rain, and has adverse effects on the human body, including the respiratory system.
[0003] In light of these issues, proposals have been made to reduce NOx emissions at cement plants, such as by selecting fuels with lower nitrogen content and by using denitrifiers to regulate NOx emissions.
[0004] Japanese Patent No. 5100432 (Patent Document 1) proposes an SCR method using urea or alcohol as a NOx denitrification technology for use in cement plants. Specifically, this is a method for treating exhaust gas in which a denitrification agent is brought into contact with exhaust gas containing nitrogen oxides to denitrify the exhaust gas. The denitrification agent used is a mixture of urea and one or more types of waste liquid selected from the group consisting of water-soluble waste liquid containing oil, waste liquid produced by washing ash with water, waste liquid containing alcohols, and waste liquid produced in cement or concrete plants, and the type of waste liquid and the mass ratio of the waste liquid to urea are determined so as to satisfy specific conditions.
[0005] However, in this method, the optimum temperature for the denitrification reaction is 800°C or higher, and the hot gas that passes through the urea spray area is not denitrified, so it can be assumed that approximately 400 ppm of NOx is emitted into the atmosphere.
[0006] Furthermore, Japanese Patent Laid-Open Publication No. 2003-175315 (Patent Document 2) proposes a nitrogen oxide absorbent that absorbs nitrogen oxides in a high-temperature gas containing oxygen and nitrogen oxides, the nitrogen oxide absorbent comprising a mixture of an oxide or hydroxide of an alkaline earth element and an oxide of a transition element, the alkaline earth element being barium (Ba) and / or strontium (Sr), and the transition element being copper (Cu) and / or iron (Fe).
[0007] Furthermore, Japanese Patent No. 5963405 (Patent Document 3) discloses a method for denitrifying a gas containing NOx to be treated, in which NOx, which is a component of the gas to be treated, is oxidized by ozone, and the NOx components in the gas to be treated after this ozone oxidation produce nitrous acid through mixing and contact with an absorbing liquid, and the release of NOx generated by the conversion of the nitrous acid into the gas phase is suppressed or prevented by ozone added in advance to the absorbing liquid, in which the molar ratio of ozone supplied to the gas to be treated is in the range of 0.1 to 2 times the molar ratio of the gas to be treated to the gas to be treated components, and ozone of 1 ppm or more and less than a saturated concentration is added in advance to the absorbing liquid that absorbs the gas to be treated, the gas to be treated to which the ozone has been supplied and the absorbing liquid to which the ozone has been added are mixed and contacted in a fibrous porous body having a gas-liquid separation function, and the gas-liquid separation is performed below the porous body.
[0008] The conventional method of Patent Document 2 is carried out under high-temperature gas conditions (300 to 600° C.), and application to cement plants makes treatment difficult because the cement combustion exhaust gas contains dust. In addition, the conventional method described in Patent Document 3 is a method for recovering NOx with water at room temperature, but it is necessary to oxidize the recovered nitrous acid using ozone or the like, which makes the process complicated and expensive, making it difficult to introduce in actual cement plants.
[0009] As described above, in the conventional method, denitrification of NOx in exhaust gas generated in cement plants can only be performed in a limited temperature range, and the process is complicated, so the captured NOx cannot be effectively reused. In addition, a method for producing ammonium nitrate that utilizes NOx in exhaust gas and sufficiently reduces the environmental load is expected. [Prior art documents] [Patent documents]
[0010] [Patent Document 1] Patent No. 5100432 [Patent Document 2] JP 2003-175315 A [Patent Document 3] Patent No. 5963405 Summary of the Invention [Problem to be solved by the invention]
[0011] An object of the present invention is to solve the above problems and to provide a method for producing ammonium nitrate using nitrogen dioxide in exhaust gas from cement, which can easily and efficiently denitrify nitrogen dioxide in waste gas generated during cement production in a cement factory, thereby suppressing emissions into the atmosphere and reducing the environmental load.
[0012] Another object of the present invention is to provide a circulation cycle that is suitable for cement plants and has excellent environmental load reduction properties, in which nitrogen dioxide in cement exhaust gas is converted into ammonium nitrate by utilizing waste heat gas emitted in the cement manufacturing process, while also reducing the environmental load in the manufacture of a catalyst used in the process of manufacturing ammonium nitrate, and the resulting residue can be effectively used in cement manufacturing. [Means for solving the problem]
[0013] (I) The method for producing ammonium nitrate using nitrogen dioxide in cement exhaust gas according to the present invention is as follows: a nitrogen dioxide recovery step (1) for contacting nitrogen dioxide in the cement exhaust gas with water to allow the water to absorb the nitrogen dioxide and recover the nitrogen dioxide as a liquid containing nitrate and nitrite nitrogen; a reduction reaction step (2) in which the reduced iron and magnetite are contacted with all or a part of the nitrate / nitrite nitrogen-containing liquid obtained in the nitrogen dioxide recovery step (1) under acidic conditions to produce iron hydroxide and ammonia; Next, an ammonia recovery step (3) is performed in which the ammonia produced in the reduction reaction step (2) is distilled and vaporized using waste heat gas from the cement production process, and then recovered. a solid-liquid separation step (4) for subjecting the remainder after the ammonia recovery step (3) to solid-liquid separation to separate the iron hydroxide from the reduction reaction step (2) that has been subjected to the ammonia recovery step (3) and the unused remainder nitrate and nitrite nitrogen; a neutralization step (5) in which the nitrate / nitrite nitrogen-containing liquid separated in the solid-liquid separation step (4) and the remaining nitrate / nitrite nitrogen-containing liquid obtained in the nitrogen dioxide recovery step (1) and not introduced into the reduction reaction step (2) are brought into contact with ammonia vaporized and recovered in the ammonia recovery step (3) to prepare ammonium nitrate; and The magnetite used in the reduction reaction step (2) is prepared by reacting iron sulfate with an aqueous sodium hydroxide solution to produce magnetite and an aqueous sodium sulfate solution, and then separating the magnetite and the aqueous sodium sulfate solution into solid and liquid. The aqueous sodium sulfate solution is separated into sodium hydroxide and sulfuric acid by electrodialysis. The resulting sodium hydroxide is recycled for use in the preparation of magnetite to be reacted with the iron sulfate. A catalyst production step (7) is provided. This is a method for producing ammonium nitrate using nitrogen dioxide in cement exhaust gas, characterized by the above.
[0014] (II) Preferably, in the method for producing ammonium nitrate utilizing nitrogen dioxide in a cement exhaust gas according to the present invention described in (I) above, the sulfuric acid obtained in the catalyst production step (7) is used to make the reduction reaction step (2) acidic, and / or is reacted with unreacted sodium hydroxide after the preparation of magnetite to produce sodium sulfate, which is then recycled for use in the electrodialysis together with the aqueous sodium sulfate solution obtained by solid-liquid separation in the catalyst production step (7).
[0015] (III) More preferably, in the method for producing ammonium nitrate utilizing nitrogen dioxide in exhaust gas from cement according to the present invention described in (I) or (II) above, the hydrogen generated during the preparation of magnetite in the catalyst production step (7) is recycled and reused as a combustion raw material during the production of cement.
[0016] (IV) More preferably, the method for producing ammonium nitrate utilizing nitrogen dioxide in cement exhaust gas according to the present invention described above in (I) or (II) further comprises a granulation step (6) of granulating the ammonium nitrate prepared in the neutralization step (5).
[0017] (V) More preferably, in the method for producing ammonium nitrate utilizing nitrogen dioxide in exhaust gas from cement production according to the present invention described in (I) or (II) above, the iron hydroxide separated in the solid-liquid separation step (4) becomes iron hydroxide oxide when exposed to air, and the iron hydroxide oxide is used as a cement raw material.
[0018] (VI) Preferably, in the method for producing ammonium nitrate utilizing nitrogen dioxide in a cement exhaust gas according to the present invention described in (I) above, the ammonium nitrate prepared in the neutralization step (5) is contained in a liquid containing ammonium nitrate and nitrate / nitrite nitrogen, the liquid is heated and distilled at 170-180°C using waste heat gas to concentrate ammonium nitrate, and the remaining nitrate / nitrite nitrogen is vaporized and circulated to the neutralization step (5), a part of the ammonia vaporized in the ammonia recovery step (3) is added to the concentrated ammonium nitrate to react with unreacted nitrate / nitrite nitrogen mixed in the concentrated ammonium nitrate to improve the purity of ammonium nitrate, and crystallized ammonium nitrate is obtained by cooling. This is a method for producing ammonium nitrate utilizing nitrogen dioxide in a cement exhaust gas, characterized in that Effect of the Invention
[0019] The method for producing ammonium nitrate of the present invention makes it possible to highly efficiently remove nitrogen dioxide from exhaust gases emitted from cement plants, which is also environmentally friendly. Furthermore, the recovered nitrate and nitrite nitrogen can be reduced without any special oxidation treatment, and the ammonium nitrate obtained as the final product can be effectively used as a blasting agent in limestone mines, which is the raw material for cement production, thus creating an environmentally friendly circulation and regeneration cycle.
[0020] Furthermore, since the waste heat gas discharged in the cement manufacturing process can be used as a heat source for producing magnetite, which is a reducing catalyst, and for vaporizing ammonia, it is also possible to effectively utilize the waste heat gas in the cement manufacturing process. Furthermore, it is possible to reduce the environmental impact in the production of a reducing catalyst used in the process of producing ammonium nitrate, and the resulting residue can be effectively used in cement production, thereby forming a circulation cycle that is suitable for cement factories and has excellent environmental impact reduction properties. [Brief description of the drawings]
[0021] [Figure 1] FIG. 1 is a flow chart showing an example of an outline of a method for producing ammonium nitrate using nitrogen dioxide in a cement exhaust gas according to the present invention. [Diagram 2] FIG. 2 is a schematic diagram showing an example of a catalyst production step (7) in FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0022] The present invention will be described below with reference to the following preferred embodiments with reference to Figs. 1 and 2, but is not limited thereto.
[0023] The method for producing ammonium nitrate using nitrogen dioxide in cement waste gas of the present invention is as follows: a nitrogen dioxide recovery step (1) for contacting nitrogen dioxide in the cement exhaust gas with water to allow the water to absorb the nitrogen dioxide and recover the nitrogen dioxide as a liquid containing nitrate and nitrite nitrogen; a reduction reaction step (2) in which the reduced iron and magnetite are contacted with all or a part of the nitrate / nitrite nitrogen-containing liquid obtained in the nitrogen dioxide recovery step (1) under acidic conditions to produce iron hydroxide and ammonia; Next, an ammonia recovery step (3) is performed in which the ammonia produced in the reduction reaction step (2) is distilled and vaporized using waste heat gas from the cement production process, and then recovered. a solid-liquid separation step (4) for subjecting the remainder after the ammonia recovery step (3) to solid-liquid separation to separate the iron hydroxide from the reduction reaction step (2) that has been subjected to the ammonia recovery step (3) and the unused remainder nitrate and nitrite nitrogen; a neutralization step (5) in which the nitrate / nitrite nitrogen-containing liquid separated in the solid-liquid separation step (4) and the remaining nitrate / nitrite nitrogen-containing liquid obtained in the nitrogen dioxide recovery step (1) and not introduced into the reduction reaction step (2) are contacted with ammonia vaporized and recovered in the ammonia recovery step (3) to prepare ammonium nitrate; and The magnetite used in the reduction reaction step (2) is prepared by reacting iron sulfate with an aqueous sodium hydroxide solution to produce magnetite and an aqueous sodium sulfate solution, and then subjecting the resulting aqueous sodium sulfate solution to solid-liquid separation. The aqueous sodium sulfate solution is separated into sodium hydroxide and sulfuric acid by electrodialysis, and the resulting sodium hydroxide is recycled for use in preparing magnetite to be reacted with the iron sulfate. This is a method for producing ammonium nitrate using nitrogen dioxide in cement exhaust gas, and includes a catalyst production step (7).
[0024] As shown in Figure 1, cement is generally produced in a cement plant through a raw material crushing process in which each raw material is crushed, a clinker calcination process in which the crushed raw materials are calcined to produce cement clinker, and then a cement finishing process in which the cement clinker is crushed and mixed with gypsum.
[0025] In order to produce cement clinker, fuel is burned at a burning temperature of about 1300 to 1500° C., and cement raw materials are burned in a cement kiln to produce cement clinker. From the perspective of making effective use of waste materials, household garbage, sewage sludge, waste acid / alkali, waste plastic, dried sludge, waste clay, wood chips, recycled oil, ASR, PKS and other waste materials are burned as fuel, and the resulting heat source is used as a heat source for the cement clinker burning process. In addition, nitrogen-containing waste materials, such as coal ash, general incineration ash, construction soil, cinders, sludge, casting sand, steelmaking dust, and slowly cooled slag, can also be used as raw materials for cement.
[0026] Here, the exhaust gas refers to the exhaust gas discharged from the burning of these waste materials, such as cement dust and CO2 used in the clinker burning process. 2 This refers to a gas that contains a large amount of the above. The exhaust gas contains various types of dust. The dust in the exhaust gas is collected, for example, by an electric dust collector, and the exhaust gas is cooled, for example, to about 30°C. The amount of NOx in the cooled exhaust gas is, for example, 300 to 400 ppm. In the present invention, by capturing NOx in the exhaust gas in the NOx capture step (1) described below, for example, if the amount of NOx contained in the exhaust gas before the NOx capture step is 350 ppm, the amount of NOx contained in the exhaust after the application of the NOx capture step (1) can be reduced to 28 ppm.
[0027] The exhaust gas, which has had dust collected from exhaust gas such as combustion gas emitted from a cement manufacturing process and has been cooled, for example to 40°C or less, is introduced into a NOx (nitrogen dioxide, etc.) recovery process (1) and brought into contact with water. The NOx recovery process (1) is a recovery process that utilizes a water-based NOx absorption and removal process.
[0028] Specifically, the cooled exhaust gas after dust collection is brought into contact with water, and the NOx contained in the exhaust gas is absorbed into the water by contacting the water with the NOx, and the NOx is collected as a liquid containing nitrate and nitrite nitrogen. For example, a heat exchanger can be used to indirectly recover heat, and NOx can be reacted with water to convert it into nitrate or nitrite nitrogen.
[0029] The NOx in the cement exhaust gas to be recovered has an equilibrium relationship as shown in the following formula (A). 2NO → 2NO 2 ←→N 2 O 4 ···(a) In addition, as shown in the following reaction formula (a), NO 2 When this comes into contact with water, it produces nitrate and nitrite nitrogen. 2NO 2 +H 2 O→HNO 3 +HNO 2 ···(stomach) (N 2 O 4 +H 2 O→HNO 3 +HNO 2 )
[0030] The ((HNO 3 +HNO 2 The volume ratio of the solvent) / containing solution is not particularly limited, but may be, for example, 0.01 to 0.15, and preferably 0.01 to 0.08. As mentioned above, this NOx recovery process uses water as the NOx absorption liquid, and does not use any chemicals such as chemicals, so costs can be kept low and the NOx-containing liquid can be recovered and reused as a nitric acid solution.
[0031] Furthermore, in the present invention, there is no need to provide a separate step for oxidizing nitrous acid to nitric acid, such as a step of converting nitrous acid to nitric acid using ozone or the like. Both nitrous acid and nitric acid can be reduced in the subsequent reduction step (2), which can shorten the reaction process.
[0032] Next, all or a part of the nitrate / nitrite nitrogen-containing liquid produced in the above NOx recovery process (1) is introduced into the next reduction reaction process (2) (arrow in the main production process in FIG. 1) for treatment. The nitrate / nitrite nitrogen-containing liquid introduced into the reduction reaction step (2) may be all or a part of the nitrate / nitrite nitrogen-containing liquid produced in the above-mentioned NOx recovery step (1). When only a part of the liquid is used, the remaining nitrate / nitrite nitrogen-containing liquid can be introduced into the neutralization step (5) described below. As an example, the nitrate / nitrite nitrogen-containing liquid produced in the above-mentioned NOx recovery step (1) containing 40 volume %, preferably 38 volume %, and more preferably about 35 volume % of the nitrate / nitrite nitrogen-containing liquid can be separated and introduced into the following neutralization step (5) without being introduced into the subsequent reduction reaction step (2).
[0033] The reduction reaction step (2) is a step in which a catalyst having a reducing action is brought into contact with a liquid containing nitrate / nitrite nitrogen under acidic conditions, for example, by adding sulfuric acid produced by bipolar membrane electrodialysis in the catalyst production step (7) described below, to cause a reaction, thereby converting the nitrate / nitrite nitrogen in the liquid containing nitrate / nitrite nitrogen into ammonia.
[0034] As the catalyst having a reducing action used in the reduction reaction step (2), a commercially available magnetic material capable of reducing nitrate nitrogen to ammonia can be used. For example, a spinel ferrite-based (R 1 -Fe 2 O 4 ), hexagonal ferrite (R 2 -Fe 12 O 19 ), Garnet ferrite (R 3 -Fe 5 O 12 ), R 3 -MB,R 3 -MB and the like can be mentioned as examples. In the above structural formula, R1, R2, R3 and M can be exemplified as follows. R 1 : Fe, Mn, Ni, Cu, Zn, R 2 :Ba, Sr, Pb, R 3 :Sc,Y,La,Ce,Pr,Nd,Sm,Gd,Eu,Tb,Dy,Ho,Er,Tm,Yb,Lu, M: Fe, Fe-Co
[0035] In particular, as a catalyst having a reducing action, among magnetic materials, magnetite and / or reduced iron powder (e.g., JIP 300R, manufactured by JFE Steel Corporation) can be suitably used. As such magnetite and reduced iron powder, any commercially available magnetite or reduced iron powder can be used, or, for example, magnetite prepared by effectively utilizing waste heat gas discharged from a cement factory can be used. In the present invention, it is preferable to use magnetite prepared by utilizing exhaust gas from such a cement factory (catalyst production process (7)). The waste heat gas used here differs from exhaust gas and refers to hot gas such as air that is heated outside the cement kiln during the cement manufacturing process and does not contain cement dust or the like.
[0036] Magnetite, which is a reducing catalyst used in the present invention, can be prepared by reacting iron sulfate with sodium hydroxide (reaction formulas (e) to (e)) and subjecting the resulting magnetite and an aqueous sodium sulfate solution to solid-liquid separation (catalyst production step (7)). As the iron sulfate, commercially available iron sulfate can be used, and an example of the iron sulfate is industrial ferrous monohydrate (manufactured by Sakai Chemical Industry Co., Ltd.). Although commercially available sodium hydroxide can be used, in the present invention, for example, sodium hydroxide obtained by bipolar membrane electrodialysis (reaction formula (c)) described below is used. Sulfuric acid can be used in the reduction reaction step (2) as described above. Na 2 SO 4 +2H 2 O → 2NaOH + H 2 SO 4 ···(cormorant)
[0037] In bipolar membrane electrodialysis, an aqueous solution containing sodium sulfate is electrodialyzed (reaction formula (c) above) to produce sulfuric acid and sodium hydroxide. The sodium sulfate produced in the following reaction formula (d) when preparing magnetite is circulated to perform bipolar membrane electrodialysis. In addition, the sulfuric acid obtained by such bipolar membrane electrodialysis can be used to make the reduction reaction step (2) under acidic conditions, and / or can be reacted with unreacted sodium hydroxide after the preparation of magnetite to form sodium sulfate, and can be recycled for the above-mentioned electrodialysis together with the aqueous sodium sulfate solution obtained by solid-liquid separation in the catalyst production step (7). In addition, the sodium hydroxide obtained by bipolar membrane electrodialysis is used to prepare magnetite to be reacted with iron sulfate as shown in the following reaction formula (E). In this way, in the catalyst production process (7), it is possible to circulate and reuse the sodium hydroxide.
[0038] Magnetite is produced by the ferrite method shown in the following reaction formulas (d) to (e) using iron sulfate and sodium hydroxide produced by the above reaction formula (c). In this manufacturing process, for example, waste heat gas is utilized to react iron sulfate with sodium hydroxide at 200 to 250° C., for example, at a pH of 8 to 13. FeSO 4 +2NaOH→Fe(OH) 2 +2Na 2 SO 4 ···(workman) Fe(OH) 2 →Fe 2 O 3 +H 2 +2H 2 O···(O) The magnetite obtained is used as a catalyst having a reducing effect in the reduction reaction step (2).
[0039] Furthermore, when unreacted sodium hydroxide remains after preparing magnetite by the above reaction formulas (d) to (e), the unreacted sodium hydroxide is reacted with sulfuric acid obtained by the above bipolar membrane electrodialysis (reaction formula (c)) to produce sodium sulfate, and the sodium sulfate can be subjected to bipolar membrane electrodialysis treatment together with the sodium sulfate produced by the above reaction formula (d).
[0040] An example of a schematic process for producing magnetite is as follows. Iron sulfate is added to an aqueous sodium hydroxide solution, and the precipitate produced by the above reaction formulas (d) to (e) is filtered using a filter press. Then, the water is evaporated and the precipitate is dried using waste heat gas from a cement factory, for example, at 70°C for about 30 minutes. The precipitate is then pulverized using a coarse pulverizer such as a hammer mill, recovered by magnetic separation, and sieved using a vibrating screen to reduce the particle size to 0.5 mm to 2 mm, thereby preparing pulverized magnetite.
[0041] The chemical composition of the obtained magnetite can be analyzed by component analysis using a fluorescent X-ray analyzer (PRIMUS IV, manufactured by Rigaku Corporation). For example, pulverized magnetite having the following composition can be prepared. Fe:68.3%, O:28.6%, C:1.2%, Mn:1.1%, Al:0.3%, S:0.3%, Si:0.2%
[0042] In addition, the obtained magnetite powder can be further pulverized and then subjected to X-ray diffraction measurement using a powder X-ray diffractometer (X'PartPowder, manufactured by PANalytical) under the following measurement conditions: measurement range: 2θ = 10 to 70°, step size: 0.017°, scan speed: 0.1012° / s, voltage: 45 kV, current: 40 mA, to confirm that it is magnetite. Specifically, the X-ray diffraction profile can be used to confirm that the material is magnetite using crystal structure analysis software (X'Part High Score Plus version 2.1b, manufactured by PANalytical) provided on the powder X-ray diffractometer.
[0043] In addition, the hydrogen generated by the above reactions (d) and (e) can be recycled and reused as a heat source for the burner when preparing cement.
[0044] In the reduction reaction step (2), as described above, nitrate and nitrite nitrogen are reacted with a catalyst having a reducing action, such as magnetite, produced in the catalyst production step (7) under acidic conditions to produce ammonia. For example, a catalyst that reduces magnetite is added to the nitrate / nitrite nitrogen-containing liquid introduced from the NOx recovery process, and a reduction reaction is carried out under acidic conditions, converting all or part of the nitrate / nitrite nitrogen into ammonia. As an example, "a portion" means that 90% by volume, preferably 93% by volume, of the nitrate and nitrite nitrogen is converted to ammonia. In order to efficiently advance the reduction reaction, it is desirable to maintain an equilibrium state so that oxygen does not enter the nitrate / nitrite nitrogen-containing liquid. For example, the reduction reaction may be carried out in a sealed state or in an inert atmosphere.
[0045] As one example, for example, the magnetite obtained in the above catalyst production step (7) and reduced iron are added in a mass ratio of 2:1 to a nitrate / nitrite nitrogen-containing liquid introduced into a reduction reaction step, and the pH of the nitrate / nitrite nitrogen-containing liquid is adjusted to 1.0 to 6.0, preferably 1.0 to 4.0, more preferably 1.0 to 2.0 at room temperature under acidic conditions, and the reduction reaction described below is carried out while stirring for, for example, 1 to 10 hours, preferably 3 to 10 hours. The reduction reaction is shown in the following formulas (f) to (g). HNO 3 +4Fe+5H 2 O→NH 3 +4Fe(OH) 2 ···(mosquito) HNO 2 +3Fe+4H 2 O→NH 3 +3Fe(OH) 2 ···(tree)
[0046] As the additive for promoting the reduction reaction of the above reaction formulas (f) to (g) under acidic conditions, any additive can be used as long as it enables the pH adjustment of the aqueous solution to be acidic and does not affect the treatment of the present invention. For example, hydrochloric acid, sulfuric acid, nitric acid, etc. are suitable. Nitric acid is preferably used, and sulfuric acid obtained by electrodialysis in the above catalyst production step (7) can be used, which is desirable from the viewpoint of recycling.
[0047] More preferably, during the reduction treatment, continuous measurement is performed with an ORP electrode, and the ORP is adjusted to be −500 mV to −200 mV, preferably −500 mV to −400 mV, so that the reduction treatment progresses effectively.
[0048] Next, the liquid containing ammonia and nitrate / nitrite nitrogen obtained in the reduction reaction step (2) is introduced into an ammonia recovery step (3) (indicated by an arrow in the main production step in FIG. 1). Next, the pH of the liquid containing ammonia and nitrate / nitrite nitrogen is adjusted to 8.0 to 14.0, preferably 10.0 to 14.0, with a base, and then distilled using waste heat gas from a cement factory to recover ammonia by heating and vaporizing it (ammonia recovery step (3)). The waste heat gas can be used for vaporizing ammonia in the ammonia recovery step (3) by circulating the waste heat gas used for heating and concentrating ammonium nitrate prepared in the neutralization step (5) described below to precipitate crystals. To recover ammonia by heating and vaporizing it, for example, a stripping method is applied, and the heating temperature is desirably set to 50 to 70°C.
[0049] A part of the vaporized ammonia is introduced into the neutralization step (5) described below, and the remaining vaporized ammonia can be used to improve the purity of ammonium nitrate by reacting with nitrate and nitrite nitrogen remaining in ammonium nitrate obtained by heating and concentrating the ammonium nitrate obtained in the neutralization step (5) described below.
[0050] As the basic agent, any agent can be used as long as it enables the pH of the aqueous solution to be adjusted to a basic state and does not affect the treatment of the present invention. Examples of the basic agent include sodium hydroxide, calcium hydroxide, potassium hydroxide, and magnesium hydroxide. Preferably, sodium hydroxide can be used. For example, sodium hydroxide obtained by electrodialysis in the above catalyst production step (7) can be used, which is desirable from the viewpoint of recycling.
[0051] Furthermore, the iron hydroxide (II) which is the residue generated by the above reaction formulas (f) and (g) is introduced into an ammonia recovery step (3) together with ammonia and a liquid containing nitrate / nitrite nitrogen. After passing through the ammonia recovery step (3), the residue is subjected to solid-liquid separation, and the iron hydroxide from the reduction reaction step (2) and the remaining unused nitrate / nitrite nitrogen are separated into solid and liquid (solid-liquid separation step (4)). The iron hydroxide separated in the solid-liquid separation step (4) becomes iron oxide hydroxide when exposed to air (reaction formula (h) below), and the iron oxide hydroxide can be reused as a cement raw material. 4Fe(OH) 2 +O 2 →4FeO(OH)+2H 2 O (K)
[0052] Next, a portion of the ammonia recovered by vaporization in the ammonia recovery step (3), the nitrate / nitrite nitrogen-containing liquid separated in the solid-liquid separation step (4), and the remaining nitrate / nitrite nitrogen-containing liquid obtained in the nitrogen dioxide recovery step (1) and not introduced into the reduction reaction step (2) are introduced into a neutralization step (5) and subjected to a catalytic reaction to produce ammonium nitrate (for example, 78% purity). In the neutralization step (5), a solution containing the produced ammonium nitrate and excess nitrate and nitrite nitrogen that was not used in the production of ammonium nitrate is obtained. For example, the reaction between nitrate nitrogen and ammonia is represented by the following formula (K), and an ammonium nitrate solution with a concentration of, for example, about 78% can be produced. HNO 3 +NH3 →NH 4 NO 3 ···(K)
[0053] The ammonium nitrate-containing liquid thus obtained is heated and distilled as necessary using waste heat gas, for example by adjusting the temperature to 170 to 180°C, to obtain a suspension containing concentrated ammonium nitrate (for example, 98% purity) and to remove residual nitrate and nitrite nitrogen (HNO 3 +HNO 2 ) is evaporated. 3 and HNO 2 It is preferable to recycle the above-mentioned neutralization step (5) for use. The remaining vaporized ammonia gas that was not introduced into the neutralization step (5) is added to the concentrated ammonium nitrate-containing suspension. By adding such ammonia gas, the suspension (concentrated ammonium nitrate) becomes weakly alkaline, and the nitrate-nitrite nitrogen (HNO 3 +HNO 2 ) the purity of ammonium nitrate can be increased (for example, to about 100%), and then cooled to precipitate ammonium nitrate crystals, which can be isolated. Preferably, such treatment is carried out prior to the granulation step (6) below.
[0054] In addition, the waste heat gas can be used to concentrate and precipitate ammonium nitrate, and then to vaporize ammonia in the ammonia recovery step (3).
[0055] Next, after isolating the ammonium nitrate, granular ammonium nitrate is produced using any commercially available granulator (granulation step (6)). In the granulation step (6), solid ammonium nitrate is mixed with light oil or the like to produce, for example, explosives or blasting materials.
[0056] According to the treatment method of the present invention, nitrogen dioxide contained in cement exhaust gas can be converted into ammonium nitrate and utilized, the content of nitrogen dioxide contained in the cement exhaust gas can be sufficiently reduced to effectively carry out denitration, the environmental burden can also be reduced in the production of a reducing catalyst used in the process of producing ammonium nitrate, waste heat gas during cement production can be utilized, and the residue obtained by the treatment method of the present invention can be effectively used in cement production, thereby forming an environmentally friendly circulation cycle. [Industrial Applicability]
[0057] Since it becomes possible to highly efficiently remove nitrogen dioxide from waste gas discharged from cement factories and form an environmentally friendly circulation cycle, the treatment method of the present invention can be effectively applied to cement factories producing cement.
Claims
1. a nitrogen dioxide recovery step (1) of contacting nitrogen dioxide in the cement exhaust gas with water to allow the water to absorb the nitrogen dioxide and recovering the nitrogen dioxide as a liquid containing nitrate and nitrite nitrogen; Next, a reduction reaction step (2) is performed in which the reduced iron and magnetite are contacted with all or a part of the nitrate / nitrite nitrogen-containing liquid obtained in the nitrogen dioxide recovery step (1) under acidic conditions to produce iron hydroxide and ammonia. Next, an ammonia recovery step (3) is performed in which the ammonia produced in the reduction reaction step (2) is distilled and vaporized using waste heat gas from the cement production process and recovered. a solid-liquid separation step (4) for separating the remainder after recovering ammonia in the ammonia recovery step (3) into a solid-liquid separation step to separate the iron hydroxide from the reduction reaction step (2) that has been subjected to the ammonia recovery step (3) and the unused remainder into nitrate and nitrite nitrogen; A neutralization step (5) of preparing ammonium nitrate by contacting the nitrate / nitrite nitrogen-containing liquid separated in the solid-liquid separation step (4) and the remaining nitrate / nitrite nitrogen-containing liquid obtained in the nitrogen dioxide recovery step (1) and not introduced into the reduction reaction step (2) with ammonia vaporized and recovered in the ammonia recovery step (3); and The magnetite used in the reduction reaction step (2) is prepared by reacting iron sulfate with an aqueous sodium hydroxide solution to produce magnetite and an aqueous sodium sulfate solution, and then separating the magnetite and the aqueous sodium sulfate solution into solid and liquid. The aqueous sodium sulfate solution is separated into sodium hydroxide and sulfuric acid by electrodialysis. The resulting sodium hydroxide is recycled for use in the preparation of magnetite to be reacted with the iron sulfate. A catalyst production step (7) is provided. A method for producing ammonium nitrate using nitrogen dioxide in cement exhaust gas, characterized by:
2. The method for producing ammonium nitrate according to claim 1, wherein the sulfuric acid obtained in the catalyst production step (7) is used to make the reduction reaction step (2) acidic, and / or is reacted with unreacted sodium hydroxide after the preparation of magnetite to produce sodium sulfate, and is recycled for the electrodialysis together with the aqueous sodium sulfate solution obtained by solid-liquid separation in the catalyst production step (7).
3. 3. The method for producing ammonium nitrate according to claim 1 or 2, wherein the hydrogen generated during the preparation of magnetite in the catalyst production step (7) is recycled and utilized as a combustion raw material during the production of cement.
4. The method for producing ammonium nitrate according to claim 1 or 2, further comprising a granulation step (6) of granulating the ammonium nitrate prepared in the neutralization step (5). The method for producing ammonium nitrate using nitrogen dioxide in cement exhaust gas.
5. 3. The method for producing ammonium nitrate according to claim 1 or 2, wherein the iron hydroxide separated in the solid-liquid separation step (4) is converted into iron oxide hydroxide by exposure to air, and the iron oxide hydroxide is used as a cement raw material.
6. In the method for producing ammonium nitrate using nitrogen dioxide in the cement exhaust gas according to claim 1, the ammonium nitrate prepared in the neutralization step (5) is contained in a liquid containing ammonium nitrate and nitrate / nitrite nitrogen, and the liquid is heated and distilled at 170 to 180°C using waste heat gas to concentrate ammonium nitrate, and the remaining nitrate / nitrite nitrogen is vaporized and circulated to the neutralization step (5). A part of the ammonia vaporized in the ammonia recovery step (3) is added to the concentrated ammonium nitrate to react with the unreacted nitrate / nitrite nitrogen mixed in the concentrated ammonium nitrate to improve the purity of ammonium nitrate, and the concentrated ammonium nitrate is cooled to obtain crystallized ammonium nitrate.
Citation Information
Patent Citations
Gorufurenshujono boorukaishusochi
JP1976000432A
Pot type kerosene burner
JP1984063405A
Nitrogen oxide absorbent, regeneration method therefor and nitrogen oxide recovery method
JP2003175315A