Compound semiconductor amplifier and circuit module
The compound semiconductor amplifier addresses transmission loss and heat generation issues by using a semi-insulating substrate with optimized thickness and a metal layer, enhancing performance in the sub-terahertz band.
Patent Information
- Application Number
- JP2023051136
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-28
- Publication Date
- 2024-10-10
- Estimated Expiration
- 2043-03-28
AI Technical Summary
Sub-terahertz band compound semiconductor amplifiers face challenges with transmission loss due to electromagnetic wave propagation within the semi-insulating substrate and increased heat generation due to low power added efficiency, which are exacerbated by the thickness of the semi-insulating substrate.
A compound semiconductor amplifier design with a semi-insulating substrate thickness of λ/4 to λ/2 and a metal layer on the back surface with a sheet resistance of 6 to 1000 Ω/□, which suppresses electromagnetic wave propagation and enhances heat dissipation.
The design effectively reduces transmission loss and heat generation, stabilizing performance in the sub-terahertz band by optimizing substrate thickness and incorporating a metal layer for improved heat diffusion.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a compound semiconductor amplifier and a circuit module. [Background technology]
[0002] In next-generation communications (for example, Beyond 5G / 6G), the use of sub-terahertz radio waves is being considered to achieve communication speeds of over 100 Gbps. For this reason, compound semiconductor amplifiers have attracted attention. Compound semiconductor amplifiers are capable of operating at higher frequencies and with higher output than silicon-based amplifiers, and are therefore expected to be applied to next-generation communications as sub-terahertz semiconductor amplifiers.
[0003] On the other hand, in order to stabilize the high-frequency and high-output characteristics of semiconductor amplifiers used in the sub-terahertz band (sub-terahertz semiconductor amplifiers), it is important to suppress unnecessary electromagnetic radiation in a very wide frequency band, for example, 250-300 GHz. Furthermore, the power-added efficiency of sub-terahertz semiconductor amplifiers is only a few percent, and most of the input power is converted into heat, increasing the amount of heat generated. In addition, beam control using array antennas is essential for mobile communications, but in this frequency band, the size of sub-terahertz semiconductor amplifiers exceeds half the wavelength (λ / 2) of air (the wavelength of a certain frequency in air), so a three-dimensional laminated antenna array structure has been proposed, which is more difficult to form a heat dissipation structure (path) for the amplifier than the planar array antenna structure usually used in the millimeter wave band. For this reason, the heat dissipation structure of sub-terahertz semiconductor amplifiers is important.
[0004] Sub-terahertz semiconductor amplifiers include, for example, high electron mobility transistors (InP-based HEMTs) in which an indium aluminum arsenide (InAlAs) electron supply layer / indium gallium arsenide (InGaAs) channel layer is formed on an indium phosphide (InP) substrate, HEMTs (metamorphic HEMTs, mHEMTs) in which an InAlAs electron supply layer / InGaAs channel layer is formed on a gallium arsenide (GaAs) substrate via a metamorphic buffer layer, and heterojunction bipolar transistors (InP-based HBTs) in which an InP emitter layer / gallium arsenide antimonide (GaAsSb) base layer / In(Al)GaAs collector layer, etc. are formed on an InP substrate. These compound semiconductor amplifiers are capable of operating at higher frequencies and with higher output than silicon-based amplifiers, and are therefore expected to be applied to Beyond 5G / 6G.
[0005] Techniques relating to amplifiers are described in the following patent documents. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] JP 2007-165430 A [Patent Document 2] JP 2011-77557 A [Patent Document 3] JP 2007-165739 A Summary of the Invention [Problem to be solved by the invention]
[0007] However, especially in the frequency band of 250 GHz or more, there are two problems: transmission loss due to electromagnetic wave propagation in the semi-insulating substrate on which these compound semiconductor amplifiers are formed, and an increase in heat generation due to a significant decrease in the power added efficiency. These two problems are in a tradeoff relationship with the thickness of the semi-insulating substrate on which the sub-terahertz compound semiconductor amplifiers are formed, making them difficult to solve.
[0008] Therefore, one disclosure provides a compound semiconductor amplifier and a circuit module that suppresses electromagnetic wave propagation while also suppressing the amount of heat generation. [Means for solving the problem]
[0009] A compound semiconductor amplifier having a compound semiconductor and an amplifier on an upper side of a semi-insulating substrate, the semi-insulating substrate having a substrate thickness that is an internal wavelength of a second range at a first frequency, and a metal layer on a lower surface thereof having a sheet resistance value in a third range, the first frequency being a maximum frequency used in the compound semiconductor amplifier, the second range being 1 / 12 to 1 / 2 the wavelength of the first frequency, and the third range being 3 to 1000 ohms. Effect of the Invention
[0010] One disclosure is capable of suppressing electromagnetic wave propagation while also suppressing the amount of heat generated. [Brief description of the drawings]
[0011] [Figure 1A] FIG. 1A is a diagram illustrating an example of a cross-sectional view of a semiconductor amplifier 100. [Figure 1B] FIG. 1B is a diagram illustrating an example of a top view of the semiconductor amplifier 100. [Figure 2A] FIG. 2A is a diagram illustrating an example of a simulation result in the first embodiment. [Figure 2B] FIG. 2B is a diagram illustrating an example of a simulation result in the first embodiment. [Figure 2C] FIG. 2C is a diagram illustrating an example of a simulation result in the first embodiment. [Figure 2D] FIG. 2D is a diagram illustrating an example of a simulation result in the first embodiment. [Figure 3A] FIG. 3A is a diagram showing an example of a manufacturing process of the semiconductor amplifier 100 according to the first embodiment. [Figure 3B] FIG. 3B is a diagram showing an example of a manufacturing process of the semiconductor amplifier 100 according to the first embodiment. [Figure 3C] FIG. 3C is a diagram showing an example of a manufacturing process of semiconductor amplifier 100 according to the first embodiment. [Figure 3D] FIG. 3D is a diagram showing an example of a manufacturing process of the semiconductor amplifier 100 according to the first embodiment. [Figure 4A] FIG. 4A is a diagram illustrating an example of a cross-sectional view of the semiconductor amplifier 100 according to the second embodiment. [Figure 4B] FIG. 4B is a diagram illustrating an example of a top view of the semiconductor amplifier 100 according to the second embodiment. [Figure 5A] FIG. 5A is a diagram illustrating an example of a simulation result in the second embodiment. [Figure 5B] FIG. 5B is a diagram illustrating an example of a simulation result in the second embodiment. [Figure 5C] FIG. 5C is a diagram illustrating an example of a simulation result in the second embodiment. [Figure 5D] FIG. 5D is a diagram illustrating an example of a simulation result in the second embodiment. [Figure 5E] FIG. 5E is a diagram illustrating an example of a simulation result in the second embodiment. [Figure 5F] FIG. 5F is a diagram illustrating an example of a simulation result in the second embodiment. [Figure 5G] FIG. 5G is a diagram illustrating an example of a simulation result in the second embodiment. [Figure 5H] FIG. 5H is a diagram illustrating an example of a simulation result in the second embodiment. [Figure 6A] FIG. 6A is a diagram showing an example of a manufacturing process of the semiconductor amplifier 100 according to the second embodiment. [Figure 6B] FIG. 6B is a diagram showing an example of a manufacturing process of the semiconductor amplifier 100 according to the second embodiment. [Figure 6C] FIG. 6C is a diagram showing an example of a manufacturing process of semiconductor amplifier 100 according to the second embodiment. [Figure 6D]FIG. 6D is a diagram showing an example of a manufacturing process of the semiconductor amplifier 100 according to the second embodiment. [Figure 6E] FIG. 6E is a diagram showing an example of a manufacturing process of semiconductor amplifier 100 according to the second embodiment. [Figure 6F] FIG. 6F is a diagram showing an example of a manufacturing process of the semiconductor amplifier 100 according to the second embodiment. [Figure 7] FIG. 7 is a diagram showing an example of a conceptual diagram of a three-dimensional laminated structure of an amplifier-integrated array antenna. [Figure 8] FIG. 8 is a diagram showing an example of a circuit module in which a chip having the configuration according to the second embodiment is flip-chip mounted on a high-frequency circuit board. [Figure 9] FIG. 9 is a diagram showing an example of a circuit module in which the back surface of a chip having the configuration according to the second embodiment is mounted on a high-frequency circuit board. [Figure 10] FIG. 10 is a diagram showing an example of Table 1 showing the characteristics of components used in the substrate. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] [First embodiment] A first embodiment will be described.
[0013] <Example of semiconductor amplifier configuration> FIG. 1A is a diagram illustrating an example of a cross-sectional view of a semiconductor amplifier 100, and FIG. 1B is a diagram illustrating an example of a top view of the semiconductor amplifier 100.
[0014] The semiconductor amplifier 100 includes, for example, a semi-insulating substrate 10, a compound semiconductor epitaxial layer 11 grown on the semi-insulating substrate 10, an amplifier 12 fabricated on the compound semiconductor epitaxial layer 11, a wiring layer formed on an interlayer insulating film 13 on the compound semiconductor epitaxial layer 11, the wiring layer including a microstrip wiring 14 and a ground wiring 15, and a metal layer 16. The metal layer 16 is deposited on the back surface of the semi-insulating substrate 10 thinned to a degree of λ / 4 to λ / 2 of a predetermined maximum frequency, and has a sheet resistance of 6 to 1000 Ω / □. For example, in the case of an InP substrate or a GaAs substrate having a dielectric constant of about 12 at 300 GHz, the metal layer 16 has a substrate thickness of about 75 to 150 μm. The predetermined maximum frequency is, for example, the maximum value of the frequency band of a transmission wave when the semiconductor amplifier 100 is used as an antenna. The predetermined maximum frequency is, for example, the maximum value of the frequency band at the output (or input) of the semiconductor amplifier 100.
[0015] The effect of the configuration in which metal layer 16 having a sheet resistance of 6 to 1000 Ω / □ is disposed on the back surface of semi-insulating substrate 10 on which semiconductor amplifier 100 is formed will be described.
[0016] FIG. 2A is a diagram showing an example of a simulation result of the dependency of the transmission characteristics of a microstrip line 14 formed on a semi-insulating substrate 10 having a metal layer 16 on the back surface of the substrate on the sheet resistance of the metal layer 16. In FIG.
[0017] The horizontal axis is frequency, and the vertical axis is maximum available gain (MAG). The semi-insulating substrate 10 is, for example, an InP substrate. The semi-insulating substrate thickness (t1) is, for example, 75 μm. When the metal layer 16 is not present on the rear surface of the semi-insulating substrate, there is a frequency range of 250-350 GHz at which the MAG drops significantly. This is because propagation occurs within the semi-insulating substrate 10 in a specific frequency band, resulting in transmission loss.
[0018] Fig. 2B is a diagram showing an example of an enlarged view of Fig. 2A at 250-300 GHz. As shown in Fig. 2B, if the sheet resistance (Rs) of the metal layer 16 arranged on the back surface of the semi-insulating substrate is in the range of 5.5-1090 Ω / □, the transmission loss due to propagation within the substrate at around 260 GHz is suppressed compared to the case where the metal layer 16 is not present. This is because when an electromagnetic wave is applied to the metal layer 16 with a sheet resistance of about 6-1000 Ω / □, a conduction current flows, the energy of the electromagnetic wave is converted into heat, and the electromagnetic wave that has been deflected is absorbed without being reflected, suppressing the electromagnetic wave propagation within the semi-insulating substrate.
[0019] On the other hand, if the sheet resistance of the metal layer 16 is smaller than 1 Ω / □, for example, the metallic behavior becomes stronger, and there is a possibility that the reflection at the interface between the metal layer 16 and the semi-insulating substrate 10 will increase the loss due to electromagnetic wave propagation within the substrate. Therefore, the preferable sheet resistance is, for example, 10.9 to 109 Ω / □.
[0020] FIG. 2C is a diagram showing an example of a simulation result of the semi-insulating substrate thickness dependency of the transmission characteristics of the microstrip wiring 14 formed on the semi-insulating substrate 10 having the metal layer 16 on the back surface of the substrate. The horizontal axis is frequency, and the vertical axis is MAG. The semi-insulating substrate 10 is, for example, an InP substrate. The sheet resistance of the metal layer 16 is, for example, 55 Ω / □. If the semi-insulating substrate thickness (t1) is in the range of 50 to 150 μm, the loss due to electromagnetic wave propagation in the substrate is suppressed and there is almost no difference in the transmission loss. However, if the semi-insulating substrate thickness is thinner than 25 μm or thicker than 150 μm, the loss in the 300 GHz band becomes large. This is because, if the semi-insulating substrate thickness is thinner than 25 μm, even electromagnetic waves other than unwanted radiation waves are absorbed by the metal layer 16. Also, this is because, if the semi-insulating substrate thickness is thicker than 150 μm, the absorption of unwanted electromagnetic waves by the metal layer 16 becomes weak.
[0021] Furthermore, FIG. 2D is a diagram showing an example of a simulation result of the semi-insulating substrate thickness dependency of the device thermal resistance of the flip-chip mounted compound semiconductor amplifier 100. The output of the sub-terahertz band compound semiconductor amplifier is assumed to be 10 mW, the efficiency is assumed to be 4.8%, and the heat source is assumed to be 0.2 W. The semi-insulating substrate 10 is, for example, an InP substrate. In the case of a conventional millimeter wave band, for example, the 77 GHz band used in automobile collision prevention radars, λ / 4 in the semi-insulating substrate is about 280 μm. In this frequency band, the device thermal resistance can be assumed to be almost constant, but in the above-mentioned sub-terahertz band, for example, in the case of not using the metal layer 16 at 300 GHz, the device thermal resistance rises sharply when the substrate thickness is reduced to about 25 μm, which is sufficient to suppress electromagnetic wave propagation in the substrate. This is because if the thickness of semi-insulating substrate 10, which has a thermal conductivity of less than 100 W / mK, is thinner than 75 μm, the heat reaches the back surface of the substrate before it has had a chance to fully diffuse laterally within the substrate, resulting in a small heat radiation area and poor heat dissipation characteristics. However, by arranging metal layer 16 on the back surface of the substrate, it is possible to increase the thickness of the semi-insulating substrate to 150 μm, which promotes heat diffusion within the semi-insulating substrate and improves heat dissipation characteristics.
[0022] From the above, in a configuration in which a metal layer 16 having a sheet resistance of 6 to 1000 Ω / □ is disposed on the back surface of a semi-insulating substrate 10 on which a compound semiconductor amplifier is formed, the thickness of the semi-insulating substrate that satisfies both electromagnetic wave propagation suppression and heat dissipation is 75 to 150 μm, which corresponds to approximately λ / 4 to λ / 2 at a predetermined maximum frequency of 300 GHz.
[0023] <Example of the manufacturing process for semiconductor amplifiers> 3A shows an example of a manufacturing process of the semiconductor amplifier 100. First, as shown in FIG. 3A, a compound semiconductor epitaxial layer 11 having a thickness of about 0.5 μm and made of an InP-based HEMT structure grown on an InP semi-insulating substrate, an amplifier 12 including a gate electrode, a source electrode, a drain electrode, an MIM capacitor, a NiCr resistor layer, etc., and a wafer having a ground microstrip wiring structure and planarized using a BCB interlayer insulating film having a thickness of about 6 μm are manufactured.
[0024] Next, as shown in FIG. 3B, an adhesive is applied to the wafer surface, and the wafer is attached to a support substrate, and then the rear surface of the InP substrate is ground to a thickness of 100 μm. The substrate thickness may be, for example, in the range of 75 to 150 μm. Chemical mechanical polishing (CMP) may or may not be performed. When CMP is performed, the substrate thickness after grinding is, for example, the sum of the final substrate thickness and the film thickness removed by CMP. Specifically, for example, when 10 μm is removed by CMP, if the final substrate thickness is 100 μm, the substrate thickness after grinding will be 110 μm.
[0025] Next, as shown in Figure 3C, for example, titanium (Ti) is deposited to a thickness of 13 nm on the backside of the InP substrate using vacuum deposition or sputtering. After removing the substrate from the vacuum device, the Ti layer is naturally oxidized to a thickness of about 3 nm, resulting in a sheet resistance of about 55 Ω / □.
[0026] Next, as shown in Fig. 3D, the wafer is peeled off from the support substrate, the adhesive is removed with an organic solvent, and the back surface of the wafer is attached to a dicing tape and cut into chips using a conventional blade dicing.
[0027] In the above example, an InP-based HEMT on an InP substrate was described, but an InP-based HBT on an InP substrate, an mHEMT on a GaAs substrate, or a GaN-based HEMT on gallium nitride (GaN), aluminum nitride (AlN), or SiC may also be used. Therefore, GaAs, InP, GaN, AlN, or SiC can be used for the semi-insulating substrate 10.
[0028] In the above example, the microstrip wiring 14 is described, but a coplanar or grounded coplanar wiring structure may be used. As the interlayer insulating film 13, methyl silsesquioxane (MSQ) or polyimide may be used in addition to BCB.
[0029] As the metal layer 16, other than Ti as in the above example, W, Mo, Ta, NiCr, Cr, Pt, Al, Au, Cu, Ag, etc. may be used. Also, a laminate of these may be used. The film thickness of the metal layer 16 is preferably 6 nm or less for W, 20 nm or less for Ta, 3 nm or less for Au, 3 nm or less for Cu, 3 nm or less for Ag, 3 nm or less for Al, 20 nm or less for Cr, 20 nm or less for Pt, 10 nm or less for Mo, and 200 nm or less for NiCr. However, since a natural oxide film is formed to a thickness of about several nm, the film thickness may be determined by the sheet resistance of the finished product.
[0030] The compound semiconductor amplifier 100 fabricated as described above can suppress the propagation of electromagnetic waves within the semi-insulating substrate, while achieving good heat dissipation characteristics.
[0031] [Second embodiment] A second embodiment will now be described.
[0032] <Example of semiconductor amplifier configuration> Fig. 4 is a diagram showing an example of a configuration of a semiconductor amplifier 100 in the second embodiment. Fig. 4A is a diagram showing an example of a cross-sectional view of the semiconductor amplifier 100, and Fig. 4B is a diagram showing an example of a top view of the semiconductor amplifier 100.
[0033] Semiconductor amplifier 100 further includes high heat dissipation substrate 17 in addition to semiconductor amplifier 100 of the first embodiment. Semiconductor amplifier 100 has semi-insulating substrate 10 thinned to an extent of λ / 12 to λ / 2 of a predetermined maximum frequency and a high heat dissipation substrate having a higher thermal conductivity than semi-insulating substrate 10 and the same or higher insulation properties bonded together by metal layer 16 having a sheet resistance of 3 to 1000 Ω / □.
[0034] For example, in the case of an InP substrate or a GaAs substrate with a dielectric constant of about 12 at 300 GHz, the semi-insulating substrate 10 has a substrate thickness of about 25 to 150 μm. In addition, the high heat dissipation substrate is, for example, a silicon carbide (SiC) substrate with a higher thermal conductivity, higher resistivity (insulation), and smaller dielectric loss than an InP or GaAs substrate. The substrate thickness may be within 1 λ within the high heat dissipation substrate. For example, in the case of a SiC substrate with a dielectric constant of 9.74 at 300 GHz (see Table 1 in FIG. 10), the substrate thickness is within about 300 μm. In addition, other high heat dissipation substrates may be, for example, gallium nitride (GaN), aluminum nitride (AlN), diamond, etc. (see Table 1 in FIG. 10).
[0035] Next, the effect of the configuration in compound semiconductor amplifier 100 in which metal layer 16 having a sheet resistance of 3 to 1000 Ω / □ is disposed at the bonding interface between semi-insulating substrate 10 formed thereon and a high heat dissipation substrate having a higher thermal conductivity than semi-insulating substrate 10 and equivalent or higher insulation properties will be described.
[0036] 5A and 5B are diagrams showing examples of simulation results of the sheet resistance dependency of the metal layer 16 of the transmission characteristics of the microstrip wiring 14 formed on the semi-insulating substrate joined to the high heat dissipation substrate by the metal layer 16. The horizontal axis is frequency and the vertical axis is MAG. The semi-insulating substrate 10 is, for example, an InP substrate, and the high heat dissipation substrate is, for example, a SiC substrate. The thicknesses (t1) of the semi-insulating substrate 10 are 25 μm (a) and 75 μm (b), respectively, and the high heat dissipation substrate thickness (t2) is 100 μm.
[0037] 5A, when there is no metal layer 16 at the interface between the semi-insulating substrate 10 and the high heat dissipation substrate, there are multiple frequencies at which the MAG drops significantly in the range of 250-350 GHz. This is because electromagnetic waves propagate into the semi-insulating substrate 10 and the high heat dissipation substrate in certain frequency bands, resulting in transmission losses.
[0038] 5C and 5D are diagrams showing examples of enlarged views of FIG. 5A and FIG. 5B at 250-300 GHz, respectively. According to FIG. 5A and FIG. 5B, when the sheet resistance (Rs) of the metal layer 16 at the interface between the semi-insulating substrate 10 and the high heat dissipation substrate is in the range of 2.75 to 1090 Ω / □, the transmission loss due to electromagnetic wave propagation in the substrate is suppressed more than when the metal layer 16 is not present, even when the semi-insulating substrate thickness (t1) is 25 μm or 75 μm. However, when the sheet resistance of the metal layer 16 is about 1 Ω / □, the MAG decreases at a semi-insulating substrate thickness (t1) of 25 μm and around 280 GHz, and at 75 μm and around 260 GHz. As a result, the preferable sheet resistance is, for example, 5.5 to 550 Ω / □ when t1=25 μm, and 11 to 55 Ω / □ when t1=75 μm.
[0039] 5E and 5F are diagrams showing examples of simulation results of the dependence of the transmission characteristics of the microstrip wiring 14 formed on the semi-insulating substrate joined to the high heat dissipation substrate by the metal layer 16 on the high heat dissipation substrate thickness. The horizontal axis is frequency, and the vertical axis is MAG. The semi-insulating substrate 10 is, for example, an InP substrate, and the high heat dissipation substrate is, for example, a SiC substrate. The semi-insulating substrate thickness (t1) is, for example, 25 μm (e) or 75 μm (f). The sheet resistance of the metal layer 16 is, for example, 55 Ω / □. According to FIG. 5E and FIG. 5F, it can be seen that when the high heat dissipation substrate thickness (t2) is in the range of 50 to 350 μm, the transmission loss due to electromagnetic wave propagation in the substrate can be suppressed for both the semi-insulating substrate thickness (t1) of 25 μm and 75 μm.
[0040] FIG. 5G is a diagram showing an example of a simulation result of the semi-insulating substrate thickness dependency of the transmission characteristics of the microstrip wiring 14 formed on the semi-insulating substrate joined to the high heat dissipation substrate by the metal layer 16. The horizontal axis is frequency, and the vertical axis is MAG. The semi-insulating substrate 10 is, for example, an InP substrate, and the high heat dissipation substrate is, for example, a SiC substrate. The high heat dissipation substrate thickness (t2) is, for example, 100 μm. The sheet resistance of the metal layer 16 is, for example, 55 Ω / □. According to FIG. 5G, if the semi-insulating substrate thickness (t1) is in the range of 50 to 150 μm, the loss due to electromagnetic wave propagation in the substrate is suppressed and there is almost no difference in the transmission loss. However, it can be seen that the transmission loss increases when the semi-insulating substrate thickness is thinner than 25 μm or thicker than 150 μm.
[0041] FIG. 5H is a diagram showing an example of a simulation result of the dependency of the device thermal resistance of the compound semiconductor amplifier 100 formed on a semi-insulating substrate bonded to the high heat dissipation substrate with a metal layer 16 on the high heat dissipation substrate thickness. As in the first embodiment, flip-chip mounting is used. Also, assuming an output of 10 mW and an efficiency of 4.8% for the sub-terahertz band compound semiconductor amplifier, the heat source is set to 0.2 W. The semi-insulating substrate 10 is, for example, an InP substrate, and the high heat dissipation substrate is, for example, a SiC substrate. The thickness (t1) of the semi-insulating substrate is, for example, 25 μm or 75 μm. Also, assuming that surface activated bonding (SAB) or atomic diffusion bonding (ADB) is used for bonding, the thermal resistance of the bonding interface is 5×10 -8 m 2The bonding is performed in a vacuum, and the bonding metal layer is not in direct contact with air, so it is possible to prevent oxidation and stabilize the sheet resistance. From FIG. 5H, it can be seen that the device thermal resistance drops rapidly when the high heat dissipation substrate thickness (t2) is 30 μm or more. On the other hand, it can be seen that the device thermal resistance is lower when the semi-insulating substrate thickness (t1) is 25 μm than when it is 75 μm, which is different from the tendency of the first embodiment. This is because the heat dissipation efficiency is higher when the heat is transferred quickly to the high heat dissipation substrate with high thermal conductivity (490 W / mK) via the bonding metal layer and the heat is diffused laterally in the high heat dissipation substrate than when the heat is diffused laterally in the semi-insulating substrate with low thermal conductivity (68 W / mK).
[0042] From the above, the thickness of the semi-insulating substrate that can suppress electromagnetic wave propagation and dissipate heat is preferably, for example, 25 to 150 μm, which corresponds to about λ / 12 to λ / 2 at the maximum predetermined frequency of 300 GHz. Also, the thickness of the high heat dissipation substrate is preferably, for example, 50 to 350 μm, which corresponds to about λ / 6 to 1λ at the maximum predetermined frequency of 300 GHz.
[0043] <Example of the manufacturing process for semiconductor amplifiers> 6A to 6C are diagrams showing an example of a manufacturing process for the semiconductor amplifier 100. Note that the formation of the front side device in FIG. 6A is similar to that in FIG. 3A in the first embodiment.
[0044] Next, as shown in FIG. 6B, an adhesive is applied to the wafer surface and the wafer is attached to a support substrate, after which the back surface of the InP substrate is ground to reduce the thickness of the InP substrate to 85 μm. Furthermore, 10 μm is removed by CMP to reduce the surface roughness (Ra) of the InP substrate to less than 1 nm. This results in a final InP substrate thickness of 75 μm. The final InP substrate thickness may also be in the range of 25 to 150 μm.
[0045] On the other hand, as shown in Figure 6C, an adhesive is applied to the wafer surface of the SiC substrate, which is a high heat dissipation substrate, and after it is attached to a support substrate, the SiC substrate is ground to a thickness of 100 μm. Furthermore, the surface roughness (Ra) of the SiC substrate is made less than 1 nm by CMP. Because the SiC substrate is a very hard material, it is hardly ground by CMP. As a result, the final SiC substrate thickness is also 100 μm.
[0046] In addition, when the silicon (Si) surface side of the SiC substrate is the front side, the carbon (C) surface side is the back side, but either surface may be used. If the final thickness of the SiC substrate is about 300 μm, the process of attaching it to a support substrate may not be necessary. The thickness of the SiC substrate may be in the range of 50 to 350 μm.
[0047] Next, as shown in Figure 6D, the two wafers described above are subjected to atomic diffusion bonding in a vacuum device. First, 5 nm of Ti is deposited simultaneously on the backsides of both wafers. Then, both wafers are pressed down with a certain pressure to bond the Ti layers deposited on the backsides of both wafers. Figure 6E shows an example after bonding.
[0048] At this time, a 10 nm thick Ti layer is formed at the bonding interface between the InP substrate and the SiC substrate, and the sheet resistance is 55 Ω / □. The Ti layer present at the bonding interface only needs to be 100 nm or less.
[0049] Next, as shown in Fig. 6F, the bonded wafer is peeled off from the support substrate, and the adhesive is removed with an organic solvent. After that, the back surface of the SiC substrate is attached to a dicing tape (not shown), and the SiC substrate is diced into chips by ultrasonic blade dicing.
[0050] In the above example, an InP-based HEMT on an InP substrate has been described, but an InP-based HBT on an InP substrate, an mHEMT on a GaAs substrate, or a GaN-based HEMT on a GaN, AlN, or SiC substrate may be used. When a GaAs or InP substrate is used as the semi-insulating substrate 10, GaN, AlN, SiC, or diamond may be used as the high heat dissipation substrate. When a GaN substrate is used as the semi-insulating substrate 10, an AlN, SiC, or diamond substrate may be used as the high heat dissipation substrate. When an AlN substrate is used as the semi-insulating substrate 10, a SiC or diamond substrate may be used as the high heat dissipation substrate. When a SiC substrate is used as the semi-insulating substrate 10, a diamond substrate may be used as the high heat dissipation substrate.
[0051] In the above example, the microstrip wiring 14 is used, but a coplanar or grounded coplanar wiring structure may be used. As the interlayer insulating film 13, methyl silsesquioxane (MSQ) or polyimide may be used in addition to BCB.
[0052] Also, other than Ti, W, Mo, Ta, NiCr, Cr, Pt, Al, Au, Cu, and Ag may be used as the metal layer 16. A laminate of these may also be used. In this case, the film thickness of the metal layer 16 after bonding is 6 nm or less for W, 20 nm or less for Ta, 3 nm or less for Au, 3 nm or less for Cu, 3 nm or less for Ag, 3 nm or less for Al, 20 nm or less for Cr, 20 nm or less for Pt, 10 nm or less for Mo, and 200 nm or less for NiCr.
[0053] In the above example, the atomic diffusion bonding technique is used for bonding, but it is also possible to deposit a metal on the back surface of the wafer and then use a surface activated bonding technique for bonding.
[0054] The semiconductor amplifier 100 manufactured as described above makes it possible to suppress electromagnetic wave propagation within the semi-insulating substrate 10 and the high heat dissipation substrate, while stabilizing the heat dissipation characteristics and the sheet resistance of the metal layer 16.
[0055] [Third embodiment] A third embodiment will be described below. In the third embodiment, an example of a circuit module applied to an amplifier-integrated array antenna three-dimensional laminated structure will be described.
[0056] FIG. 7 is a diagram showing an example of a conceptual diagram of a three-dimensional laminated structure of an amplifier-integrated array antenna. The structure is such that four 1×4 amplifier-integrated array antennas, each having an antenna, a compound semiconductor amplifier 100, and a phase shifter or mixer arranged on a single high-frequency circuit board, are laminated vertically. In this case, in order to suppress unnecessary grating lobes, the antenna spacing is set to less than one wavelength (λ) of air in both the horizontal and vertical directions. Preferably, it is set to λ / 2. In other words, control of the thickness in the vertical direction is important.
[0057] 8 is a diagram showing an example of a circuit module in which a chip having the configuration of the second embodiment is flip-chip mounted on a high-frequency circuit board. The high-frequency circuit board is, for example, a high-frequency circuit board including a Si substrate of the prior application (application number: 2022-056168), a back metal formed on the back surface of the Si substrate, a primary ground metal connected to the back metal by a Si substrate through-via, a resin layer such as polyimide formed on the primary ground metal, and a surface metal connected to the primary ground metal by a via penetrating the resin layer.
[0058] The high-frequency circuit board is supported by silicon interposers and metal pillars (not shown) at the top and bottom. The high-frequency circuit board thickness (s1) is 245 μm. The bump height (b1) is 15 μm. The device layer thickness (d1) is 10 μm in the case of an InP-based HEMT. The antenna interval (a1) is 1 mm (1000 μm) when the antenna interval (a1) is 1 λ at the predetermined maximum frequency of 300 GHz, and the difference is 730 μm. The film thickness of the metal layer 16 is negligible because it is less than 0.2 μm at most. The sum of the SiC substrate thickness (t2) and the InP substrate thickness (t1) in the second embodiment is 500 μm at most. On the other hand, when the antenna interval (a1) is λ / 2 (500 μm), the difference is 230 μm. In the second embodiment, as long as the sum of the SiC substrate thickness (t2) and the InP substrate thickness (t1) is less than 230 μm, mounting is possible. For example, even if the InP substrate thickness is 75 μm, the SiC substrate thickness can be up to 150 μm. In addition, a TIM (Thermal Interface Material) material may be sandwiched between the back surface of the amplifier 12 chip flip-chip mounted on the high-frequency circuit board and the high-frequency circuit board above it. In addition, since the substrate thickness of the chip in the configuration in the first embodiment is a maximum of 150 μm, mounting is easy.
[0059] FIG. 9 is a diagram showing an example of a circuit module in which the back surface of a chip having the configuration of the second embodiment is mounted on a high-frequency circuit board. A general LTCC (Low Temperature Co-fired Ceramics) board is used as the high-frequency circuit board. This high-frequency circuit board is supported by metal pillars (not shown) on the top and bottom. The high-frequency circuit board is configured with multilayer wiring embedded in a ceramic layer, a surface metal (ground only) connected to the back metal by vias, and a metal plate for heat dissipation embedded in a position where the surface metal and the surface of the compound semiconductor amplifier chip are flush (minus the mounting material). The metal plate is copper (Cu). When the surface metal of the high-frequency circuit board and the microstrip and ground wiring of the compound semiconductor amplifier 100 are connected by wire bonding, the wiring height (w1) is about 90 μm in loop height. If the antenna interval (a1) is 1 λ (1 mm) at a predetermined maximum frequency of 300 GHz, the difference is 910 μm. The high frequency circuit board thickness (c1) is set to 900 μm, allowing for a 10 μm margin to prevent contact with the back metal of the upper high frequency circuit board. The device layer thickness (d1) is 10 μm in the case of an InP-based HEMT. When the amplifier chip is mounted on a metal plate with Ag paste, the mounting thickness (p1) is 25 μm. Since the sum of the SiC substrate thickness (t2) and the InP substrate thickness (t1) in the second embodiment is 500 μm at most, the metal plate thickness (m1) is 415 μm, which functions properly as a heat sink. On the other hand, when the antenna interval (a1) is λ / 2 (500 μm), the high frequency circuit board thickness (c1) is 400 μm. In this case, if the metal plate thickness (m1) is halved to 200 μm, the difference is 200 μm. In the second embodiment, mounting is possible as long as the sum of the SiC substrate thickness (t2) and the InP substrate thickness (t1) is less than 165 μm, which is obtained by subtracting the mounting thickness (p1) of 25 μm and the device layer thickness (d1) of 10 μm. For example, even if the SiC substrate thickness is 100 μm, the InP substrate thickness can be up to 65 μm.
[0060] As described above, the circuit module in the third embodiment can vertically stack high-frequency circuit boards, each mounting a semiconductor amplifier having the configurations of the first and second embodiments, at intervals of λ / 2 to λ of air, thereby enabling beam control with suppressed grating lobes in an array antenna to which the circuit module is applied.
[0061] In the third embodiment, by equipping a transceiver with an array antenna to which the circuit module is applied, it is possible to provide, for example, communication system equipment for Beyond 5G / 6G.
[0062] [Other embodiments] For example, the circuit module in the third embodiment may include both the semiconductor amplifier 100 in the first embodiment and the semiconductor amplifier 100 in the second embodiment, depending on the cost and the purpose of use.
[0063] In addition, the components in each embodiment are not limited to the substances described in the examples. For example, the components may be replaced with other substances having similar actions, effects, or properties. [Explanation of symbols]
[0064] 10: Semi-insulating substrate 11: Compound semiconductor epitaxial layer 12: Amplifier 13: Interlayer insulating film 14: Microstrip wiring 15: Ground wiring 16: Metal layer 17: High heat dissipation board 100: Compound semiconductor amplifier
Claims
1. A compound semiconductor amplifier having a compound semiconductor and an amplifier on an upper side of a semi-insulating substrate, the semi-insulating substrate has a substrate thickness within a second range of wavelengths at a first frequency; a metal layer having a sheet resistance value in a third range on a lower surface; the first frequency is a maximum frequency used in the compound semiconductor amplifier, the second range is from 1 / 12 to 1 / 2 of the wavelength of the first frequency; The third range is from 3 to 1000 ohms. Compound semiconductor amplifier.
2. the second range is from ¼ to ½ of a wavelength of the first frequency; The third range is from 6 to 1000 ohms.
2. The compound semiconductor amplifier according to claim 1.
3. the metal layer has a high heat dissipation substrate opposite the semi-insulating substrate; The high heat dissipation substrate has a thermal conductivity higher than that of the semi-insulating substrate and a resistivity equal to or higher than that of the semi-insulating substrate.
2. The compound semiconductor amplifier according to claim 1.
4. The semi-insulating substrate composition includes gallium arsenide, indium phosphide, gallium nitride, aluminum nitride, or silicon carbide.
2. The compound semiconductor amplifier according to claim 1.
5. The composition of the high heat dissipation substrate includes gallium nitride, aluminum nitride, silicon carbide, or diamond.
4. The compound semiconductor amplifier according to claim 3.
6. The high heat dissipation substrate has an internal substrate thickness that is 1 / 6 to 1 of the wavelength of the first frequency.
4. The compound semiconductor amplifier according to claim 3.
7. The composition of the metal layer includes titanium, tungsten, molybdenum, tantalum, nichrome, chromium, platinum, aluminum, gold, copper, silver, or a laminate thereof.
2. The compound semiconductor amplifier according to claim 1.
8. A circuit module in which high-frequency circuit boards on which compound semiconductor amplifiers are mounted are stacked at intervals of 1 / 2 to 1 wavelength in air at a first frequency, the compound semiconductor amplifier includes a compound semiconductor and an amplifier on an upper side of a semi-insulating substrate, the semi-insulating substrate having a substrate thickness that corresponds internally to a second range of wavelengths at the first frequency, and a metal layer on a lower surface thereof, the metal layer having a sheet resistance value in a third range; the first frequency is a maximum frequency used in the compound semiconductor amplifier, the second range is from 1 / 12 to 1 / 2 of the wavelength of the first frequency; The third range is from 3 to 1000 ohms. Circuit module.
9. the metal layer has a high heat dissipation substrate opposite the semi-insulating substrate; the high heat dissipation substrate has a thermal conductivity higher than that of the semi-insulating substrate and a resistivity equal to or higher than that of the semi-insulating substrate; The sum of the thickness of the semi-insulating substrate and the thickness of the high heat dissipation substrate is in a fourth range. The circuit module according to claim 8.
10. The fourth range is from 75 to 500 micrometers. The circuit module of claim 9.
Citation Information
Patent Citations
Semiconductor integrated circuit
JP2000269429A
Semiconductor device and its manufacturing method
JP2001257234A
Circuit module
JP2007165430A
Electronic device and semiconductor device
JP2007165739A
Circuit module
JP2011077557A