Method for producing oxidation product by multitubular reactor
By varying the raw material gas supply rate and using inert materials with specific particle sizes and baffles, the method addresses hot spots and inefficient gas distribution in shell-and-tube reactors, ensuring stable and high production rates of oxidation products.
Patent Information
- Application Number
- JP2023051354
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-28
- Publication Date
- 2024-10-10
- Estimated Expiration
- 2043-03-28
AI Technical Summary
Existing shell-and-tube reactors face challenges in maintaining high production rates of oxidation products due to hot spots and inefficient raw material gas distribution, leading to decreased yields and potential runaway reactions.
Implementing a method to vary the raw material gas supply rate uniformly across reaction tubes in a multitubular reactor by controlling the relative standard deviation of gas supply within a specific range, using inert materials with varying particle sizes and baffles to manage heat distribution.
This approach maintains a high and stable production rate of oxidation products over time, preventing hot spots and enhancing yield by optimizing gas distribution and heat management.
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for producing an oxidation product using a multi-tubular reactor. The present invention relates to a method for producing an oxidation product using a multi-tubular reactor that improves the production amount of the oxidation product in a simple manner. do. [Background technology]
[0002] Acrolein is produced by catalytic gas-phase oxidation of unsaturated hydrocarbons such as propylene and isobutylene. Unsaturated aldehydes such as methacrolein, and unsaturated carboxylates such as acrylic acid and methacrylic acid. For commercial production of acid, a multi-tube reactor is usually used. The well contains multiple reaction tubes, and oxidation is carried out by a heat transfer medium circulating inside the cylindrical shell. Efforts are made to control the heat generated by the reaction.
[0003] On the other hand, with the recent expansion of market demand for chemical products, two measures are being considered. The problem is the enlargement of the multi-tube reactor. In Patent Document 1, the reactor has two fan-shaped tube plates and both ends are fixed to them. The reaction tubes and the plates covering their sides are manufactured in the equipment manufacturing plant. The method is to transport them to a chemical plant and combine them in the chemical plant to form a cylindrical reactor. However, the cost of production is relatively high and the production period is long, so In reality, this method is only used when transportation to the scientific plant is an issue.
[0004] Another approach is to increase the production capacity in existing multi-tube reactors. In the case of a gas-type reactor, the costs of manufacturing and installing new equipment and removing existing equipment are high. Therefore, it is preferable to continue using the existing multi-tubular reactor. With the increase in production, the biggest concern is the occurrence of hot spots. The temperature of the catalyst bed, which is the site of the oxidation reaction in the reaction tube and is filled with solid catalysts, increases as the temperature of the catalyst bed increases. The temperature rises because the removal is insufficient, and the temperature rise in the catalyst layer further increases the oxidation reaction rate. This leads to a vicious cycle in which the heat generated by the oxidation reaction increases even more. In the case of the partial oxidation of the raw material to obtain the desired oxidation product, the amount of carbon monoxide and This accelerates side reactions that produce carbon dioxide and the like, resulting in a significant decrease in the yield of the oxidation product. If the temperature continues to rise, it will lead to an uncontrollable runaway reaction, and the oxidation reaction in the multi-tubular reactor will stop. Replacement of deteriorated solid catalysts due to shutdowns and prolonged exposure to excessive temperatures To be rotten.
[0005] Conventionally, methods for suppressing hot spots have been proposed. A disk-and-doughnut type baffle is used, and the heat medium supply and heat to the multi-tubular reactor are also By using an annular conduit for medium withdrawal, the flow of the heat medium in the radial direction of the multi-tubular reactor and The method for uniformly forming a flow of a heat transfer medium perpendicular to the reaction tube is shown. In addition to the method described in Patent Document 2, Patent Document 3 uses a simulation based on a thermodynamic method. The heat transfer coefficient of the heat medium, i.e., the heat removal capacity, is calculated and the value is multiplied by 1000W / (m 2 ·K) In Patent Document 4, a method for suppressing hot spots is shown. By setting the outer diameter and wall thickness of the reaction tube to a predetermined value or less, the amount of catalyst packed in each reaction tube and By equalizing the amount of reaction gas flowing through each reaction tube, the amount of heat generated in each reaction tube is uniform. A method for suppressing spots is disclosed. Patent Document 5 discloses a method for suppressing spots in a reaction tube filled with a catalyst. Adjust the pressure difference that occurs when a constant flow rate of gas is passed through all reaction tubes to within ±20%. This makes it possible to equalize the amount of raw gas flowing through each reaction tube and the amount of heat generated by each reaction tube, thereby eliminating hot spots. Patent Document 6 discloses a method for suppressing the thermodynamic simulation described in Patent Document 3. Based on the simulation, the catalyst packing specifications (type of catalyst) were adjusted for the reaction tube with a low heat transfer coefficient. In addition, reaction tubes with extremely low heat transfer coefficients should be closed. A method for suppressing hot spots is shown in which the supply of source gas is stopped. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] Japanese Patent Application Publication No. 52-43778 [Patent Document 2] Japanese Unexamined Patent Publication No. 48-80473 [Patent Document 3] JP 2004-83430 A [Patent Document 4] JP 2004-944 A [Patent Document 5] JP 2003-252807 A [Patent Document 6] JP 2003-206244 A Summary of the Invention [Problem to be solved by the invention]
[0007] By using the various methods described above, it is possible to uniformly supply raw gas to each reaction tube in a multi-tubular reactor. In the method of increasing the amount of gas, the amount of oxidation product obtained by the gas-phase oxidation reaction is increases in proportion to the increase in the amount of raw gas, but the amount of oxidation products decreases over time. As a result, it was found that the amount of oxidation products was ultimately reduced compared to before the increase in the amount of raw material gas.
[0008] The present invention improves the above-mentioned problems and produces oxidants by gas-phase catalytic oxidation using a multi-tube reactor. In the method for producing an oxidation product, it is possible to continuously maintain a high production rate to obtain an oxidation product. The purpose is to provide a way in which this can be done. [Means for solving the problem]
[0009] As a result of intensive research into solving the above problems, the present inventors have found that The idea of increasing the amount of raw gas supplied as evenly as possible was reviewed, and the amount of gas supplied to the entire multi-tubular reactor was increased. Even if the amount of raw gas supplied is increased, some reaction tubes, especially those with relatively poor heat removal capacity, By reducing the amount of raw gas supplied, the amount of oxidation product produced per unit time can be increased. It was found that an increase was possible.
[0010] The present invention has been achieved based on these findings, and has the following gist.
[0011] [1] A preheating layer filled with an inert material and a catalyst layer filled with a solid catalyst. In a multi-tubular reactor in which a plurality of reaction tubes are accommodated in a cylindrical shell, While circulating the heat transfer medium, the raw material gas is supplied to the preheating layer of each reaction tube, and catalytic gas phase oxidation is performed in the catalyst layer. A method for producing an oxidation product by a chemical reaction, comprising: The feed rate per unit of time is not uniform among all reaction tubes, but is calculated by the following formula (1) for each reaction tube. The relative standard deviation (σ) of the feed rate of the raw gas supplied to the preheating layer is 0.3% or more and 3% or less. A method for producing an oxidation product comprising the steps of:
[0012] Relative standard deviation (σ) of the feed rate of the raw gas supplied to the preheating layer of each reaction tube = Standard deviation (s) of the feed rate of the raw gas supplied to the preheating layer of each reaction tube / per reaction tube Average feed gas flow rate to the preheater (1) Here, the standard deviation (s) of the raw material gas supply rate supplied to the preheating layer of each reaction tube is expressed as follows: will be done.
[0013]
number
[0014] [2] Some reactors have a larger average particle size of the inert material packed in the preheat layer than other reactors. In the reaction tube (hereinafter referred to as "reaction tube A"), the average particle size of the inert material packed in the preheating layer is smaller than that of the inert material packed in the preheating layer. The number of reaction tubes A is 0.5% or more and 30% or less of the total number of reaction tubes in the multi-tubular reactor. The method for producing an oxidation product according to [1], [3] A disk-and-donut type valve is provided in the heat transfer medium circulation path in the cylindrical shell. The method for producing an oxidation product according to [1] or [2], wherein the baffle is a circular or partially circular baffle. . [4] The reaction tube A is located near the center and / or near the outside of the cylindrical shell. A method for producing an oxidation product according to [2] or [3]. [5] The preheating layer of the reaction tube A is divided into two layers, and the preheating layer on the raw gas supply side is packed with The average particle size of the inert material packed in the preheating layer on the raw gas exhaust side is The method for producing an oxidation product according to any one of [2] to [4], wherein the average particle size is smaller than the average particle size. [6] The reaction layer of the reaction tube A is filled with a mixture of a solid catalyst and an inert material. The average particle size of the inactive substance is 0.5 to 1.5 times the average particle size of the solid catalyst. The method for producing an oxidation product according to any one of [2] to [5], wherein the oxidation reaction is less than 0 times. [7] The raw material gas contains an olefin, and the oxidation product contains an unsaturated aldehyde. A method for producing an oxidation product according to any one of [1] to [6]. [8] The raw material gas contains an unsaturated aldehyde, and the oxidation product is an unsaturated carboxylic acid. A method for producing an oxidation product according to any one of [1] to [6], comprising: Effect of the Invention
[0015] According to the present invention, the amount of raw material gas supplied to some of the reaction tubes in the multi-tubular reactor is reduced. This enabled the production of oxidation products at a continuously high rate. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0016] Hereinafter, the embodiment of the present invention will be described in detail. Note that the present invention is not limited to the following description. The present invention is not limited to the above, and various modifications can be made within the scope of the present invention.
[0017] The multi-tubular reactor used in the production method of the present invention contains multiple reaction tubes in a cylindrical shell. The number of the reaction tubes is preferably 10,000 or more. It is preferable that the number of the fibers is 13,000 or more, and more preferable that the number of the fibers is 20,000 or more. The upper limit is preferably 80,000, and more preferably 60,000. By setting the number of the tubes within the above range, the multi-tubular reactor is economical and safe. In addition, the arrangement of the reaction tubes is such that each reaction tube is In order to equalize the spacing between adjacent reaction tubes, both ends of the reaction tubes are attached to the tube plate in a staggered manner. It is preferable that the electrodes are staggered at 45°, and more preferable that the electrodes are staggered at 60°. It is more preferable that the reaction tubes are arranged in a staggered manner. The packing density of the inert material or solid catalyst inside the reactor may become uneven, and the gas may flow unevenly. In order to avoid this, it is preferable that the reaction tubes are cylindrical. Therefore, it is preferable that the inner diameter of the tube is uniform. In addition, the reaction may vary in each reaction tube. In order to ensure that the reaction proceeds efficiently without causing any gaps, both ends of all reaction tubes are aligned at the same position on the tube plate. It is preferable that they are mounted within a circle. The cylindrical portion of the cylindrical shell is preferably vertical.
[0018] It is preferable that the reaction tubes are housed in the multi-tubular reactor with their tube axes oriented vertically. By storing the raw gas in a small amount of water, the catalytic gas phase oxidation reaction of the raw gas may proceed efficiently. The end of each reaction tube has a preheating layer filled with an inert material, and the reaction tube is The inside of the reactor is filled with a catalyst layer. The raw gas is introduced into the preheating layer at the end of each reactor tube. The catalyst is then heated and then subjected to a catalytic gas phase oxidation reaction in a catalyst bed filled with a solid catalyst. The preheating layer is the upper end of the reaction tube when it is placed in the multi-tube reactor. However, it does not matter whether it is at the upper end or the lower end, but various high-temperature products other than the target oxidation product are Boiling by-products and carbides resulting from them are generated, and these are caused by the flow direction of the reaction gas being lead. The rate of deposition inside the reaction tube is higher when the nozzle is vertically upward than when it is directly downward. It is preferable that the flow direction of the reaction gas is vertically downward, that is, the preheating layer is located at the upper end.
[0019] A heat transfer medium is circulated within the cylindrical shell of the multi-tubular reactor. In addition, the preheating layer can prevent excessive heat generation due to the catalytic gas phase oxidation reaction. When the raw material gas flows downward from the top of the reaction tube, the catalytic gas phase oxidation reaction When the reaction proceeds, conversely, when the preheating layer is at the bottom of the reaction tube, i.e., when the raw material gas is reacting, In either case, the heat transfer medium flows upward from the bottom of the tube and the catalytic gas phase oxidation reaction proceeds. The reaction mixture produced in the catalytic gas phase oxidation reaction is preferably circulated upwards in the cylindrical shell. As heat is transferred to the heat transfer medium, the temperature of the heat transfer medium becomes higher at the outlet side than at the inlet side. As the heat transfer medium expands, its specific gravity decreases, allowing for more efficient circulation of the heat transfer medium. do.
[0020] The heat transfer medium circulation path in the cylindrical shell has a flow perpendicular to the axis of the reaction tube. It is effective from the viewpoint of heat transfer to use a disk-and-donut type baffle or a segmented circle. It is preferred to have a baffle of the disk-and-doughnut type. However, this is particularly preferred because of the high symmetry of the heat transfer medium passage.
[0021] The raw material gas contains components for producing an oxidation product. The oxidation product is For example, in the case of unsaturated aldehydes such as acrolein and methacrolein, The oxidation reaction of olefins such as propylene and isobutylene, which are the source of unsaturated aldehydes, The essential component is oxygen-containing gas to be propelled, and other inert gases such as nitrogen and water vapor are also included. In addition, the oxidation product may be an unsaturated carboxylic acid such as acrylic acid or methacrylic acid. In this case, the raw material gas is acrolein or methacrolein, which is the source of unsaturated carboxylic acids. The essential components are unsaturated aldehydes such as aldehydes and oxygen-containing gases that promote the oxidation reaction, and other The gas may contain an inert gas such as nitrogen or water vapor.
[0022] The present invention relates to a method for producing an oxidation product using the above-mentioned multi-tubular reactor, The relative standard deviation of the raw gas supply rate supplied to the preheating layer of each reaction tube (hereinafter referred to as the "relative standard deviation") The lower limit of the relative standard deviation (sometimes called the "standard deviation") is 0.3% or more and 3% or less. is preferably 0.4%, more preferably 0.5%, and even more preferably 0.6%. The upper limit is preferably 2.7%, more preferably 2.3%, and even more preferably 2.0%. . The relative standard deviation of the feed rate of the raw material gas supplied to the preheating layer of each reaction tube is calculated by the following formula ( 1) can be expressed as follows.
[0023] Relative standard deviation (σ) of the feed rate of the raw gas supplied to the preheating layer of each reaction tube = Standard deviation (s) of the feed rate of the raw gas supplied to the preheating layer of each reaction tube / per reaction tube Average feed gas flow rate to the preheater (1) Here, the standard deviation (s) of the raw material gas supply rate supplied to the preheating layer of each reaction tube is expressed as follows: will be done.
[0024]
number
[0025] The necessity of controlling the relative standard deviation within the above range is considered to be as follows. There is a demand for large-scale production of oxidation products in multi-tubular reactors. A method of adding up the oxidation products produced using multiple multi-tubular reactors is considered. However, the production of multiple multi-tubular reactors requires a large cost, and the cost of production increases with the increase in the size of the facilities. The economic benefits of the proposed method were greatly diminished. In the conventional technology, the raw material gas was uniformly supplied to all reaction tubes in the multi-tubular reactor. The feed rate per unit time of the gas is increased, and the feed rate difference between the reaction tubes, i.e., Hot spots were suppressed by making the standard deviation as close to 0 as possible, but the oxidation products The increase in production rate could not be sustained for long.
[0026] The inventors of the present invention have investigated the state of temperature control by a heat transfer medium in a multi-tubular reactor. The reaction tubes in a specific area of the reactor are designed to increase the supply rate of the raw gas. It is better to adopt a method of not increasing or decreasing the supply rate of the raw material gas outside a specific range. It has been found that the supply rate of the raw material gas to the reaction tube can be increased. The supply rate of the raw material gas per unit time to the heating layer should be uniform in all reaction tubes. The relative standard deviation of the feed rate of the raw material gas supplied to the preheating layer of each reaction tube is controlled within a specific range. By doing so, it is possible to maintain a high production rate of oxidation products for a long period of time. do.
[0027] The supply rate of the raw material gas supplied to the reaction tube can be controlled by, for example, filling the reaction tube with By increasing the surface area of the packing, the supply rate of the source gas can be reduced. By decreasing the porosity of the reaction tube, the supply rate of the raw material gas can be decreased. In order to achieve this, the average particle size of the packing material packed in the reaction tube is reduced, thereby increasing the surface area of the packing material. In addition, when the average particle diameter of the packing is 1 / 10 or more of the inner diameter of the reaction tube, In this case, the smaller the average particle size, the lower the porosity. The void ratio is lower when particles having different particle sizes are mixed and packed compared to when particles having different particle sizes are mixed and packed. Therefore, the method of reducing the average particle size of the packing material is to increase the surface area of the packing material and to increase the average particle size. By mixing catalysts with different particle sizes, the void ratio in the reaction tube can be effectively reduced. is preferable.
[0028] The reaction tubes present in a specific area in the multi-tubular reactor are those in which the multi-tubular reactor is a disk-and-tube type. If the baffle is a doughnut type, it is placed near the center of the cylindrical shell and / or The reaction tube is located near the outside. The flow of the heat transfer medium is not perpendicular to the axis of the reaction tube at that point. This is because the film heat transfer coefficient at the outer surface of the reaction tube is lower than that of other reaction tubes. In addition, when the multi-tubular reactor has a segmented circular baffle, the reaction in the specific range is The reaction tube is a reaction tube located near the outside of a cylindrical shell. The flow of the heat transfer medium is The reaction tube axis is not perpendicular to the reaction tube, and the film heat transfer coefficient on the outer surface of the reaction tube is smaller than that of other reaction tubes. By becoming lower.
[0029] Some of the reaction tubes had a larger average particle size of the inert material packed in the preheating layer than other reaction tubes. The average particle size of the inert material packed in the reaction tube (hereinafter referred to as "reaction tube A") is smaller than that of the inert material packed in the reaction tube. The number of reaction tubes A is preferably 0 to the total number of reaction tubes in the multi-tubular reactor. It is preferably 0.5% or more and less than 50%, more preferably 1% or more and less than 30%, and even more preferably By setting the ratio of the number of reaction tubes A in the above range, it is possible to It is possible to continuously maintain a high production rate of the oxidation product.
[0030] The preheating layer of the reaction tube A is divided into two layers. The average particle size of the inert material is the average particle size of the inert material packed in the preheating layer on the raw gas exhaust side. It is more preferable that the diameter of the preheating layer of the reaction tube A is smaller than that of the preheating layer of the reaction tube A. This makes it easier to control the feed gas supply rate to the reaction tube A, and high oxidation production can be achieved for a long period of time. It becomes possible to maintain the production rate of goods.
[0031] The reaction layer of the reaction tube A is filled with a mixture of a solid catalyst and an inert material. The average particle size of the inactive substance is preferably 0.5 times or more the average particle size of the solid catalyst. It is less than 1.0 times, more preferably 0.5 to 0.9, and even more preferably 0. The reaction layer of the reaction tube A is configured as described above, The feed rate of the raw gas to the reaction tube A can be easily controlled, and high oxidation product production can be achieved for a long time. This allows the production rate to be maintained.
[0032] The inert material is stable to oxidation reactions and does not react with the source gas and oxidation products. There is no particular limitation as long as the material is used. Specifically, the material may be alumina, silicon carbide, silica, or acid. Zirconia oxide and titanium oxide are preferred. There is no limitation on the shape, and the shape may be a sphere, a cylinder, a star, a ring, a small piece, a net, etc. However, from the viewpoint of reducing the porosity, it is preferable to use a spherical shape or an amorphous shape. A cylindrical shape is preferable. In addition, in order to reduce the separation of the solid catalyst particles during the packing operation, It is also preferable to use a catalyst having a shape similar to that of the catalyst. The size should be determined taking into consideration the reaction tube diameter and pressure loss. The decision can be made based on the above. The average particle size of the inactive substance is determined by randomly selecting at least 100 particles of the inactive substance, The shape of the extracted inactive material is measured, its volume and surface area are measured, and the sum of the volumes is calculated as the surface area. The value is calculated by dividing the total value by 6. The particle size is measured by taking out each particle and measuring it with a vernier caliper. The measurement can be done manually or automatically by image analysis.
[0033] When the oxidation product is an unsaturated aldehyde such as acrolein or methacrolein, the solid The solid catalyst preferably has a catalytic component element represented by the following formula (2). Mo 12 Bi a Fe b Co c Ni d X e Y f Z g S h O i (2) (In formula (2), X is at least one selected from the group consisting of Na, K, Rb, Cs, and Tl.) Y is selected from the group consisting of Mg, Ca, Sr, Ba, Mn and Zn. At least one element is represented, Z is selected from the group consisting of F, Cl, B, P, As, W and Nb. At least one selected element is shown. a to i indicate the atomic ratio of each element, 0.5 ≦a≦7, 0.05≦b≦5, 0≦c≦10, 0≦d≦10, 0≦e≦2, 0≦f≦5, The ranges are 0≦g≦5 and 0≦h≦500, and i is a value that satisfies the oxidation states of other elements. ( Furthermore, the average particle size of the solid catalyst is determined by randomly selecting at least 100 inactive particles, The shape of the extracted inactive material is measured to calculate its volume and surface area, and the total volume is added to the surface area. The value is calculated by dividing the total value by 6. The particle size is measured by taking out each particle and measuring it with a vernier caliper. The measurement can be done manually or automatically by image analysis.
[0034] When the oxidation product is an unsaturated carboxylic acid such as acrylic acid or methacrylic acid, the solid catalyst The catalyst is preferably a solid catalyst having a catalytic component element represented by the following formula (3). Mo 12 V a X b Cu c Y d Sb e Z f S g C h O i (3) (In formula (3), X represents Nb and / or W, and Y represents any one of Mg, Ca, Sr, Ba and Zn.) Z represents at least one element selected from the group consisting of Fe, Co, Ni and Bi. At least one element selected from the group consisting of a to i represents the atomic ratio of each element. , 0 <a≦12、0≦b≦12、0<c≦12、0≦d≦8、0≦e≦500、0≦f≦ 500, 0≦g≦500, 0≦h≦500, and i satisfies the oxidation state of other elements. It is the value that makes it possible to Furthermore, the average particle size of the solid catalyst is determined by randomly selecting at least 100 inactive particles, The shape of the extracted inactive material is measured to calculate its volume and surface area, and the total volume is added to the surface area. The value is calculated by dividing the total value by 6. The particle size is measured by taking out each particle and measuring it with a vernier caliper. The measurement can be done manually or by image analysis.
[0035] According to the method for producing an oxidation product of the present invention, it is possible to produce an oxidation product for a long period of time without increasing the size of the equipment. It is possible to stably produce large amounts of oxidation products for a long period of time.
Claims
1. A reaction tube having a preheating layer filled with an inert material and a catalyst layer filled with a solid catalyst. In a multi-tubular reactor in which a plurality of the above-mentioned components are accommodated in a cylindrical shell, a heat transfer medium is placed in the cylindrical shell. While circulating the gas, the raw gas is supplied to the preheating layer of each reaction tube, and catalytic gas phase oxidation reaction takes place in the catalyst layer. A method for producing an oxidation product by The relative standard of the raw material gas supply rate supplied to the preheating layer of each reaction tube, calculated by the following formula (1), A method for producing an oxidation product, the deviation being 0.3% or more and 3% or less. Relative standard deviation (σ) of the feed rate of the raw material gas supplied to the preheating layer of each reaction tube = Standard deviation (s) of the raw gas supply rate supplied to the preheating layer of each reaction tube / per reaction tube Average feed gas flow rate to the preheater (1) Here, the standard deviation (s) of the raw material gas supply rate supplied to the preheating layer of each reaction tube is expressed as follows: will be done. [0010]
2. Some of the reaction tubes had a larger average particle size of the inert material packed in the preheating layer than other reaction tubes. A reaction tube (hereinafter referred to as "reaction tube A") having an average particle size smaller than the average particle size of the inert material packed in the reaction tube. , The number of reaction tubes A is 0.5% or more and 30% or less of the total number of reaction tubes in the multi-tubular reactor. A method for producing the oxidation product according to claim 1.
3. A disk-and-donut type baffle is provided in the heat transfer medium circulation path in the cylindrical shell. The method for producing an oxidation product according to claim 1 or 2, further comprising the step of:
4. The reaction tube A is located near the center and / or near the outside of the cylindrical shell. Item 2 or 3. A method for producing an oxidation product according to item 2 or 3.
5. The preheating layer of the reaction tube A is divided into two layers, and the preheating layer on the raw material gas supply side is filled with The average particle size of the inert material is the average particle size of the inert material packed in the preheating layer on the raw gas exhaust side. The method for producing an oxidation product according to claim 2 or 3, wherein the diameter of the oxidized product is smaller than that of the oxidized product.
6. The reaction layer of the reaction tube A is filled with a mixture of a solid catalyst and an inert material. The average particle size of the inactive substance is 0.5 to 1.0 times the average particle size of the solid catalyst. The method for producing an oxidation product according to claim 2 or 3, wherein the oxidation product is less than 100%.
7. The feed gas comprises an olefin, and the oxidation product comprises an unsaturated aldehyde. Item 3. A method for producing an oxidation product according to item 1 or 2.
8. The raw material gas contains an unsaturated aldehyde, and the oxidation product contains an unsaturated carboxylic acid. A method for producing the oxidation product according to claim 1 or 2.
Citation Information
Patent Citations
Method for hydrogenation reaction of unsaturated hydrocarbon compound
JP1993279269A
Gas phase catalytic oxidation reactor
JP2001137689A
Method for vapor-phase catalytic oxidation
JP2003252807A
Method for gas phase catalytic oxidation using multitubular reactor
JP2004083430A
Method for producing unsaturated fatty acid
JP2008528683A