Image display device

The image display device uses a laminate structure with minimized refractive index differences and optional dummy wiring layers to conceal the wiring board, addressing visibility and functionality challenges in miniaturized mobile devices.

JP2024140632APending Publication Date: 2024-10-10DAI NIPPON PRINTING CO LTD
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
JP2023051866
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-28
Publication Date
2024-10-10

AI Technical Summary

Technical Problem

The challenge of making film antennas in mobile terminal devices less visible while maintaining radio wave sensitivity is exacerbated by limited mounting space and reduced design freedom due to device miniaturization.

Method used

An image display device with a laminate structure that includes a wiring board with a mesh wiring layer on a transparent substrate, sandwiched between transparent adhesive layers, where the refractive index differences are minimized to reduce visibility and deformation, and optionally enhanced with dummy wiring layers to obscure the mesh pattern.

Benefits of technology

The solution effectively conceals the wiring board within the display device, maintaining transparency and radio wave functionality while preventing deformation and visibility of the antenna components.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024140632000001_ABST
    Figure 2024140632000001_ABST
Patent Text Reader

Abstract

To provide an image display device which makes existence of a wiring board existing in the image display device difficult to be seen.SOLUTION: In an image display device 60, a laminate 70 for an image display device has: a wiring board 10 which has a board 11 including a first surface 11a and a second surface 11b located on the opposite side of the first surface 11a and a mesh wiring layer 20 arranged on the first surface 11a of the board 11; a first adhesive layer 95 which is located on the first surface 11a side of the board 11; and a second adhesive layer 96 which is located on the second surface 11b side of the board 11. The board 11 has transparency. A partial area of the board 11 is arranged in a partial area between the first adhesive layer 95 and the second adhesive layer 96. A difference between a refractive index of the board 11 and a refractive index of the first adhesive layer 95 is equal to or less than 0.05. A difference between the refractive index of the board 11 and a refractive index of the second adhesive layer 96 is equal to or less than 0.05. At least one of the first adhesive layer 95 and the second adhesive layer 96 contains resin materials with a softening point of 50°C or more and 200°C or less.SELECTED DRAWING: Figure 2A
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to an image display device. [Background technology]

[0002] Currently, mobile terminal devices such as smartphones, tablets, and smart glasses (AR, MR, etc.) are becoming more functional, smaller, thinner, and lighter. These mobile terminal devices use multiple communication bands. For this reason, multiple antennas corresponding to the communication bands are required. For example, mobile terminal devices are equipped with multiple antennas such as a telephone antenna, a WiFi (Wireless Fidelity) antenna, a 3G (Generation) antenna, a 4G (Generation) antenna, a 5G (Generation) antenna, an LTE (Long Term Evolution) antenna, a Bluetooth (registered trademark) antenna, and an NFC (Near Field Communication) antenna. However, as mobile terminal devices become smaller, the space for mounting the antennas is limited, and the freedom of antenna design is narrowed. In addition, since the antennas are built into a limited space, the radio wave sensitivity is not necessarily satisfactory.

[0003] For this reason, a film antenna that can be mounted in the display area of ​​a mobile terminal device or the transparent area of ​​a smart glass has been developed. This film antenna is a transparent antenna in which an antenna pattern is formed on a transparent substrate. The antenna pattern is formed by a mesh-shaped conductive mesh layer. The conductive mesh layer includes a conductor portion as a formed portion of an opaque conductive layer and a large number of openings as a non-formed portion. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2011-66610 A [Patent Document 2] Patent No. 5636735 specification [Patent Document 3] Patent No. 5695947 specification Summary of the Invention [Problem to be solved by the invention]

[0005] Incidentally, when a film antenna is mounted on a mobile terminal device, it is required to make the presence of the film antenna inside the mobile terminal device less visible.

[0006] The present embodiment provides an image display device that can make the presence of a wiring board present inside the image display device less visible. [Means for solving the problem]

[0007] The embodiments of the present disclosure relate to the following [1] to [6].

[0008] [1] An image display device comprising: a laminate for an image display device; and a display device laminated on the laminate for an image display device, the laminate for an image display device comprising: a substrate including a first surface and a second surface opposite to the first surface; a wiring substrate having a mesh wiring layer arranged on the first surface of the substrate; a first adhesive layer located on the first surface side of the substrate; and a second adhesive layer located on the second surface side of the substrate, the substrate being transparent; a portion of the substrate being arranged in a portion between the first adhesive layer and the second adhesive layer; a difference between the refractive index of the substrate and the refractive index of the first adhesive layer is 0.05 or less; a difference between the refractive index of the substrate and the refractive index of the second adhesive layer is 0.05 or less; and at least one of the first adhesive layer and the second adhesive layer comprises a resin material having a softening point of 50°C or more and 200°C or less.

[0009] [2] The image display device according to [1], wherein the first adhesive layer and the second adhesive layer contain a resin material having a softening point of 50°C or higher and 200°C or lower.

[0010] [3] The image display device described in [1] or [2], wherein the difference between the refractive index of the substrate and the refractive index of the first adhesive layer is 0.02 or less, and the difference between the refractive index of the substrate and the refractive index of the second adhesive layer is 0.02 or less.

[0011] [4] The image display device according to any one of [1] to [3], wherein the wiring board has a radio wave transmitting and receiving function.

[0012] [5] An image display device according to any one of [1] to [4], wherein a dummy wiring layer electrically independent from the mesh wiring layer is provided around the mesh wiring layer in the wiring substrate.

[0013] [6] The image display device described in [5], wherein a plurality of the dummy wiring layers are provided in the wiring substrate, and the aperture ratios of the mesh wiring layer and the dummy wiring layer gradually increase from the mesh wiring layer to the dummy wiring layer farther from the mesh wiring layer. Effect of the Invention

[0014] According to the embodiment of the present disclosure, the presence of a wiring board in an image display device can be made less visible. [Brief description of the drawings]

[0015] [Figure 1] FIG. 1 is a plan view showing an image display device according to an embodiment. [Figure 2A] FIG. 2A is a cross-sectional view (a cross-sectional view taken along line IIA-IIA in FIG. 1) showing an image display device according to an embodiment. [Figure 2B] FIG. 2B is a graph illustrating nanoTA measurement. [Diagram 3] FIG. 3 is a plan view showing the wiring board according to the embodiment. [Figure 4] FIG. 4 is an enlarged plan view showing the wiring board according to the embodiment. [Diagram 5] FIG. 5 is a cross-sectional view (cross-sectional view taken along line VV in FIG. 4) showing the wiring board according to the embodiment. [Figure 6] FIG. 6 is a cross-sectional view (a cross-sectional view taken along line VI-VI in FIG. 4) showing the wiring board according to the embodiment. [Figure 7] FIG. 7 is a cross-sectional view showing a module according to one embodiment. [Figure 8] 8(a)-(f) are cross-sectional views showing a method for manufacturing a wiring board according to one embodiment. [Figure 9] 9(a)-(c) are cross-sectional views showing a method for manufacturing a module according to an embodiment. [Figure 10] 10(a)-(d) are cross-sectional views illustrating a method for manufacturing an image display device according to an embodiment. [Figure 11] FIG. 11 is a cross-sectional view (corresponding to FIG. 2A) showing an image display device as a comparative example. [Figure 12] FIG. 12 is a plan view showing a wiring board of an image display device according to a first modified example. [Figure 13] FIG. 13 is an enlarged plan view showing a wiring board of an image display device according to a first modified example. [Figure 14] FIG. 14 is a plan view showing a wiring board of an image display device according to a second modified example. [Figure 15] FIG. 15 is an enlarged plan view showing a wiring board of an image display device according to a second modified example. [Figure 16] FIG. 16 is an enlarged plan view showing a wiring board of an image display device according to a third modified example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0016] First, one embodiment will be described with reference to Figures 1 to 11. Figures 1 to 11 are diagrams showing this embodiment.

[0017] The figures shown below are schematic diagrams. Therefore, the size and shape of each part are appropriately exaggerated to facilitate understanding. In addition, the present invention can be modified appropriately without departing from the technical concept. In each of the figures shown below, the same parts are given the same reference numerals, and some detailed explanations may be omitted. In addition, the numerical values ​​such as dimensions of each member and the material names described in this specification are examples of embodiments, and are not limited thereto, and can be appropriately selected and used. In this specification, terms that specify shapes and geometric conditions, such as parallel, orthogonal, and vertical, are interpreted to include substantially the same state in addition to their strict meanings.

[0018] In the following embodiments, the "X direction" is a direction parallel to one side of the image display device. The "Y direction" is a direction perpendicular to the X direction and parallel to the other side of the image display device. The "Z direction" is a direction perpendicular to both the X direction and the Y direction and parallel to the thickness direction of the image display device. The "front surface" refers to a surface on the positive side of the Z direction, which is the light-emitting surface side of the image display device and faces the observer. The "rear surface" refers to a surface on the negative side of the Z direction, which is the opposite side to the light-emitting surface of the image display device and the surface facing the observer. In the present embodiment, the mesh wiring layer 20 is described as having a radio wave transmission / reception function (function as an antenna), but the mesh wiring layer 20 does not have to have a radio wave transmission / reception function (function as an antenna).

[0019] The configuration of an image display device according to the present embodiment will be described with reference to FIGS. 1 and 2A.

[0020] As shown in FIG. 1 and FIG. 2A, the image display device 60 according to the present embodiment includes a laminate 70 for an image display device and a display device 61 laminated on the laminate 70 for an image display device. As shown in FIG. 2A, the laminate 70 for an image display device includes a wiring board 10, a first transparent adhesive layer (first adhesive layer) 95, and a second transparent adhesive layer (second adhesive layer) 96. The laminate 70 for an image display device includes a cover glass 75 and a decorative layer 74. The cover glass 75 and the decorative layer 74 are disposed on the wiring board 10 via the first transparent adhesive layer 95. Note that an impact absorbing layer (not shown) or the like may be disposed between the first transparent adhesive layer 95 and the cover glass 75. The wiring board 10 and a power supply line 85 electrically connected to the wiring board 10 constitute a module 80A.

[0021] The wiring board 10 of the module 80A includes a substrate 11, a mesh wiring layer 20, and a power supply unit 40. As shown in FIG. 2A, the substrate 11 includes a first surface 11a and a second surface 11b located on the opposite side of the first surface 11a. The mesh wiring layer 20 is disposed on the first surface 11a of the substrate 11. The power supply unit 40 is electrically connected to the mesh wiring layer 20.

[0022] 2A, the image display device 60 has a light-emitting surface 64. The above-mentioned wiring board 10 is located on the light-emitting surface 64 side (positive side in the Z direction) with respect to the display device 61. A communication module 63 is disposed on the opposite side of the light-emitting surface 64 with respect to the display device 61 (negative side in the Z direction). The laminate 70 for the image display device, the display device 61, and the communication module 63 are housed in a housing 62.

[0023] 1 and 2A, radio waves of a predetermined frequency (for example, a frequency higher than 1 GHz) can be transmitted and received via the communication module 63, and communication can be performed. The communication module 63 may include any of a millimeter wave antenna, a telephone antenna, a WiFi antenna, a 3G antenna, a 4G antenna, a 5G antenna, an LTE antenna, a Bluetooth (registered trademark) antenna, an NFC antenna, and the like. Examples of such an image display device 60 include mobile terminal devices such as smartphones and tablets.

[0024] The display device 61 is, for example, an organic EL (Electro Luminescence) display device. The display device 61 may be configured to be easily deformable. For example, the rigidity of the display device 61 may be lower than the rigidity of the cover glass 75. The display device 61 may include, for example, a metal layer, a support substrate, a resin substrate, a thin film transistor (TFT), and an organic EL layer, which are not shown. A touch sensor, which is not shown, may be disposed on the display device 61. Note that the display device 61 is not limited to an organic EL display device. For example, the display device 61 may be another display device having a function of emitting light by itself, or may be a micro LED display device including a micro LED element (light emitter). The display device 61 may also be a liquid crystal display device including liquid crystal.

[0025] Next, the laminate 70 for an image display device will be described in detail. As described above, the laminate 70 for an image display device includes the wiring board 10, the first transparent adhesive layer 95, and the second transparent adhesive layer 96. As described above, the laminate 70 for an image display device includes the cover glass 75 and the decorative layer 74. The laminate 70 for an image display device may be incorporated into a head-mounted display (smart glasses) by being attached to a frame (not shown).

[0026] The cover glass 75 of the laminate 70 for an image display device is located on the first surface 11a side of the substrate 11 of the wiring board 10. The first transparent adhesive layer 95 is located between the substrate 11 of the wiring board 10 and the cover glass 75. The decorative layer 74 is located between the cover glass 75 and the first transparent adhesive layer 95. The second transparent adhesive layer 96 is located on the second surface 11b side of the substrate 11 of the wiring board 10. Here, the first transparent adhesive layer 95 of the laminate 70 for an image display device will be described first. Details of the wiring board 10 will be described later.

[0027] The first transparent adhesive layer 95 is an adhesive layer that directly or indirectly adheres the wiring board 10 to the decorative layer 74 and the cover glass 75. This first transparent adhesive layer 95 is located on the first surface 11a side of the substrate 11. The first transparent adhesive layer 95 has optical transparency and may be an OCA (Optical Clear Adhesive) layer. The OCA layer is a layer prepared, for example, as follows. First, a liquid curable adhesive layer composition containing a polymerizable compound is applied onto a release film such as polyethylene terephthalate (PET). Next, the liquid curable adhesive layer composition is cured, for example, using ultraviolet light (UV) to obtain an OCA sheet. After the OCA sheet is attached to an object, the release film is peeled off and removed to obtain the OCA layer. The material of the first transparent adhesive layer 95 may be an acrylic resin, a silicone resin, a urethane resin, or the like. In particular, the first transparent adhesive layer 95 may contain an acrylic resin. In this case, it is preferable that the second transparent adhesive layer 96 contains an acrylic resin. This substantially eliminates the difference in refractive index between the first transparent adhesive layer 95 and the second transparent adhesive layer 96, and more reliably suppresses reflection of visible light at the interface B3 between the first transparent adhesive layer 95 and the second transparent adhesive layer 96.

[0028] The first transparent adhesive layer 95 may have a visible light transmittance of 85% or more, and preferably 90% or more. The first transparent adhesive layer 95 has no particular upper limit for the visible light transmittance, but may have a transmittance of, for example, 100% or less. By setting the visible light transmittance of the first transparent adhesive layer 95 within the above range, the transparency of the laminate 70 for an image display device can be increased, and the display device 61 of the image display device 60 can be easily viewed. Visible light refers to light having a wavelength of 400 nm or more and 700 nm or less. The visible light transmittance of 85% or more means that when the absorbance of the member to be measured (for example, the first transparent adhesive layer 95) is measured, the transmittance is 85% or more in the entire wavelength range of 400 nm or more and 700 nm or less. The absorbance can be measured using a spectrophotometer (V-670 spectrometer manufactured by JASCO Corporation).

[0029] As described above, the wiring board 10 is disposed on the light-emitting surface 64 side with respect to the display device 61. In this case, the wiring board 10 is located between the first transparent adhesive layer 95 and the second transparent adhesive layer 96. More specifically, a part of the substrate 11 of the wiring board 10 is disposed in a part of the region between the first transparent adhesive layer 95 and the second transparent adhesive layer 96. In this case, the first transparent adhesive layer 95, the second transparent adhesive layer 96, the display device 61, and the cover glass 75 each have a larger area than the substrate 11 of the wiring board 10. In this way, by disposing the substrate 11 of the wiring board 10 in a part of the image display device 60 instead of the entire surface thereof in a plan view, the area of ​​the wiring board 10 can be reduced. Therefore, when the first directional wiring 21 and the second directional wiring 22 of the wiring board 10 described later are manufactured, a large number of the first directional wiring 21 and the second directional wiring 22 can be manufactured at once. Therefore, the manufacturing cost per wiring board 10 can be reduced. Note that substrate 11 of wiring board 10 may be disposed over the entire surface of image display device 60 in plan view. In this case, the time required for positioning wiring board 10 on display device 61 can be shortened.

[0030] As described above, the wiring board 10 includes the substrate 11 having transparency and the mesh wiring layer 20 disposed on the first surface 11a of the substrate 11. The power supply unit 40 is electrically connected to the mesh wiring layer 20. The power supply unit 40 is electrically connected to the communication module 63 via the power supply line 85. A part of the wiring board 10 is not disposed between the first transparent adhesive layer 95 and the second transparent adhesive layer 96, but protrudes outward (to the negative Y-direction side) from between the first transparent adhesive layer 95 and the second transparent adhesive layer 96. Specifically, the region of the wiring board 10 where the power supply unit 40 is provided protrudes outward. This makes it easy to electrically connect the power supply unit 40 to the communication module 63. On the other hand, the region of the wiring board 10 where the mesh wiring layer 20 is provided is located between the first transparent adhesive layer 95 and the second transparent adhesive layer 96. Details of the wiring board 10 will be described later.

[0031] The second transparent adhesive layer 96 is an adhesive layer that directly or indirectly adheres the display device 61 to the wiring substrate 10. The second transparent adhesive layer 96 is located on the second surface 11b side of the substrate 11. The second transparent adhesive layer 96 has optical transparency like the first transparent adhesive layer 95, and may be an OCA (Optical Clear Adhesive) layer. The material of the second transparent adhesive layer 96 may be an acrylic resin, a silicone resin, a urethane resin, or the like. In particular, the second transparent adhesive layer 96 may contain an acrylic resin. This substantially eliminates the difference in refractive index between the first transparent adhesive layer 95 and the second transparent adhesive layer 96, and more reliably suppresses the reflection of visible light at the interface B3 between the first transparent adhesive layer 95 and the second transparent adhesive layer 96.

[0032] The second transparent adhesive layer 96 may have a visible light (light having a wavelength of 400 nm or more and 700 nm or less) transmittance of 85% or more, and preferably 90% or more. There is no particular upper limit to the visible light transmittance of the second transparent adhesive layer 96, but it may be, for example, 100% or less. By setting the visible light transmittance of the second transparent adhesive layer 96 to the above range, the transparency of the laminate 70 for an image display device can be increased, and the display device 61 of the image display device 60 can be easily viewed.

[0033] In such an image display device 60, the difference between the refractive index of the substrate 11 and the refractive index of the first transparent adhesive layer 95 is 0.05 or less, and preferably 0.02 or less. The difference between the refractive index of the substrate 11 and the refractive index of the second transparent adhesive layer 96 is 0.05 or less, and preferably 0.02 or less. Furthermore, the difference between the refractive index of the first transparent adhesive layer 95 and the refractive index of the second transparent adhesive layer 96 is preferably 0.05 or less, and more preferably 0.02 or less. For example, when the material of the first transparent adhesive layer 95 and the material of the second transparent adhesive layer 96 are acrylic resins with a refractive index of 1.49, the refractive index of the substrate 11 is set to 1.45 or more and 1.54 or less. Examples of such materials include fluororesins, silicone resins, polyolefin resins, polyester resins, acrylic resins, polycarbonate resins, polyimide resins, and cellulose resins.

[0034] In this way, by suppressing the difference between the refractive index of the substrate 11 and the refractive index of the first transparent adhesive layer 95 to 0.05 or less, the reflection of visible light at the interface B1 between the substrate 11 and the first transparent adhesive layer 95 can be suppressed, and the substrate 11 can be made difficult to be seen by the naked eye of the observer. In addition, by suppressing the difference between the refractive index of the substrate 11 and the refractive index of the second transparent adhesive layer 96 to 0.05 or less, the reflection of visible light at the interface B2 between the substrate 11 and the second transparent adhesive layer 96 can be suppressed, and the substrate 11 can be made difficult to be seen by the naked eye of the observer. Furthermore, by suppressing the difference between the refractive index of the first transparent adhesive layer 95 and the refractive index of the second transparent adhesive layer 96 to 0.05 or less, the reflection of visible light at the interface B3 between the first transparent adhesive layer 95 and the second transparent adhesive layer 96 can be suppressed. Therefore, the first transparent adhesive layer 95 and the second transparent adhesive layer 96 can be made difficult to be seen by the naked eye of the observer.

[0035] In particular, it is preferable that the material of the first transparent adhesive layer 95 and the material of the second transparent adhesive layer 96 are the same as each other. This makes it possible to further reduce the difference in refractive index between the first transparent adhesive layer 95 and the second transparent adhesive layer 96, and suppress reflection of visible light at the interface B3 between the first transparent adhesive layer 95 and the second transparent adhesive layer 96.

[0036] At least one of the first transparent adhesive layer 95 and the second transparent adhesive layer 96 may contain a resin material having a softening point of 50° C. or more and 200° C. or less. In this case, the first transparent adhesive layer 95 and the second transparent adhesive layer 96 may contain a resin material having a softening point of 50° C. or more and 200° C. or less. As described above, the first transparent adhesive layer 95 and the second transparent adhesive layer 96 may be an OCA layer constituted by a composition for a curable adhesive layer. In this case, the softening point of the resin material means the softening point after curing.

[0037] Here, the resin material having a softening point of 50°C or more and 200°C or less after hardening may have a softening point of about 25°C or more and about 50°C or less before hardening. In this way, when the material of the first transparent adhesive layer 95 or the like is a resin material having a softening point of 25°C or more and 50°C or less before hardening, the fluidity of the resin material is high. Therefore, when the display device 61 is laminated on the first transparent adhesive layer 95 or the like, it is possible to suppress deformation of the display device 61. That is, when the display device 61 is laminated on the first transparent adhesive layer 95 or the like, it is possible to suppress a large force from being locally applied to the display device 61 from the resin material constituting the first transparent adhesive layer 95 or the like. Therefore, even if the rigidity of the display device 61 is lower than the rigidity of the cover glass 75, it is possible to suppress deformation of the display device 61 when the display device 61 is laminated on the first transparent adhesive layer 95 or the like.

[0038] The softening point of the resin material is measured by nanoTA measurement. When measuring the softening point of the resin material by nanoTA measurement, first, a scanning probe microscope (nanoTA, manufactured by Anasys Instruments) is prepared. At this time, a PR-EXP-AN2-300-5 probe manufactured by Anasys Instruments is used. Next, the probe is heated to 40°C. Next, the probe of the scanning probe microscope is further heated with the tip of the probe in contact with the resin material. At this time, the heating rate of the probe is set to 5°C / sec. By heating the probe, heat is transferred to the part of the resin material with which the probe is in contact. As a result, the part with which the probe is in contact thermally expands. Then, due to the thermal expansion of the resin material, the probe is deformed, and the tip of the probe is displaced (see part A in FIG. 2B). Next, by further heating the probe, the resin material softens, and the tip of the probe penetrates into the resin material. As a result, the deformation of the probe is eliminated, and the displacement of the tip of the probe becomes smaller (see part B in FIG. 2B). The temperature at the apex is set as the softening point of the resin material (see point C in FIG. 2B).

[0039] 2A, at least one of the thickness T3 of the first transparent adhesive layer 95 and the thickness T4 of the second transparent adhesive layer 96 may be 1.5 times or more, preferably 2 times or more, and more preferably 2.5 times or more, of the thickness T1 of the substrate 11. In this way, by making the thickness T3 of the first transparent adhesive layer 95 or the thickness T4 of the second transparent adhesive layer 96 sufficiently thicker than the thickness T1 of the substrate 11, the first transparent adhesive layer 95 or the second transparent adhesive layer 96 deforms in the thickness direction in the region overlapping with the substrate 11, absorbing the thickness of the substrate 11. This makes it possible to suppress the occurrence of a step in the first transparent adhesive layer 95 or the second transparent adhesive layer 96 at the periphery of the substrate 11, making it difficult for an observer to recognize the presence of the substrate 11.

[0040] At least one of the thickness T3 of the first transparent adhesive layer 95 and the thickness T4 of the second transparent adhesive layer 96 is preferably 10 times or less, and more preferably 5 times or less, the thickness T1 of the substrate 11. This prevents the thickness T3 of the first transparent adhesive layer 95 or the thickness T4 of the second transparent adhesive layer 96 from becoming too thick, and allows the overall thickness of the image display device 60 to be thin.

[0041] 2A, the thickness T3 of the first transparent adhesive layer 95 may be thicker than the thickness T4 of the second transparent adhesive layer 96. Here, as described above, the first transparent adhesive layer 95 is located on the first surface 11a side of the substrate 11 of the wiring substrate 10. In addition, the mesh wiring layer 20 is disposed on the first surface 11a of the substrate 11 of the wiring substrate 10. Therefore, due to the unevenness formed by the mesh wiring layer 20, unevenness may be formed on the surface of the first transparent adhesive layer 95. In contrast, since the thickness T3 of the first transparent adhesive layer 95 is thicker than the thickness T4 of the second transparent adhesive layer 96, it is possible to suppress the formation of unevenness on the surface of the first transparent adhesive layer 95, and the surface of the first transparent adhesive layer 95 can be made smooth.

[0042] The difference between the thickness T3 of the first transparent adhesive layer 95 and the thickness T4 of the second transparent adhesive layer 96 is preferably 100 μm or less. Here, as described above, the first transparent adhesive layer 95 and the second transparent adhesive layer 96 may be OCA layers. For this reason, tensile stress acting to shrink the first transparent adhesive layer 95 and the second transparent adhesive layer 96 may be generated in the first transparent adhesive layer 95 and the second transparent adhesive layer 96 due to residual stress that may be generated in the OCA layer when the OCA layer is produced. This tensile stress may increase as the thickness T3 of the first transparent adhesive layer 95 or the thickness T4 of the second transparent adhesive layer 96 increases. And, when the difference between the tensile stress generated in the first transparent adhesive layer 95 and the tensile stress generated in the second transparent adhesive layer 96 becomes large, the wiring board 10 may be warped. In contrast, by setting the difference between the thickness T3 of the first transparent adhesive layer 95 and the thickness T4 of the second transparent adhesive layer 96 to 100 μm or less, it is possible to reduce the difference between the tensile stress generated in the first transparent adhesive layer 95 and the tensile stress generated in the second transparent adhesive layer 96. This makes it possible to reduce warping of the wiring board 10 caused by the difference between the tensile stress generated in the first transparent adhesive layer 95 and the tensile stress generated in the second transparent adhesive layer 96.

[0043] In FIG. 2A, the thickness T3 of the first transparent adhesive layer 95 and the thickness T4 of the second transparent adhesive layer 96 may be the same as each other. In this case, the thickness T3 of the first transparent adhesive layer 95 and the thickness T4 of the second transparent adhesive layer 96 may be 1.5 times or more, and preferably 2.0 times or more, of the thickness T1 of the substrate 11. That is, the sum (T3+T4) of the thickness T3 of the first transparent adhesive layer 95 and the thickness T4 of the second transparent adhesive layer 96 is three times or more of the thickness T1 of the substrate 11. In this way, by making the sum of the thicknesses T3 and T4 of the first transparent adhesive layer 95 and the second transparent adhesive layer 96 sufficiently thicker than the thickness T1 of the substrate 11, the first transparent adhesive layer 95 and the second transparent adhesive layer 96 deform (shrink) in the thickness direction in the region overlapping with the substrate 11. As a result, the first transparent adhesive layer 95 and the second transparent adhesive layer 96 absorb the thickness of the substrate 11. This makes it possible to prevent steps from occurring in the first transparent adhesive layer 95 or the second transparent adhesive layer 96 at the periphery of the substrate 11, making it difficult for an observer to recognize the presence of the substrate 11.

[0044] When the thickness T3 of the first transparent adhesive layer 95 and the thickness T4 of the second transparent adhesive layer 96 are the same, the thickness T3 of the first transparent adhesive layer 95 and the thickness T4 of the second transparent adhesive layer 96 may each be 5 times or less, and preferably 3 times or less, the thickness T1 of the substrate 11. This prevents the thicknesses T3, T4 of the first transparent adhesive layer 95 and the second transparent adhesive layer 96 from becoming too thick, and allows the overall thickness of the image display device 60 to be thin.

[0045] Specifically, the thickness T1 of the substrate 11 may be, for example, 2 μm or more, 10 μm or more, and preferably 15 μm or more. By setting the thickness T1 of the substrate 11 to 2 μm or more, the strength of the wiring substrate 10 can be maintained, and the first directional wiring 21 and the second directional wiring 22 of the mesh wiring layer 20 described later can be made less likely to deform. Furthermore, the thickness T1 of the substrate 11 may be, for example, 200 μm or less, 50 μm or less, and preferably 25 μm or less. By setting the thickness T1 of the substrate 11 to 200 μm or less, the occurrence of steps in the first transparent adhesive layer 95 and the second transparent adhesive layer 96 at the periphery of the substrate 11 can be suppressed, and the presence of the substrate 11 can be made less noticeable to the observer. Furthermore, by setting the thickness T1 of the substrate 11 to 50 μm or less, the occurrence of steps in the first transparent adhesive layer 95 and the second transparent adhesive layer 96 at the periphery of the substrate 11 can be further suppressed, and the presence of the substrate 11 can be made less noticeable to the observer.

[0046] The thickness T3 of the first transparent adhesive layer 95 may be, for example, 15 μm or more, and preferably 20 μm or more. The thickness T3 of the first transparent adhesive layer 95 may be, for example, 500 μm or less, and is preferably 300 μm or less, and more preferably 250 μm or less. By making the thickness T3 of the first transparent adhesive layer 95 500 μm or less, the thickness T3 of the first transparent adhesive layer 95 does not become too thick, and the overall thickness of the image display device 60 can be made thinner. In addition, by making the thickness T3 of the first transparent adhesive layer 95 300 μm or less, the overall thickness of the image display device 60 can be made even thinner.

[0047] The thickness T4 of the second transparent adhesive layer 96 may be, for example, 15 μm or more, and preferably 20 μm or more. The thickness T4 of the second transparent adhesive layer 96 may be, for example, 500 μm or less, and preferably 300 μm or less, and more preferably 250 μm or less. By making the thickness T4 of the second transparent adhesive layer 96 500 μm or less, the thickness T4 of the second transparent adhesive layer 96 does not become too thick, and the overall thickness of the image display device 60 can be made thin. In addition, by making the thickness T4 of the second transparent adhesive layer 96 300 μm or less, the overall thickness of the image display device 60 can be made even thinner.

[0048] As described above, the laminate 70 for an image display device is composed of the wiring board 10, the first transparent adhesive layer 95 having an area larger than the substrate 11 of the wiring board 10, and the second transparent adhesive layer 96 having an area larger than the substrate 11. In the present embodiment, such a laminate 70 for an image display device is also provided.

[0049] Referring again to FIG. 2A, the cover glass 75 is directly or indirectly disposed on the first transparent adhesive layer 95. The cover glass 75 is located on the positive side of the first transparent adhesive layer 95 in the Z direction and is disposed on the decorative layer 74. The cover glass 75 is a glass member that transmits light. The cover glass 75 is plate-shaped, and the shape of the cover glass 75 may be rectangular in a plan view. The thickness of the cover glass 75 may be, for example, 200 μm or more and 1000 μm or less, and preferably 300 μm or more and 700 μm or less. The length of the cover glass 75 in the longitudinal direction (Y direction) may be, for example, 20 mm or more and 500 mm or less, and preferably 100 mm or more and 200 mm or less. The length of the cover glass 75 in the lateral direction (X direction) may be, for example, 20 mm or more and 500 mm or less, and preferably 50 mm or more and 100 mm or less.

[0050] At least a portion of the decorative layer 74 is disposed on the first transparent adhesive layer 95. The decorative layer 74 may be a decorative film. For example, the decorative layer 74 has an opening in all or part of a portion that overlaps with the display area of ​​the display device 61 when viewed from the observer side, and blocks light from the portion other than the display area. That is, the decorative layer 74 is disposed so as to cover the end of the display device 61 when viewed from the observer side.

[0051] As shown in Fig. 1, the shape of the image display device 60 is generally rectangular in plan view, with its longitudinal direction parallel to the Y direction and its lateral direction parallel to the X direction. The length L4 of the image display device 60 in the longitudinal direction (Y direction) can be selected, for example, from 20 mm to 500 mm, preferably from 100 mm to 200 mm. The length L5 of the image display device 60 in the lateral direction (X direction) can be selected, for example, from 20 mm to 500 mm, preferably from 50 mm to 100 mm. The planar shape of the image display device 60 may be a rectangle with rounded corners.

[0052] Next, the configuration of the wiring board will be described with reference to Figures 3 to 6. Figures 3 to 6 are diagrams showing the wiring board according to the present embodiment.

[0053] The wiring board 10 according to the present embodiment is a board used in the above-mentioned image display device 60 (see Figs. 1 and 2A). The wiring board 10 can be disposed on the light-emitting surface 64 side of the display device 61, between a first transparent adhesive layer 95 and a second transparent adhesive layer 96 (see Fig. 2A). As shown in Fig. 3, such a wiring board 10 has a transparent substrate 11 and a mesh wiring layer 20 disposed on the substrate 11, as described above. In addition, a power supply unit 40 is electrically connected to the mesh wiring layer 20.

[0054] The shape of the substrate 11 is substantially rectangular in plan view. In the illustrated example, the longitudinal direction is parallel to the X direction, and the lateral direction is parallel to the Y direction. The substrate 11 is transparent and substantially flat, and its thickness is substantially uniform overall. The length L1 (see FIGS. 1 and 3) of the substrate 11 in the longitudinal direction (Y direction) of the image display device 60 can be selected, for example, in the range of 10 mm to 200 mm. The length L2 (see FIG. 1) of the substrate 11 in the lateral direction (X direction) of the image display device 60 can be selected, for example, in the range of 3 mm to 100 mm. The planar shape of the substrate 11 may be a rectangle with rounded corners.

[0055] The material of the substrate 11 may be any material that has transparency in the visible light region and electrical insulation. For example, organic insulating materials such as polyester resin, acrylic resin, polycarbonate resin, polyimide resin, polyolefin resin, cellulose resin, or fluororesin material are preferably used as the material of the substrate 11. The polyester resin may be polyethylene terephthalate or the like. The acrylic resin may be polymethyl methacrylate or the like. The polyolefin resin may be cycloolefin polymer or the like. The cellulose resin may be triacetyl cellulose or the like. The fluororesin material may be PTFE or PFA or the like. For example, organic insulating materials such as cycloolefin polymer (for example, ZF-16 manufactured by Nippon Zeon Co., Ltd.) or polynorbornene polymer (manufactured by Sumitomo Bakelite Co., Ltd.) may be used as the material of the substrate 11. In addition, glass, ceramics, or the like may be appropriately selected as the material of the substrate 11 depending on the application. Although the substrate 11 is illustrated as being made up of a single layer, the present invention is not limited thereto and may be made up of a laminate of multiple base materials or layers. The substrate 11 may be a film-like member or a plate-like member.

[0056] The dielectric loss tangent of the substrate 11 is preferably 0.002 or less. By having the dielectric loss tangent of the substrate 11 in the above range, it is possible to reduce the gain loss (reduction in sensitivity) associated with the transmission and reception of electromagnetic waves, particularly when the electromagnetic waves (e.g., millimeter waves) transmitted and received by the mesh wiring layer 20 are high frequency.

[0057] The relative dielectric constant of the substrate 11 is preferably 2 or more and 10 or less. By making the relative dielectric constant of the substrate 11 2 or more, the number of choices of materials for the substrate 11 can be increased. In addition, by making the relative dielectric constant of the substrate 11 10 or less, the gain loss associated with the transmission and reception of electromagnetic waves can be reduced. That is, when the relative dielectric constant of the substrate 11 becomes large, the influence of the thickness of the substrate 11 on the propagation of electromagnetic waves becomes large. In addition, when there is an adverse effect on the propagation of electromagnetic waves, the dielectric loss tangent of the substrate 11 becomes large, and the gain loss associated with the transmission and reception of electromagnetic waves can become large. In contrast, by making the relative dielectric constant of the substrate 11 10 or less, the influence of the thickness of the substrate 11 on the propagation of electromagnetic waves can be reduced. Therefore, the gain loss associated with the transmission and reception of electromagnetic waves can be reduced. In particular, when the electromagnetic waves (e.g., millimeter waves) transmitted and received by the mesh wiring layer 20 are high frequency, the gain loss associated with the transmission and reception of electromagnetic waves can be reduced.

[0058] The dielectric loss tangent and the relative dielectric constant of the substrate 11 can be measured in accordance with IEC 62562. Specifically, first, a test piece is prepared by cutting out a portion of the substrate 11 where the mesh wiring layer 20 is not formed. The dimensions of the test piece are a width of 10 mm to 20 mm, and a length of 50 mm to 100 mm. Next, the dielectric loss tangent or the relative dielectric constant is measured in accordance with IEC 62562.

[0059] In this embodiment, the substrate 11 has transparency. In this specification, "having transparency" means that the transmittance of visible light (light having a wavelength of 400 nm or more and 700 nm or less) is 85% or more. The substrate 11 may have a visible light transmittance of 85% or more, and preferably has a visible light transmittance of 90% or more. There is no particular upper limit to the visible light transmittance of the substrate 11, but it may be, for example, 100% or less. By setting the visible light transmittance of the substrate 11 within the above range, the transparency of the wiring substrate 10 can be increased, and the display device 61 of the image display device 60 can be easily viewed.

[0060] In this embodiment, the mesh wiring layer 20 is made of an antenna pattern that functions as an antenna. This mesh wiring layer 20 may be configured as an array antenna. In this way, when the mesh wiring layer 20 is configured as an array antenna, it is possible to improve the performance of the millimeter wave antenna that transmits and receives highly linear millimeter waves. Note that an array antenna is an antenna in which multiple antenna elements (radiating elements) are regularly arranged, and the amplitude and phase of the excitation of the elements can be independently controlled.

[0061] As shown in FIG. 3, a plurality of mesh wiring layers 20 are formed on the substrate 11. It is preferable that four or more mesh wiring layers 20 are provided. In the illustrated example, four mesh wiring layers 20 are formed on the substrate 11 (see FIG. 1). Also, as shown in FIG. 3, the mesh wiring layers 20 may not be present on the entire surface of the substrate 11, but may be present only in a partial region on the substrate 11. Each mesh wiring layer 20 may have the same shape as the others. In this case, each mesh wiring layer 20 has a length (Y direction distance) L of a tip side portion 20b described later. a Error and width (X direction distance) W a It is preferable that the error of each is within 10%, which can effectively improve the performance of the millimeter wave antenna.

[0062] The mesh wiring layer 20 has a base end portion (transmission portion) 20a on the power supply unit 40 side and a tip end portion (transmission / reception portion) 20b connected to the base end portion 20a. The base end portion 20a is connected to the power supply unit 40. In this case, the base end portion (transmission portion) 20a may be configured as a microstrip line or a coplanar line. The shape of the base end portion 20a and the shape of the tip end portion 20b are each approximately rectangular in a plan view. In this case, the length (Y direction distance) of the tip end portion 20b is approximately the same as the length (Y direction distance) of the base end portion 20a, and the width (X direction distance) of the tip end portion 20b is wider than the width (X direction distance) of the base end portion 20a.

[0063] The tip portion 20b of the mesh wiring layer 20 corresponds to a predetermined frequency band. a The length L of the tip portion 20b corresponds to a specific frequency band. a The length of the mesh wiring layer 20 becomes longer. In addition to the millimeter wave antenna, the mesh wiring layer 20 may correspond to any of a telephone antenna, a WiFi antenna, a 3G antenna, a 4G antenna, a 5G antenna, an LTE antenna, an Bluetooth (registered trademark) antenna, an NFC antenna, etc. The lengths of the multiple tip side portions 20b may be different from each other and each may correspond to a different frequency band. Alternatively, when the wiring board 10 does not have a radio wave transmission / reception function, each mesh wiring layer 20 may perform a function such as a hovering function, a fingerprint authentication, a heater, a noise cut (shield), etc. The hovering function refers to a function that allows a user to operate the display without directly touching it.

[0064] In the illustrated example, the tip portion 20b has a longitudinal direction parallel to the X direction and a lateral direction parallel to the Y direction. The tip portion 20b may have a longitudinal direction parallel to the Y direction and a lateral direction parallel to the X direction. The length L of the tip portion 20b in the Y direction is a The width W of the tip portion 20b in the X direction can be selected, for example, in the range of 1 mm to 100 mm. aIn particular, when the mesh wiring layer 20 is a millimeter wave antenna, the length L of the tip portion 20b can be selected within a range of, for example, 1 mm or more and 100 mm or less. a When the mesh wiring layer 20 is a millimeter wave antenna, the length L of the tip portion 20b can be selected in the range of 1 mm or more, more preferably 1.5 mm or more. a can be selected in the range of 10 mm or less, more preferably 5 mm or less.

[0065] The distance between the mesh wiring layers 20 is preferably 0.2 mm or more and 5 mm or less. 20b The distance D between the tip portions 20b (see FIG. 3) is preferably 0.2 mm or more and 5 mm or less. 20b By setting the distance D between the tip portions 20b to 0.2 mm or more, unintended interference of electromagnetic waves between the antenna elements can be suppressed. 20b By making the distance D between the tip end portions 20b equal to or less than 5 mm, it is possible to reduce the size of the entire array antenna formed by the mesh wiring layer 20. For example, in the case where the mesh wiring layer 20 is a millimeter wave antenna of 28 GHz, 20b In addition, when the mesh wiring layer 20 is a millimeter wave antenna of 60 GHz, the distance D between the tip side portions 20b may be 3.5 mm. 20b may be 1.6 mm.

[0066] 4, the mesh wiring layer 20 has a pattern shape in which metal wires are arranged in a lattice or mesh shape. This pattern shape is repeatedly arranged in the X direction and the Y direction. That is, the mesh wiring layer 20 has a pattern shape composed of a portion (first direction wiring 21 described later) extending in a first direction (e.g., Y direction) and a portion (second direction wiring 22 described later) extending in a second direction (e.g., X direction).

[0067] The mesh wiring layer 20 has a plurality of wires. Specifically, the mesh wiring layer 20 has a plurality of first directional wires 21 and a plurality of second directional wires 22 connecting the plurality of first directional wires 21. The plurality of first directional wires 21 and the plurality of second directional wires 22 are integrated as a whole to form a lattice or mesh shape. Each of the first directional wires 21 extends in the longitudinal direction (Y direction) of the mesh wiring layer 20. Each of the second directional wires extends linearly in the width direction (X direction) of the mesh wiring layer 20. The first directional wires 21 and the second directional wires 22 may extend in a direction that is not parallel to either the X direction or the Y direction.

[0068] In the mesh wiring layer 20, a plurality of openings 23 are formed by being surrounded by adjacent first directional wires 21 and adjacent second directional wires 22. The transparent substrate 11 is exposed from each opening 23. This can increase the transparency of the wiring substrate 10 as a whole.

[0069] The planar shape of each opening 23 is approximately square in plan view. That is, the first direction wiring 21 and the second direction wiring 22 are arranged at equal intervals from each other. The first direction wirings 21 are arranged at equal intervals from each other, and the pitch P1 may be, for example, in the range of 0.01 mm to 1 mm. The second direction wirings 22 are arranged at equal intervals from each other, and the pitch P2 may be, for example, in the range of 0.01 mm to 1 mm. In this way, since the first direction wirings 21 and the second direction wirings 22 are arranged at equal intervals, the size of the openings 23 in the mesh wiring layer 20 does not vary, and the mesh wiring layer 20 can be made difficult to see with the naked eye. The pitch P1 of the first direction wirings 21 is equal to the pitch P2 of the second direction wirings 22. For this reason, as described above, each opening 23 is approximately square in plan view, and the transparent substrate 11 is exposed from each opening 23. Therefore, by increasing the area of ​​each opening 23, the transparency of the wiring board 10 as a whole can be increased. The length L3 of one side of each opening 23 may be, for example, in the range of 0.01 mm to 1 mm. The first directional wires 21 and the second directional wires 22 are perpendicular to each other, but are not limited to this and may intersect at an acute angle or an obtuse angle. The shape of the openings 23 is preferably the same shape and size over the entire surface, but it does not have to be uniform over the entire surface and may vary depending on the location.

[0070] As shown in FIG. 5, each of the first directional wirings 21 has a cross section (X-direction cross section) perpendicular to its longitudinal direction that is substantially rectangular or square. In this case, the cross-sectional shape of the first directional wirings 21 is substantially uniform along the longitudinal direction (Y-direction) of the first directional wirings 21. As shown in FIG. 6, each of the second directional wirings 22 has a cross section (Y-direction cross section) perpendicular to its longitudinal direction that is substantially rectangular or square, and has substantially the same shape as the cross-sectional (X-direction cross section) shape of the first directional wirings 21 described above. In this case, the cross-sectional shape of the second directional wirings 22 is substantially uniform along the longitudinal direction (X-direction) of the second directional wirings 22. The cross-sectional shapes of the first directional wirings 21 and the second directional wirings 22 do not necessarily have to be substantially rectangular or square. For example, the cross-sectional shape of the first directional wiring 21 and the cross-sectional shape of the second directional wiring 22 may be an approximate trapezoid in which the front side (positive side in the Z direction) is narrower than the back side (negative side in the Z direction), or a shape in which the side surfaces on both sides in the longitudinal direction are curved.

[0071] In this embodiment, the line width W1 of the first direction wiring 21 (see FIG. 5) and the line width W2 of the second direction wiring 22 (see FIG. 6) are not particularly limited and can be appropriately selected depending on the application. Here, the line width W1 of the first direction wiring 21 is the width (X-direction distance) in a cross section perpendicular to its longitudinal direction, and the line width W2 of the second direction wiring 22 is the width (Y-direction distance) in a cross section perpendicular to its longitudinal direction. For example, the line width W1 of the first direction wiring 21 can be selected in the range of 0.1 μm to 5.0 μm, and is preferably 0.2 μm to 2.0 μm. In addition, the line width W2 of the second direction wiring 22 can be selected in the range of 0.1 μm to 5.0 μm, and is preferably 0.2 μm to 2.0 μm.

[0072] The height H1 of the first directional wiring 21 (see FIG. 5) and the height H2 of the second directional wiring 22 (see FIG. 6) are not particularly limited and can be appropriately selected depending on the application. Here, the height H1 of the first directional wiring 21 and the height H2 of the second directional wiring 22 are lengths in the Z direction. The height H1 of the first directional wiring 21 and the height H2 of the second directional wiring 22 can each be selected within a range of, for example, 0.1 μm or more, and preferably 0.2 μm or more. The height H1 of the first directional wiring 21 and the height H2 of the second directional wiring 22 can each be selected within a range of, for example, 5.0 μm or less, and preferably 2.0 μm or less.

[0073] The material of the first directional wiring 21 and the second directional wiring 22 may be any metal material having electrical conductivity. In the present embodiment, the material of the first directional wiring 21 and the second directional wiring 22 is copper, but is not limited thereto. The material of the first directional wiring 21 and the second directional wiring 22 may be, for example, a metal material such as gold, silver, copper, platinum, tin, aluminum, iron, or nickel, or an alloy containing these metals. The first directional wiring 21 and the second directional wiring 22 may be a plating layer formed by an electrolytic plating method.

[0074] The overall aperture ratio At of the mesh wiring layer 20 may be, for example, in the range of 87% or more and less than 100%. By setting the overall aperture ratio At of the mesh wiring layer 20 in this range, the conductivity and transparency of the wiring board 10 can be ensured. The overall aperture ratio At of the mesh wiring layer 20 is preferably 95% or more and less than 100%. This allows the transparency of the wiring board 10 to be increased while ensuring the conductivity of the wiring board 10. The aperture ratio refers to the ratio (%) of the area of ​​the opening region to the unit area of ​​a predetermined region (for example, the entire region of the mesh wiring layer 20). The opening region refers to a region where no metal parts such as the first directional wiring 21 and the second directional wiring 22 exist and the substrate 11 is exposed.

[0075] Although not shown, a protective layer may be formed on the first surface 11a of the substrate 11 so as to cover the mesh wiring layer 20. The protective layer protects the mesh wiring layer 20 and is formed so as to cover at least the mesh wiring layer 20 of the substrate 11. As a material for the protective layer, colorless and transparent insulating resins such as acrylic resins such as polymethyl (meth)acrylate and polyethyl (meth)acrylate, modified resins thereof, and copolymers thereof, polyester, polyvinyl alcohol, polyvinyl acetate, polyvinyl acetal, polyvinyl butyral, and copolymers thereof, polyurethane, epoxy resin, polyamide, and chlorinated polyolefin can be used.

[0076] 3, power supply unit 40 is electrically connected to mesh wiring layer 20. Power supply unit 40 is made of a substantially rectangular conductive thin plate member. The longitudinal direction of power supply unit 40 is parallel to the X direction, and the lateral direction of power supply unit 40 is parallel to the Y direction.

[0077] Moreover, power supply unit 40 is disposed at a longitudinal end (negative end in the Y direction) of substrate 11. The material of power supply unit 40 may be, for example, a metal material such as gold, silver, copper, platinum, tin, aluminum, iron, or nickel, or an alloy containing these metals.

[0078] When the wiring board 10 is incorporated into the image display device 60 (see FIGS. 1 and 2A), the power supply unit 40 is electrically connected to the communication module 63 of the image display device 60 via the power supply line 85. The power supply unit 40 is provided on the first surface 11a of the substrate 11, but is not limited thereto, and a part or the whole of the power supply unit 40 may be located outside the periphery of the substrate 11. The power supply unit 40 may be configured to be flexible so that it wraps around the side surface or back surface of the image display device 60. In this case, the power supply unit 40 may be electrically connected to the communication module 63 on the side surface or back surface of the image display device 60.

[0079] The mesh wiring layer 20 is electrically connected to the power supply unit 40 on the positive side in the Y direction. In this case, the power supply unit 40 is formed integrally with the mesh wiring layer 20. The thickness T5 (Z direction distance, see FIG. 6) of the power supply unit 40 can be set to be the same as the height H1 (see FIG. 5) of the first direction wiring 21 and the height H2 (see FIG. 6) of the second direction wiring 22, and can be selected, for example, in the range of 0.1 μm to 5.0 μm.

[0080] Next, the configuration of the module will be described with reference to Fig. 7. Fig. 7 is a diagram showing the module according to this embodiment.

[0081] 7, the module 80A includes the above-mentioned wiring board 10 and a power supply line 85 electrically connected to the power supply unit 40 via an anisotropic conductive film 85c. As described above, when the module 80A is incorporated into the image display device 60, the power supply unit 40 of the wiring board 10 is electrically connected to the communication module 63 of the image display device 60 via the power supply line 85.

[0082] The power supply line 85 is pressure-bonded to the wiring board 10 via an anisotropic conductive film (ACF) 85c. The anisotropic conductive film 85c contains a resin material such as an acrylic resin or an epoxy resin, and conductive particles 85d. In the illustrated example, the anisotropic conductive film 85c covers a part of the power supply unit 40. This makes it possible to suppress corrosion of the power supply unit 40.

[0083] The anisotropic conductive film 85c is disposed to face the power supply unit 40. A portion of the conductive particles 85d is in contact with the power supply unit 40. This electrically connects the power supply line 85 to the power supply unit 40. Note that a portion of the anisotropic conductive film 85c may be dissolved around the power supply line 85 when the power supply line 85 is pressure-bonded to the wiring board 10. The particle diameter of the conductive particles 85d may be, for example, about 7 μm.

[0084] The power supply line 85 may be, for example, a flexible printed circuit board. The power supply line 85 has a base material 85a and a metal wiring portion 85b laminated on the base material 85a. Of these, the base material 85a may contain, for example, a resin material such as polyimide or a liquid crystal polymer. The metal wiring portion 85b may contain, for example, copper. The metal wiring portion 85b is electrically connected to the power supply unit 40 via conductive particles 85d.

[0085] [Method of manufacturing a wiring board, a method of manufacturing a module, and a method of manufacturing a laminate for an image display device] Next, with reference to Figures 8(a)-(f), 9(a)-(c), and 10(a)-(d), a method for manufacturing the wiring board 10, the module 80A, and the image display device 60 according to the present embodiment will be described. Figures 8(a)-(f) are cross-sectional views showing a method for manufacturing the wiring board 10 according to the present embodiment. Figures 9(a)-(c) are cross-sectional views showing a method for manufacturing the module 80A according to the present embodiment. Figures 10(a)-(d) are cross-sectional views showing a method for manufacturing the image display device 60 according to the present embodiment.

[0086] First, the method for manufacturing the wiring board according to the present embodiment will be described with reference to FIGS.

[0087] 8(a), a substrate 11 is prepared, which includes a first surface 11a and a second surface 11b located on the opposite side to the first surface 11a. The substrate 11 is transparent.

[0088] Next, on the first surface 11a of the substrate 11, the mesh wiring layer 20 and the power supply section 40 electrically connected to the mesh wiring layer 20 are formed.

[0089] 8(b), first, metal foil 51 is laminated over substantially the entire first surface 11a of substrate 11. In this embodiment, metal foil 51 may have a thickness of 0.1 μm or more and 5.0 μm or less. In this embodiment, metal foil 51 may contain copper.

[0090] 8(c), a photocurable insulating resist 52 is applied to substantially the entire surface of the metal foil 51. As the photocurable insulating resist 52, for example, an organic resin such as an acrylic resin or an epoxy resin can be used.

[0091] 8(d), the insulating layer 54 is formed by photolithography. In this case, the photo-curable insulating resist 52 is patterned by photolithography to form the insulating layer 54 (resist pattern). At this time, the insulating layer 54 is formed so that the metal foil 51 corresponding to the first directional wiring 21 and the second directional wiring 22 is exposed.

[0092] 8(e), the metal foil 51 located on the first surface 11a of the substrate 11 and not covered with the insulating layer 54 is removed. At this time, a wet treatment is performed using ferric chloride, cupric chloride, a strong acid such as sulfuric acid or hydrochloric acid, a persulfate, hydrogen peroxide, or an aqueous solution of these, or a combination of these, to etch the metal foil 51 so as to expose the first surface 11a of the substrate 11.

[0093] 8(f), the insulating layer 54 is removed. In this case, the insulating layer 54 on the metal foil 51 is removed by performing a wet treatment using a permanganate solution, N-methyl-2-pyrrolidone, an acid or alkaline solution, or a dry treatment using oxygen plasma.

[0094] In this manner, a wiring board 10 is obtained, which includes the substrate 11 and the mesh wiring layer 20 provided on the first surface 11a of the substrate 11. In this case, the mesh wiring layer 20 includes first directional wiring 21 and second directional wiring 22. At this time, the power supply unit 40 may be formed by a part of the metal foil. Alternatively, a flat-plate-shaped power supply unit 40 may be separately prepared and electrically connected to the mesh wiring layer 20.

[0095] Next, a method for manufacturing the module according to this embodiment will be described with reference to FIGS.

[0096] First, as shown in Fig. 9(a), the wiring board 10 is prepared. At this time, the wiring board 10 is fabricated, for example, by the method shown in Figs. 8(a)-(f).

[0097] Next, the power supply line 85 is electrically connected to the power supply unit 40 via an anisotropic conductive film 85c including conductive particles 85d. At this time, first, the anisotropic conductive film 85c and the power supply line 85 are disposed on the wiring board 10 as shown in FIG. 9(b). At this time, the anisotropic conductive film 85c is disposed between the power supply line 85 and the power supply unit 40.

[0098] 9(c), the power supply line 85 is pressure-bonded to the wiring board 10. At this time, pressure and heat are applied to the power supply line 85, thereby pressure-bonding the power supply line 85 to the wiring board 10. Then, some of the conductive particles 85d come into contact with the power supply unit 40. In this manner, the power supply line 85 is electrically connected to the power supply unit 40. At this time, some of the anisotropic conductive film 85c may dissolve around the power supply line 85.

[0099] In this manner, a module 80A is obtained that includes the wiring board 10 and the power supply line 85 electrically connected to the power supply unit 40 via the anisotropic conductive film 85c that contains conductive particles 85d.

[0100] Next, a method for manufacturing the image display device 60 according to the present embodiment will be described with reference to FIGS.

[0101] At this time, as shown in FIG. 10(a), for example, the cover glass 75, the decorative layer 74, and the first transparent adhesive layer 95 are laminated together. At this time, a liquid composition for a curable adhesive layer containing a polymerizable compound may be used as the first transparent adhesive layer 95. This composition for a curable adhesive layer may contain a polar group-containing monomer. When the cover glass 75, the decorative layer 74, and the first transparent adhesive layer 95 are laminated together, the first transparent adhesive layer 95 and the like may be heated, for example, so that the first transparent adhesive layer 95 is at about 60°C.

[0102] Next, as shown in FIG. 10(b), the wiring substrate 10 of the module 80A is laminated on the first transparent adhesive layer 95.

[0103] Next, as shown in FIG. 10(c), a second transparent adhesive layer 96 is laminated on the wiring board 10. At this time, a liquid composition for a curable adhesive layer containing a polymerizable compound may be used as the second transparent adhesive layer 96. The composition for a curable adhesive layer may contain a polar group-containing monomer. In this way, by laminating the second transparent adhesive layer 96 on the wiring board 10, the wiring board 10 is sandwiched between the first transparent adhesive layer 95 and the second transparent adhesive layer 96. In this way, a laminate 70 for an image display device including the first transparent adhesive layer 95, the second transparent adhesive layer 96, and the wiring board 10 is obtained. When laminating the second transparent adhesive layer 96 on the wiring board 10, the first transparent adhesive layer 95 and the like may be heated, for example, so that the first transparent adhesive layer 95 and the second transparent adhesive layer 96 are at about 60°C.

[0104] 10(d), the display device 61 is laminated on the second transparent adhesive layer 96. At this time, the first transparent adhesive layer 95 and the second transparent adhesive layer 96 may be heated, for example, so that the first transparent adhesive layer 95 and the second transparent adhesive layer 96 are heated to about 60° C.

[0105] Here, as described above, at least one of the first transparent adhesive layer 95 and the second transparent adhesive layer 96 contains a resin material having a softening point of 50°C or more and 200°C or less. In addition, a resin material having a softening point of 50°C or more and 200°C or less after curing may have a softening point of about 25°C or more and about 50°C or less before curing. In this way, when the material of the first transparent adhesive layer 95 or the like is a resin material having a softening point of 25°C or more and 50°C or less before curing, the fluidity of the resin material increases when the first transparent adhesive layer 95 or the like is heated to about 60°C. Therefore, when the display device 61 is laminated on the first transparent adhesive layer 95 or the like, the first transparent adhesive layer 95 and the second transparent adhesive layer 96 deform in the thickness direction in the region where the display device 61 overlaps with the wiring board 10, and absorb the thickness of the wiring board 10. This makes it possible to suppress the occurrence of a step in the second transparent adhesive layer 96 at the periphery of the wiring board 10. Therefore, deformation of the display device 61 due to a step generated in the second transparent adhesive layer 96 can be suppressed.

[0106] Next, the first transparent adhesive layer 95 and the second transparent adhesive layer 96 are cured using, for example, ultraviolet (UV) rays.

[0107] In this manner, the image display device 60 including the laminate for an image display device 70 and the display device 61 laminated on the laminate for an image display device 70 is obtained.

[0108] [Operation of this embodiment] Next, the operation of this embodiment having the above configuration will be described.

[0109] 1 and 2A, the wiring board 10 is incorporated into an image display device 60 having a display device 61. At this time, the wiring board 10 is placed on the display device 61. The mesh wiring layer 20 of the wiring board 10 is electrically connected to the communication module 63 of the image display device 60 via the power supply unit 40 and the power supply line 85. In this way, radio waves of a predetermined frequency can be transmitted and received via the mesh wiring layer 20, and communication can be performed using the image display device 60.

[0110] According to this embodiment, a part of the substrate 11 is disposed in a part between the first transparent adhesive layer 95 and the second transparent adhesive layer 96. In addition, the difference between the refractive index of the substrate 11 and the refractive index of the first transparent adhesive layer 95 is 0.05 or less, and the difference between the refractive index of the substrate 11 and the second transparent adhesive layer 96 is 0.05 or less. This suppresses the reflection of visible light at the interface B1 between the substrate 11 and the first transparent adhesive layer 95 and the interface B2 between the substrate 11 and the second transparent adhesive layer 96, making the substrate 11 difficult to be seen by the naked eye of the observer. Furthermore, at least one of the first transparent adhesive layer 95 and the second transparent adhesive layer 96 contains a resin material having a softening point of 50° C. or more and 200° C. or less. This increases the fluidity of the resin material, and suppresses the display device 61 from being deformed when the display device 61 is laminated on the first transparent adhesive layer 95 or the like.

[0111] Here, if the fluidity of the resin material constituting the first transparent adhesive layer 95, etc. is low, when the display device 61 is laminated on the first transparent adhesive layer 95, etc., a large force may be locally applied to the display device 61. As described above, in this embodiment, a part of the substrate 11 is disposed in a part between the first transparent adhesive layer 95 and the second transparent adhesive layer 96. In addition, the rigidity of the display device 61 may be lower than the rigidity of the cover glass 75. Therefore, as a comparative example, if the fluidity of the resin material constituting the first transparent adhesive layer 95, etc. is low, a step may occur in the second transparent adhesive layer 96 at the periphery of the wiring substrate 10 due to the thickness of the wiring substrate 10. In this way, if a step occurs in the second transparent adhesive layer 96 at the periphery of the wiring substrate 10, the display device 61 may be deformed due to the step occurring in the second transparent adhesive layer 96 (see FIG. 11).

[0112] In contrast, according to the present embodiment, at least one of the first transparent adhesive layer 95 and the second transparent adhesive layer 96 contains a resin material having a softening point of 50° C. or more and 200° C. or less. This can increase the fluidity of the resin material constituting the first transparent adhesive layer 95, etc. Therefore, when the display device 61 is laminated on the first transparent adhesive layer 95, etc., it is possible to suppress the application of a large force locally to the display device 61 from the resin material constituting the first transparent adhesive layer 95, etc. As a result, it is possible to suppress the display device 61 from being deformed when the display device 61 is laminated on the first transparent adhesive layer 95, etc. Therefore, it is possible to make it difficult for an observer to recognize the presence of the wiring board 10.

[0113] Also, according to this embodiment, the wiring board 10 includes the substrate 11 and the mesh wiring layer 20 disposed on the substrate 11. The substrate 11 is transparent. The mesh wiring layer 20 has a conductor portion as a forming portion of an opaque conductive layer and a mesh-like pattern with a large number of openings. This ensures the transparency of the wiring board 10. As a result, when the wiring board 10 is disposed on the display device 61, the display device 61 can be seen through the openings 23 of the mesh wiring layer 20, and the visibility of the display device 61 is not hindered.

[0114] Next, modified examples of the wiring board will be described.

[0115] Figures 12 and 13 show a first modified example of the wiring board. The modified example shown in Figures 12 and 13 is different in that a dummy wiring layer 30 is provided around the mesh wiring layer 20, and other configurations are substantially the same as the embodiment shown in Figures 1 to 11 described above. In Figures 12 and 13, the same parts as those in the embodiment shown in Figures 1 to 11 are given the same reference numerals and detailed description will be omitted.

[0116] 12, a dummy wiring layer 30 is provided along the periphery of the mesh wiring layer 20. Unlike the mesh wiring layer 20, this dummy wiring layer 30 does not substantially function as an antenna.

[0117] As shown in FIG. 13, the dummy wiring layer 30 is composed of repeated dummy wirings 30a having a predetermined pattern shape. That is, the dummy wiring layer 30 includes a plurality of dummy wirings 30a, and each dummy wiring 30a is electrically independent from the mesh wiring layer 20 (the first directional wiring 21 and the second directional wiring 22). The plurality of dummy wirings 30a are regularly arranged over the entire area of ​​the dummy wiring layer 30. The plurality of dummy wirings 30a are spaced apart from each other in the planar direction and are arranged protruding above the substrate 11. That is, each dummy wiring 30a is electrically independent from the mesh wiring layer 20, the power supply section 40, and other dummy wirings 30a. The shape of each dummy wiring 30a is approximately L-shaped in a planar view.

[0118] In this case, the dummy wiring 30a has a shape in which a part of the pattern shape of the mesh wiring layer 20 described above is missing. This makes it difficult to visually recognize the difference between the mesh wiring layer 20 and the dummy wiring layer 30, and makes the mesh wiring layer 20 arranged on the substrate 11 difficult to see. As shown in FIG. 13, the dummy wiring 30a extends parallel to the first directional wiring 21 or the second directional wiring 22. Specifically, the dummy wiring 30a includes a first portion 31a extending parallel to the first directional wiring 21 and a second portion 32a extending parallel to the second directional wiring 22. In this way, the dummy wiring 30a extends parallel to the first directional wiring 21 or the second directional wiring 22, making it possible to make the mesh wiring layer 20 arranged on the substrate 11 even more difficult to see. The aperture ratio of the dummy wiring layer 30 may be the same as or different from the aperture ratio of the mesh wiring layer 20, but is preferably close to the aperture ratio of the mesh wiring layer 20.

[0119] As in this modified example, the dummy wiring layer 30 that is electrically independent from the mesh wiring layer 20 is provided around the mesh wiring layer 20, thereby making the outer edge of the mesh wiring layer 20 unclear. This makes it possible to make the mesh wiring layer 20 less visible on the surface of the image display device 60, and makes it difficult for a user of the image display device 60 to recognize the mesh wiring layer 20 with the naked eye.

[0120] Figures 14 and 15 show a second modified example of the wiring board. The modified example shown in Figures 14 and 15 is different in that a plurality of dummy wiring layers 30A, 30B having different aperture ratios are provided around the mesh wiring layer 20, and other configurations are substantially the same as those shown in Figures 1 to 13. In Figures 14 and 15, the same parts as those shown in Figures 1 to 13 are given the same reference numerals and detailed description is omitted.

[0121] 14, a plurality of (two in this case) dummy wiring layers 30A, 30B (a first dummy wiring layer 30A and a second dummy wiring layer 30B) having different aperture ratios are provided along the periphery of the mesh wiring layer 20. Specifically, the first dummy wiring layer 30A is disposed along the periphery of the mesh wiring layer 20, and the second dummy wiring layer 30B is disposed along the periphery of the first dummy wiring layer 30A. Unlike the mesh wiring layer 20, these dummy wiring layers 30A, 30B do not substantially function as antennas.

[0122] As shown in FIG. 15, the first dummy wiring layer 30A is composed of repeated dummy wirings 30a1 having a predetermined pattern shape. The second dummy wiring layer 30B is composed of repeated dummy wirings 30a2 having a predetermined pattern shape. That is, the dummy wiring layers 30A and 30B each include a plurality of dummy wirings 30a1 and 30a2, and each of the dummy wirings 30a1 and 30a2 is electrically independent from the mesh wiring layer 20. The dummy wirings 30a1 and 30a2 are regularly arranged over the entire area of ​​the dummy wiring layers 30A and 30B, respectively. The dummy wirings 30a1 and 30a2 are spaced apart from each other in the planar direction and are arranged to protrude above the substrate 11. The dummy wirings 30a1 and 30a2 are electrically independent from the mesh wiring layer 20, the power supply unit 40, and the other dummy wirings 30a1 and 30a2, respectively. Each of the dummy wirings 30a1 and 30a2 has a substantially L-shape in plan view.

[0123] In this case, the dummy wirings 30a1 and 30a2 have a shape in which a part of the pattern shape of the mesh wiring layer 20 described above is missing. This makes it difficult to visually recognize the difference between the mesh wiring layer 20 and the first dummy wiring layer 30A and the difference between the first dummy wiring layer 30A and the second dummy wiring layer 30B, and makes it difficult to see the mesh wiring layer 20 arranged on the substrate 11. As shown in FIG. 15, the dummy wirings 30a1 and 30a2 extend parallel to the first directional wiring 21 or the second directional wiring 22. Specifically, the dummy wiring 30a1 includes a first portion 31a1 extending parallel to the first directional wiring 21 and a second portion 32a1 extending parallel to the second directional wiring 22. The dummy wiring 30a2 includes a first portion 31a2 extending parallel to the first directional wiring 21 and a second portion 32a2 extending parallel to the second directional wiring 22.

[0124] The area of ​​each dummy wiring 30a1 in the first dummy wiring layer 30A is larger than the area of ​​each dummy wiring 30a2 in the second dummy wiring layer 30B. In this case, the line width of each dummy wiring 30a1 is the same as the line width of each dummy wiring 30a2, but this is not limited thereto, and the line width of each dummy wiring 30a1 may be larger than the line width of each dummy wiring 30a2. Other configurations of the dummy wirings 30a1 and 30a2 are similar to the configuration of the dummy wiring 30a in the third modified example, so detailed description will be omitted here.

[0125] In this modification, the aperture ratio of the mesh wiring layer 20 and the plurality of dummy wiring layers 30A, 30B is preferably increased stepwise from the mesh wiring layer 20 toward the dummy wiring layers 30A, 30B far from the mesh wiring layer 20. In other words, the aperture ratio of each dummy wiring layer is preferably gradually increased from the one closer to the mesh wiring layer 20 toward the one farther from the mesh wiring layer 20. In this case, the aperture ratio of the first dummy wiring layer 30A is preferably larger than the aperture ratio of the mesh wiring layer 20. The aperture ratio of the second dummy wiring layer 30B is preferably larger than the aperture ratio of the first dummy wiring layer 30A. This makes it possible to further obscure the outer edges of the mesh wiring layer 20 and the dummy wiring layers 30A, 30B. Therefore, it is possible to further make the mesh wiring layer 20 less visible on the surface of the image display device 60.

[0126] In this manner, by disposing the dummy wiring layers 30A and 30B electrically independent from the mesh wiring layer 20, the outer edge of the mesh wiring layer 20 can be made more unclear. This makes it possible to make the mesh wiring layer 20 less visible on the surface of the image display device 60, and makes it difficult for a user of the image display device 60 to recognize the mesh wiring layer 20 with the naked eye. Note that three or more dummy wiring layers having different aperture ratios may be provided around the mesh wiring layer 20.

[0127] Fig. 16 shows a third modified example of the wiring board. The modified example shown in Fig. 16 differs in the planar shape of the mesh wiring layer 20, and other configurations are substantially the same as those shown in Figs. 1 to 15. In Fig. 16, the same parts as those shown in Figs. 1 to 15 are given the same reference numerals and detailed description is omitted.

[0128] 16, the first directional wiring 21 and the second directional wiring 22 intersect at an angle (non-right angle), and each opening 23 is formed in a diamond shape in a plan view. The first directional wiring 21 and the second directional wiring 22 are not parallel to either the X direction or the Y direction, but either one of the first directional wiring 21 and the second directional wiring 22 may be parallel to the X direction or the Y direction.

[0129] [Example] Next, a specific example of this embodiment will be described.

[0130] Example 1 An image display device 60 having the configuration shown in FIG. 2A was fabricated.

[0131] At this time, a cycloolefin polymer substrate having a thickness of 13 μm was used as substrate 11 of wiring board 10. Substrate 11 had a refractive index of 1.535.

[0132] In addition, an OCA layer made of an acrylic resin having a thickness of 100 μm was used as the first transparent adhesive layer 95 and the second transparent adhesive layer 96. At this time, a composition for a curable adhesive layer was used as the resin material constituting the first transparent adhesive layer 95 and the second transparent adhesive layer 96. Specifically, a resin material having a softening point of 40° C. before curing was used as the resin material constituting the first transparent adhesive layer 95 and the second transparent adhesive layer 96. The softening points of the first transparent adhesive layer 95 and the second transparent adhesive layer 96 after curing were 100° C. The softening points of the first transparent adhesive layer 95 and the second transparent adhesive layer 96 were measured by nanoTA measurement. In the nanoTA measurement, a scanning probe microscope (nanoTA manufactured by Anasys Instruments) was used. At this time, the probe used was PR-EXP-AN2-300-5 manufactured by Anasys Instruments. In addition, the refractive index of the first transparent adhesive layer 95 and the second transparent adhesive layer 96 was 1.534, respectively.

[0133] Next, a visibility evaluation test was conducted. In the visibility evaluation test, the visibility of the wiring board in the image display device was confirmed. Specifically, the image display device was observed from the light emitting surface side and the opposite side to the light emitting surface, and the visibility of the wiring board 10 was confirmed.

[0134] Comparative Example 1 A visibility evaluation test was performed in the same manner as in Example 1, except that a non-curable resin material was used as the material for the first transparent adhesive layer 95 and the second transparent adhesive layer 96, the softening points of the first transparent adhesive layer 95 and the second transparent adhesive layer 96 were 270°C, and the refractive indexes of the first transparent adhesive layer 95 and the second transparent adhesive layer 96 were each 1.531.

[0135] The above results are shown in Tables 1 to 4. In Table 4, "A (excellent)" means that no deformation (distortion) occurred in the display device 61 at the periphery of the wiring board 10. Also, "B (poor)" means that deformation (distortion) occurred in the display device 61 at the periphery of the wiring board 10.

[0136] [Table 1]

[0137] [Table 2]

[0138] [Table 3]

[0139] [Table 4]

[0140] As a result, as shown in Table 1, in Comparative Example 1, deformation (distortion) occurred in display device 61 at the periphery of wiring board 10. In contrast, in Example 1, deformation (distortion) did not occur in display device 61 at the periphery of wiring board 10. For this reason, it was found that image display device 60 according to the present embodiment can make it difficult for an observer to recognize the presence of wiring board 10.

[0141] It is also possible to combine the multiple components disclosed in the above embodiment and each modification as necessary, or to delete some of the components disclosed in the above embodiment and each modification.

Claims

1. A laminate for an image display device; a display device laminated on the laminate for an image display device, The laminate for an image display device is A wiring board including a substrate including a first surface and a second surface located opposite to the first surface, and a mesh wiring layer disposed on the first surface of the substrate; A first adhesive layer located on the first surface side of the substrate; a second adhesive layer located on the second surface side of the substrate, The substrate is transparent, a portion of the substrate is disposed in a portion between the first adhesive layer and the second adhesive layer; a difference between a refractive index of the substrate and a refractive index of the first adhesive layer is 0.05 or less; a difference between a refractive index of the substrate and a refractive index of the second adhesive layer is 0.05 or less; At least one of the first adhesive layer and the second adhesive layer contains a resin material having a softening point of 50° C. or higher and 200° C. or lower.

2. The image display device according to claim 1 , wherein the first adhesive layer and the second adhesive layer contain a resin material having a softening point of 50° C. or more and 200° C. or less.

3. a difference between a refractive index of the substrate and a refractive index of the first adhesive layer is 0.02 or less; The image display device according to claim 1 , wherein a difference between a refractive index of the substrate and a refractive index of the second adhesive layer is 0.02 or less.

4. The image display device according to claim 1 , wherein the wiring board has a radio wave transmitting and receiving function.

5. 2. The image display device according to claim 1, wherein the wiring substrate is provided with a dummy wiring layer around the mesh wiring layer, the dummy wiring layer being electrically independent from the mesh wiring layer.

6. 6. The image display device according to claim 5, wherein a plurality of the dummy wiring layers are provided in the wiring substrate, and the aperture ratios of the mesh wiring layer and the dummy wiring layer are gradually increased from the mesh wiring layer to the dummy wiring layer farther from the mesh wiring layer.

Citation Information

Patent Citations

  • Liquid crystal display and its manufacturing method

    JP2004013001A

  • EMI shield film and manufacturing method therefor

    JP2004039981A

  • Laminate for image display device and image display device

    JP2022161726A

  • Adhesive composition, adhesive layer, and adhesive sheet

    JP2023016420A

  • Display Module

    JP7666509B2