Inspection device with reaction part containing microparticles

The microchip with embedded fine particles in a water-soluble immobilizing agent addresses dispersion and stability issues, improving reaction uniformity and measurement accuracy for biologically derived components.

JP2024142218APending Publication Date: 2024-10-10FUJIMORI KOGYO CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2023054291
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-29
Publication Date
2024-10-10

AI Technical Summary

Technical Problem

Existing microchips used for analyzing biologically derived components face challenges in dispersing fine particles containing reactive substances like antibodies, antigens, proteins, sugar chains, and nucleic acids, leading to difficulties in maintaining the stability and accuracy of reaction dispersion and measurement results.

Method used

The microchip incorporates a reaction part with fine particles carrying reactive substances embedded in a water-soluble immobilizing agent, allowing for efficient dispersion and fixation during use, using a curing agent to stabilize the particles and improve measurement accuracy.

Benefits of technology

The solution ensures uniform reaction dispersion and enhances the accuracy of measurement results by stabilizing reactive substances over time, facilitating efficient and accurate analysis of biological components.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024142218000001_ABST
    Figure 2024142218000001_ABST
Patent Text Reader

Abstract

To provide an inspection device with a reaction part containing microparticles carrying reactive substances on the surfaces capable of improving the accuracy of measurement results using the inspection device by increasing the dispersion of microparticles during and after the reaction while fixing microparticles when not in use and suppressing the deterioration of reactive substances over time.SOLUTION: The inspection device has a reaction part containing microparticles carrying reactive substances on the surfaces to analyze the target substance in a liquid sample by allowing a reaction with a reactive substance by adding or injecting liquid into the reaction part. In the inspection device, the microparticles are embedded in a water-soluble fixative and are fixed to the reaction part.SELECTED DRAWING: Figure 5
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an inspection device such as a microchip used for analyzing or testing components derived from living organisms, and a manufacturing method thereof, and more particularly to an inspection device such as a microchip provided with a reaction portion containing fine particles carrying a reactive substance on the surface thereof, and a manufacturing method thereof. [Background technology]

[0002] Microchips used to analyze and test components of biological origin contain microparticles in the reaction section that carry reactive substances such as antibodies that bind to the components of biological origin, and detect and analyze the reaction between the components of biological origin (substances to be measured) and the reactive substances. Patent Document 1 (WO2009 / 136541) describes an insoluble carrier particle carrying an antibody or an antigen on the particle surface. Although a method for producing the particles is disclosed, as described in paragraph 0005 etc., there is a problem in that it is difficult to disperse the particles immediately. Patent Document 2 (JP 2000-219820 A) and Patent Document 3 (JP 2003-213151 A) disclose that a dispersion aid that forms a protective colloid in a dispersion medium is added to stabilize the dispersion state. However, although these methods can stabilize the dispersion state, it is difficult to quickly redisperse fine particles that have once adhered. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] WO2009 / 136541 [Patent Document 2] Patent Publication No. 2000-219820 [Patent Document 3] Patent Publication No. 2003-213151 Summary of the Invention [Problem to be solved by the invention]

[0004] The present invention aims to improve the accuracy of measurement results using a testing device equipped with a reaction section containing microparticles carrying reactive substances such as proteins, glycans, and nucleic acids on their surfaces, by suppressing deterioration of the reactive substances over time, fixing the microparticles when not in use, and increasing the dispersibility of the microparticles during and after the reaction. [Means for solving the problem]

[0005] The present inventors have conducted intensive research to solve the above problems. As a result, in a test device having a reaction section in which microparticles carrying a reactive substance are accommodated, and for adding or flowing a liquid into the reaction section to react the reactive substance with a substance to be measured in a liquid sample for analysis, the microparticles are fixed to the reaction section in a state where they are embedded in a water-soluble immobilizing agent, so that when a liquid is added or flowed into the reaction section to perform a reaction, the reactive substance is stabilized by the water-soluble immobilizing agent when not in use, and the microparticles are efficiently dispersed when in use, so that the reaction can be performed uniformly and the accuracy of the measurement result can be improved. Furthermore, the present inventors have found a preferred form of a microchip as one embodiment of a test device containing such microparticles, and have completed the present invention.

[0006] One aspect of the present invention relates to an inspection device having a reaction section containing microparticles carrying a reactive substance on their surface, and for analysis by adding or flowing liquid into the reaction section to react the reactive substance with a substance to be measured in a liquid sample, characterized in that the microparticles are fixed to the reaction section in a state embedded in a water-soluble immobilizing agent.

[0007] Another aspect of the present invention is A step of preparing a substrate having an area to be a reaction portion; The fine particles carrying a reactive substance on their surface are dispersed in an aqueous solution of 0.5 to 5.0 vol% water-soluble immobilizing agent. preparing a microparticle dispersion; adding the microparticle dispersion to a region of the substrate that will become a reaction portion; and drying the microparticle dispersion; The present invention relates to a method for producing an assay device having a reaction portion in which fine particles carrying a reactive substance on the surface are fixed in a state embedded in a water-soluble immobilizing agent, the method comprising the steps of: Effect of the Invention

[0008] According to the testing device of the present invention, microparticles carrying reactive substances on their surfaces are dispersed in an aqueous solution of a water-soluble fixing agent and then fixed to the reaction section of the testing device in a state embedded in the water-soluble fixing agent, thereby suppressing deterioration over time of reactive substances such as proteins, glycans, and nucleic acids carried on the surface of the microparticles, while when a liquid sample is added or poured in to cause a reaction, the microparticles are efficiently dispersed, allowing the reaction to be carried out uniformly and improving the accuracy of the measurement results. By using a biochip in which microparticles are fixed to a reaction section, tests can be easily performed by adding a liquid sample such as a specimen and causing it to react with reactive substances such as proteins bound to the surface of the microparticles. [Brief description of the drawings]

[0009] [Figure 1] FIG. 2 shows a substrate of a microchip according to one embodiment of the present invention prior to application of adhesive. [Diagram 2] FIG. 2 shows a substrate of a microchip according to one embodiment of the present invention after application of adhesive. [Diagram 3] FIG. 2 is a diagram showing a completed microchip according to one embodiment of the present invention in which a film is attached to a substrate. [Figure 4] FIG. 2 is a diagram showing a part of the AA cross section of a microchip according to one embodiment of the present invention. [Diagram 5] FIG. 13 is a diagram showing a state in which a liquid sample is introduced. [Figure 6] FIG. 13 is a diagram showing how beads are blocked by a wall. [Figure 7] FIG. 1 shows a substrate of a microchip according to one embodiment of the present invention. [Figure 8] FIG. 1 shows a film of a microchip according to one embodiment of the present invention. [Figure 9] FIG. 2 is a diagram showing bonding of a substrate and a film of a microchip according to one embodiment of the present invention. [Figure 10] FIG. 2 is a completed view of a microchip according to one embodiment of the present invention. [Figure 11] Photographs showing the state of magnetic nanoparticles before and after injection into a microchip (with and without glycerin treatment). [Figure 12] 1 is a graph showing the results of evaluating the enzymatic activity of thrombin using the S-2238 reagent. [Figure 13] FIG. 1 shows a substrate of a microchip according to one embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] The microchip of the present invention is an inspection device having a reaction section containing microparticles carrying a reactive substance on their surface, and for analysis by adding or flowing liquid into the reaction section to cause a reaction between the substance to be measured in the liquid sample and the reactive substance, characterized in that the microparticles are fixed to the reaction section in a state where they are embedded in a water-soluble immobilizing agent.

[0011] The testing device is not particularly limited as long as it contains particles and has a reaction section to which a liquid can be added. For example, the testing device may have a substrate having a depression on the surface that serves as the reaction section. The type of the test device is not particularly limited, but a preferred example is a microchip.

[0012] The material of the substrate of the testing device can be metal, glass, plastic, silicone, etc., but from the viewpoint of detecting the reaction by light emission, color development, or visually, a transparent material is preferable, and a transparent plastic is more preferable. Examples include polyethylene, polypropylene, polystyrene, polymethyl methacrylate, cycloolefin polymer, cycloolefin copolymer, polyphenylene oxide, polyethylene terephthalate, polyethylene naphthalate, polycarbonate, polyamide, polyimide, phenol resin, epoxy resin, polyvinylidene chloride, polyvinyl chloride, ABS resin, poly(2-methoxyethyl acrylate) (PMEA) resin, etc.

[0013] The grooves and holes in the substrate of the testing device can be dug with a blade or a laser beam, but if the material of the microchip is plastic, they can also be formed by injection molding, which is preferable because it allows efficient production of microchips of consistent quality.

[0014] The test device preferably has a flow path (inlet flow path) that is connected to the reaction section and can supply a liquid sample to the reaction section. Such a flow path can be produced by providing a groove on the surface of the substrate that is connected to a depression that serves as the reaction section. The test device may also have a flow path (outlet flow path) that is connected to the reaction section and can allow the liquid sample to flow out from the reaction section. The test device may also include a member such as a film that covers the reaction section and the flow channel. Such an embodiment of the microchip will be described later.

[0015] There are no particular limitations on the size of the microparticles as long as they are capable of carrying a reactive substance on their surface and are capable of being dispersed when a liquid sample is added, but the size of the microparticles is preferably an average particle size of 50 nm to 5 μm, and more preferably 1 to 5 μm. The material of the microparticles is not particularly limited as long as it does not inhibit the reaction between the substance to be measured in the liquid sample and the reactive substance, and examples of the material include metals, polymeric materials such as polystyrene, and inorganic materials such as silica. However, magnetic microparticles are preferred when using magnetism to stir the liquid in the flow path or when recovering and analyzing the microparticles after the reaction.

[0016] The magnetic fine particles are not particularly limited as long as they are magnetic particles. Examples of the magnetic fine particles include ferrite magnets, samarium-cobalt magnets, rare earth magnets, iron, manganese, cobalt, and trioxide. The particles may be fine particles of a magnetic metal or metal compound such as iron, ferric oxide, ferritic stainless steel, martensitic stainless steel, amorphous alloy, silicon-iron weak magnetic crystal, nickel, chromium, etc. If necessary, the particles may be coated with or contain a polymer or an oleophilizing agent. For example, "Dynabeads M-270 Carboxylic acid" (Veritas) is a paramagnetic or superparamagnetic particle. Paramagnetic particles are coated with a polymer, and the polymer has a carboxyl group.

[0017] The microparticles used have a substance (reactive substance) on the surface that can react with components in a liquid sample. The reactive substance may be any substance that reacts with the target (detection target) component in the liquid sample, and can be appropriately selected depending on the type of target substance. The reactivity of the reactive substance can be a biological reaction or a chemical reaction, and biological reactions also include binding reactions. The binding reaction includes not only the formation of covalent bonds, but also the formation of hydrogen bonds, hydrophobic interactions, and binding between a substrate and a receptor or enzyme. Reactive substances include proteins (including peptides), sugars, nucleic acids, low molecular weight compounds, and the like. For example, substances such as antibodies that specifically bind to the target substance, and substances that use the target substance as a substrate are also available. Examples of the target substance include blood coagulation factors such as enzyme proteins and PT reagents. In addition, when the target substance is a nucleic acid, a nucleic acid probe or a polymerase that amplifies a nucleic acid (nucleic acid amplification enzyme) may be used.

[0018] The magnetic particles are fixed to the reaction zone in a state where they are embedded in a water-soluble immobilizing agent. For example, microparticles are dispersed in an aqueous solution of a water-soluble fixing agent, and the resulting microparticle dispersion is spotted onto an area of ​​the substrate that will become a reaction site, and then dried, whereby the microparticles are dried and fixed to the reaction site in the concentrated water-soluble fixing agent.

[0019] A water-soluble fixative is a compound that can fix fine particles to a substrate in the presence of a trace amount of moisture or in the absence of moisture, and that dissolves or disperses in water or an aqueous solution when immersed in water or an aqueous solution. Examples of water-soluble fixatives include water-soluble polymers, salts of water-soluble polymers, water-soluble and nonionic organic compounds, water-soluble organic compounds having anionic substituents, salts of water-soluble organic compounds having anionic substituents and cations, water-soluble organic compounds having cationic substituents, salts of water-soluble organic compounds having cationic substituents and anions, water-soluble organic compounds having cationic and anionic substituents, salts of water-soluble organic compounds having cationic and anionic substituents and anions or cations.

[0020] Examples of the water-soluble polymer include partially saponified polyvinyl acetate, polyvinyl alcohol, water-soluble polyethers such as polyethylene glycol, poly(meth)acrylic acid, water-soluble proteins such as collagen, water-soluble polysaccharides such as gelatin and alginic acid, peptides, protein hydrolysates, polyglycerin, polystyrene sulfonic acid, polyphosphoric acid, water-soluble polyethyleneimine, polylysine, polyglutamic acid, polyaspartic acid, polyhistidine, poly(meth)acrylamide, water-soluble polyhydroxycarboxylic acid, water-soluble polyamide, and water-soluble polyester.

[0021] Examples of the water-soluble, nonionic organic compounds include polyhydric alcohols such as ethylene glycol and glycerin; ethylene oxide adducts of polyhydric alcohols such as ethylene oxide adducts of glycerin; partial ester compounds of polyhydric alcohols such as glycerin monoesters and glycerin diesters; and sugars such as trehalose, dextrin, maltodextrin, guar gum, gum arabic, tamarind gum, xanthan gum, cationized xanthan gum, hyaluronic acid, hyaluronate salts, and carboxymethylcellulose. Examples of the water-soluble organic compound having an anionic substituent include polycarboxylic acids such as maleic acid and aconitic acid, and partial saponification products of polycarboxylic acid esters such as aconitic acid monoesters and aconitic acid diesters. Examples of the organic compound that is water-soluble and has a cationic substituent include (meth)acrylamide, lysine, histidine, and tryptophan.

[0022] Here, the aqueous solution of the water-soluble fixing agent is an aqueous solution of 0.5 to 5.0 vol % water-soluble fixing agent. It is preferable to use a water-soluble immobilizing agent, which is spotted on the above region and dried so that the concentration of the water-soluble immobilizing agent that encapsulates the microparticles in the reaction section becomes 50 to 95 vol %.

[0023] The testing device of the present invention can be used by adding or flowing a liquid sample into the reaction section, and reacting the target substance in the liquid sample with the reactive substance on the surface of the microparticles. By adding the liquid sample to the reaction section, the microparticles are dispersed in the reaction section, and the target substance in the liquid sample reacts with the reactive substance on the surface of the microparticles. By detecting this reaction, the target substance in the liquid sample can be detected, and by quantifying the reaction, the target substance can be quantified. In addition, when the microparticles are magnetic microparticles, the magnetic microparticles after the reaction can be collected with a magnet or the like for detection or quantification.

[0024] The test device of the present invention can be manufactured by the following steps. A step of preparing a substrate having an area to be a reaction portion; The microparticles carrying a reactive substance on their surface are dispersed in a 0.5 to 5.0 vol% aqueous solution of a water-soluble immobilizing agent. preparing a microparticle dispersion; adding the microparticle dispersion to a region of the substrate that will become a reaction portion; and A step of drying the fine particle dispersion.

[0025] The substrate may be a substrate having a depression on its surface as described above. A film or the like may be attached onto the depression to serve as the reaction site, to form a testing device having a reaction site inside.

[0026] The concentration of the water-soluble immobilizing agent solution in which the magnetic particles are dispersed should be 0.5 to 5.0 vol%. However, the concentration is preferably 1.0 to 2.5 vol %. If the agent concentration is too high, the water-soluble fixing agent layer after drying will become bulky, causing problems such as poor drying and fixing, etc. The concentration of the fine particles in the dispersion is preferably 1.0 to 5.0 wt %. The dispersion time is preferably from 30 minutes to 24 hours.

[0027] There are no particular limitations on the method for adding the dispersion to the region that will become the reaction portion of the testing device, but it is preferable to add it dropwise using a dispenser, inkjet, pipette, or the like.

[0028] The surface of the substrate of the testing device to which the microparticles are fixed in the reaction area preferably has a water contact angle in the range of 30° to 100°. Although it is preferable to use a substrate having a water contact angle in the range of 30° to 100°, the surface may be subjected to a surface treatment so that the water contact angle of the surface to which the microparticles are fixed in the reaction area is in the range of 30° to 100°. By setting the water contact angle in this range, the microparticle dispersion can be efficiently spotted, and by drying, a layer of the water-soluble immobilizing agent in which the microparticles are embedded can be efficiently formed.

[0029] The surface treatment is preferably a coating of a reagent that changes the water contact angle of the surface, a plasma treatment, an excimer treatment, or a corona treatment. Examples of the reagent that changes the water contact angle of the surface include Beamset 1461 (Arakawa Chemical Industries, Ltd.), RX-6-AQ P-2200 (Nippon Shokubai Co., Ltd.), and HFC-ASL8 (Harima Chemicals Co., Ltd.).

[0030] The drying method is not particularly limited, and examples thereof include drying by a blower. The air blown by the blower may be at room temperature, or may be hot air or cold air. The air blown by the blower may be directly applied to the microchip, or the gas may be circulated in the drying chamber. In addition to drying by a blower, drying by reduced pressure, drying by freeze-drying, and drying by irradiation with energy rays such as microwaves, high frequency waves, and infrared rays may be used. Furthermore, a combination of the above drying methods may be used. The method may be appropriately selected according to the type of fine particles and the properties of the substance solidified on the surface of the fine particles. The concentration of the water-soluble immobilizing agent after drying is preferably 50 to 95 vol%. In the case of drying at room temperature and normal pressure, the concentration of the water-soluble immobilizing agent is equilibrated at about 95 vol%, and the water-soluble immobilizing agent can be immobilized in the reaction section in this state.

[0031] Hereinafter, the microchip, which is one embodiment of the testing device of the present invention, will be described with reference to preferred embodiments, although the testing device of the present invention is not limited to the following embodiments.

[0032] The microchip, which is one embodiment of the testing device of the present invention, has a reaction section in which microparticles carrying a reactive substance on their surface (hereinafter, sometimes simply referred to as microparticles) are fixed in a state embedded in a water-soluble fixing agent, an inlet side flow path connected to the reaction section and for flowing liquid into the reaction section, and an outlet side flow path connected to the reaction section and for flowing liquid out of the reaction section. The microchip, which is one embodiment of the test device of the present invention, has a connecting portion between the reaction portion and the outlet side flow channel. In this case, the reaction chamber may have a wall for blocking the particles, which can prevent the particles from flowing out of the reaction chamber when the liquid sample is introduced into the reaction chamber and reacted therewith, and after the reaction has occurred, thereby enabling more efficient and accurate measurement.

[0033] The microchip may have the reaction section, the inlet flow channel, and the outlet flow channel inside. That is, the microchip may be a microchip for analyzing components in a sample by passing a liquid sample through a flow channel formed inside the microchip and reacting a substance to be measured in the liquid sample with a reactive substance supported on microparticles placed in the reaction section in the flow channel. In such a case, an inlet may be provided at the start of the inlet flow path to supply liquid to the inlet flow path, and an outlet may be provided at the end of the outlet flow path to allow the liquid to flow out. In another embodiment, a waste liquid reservoir for accumulating liquid may be provided at the end of the outlet flow path.

[0034] Such a microchip having the reaction part, the inlet-side flow path, and the outlet-side flow path inside may be a microchip obtained by bonding a substrate and a film. In such a case, a microchip obtained by bonding a substrate having a depression on the surface that serves as the reaction part and a groove that serves as the flow path (inlet-side flow path and outlet-side flow path) to a film with an adhesive or the like is exemplified. With regard to the inlet and outlet, through holes may be provided at the starting end side of the inlet-side flow path and the terminal end side of the outlet-side flow path of the substrate, respectively, to serve as the inlet and outlet, or holes may be provided at the corresponding positions on the film side. Microparticles embedded in a water-soluble fixing agent are fixed to the reaction area; the microparticles embedded in a water-soluble fixing agent may be fixed to the bottom surface of a depression that becomes the reaction area of ​​the substrate, or the microparticles embedded in a water-soluble fixing agent may be fixed to a part of the film that corresponds to the reaction area.

[0035] As a preferred embodiment of the microchip of the present invention, a substrate having a bonding surface provided with a depression that serves as a reaction section, a first groove that is connected to the depression and serves as an inlet-side flow path, and a second groove that is connected to the depression and serves as an outlet-side flow path; a film that is attached to the bonding surface of the base material by an adhesive and / or a pressure-sensitive adhesive that is applied to an area of ​​the bonding surface other than the depressions and grooves, thereby forming the flow path and the reaction portion; Microparticles carrying a reactive substance on their surfaces; and the microparticles are fixed to at least one of the recesses of the substrate and the regions of the film overlapping with the reaction sections in a state where they are embedded in a water-soluble immobilizing agent.

[0036] As a further preferred embodiment of the microchip of the present invention, A depression serving as a reaction section, a first groove connected to the depression and forming an inflow flow path, a second groove connected to the depression and forming an outflow flow path, and a connecting portion between the depression and the second groove. a substrate having a bonding surface provided with a wall portion that blocks the fine particles from entering the reaction portion; a film that is bonded to the joining surface of the base material by an adhesive and / or a pressure-sensitive adhesive that is applied to areas other than the groove, the recess, and the end surface of the wall portion at the joining surface with the base material, thereby forming the flow path and the reaction portion; Microparticles carrying a reactive substance on their surfaces; and the microparticles are fixed to at least one of the recesses of the substrate and the regions of the film overlapping with the reaction sections in a state where they are embedded in a water-soluble immobilizing agent. Here, the height of the gap between the end face of the wall portion and the film covering the end face of the wall portion is preferably a height that allows the liquid sample to pass through but does not allow the fine particles to pass through.

[0037] The microchip for liquid sample analysis having the above-mentioned wall portion and the method for manufacturing the same of the present invention will be described below with reference to the drawings. However, the following is merely an example, and the microchip of the present invention is not limited to the following embodiment.

[0038] 1 to 3 are conceptual diagrams showing examples of the manufacturing process of microchip 100. Fig. 1 is a diagram showing substrate 110 of microchip 100 before adhesive is applied. Fig. 2 is a diagram showing substrate 110 of microchip 100 after adhesive has been applied. Fig. 3 is a diagram showing the completed microchip 100 in which film 120 is bonded to substrate 110.

[0039] <Base material> 1 shows a plan view of a substrate 110 having a surface on which a groove (groove 111a) forming an inlet flow path 111a of a microchip 100, a groove (groove 111b) forming an outlet flow path 111b, and a depression (depression 115) forming a reaction section 115 are carved. The surface on which these grooves and depressions are carved is the surface to be bonded to a film 120, and is also referred to as a bonding surface 116.

[0040] A through hole serving as inlet 112 for the liquid sample is provided at the start side of groove 111a, and a through hole serving as outlet 113 (outlet) is provided at the end side of groove 111b. A depression serving as reaction section 115 is provided between groove 111a and groove 111b, i.e., in a portion between the through hole serving as inlet 112 and the through hole serving as outlet 113, and a wall section 114 for blocking particles is provided at the junction between the depression and the downstream side flow channel. The surface of wall section 114 facing film 120 to be bonded is also referred to as end surface 114a.

[0041] The shapes of the channels 111a and 111b are not limited and may be linear or curved. The channel 111a may have a branch. In that case, there may be two or more inlets 112. For example, two inlets 112 may be provided, and the liquid sample is allowed to flow from the first inlet into the first channel, and the reaction substrate liquid is allowed to flow from the second inlet into the second channel. The reaction section 115 may be provided at or beyond the junction of the first channel and the second channel, the wall section 114 may be provided at the junction of the reaction section 115 and the outlet channel 111b, and the outlet 113 may be provided at the end of the downstream channel.

[0042] The inlet 112 and the outlet 113 may be provided on either the substrate 110 or the film 120. For example, a groove serving as a flow path may be provided on the substrate 110, and a film 120 having through-holes at positions overlapping both ends of the groove (positions corresponding to the inlet and the outlet) may be prepared and attached to the substrate 110. One of the through-holes serving as the inlet 112 and the outlet 113 may be provided in the substrate 110, and the other in the film 120.

[0043] The cross-sectional shape of the groove serving as the flow path may be any shape, such as a concave shape, a U shape, or a V shape. The depth of the groove serving as the flow path is preferably 10 to 500 μm, and the width is preferably 10 μm to 3 mm. The length of the flow path (from the inlet to the outlet, including the reaction section) is, for example, 3 mm to 5 cm. The width of the groove may be constant or may vary. The depth of the groove may be constant or may vary.

[0044] Wall 114 is provided to block microparticles 117 in reaction section 115. On the other hand, the liquid sample passes through a gap between end surface 114a of wall 114 and film 120 covering the flow path.

[0045] The height of the wall 114 is set so that the liquid sample can pass through the gap between the end face 114a of the wall 114 and the film 120 covering the flow path. In other words, the height of the gap between the wall 114 and the film 120 is set so that the liquid sample can pass through but the fine particles 117 cannot. The wall 114 only needs to be able to block the fine particles 117, and may be formed lower than the joining surface 116. In other words, the height of the wall 114 is set so that the fine particles 117 may come into contact with the film 120 and the wall It is sufficient if the height does not pass through the gap between 114 and film 120.

[0046] Furthermore, in the case where the film 120 is deformable so as to widen the gap when the liquid sample passes through the gap between the end face 114a of the wall 114 and the film 120, the wall 114 may be made to have approximately the same height as the joining surface 116. However, the film 120 is deformable to an extent that the fine particles 117 do not enter the gap between the wall 114 and the film 120.

[0047] The thickness of wall 114 (the length in the longitudinal direction of the flow path) may be such that the liquid sample can pass through the gap between end face 114a of wall 114 and film 120. The wall surface of wall 114 on the side that blocks microparticles 117 may have a recess.

[0048] The size of the through-hole serving as the inlet 112 may be any size that allows a liquid sample such as blood to be injected using a microsyringe or the like. The size of the through-hole serving as the inlet 112 may be, for example, 0.2 to 3 mm in diameter. The size of the through-hole serving as the outlet 113 is not particularly limited as long as it functions as an outlet for the liquid sample. The size of the through-hole serving as the outlet 113 may be, for example, 0.2 to 2 mm in diameter.

[0049] <Film> The material of the film 120 is preferably a transparent plastic, and more preferably, for example, polyethylene terephthalate (PET) resin, cycloolefin polymer (COP) resin, cycloolefin copolymer (COC) resin, polystyrene (PS) resin, polycarbonate (PC) resin, or polymethyl methacrylate (PMMA) resin. The thickness of the film 120 is preferably, for example, 50 to 200 μm, and more preferably 100 to 200 μm.

[0050] The microparticles 117 are fixed in a state of being embedded in a water-soluble fixing agent at the positions of the film 120 corresponding to the reaction areas 115. A microparticle dispersion liquid in which the microparticles are dispersed in a water-soluble fixing agent solution having a water-soluble fixing agent concentration of 0.5 to 5.0 vol % is applied to the positions of the film 120 corresponding to the reaction areas 115. By spotting the above onto the substrate and drying it, the microparticles can be fixed in a state where they are embedded in the water-soluble fixing agent.

[0051] <Adhesive and / or pressure sensitive adhesive application process> An adhesive is used to attach the film 120 onto the substrate 110. Examples of the adhesive include (meth)acrylic resin adhesives, natural rubber adhesives, urethane resin adhesives, ethylene-vinyl acetate resin emulsion adhesives, ethylene-vinyl acetate resin adhesives, epoxy resin adhesives, vinyl chloride resin solvent adhesives, chloroprene rubber adhesives, cyanoacrylate adhesives, silicone adhesives, styrene-butadiene rubber solvent adhesives, nitrile rubber adhesives, nitrocellulose adhesives, phenolic resin adhesives, modified silicone adhesives, polyester adhesives, polyamide adhesives, polyimide adhesives, olefin resin adhesives, vinyl acetate resin emulsion adhesives, polystyrene resin solvent adhesives, polyvinyl alcohol adhesives, polyvinylpyrrolidone resin adhesives, polyvinyl butyral adhesives, polybenzimidazole adhesives, polymethacrylate resin solvent adhesives, melamine resin adhesives, urea resin adhesives, and resorcinol adhesives. The adhesives can be used alone or in combination of two or more.

[0052] Furthermore, a pressure-sensitive adhesive, which is a type of adhesive, may be used to attach film 120 onto substrate 110. Examples of pressure-sensitive adhesives include rubber-based pressure-sensitive adhesives, (meth)acrylic-based pressure-sensitive adhesives, silicone-based pressure-sensitive adhesives, urethane-based pressure-sensitive adhesives, vinyl alkyl ether-based pressure-sensitive adhesives, polyvinyl alcohol-based pressure-sensitive adhesives, polyvinyl pyrrolidone-based pressure-sensitive adhesives, polyacrylamide-based pressure-sensitive adhesives, and cellulose-based pressure-sensitive adhesives. Such pressure-sensitive adhesives may be used alone or in combination of two or more types.

[0053] The adhesive or pressure-sensitive adhesive is preferably a photocurable type (which may be either radically reactive or cationic polymerizable), and more preferably a UV-curable type. In the case of a UV-curable adhesive (including a UV-curable pressure-sensitive adhesive), the curing reaction can be started quickly by irradiating UV after the coating process, and the adhesive can be bonded. As the UV-curable adhesive, for example, an acrylic UV-curable adhesive such as UVX-8204 (manufactured by Denka Co., Ltd.), UVX-8400 (Denka Co., Ltd.), SX-UV100A (manufactured by Cemedine Co., Ltd.), SX-UV200 (Cemedine Co., Ltd.), BBX-UV300 (Cemedine Co., Ltd.), U-1340 (Chemitech Co., Ltd.), U-1455B (Chemitech Co., Ltd.), U-1558B (Chemitech Co., Ltd.), Aronix UV-3000 (Toagosei Co., Ltd.), TB3094 (Threebond Co., Ltd.), and Hitaloid 7975D (Hitachi Chemical Co., Ltd.) are more preferable. The UV-curable adhesive is preferably an acrylic UV-curable adhesive such as UV-3630ID80 (Mitsubishi Chemical Corporation), UX-3204 (Nippon Kayaku Co., Ltd.), or Finetack RX-104 (DIC Corporation). Acrylic UV-curable adhesives and adhesives exhibit good adhesion to a wide range of plastic materials and can rapidly develop strength after UV irradiation. The viscosity of the adhesive (including the adhesive) used to bond the film 120 onto the substrate 110 is preferably, for example, 2,000 to 31,000 mPa·s.

[0054] 2, a process of preparing substrate 110 and applying adhesive 117 to bonding surface 116 by screen printing will be described. When film 120 is attached to substrate 110 with a pressure-sensitive adhesive, which is a type of adhesive 117, the pressure-sensitive adhesive may be applied to substrate 110 in the same manner as adhesive 117. FIG. 2 is a diagram showing substrate 110 of microchip 100 after the adhesive has been applied.

[0055] The following description will be given using an adhesive as an example, but the same applies when a pressure-sensitive adhesive is used instead of an adhesive. Therefore, the description of "adhesive" can be read as "adhesive and / or pressure-sensitive adhesive."

[0056] The adhesive 117 is applied to an area provided on the joining surface 116 of the base material 110 other than the grooves 111a and 111b, the depressions 115, and the end surface 114a of the wall portion 114 (hereinafter also referred to as a predetermined application area).

[0057] In order to apply the adhesive 117 more accurately to the predetermined application area, it is preferable to apply the adhesive 117 by a printing technique, and particularly preferable to use screen printing. By using screen printing, even if the adhesive 117 is filled in the screen printing plate in the area corresponding to the entire surface of the substrate 110, the adhesive 117 is transferred to the predetermined application area that contacts the screen printing plate, but the adhesive 117 is not transferred to the grooves 111a, 111b, and depressions 115 that do not contact the screen printing plate. Furthermore, by providing a mask portion having the same shape as the end face 114a on the screen printing plate and printing in alignment with the end face 114a provided on the joining surface 116 of the substrate 110, the adhesive 117 is transferred to the predetermined area not covered by the mask portion of the screen printing plate, but the adhesive 117 is not applied to the end face 114a. Therefore, the adhesive 117 can be applied satisfactorily to the predetermined application area.

[0058] The thickness of the adhesive 117 applied to the substrate 110 is preferably 5 to 15 μm. To control the thickness of the adhesive 117, the number of meshes per inch of the screen is preferably, for example, 500 to 730. The opening ratio of the mesh is preferably, for example, 39 to 47%. The thickness of the mesh is preferably, for example, 15 to 28 μm. As a result, the thickness of the applied adhesive 117 is preferably 5 to 15 μm.

[0059] Other methods for applying adhesive 117 to substrate 110 include inkjet printing and gravure printing. It is possible to precisely apply the adhesive 117 to a predetermined application area by using a printer, a dispenser, or the like.

[0060] The adhesive 117 may be applied after subjecting the bonding surface 116 of the substrate 110 to a hydrophilic treatment. The hydrophilic treatment is preferably a plasma treatment, a corona treatment, or an excimer treatment. By subjecting the substrate 110 to a hydrophilic treatment so that the substrate 110 does not repel the adhesive 117 and the adhesive 117 spreads on the substrate 110 and does not flow into the grooves 111a, the substrate 110 and the film 120 can be satisfactorily bonded to each other.

[0061] In film 120, microparticles 117 are embedded with a water-soluble fixing agent in a region that overlaps with a reaction section on the substrate 110 side when film 120 and substrate 110 are laminated, and this portion forms a reaction section containing microparticles 117 when film 120 and substrate 110 are laminated. Microparticles 117 may be embedded with a water-soluble fixing agent in a region that becomes a reaction field on the substrate 110 side. The particles 117 may have any size as long as they do not pass through the gap between the end surface 114a of the wall portion 114 and the film 120, and may be, for example, about 10 μm.

[0062] The particles 117 are supported on their surfaces as reactive substances. The reactive substance may be any substance that reacts with the target (detection target) component in the liquid sample, and may be appropriately selected depending on the type of target substance. Reactions of reactive substances include biological reactions and chemical reactions, and biological reactions also include binding reactions. Reactive substances include proteins (including peptides), sugars, nucleic acids, low molecular weight compounds, and the like. Examples include substances such as antibodies that specifically bind to the target substance, and enzyme proteins that use the target substance as a substrate. In addition, when the target substance is a nucleic acid, a nucleic acid probe or a polymerase (nucleic acid amplification enzyme) that amplifies nucleic acid may be used.

[0063] <Lamination process> Fig. 3 is a diagram of a completed microchip in which film 120 is bonded to substrate 110. Fig. 3 shows a plan view of microchip 100 obtained by bonding film 120 to bonding surface 116 of substrate 110, in which grooves 111a, grooves 111b, and depressions 115 are dug. Channel 111 formed inside microchip 100 is indicated by a dashed line.

[0064] By laminating and bonding film 120 onto substrate 110, grooves 111a, grooves 111b, depressions 115, and upper portions of end faces 114a of wall portions 114 are covered with film 120, and gaps are formed between channels 111a, 111b, reaction portions 115, and end faces 114a through which a liquid sample passes, and film 120. In this manner, by applying adhesive 117 to a predetermined application area by screen printing, and laminating and bonding film 120 onto substrate 110, bonding of substrate 110 and film 120 and formation of a damming structure can be achieved in the same process.

[0065] Moreover, the through-holes of the substrate 110 are sealed on the bonding surface 116 side by laminating the film 120, and only the surface opposite to the bonding surface 116 becomes an opening. As a result, the through-holes of the substrate 110 function as the inlet 112 and the outlet 113. That is, the liquid sample introduced from the inlet 112 passes through the inlet-side flow path and reaches the reaction section, at which time the adhering fine particles are eluted from the film and are contained in the reaction section 115. Then, in a state in which the fine particles 117 are blocked by the wall section 114, the reactive substance supported by the fine particles reacts with the measurement target substance in the liquid sample, and is then discharged from the outlet 113. The measurement target substance in the liquid sample can be measured by observing or detecting the reaction in the reaction section, or the measurement target substance or its reaction product in the sample discharged from the outlet 113 can be measured. Examples of the reaction include, but are not limited to, a color reaction, a luminescence reaction, an amplification reaction, and an agglutination reaction.

[0066] 4 to 6, the behavior of microparticles 117 in the reaction section when a liquid sample is flowed into the flow path of microchip 100 will be described. Fig. 4 is a diagram showing a part of the AA cross section of microchip 100 shown in Fig. 3. Film 120 is attached to substrate 110, and flow path 111a on the inlet 112 side, reaction section 115, and flow path 111b on the outlet 113 side are communicated with each other through a gap between end face 114a of wall portion 114 and film 120.

[0067] Microparticles 117 embedded in a water-soluble fixing agent are fixed to the region of film 120 forming the upper surface of the flow channel that overlaps with the reaction section before laminating film 120 and substrate 110. Note that microparticles 117 may be fixed to depressions 115 of substrate 110 in a state where they are embedded in a water-soluble fixing agent.

[0068] 5 is a diagram showing a state in which a liquid sample is flowed into a flow channel. The liquid sample flows from inlet 112 into inlet-side flow channel 111a and reaches reaction section 115. When the liquid sample comes into contact with microparticles 117 fixed to film 120 just before wall section 114, microparticles 117 are eluted from the film and dispersed in reaction section 115. Then, the measurement target substance in the liquid sample reacts with the reactive substance supported on the surface of microparticles 117. Thereafter, by passing more liquid, the liquid sample after the reaction moves to outlet 113 through the gap between end surface 114a and film 120.

[0069] 6 is a diagram showing how the microparticles 117 are blocked by the wall portion 114. When a liquid sample, a cleaning solution, or the like is introduced into the inlet side flow channel 111a from the inlet 112 using a microsyringe or the like and pressurized, the liquid sample proceeds from the reaction section beyond the wall portion 114, but the microparticles 117 are blocked by the wall surface on the inlet 112 side of the wall portion 114. This prevents the microparticles from flowing out, and allows the reaction to occur efficiently.

[0070] 13, the width of the wall 114 (in the direction perpendicular to the longitudinal direction of the flow channel and the depth direction of the flow channel) and the width of the outlet side flow channel 111b can be made wider, for example, to be approximately the same as the width of the reaction section. If the wall is extremely narrower than the reaction section, the cross-sectional area of ​​the flow path decreases suddenly at the wall, so the flow rate on the wall becomes the rate-limiting factor, and the flow rate suddenly decreases after the reaction section is filled, but this can be prevented by widening the wall and widening the flow path downstream of the wall. This embodiment is useful when the reaction between the target substance and the reactive substance in the reaction section is sufficiently fast.

[0071] The test device of the present invention may be provided as a package sealed with a packaging material together with a desiccant, and may be opened when used. This allows the concentration of the water-soluble immobilizing agent to be kept high and the variation in the concentration of the water-soluble immobilizing agent to be suppressed. Examples of the desiccant include silica gel.

[0072] The present invention will be described in detail below with reference to examples, although the present invention is not limited to the embodiments of the examples. EXAMPLES

[0073] <Coating magnetic particles and creating microchips> A substrate 1 (COP injection molding) (size 55.4×20.2 mm, thickness 3.0 mm) shown in FIG. 7 was prepared. In the substrate 1, the length of the flow path 2 was 47.4 mm, the depth was 500 μm, and the width of the inlet was 500 μm. It also had a reaction section 3 (diameter 2.0 mm), a liquid injection section 4 (diameter 2.0 mm), and a liquid waste section 5 (diameter 2.0 mm). The film 6 shown in FIG. 8 was prepared as ZF14-100 (made of COP resin) (size 55.4 × 20.2 mm, thickness 100 μm).

[0074] The magnetic particles were Dynabeads M-270 Carboxylic acid (Veritas) with an average particle size of 2.8 μm. The magnetic particles were replaced with a 2.5 vol% glycerin aqueous solution so that the magnetic particles were 5 wt% and used in a dispersed state. 1 μL of the magnetic particle dispersion liquid was dropped onto the magnetic particle coating portion 7 of the film 6 and dried overnight at room temperature and normal pressure to form the magnetic particles. The particles were fixed onto film 6.

[0075] An adhesive was used to bond the substrate 1 and the film 6. The adhesive was UVX-8204, a solvent-free radical-reactive acrylic UV-curable adhesive. The adhesive was applied by screen printing to the surface of the substrate 1 on which the flow path 2 was formed. The screen used had a mesh number of 640, an opening rate of 39%, and the adhesive was applied to a thickness of approximately 7 μm.

[0076] As shown in Figure 9, the substrate 1 was laminated while aligning the reaction area 3 and the magnetic particle coating area 7 of the film 6 so that they overlapped. A UV-LED light source was used to irradiate ultraviolet light with a wavelength of 365 nm for 10-20 seconds to initiate the curing reaction of the adhesive, and the film was then laminated on the substrate 1 as shown in Figure 10. The reaction section 3 is joined to the magnetic film 6 to prepare a microchip including the magnetic particle coating section 7 in the reaction section 3. Ta.

[0077] <Evaluation of microchip dispersibility> 5 μL of saline colored with food coloring was injected into the injection part 4 of the prepared microchip. The liquid dispersion of the magnetic particles was confirmed when the magnetic particles reached the reaction section 3. As shown in FIG. A comparison was made between the presence or absence of glycerin when drying the particles onto film 6. When glycerin is not added, the film does not disperse in the saline solution even when it comes into contact with the saline solution. On the other hand, when glycerin was added, the magnetic particles maintained their wettability even after drying, and were confirmed to disperse instantly when they came into contact with saline. These results demonstrate that the liquid dispersibility of magnetic particles is improved by drying and fixing them together with glycerin.

[0078] <Evaluation of water contact angle> The effect of changing the water contact angle of the substrate on the liquid dispersion of magnetic particles was confirmed. Film 6 After surface treatment, 1 μL of 5 wt% magnetic particles replaced with 2.5 vol% glycerin aqueous solution was applied. After drying overnight at room temperature and normal pressure, physiological saline was poured over the sample to evaluate its liquid dispersibility. The surface treatment method of the film 6 was selected as a hydrophilic treatment by corona treatment. Immediately after the treatment, the surface can be treated with hydrophilizing agents such as SPRA-202 and Lipidure-NH01. We also investigated how to reduce the contact angle. The surface coating was performed.

[0079] Magnetic particles were mixed with glycerin to form film 6 (contact angle 94°) and corona-treated film 7. Film 6 (contact angle 39°) dried had excellent liquid dispersibility, and almost no magnetic particles were observed adsorbed onto the surface of Film 6. On the other hand, when Film 6 was treated with SPRA-202 (contact angle 10°), Lipidure-NH01 (contact angle 21°), or Lipidure-CM5206 (contact angle 124°), From the above results, it was found that the magnetic particles were adsorbed on the film surface, and the liquid dispersion property was deteriorated. It was confirmed that the material could be dispersed in liquid on a substrate of this degree.

[0080] <Evaluation of glycerin concentration> When drying a glycerin solution, glycerin (boiling point 290°) hardly evaporates, Since only water evaporates, the glycerin concentration gradually increases. Meanwhile, glycerin is hygroscopic and absorbs moisture from the air, so the concentration of the glycerin solution gradually reaches equilibrium. Since the final concentration of the glycerin solution is greatly affected by the temperature and moisture content of the environment, we confirmed to what extent the concentration of the glycerin solution would increase under the conditions for actually fabricating the microchip. First, 200 μL of a 50 vol% glycerin aqueous solution was applied onto film 6, and the film was left at room temperature (temperature 23.4°C, phase The weight change was measured over time while drying at a relative humidity of 55%. The concentration of the glycerin aqueous solution reached 70 vol% in 31.5 hours, and no change in concentration was observed thereafter.

[0081] <Evaluation of antibody activity on magnetic particle surface> We verified whether it is possible to maintain the antigen binding ability of the antibody by storing the antibody-modified magnetic particles in glycerin. The antigen binding ability of the antibody was measured by sandwich ELISA. The magnetic particles used were Dynabeads M-270 Carboxyl acid (Veritas Corporation), and For sandwich ELISA, a commercially available IL-6 detection ELISA kit (Human IL-6 DuoSet ELISA) (R&D Systems) and reaction reagent set (DuoSet ELISA Ancillary Reagent Kit 2) (R&D Systems) were used.

[0082] First, the magnetic particles were modified with the IL-6 antibody. After thoroughly stirring the magnetic particles with a vortex mixer, 240 μL was placed in a 2 mL microtube and allowed to stand on a magnetic stand (e.g., Magnetic Stand (6 tubes) (Takara Bio Inc.)) for at least 30 seconds. The supernatant was removed without disturbing the particles. Then, 200 μL of MES buffer (25 mM MES, pH 6.0) was added, and the procedure of removing the supernatant was repeated twice to completely soak the magnetic particles in the MES buffer. Before the magnetic particles were dried, 50 μL of MES buffer in which 50 mg / mL 1-ethyl-3-[3-(dimethylamino)propyl]carbodiimide hydrochloride was dissolved and 50 mg / mL N-hydroxybutyric acid were added. 50 μL of MES buffer in which cis-succinimide was dissolved was added, and the mixture was incubated at room temperature for 30 minutes while mixing by inversion. After the reaction, the supernatant was removed, and the mixture was washed twice with 200 μL of MES buffer. Then, 150 μL of MES buffer in which 24 μg / mL IL-6 antibody was dissolved was added, and the mixture was incubated at room temperature for 2 hours while mixing by inversion. Finally, the supernatant was removed, and the mixture was washed twice with 200 μL of MES buffer. After repeated washing, the mixture was dispersed in 490 μL of MES buffer.

[0083] The IL-6 antibody modified magnetic particles were dispensed into 96-well plates for ELISA at 40 μL each, and the supernatant was removed using a magnet. 7.3 μL of glycerin solution with a concentration of 0 to 2.5 vol% was added thereto. The magnetic particles dried on the 96-well plate were suspended in the washing buffer of the ELISA kit and collected in a 2 mL microtube, and the antigen binding ability of the IL-6 antibody modified on the surface of the magnetic particles was evaluated by sandwich ELISA.

[0084] The specific experimental procedure for the sandwich ELISA method is as follows. After washing the magnetic particles three times with 200 μL of washing buffer, add 200 μL of blocking solution and invert the The mixture was allowed to react at room temperature for 1 hour while mixing. After washing the magnetic particles three times with 200 μL of washing buffer, 250 pg / mL IL-6 antibody diluted with ultrapure water was added. 100 μL of the original solution was added, and the mixture was allowed to react at room temperature for 2 hours while being mixed by inversion. After washing the magnetic particles three times with 200 μL of washing buffer, 100 μL of 50 ng / mL biotin-modified secondary antibody solution diluted with blocking solution was added, and the mixture was allowed to react at room temperature for 2 hours while being mixed by inversion. After washing the magnetic particles three times with 200 μL of washing buffer, 100 μL of HRP-labeled streptavidin diluted 40-fold with ultrapure water was added and reacted at room temperature for 30 minutes while mixing by inversion. After washing the magnetic particles three times with 200 μL of washing buffer, 100 μL of TMB color developing solution was added and reacted at room temperature for 30 minutes while mixing by inversion. The reaction was stopped by adding 50 μL of stop solution and mixing with a vortex mixer. 100 μL of the supernatant was transferred to a 96-well plate and the absorbance at a wavelength of 450 nm was measured.

[0085] The activity of the antibodies on the surface of the magnetic microparticles was evaluated by the sandwich ELISA method, and the results are shown in Table 1. It was confirmed that the antibody activity was maintained when glycerin was added when the magnetic microparticles were dried. It was also confirmed that the antibody activity was maintained more effectively as the amount of glycerin added increased.

[0086] [Table 1] EXAMPLES

[0087] <Confirmation of the effect of high-concentration glycerin on proteins> In general, when storing proteins in a frozen state, an antifreeze solution containing glycerin at a concentration of 20 to 50 vol% is used. On the other hand, as shown in Example 1, a glycerin aqueous solution is used together with a silica gel desiccant. It was found that when the protein was dried, the glycerin concentration rose to 95 vol%. We then confirmed whether proteins could be stored stably even in such a high concentration of glycerin. The protein selected for use was thrombin, which is known to be a low-stability enzyme. In addition, a method was examined for evaluating thrombin activity using S-2238 reagent (Sekisui Medical Co., Ltd.), a chromogenic synthetic substrate. When the peptide bond of S-2238 reagent is cleaved by thrombin, 4-nitroaniline is released, which can be detected at 405 nm using a spectrophotometer. Therefore, The change in absorbance at 405 nm was measured over time while reacting thrombin with the S-2238 reagent. Thus, thrombin activity can be quantified.

[0088] Thrombin was actually stored in a 0-95 vol% glycerin aqueous solution, and then activity was evaluated. First, as shown in Table 2, thrombin solution (Mochida Pharmaceutical Co., Ltd.) (1000 units / mL), glycerin, and TBS buffer (50 mM Tris, pH 7.5) were added to a 5 mL vial, and the mixture was thoroughly mixed by inversion. After storing at room temperature for 7 days, 4 mL of TBS buffer was added for dilution. In addition, S-2238 reagent was dissolved in TBS buffer to 5 mM in a 2 mL microtube. 90 μL of S-2238 reagent solution and 10 μL of diluted thrombin sample were added to a 96-well plate, and the absorbance at a wavelength of 405 nm was measured while stirring in a plate reader heated to 37°C.

[0089] [Table 2]

[0090] The results of evaluating the thrombin activity after storage at each glycerin concentration are shown in Figure 12. When no glycerin was added, the thrombin activity was significantly reduced, but when glycerin was added at 50 to 95 vol% the activity was significantly reduced. By adding glycerin 95 vol%, thrombin activity was maintained. Even under high concentration conditions, the activity maintenance effect was equivalent to that of 50 vol% glycerin, and it was confirmed that there were no problems. [Explanation of symbols]

[0091] 100: Microchip, 110: Base material, 111a, 111b: Flow channel (groove) , 112 ··· inlet, 113 ··· outlet, 114 ··· wall portion, 115 ··· reaction portion (recess), 116 ··· joint surface, 117 ··· fine particle, 120 ··· film

[0092] 1...Substrate (COP injection molding), 2...Flow path (groove), 3...Reaction part (recess), 4... 1. Inlet (liquid inlet), 2. Outlet (liquid waste), 3. Film, 4. Fine particle coating Department

Claims

1. The present invention relates to an inspection device having a reaction section containing microparticles carrying a reactive substance on their surface, and for analyzing a liquid sample by adding or flowing a liquid into the reaction section to react the reactive substance with a substance to be measured in the liquid sample, characterized in that the microparticles are fixed to the reaction section in a state embedded in a water-soluble fixing agent.

2. The inspection device according to claim 1, wherein the microparticles have an average particle size of 50 nm to 5 μm.

3. The test device according to claim 1 , wherein the reactive substance is a protein, a sugar chain, or a nucleic acid.

4. The testing device of claim 1 , wherein the microparticles are magnetic microparticles.

5. 10. The test device of claim 1 which is a microchip.

6. 6. The testing device according to claim 5, wherein the microchip has an inlet side flow path connected to the reaction section and for causing a liquid to flow into the reaction section, and an outlet side flow path connected to the reaction section and for causing a liquid to flow out of the reaction section.

7. The testing device according to claim 6 , further comprising a wall portion for blocking the particles at a connection portion between the reaction portion and the outlet side flow channel.

8. a substrate having a bonding surface on which a first groove forming the inlet-side flow path, a second groove forming the outlet-side flow path, and a recess disposed between the first groove and the second groove and forming the reaction portion are provided; a film that is bonded to the bonding surface of the base material by an adhesive and / or a pressure-sensitive adhesive that is applied to an area of ​​the bonding surface other than the first and second grooves and the depressions, thereby forming the flow path and the reaction portion; Microparticles carrying the reactive substance on their surfaces; 7. The testing device according to claim 6, wherein the microparticles are fixed to at least one of the depressions of the substrate and the areas of the film overlapping with the reaction areas in a state where they are embedded in a water-soluble immobilizing agent.

9. a substrate having a joining surface on which a first groove forming the inlet-side flow path, a second groove forming the outlet-side flow path, a recess disposed between the first groove and the second groove and forming the reaction section, and a wall section provided at a connection between the reaction section and the outlet-side flow path and blocking the fine particles; a film that is bonded to the bonding surface of the base material by an adhesive and / or a pressure-sensitive adhesive that is applied to an area of ​​the bonding surface other than the first and second grooves, the recesses, and the end faces of the wall portion, thereby forming the flow path and the reaction portion; Microparticles carrying the reactive substance on their surfaces; The testing device according to claim 7 , wherein the microparticles are fixed to at least one of the depressions of the substrate and the areas of the film overlapping with the reaction areas in a state where they are embedded in a water-soluble immobilizing agent.

10. The testing device according to claim 9 , wherein the height of a gap between the end surface of the wall portion and the film covering the end surface of the wall portion is such that the liquid sample can pass through but the fine particles cannot.

11. A step of preparing a substrate having an area to be a reaction portion; Microparticles carrying reactive substances on their surfaces are dispersed in a 0.5-5.0 vol% aqueous solution of a water-soluble immobilizing agent. preparing a microparticle dispersion; adding the microparticle dispersion to a region of the substrate that will become the reaction portion; and drying the microparticle dispersion; The present invention relates to a method for producing an inspection device having a reaction portion in which fine particles carrying a reactive substance on the surface are fixed in a state embedded in a water-soluble fixing agent, the method comprising the steps of:

12. The test device according to claim 10, wherein in a substrate having an area serving as the reaction portion, the contact angle of the surface of the area is from 30° to 100°.

13. A package in which a desiccant and the testing device according to claim 9 are sealed in a packaging material.

Citation Information

Patent Citations

  • Surface-treated powder

    JP2000219820A

  • Method for manufacturing easily dispersible organic pigment powder

    JP2003213151A

  • Method for production of insoluble carrier particle, insoluble carrier particle, measurement reagent, sample analysis tool, and immunology turbidimetric method

    WO2009136541A1