Optical fiber fusion device and optical fiber fusion method

The optical fiber fusion device uses a 2.7 μm to 3.0 μm laser wavelength for precise temperature control, addressing the challenges of plastic optical fiber fusion in existing devices by enabling easy and contamination-free fusion in an air atmosphere.

JP2024142845APending Publication Date: 2024-10-11AKITA PREFECTURAL UNIVERSITY +1
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
JP2023055199
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-30
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

Existing plastic optical fiber fusion devices require nonflammable gas-filled boxes and struggle with fine temperature control due to the low melting point of plastic, making the fusion process challenging.

Method used

An optical fiber fusion device and method using a laser irradiation unit that emits a wavelength of 2.7 μm to 3.0 μm to fuse plastic optical fibers, allowing precise temperature control and non-contact welding without the need for nonflammable gas, using a laser beam to absorb by the plastic optical fibers.

Benefits of technology

Enables easy fusion of plastic optical fibers with precise temperature control, reducing contamination and process complexity while maintaining mechanical properties, and allowing fusion in an air atmosphere.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024142845000001_ABST
    Figure 2024142845000001_ABST
Patent Text Reader

Abstract

To provide an optical fiber fusion device and an optical fiber fusion method that easily fuse a plastic optical fiber.SOLUTION: An optical fiber fusion device 100 comprises a first holding unit 10A, a second holding unit 10B, and a laser irradiation unit 20. The first holding unit 10A holds a first optical fiber F1. The second holding unit 10B holds a second optical fiber F2, with a leading end of the first optical fiber F1 and a leading end of the second optical fiber F2 facing each other. The laser irradiation unit 20 irradiates the leading end of the first optical fiber F1 and the leading end of the second optical fiber F2 with a laser beam having a wavelength of 2.7 μm or more and 3.0 μm or less.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an optical fiber fusing apparatus and an optical fiber fusing method. [Background technology]

[0002] Optical fibers are used to transmit light. Among optical fibers, plastic optical fiber (POF) is characterized by excellent durability and relatively low cost. Its excellent durability allows it to be used in a variety of environments, making it suitable for transmitting information in local spaces such as inside a car. In addition, it is less expensive than quartz fiber, making it easy to introduce into existing environments, and it is expected to contribute to IoT (Internet of Things) technology as a useful optical transmission system. In order for POF to become more widespread, a method for repairing POF when it breaks is required.

[0003] Patent document 1 discloses a plastic optical fiber fusion device that encloses the connection portion of the POF and the discharge electrode portion in a box, fills it with non-flammable gas, discharges electricity inside the box, and uses the heat to melt the tip portion of the POF to fuse the POF. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2004-102202 A Summary of the Invention [Problem to be solved by the invention]

[0005] The plastic optical fiber fusion device disclosed in the cited document 1 requires a box filled with non-flammable gas, and has the problem that it is not easy to precisely control the temperature due to the low melting point of plastic. For this reason, there is a demand for an easy way to fuse POF.

[0006] SUMMARY OF THE PRESENT INVETION The present invention has been made to solve the above-mentioned problems, and an object of the present invention is to provide an optical fiber fusing device and an optical fiber fusing method that can easily fuse plastic optical fibers. [Means for solving the problem]

[0007] In order to achieve the object of the present invention, one aspect of the optical fiber fusion splicing apparatus according to the present invention comprises: a first holding portion that holds a first optical fiber; a second holding portion that holds the second optical fiber by facing a tip portion of the first optical fiber and a tip portion of the second optical fiber; a laser irradiation unit that irradiates a tip end of the first optical fiber and a tip end of the second optical fiber with a laser beam having a wavelength of 2.7 μm or more and 3.0 μm or less; The present invention is characterized by comprising:

[0008] In order to achieve the object of the present invention, one aspect of a method for fusing optical fibers according to the present invention comprises the steps of: a tip end of a first optical fiber and a tip end of a second optical fiber are held facing each other, and a laser light having a wavelength of 2.7 μm or more and 3.0 μm or less is irradiated onto the tip end of the first optical fiber and the tip end of the second optical fiber; It is characterized by: Effect of the Invention

[0009] According to the present invention, it is possible to provide an optical fiber fusing device and an optical fiber fusing method that can easily fuse a plastic optical fiber. [Brief description of the drawings]

[0010] [Figure 1] FIG. 1A is a top view showing an optical fiber fusing device according to an embodiment, and FIG. 1B is a side view showing an optical fiber fusing device according to an embodiment. [Diagram 2] FIG. 2 is a cross-sectional view showing a laser irradiation unit according to the embodiment. [Diagram 3]3 is a flowchart showing a method for fusing optical fibers according to an embodiment. [Figure 4] 1A to 1C are diagrams illustrating a method for fusing optical fibers according to an embodiment. [Diagram 5] 1A to 1C are diagrams illustrating a method for fusing optical fibers according to an embodiment. [Figure 6] 1A to 1C are diagrams illustrating a method for fusing optical fibers according to an embodiment. [Figure 7] 4A and 4B are diagrams showing a fusion state of the optical fiber according to the embodiment. [Figure 8] 4A and 4B are diagrams showing a fusion state of the optical fiber according to the embodiment. [Figure 9] 4A and 4B are diagrams showing a fusion state of the optical fiber according to the embodiment. [Figure 10] FIG. 13 is a diagram showing the relationship between the one-side push amount and the transmittance of the optical fiber according to the embodiment. [Figure 11] FIG. 13 is a diagram showing the relationship between the one-side push-in amount and the tensile strength and allowable bending radius of the optical fiber according to the embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS An optical fiber fusing apparatus and an optical fiber fusing method according to an embodiment of the present invention will now be described with reference to the drawings.

[0012] 1(A) and 1(B), the optical fiber fusion device 100 according to the present embodiment is a device for fusing a first optical fiber F1 and a second optical fiber F2, and includes a first holding unit 10A for holding the first optical fiber F1, a second holding unit 10B for holding the second optical fiber F2, a laser irradiation unit 20 for irradiating the tip of the first optical fiber F1 and the tip of the second optical fiber F2 with laser light, and observation units 30A and 30B for observing the tip of the first optical fiber and the tip of the second optical fiber. The first optical fiber F1 and the second optical fiber F2 include plastic optical fibers (POFs), and are optical fibers made of, for example, PMMA (Polymethyl Methacrylate).

[0013] For ease of understanding, a Cartesian coordinate system is set in which the extension direction of the first and second optical fibers F1, F2 is the x-direction, the irradiation direction of the laser light is the z-direction, and the direction perpendicular to the x-direction and z-direction is the y-direction, and will be referred to as appropriate.

[0014] The first holding unit 10A holds the first optical fiber F1 so as to extend in the x-direction, and includes a three-axis stage 11A capable of moving the first optical fiber F1 in the x-direction, y-direction, and z-direction.

[0015] The second holding unit 10B holds the second optical fiber F2 so that the tip of the first optical fiber faces the tip of the second optical fiber and extends it in the x-direction, and is provided with a three-axis stage 11B that can move the second optical fiber F2 in the x-direction, y-direction, and z-direction.

[0016] The laser irradiation unit 20 irradiates a laser beam having a wavelength of 2.7 μm or more and 3.0 μm or less. The wavelength of 2.7 μm or more and 3.0 μm or less is within the wavelength range absorbed by POF. The laser irradiation unit 20 preferably irradiates a laser beam having a wavelength of 2.8 μm. Specifically, as shown in FIG. 2, the laser irradiation unit 30 is a mid-infrared fiber laser including a laser medium 21 having a fiber shape, a resonator 22 arranged to sandwich the laser medium 21, an excitation light source 23 that supplies excitation light to the laser medium 21, and end caps 24A and 24B that protect the ends of the laser medium 21. When the first optical fiber F1 and the second optical fiber F2 are optical fibers made of PMMA, the laser irradiation unit 20 preferably irradiates a laser beam having a wavelength of 2.8 μm, which is within the wavelength range absorbed by PMMA.

[0017] The laser medium 21 amplifies light by absorbing the excitation light irradiated from the excitation light source 23 and causing stimulated emission. The laser medium 21 is, for example, Er:ZBLAN (ZrF 4 -BaF 2 -LaF 3 -AlF 3-NaF), which absorbs pump light and induces light emission, and a cladding 26 with a lower refractive index than the core 25. Er:ZBLAN is ZBLAN doped with erbium (Er), and oscillates laser light of 2.7 μm to 2.9 μm. The base material of the laser medium 21 can be HBLAN (HfF 4 -BaF 2 -YF 3 -AlF 3 -NaF) glass, ZBYA (ZrF 4 -BaF 2 -YF 3 -AlF 3 ) Glass containing ZrF 4 Glasses, AlF 3 -BaF 2 -YF 3 -CaF 2 , AlF 3 -BaF 2 -YF 3 -ThF 4 , AlF 3 -BaF 2 -SrF 2 -CaF 2 -MgF 2 -YF 3 Including AlF 3 Glasses, InF 3 -ZnF 2 -BaF 2 -SrF 2 -LaF 3 , InF 3 -BaF 2 -YF 3 , InF 3 -ZnF 2 -SrF 2 -BaF 2 Including InF 3 The fiber may be a fluoride glass such as Er:ZBLAN fiber or Er,Pr:ZBLAN fiber, as long as it is used in a fiber laser.

[0018] The resonator 22 includes a reflecting mirror 22A that reflects the stimulated emission light, and an output mirror 22B that can extract a part of the laser light to the outside. In this example, the reflecting mirror 22A is a high-reflection FBG (Fiber Bragg Grating) having a diffraction grating formed in an optical fiber, and reflects the stimulated emission light from the laser medium 21. The output mirror 22B is a low-reflection FBG having a diffraction grating formed in an optical fiber, and transmits a part of the light of the wavelength stimulated emission from the laser medium 21 and reflects the remainder.

[0019] The excitation light source 23 includes a semiconductor laser and is disposed to face the reflecting mirror 22A. The excitation light source 23 irradiates the laser medium 21 disposed in the resonator 22 with laser light as excitation light. The excitation light irradiated from the excitation light source 23 is collected by a lens 41 and supplied to the laser medium 21. For example, when Er:ZBLAN is used for the laser medium 21, the excitation light source 23 that irradiates a laser light of 976 nm is used. The lens 41 collects the light L irradiated from the excitation light source 23 on the core 24 of the laser medium 21. The lens 42 collimates or collects the light L irradiated from the laser medium 21.

[0020] As shown in FIG. 1(A) and FIG. 1(B), the observation units 30A and 30B include a camera or a microscope for observing the tip of the first optical fiber F1 and the tip of the second optical fiber F2. The observation unit 30A observes the tip of the first optical fiber and the tip of the second optical fiber in the z direction. The observation unit 30B observes the tip of the first optical fiber and the tip of the second optical fiber in the y direction. By operating the three-axis stage 11A of the first holding unit 10A and the three-axis stage 11B of the second holding unit 10B while observing using the observation units 30A and 30B, the tip of the first optical fiber and the tip of the second optical fiber can be aligned to the irradiation position of the laser light.

[0021] Next, an optical fiber fusion method for fusion-splicing optical fibers using the optical fiber fusion device 100 having the above-described configuration will be described.

[0022] As shown in FIG. 3, the optical fiber fusion method includes an optical fiber holding step (step S101), a preheating step (step S102), a fusion step (step S103), and a positioning step (step S104).

[0023] In the optical fiber holding step (step S101), the first holding unit 10A holds the first optical fiber F1 so as to extend in the x-direction, and the second holding unit 10B holds the second optical fiber F2 so as to extend in the x-direction. The three-axis stage 11A of the first holding unit 10A and the three-axis stage 11B of the second holding unit 10B are operated to align the tip of the first optical fiber F1 with the tip of the second optical fiber F2 as shown in Fig. 4, and align them with the irradiation position of the laser light. At this time, a gap is provided between the tip of the first optical fiber F1 and the tip of the second optical fiber F2.

[0024] Next, in the preheating step (step S102), as shown in Fig. 5, the laser irradiation unit 20 irradiates the tip of the first optical fiber and the tip of the second optical fiber with a first light amount of laser light having a wavelength of 2.7 µm or more and 3.0 µm or less. This preheats the tip of the first optical fiber F1 and the tip of the second optical fiber F2. Preheating makes it possible to process the end faces of the first and second optical fibers F1 and F2, and does not require pretreatment after fiber breakage.

[0025] Next, in the fusion step (step S103), as shown in FIG. 6, the laser irradiation unit 20 irradiates the tip of the first optical fiber F1 and the tip of the second optical fiber F2 with a laser light having a wavelength of 2.7 μm or more and 3.0 μm or less with a second light amount larger than the first light amount. When the tip of the first optical fiber F1 and the tip of the second optical fiber F2 start to melt, the first optical fiber F1 and the second optical fiber F2 are pressed against each other. Specifically, it is preferable to press the tip of the second optical fiber against the tip of the first optical fiber by a pressing amount of 0.1 mm or more and 1.0 mm or less. As a result, the tip of the first optical fiber F1 and the tip of the second optical fiber F2 are fused together.

[0026] In the positioning step (step S104), the observation units 30A and 30B check whether the tip of the first optical fiber F1 and the tip of the second optical fiber F2 have been fused without any axial misalignment. If the tip of the first optical fiber F1 and the tip of the second optical fiber F2 have been fused without any axial misalignment, the laser irradiation is stopped. This completes the fusion of the first optical fiber F1 and the second optical fiber F2. If there is an axial misalignment between the tip of the first optical fiber F1 and the tip of the second optical fiber F2, the positions are adjusted by operating the three-axis stage 11A of the first holding unit 10A and the three-axis stage 11B of the second holding unit 10B. When there is no axial misalignment, the laser irradiation is stopped. This completes the fusion of the first optical fiber F1 and the second optical fiber F2.

[0027] As described above, according to the optical fiber fusion device 100 and the optical fiber fusion method of the present embodiment, the first optical fiber F1 and the second optical fiber F2 can be easily fused together by irradiating the tip of the first optical fiber F1 and the tip of the second optical fiber F2 with laser light having a wavelength of 2.7 μm or more and 3.0 μm or less. By using laser light for fusion, it is easy to finely control the temperature for the low melting point of plastic. In addition, by using laser light, fusion can be performed without contact and with a minimum heating area, contamination during fusion can be reduced, the process is simple, and no consumables are required. In addition, fusion can be performed in an air atmosphere, and no non-flammable gas is required. In addition, as shown in the examples described later, the mechanical properties are the same as before the breakage, and the practical performance is satisfied.

[0028] (Modification) In the above embodiment, an example in which the laser irradiation unit 20 includes a fiber laser has been described. However, the laser irradiation unit 20 may be any laser that irradiates laser light having a wavelength of 2.7 μm or more and 3.0 μm or less, and may be any laser such as an Er:YAG laser or an Er:YAG laser. 2 O 3 The laser irradiation unit 20 may be equipped with other types of lasers such as various bulk solid-state lasers, microchip lasers, or disk lasers that use erbium as an active element and oscillate in the wavelength range, or may be equipped with chalcogenide solid-state lasers that oscillate in the wavelength range and use a transition metal as an active element, such as Cr:ZnSe or Cr:ZnS laser. The laser irradiation unit 20 may also be equipped with a quantum cascade laser or an interband cascade laser. The laser irradiation unit 20 may oscillate the laser light in a continuous wave form or may irradiate a pulsed laser. By using a wavelength-tunable laser light source such as a quantum cascade laser or an interband cascade laser, it is possible to irradiate a laser with an optimal wavelength for each target material.

[0029] In the above embodiment, an example has been described in which the first and second holding units 10A and 10B are equipped with the three-axis stages 11A and 11B, but at least either the first holding unit 10A or the second holding unit 10B may be capable of moving the first optical fiber F1 or the second optical fiber F2 in the x direction. For example, either the first holding unit 10A or the second holding unit 10B may be equipped with a one-axis stage that moves the first optical fiber F1 or the second optical fiber F2 in the x direction. In this way, the structure of the optical fiber fusion device 100 can be simplified.

[0030] In the above embodiment, an example of the optical fiber fusion method including a preheating step (step S102) and a fusion step (step S103) has been described, but the optical fiber fusion method may be any method capable of fusion of the first optical fiber F1 and the second optical fiber F2, and the fusion step (step S103) may be performed without performing the preheating step (step S102). In this way, the first optical fiber F1 and the second optical fiber F2 can be fused in a short time. EXAMPLES

[0031] The effects of the optical fiber fusing device and the optical fiber fusing method are demonstrated below by examples. These examples show one embodiment of the present disclosure, and the present disclosure is not limited thereto in any way.

[0032] Here, an example will be described in which a first optical fiber F1 and a second optical fiber F2, which are PMMA optical fibers with a diameter of 0.5 mm, are fusion-spliced. PMMA optical fibers soften and deform at temperatures between 80°C and 100°C, and have a melting point of about 165°C.

[0033] First, as shown in Fig. 1(A) and Fig. 1(B), the first optical fiber F1 and the second optical fiber F2 were held, and the three-axis stage 11A of the first holding part 10A and the three-axis stage 11B of the second holding part 10B were operated to face the tip of the first optical fiber F1 to the tip of the second optical fiber F2, and aligned with the irradiation position of the laser light. At this time, a gap was left between the tip of the first optical fiber F1 and the tip of the second optical fiber F2.

[0034] Next, a laser beam having a wavelength of 2.8 μm was irradiated at a first light intensity onto the tip of the first optical fiber F1 and the tip of the second optical fiber F2, and preheated as shown in Fig. 7. The first light intensity had an output of 100 mW or less and a spot size of 15 μm. Preheating makes it possible to process the end faces of the first and second optical fibers F1 and F2, and does not require pretreatment after fiber breakage.

[0035] Next, a laser beam having a wavelength of 2.8 μm, which is a second light amount larger than the first light amount, was irradiated onto the tip of the first optical fiber F1 and the tip of the second optical fiber F2. The second light amount had an output of 120 mW. When the tip of the first optical fiber F1 and the tip of the second optical fiber F2 started to melt as shown in FIG. 8, the first optical fiber F1 and the second optical fiber F2 were pressed against each other by a push amount of 0.5 mm on each side as shown in FIG. 9. As a result, the tip of the first optical fiber F1 and the tip of the second optical fiber F2 were fused together.

[0036] Next, it was observed whether the tip of the first optical fiber F1 and the tip of the second optical fiber F2 were fused without any axial misalignment, and if they were fused without any axial misalignment, the laser irradiation was stopped. This completed the fusion of the first optical fiber F1 and the second optical fiber F2. If there was any axial misalignment between the tip of the first optical fiber F1 and the tip of the second optical fiber F2, the positions were adjusted by operating the three-axis stage 11A of the first holding unit 10A and the three-axis stage 11B of the second holding unit 10B. When there was no axial misalignment, the laser irradiation was stopped. This completed the fusion of the first optical fiber F1 and the second optical fiber F2.

[0037] Next, the transmittance of the fused first optical fiber F1 and second optical fiber F2 was measured. The measurement results of the transmittance of the first optical fiber F1 and second optical fiber F2, which were fused by pushing in 0.5 mm on one side, are shown in Table 2. The average transmittance was 58.0%, which was at a practical level.

[0038] [Table 1]

[0039] Next, the tensile strength of the first optical fiber F1 and the second optical fiber F2, which were fused by pushing in 0.5 mm on each side, was measured using a force gauge, and the results are shown in Table 1. The tensile strength of all samples was 13.5 N. This is the same as the stretch limit of the original first optical fiber F1 and second optical fiber F2 used in the measurement, and it was found that the tensile strength was equivalent before and after the fusion.

[0040] [Table 2]

[0041] Next, the relationship between the transmittance and each one-side push-in amount Δx (mm) was measured. The measurement results are shown in Figure 10. Since the transmittance changes depending on the one-side push-in amount Δx, it was found that there is a possibility of improving the transmittance by adjusting the one-side push-in amount Δx (mm).

[0042] Next, the relationship between the tensile strength (N) and the allowable bending radius (mm) for each one-sided push-in amount Δx (mm) was measured. The measurement results are shown in Figure 11. Since the tensile strength and the allowable bending radius change depending on the one-sided push-in amount Δx, it was found that there is a possibility of improving the tensile strength and the allowable bending radius by adjusting the one-sided push-in amount Δx.

[0043] As described above, it was found that the first optical fiber F1 and the second optical fiber F2, which are PMMA optical fibers with a diameter of 0.5 mm, can be fused by irradiating them with a laser beam having a wavelength of 2.8 μm. The results showed that the transmittance, tensile strength, allowable bending radius, etc. were sufficient for practical use. It is considered that the transmittance, tensile strength, allowable bending radius, etc. can be further improved by adjusting other parameters such as the laser output and irradiation time in addition to the one-side push-in amount Δx. It is also considered that plastic optical fibers other than PMMA optical fibers can be fused in the same way.

[0044] The present invention allows various embodiments and modifications without departing from the broad spirit and scope of the present invention. The above-described embodiments are for the purpose of explaining the present invention and do not limit the scope of the present invention. That is, the scope of the present invention is indicated by the claims, not the embodiments. Various modifications made within the scope of the claims and the scope of the invention equivalent thereto are considered to be within the scope of the present invention. [Explanation of symbols]

[0045] 10A First holding part 10B Second holding part 11A 3-axis stage 11B 3-axis stage 20 Laser irradiation unit 21 Laser medium 22 resonator 23 Excitation light source 24A, 24B End Caps 25 cores 26 Clad 22A Reflector 22B output mirror 100 Optical fiber fusion device F1 First Optical Fiber F2 Second optical fiber

Claims

1. a first holding portion that holds a first optical fiber; a second holding portion that holds the second optical fiber with a tip end portion of the first optical fiber facing a tip end portion of the second optical fiber; a laser irradiation unit that irradiates a tip end of the first optical fiber and a tip end of the second optical fiber with a laser beam having a wavelength of 2.7 μm or more and 3.0 μm or less; An optical fiber fusion device comprising:

2. At least one of the first holding portion and the second holding portion holds the first optical fiber or the second optical fiber movably in a direction in which the first optical fiber and the second optical fiber extend.

2. The optical fiber fusing apparatus according to claim 1.

3. an observation unit for observing the tip end of the first optical fiber and the tip end of the second optical fiber; 3. The optical fiber fusion splicing apparatus according to claim 1 or 2.

4. a tip end of a first optical fiber and a tip end of a second optical fiber are held facing each other, and a laser light having a wavelength of 2.7 μm or more and 3.0 μm or less is irradiated onto the tip end of the first optical fiber and the tip end of the second optical fiber; 1. A method for fusing optical fibers comprising the steps of:

5. a preheating step of preheating the tip portion of the first optical fiber and the tip portion of the second optical fiber by irradiating the tip portion of the first optical fiber with the laser light at a first light amount; 5. The method for fusing optical fibers according to claim 4.

6. a fusion step of irradiating the laser light with a second light amount greater than the first light amount to the tip portion of the first optical fiber and the tip portion of the second optical fiber which have been preheated, 6. The method for fusing optical fibers according to claim 5.

7. In the fusion step, a tip end portion of the second optical fiber is pushed into a tip end portion of the first optical fiber.

7. The method for fusion splicing optical fibers according to claim 6.

Citation Information

Patent Citations

  • Device and method for preparing thick-waist tapered optical fiber

    CN104316997A

  • Joining method of plastic optical fiber

    JP1984040614A

  • Apparatus and method for production of optical fiber type optical parts

    JP1995306332A

  • Melt-sticking method of thermoplastic resin member

    JP2009125963A

  • Welding apparatus and welding method of thermoplastic resin tube