Production method of catalyst for producing unsaturated aldehyde, unsaturated carboxylic acid or conjugated diene

By controlling gas flow and composition in the catalyst firing process, the method enhances catalyst efficiency and selectivity for unsaturated aldehydes and carboxylic acids, addressing yield and stability issues while minimizing environmental hazards and costs.

JP2024142970APending Publication Date: 2024-10-11NIPPON KAYAKU CO LTD
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
JP2023055398
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-30
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

Existing catalysts for producing unsaturated aldehydes and unsaturated carboxylic acids, such as methacrylic acid, suffer from low effective yield, selectivity, short life, and mechanical strength, and are associated with increased costs and environmental hazards due to nitrogen oxide generation during calcination.

Method used

A method for producing a catalyst by controlling the volume of gas flow during the firing process of a catalyst molded body containing alcohol, using a specific composition and conditions to enhance catalyst efficiency and selectivity, including a firing process where the weight of the catalytic active component and gas volume satisfy a specific ratio, and employing a composition represented by Mo10V a1 P b1 Cu c1 As d1 X e1 Y f1 O g1, with careful selection of inert carriers and binders.

Benefits of technology

The method results in a highly active catalyst with improved selectivity and stability, particularly in methacrylic acid production, reducing the risk of catalyst reduction and explosion while maintaining mechanical strength and lowering production costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024142970000001
    Figure 2024142970000001
Patent Text Reader

Abstract

To provide a catalyst which can drastically improve selectivity of a target compound in a gas phase catalytic oxidation method, especially in a reaction to produce methacrylic acid by using methacrolein as a raw material, leading to the tremendous effect and obtaining methacrylic acid with higher selectivity by using the catalyst produced by a production method of the invention.SOLUTION: A production method of a catalyst for producing an unsaturated aldehyde, an unsaturated carboxylic acid, or a conjugated diene, is a production method of the catalyst having a step (A) to prepare a slurry liquid by blending raw materials, a step (B) to dry the slurry liquid, a molding step (C), and a calcination step (D) of a catalyst molded body containing an alcohol. In the calcination step (D) of the catalyst molded body containing the alcohol, a weight of a catalyst active ingredient obtained by excluding a carrier, an auxiliary for hardness, and a binder from the catalyst molded body is represented by α(g), and a volume of gas introduced into a calcination furnace per second in calcination time is represented by β(Nm3 / sec), α and β satisfy the formula (1). 1,000,000≤α / β≤7,000,000...(1).SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for producing a catalyst for obtaining an unsaturated aldehyde, an unsaturated carboxylic acid, or a conjugated diene by an oxidation reaction, and relates to a method for producing a highly active catalyst capable of obtaining the target product with a higher selectivity than conventional catalysts. [Background technology]

[0002] Methods for producing unsaturated aldehydes and unsaturated carboxylic acids, and gas-phase catalytic oxidation methods for producing 1,3-butadiene from butenes are widely practiced industrially, and the use of composite metal oxide catalysts containing bismuth and molybdenum as main components is well known to those skilled in the art. In particular, with regard to methods for producing the corresponding unsaturated aldehydes and unsaturated carboxylic acids from raw materials such as propylene, isobutylene, and t-butyl alcohol, many reports have been made on means for improving the yield.

[0003] Among these, many proposals have been made so far regarding catalysts for producing methacrylic acid. Among these, there are some in which the microstructure of the catalyst, such as pore volume and pore distribution, is adjusted by the catalyst molding method or molding conditions. For example, Patent Document 1 proposes a catalyst for producing methacrylic acid in which the ratio of the pore volume of pores with a pore diameter radius of 0.005 to 0.05 μm to the pore volume of pores with a pore diameter radius of 0.005 to 10 μm is 20% or more.

[0004] Patent Document 2 proposes a catalyst for producing methacrylic acid, in which the pore volume of the catalyst is 0.1 cc / g or more and 0.9 cc / g or less, the pore volume occupied by pores with a pore diameter of less than 0.1 μm is 15% or less of the total pore volume, the pore volume occupied by pores with a pore diameter of 0.1 μm or more and less than 1 μm is less than 15% of the total pore volume, and the pore volume occupied by pores with a pore diameter of 1 μm or more and less than 10 μm is 65% or more of the total pore volume. Patent Document 3 proposes a catalyst for producing methacrylic acid, in which the pore volume of a pore with a pore radius of 0.05 μm or less is 0.01 cc / g or less, and the volume of a pore with a pore radius of more than 0.05 μm is 0.2 cc / g or more. However, the catalysts obtained as in Patent Documents 1 to 3 have problems such as low effective yield and selectivity of the target product, short life, and low mechanical strength, and further improvement is desired for use as an industrial catalyst.

[0005] In addition, Patent Document 4 proposes a method of calcining a catalyst in which calcination is not performed in multiple stages and the gas during calcination is changed. In addition, Patent Document 5 also proposes a method of calcining with a gas having a reduced oxygen concentration as a similar calcination method. However, these catalyst manufacturing methods require calcination in multiple stages, changing the gas during calcination, or both, and have problems such as reduced productivity and increased costs. For this reason, a method for manufacturing a catalyst with a high effective yield and selectivity of the target product in a simpler manner has been desired. In addition, Patent Document 6 proposes a method of using a catalyst precursor containing an ammonium root or a nitrogen-containing organic compound, circulating a gas at an appropriate flow rate, and calcining at an appropriate temperature. However, these methods have problems such as increased costs for treating exhaust gases due to the generation of nitrogen oxides that are harmful to the human body during calcination. For this reason, a method for manufacturing a catalyst with a high effective yield and selectivity of the target product without generating nitrogen oxides has been desired. In these patent documents, organic compounds such as alcohols that have low flash points tend to be avoided as binders because they are flammable and explosive, and because they are less safe and the catalyst is sintered or reduced due to the oxidation and combustion of the alcohol. For this reason, there were no documents that disclosed a method for firing a catalyst molded body containing alcohol used as a binder by controlling the air volume. [Prior art documents] [Patent documents]

[0006] [Patent Document 1] Japanese Patent No. 3710944 [Patent Document 2] Japanese Patent Application Publication No. 2017-176932 [Patent Document 3] Japanese Patent Publication No. 2003-10690 [Patent Document 4] Japanese Patent Application Publication No. 2000-210566 [Patent Document 5] Japanese Patent Publication No. 5-279291 [Patent Document 6] Japanese Patent Publication 2009-213969 Summary of the Invention [Problem to be solved by the invention]

[0007] An object of the present invention is to provide a method for producing a highly active catalyst capable of stably producing methacrylic acid with excellent selectivity. [Means for solving the problem]

[0008] As a result of thorough research into the current situation and problems described above, the inventors of the present application discovered that the selectivity and activity of the catalyst can be improved by controlling the volume of gas blown in to a certain extent in the process of calcining an alcohol-containing catalyst molded body, and thus arrived at the present invention.

[0009] That is, the present invention relates to the following 1) to 7). 1) A method for producing a catalyst, comprising: (A) a step of mixing raw materials to prepare a slurry liquid; (B) a step of drying the slurry liquid; (C) a molding step; and (D) a step of calcining an alcohol-containing molded catalyst body, (D) In ​​the calcination process of the catalyst molded body containing alcohol, the weight of the catalytic active component is α (g), and the volume of gas introduced into the calcination furnace per second during the calcination time is β (Nm 3 / sec), α and β satisfy the following formula (1): 1000000 ≦ α / β ≦ 7000000 (1) 2) In the above formula (1), β is 0.00001 (Nm 3 / sec) or more 0.04 (Nm) 3 1) Catalyst for producing an unsaturated aldehyde, an unsaturated carboxylic acid, or a conjugated diene, wherein the reaction rate is 1 / sec or less. 3) In the above formula (1), the method for producing a catalyst for producing an unsaturated aldehyde, an unsaturated carboxylic acid, or a conjugated diene according to 1) above, wherein the weight ratio γ / α of the alcohol weight γ (g) contained in the catalyst active component weight α (g) is 0.01 or more and 0.4 or less. 4) The method for producing a catalyst for producing an unsaturated aldehyde, an unsaturated carboxylic acid, or a conjugated diene according to any one of 1) to 3) above, which contains a catalyst active component represented by the following formula (2). Mo 10 V a1 P b1 Cu c1 As d1 X e1 Y f1 O g1 (2) (In the formula, Mo, V, P, Cu, As, and O represent molybdenum, vanadium, phosphorus, copper, arsenic, and oxygen, respectively. X represents at least one element selected from the group consisting of Ag, Mg, Zn, Al, B, Ge, Sn, Pb, Ti, Zr, Sb, Cr, Re, Bi, W, Fe, Co, Ni, Ce, and Th. Y represents at least one element selected from the group consisting of K, Rb, Cs, and Tl. a1, b1, c1, d1, e1, and g1 represent the atomic ratios of the respective elements. a1 satisfies 0 < a1 ≤ 6, b1 satisfies 0 ≤ b1 ≤ 6, c1 satisfies 0 < c1 ≤ 3, d1 satisfies 0 < d1 < 3, e1 satisfies 0 ≤ e1 ≤ 3, f1 satisfies 0 ≤ f1 ≤ 3, and g1 is a value determined by the valences and atomic ratios of other elements.) 5) The method for producing a catalyst for producing an unsaturated aldehyde, an unsaturated carboxylic acid, or a conjugated diene according to 4) above, wherein in the above formula (2), a1 and c1 satisfy the following formula (3). 0.5 ≤ a1 / c1 ≤ 5.0 (3) 6) Furthermore, the method for producing a catalyst for producing an unsaturated aldehyde, an unsaturated carboxylic acid, or a conjugated diene according to any one of 1) to 3) above, wherein the (D) shaping step includes a step of supporting on an inert carrier. 7) The method for producing a catalyst for producing an unsaturated aldehyde, an unsaturated carboxylic acid, or a conjugated diene according to the above 6), wherein the inert carrier is silica or alumina. Effect of the Invention

[0010] The catalyst produced by the production method of the present invention can greatly improve the selectivity of the target compound in a gas-phase catalytic oxidation process. In particular, the effect is significant in the reaction of producing methacrylic acid from methacrolein as a raw material, and the target compound can be obtained with a higher selectivity. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] The catalyst production method of the present invention is a catalyst production method comprising: (A) a step of mixing raw materials to prepare a slurry liquid; (B) a step of drying the slurry liquid; (C) a molding step; and (D) a step of calcining an alcohol-containing molded catalyst body, (D) In ​​the calcination process of the catalyst molded body containing alcohol, the weight of the catalytic active component is α (g), and the volume of gas introduced into the calcination furnace per second during the calcination time is β (Nm 3 / sec), α and β satisfy the above formula (1).

[0012] [(D) Calcination process of the catalyst molded body containing alcohol] The method for producing a catalyst of the present invention includes (A) a step of mixing raw materials to prepare a slurry liquid, (B) a step of drying the slurry liquid, (C) a molding step, and (D) a step of calcining the alcohol-containing molded catalyst body. First, the step (D) will be described. The main purpose of step (D) is to remove the alcohol used as a binder in step (C). That is, as long as the purpose is achieved, there is no particular limitation on the conditions, but for example, a method in which the catalyst molded body obtained by steps (A) to (C) is charged into a vat in a calcination furnace and calcined by a batch method can be exemplified. The alcohol used as a binder in step (C), contained in the catalyst molded body, and removed in step (D) is not particularly limited as long as it is a hydrocarbon having a hydroxyl group in the molecule, but examples thereof include linear or branched monoalcohols having 1 to 4 carbon atoms such as methanol, ethanol, propanol, and butanol, polyhydric alcohols such as ethylene glycol and glycerin, polyvinyl alcohol as a polymer binder, crystalline cellulose, methyl cellulose, ethyl cellulose, and other celluloses. Among these, linear monoalcohols having 1 to 4 carbon atoms are preferred, and ethanol is particularly preferred. As for the firing conditions, for example, the binder component can be removed by firing at about 200°C to 1000°C, preferably 250°C to 700°C, and more preferably 250°C to 600°C under air flow. The firing time is preferably about 1 minute to 12 hours, and more preferably 5 minutes to 8 hours. The firing time here does not include the time required for the temperature increase and decrease steps, and means the time within the range of the maximum set temperature in the firing step ±5°C. The temperature increase rate is preferably 0.1 to 10°C / min, and more preferably 0.5 to 5°C / min. The gas atmosphere during firing is not particularly limited, but an oxidizing gas such as air can be used.

[0013] In the present invention, in the step (D), the weight of the catalytic active component α (g) and the volume of gas introduced into the calcination furnace per second during the calcination time are β (Nm 3 / sec), α and β satisfy formula (1). The weight of catalytic active components α (g) means the weight of catalytic active components excluding the carrier, strength aid, alcohol, and other binders added as necessary from the weight of the catalyst molded body. Details will be explained in step (C). [Formula (1)] 1000000 ≦ α / β ≦ 7000000 (1) The lower limit of this α / β is more preferably, in order, 1,200,000, 1,300,000, 1,500,000, and 1,700,000, and particularly preferably, 1,800,000. The upper limit is more preferably, in order, 6,000,000, 5,000,000, 4,500,000, 4,000,000, and 3,500,000, and particularly preferably, 3,200,000. In other words, α / β is most preferably 1,800,000 or more and 3,200,000 or less.

[0014] Furthermore, there is a preferred range for the above β. If β is too small, there is a risk of promoting the reduction of the catalyst, and a large amount of alcohol will remain in the furnace, which may cause an explosion. If β is too large, a large blower is required, which increases costs. Therefore, β should be 0.00001 Nm 3 / sec or more 0.04Nm 3 More preferably, the lower limit is 0.00002 Nm / sec or less. 3 / sec, 0.00003Nm 3 / sec, 0.00004Nm 3 / sec, 0.00005Nm 3 / sec, 0.00006Nm 3 / sec, 0.00007Nm 3 / sec, 0.00008Nm 3 / sec, and particularly preferably 0.00010 Nm 3 More preferably, the upper limit is 0.038 Nm 3 / sec, 0.035Nm 3 / sec, 0.030Nm 3 / sec, 0.025Nm 3 / sec, 0.020Nm 3 / sec, and particularly preferably 0.015 Nm 3 / sec. Therefore, the most preferable range of β is 0.00010 Nm 3 / sec or more 0.015Nm 3 / sec or less.

[0015] [(A) Process of mixing raw materials to prepare slurry liquid] For the sake of convenience, step (D) has been described above in light of the content of the present invention. However, the catalyst production process usually starts with step (A), and proceeds through steps (B) and (C) to step (D). Step (A) is a step of preparing a slurry liquid by mixing raw materials, more specifically, a step of dispersing compounds containing one or more of the constituent metals (hereinafter also referred to as active component elements) in water to prepare an aqueous solution or aqueous dispersion of these compounds (hereinafter both are referred to as a slurry liquid). Note that this step also includes a step of preparing compounds containing one or more of the constituent metals and a step of mixing these compounds with water. In step (A), a compound containing the essential active component element and any active component element of the catalyst of the present invention is used. Examples of the compound include chlorides, sulfates, nitrates, oxides, and acetates of the active component elements. More specific examples of preferred compounds include nitrates such as cobalt nitrate, acetates such as copper acetate, oxides such as molybdenum oxide, vanadium pentoxide, copper oxide, antimony trioxide, cerium oxide, zinc oxide, and germanium oxide, and acids (or salts thereof) such as orthophosphoric acid, phosphoric acid, boric acid, aluminum phosphate, and 12-tungstophosphoric acid, but are not limited thereto. These compounds containing active components may be used alone or in combination of two or more. In step (A), each active component-containing compound and water are uniformly mixed to obtain a slurry liquid. In the slurry liquid, it is not necessary for all components to be dissolved in water, and it is acceptable for some or all of them to be in a suspended state. There is no particular restriction on the amount of water used in the slurry liquid as long as it is an amount that can completely dissolve all of the compounds used or can be uniformly mixed. The amount of water to be used may be appropriately determined taking into consideration the drying method and drying conditions in step (B). Usually, the amount of water is about 200 to 2000 parts per 100 parts of the total mass of the raw materials. The more water, the better, but if there is too much water, there are many disadvantages, such as high energy costs for the drying step in step (B) and in some cases in which complete drying is not possible.

[0016] In the present invention, the shape of the stirring blades of the stirrer used in step (A) is not particularly limited, and any stirring blade such as a propeller blade, turbine blade, paddle blade, inclined paddle blade, screw blade, anchor blade, ribbon blade, large lattice blade, etc. can be used in one stage or in two or more stages of the same blade or different blades in the vertical direction. In addition, a baffle (baffle plate) may be installed in the reaction tank as necessary.

[0017] [(B) Step of drying the slurry liquid] In step (B), the slurry liquid obtained in step (A) is completely dried. The drying method is not particularly limited, but examples thereof include drum drying, freeze drying, spray drying, and evaporation to dryness. Among these, in the present invention, spray drying is preferred, which can dry the slurry liquid into powder or granules in a short time. The drying temperature of spray drying varies depending on the concentration of the slurry liquid, the liquid sending speed, etc., but the temperature at the outlet of the dryer is generally 70 to 150°C.

[0018] [(C) Molding process] In step (C), the dried slurry obtained in step (B) (hereinafter referred to as dry powder) is molded. The mechanical strength and catalytic performance may be improved if the dried powder is calcined at about 250°C to 350°C before molding, so the dried powder may be calcined before molding (hereinafter, this step may be referred to as pre-calcination). There are no particular restrictions on the molding method, and in order to reduce the pressure loss of the reaction gas in the oxidation reaction, the dried powder may be molded into a columnar object, tablet, ring, sphere, etc., or the dried powder may be coated on an inert carrier. Of these, it is preferable to coat the dried powder on an inert carrier to form a coated catalyst, since it is expected to improve selectivity and remove reaction heat. For this coating step, the rolling granulation method described below is preferable. In this method, for example, a flat or uneven disk is rotated at high speed in an apparatus at the bottom of a fixed container, and the carrier in the container is vigorously stirred by repeated rotation and revolution, and the alcohol, the dry powder obtained in step (B), and other additives such as molding aids and strength improvers are added to the coating mixture, which is then coated on the carrier. The binder can be added in any of the following ways: 1) premixed with the coating mixture, 2) added at the same time as the coating mixture is added to the fixed container, 3) added after the coating mixture is added to the fixed container, 4) added before the coating mixture is added to the fixed container, 5) divided into the coating mixture and the alcohol, and the total amount is added by appropriately combining 2) to 4). In 5), it is preferable to adjust the addition speed using an autofeeder or the like so that a predetermined amount is loaded on the carrier without adhesion of the coating mixture to the wall of the fixed container or aggregation of the coating mixture. If the weight γ (g) of the alcohol such as ethanol used during molding is too high, it may promote the reduction of the catalyst, and a large amount of alcohol may remain in the furnace, causing a risk of explosion. If γ is too small, the wear degree may worsen. Also, when the alcohol is diluted with other binders such as water as described below in [Other binders], this γ does not include the weight of other binders such as water. The weight content γ / α of the alcohol relative to the catalytically active component is preferably 0.01 or more and 0.4 or less. When it is in this range, the catalytic activity can also be improved.More preferable lower limits of γ / α are 0.02, 0.03, 0.04, 0.05, 0.06, 0.07, 0.08, and 0.09, respectively, and particularly preferably 0.10. More preferable upper limits of γ / α are 0.35, 0.30, 0.25, 0.20, 0.15, 0.14, and 0.13, respectively, and particularly preferably 0.12. Therefore, the most preferable range of γ / α is 0.10 or more and 0.12 or less.

[0019] Specific examples of the inert carrier in the coating include silicon carbide, alumina, silica, silica alumina, mullite, alundum, steatite, etc., preferably silicon carbide, alumina, silica, silica alumina, steatite, more preferably alumina, silica, and silica alumina. The diameter of the carrier is 1 to 15 mm, preferably a spherical carrier having a diameter of 2.5 to 10 mm. The component in the carrier is preferably 90 mass% or more, more preferably 95 mass% or more. These carriers are usually used with a porosity of 10 to 70%. The ratio of the carrier and the mixture for coating is usually 10 to 75 mass% of the mixture for coating / (mixture for coating+carrier) and is preferably 15 to 60 mass%. When the ratio of the mixture for coating is large, the reaction activity of the coated catalyst increases, but the mechanical strength tends to decrease. Conversely, when the ratio of the mixture for coating is small, the mechanical strength increases, but the reaction activity tends to decrease. In the above, examples of the molding aid used as needed include silica gel, diatomaceous earth, and alumina powder. The amount of the molding aid used is usually 1 to 60 parts by mass per 100 parts by mass of the catalytically active component solid. Furthermore, if necessary, inorganic fibers (e.g., ceramic fibers or whiskers) inactive to the catalytically active component and the reaction gas are used as a strength improver, which is useful for improving the mechanical strength of the catalyst. The amount of these fibers used is usually 1 to 30 parts by mass per 100 parts by mass of the catalytically active component solid. The inactive carrier in the present invention is a carrier that has no activity against the raw materials and the product, and for example, the conversion rate of methacrolein under generally known reaction conditions is 3.0% or less.

[0020] The weight α of the catalytic active component is the weight of the catalyst molded body excluding alcohol, any other binders or inert carriers, inorganic fibers, etc. The catalyst molded body is a molded body obtained in the above step (C) and is composed of a dry powder, any other inert carriers, inorganic fibers, etc. The above α is the weight of only the dry powder and is the weight of the catalyst molded body excluding alcohol, any other binders or inert carriers, inorganic fibers, etc. In addition, the powder may contain a small amount of moisture, and the moisture contained in this small amount of dry powder is included in the weight α.

[0021] [Catalytic active component composition] A preferred composition of the catalytically active component of the catalyst of the present invention is represented by the following general formula (1). [C1] Mo 10 V a1 P b1 Cu c1 As d1 X e1 Y f1 O g1 (1) Here, Mo, V, P, Cu, As, and O represent molybdenum, vanadium, phosphorus, copper, arsenic, and oxygen, respectively. X represents at least one element selected from the group consisting of Ag (silver), Mg (magnesium), Zn (zinc), Al (aluminum), B (boron), Ge (germanium), Sn (tin), Pb (lead), Ti (titanium), Zr (zirconium), Sb (antimony), Cr (chromium), Re (rhenium), Bi (bismuth), W (tungsten), Fe (iron), Co (cobalt), Ni (nickel), Ce (cerium), and Th (thorium). Y represents at least one element selected from the group consisting of K (potassium), Rb (rubidium), Cs (cesium), and Tl (thallium). a1, b1, c1, d1, e1, f1, and g1 represent the atomic ratios of the respective elements. a1 satisfies 0 < a1 ≤ 6, b1 satisfies 0 ≤ b1 ≤ 6, c1 satisfies 0 < c1 ≤ 3, d1 satisfies 0 ≤ d1 < 3, e1 satisfies 0 ≤ e1 ≤ 3, f1 satisfies 0 ≤ f1 ≤ 3, and g1 is a value determined by the valences and atomic ratios of the other elements. Also, the composition in the present invention means the active ingredient, and as the inert carrier, silicon carbide, alumina, silica, silica alumina, mullite, alundum, steatite, etc. can be used.

[0022] In the composition of the above formula (1), preferred ones for X are Zn, Ag, Fe, and Sb, more preferably Ag, Fe, and Sb, particularly preferably Fe and Sb, and most preferably Sb.

[0023] In the composition of the above formula (1), preferred ones for Y are K, Rb, and Cs, more preferably K and Cs, and most preferably Cs. However, a catalyst not containing the Y component tends to particularly exhibit the effects of the present invention significantly.

[0024] In the composition of the above formula (1), the preferred ranges of a1 to g1 are as follows. The lower limit of a1 is, in order of preference, 0.1, 0.2, 0.25, 0.3, 0.35, 0.4, and 0.5, and is most preferably 0.55. The upper limit of a1 is, in order of preference, 5, 3, 2, 1, 0.8, and 0.7, and is most preferably 0.65. That is, the most preferable range of a1 is 0.55≦a1≦0.65. The lower limit of b1 is, in order of preference, 0, 0.1, 0.3, 0.5, 0.7, 0.9, 1.0, and most preferably 1.1. The upper limit of b1 is, in order of preference, 5, 4, 3, 2, and most preferably 1.5. That is, the most preferable range of b1 is 1.1≦b1≦1.5. The lower limit of c1 is, in order of preference, 0.1, 0.2, 0.3, and most preferably 0.4. The upper limit of c1 is, in order of preference, 2, 1.5, 1.2, 1.0, 0.8, and most preferably 0.6. That is, the most preferable range of c1 is 0.4≦c1≦0.6. The lower limit of d1 is, in order of preference, 0, 0.1, 0.2, 0.3, and 0.4, and is most preferably 0.45. The upper limit of d1 is, in order of preference, 2, 1.5, 1.2, 1.0, and 0.8, and is most preferably 0.6. That is, the most preferable range of d1 is 0.45≦d1≦0.6. The lower limit of e1 is, in order of preference, 0.01, 0.05, and 0.07, and most preferably 0.08. The upper limit of e1 is, in order of preference, 2, 1.5, 1, 0.5, and 0.3, and most preferably 0.2. The lower limit of e1 is 0, and X is not contained, that is, the most preferred range of e1 is 0.08≦c1≦0.2. The upper limit of f1 is, in order of preference, 2, 1.5, 1, 0.5, 0.1, and most preferably 0.05. The lower limit of f1 is 0, and Y is not contained, that is, f1=0 is the most preferred composition of the catalyst (A).

[0025] In the above formula (1), when the relationship a1 / c1 is 0.1 or more and 5.0 or less, this is a particularly preferable catalyst composition for the catalyst of the present invention. The upper limit of a1 / c1 is preferably 4, 3, 2, 1.8, 1.5, and particularly preferably 1.3. The lower limit is preferably 0.2, 0.5, 0.7, 0.8, and particularly preferably 1.0. Therefore, the most preferable range of a1 / c1 is 1.0≦a1 / c1≦1.3.

[0026] [Other binders] In the present invention, alcohol is used as a binder in the molding step (C), but may be used in combination with other binders. Examples of other binders that can be suitably used include water, organic compounds having a boiling point of 150° C. or less at 1 atm or less, or their aqueous solutions, inorganic binders such as silica sol aqueous solutions, etc. Examples of organic compounds having a boiling point of 150° C. or less include ethers such as ethyl ether, butyl ether, and dioxane, esters such as ethyl acetate and butyl acetate, and ketones such as acetone and methyl ethyl ketone. Among these, water is preferred, that is, a certain amount of water is used in combination with alcohol to form an alcohol aqueous solution. In this case, the ratio of alcohol to water is preferably 99 / 1 to 1 / 99 (mass ratio) for alcohol / water, more preferably 98 / 2 to 50 / 50, and particularly preferably 95 / 5 to 80 / 20.

[0027] [Uses of the catalyst produced by the present invention] The catalyst obtained by the production method of the present invention can be applied to reactions for producing corresponding unsaturated aldehydes and unsaturated carboxylic acids using propylene, isobutylene, t-butyl alcohol, etc. as raw materials, and for producing 1,3-butadiene from butenes, and enables stable operation with high selectivity. In particular, when used in a reaction for producing methacrylic acid by gas-phase catalytic oxidation of methacrolein with molecular oxygen or a molecular oxygen-containing gas, the effect can be confirmed more significantly. In the method for producing methacrolein or methacrylic acid, the method for flowing the raw material gas may be a normal single flow method or a recycle method, and may be carried out under generally used conditions and is not particularly limited. For example, a mixed gas consisting of 1 to 10 volume %, preferably 4 to 9 volume %, of starting raw materials at room temperature, 3 to 20 volume %, preferably 4 to 18 volume %, of molecular oxygen, 0 to 60 volume %, preferably 4 to 50 volume %, of water vapor, and 20 to 80 volume %, preferably 30 to 60 volume %, of inert gas such as carbon dioxide or nitrogen, is filled in a reaction tube and then, at 240 to 450° C., under a pressure of normal pressure to 10 atm, at a space velocity of 300 to 5000 h , over the catalyst of the present invention. -1 The volumes of all the raw gases are calculated assuming that they are ideal gases. EXAMPLES

[0028] The present invention will be described in more detail below with reference to examples, but the present invention is not limited to these examples. In the examples, "parts" means parts by weight, and "%" means % by weight.

[0029] [Example 1] 1) Preparation of catalyst Molybdenum oxide, vanadium pentoxide, cupric oxide, an aqueous solution of phosphoric acid, an aqueous solution of arsenic acid, and antimony trioxide were weighed out so that the catalytically active solid component had the following composition. Mo 10 V 0.6 P 1.2 As 0.5 Sb 0.1 Cu 0.5 O g (g is a value determined by the valence and atomic ratio of other elements.) Molybdenum oxide, vanadium pentoxide, cupric oxide, phosphoric acid aqueous solution, and arsenic acid aqueous solution were added to pure water (7 times the amount of molybdenum oxide by weight), and the mixture was heated and stirred at 92°C for 4 hours to obtain a slurry liquid. Antimony trioxide was then added to this solution, and the mixture was heated and stirred to obtain a slurry liquid solution. This solution was then spray-dried to obtain a dried product. Next, 214 parts of the obtained dried slurry product and 29.8 parts of a strength improving material (alumina-silica fiber) were uniformly mixed, and 200 parts of a spherical porous alumina carrier (particle size 3.5 mm) were coated with about 30 parts of a 90% ethanol aqueous solution as a binder and molded. Next, the obtained molded product was introduced into a furnace so that the weight α of the catalytic active components excluding the carrier, strength aid, and binder in the catalyst molded body was 270 g, and then the gas introduction volume β into the baking furnace per second during the baking time was 0.00013 Nm 3 The catalyst was calcined at 310°C for 4 hours and 40 minutes while air was circulated at a rate of 1 / sec to obtain a catalyst (coated catalyst) of the present invention. At this time, the weight γ of the alcohol contained in the catalyst molded body introduced into the furnace was 27 g.

[0030] 2) Parameters α and β The values ​​of the parameters α / β were as follows: α = Weight of catalytic active components excluding carriers, strength aids, and binders in the catalyst molded body β = Volume of gas introduced into the furnace per second during firing Calculating from this formula, under the conditions of Example 1, the value of the parameter α / β is 2100000g sec / Nm 3 It was.

[0031] 3) Production of methacrylic acid 13.7 ml of the obtained coated catalyst of the present invention was packed into a stainless steel reaction tube having an inner diameter of 18.4 mm, and the raw material gas (composition (molar ratio); methacrolein: oxygen: water vapor: nitrogen = 1: 2: 4: 18.6) was added at a space velocity (SV) of 900 h -1The oxidation reaction of methacrolein was carried out under the above conditions. The reaction bath temperature was adjusted between 290℃ and 330℃, and the methacrylic acid selectivity at a methacrolein conversion rate of 77mol% and the reaction bath temperature at a methacrolein conversion rate of 77mol% were calculated. The lower the reaction bath temperature, the higher the activity, which is advantageous in terms of catalyst life and energy costs. The conversion rate and selectivity are defined as follows. Conversion rate = moles of methacrolein reacted / moles of methacrolein fed × 100 Selectivity = moles of methacrylic acid produced / moles of methacrolein reacted × 100

[0032] [Example 2] In Example 1, the weight of the molded body was changed so that the weight α of the catalytic active components excluding the carrier, strength aid, and binder in the molded catalyst body was 220 g, and the gas introduction volume β into the firing furnace per second during the firing time was 0.00007 Nm 3 A catalyst was prepared in the same manner as in Example 1, except that the parameter α / β was 3,100,000 g sec / Nm 3 The weight γ of the alcohol contained in the catalyst molded body introduced into the furnace was 24 g.

[0033] [Example 3] In Example 1, the weight of the molded body was changed so that the weight α of the catalytic active components excluding the carrier, strength aid, and binder in the molded catalyst body was 330 g, and the gas introduction volume β into the firing furnace per second during the firing time was 0.0002 Nm 3 A catalyst was prepared in the same manner as in Example 1, except that the parameter α / β was 1,300,000 g sec / Nm 3 The weight γ of the alcohol contained in the catalyst molded body introduced into the furnace was 35 g.

[0034] [Example 4] In Example 1, the weight of the molded body was changed so that the weight α of the catalytic active components excluding the carrier, strength aid, and binder in the molded catalyst body was 330 g, and the gas introduction volume β into the firing furnace per second during the firing time was 0.00007 Nm3 A catalyst was prepared in the same manner as in Example 1, except that the parameter α / β was 4,700,000 g sec / Nm 3 The weight γ of the alcohol contained in the catalyst molded body introduced into the furnace was 35 g. [Example 5] In Example 1, the binder was changed to about 36 parts of a 70% ethanol aqueous solution, the weight of the molded body was changed so that the weight α of the catalytic active component excluding the carrier, strength aid, and binder in the catalyst molded body was 270 g, and the gas introduction volume β into the firing furnace per second during the firing time was 0.00013 Nm 3 A catalyst was prepared in the same manner as in Example 1, except that the parameter α / β was 2100000 g sec / Nm 3 The weight γ of the alcohol contained in the catalyst molded body introduced into the furnace was 22 g.

[0035] [Comparative Example 1] In Example 1, the weight of the molded body was changed so that the weight α of the catalytic active components excluding the carrier, strength aid, and binder in the molded catalyst body was 330 g, and the gas introduction volume β into the firing furnace per second during the firing time was 0.00043 Nm 3 A catalyst was prepared in the same manner as in Example 1, except that the parameter α / β was 770000 g sec / Nm 3 The weight γ of the alcohol contained in the catalyst molded body introduced into the furnace was 35 g.

[0036] The results of the production of methacrylic acid using the catalysts of Examples 2 to 4 and Comparative Example 1 in the same manner as in Example 1 are shown in Table 1 together with the results for the catalyst of Example 1.

[0037] [Table 1]

[0038] As is clear from Table 1, it can be confirmed that the catalyst obtained by the production method of the present invention has excellent selectivity for methacrylic acid, and in particular, the reaction bath temperature can be kept low by γ / α. [Industrial Applicability]

[0039] According to the present invention, it is possible to provide a catalyst capable of producing an unsaturated aldehyde, an unsaturated carboxylic acid or a conjugated diene with high selectivity and having a long life, and therefore, in a gas phase catalytic oxidation reaction using the catalyst, the target compound can be obtained with high selectivity and stably for a long period of time.

Claims

1. A method for producing a catalyst, comprising: (A) a step of mixing raw materials to prepare a slurry liquid; (B) a step of drying the slurry liquid; (C) a molding step; and (D) a step of calcining an alcohol-containing molded catalyst body, (D) In ​​the calcination process of the catalyst molded body containing alcohol, the weight of the catalytic active component is α (g), and the volume of gas introduced into the calcination furnace per second during the calcination time is β (Nm 3 / sec), α and β satisfy the following formula (1): 1000000 ≦ α/β ≦ 7000000・・・(1)

2. In the formula (1), β is 0.00001 (Nm 3 / sec) or more 0.04 (Nm 3 2. The method for producing a catalyst for producing an unsaturated aldehyde, an unsaturated carboxylic acid or a conjugated diene according to claim 1, wherein the reaction time is 100 min. / sec or less.

3. 3. The method for producing a catalyst for producing an unsaturated aldehyde, an unsaturated carboxylic acid, or a conjugated diene according to claim 1 or 2, wherein in the formula (1), the weight ratio γ / α of the weight α (g) of the catalytically active component to the weight (γ) of the alcohol contained therein is 0.01 or more and 0.4 or less.

4. 3. A method for producing a catalyst for producing an unsaturated aldehyde, an unsaturated carboxylic acid, or a conjugated diene according to claim 1 or 2, which comprises a catalytically active component represented by the following formula (2): Mỏ 10 V a1 P b1 Cổ c1 A d1 X e1 Y f1 O g1 (2) (In the formula, Mo, V, P, Cu, As, and O represent molybdenum, vanadium, phosphorus, copper, arsenic, and oxygen, respectively; X represents at least one element selected from the group consisting of Ag, Mg, Zn, Al, B, Ge, Sn, Pb, Ti, Zr, Sb, Cr, Re, Bi, W, Fe, Co, Ni, Ce, and Th; Y represents at least one element selected from the group consisting of K, Rb, Cs, and Tl; a1, b1, c1, d1, e1, f1, and g1 represent atomic ratios of each element, where a1 is 0<a1≦6, b1 is 0≦b1≦6, c1 is 0<c1≦3, d1 is 0<d1<3, e1 is 0≦e1≦3, f1 is 0≦f1≦3, and g1 is a value determined by the valence and atomic ratio of other elements.)

5. The method for producing a catalyst for producing an unsaturated aldehyde, an unsaturated carboxylic acid, or a conjugated diene according to claim 4, wherein in the formula (2), a1 and c1 satisfy the following formula (3): 0.5 ≦ a1 / c1 ≦ 5.0 (3)

6. 3. The method for producing a catalyst for producing an unsaturated aldehyde, an unsaturated carboxylic acid, or a conjugated diene according to claim 1 or 2, wherein the molding step (D) further comprises a step of supporting the catalyst on an inert carrier.

7. 7. The method for producing a catalyst for producing an unsaturated aldehyde, an unsaturated carboxylic acid, or a conjugated diene according to claim 6, wherein the inert carrier is silica or alumina.

Citation Information

Patent Citations

  • Method for producing unsaturated aldehyde and unsaturated carboxylic acid

    JP2005187460A

  • Catalyst for producing acrolein and method of producing acrolein and / or acrylic acid using the catalyst

    JP2010214217A

  • Method for manufacturing methacrylic acid-producing catalyst, and method for manufacturing methacrylic acid

    JP2012148202A

  • Catalyst, and method for producing unsaturated carboxylic acid using same

    WO2022163727A1

  • Production of methacrylic acid

    JP1993279291A