Method of producing activated polyethylene glycol derivative

A controlled drying and solvent treatment process for polyethylene glycol compounds addresses the challenges of maintaining activation purity and polydispersity in producing activated polyethylene glycol derivatives, resulting in high-quality products suitable for pharmaceutical applications.

JP2024144233APending Publication Date: 2024-10-11NOF CORP

Patent Information

Application Number
JP2024043067
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-28
Filing Date
2024-03-19
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

Existing methods for producing activated polyethylene glycol derivatives face challenges in maintaining high activation purity and suppressing polydispersity due to thermal history, especially at larger production scales.

Method used

A method involving specific drying and solvent treatment processes is employed, including drying polyethylene glycol compounds at controlled temperatures and using organic solvents with low moisture content to produce activated polyethylene glycol derivatives with high chemical purity and reduced polydispersity.

Benefits of technology

The method effectively increases activation purity and suppresses polydispersity, enabling the industrial production of high-quality activated polyethylene glycol derivatives.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024144233000001_ABST
    Figure 2024144233000001_ABST
Patent Text Reader

Abstract

To provide a method of producing an activated polyethylene glycol derivative that has high activation purity, can suppress an increase in polydispersity due to increase in thermal history, and is industrially feasible.SOLUTION: A method of producing an activated polyethylene glycol derivative having at its terminal a functional group capable of reacting with a biologically relevant substance or a precursor of the functional group comprises Steps (A), (B), and (C); i.e., Step (A): a step of drying a powdered or granular polyethylene glycol compound having at its terminal one or more groups selected from the group consisting of a carboxy group, a mercapto group, a hydroxy group, and an amino group in an atmosphere at 0°C or higher and 50°C or lower to obtain a dried powdered or granular material with a moisture content of 0.10 mass% or less; Step (B): a step of adding an organic solvent with a moisture content of 200 ppm or less by mass to the dried powdered or granular material obtained in Step (A), thereby dissolving the dried powdered or granular material in the organic solvent to obtain a solution; and Step (C): a step of reacting a polyethylene glycol compound contained in the solution obtained in Step (B) with an activating agent to obtain an activated polyethylene glycol derivative.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for producing an activated polyethylene glycol derivative. [Background technology]

[0002] When drugs using bio-related substances such as hormones, cytokines, and enzymes are administered to the body, they are usually quickly excreted from the body by glomerular filtration in the kidneys and uptake by macrophages in the liver and spleen. Therefore, their half-life in the blood is short, and it is often difficult to obtain sufficient pharmacological effects. To solve this problem, attempts have been made to chemically modify bio-related substances with water-soluble polymers such as polyethylene glycol (hereinafter sometimes referred to as "PEG"). As a result, it is possible to extend the half-life in the blood of bio-related substances by increasing the molecular weight and forming a hydration layer. It is also well known that these modifications can reduce the toxicity and antigenicity of bio-related substances and improve their coagulation properties.

[0003] Activated polyethylene glycol derivatives usually have an active group at the end of the polyethylene glycol chain that chemically bonds with a functional group such as an amino group, a mercapto group, a carboxy group, or an unsaturated bond present on the surface of a protein or the like to be modified. For example, when modifying an amino group, an active group such as a formyl group, an epoxy group, a p-nitrophenyl ester group, or an N-hydroxysuccinimidyl ester group is present at the end of the polyethylene glycol chain. For a mercapto group, an active group such as a mercapto group, a maleimidyl group, a substituted maleimidyl group, an allyl group, or an N-hydroxysuccinimidyl ester group is present at the end of the polyethylene glycol chain. For a carboxyl group, an active group such as a mercapto group or an amino group is present at the end of the polyethylene glycol chain. For an unsaturated bond, an active group such as a mercapto group is present at the end of the polyethylene glycol chain.

[0004] From the viewpoint of drug uniformity, it is necessary to use high-purity activated polyethylene glycol derivatives with a small polydispersity index (weight-average molecular weight (Mw) / number-average molecular weight (Mn)) for use in modifying drugs, in order to suppress variations in the drug's blood retention, immunogenicity, efficacy, etc. In addition, it is preferable that the conversion rate to reactive functional groups during the synthesis of activated polyethylene glycol derivatives is high in order to suppress by-products such as PEG-based impurities and PEGylated preparations with different bonds.

[0005] An activated polyethylene glycol derivative having a functional group or a precursor thereof at its terminal that can react with a biologically relevant substance can be obtained by reacting a polyethylene glycol compound raw material having a hydroxyl group, an amino group, or the like at its terminal with an activator which is a low molecular weight compound.

[0006] However, some activators are hydrolyzable and react sharply with water in the reaction system, resulting in inactivation. When the activator is inactivated, the purity of the activated polyethylene glycol derivative decreases, and adding an excessive amount of activator in anticipation of inactivation also increases impurities derived from the activator, which in turn increases the load on the purification process, and therefore, it is necessary to keep the amount of activator to a minimum.

[0007] Polyethylene glycol compounds having carboxyl, mercapto, hydroxyl or amino groups at their termini are available in a variety of forms, including hard wax, roughly crushed flakes, and powder. Polyethylene glycol compounds having hydroxyl groups at their termini are obtained by anionic polymerization of active hydrogen compounds and ethylene oxide. The polymerization is carried out under almost anhydrous conditions, but after polymerization, the polyethylene glycol compounds are removed in liquid form from a high-temperature kettle and absorb moisture when cooled and solidified in an atmospheric environment. In addition, polyethylene glycol compounds after some reaction or purification may be converted into powder by reprecipitation using a solvent. Powders have a larger surface area than wax-like or flake-like solids, and therefore are highly hygroscopic, and even if they are dried during production, the moisture content is likely to increase when handled in an atmospheric environment.

[0008] For the above reasons, the powdered polyethylene glycol compound before the activation reaction usually contains 0.1 to 2 mass% of moisture. Since this is a level that affects the deactivation of the activator in the activation reaction, it is necessary to reduce the amount of moisture in the system by carrying out some kind of drying step before the reaction.

[0009] Patent Document 1 describes a method of mixing a polyethylene glycol compound with a solvent capable of forming an azeotropic mixture with water to obtain a mixture, drying the mixture by azeotropic distillation, and then activating the polyethylene glycol compound in the solution. [Prior art documents] [Patent documents]

[0010] [Patent Document 1] JP 2013-227543 A Summary of the Invention [Problem to be solved by the invention]

[0011] However, as described in Patent Document 1, in the method for producing an activated polyethylene glycol derivative, in which a polyethylene glycol compound in a solution is dried by azeotropic distillation and then activated, the quality of the activated polyethylene glycol derivative may be reduced. This is because the thermal history increases by continuously heating the solution of the raw material polyethylene glycol compound at a high temperature, which causes an increase in polydispersity due to oxidative decomposition of the PEG chain. In general, as the production scale increases, the time required for heating and cooling becomes longer, and therefore the increase in polydispersity due to the increase in thermal history becomes more noticeable.

[0012] Thus, although activated polyethylene glycol derivatives are important materials for medical applications, it is difficult to obtain them easily.

[0013] An object of the present invention is to provide an industrially practicable method for producing an activated polyethylene glycol derivative which has high activation purity and is capable of suppressing an increase in polydispersity due to an increase in thermal history. [Means for solving the problem]

[0014] Means for Solving the Problems The present inventors have conducted intensive research to achieve the above object, and as a result have found that an activated polyethylene glycol derivative having high activation purity and suppressed deterioration in quality can be obtained by using a polyethylene glycol compound having specific properties as a raw material and carrying out an activation reaction after a specific drying step.

[0015] That is, the present invention is as follows. [1] A method for producing an activated polyethylene glycol derivative having at its terminal a functional group capable of reacting with a biologically relevant substance or a precursor of said functional group, the method comprising the following steps (A), (B) and (C): Step (A): A step of drying a powder of a polyethylene glycol compound having at least one group selected from the group consisting of a carboxyl group, a mercapto group, a hydroxyl group, and an amino group at its terminal in an atmosphere of 0°C or higher and 50°C or lower to obtain a dry powder having a moisture content of 0.10% by mass or less. Step (B): A step of adding an organic solvent having a water content of 200 ppm or less by mass to the dry powder or granule obtained in the step (A), and dissolving the dry powder or granule in the organic solvent in a sealed environment to obtain a solution. Step (C): A step of reacting the polyethylene glycol compound contained in the solution obtained in step (B) with an activator to obtain an activated polyethylene glycol derivative.

[0016] [2] The method for producing an activated polyethylene glycol derivative according to [1], wherein the organic solvent is an aprotic solvent.

[0017] [3] The method for producing an activated polyethylene glycol derivative according to [1] or [2], wherein the powder or granule in the step (A) has an average particle size of 0.1 μm or more and 10 mm or less.

[0018] [4] The method for producing an activated polyethylene glycol derivative according to [1] or [2], wherein the polyethylene glycol compound in the step (A) has a number average molecular weight of 2,000 daltons or more and 80,000 daltons or less.

[0019] [5] The method for producing the polyethylene glycol derivative according to [1] or [2], wherein the activated polyethylene glycol derivative is represented by the following formula (1): PEG-X···(1) (In formula (1), PEG is a polyethylene glycol moiety having a linear or branched structure; X is a functional group or a precursor of a functional group capable of reacting with a biologically relevant substance.

[0020] [6] The method for producing a polyethylene glycol derivative according to [1] or [2], wherein the activator is one or more compounds selected from the group consisting of disuccinimidyl carbonate, p-nitrophenyl chloroformate, di(1-benzotriazolyl) carbonate, trichlorophenyl chloroformate, p-nitrophenyl succinimidyl carbonate, p-nitrophenyl 1-benzotriazolyl carbonate, pentafluorophenyl chloroformate, 1,1'-carbonyldiimidazole, succinic anhydride, glutaric anhydride, methanesulfonyl halides, trifluoromethanesulfonyl halides, p-toluenesulfonyl halides, 6-alkyl hexanoates, azodicarboxylates, N,N'-dicyclohexylcarbodiimide and N-hydroxysuccinimide. Effect of the Invention

[0021] According to the present invention, it is possible to obtain the effects of increasing the activation purity, suppressing an increase in polydispersity due to an increase in thermal history, and enabling the production of an activated polyethylene glycol derivative that can be industrially implemented. [Brief description of the drawings]

[0022] [Figure 1] 1 is a graph showing the relationship between temperature, relative humidity, and the rate of mass change of a measurement sample during moisture adsorption / desorption measurement in Experimental Example 1. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0023] [Activated polyethylene glycol derivatives] The activated polyethylene glycol derivative of the present invention has at its terminal a functional group capable of reacting with a biologically relevant substance or a precursor of said functional group. In a preferred embodiment, the activated polyethylene glycol derivative has the following formula (2): PEG-X···(2) In formula (2), PEG is a polyethylene glycol moiety having a linear or branched structure, and X is a functional group capable of reacting with a biologically relevant substance or a precursor of the functional group.

[0024] More specifically, an activated polyethylene glycol derivative as shown in formula (3) can be exemplified. [ka]

[0025] Here, Z is a residue obtained by removing active hydrogen groups from a compound (Z(GH)n: n=2 to 8) having 2 to 8 active hydrogen groups (-GH). The active hydrogen group is a functional group having active hydrogen. Examples of the active hydrogen group (-GH) include a hydroxyl group, a carboxyl group, an amino group, a secondary amino group, and a mercapto group. When the active hydrogen group (-GH) is a hydroxyl group or a carboxyl group, the residue Z is a dehydroxylated residue, and when the active hydrogen group (-GH) is an amino group, a secondary amino group, or a mercapto group, the residue Z is a dehydrogenated residue.

[0026] Specific examples of compounds having 2 to 8 active hydrogen groups (-GH) (Z(GH)n: n = 2 to 8) include polyhydric alcohols such as ethylene glycol, propylene glycol, trimethylene glycol, isopropylene glycol, butylene glycol, tetramethylene glycol, trimethylolpropane, glycerin, diglycerin, triglycerin, hexaglycerin, pentaerythritol, dipentaerythritol, and xylitol; amino acids and peptides having an amino group, a carboxyl group, or a mercapto group, such as lysine and glutamic acid; and organic amines and organic carboxylic acids.

[0027] a, b, c, and d are integers that satisfy "0≦a≦8, 0≦b≦8, 0≦c≦7, 0≦d≦7" and "1≦a+b≦8, 2≦a+b+c+d≦8".

[0028] Y1, Y 2、 Y3 and Y4 each independently represent an ether bond, an amide bond, an ester bond, a urethane bond, a carbonate bond, a secondary amino group, a thioether bond, a disulfide bond, a thioester bond, or an alkylene group which may contain these.Preferred alkylene groups include methylene, ethylene, propylene, isopropylene, butylene, isobutylene, pentylene, isopentylene, and hexylene, which may be branched.

[0029] Polymer 1 and Polymer 2 are linear or branched polyethylene glycol chains. A branched polyethylene glycol chain is a polyethylene glycol chain that is branched into two or more chains via a linker in the middle, and may have multiple branching points. An example is a polyethylene glycol chain that is branched into two or more chains with a polyhydric alcohol such as glycerin as a branching point, as shown in the following formula (i).

[0030] [ka] (wherein m1, m2, and m3 are integers, preferably 1 to 3636, more preferably 1 to 2728, and further preferably 1 to 1818.)

[0031] The PEG in the present invention is a polymer having a polydispersity, as analyzed by gel permeation chromatography (GPC), of preferably 1.2 or less, more preferably 1.1 or less, and most preferably 1.07 or less.

[0032] The number average molecular weight of the PEG moiety in formula (2) is a value obtained by GPC analysis, and is a number average molecular weight calculated based on a calibration curve prepared using PEGs of various known molecular weights. The number average molecular weight of the PEG moiety is not particularly limited, but is preferably 2,000 daltons or more and 80,000 daltons or less, more preferably 2,000 daltons or more and 60,000 daltons or less, and even more preferably 2,000 daltons or more and 50,000 daltons or less.

[0033] In formula (3), A1 and A2 each independently represent -L1-(CH2)l1-, -L1-(CH2)l1-L2-(CH2)l2- or a single bond; L1 represents an ether bond, an amide bond, a urethane bond, a secondary amino group or a single bond; L2 represents an ether bond, an amide bond, a urethane bond, a single bond or a thioether bond; and l1 and l2 each independently represent an integer of 0 to 5.

[0034] X1 and X2 are each independently a functional group capable of reacting with a biologically relevant substance or a precursor of the functional group. The functional group or the precursor of the functional group in the activated polyethylene glycol derivative may be of one type or of two or more types.

[0035] R1 and R2 are each independent and have a structure that does not react with the activator in the reaction of the present invention. The structure is not particularly limited, but may have a functional group capable of reacting with a biologically relevant substance, a precursor of the functional group, or a hydrocarbon. The structure is exemplified below. Alkynyl group, substituted alkynyl group (for example, an alkynyl group substituted with a hydrocarbon group having 1 to 5 carbon atoms), alkenyl group (for example, an allyl group, a vinyl group), alkyl group, ester group, carbonate group (for example, a succinimidyl carbonate group, a p-nitrophenyl carbonate group), formyl group, isocyanate group, isothiocyanate group, epoxide group, carboxyl group, maleimidyl group, substituted maleimidyl group, dithiopyridyl group, substituted sulfonyl group (for example, a mesyl group, a tosyl group), vinylsulfonyl group, iodoacetamide group, alkylcarbonyl group, azide group, acryloyl group, sulfonyloxy group (for example, an alkylsulfonyloxy group), α-haloacetyl group

[0036] In the present invention, examples of the functional group capable of reacting with a biologically relevant substance possessed by the activated polyethylene glycol derivative or the precursor of the functional group are given below. Epoxy group, p-nitrophenyl ester group, N-hydroxysuccinimidyl ester group, mercapto group, maleimidyl group, substituted maleimidyl group, allyl group, azido group, biotin group, formyl group, amino group, mesyl group, tosyl group, phthalimidyl group, carboxyl group, acetal-protected formyl group, 9-fluorenylmethyloxycarbonyl-protected amino group, t-butoxycarbonyl-protected amino group and benzyloxycarbonyl-protected amino group.

[0037] The production method of the present invention comprises steps (A), (B) and (C). Each step will be described in turn below.

[0038] Step (A): A step of drying a powder of a polyethylene glycol compound having at least one group selected from the group consisting of a carboxyl group, a mercapto group, a hydroxyl group, and an amino group at its terminal in an atmosphere of 0°C or higher and 50°C or lower to obtain a dry powder having a moisture content of 0.10% by mass or less.

[0039] The raw material in step (A) is a polyethylene glycol compound having at least one terminal group selected from the group consisting of a carboxyl group, a mercapto group, a hydroxyl group, and an amino group. This polyethylene glycol compound is preferably PEG having a structure as shown in formula (4). [ka]

[0040] In formula (4), W1 and W2 are each independently a carboxyl group, a mercapto group, a hydroxyl group, or an amino group. The other symbols are the same as defined in formula (2).

[0041] The polyethylene glycol compound is in the form of a powder or granule that can be dried. The drying method is not particularly limited, but examples include drying under reduced pressure and drying by circulating dry gas. The average particle size of the powder or granule, as analyzed by a sieving method, is preferably 0.1 μm or more and 10 mm or less, more preferably 0.1 μm or more and 1 mm or less.

[0042] The container used in the method of the present invention is capable of drying the powdered polyethylene glycol compound and adding a solvent to the dried powdered polyethylene glycol derivative without exposing it to the atmosphere. Here, "without exposing it to the atmosphere" means that the container is sealed or filled with an inert gas to create a positive pressure inside the container with the inert gas, or the container is placed in an apparatus to create a sealed state and the apparatus is filled with an inert gas or filled with an inert gas to create a positive pressure inside the apparatus with the inert gas, thereby preventing contact with the atmosphere.

[0043] The moisture content of the powder or grain after drying is preferably 0.10% by mass or less. When drying powder or granules by reduced pressure drying, the pressure is preferably −0.01 MPaG or less and −1.0 MPaG or more, and more preferably −0.1 MPaG or less and −1.0 MPaG or more. The atmosphere during reduced pressure drying is not particularly limited, but an inert gas such as nitrogen or argon gas is preferable. When drying powder or granules by circulating a dry gas, the type of gas is not particularly limited, but an inert gas such as nitrogen or argon gas is preferable. The temperature for drying the powder or granules is not particularly limited, but any temperature below the melting point of the powder or granules of the polyethylene glycol compound is applicable, and the temperature is preferably from 0°C to 50°C, and more preferably from 15°C to 35°C.

[0044] Step (B): A step of adding an organic solvent having a water content of 200 ppm or less by mass to the dry powder or granule obtained in step (A) to dissolve the dry powder or granule in the organic solvent to obtain a solution.

[0045] When an organic solvent having a water content of 200 ppm or less is added to a dry powder and granule to dissolve the powder and granule to obtain a solution, the method of adding the organic solvent is not particularly limited. It is sufficient that the organic solvent can be added to a container without exposing the powder and granule of the polyethylene glycol derivative to the outside air. Examples of the method of adding the organic solvent include pump transfer, pressurized transfer, and reduced pressure transfer.

[0046] The water content of the organic solvent used in steps (B) and (C) is 200 ppm or less, preferably 150 ppm or less, and more preferably 100 ppm or less. There is no particular lower limit for this water content, and it may be 0 ppm.

[0047] The organic solvent used in the present invention is preferably an aprotic solvent that does not react with the activator. Exemplary solvents include toluene, benzene, ethyl acetate, dimethylformamide, dimethylsulfoxide, diethyl ether, methyl tert-butyl ether, tetrahydrofuran, acetonitrile, acetone, chloroform, dichloromethane, etc. The necessary conditions for the solvent in the present invention are that PEG dissolves, the reaction proceeds, the activator is not inactivated, and the functional group after the reaction is not decomposed. Lower alcohols such as methanol and ethanol, which are generally used as reaction solvents, are not preferred because they are highly likely to decompose the activator or the functional group after the reaction.

[0048] Step (C): A step of reacting the polyethylene glycol compound contained in the solution obtained in step (B) with an activator to obtain an activated polyethylene glycol derivative.

[0049] The activator reacts with one or more groups selected from the group consisting of a carboxyl group, a mercapto group, a hydroxyl group and an amino group of a polyethylene glycol compound to produce an activated polyethylene glycol derivative having at its terminal a functional group capable of reacting with a biologically relevant substance or a precursor of the functional group.

[0050] Suitable examples of the activator include the following. One or more compounds selected from the group consisting of disuccinimidyl carbonate, p-nitrophenyl chloroformate, di(1-benzotriazolyl) carbonate, trichlorophenyl chloroformate, p-nitrophenyl succinimidyl carbonate, p-nitrophenyl 1-benzotriazolyl carbonate, pentafluorophenyl chloroformate, 1,1'-carbonyldiimidazole, succinic anhydride, glutaric anhydride, methanesulfonyl halide, trifluoromethanesulfonyl halide, p-toluenesulfonyl halide, 6-alkyl halide hexanoates, azodicarboxylates, N,N'-dicyclohexylcarbodiimide, and N-hydroxysuccinimide.

[0051] In the reaction of step (C), a catalyst such as a base may be used as a reaction accelerator, and the base may be either an inorganic base or an organic base.

[0052] Examples of the base include salts such as hydroxides, carbonates, bicarbonates, acetates, citrates, phosphates, borates, citrates, phthalates, tartrates, or lactates of alkali metals and alkaline earth metals, or amine compounds. Exemplary salts include sodium carbonate, sodium bicarbonate, sodium acetate, etc. As for amine compounds, since primary amines and secondary amines may react with the activator or the functional group after the reaction, tertiary amines are more preferred. Exemplary bases as tertiary amines include triethylamine, N-methylmorpholine, N-phenylmorpholine, N,N-diisopropylethylamine, pyridine, 2,6-lutidine, 4-dimethylaminopyridine, 1,4-diazabicyclo[2.2.2]octane, diazabicycloundecene, etc. When using salts, since the salts may contain moisture, they may be added together with the powder of the polyethylene glycol compound at the time of step (A) and dried.

Examples

[0053] Hereinafter, the present invention will be described more specifically with reference to examples. For the measurement of the GPC polydispersity of the polyethylene glycol derivative, the following analysis method A was used. For the measurement of the activation rate of the polyethylene glycol derivative, the following analysis method B was used. For the measurement of the moisture content of the polyethylene glycol derivative, the following analysis method C was used.

[0054] <Analysis method for GPC polydispersity> (Analysis method A) GPC system: Prominence manufactured by Shimadzu Corporation Detector: Refractive index detector RID-20A manufactured by Shimadzu Corporation GPC column: Two PL gel MIXED-D columns manufactured by Agilent Technologies connected in series Column oven temperature: 65 °C Eluent: 10mmol / L lithium bromide in N,N-dimethylformamide Flow rate: 0.7mL / min Sample concentration: 1mg / mL Injection volume: 0.1mL Calibration standard: Agilent Technologies Polymer Standards for GPC of PEG with molecular weights of 600 to 70,000 Data analysis: Shimadzu Lab Solution

[0055] <How to analyze activation rate> The activation rate was analyzed by proton nuclear magnetic resonance (1H-NMR). (Analysis method B) 1H-NMR device: JNM-ECA600 manufactured by JEOL Measurement temperature: 25℃ Measurement solvent: deuterated chloroform manufactured by Kanto Chemical Co., Ltd. Sample concentration: 25mg / mL Measured nuclide: 1H Number of times: 64 to 256 Data analysis: JEOL ALICE2

[0056] <Method of moisture value analysis> The moisture content was measured using a Karl Fischer moisture meter. (Analysis method C) Karl Fischer moisture meter: Kyoto Electronics Manufacturing Co., Ltd. MKC-501 Karl Fischer reagent: Honeywell Hydranal Coulter AG (anode), Honeywell Hydranal Coulter CG (cathode) Measurement temperature: 25℃ Measurement amount: 1g

[0057] <Experimental Example 1> In order to confirm the hygroscopicity of powder particles of polyethylene glycol compounds, the following study was carried out. The powder (Mw 2,000 Daltons, reactive functional group: one hydroxyl group, 27.8 mg) of the raw material (polyethylene glycol compound) represented by formula (5) was subjected to moisture adsorption / desorption measurement using a Hiden Isochema IGA sorp. As a pretreatment, the powder of the polyethylene glycol compound was placed in a SUS mesh holder and dried for 5 hours at 25°C and 0% RH to obtain a dry powder.

[0058] 27.46 mg of the dry powder was left to stand for 1 hour in an environment controlled at 25°C and at a given relative humidity, and the mass after standing was measured. The measurement results are shown in Table 1 and Figure 1. As a result, it was revealed that the polyethylene glycol compound dry powder particles absorb moisture and increase in mass with an increase in relative humidity. In addition, it was revealed that the polyethylene glycol compound powder particles absorb moisture immediately after the increase in relative humidity, and are strongly affected by the environmental temperature and humidity.

[0059] Therefore, when a powder of a polyethylene glycol compound is reacted with an activator to obtain a desired activated polyethylene glycol derivative, if a powder of a polyethylene glycol compound that has absorbed moisture is used as a raw material, there is a high possibility that the progress of the reaction will be hindered.

[0060] [ka]

[0061] [Table 1]

[0062] <Experimental Example 2> The following study was carried out to confirm the change in quality of a polyethylene glycol compound when azeotropic distillation was carried out to dry powder particles of the polyethylene glycol compound.

[0063] A 300 mL four-neck round-bottom flask equipped with a mechanical stirrer, a Dimroth condenser, a water content receiver, a thermometer, and a nitrogen inlet tube was charged with a powder of a polyethylene glycol compound represented by formula (6) (Mw: 40,000 Daltons, reactive functional groups: two hydroxyl groups, 10 g, water content: 1.1% by mass) and toluene (70 g, water content: 68 ppm), which were dissolved at 50°C using a mantle heater while stirring under nitrogen. Then, azeotropic distillation was performed at 115°C using a mantle heater. Table 2 shows the relationship between the azeotropic distillation time and the GPC polydispersity (Mw / Mn) using analysis method A.

[0064] As a result, it was revealed that the polyethylene glycol compound deteriorates and the polydispersity increases with the extension of the azeotropic distillation time. When drying by azeotropic distillation, it was found that the larger the production scale, the longer the heating time until the temperature at which azeotropic distillation can be reached is extended, and therefore the deterioration of the polyethylene glycol compound is accelerated and the polydispersity increases.

[0065] [ka]

[0066] [Table 2]

[0067] <Example 1> A powder of a polyethylene glycol compound represented by formula (6) (Mw: 40,000, reactive functional groups: two hydroxyl groups, 10 g, 250 μmol, moisture value: 1.1 mass%, GPC polydispersity: 1.11) was placed in a 300 mL four-neck round-bottom flask equipped with a mechanical stirrer, an L-shaped tube connected to a vacuum pump, a check valve, a three-way cock connected to a nitrogen line, and a glass stopper, and the pressure was reduced to -0.1 MPaG or less using a vacuum pump. The mixture was dried for 3 hours to obtain a dry powder with a moisture value of 0.01 mass% (step (A)).

[0068] After step (A), the pressure was restored with nitrogen, and toluene (70 g, moisture content: 129 ppm) was added using a glass syringe and needle while maintaining the dry powder under a nitrogen atmosphere and preventing it from coming into contact with the outside air. The mixture was then heated to 40°C and stirred to dissolve, obtaining a solution (step (B)).

[0069] To the obtained solution, triethylamine (TEA, 58 mg, 1150 mmol) as a base catalyst and methanesulfonyl chloride (57 mg, 1000 mmol) as an activator were added, and the mixture was reacted at 40°C for 3 hours under nitrogen. Ethyl acetate (500 g) was added to the reaction solution after the reaction, and the mixture was mixed at 40°C. After adding hexane (500 g) and crystallizing at 25°C, the mixture was filtered by suction to obtain crystals. The obtained crystals were added with ethyl acetate (500 g), dissolved at 40°C, and crystallized at 25°C by adding hexane (500 g), and the operation was repeated to remove low molecular weight impurities, and then dried under reduced pressure to obtain a polyethylene glycol derivative represented by formula (7) (step (C)).

[0070] The polyethylene glycol derivative obtained in the step (C) was subjected to 1H-NMR measurement with an accumulation number of 256 times, and it was confirmed that the activation rate was 85%. GPC measurement was performed to confirm that the polydispersity was 1.10. Moisture measurement was performed to confirm that the moisture value was 0.2% by mass.

[0071] [ka]

[0072] <Example 2> A powder of a polyethylene glycol compound represented by formula (8) (Mw: 43,000 daltons, reactive functional group: one hydroxyl group, 10 g, 233 μmol, moisture value: 0.1 mass%, GPC polydispersity: 1.04) was placed in a 100 mL three-neck round-bottom flask equipped with a mechanical stirrer, an L-shaped tube connected to a vacuum pump, and a three-way cock connected to a check valve and a nitrogen line, and the pressure was reduced to -0.1 MPaG or less using a vacuum pump. The mixture was dried for 1 hour to obtain a dry powder with a moisture value of 0.02 mass% (step (A)).

[0073] After step (A), the pressure was restored with nitrogen, and dichloromethane (70 g, moisture content: 42 ppm) was charged using a glass syringe and needle to the dry powder particles under a nitrogen atmosphere without exposing them to air, and the powder was dissolved by stirring at 25°C to obtain a solution (step (B)).

[0074] To the solution obtained in step (B), disuccinimidyl carbonate (DSC, 918 mg, 3584 μmol) as an activator and pyridine (434 μL, 5233 μmol) as a base catalyst were added, and the mixture was reacted at 27 ° C. for 15 hours under nitrogen. Ethyl acetate (500 g) was added to the solution after the reaction, mixed at 40 ° C., hexane (500 g) was added, crystallization was performed at 25 ° C., and then suction filtration was performed to obtain crystals. Ethyl acetate (500 g) was added to the obtained crystals, dissolved at 40 ° C., hexane (500 g) was added, and crystallization was performed at 25 ° C. by repeatedly performing the operation of removing low molecular weight impurities, and then drying under reduced pressure to obtain an activated polyethylene glycol derivative represented by formula (9) (step (C)).

[0075] The activated polyethylene glycol derivative obtained in the step (C) was subjected to 1H-NMR measurement with an accumulation number of 256 times, and it was confirmed that the activation rate was 98%. It was also confirmed by GPC measurement that the polydispersity was 1.04. It was also confirmed by moisture measurement that the moisture value was 0.3% by mass.

[0076] [ka]

[0077] [ka]

[0078] <Example 3> A 100 mL three-neck round-bottom flask equipped with a mechanical stirrer, an L-shaped tube connected to a vacuum pump, and a three-way cock connected to a check valve and a nitrogen line was charged with a powder of a polyethylene glycol compound represented by formula (5) (Mw: 2,000 daltons, reactive functional group: one hydroxyl group, 5 g, 2.5 mmol, moisture value: 0.5 mass%, GPC polydispersity: 1.06) and sodium acetate (15 mg) as a base catalyst, and the pressure was reduced to -0.1 MPaG or less using a vacuum pump. The mixture was dried for 1 hour to obtain a dry powder with a moisture value of 0.08 mass% (step (A)).

[0079] After step (A), the pressure was restored with nitrogen, and toluene (5 g, moisture content: 67 ppm) was charged into the dry powder using a glass syringe and needle under a nitrogen atmosphere without exposing the powder to air. The mixture was then heated to 40°C and dissolved by stirring to obtain a solution (step (B)).

[0080] To the resulting solution, succinic anhydride (263 mg, 2.63 mmol) was added as an activator, and the mixture was reacted at 70° C. for 12 hours under nitrogen. Ethyl acetate (500 g) was added to the reaction solution and mixed at 40° C., hexane (500 g) was added and crystallized at 25° C., and then suction filtration was performed to obtain crystals. Ethyl acetate (500 g) was added to the resulting crystals, dissolved at 40° C., and hexane (500 g) was added and crystallized at 25° C. The procedure was repeated to remove low molecular weight impurities, and then the mixture was dried under reduced pressure to obtain an activated polyethylene glycol derivative represented by formula (10) (step (C)).

[0081] The activated polyethylene glycol derivative obtained in step (C) was subjected to 1H-NMR measurement with an accumulation number of 64 times, and it was confirmed that the activation rate was 91%. It was also confirmed by GPC measurement that the polydispersity was 1.06. It was also confirmed by moisture measurement that the moisture value was 0.3% by mass.

[0082] [ka]

[0083] <Example 4> A 100 mL three-neck round-bottom flask equipped with a mechanical stirrer, an L-shaped tube connected to a vacuum pump, and a three-way cock connected to a check valve and a nitrogen line was charged with a powder of a polyethylene glycol compound represented by formula (11) (Mw: 10,000 daltons, reactive functional groups: four amino groups, 5 g, 500 μmol, moisture value: 0.5 mass%, GPC polydispersity: 1.06) and sodium acetate (15 mg) as a base catalyst, and the pressure was reduced to -0.1 MPaG or less using a vacuum pump. The mixture was dried for 2 hours to obtain a dry powder with a moisture value of 0.07 mass% (step (A)).

[0084] After step (A), the pressure was restored with nitrogen, and toluene (5 g, moisture content: 92 ppm) was charged using a glass syringe and needle under a nitrogen atmosphere without exposing the dry powder to air, and the mixture was heated to 40°C and stirred to dissolve, obtaining a solution (step (B)).

[0085] To the solution obtained in step (B), succinic anhydride (210 mg, 525 μmol) was added as an activator, and the mixture was reacted at 70° C. for 12 hours under nitrogen. Ethyl acetate (500 g) was added to the reaction solution after the reaction, and the mixture was mixed at 40° C., hexane (500 g) was added, and crystallization was performed at 25° C., followed by suction filtration to obtain crystals. The crystals obtained were added with ethyl acetate (500 g), dissolved at 40° C., and hexane (500 g) was added, and crystallization was performed at 25° C. by repeating the above steps to remove low molecular weight impurities, and then dried under reduced pressure to obtain an activated polyethylene glycol derivative represented by formula (12) (step (C)).

[0086] The activated polyethylene glycol derivative obtained in step (C) was subjected to 1H-NMR measurement with an accumulation number of 128 times, and it was confirmed that the activation rate was 95%. It was also confirmed by GPC measurement that the polydispersity was 1.05. It was also confirmed by moisture measurement that the moisture value was 0.5% by mass.

[0087] [ka]

[0088] [ka]

[0089] <Example 5> A powder of the polyethylene glycol compound represented by formula (5) (Mw: 2,000 daltons, reactive functional group: one hydroxyl group, 1 g, 500 μmol, moisture value: 0.5% by mass, GPC polydispersity: 1.03) was placed in a 20 mL screw-cap glass bottle, placed in a glove box, and dried by stirring with a spatula for 1 hour while circulating dry nitrogen, to obtain a dry powder with a moisture value of 0.08% by mass (step (A)).

[0090] After step (A), a stirrer was placed in a screw-cap glass bottle in a glove box, and toluene (2 g, moisture value: 62 ppm) and chloroform (18 g, moisture value: 68 ppm) were charged into the bottle. The bottle was then closed and taken out of the glove box. The bottle was then stirred with a magnetic stirrer at 25°C to dissolve the contents, thereby obtaining a solution (step (B)).

[0091] To the obtained solution, phthalimide (129 mg, 875 μmol), triphenylphosphine (TPP, 230 mg, 875 μmol) and diisopropyl azodicarboxylate (DIAD, 152 mg, 750 mol) were added, and the mixture was reacted at 25 ° C. for 2 hours and 30 minutes under nitrogen. Ethyl acetate (100 g) was added to the reaction solution after the reaction, and the mixture was mixed at 40 ° C., hexane (100 g) was added, and crystallization was performed at 25 ° C., and then the mixture was suction filtered to obtain crystals. The obtained crystals were added with ethyl acetate (100 g), dissolved at 40 ° C., and hexane (100 g) was added, and crystallization was performed at 25 ° C. by repeating the above operations to remove low molecular weight impurities, and then dried under reduced pressure to obtain an activated polyethylene glycol derivative represented by formula (13) (step (C)).

[0092] The activated polyethylene glycol derivative obtained in the step (C) was subjected to 1H-NMR measurement with an accumulation number of 64 times, and it was confirmed that the activation rate was 88%. It was also confirmed by GPC measurement that the polydispersity was 1.03. It was also confirmed by moisture measurement that the moisture value was 0.5% by mass.

[0093] [ka]

[0094] <Example 6> A powder of a polyethylene glycol compound represented by formula (6) (Mw: 40,000 daltons, reactive functional groups: two hydroxyl groups, 10 g, 250 μmol, moisture value: 1.1 mass%, GPC polydispersity: 1.11) was placed in a 100 mL three-neck round-bottom flask equipped with a mechanical stirrer, an L-shaped tube connected to a vacuum pump, and a three-way cock connected to a check valve and a nitrogen line, and the pressure was reduced to -0.1 MPaG or less using a vacuum pump. The mixture was dried for 1 hour to obtain a dry powder with a moisture value of 0.03 mass% (step (A)).

[0095] After step (A), the pressure was restored with nitrogen, and dichloromethane (70 g, moisture content: 51 ppm) was charged using a glass syringe and needle under a nitrogen atmosphere to the dry powder particles without exposing them to air, and the mixture was dissolved by stirring at 25°C to obtain a solution (step (B)).

[0096] To the solution obtained in step (B), disuccinimidyl carbonate (DSC, 643 mg, 2510 μmol) as an activator and pyridine (303 μL, 3750 μmol) as a base catalyst were added, and the mixture was reacted under nitrogen at 25 ° C. for 16 hours. Ethyl acetate (500 g) was added to the solution after the reaction, mixed at 40 ° C., hexane (500 g) was added, crystallization was performed at 25 ° C., and then suction filtration was performed to obtain crystals. Ethyl acetate (500 g) was added to the obtained crystals, dissolved at 40 ° C., hexane (500 g) was added, and crystallization was performed at 25 ° C. by repeatedly performing the operation of removing low molecular weight impurities, and then drying under reduced pressure to obtain an activated polyethylene glycol derivative represented by formula (14) (step (C)).

[0097] The activated polyethylene glycol derivative obtained in the step (C) was subjected to 1H-NMR measurement with an accumulation number of 256 times, and it was confirmed that the activation rate was 100%. It was also confirmed by GPC measurement that the polydispersity was 1.11. It was also confirmed by moisture measurement that the moisture value was 0.3% by mass.

[0098] [ka]

[0099] <Example 7> A powder of a polyethylene glycol compound represented by formula (15) (Mw: 80,000 daltons, reactive functional group: one hydroxyl group, 2 g, 25 μmol, moisture value: 1.0 mass%, GPC polydispersity: 1.06) was placed in a 100 mL three-neck round-bottom flask equipped with a mechanical stirrer, an L-shaped tube connected to a vacuum pump, and a three-way cock connected to a check valve and a nitrogen line, and the pressure was reduced to -0.1 MPaG or less using a vacuum pump. The mixture was dried for 3 hours to obtain a dry powder with a moisture value of 0.08 mass% (step (A)).

[0100] After step (A), the pressure was restored with nitrogen, and dichloromethane (10 g, moisture content: 106 ppm) was charged using a glass syringe and needle under a nitrogen atmosphere to the dry powder particles without exposing them to air, and the mixture was dissolved by stirring at 25°C to obtain a solution (step (B)).

[0101] To the solution obtained in step (B), disuccinimidyl carbonate (DSC, 96 mg, 375 μmol) as an activator and pyridine (46 μL, 569 μmol) as a base catalyst were added, and the mixture was reacted at 25 ° C. for 2 hours under nitrogen. Ethyl acetate (500 g) was added to the solution after the reaction, mixed at 40 ° C., hexane (500 g) was added, crystallization was performed at 25 ° C., and then suction filtration was performed to obtain crystals. Ethyl acetate (500 g) was added to the obtained crystals, dissolved at 40 ° C., hexane (500 g) was added, and crystallization was performed at 25 ° C. by repeatedly performing the operation of removing low molecular weight impurities, and then drying under reduced pressure to obtain an activated polyethylene glycol derivative represented by formula (16) (step (C)).

[0102] The activated polyethylene glycol derivative obtained in the step (C) was subjected to 1H-NMR measurement with an accumulation number of 256 times, and it was confirmed that the activation rate was 100%. It was also confirmed by GPC measurement that the polydispersity was 1.06. It was also confirmed by moisture measurement that the moisture value was 0.3% by mass.

[0103] [ka]

[0104] [ka]

[0105] <Example 8> A powder of a polyethylene glycol compound represented by formula (17) (Mw: 40,000 daltons, reactive functional groups: eight hydroxyl groups, 2 g, 50 μmol, moisture value: 0.8 mass%, GPC polydispersity: 1.07) was placed in a 100 mL three-neck round-bottom flask equipped with a mechanical stirrer, an L-shaped tube connected to a vacuum pump, and a three-way cock connected to a check valve and a nitrogen line, and the pressure was reduced to -0.1 MPaG or less using a vacuum pump. The mixture was dried for 3 hours to obtain a dry powder with a moisture value of 0.09 mass% (step (A)).

[0106] After step (A), the pressure was restored with nitrogen, and dichloromethane (10 g, moisture content: 104 ppm) was charged using a glass syringe and needle under a nitrogen atmosphere to the dry powder particles without exposing them to air, and the mixture was dissolved by stirring at 25°C to obtain a solution (step (B)).

[0107] To the solution obtained in step (B), disuccinimidyl carbonate (DSC, 206 mg, 804 μmol) as an activator and pyridine (97 μL, 1199 μmol) as a base catalyst were added, and the mixture was reacted at 25 ° C. for 2 hours under nitrogen. Ethyl acetate (500 g) was added to the solution after the reaction, mixed at 40 ° C., hexane (500 g) was added, crystallization was performed at 25 ° C., and then suction filtration was performed to obtain crystals. Ethyl acetate (500 g) was added to the obtained crystals, dissolved at 40 ° C., hexane (500 g) was added, and crystallization was performed at 25 ° C. by repeatedly performing the operation of removing low molecular weight impurities, and then drying under reduced pressure to obtain an activated polyethylene glycol derivative represented by formula (18) (step (C)).

[0108] The activated polyethylene glycol derivative obtained in the step (C) was subjected to 1H-NMR measurement with an accumulation number of 256 times, and it was confirmed that the activation rate was 99%. It was also confirmed by GPC measurement that the polydispersity was 1.07. It was also confirmed by moisture measurement that the moisture value was 0.3% by mass.

[0109] [ka]

[0110] [ka]

[0111] <Example 9> A 100 mL three-neck round-bottom flask equipped with a mechanical stirrer, an L-shaped tube connected to a vacuum pump, and a three-way cock connected to a check valve and a nitrogen line was charged with a powder of a polyethylene glycol compound represented by formula (5) (Mw: 2,000 daltons, reactive functional group: one hydroxyl group, 10 g, 5.0 mmol, moisture value: 0.5 mass%, GPC polydispersity: 1.03) and sodium acetate (3 mg) as a base catalyst, and the pressure was reduced to -0.1 MPaG or less using a vacuum pump. The mixture was dried for 3 hours to obtain a dry powder with a moisture value of 0.03 mass% (step (A)).

[0112] After step (A), the pressure was restored with nitrogen, and 4-methyltetrahydropyran (MTHP, 10 g, moisture value: 94 ppm) was charged into the dry powdery granules using a glass syringe and needle under a nitrogen atmosphere without exposing the powder to air, and the mixture was heated to 40°C and stirred to dissolve, thereby obtaining a solution (step (B)).

[0113] To the resulting solution, succinic anhydride (528 mg, 5.28 mmol) was added as an activator, and the mixture was reacted at 70° C. for 12 hours under nitrogen. Ethyl acetate (500 g) was added to the reaction solution and mixed at 40° C., hexane (500 g) was added and crystallized at 25° C., and then suction filtration was performed to obtain crystals. Ethyl acetate (500 g) was added to the resulting crystals, dissolved at 40° C., and hexane (500 g) was added and crystallized at 25° C. The procedure was repeated to remove low molecular weight impurities, and the mixture was dried under reduced pressure to obtain an activated polyethylene glycol derivative represented by formula (10) (step (C)).

[0114] The activated polyethylene glycol derivative obtained in step (C) was subjected to 1H-NMR measurement with an accumulation number of 64 times, and it was confirmed that the activation rate was 85%. It was also confirmed by GPC measurement that the polydispersity was 1.03. It was also confirmed by moisture measurement that the moisture value was 0.4% by mass.

[0115] <Example 10> A 100 mL three-neck round-bottom flask equipped with a mechanical stirrer, an L-shaped tube connected to a vacuum pump, and a three-way cock connected to a check valve and a nitrogen line was charged with a powder of a polyethylene glycol compound represented by formula (19) (Mw: 5,000 daltons, reactive functional group: one carbonyl group, 2 g, 400 μmol, moisture value: 0.9 mass%, GPC polydispersity: 1.03), and the pressure was reduced to -0.1 MPaG or less using a vacuum pump. The mixture was dried for 3 hours to obtain a dry powder with a moisture value of 0.02 mass% (step (A)).

[0116] After step (A), the pressure was restored with nitrogen, and toluene (10 g, moisture content: 83 ppm) was charged into the dry powder using a glass syringe and needle under a nitrogen atmosphere without exposing the powder to air. The mixture was then heated to 40°C and stirred to dissolve, obtaining a solution (step (B)).

[0117] To the obtained solution, activators N,N'-dicyclohexylcarbodiimide (DCC, 165 mg, 800 μmol) and N-hydroxysuccinimide (NHS, 101 mg, 878 μmol) were added, and the mixture was reacted at 40 ° C. for 3 hours under nitrogen. Ethyl acetate (500 g) was added to the reaction solution after the reaction, and the mixture was mixed at 40 ° C., and hexane (500 g) was added to the filtrate obtained by suction filtration, and crystallization was performed at 25 ° C., and then suction filtration was performed to obtain crystals. Ethyl acetate (500 g) was added to the obtained crystals, and the mixture was dissolved at 40 ° C., and hexane (500 g) was added and crystallization was performed at 25 ° C. The operation was repeated to remove low molecular weight impurities, and the mixture was dried under reduced pressure to obtain an activated polyethylene glycol derivative represented by formula (20) (step (C)).

[0118] The activated polyethylene glycol derivative obtained in step (C) was subjected to 1H-NMR measurement with an accumulation number of 128 times, and it was confirmed that the activation rate was 99%. It was also confirmed by GPC measurement that the polydispersity was 1.03. It was also confirmed by moisture measurement that the moisture value was 0.2% by mass.

[0119] [ka]

[0120] [ka]

[0121] <Example 11> A 100 mL three-neck round-bottom flask equipped with a mechanical stirrer, an L-shaped tube connected to a vacuum pump, and a three-way cock connected to a check valve and a nitrogen line was charged with a powder of a polyethylene glycol compound represented by formula (5) (Mw: 2,000 daltons, reactive functional group: one hydroxyl group, 10 g, 5.0 mmol, moisture value: 0.5 mass%, GPC polydispersity: 1.03), and the pressure was reduced to -0.1 MPaG or less using a vacuum pump. The mixture was dried for 3 hours to obtain a dry powder with a moisture value of 0.01 mass% (step (A)).

[0122] After step (A), the pressure was restored with nitrogen, and toluene (11 g, moisture content: 93 ppm) was charged into the dry powder using a glass syringe and needle under a nitrogen atmosphere without exposing the powder to air. The mixture was heated to 40°C and stirred to dissolve, thereby obtaining a solution (step (B)).

[0123] To the obtained solution, p-nitrophenyl chloroformate (1.11 g, 5.5 mmol) as an activator and triethylamine (TEA, 837 μL, 6.0 μmol) as a base catalyst were added, and the mixture was reacted at 60° C. for 2 hours under nitrogen. Ethyl acetate (500 g) was added to the reaction solution after the reaction, and the mixture was mixed at 40° C., hexane (500 g) was added, and crystallization was performed at 25° C., and then the mixture was suction filtered to obtain crystals. The crystals obtained were added with ethyl acetate (500 g), dissolved at 40° C., and hexane (500 g) was added, and crystallization was performed at 25° C. by repeating the above steps to remove low molecular weight impurities, and then the mixture was dried under reduced pressure to obtain an activated polyethylene glycol derivative represented by formula (21) (step (C)).

[0124] The activated polyethylene glycol derivative obtained in step (C) was subjected to 1H-NMR measurement with an accumulation number of 64 times, and it was confirmed that the activation rate was 91%. It was also confirmed by GPC measurement that the polydispersity was 1.03. It was also confirmed by moisture measurement that the moisture value was 0.3% by mass.

[0125] [ka]

[0126] In order to confirm the effect on the reaction when the powder particles of the polyethylene glycol compound absorb moisture, the following study was carried out.

[0127] <Comparative Example 1> A 300 mL four-neck round-bottom flask equipped with a mechanical stirrer, a Dimroth condenser, a thermometer, and a nitrogen inlet tube was charged with a powder of a polyethylene glycol compound represented by formula (6) (Mw: 40,000 daltons, reactive functional groups: two hydroxyl groups, 10 g, 250 μmol, moisture value: 1.1 mass%, GPC polydispersity: 1.11), and toluene (70 g, moisture value: 41 ppm) was added. The mixture was then heated to 40° C. in a water bath and dissolved with stirring to obtain a solution.

[0128] To the obtained solution, triethylamine (TEA, 58 mg, 1150 μmol) and methanesulfonyl chloride (MsCl, 57 mg, 1000 μmol) were added, and the mixture was reacted at 40° C. for 3 hours under nitrogen. Ethyl acetate (500 g) was added to the reaction solution after the reaction, and the mixture was mixed at 40° C., hexane (500 g) was added, and crystallization was performed at 25° C., and then the mixture was suction filtered to obtain crystals. The crystals obtained were added with ethyl acetate (500 g), dissolved at 40° C., and hexane (500 g) was added, and crystallization was performed at 25° C. by repeating the above steps to remove low molecular weight impurities, and then the mixture was dried under reduced pressure to obtain the activated polyethylene glycol derivative represented by formula (7).

[0129] The obtained activated polyethylene glycol derivative was subjected to 1H-NMR measurement with an accumulation number of 256 times, and it was confirmed that the activation rate was very low at 25%. GPC measurement confirmed that the polydispersity was 1.11. Moisture measurement confirmed that the moisture value was 0.2 mass%.

[0130] <Comparative Example 2> A 100 mL three-neck round-bottom flask equipped with a mechanical stirrer, a Dimroth condenser, a thermometer, and a nitrogen inlet tube was charged with a powder of a polyethylene glycol compound represented by formula (6) (Mw: 40,000 daltons, reactive functional groups: two hydroxyl groups, 10 g, 250 μmol, moisture value: 0.8 mass%, GPC polydispersity: 1.06), and dichloromethane (72 g, moisture value: 104 ppm) was added thereto, followed by stirring at 25° C. to dissolve the mixture, thereby obtaining a solution.

[0131] To the obtained solution, disuccinimidyl carbonate (DSC, 643 mg, 2510 μmol) as an activator and pyridine (303 μL, 3750 μmol) as a base catalyst were added, and the mixture was reacted at 25 ° C. for 18 hours under nitrogen. Ethyl acetate (500 g) was added to the reaction solution after the reaction, and the mixture was mixed at 40 ° C., hexane (500 g) was added, and crystallization was performed at 25 ° C., and then the mixture was filtered by suction to obtain crystals. The obtained crystals were added with ethyl acetate (500 g), dissolved at 40 ° C., and hexane (500 g) was added, and crystallization was performed at 25 ° C. by repeating the above operations to remove low molecular weight impurities, and then dried under reduced pressure to obtain an activated polyethylene glycol derivative represented by formula (14).

[0132] The obtained activated polyethylene glycol derivative was subjected to 1H-NMR measurement with an accumulation number of 256 times, and it was confirmed that the activation rate was very low at 61%. GPC measurement confirmed that the polydispersity was 1.06. Moisture measurement confirmed that the moisture value was 0.3% by mass.

[0133] Table 3 shows the results of Example 1 and Comparative Example 1, and Example 6 and Comparative Example 2. As shown in Table 3, in Comparative Examples 1 and 2, it was shown that the activation rate of the activated polyethylene glycol derivative was significantly decreased.

[0134] [Table 3]

[0135] The results of Examples 1 to 11 are shown in Table 4. As shown in Table 4, according to the present invention, polyethylene glycol derivatives with high activation purity could be produced without increasing the polydispersity even under each reaction condition.

[0136] [Table 4]

Claims

1. A method for producing an activated polyethylene glycol derivative having, at its terminal, a functional group capable of reacting with a biologically relevant substance or a precursor of said functional group, the method comprising the following steps (A), (B) and (C): Step (A): A step of drying a powder of a polyethylene glycol compound having at least one group selected from the group consisting of a carboxyl group, a mercapto group, a hydroxyl group, and an amino group at its terminal in an atmosphere of 0° C. or higher and 50° C. or lower to obtain a dry powder having a moisture content of 0.10% by mass or less. Step (B): A step of adding an organic solvent having a water content of 200 ppm or less by mass to the dry powder or grain obtained in the step (A) to dissolve the dry powder or grain in the organic solvent to obtain a solution. Step (C): A step of reacting the polyethylene glycol compound contained in the solution obtained in step (B) with an activator to obtain an activated polyethylene glycol derivative.

2. 2. The method for producing an activated polyethylene glycol derivative according to claim 1, wherein the organic solvent is an aprotic solvent.

3. 3. The method for producing an activated polyethylene glycol derivative according to claim 1, wherein the powder or granule in step (A) has an average particle size of 0.1 μm or more and 10 mm or less.

4. 3. The method for producing an activated polyethylene glycol derivative according to claim 1 or 2, wherein the polyethylene glycol compound in the step (A) has a number average molecular weight of 2,000 daltons or more and 80,000 daltons or less.

5. The method for producing a polyethylene glycol derivative according to claim 1 or 2, wherein the activated polyethylene glycol derivative is represented by the following formula (1): PEG-X...(1) (In formula (1), PEG is a polyethylene glycol moiety having a linear or branched structure; X is a functional group or a precursor of a functional group capable of reacting with a biologically relevant substance.

6. The method for producing a polyethylene glycol derivative according to claim 1 or 2, characterized in that the activator is one or more compounds selected from the group consisting of disuccinimidyl carbonate, p-nitrophenyl chloroformate, di(1-benzotriazolyl) carbonate, trichlorophenyl chloroformate, p-nitrophenyl succinimidyl carbonate, p-nitrophenyl 1-benzotriazolyl carbonate, pentafluorophenyl chloroformate, 1,1'-carbonyldiimidazole, succinic anhydride, glutaric anhydride, methanesulfonyl halide, trifluoromethanesulfonyl halide, p-toluenesulfonyl halide, 6-alkyl halide hexanoate, azodicarboxylate, N,N'-dicyclohexylcarbodiimide and N-hydroxysuccinimide.

Citation Information

Patent Citations

  • Multi-arm polyethylene glycol derivative, and intermediate and production method thereof

    JP2013227543A

Cited By

  • Activated branched polyethylene glycol derivative having active group at terminal and method for producing same

    WO2026034359A1