Method for recovering electrode of power storage device, method for manufacturing power storage device, and electric storage device
Mechanical treatment of secondary battery electrodes by cutting or laser irradiation addresses the challenge of restoring performance and minimizing environmental impact, achieving efficient recovery and reuse of electrodes in power storage devices.
Patent Information
- Application Number
- JP2023056970
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-31
- Publication Date
- 2024-10-15
AI Technical Summary
Existing methods for recovering secondary battery electrodes fail to sufficiently restore performance while minimizing environmental impact, as cleaning the electrodes leads to surface layer deterioration.
A method involving mechanical treatment to remove a portion of the electrode's surface layer, such as cutting or laser irradiation, to expose a new surface without separating the active material, thereby restoring electrode function while reducing environmental burden.
The method effectively restores electrode performance by removing less than 20% of the electrode thickness, maintaining shape and reducing environmental impact, and allows for the reuse of electrodes in power storage devices.
Smart Images

Figure 2024144832000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for restoring electrodes of an electricity storage device, a method for manufacturing an electricity storage device, and an electricity storage device. [Background technology]
[0002] In recent years, development has progressed for vehicles that run on electric motors that use electricity supplied from power storage devices (also called batteries) such as secondary batteries, such as EVs (Electric Vehicles) and HEVs (Hybrid Electric Vehicles). Batteries that are determined to have deteriorated through use are collected and subjected to recycling processes, such as removing the electrodes, separating them from the active material, and reconstructing the cells, and are then used as regenerated batteries. In recent years, research and development has also been conducted into secondary batteries that contribute to energy efficiency, in order to ensure that more people have access to affordable, reliable, sustainable and advanced energy.
[0003] For example, Patent Document 1 discloses a technology for regenerating and reusing the electrodes of used lithium ion batteries while maintaining the shape of the coated electrodes (electrode active material layers coated on a current collector) to obtain a regenerated battery. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2012-022969 A Summary of the Invention [Problem to be solved by the invention]
[0005] However, in the technology related to secondary batteries, it is an issue to sufficiently recover the performance of the electrode while suppressing the environmental load when recovering used secondary batteries. In the technology of Patent Document 1, the electrode is washed with a polar solvent to attempt to regenerate and reuse the electrode while maintaining its shape after dismantling the battery, but there is a problem that the deteriorated layer generated on the electrode surface cannot be removed by washing alone. This may result in insufficient recovery of the performance of the electrode.
[0006] The present invention has been made in consideration of the above, and aims to provide a method for restoring an electrode of an energy storage device that can fully restore the performance of the electrode while reducing the environmental impact, a method for manufacturing an energy storage device, and an energy storage device. [Means for solving the problem]
[0007] (1) A method for recovering an electrode of a power storage device according to one embodiment of the present invention includes the steps of: A method for recovering electrodes of a used electricity storage device, comprising the steps of: a first step of removing the electrode from the used electricity storage device; a second step of removing at least a portion of the surface layer of the electrode taken out in the first step by mechanical processing; The present invention is characterized by comprising: The method for recovering an electrode of an energy storage device having the above-mentioned configuration can recover the function of the electrode by removing at least a portion of the surface layer of the electrode whose performance as an electrode has deteriorated by mechanical treatment, and can reduce the environmental load because the electrode can be recovered without separating the active material from the electrode. (2) In the method for recovering an electrode of an electricity storage device described in (1) above, The portion of the surface layer of the electrode that is removed by the mechanical treatment may be a portion from the surface of the electrode that is less than 20% of the thickness of the electrode. The method for recovering an electrode for an energy storage device having the above-mentioned configuration can, in addition to the above-mentioned effects, by removing a portion of the electrode that is less than 20% of its thickness, re-form a surface that can be used as an electrode while maintaining the shape of the electrode, thereby effectively recovering its function as an electrode. (3) In the method for recovering an electrode of an electricity storage device according to (1) or (2) above, The method further includes a calculation step of calculating an increase in thickness of the electrode before the second step, A thickness corresponding to the increase in thickness calculated in the calculating step may be removed by the mechanical treatment. The method for recovering an electrode for an energy storage device having the above-described configuration removes a thickness equivalent to the increase in thickness of the electrode, and therefore, in addition to the above-described effects, can return the thickness of the electrode to its initial state, and can restore the electrode's function to the desired performance without carrying out any further processes. (4) In the method for recovering an electrode of an electricity storage device according to any one of (1) to (3), The mechanical treatment may be a treatment for cutting at least a part of a surface layer of the electrode. The method for recovering an electrode for an electricity storage device having the above-mentioned configuration not only achieves the above-mentioned effects but also makes it possible to more efficiently expose a fresh surface of the electrode by performing removal by cutting. (5) In the method for recovering an electrode of an electricity storage device according to any one of (1) to (3), The mechanical treatment may be a treatment of heating at least a part of a surface layer of the electrode by irradiating it with a laser beam. The method for recovering an electrode for an electricity storage device having the above-described configuration heats and removes the surface layer of the electrode by irradiating it with a laser beam, thereby not only achieving the above-described effects but also more efficiently exposing a fresh surface of the electrode. (6) A method for manufacturing a power storage device according to one embodiment of the present invention includes the steps of: A method for manufacturing an electricity storage device, comprising: A first step of removing electrodes from a used electricity storage device; a second step of removing at least a portion of the surface layer of the electrode taken out in the first step by mechanical processing; a third step of assembling an electricity storage device including the electrode treated in the second step; The present invention is characterized by comprising: The method for producing an electricity storage device having the above configuration can restore the function of the electrode and can reduce the environmental load because the electrode can be restored without separating the active material from the electrode. (7) A power storage device according to one embodiment of the present invention includes: The electricity storage device is manufactured by the electricity storage device manufacturing method described in (6) above. The electricity storage device having the above-mentioned configuration is a regenerated electricity storage device in which the function as an electrode is restored by a manufacturing method that reduces the environmental load. Effect of the Invention
[0008] According to the method for recovering an electrode of an electricity storage device, the method for manufacturing an electricity storage device, and the electricity storage device of the present invention, it is possible to sufficiently recover the performance of the electrode while suppressing the environmental load associated with the manufacture of the electricity storage device. [Brief description of the drawings]
[0009] [Figure 1] FIG. 1 is a schematic diagram for explaining the basic configuration of a cell (single battery) that constitutes an electricity storage device according to an embodiment. [Diagram 2] 4 is a flow chart for explaining the overall flow of a method for recovering electrodes of an energy storage device according to an embodiment. FIG. [Diagram 3] FIG. 13 is a schematic cross-sectional view for explaining a step of cutting the negative electrode of the power storage device according to the embodiment, showing a state in which a cutting blade has entered the negative electrode active material layer. [Figure 4] FIG. 11 is a schematic cross-sectional view for explaining a step of cutting a negative electrode of an energy storage device according to an embodiment, showing a state in which a cutting blade has penetrated to a predetermined depth into a negative electrode active material layer (SEI coating). [Diagram 5] FIG. 13 is a schematic cross-sectional view for explaining a process for cutting a negative electrode of an energy storage device according to an embodiment, showing a state in which a cutting blade is inserted to a predetermined depth into a negative electrode active material layer (SEI coating) and moved in an in-plane direction. [Figure 6]FIG. 13 is a schematic cross-sectional view for explaining a step of cutting a negative electrode of an energy storage device according to an embodiment, showing a state in which a cutting blade has penetrated to a predetermined depth into a negative electrode active material layer including an SEI coating. [Figure 7] FIG. 13 is a diagram for explaining a graph for creating a calibration curve according to the embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] Hereinafter, the embodiments of the present invention will be described with reference to examples, but it is obvious that the present invention is not limited to the examples described below. In the following description, specific numerical values and materials may be exemplified, but other numerical values and materials may be applied as long as the effects of the present invention can be obtained. In addition, the components of the following embodiments can be combined with each other. In this specification, a numerical range expressed using "to" means a range including the numerical values before and after "to" as the lower and upper limits. In this specification, the term "process" includes not only an independent process, but also a process that cannot be clearly distinguished from other processes, as long as the intended purpose of the process is achieved.
[0011] (Electricity storage device) The power storage device according to the present embodiment is not particularly limited as long as it is a power storage device that can be regenerated and reused. For example, it may be a secondary battery such as a lithium ion battery. When the power storage device according to the present embodiment is classified by its shape and structure, it can be applied to any of the conventionally known shapes and structures such as a wound (cylindrical) battery and a laminated (flat) battery.
[0012] The power storage device of this embodiment is a secondary battery capable of repeating charging and discharging, such as a lithium ion battery. The secondary battery constituting the power storage device may be, for example, a lead storage battery, a nickel-metal hydride battery, a sodium ion battery, a capacitor such as an electric double layer capacitor, or a composite battery combining a secondary battery and a capacitor. The power storage device may be, for example, a cassette-type battery pack that is detachably mounted on a vehicle or the like. In this case, the power storage device stores power introduced from an external charger such as a vehicle, and discharges the power for running the vehicle. The power storage device of this embodiment is a regenerative battery. The power storage device may be a portable battery also called a mobile battery.
[0013] FIG. 1 is a schematic diagram for explaining the basic configuration of a cell (single cell) 1 constituting the electricity storage device of this embodiment. As shown in FIG. 1, the cell 1 of the recyclable and reusable electricity storage device has a structure in which components for generating electricity, in which the actual charge and discharge reactions proceed, are sealed inside an exterior material (not shown). Here, the cell 1 has a configuration in which a negative electrode 20 in which a negative electrode active material layer 22 is arranged on one side of a negative electrode collector 21, a positive electrode 30 in which a positive electrode active material layer 32 is arranged on one side of a positive electrode collector 31, and an electrolyte layer 40 provided between the negative electrode 20 and the positive electrode 30 are laminated.
[0014] In the example of FIG. 1, the negative electrode 20, the electrolyte layer 40, and the positive electrode 30 are laminated in this order, so that one negative electrode active material layer 22 and an adjacent positive electrode active material layer 32 face each other with the electrolyte layer 40 interposed therebetween. The positive electrode current collector 31 and the negative electrode current collector 21 are each connected to an electrode tab or the like (not shown).
[0015] (current collector) The positive electrode current collector 31 or the negative electrode current collector 21 is made of a conductive material. The size of the positive electrode current collector 31 or the negative electrode current collector 21 may be determined depending on the intended use of the electricity storage device. For example, if it is used as a large battery, it is preferable to use a current collector with a large area. There is no particular restriction on the thickness of the positive electrode current collector 31 or the negative electrode current collector 21, and the thickness is usually about 1 to 100 μm.
[0016] There is no particular limitation on the material constituting the positive electrode current collector 31 or the negative electrode current collector 21. For example, metals, resins in which conductive polymer materials or non-conductive polymer materials are added with conductive fillers, or the like, may be used. Specifically, as metals, aluminum, nickel, iron, stainless steel, titanium, copper, clad materials of nickel and aluminum, clad materials of copper and aluminum, or plated materials of combinations of these metals, or the like, are preferably used. Also, foils in which the metal surface is coated with aluminum may be used.
[0017] As the conductive polymer material, from the viewpoint of reducing the manufacturing cost and the weight of the current collector, for example, polyaniline, polypyrrole, polythiophene, polyacetylene, polyparaphenylene, polyphenylenevinylene, polyacrylonitrile, polyoxadiazole, and the like are preferably used.
[0018] As the non-conductive polymer material, from the viewpoint of electric potential resistance and solvent resistance, for example, polyethylene, polypropylene, polyethylene terephthalate, polyether nitrile, polyimide, polyamideimide, polyamide, polytetrafluoroethylene, styrene-butadiene rubber, polyacrylonitrile, polymethyl acrylate, polymethyl methacrylate, polyvinyl chloride, polyvinylidene fluoride, polystyrene, or the like is preferably used.
[0019] A conductive filler may be added to the conductive polymer material or non-conductive polymer material as necessary. The conductive filler is not particularly limited as long as it is a material having conductivity, and examples of materials having excellent conductivity, potential resistance, or lithium ion blocking properties include metals and conductive carbon. The metal is not particularly limited, but preferably includes at least one metal selected from the group consisting of Ni, Ti, Al, Cu, Pt, Fe, Cr, Sn, Zn, In, Sb, and K, or an alloy containing these metals, or a metal oxide of these metals. The conductive carbon is not particularly limited, but examples of the conductive carbon include acetylene black, vulcan, black pearl, carbon nanofiber, ketjen black, carbon nanotube, carbon nanohorn, carbon nanoballoon, and fullerene.
[0020] (Positive and negative electrode active material layer) The positive electrode active material layer 32 or the negative electrode active material layer 22 contains an active material, and further contains other additives as necessary.
[0021] The positive electrode active material layer 32 includes a positive electrode active material. Examples of the positive electrode active material include lithium-transition metal composite oxides such as LiMn2O4, LiCoO2, LiNiO2, Li(Ni-Co-Mn)O2, LiFePO4, and those in which a part of the transition metals in these are replaced with other elements, lithium-transition metal phosphate compounds, and lithium-transition metal sulfate compounds. Two or more positive electrode active materials may be used in combination. Note that positive electrode active materials other than those exemplified above may also be used.
[0022] The negative electrode active material layer 22 includes a negative electrode active material. Examples of the negative electrode active material include carbon materials such as natural graphite, MCMB (mesophase carbon microbeads) type graphite, graphite, soft carbon, and hard carbon, and lithium-transition metal composite oxides (e.g., Li4Ti5O 12 ), Si, Ge, Sn, Pb, Al, In, Zn, and other materials that can be alloyed with lithium, and lithium alloy-based negative electrode materials. Two or more types of negative electrode active materials may be used in combination. Note that negative electrode active materials other than those exemplified above may also be used.
[0023] The positive electrode active material layer 32 and the negative electrode active material layer 22 contain a binder. The binder used in the positive electrode active material layer 32 and the negative electrode active material layer 22 is not particularly limited, and examples thereof include polyethylene, polypropylene, polyethylene terephthalate, polyether nitrile, polyacrylonitrile, polyimide, polyamide, cellulose, carboxymethyl cellulose, ethylene-vinyl acetate copolymer, polyvinyl chloride, styrene-butadiene rubber, isoprene rubber, butadiene rubber, ethylene-propylene rubber, ethylene-propylene-diene copolymer, styrene-butadiene-styrene block copolymer and hydrogenated products thereof, styrene-isoprene-styrene block copolymer and hydrogenated products thereof, etc. Examples of such fluororesins include thermoplastic polymers, polyvinylidene fluoride (PVdF), polytetrafluoroethylene, tetrafluoroethylene-hexafluoropropylene copolymers, tetrafluoroethylene-perfluoroalkyl vinyl ether copolymers, ethylene-tetrafluoroethylene copolymers, polychlorotrifluoroethylene, ethylene-chlorotrifluoroethylene copolymers, and polyvinyl fluoride, vinylidene fluoride-hexafluoropropylene-based fluororubbers, vinylidene fluoride-hexafluoropropylene-tetrafluoroethylene-based fluororubbers, vinylidene fluoride-based fluororubbers, and epoxy resins.
[0024] From the viewpoint of excellent heat resistance, a very wide potential window, stability at both positive and negative electrode potentials, and usability in the active material layer, polyvinylidene fluoride, polyimide, styrene-butadiene rubber, carboxymethyl cellulose, polypropylene, polytetrafluoroethylene, polyacrylonitrile, and polyamide are more preferable. These binders may be used alone or in combination of two or more.
[0025] Other additives that may be included in the positive electrode active material layer 32 and the negative electrode active material layer 22 include, for example, a conductive assistant, an electrolyte salt (lithium salt), an ion-conductive polymer, and the like. The conductive assistant refers to an additive that is blended to improve the conductivity of the positive electrode active material layer 32 and the negative electrode active material layer 22. Examples of the conductive assistant include carbon materials such as carbon black such as acetylene black, graphite, and vapor-grown carbon fiber. When the active material layer includes a conductive assistant, an electronic network is effectively formed inside the active material layer, which can contribute to improving the output characteristics of the battery. Examples of the electrolyte salt (lithium salt) include Li(C2F5SO2)2N, LiPF6, LiBF4, LiClO4, LiAsF6, LiCF3SO3, LiBETI, and the like. Examples of the ion-conductive polymer include, for example, polyethylene oxide (PEO)-based and polypropylene oxide (PPO)-based polymers.
[0026] There are no particular limitations on the compounding ratio of the components contained in the positive electrode active material layer 32 and the negative electrode active material layer 22. This compounding ratio can be adjusted according to the desired performance of the electricity storage device.
[0027] The thicknesses of the positive electrode active material layer 32 and the negative electrode active material layer 22 are not particularly limited, and conventionally known knowledge regarding cells of electricity storage devices may be appropriately referred to. As an example, the thicknesses of the positive electrode active material layer 32 and the negative electrode active material layer 22 are preferably about 2 to 100 μm each. More preferably, the thickness of the positive electrode active material layer 32 is 45 to 85 μm. More preferably, the thickness of the negative electrode active material layer 22 is 60 to 80 μm.
[0028] An SEI (solid electrolyte interface) coating 23 is formed on the surface of the negative electrode active material layer 22 on the side to which the negative electrode current collector 21 is not connected, in other words, on the surface of the negative electrode active material layer 22 located on the electrolyte layer 40 side. The SEI coating 23 is a coating generated by decomposition of the electrolyte, and is formed at the interface between the negative electrode active material layer 22 and the electrolyte layer 40. If the SEI coating 23 is too thin, the decomposition reaction of the electrolyte will proceed, but if the SEI coating 23 is too thick, the electrical resistance will increase, affecting the life and efficiency of the battery.
[0029] As the electricity storage device is used, a deteriorated altered layer (not shown) is formed on the surface of the positive electrode active material layer 32 on the side to which the positive electrode current collector 31 is not connected, in other words, on the surface of the positive electrode active material layer 32 located on the electrolyte layer 40 side. Such an altered layer affects the life and efficiency of the battery.
[0030] (Electrolyte layer (electrolyte-impregnated separator)) An electrolytic solution (liquid electrolyte) may be used as the electrolyte constituting the electrolyte layer 40. The liquid electrolyte has a form in which a lithium salt, which is a supporting salt, is dissolved in an organic solvent, which is a plasticizer. Examples of the organic solvent used as a plasticizer include carbonates such as ethylene carbonate (EC), propylene carbonate, and diethyl carbonate (DEC). Examples of the supporting salt (lithium salt) include compounds that can be added to the active material layer of an electrode, such as LiBETI.
[0031] The specific form of the separator constituting the electrolyte layer 40 may be, for example, a microporous film made of polyolefin such as polyethylene or polypropylene. A separator made of nonwoven fabric may also be used. Furthermore, a separator having a heat-resistant layer made of organic resin or inorganic particles on the surface may also be used.
[0032] 1 according to the desired shape of the electricity storage device, or may have a structure in which the positive electrode active material layer 32, the positive electrode current collector 31, the negative electrode active material layer 22, the negative electrode current collector 21, and the electrolyte layer 40 are appropriately laminated. Alternatively, the positive electrode 30 and the negative electrode 20 described above may have a structure in which the electrolyte layer 40 separating them is laminated and wound up.
[0033] (Electrode tab) In order to extract current to the outside of the battery, the positive electrode current collector 31 and the negative electrode current collector 21 may each be connected to an electrode tab (not shown). The electrode tab is electrically connected to these current collectors and is taken out, for example, to the outside of the exterior material of the cell.
[0034] The material constituting the electrode tab is not particularly limited, and a known highly conductive material conventionally used for electrode tabs is preferably used. As the material constituting the electrode tab, for example, a metal material such as aluminum, copper, titanium, nickel, stainless steel, and alloys thereof is preferable, and more preferably, aluminum, copper, etc. are mentioned from the viewpoints of light weight, corrosion resistance, and high conductivity.
[0035] (Battery exterior materials) As the battery exterior material, a known metal can case can be used, or a bag-shaped case using a laminate film containing aluminum that can cover the power generating element can be used. As the laminate film, for example, a three-layer laminate film formed by laminating polypropylene, aluminum, and nylon in this order can be used. From the viewpoint of being excellent in high output and cooling performance and being suitable for use in batteries for large equipment such as EVs and HEVs, a laminate film is desirable as the battery exterior material.
[0036] Positive and negative electrode terminal leads (both not shown) connected to the electrode tabs may be used as necessary. Known materials may be used for the positive and negative electrode terminal leads. The parts removed from the battery exterior material are preferably covered with a heat-resistant insulating heat shrink tube or the like so as not to affect products (e.g., automobile parts, particularly electronic devices, etc.) by contacting peripheral devices or wiring, causing electric leakage. In addition, in a wound-type electricity storage device, the terminals may be formed using, for example, a cylindrical can (metal can) instead of the electrode tabs.
[0037] The recyclable and reusable electric storage device may be, for example, a cylindrical one in the case of a wound type, or may be one obtained by deforming a cylindrical one into a flat rectangular shape. In the case of a cylindrical one, a laminate sheet or a conventional cylindrical can (metal can) may be used as an exterior material, and there is no particular limitation. Preferably, the power generating element (battery element) may be exteriorly covered with an aluminum laminate film.
[0038] The power storage device of this embodiment may be a battery that is suitably used as a vehicle driving power source or auxiliary power source for an electric vehicle, a hybrid electric vehicle, a fuel cell vehicle, a hybrid fuel cell vehicle, or the like.
[0039] The method for restoring electrodes of an electricity storage device according to this embodiment will be described below with reference to FIGS. Fig. 2 shows a flow diagram for explaining the overall flow of the method for recovering an electrode of an electricity storage device according to this embodiment. Fig. 3 to Fig. 6 show schematic cross-sectional views for explaining the process of cutting the negative electrode 20 taken out by disassembling the cell. Fig. 7 shows an example of a graph for creating a calibration curve used in the calculation process described later.
[0040] First, the first step (S20) and the second step (S30) in Fig. 2 will be described. The calculation step (S10) in Fig. 2 will be described later.
[0041] [1st step] In the first step (S20), electrodes are removed from a used electricity storage device. As described above, the shape of the electrodes varies depending on the shape of the electricity storage device, but the electrodes made of a wound body or a laminate are separated into a positive electrode 30 and a negative electrode 20 and removed. The electrodes are, for example, sheet-shaped electrodes. The electrodes are then arranged into a flat plate shape and are provided to the second step (S30).
[0042] [Second process] In the second step (S30), at least a part of the surface layer of the electrode (positive electrode 30 or negative electrode 20) taken out in the first step (S20) is removed by mechanical processing. The surface layer of the electrode means the layer on the surface side of each electrode that is not provided with a current collector (positive electrode current collector 31 or negative electrode current collector 21) and is in contact with the electrolyte layer 40. At least a part of the surface layer may be removed, or the entire surface layer may be removed to a desired thickness.
[0043] The portion of the surface layer of the positive electrode 30 or the negative electrode 20 removed by the mechanical treatment may be a portion that is less than 20% of the thickness of the positive electrode 30 or the negative electrode 20 from the surface of the positive electrode 30 or the negative electrode 20. This allows the surface to be reformed so that the electrode shape can be maintained while the function of the positive electrode 30 or the negative electrode 20 can be effectively restored. The thickness of the positive electrode 30 or the negative electrode 20 is measured by manual measurement using a micrometer or in-line detection using a β-ray thickness meter. The thickness is measured at three points, both ends and the center, for each of the positive electrode 30 or the negative electrode 20, and the arithmetic average is calculated.
[0044] The mechanical treatment in the second step (S30) may be a treatment for cutting at least a part of the surface layer of the electrode. The means used for cutting is not particularly limited as long as it can cut the active material layer of the electrode, and an example of the means is a diamond knife. The diamond knife is a cutting blade made of diamond, and has a blade width of, for example, 1 to 5 mm.
[0045] The process of cutting the negative electrode 20 will be described as an example with reference to Fig. 3 to Fig. 6. Fig. 3 to Fig. 6 are schematic diagrams showing enlarged views of the vicinity of the surface layer of the negative electrode 20. The examples of Fig. 3 to Fig. 6 show an example in which only the SEI coating 23 on the negative electrode active material layer 22 is cut and removed. This corresponds to the process of S40 in Fig. 2.
[0046] First, as shown in FIG. 3, the cutting blade B is inserted into the negative electrode active material layer 22 (here, the SEI coating 23) from the surface 23a side of the SEI coating 23 at a predetermined angle and moving speed. The cutting blade B may have, for example, a rake angle of 15 to 25° and a clearance angle of 5 to 15°. In cutting, it is desirable to cut as thin as possible, so it is preferable to use a thin cutting blade B and adjust the insertion angle α to start cutting. The moving speed in a direction parallel to the surface of the negative electrode 20 (positive direction of the X coordinate axis in FIG. 3, etc.) may be about 1 μm / s. In the initial stage of inserting the cutting blade B into the negative electrode active material layer 22 (i.e., the SEI coating 23), for example, the cutting blade B is moved so that the moving speed in a direction perpendicular to the surface of the negative electrode 20 (positive direction of the Z coordinate axis in FIG. 3, etc.) is 0.1 μm / s and the moving speed in a direction parallel to the surface of the negative electrode 20 (positive direction of the X coordinate axis in FIG. 3, etc.) is 1 μm / s.
[0047] As shown in Figure 4, when the cutting blade B reaches the target depth d (the position of the dotted line l in Figure 4, etc.), the movement in the direction perpendicular to the surface of the negative electrode 20 is stopped, and cutting is continued by switching to a direction only parallel to the surface of the negative electrode 20 as shown in Figure 5.
[0048] In addition, since the load on the cutting blade B corresponds to the amount of cutting, it is preferable to perform cutting while adjusting the load on the cutting blade B so that it does not exceed a certain value. For example, if the load is released, it is determined that the cutting blade has reached the current collector of the electrode.
[0049] In addition, in the case of an electrode for a cylindrical cell, the portion close to the winding core is less likely to contribute to the reaction, so by starting cutting from the winding core side, it is possible to reduce losses in the portion that is not sufficiently cut at the beginning of cutting.
[0050] In the method for recovering an electricity storage device according to the present embodiment, as shown in Fig. 6, a part of the negative electrode active material layer 22 of the negative electrode 20 may also be cut and removed by setting the target depth of the cutting blade B to be greater than the thickness of the SEI coating 23. This corresponds to the step S50 in Fig. 2.
[0051] As shown in FIG. 6, by removing a fixed amount (fixed depth) of the negative electrode 20, the newly formed surface of the electrode can be more efficiently exposed.
[0052] For example, the reaction mechanism of a lithium ion battery progresses from the surface layer of the electrode through the electrolyte layer, so that the deterioration progresses from the surface layer of the electrode toward the current collector. A thick coating containing deactivated metallic Li that does not contribute to charging and discharging grows on the negative electrode that has deteriorated due to the use of the storage device, and a thin coating of this kind also grows on the positive electrode side. The method for recovering the storage device of this embodiment can remove such a deteriorated layer that cannot be removed by a process such as washing.
[0053] 1 and 3 to 6, the cutting plane is parallel to the X- and Z-coordinate axes. The X-, Y-, and Z-coordinate axes in Fig. 1 and 3 to 6 are perpendicular to each other.
[0054] In the method for recovering an electric storage device according to the present embodiment, the mechanical treatment may be a treatment for heating at least a part of the surface layer of the electrode by irradiating it with a laser beam. By irradiating it with a laser beam, oxides and organic matter on the surface layer of the electrode are burned off, so that the altered layer formed on the surface layer of the positive electrode and the SEI coating on the surface layer of the negative electrode can be removed. Such a means is also called, for example, laser peeling or laser cleaning.
[0055] The laser irradiation may be performed in either a wet or dry manner. The depth to which the electrode is heated may be adjusted by adjusting the output and scanning speed of the laser beam. In addition, the active material and binder thermally decomposed by this treatment are preferably removed from the electrode surface by ultrasonic vibration or cleaning.
[0056] In the above example, the negative electrode 20 having the SEI coating 23 is cut, but the mechanical treatment may be performed on either or both of the negative electrode 20 and the positive electrode 30. When the mechanical treatment is performed on the positive electrode 30 side, only the altered layer formed on the surface layer of the positive electrode 30 may be removed, or a part of the positive electrode active material layer 32 may be removed together with the altered layer.
[0057] [Calculation process] In the method for restoring an electrode of an electricity storage device according to the present embodiment, a calculation step (S10) may be performed prior to the first step (S20) of Fig. 2. Then, a thickness equivalent to the increase in thickness calculated in the calculation step (S10) may be removed by mechanical processing in a second step (S30).
[0058] The calculation step (S10) may be performed before the first step, as shown as step S10 in FIG. 2. In this case, before the electrodes are removed from the storage device, the capacity degradation rate is measured by diagnosing the degradation state of the capacity of the used storage device including the positive electrode and the negative electrode, and the increment in the thickness of the negative electrode is calculated based on a calibration curve created in advance. In the calculation step (S10), the capacity degradation rate of the positive electrode or the negative electrode may be calculated by comparing the differential capacity curve (dV / dQ curve) in the initial state of the used storage device with the differential capacity curve of the used storage device (for example, by comparing the change in the peak width of the positive electrode or the negative electrode). Note that in the calculation step (S10), the degradation state of the capacity of the used storage device may be diagnosed based on physical quantity data obtained when the used storage device is charged and discharged. The physical quantity data is, for example, a voltage value and a current value during charging.
[0059] FIG. 7 shows an example of a graph for creating a calibration curve. The horizontal axis of the graph in FIG. 7 is the capacity decrease rate relative to the initial state, and the vertical axis is the increase in the thickness of the negative electrode relative to the initial state. For a storage device having the same specifications as the target storage device, the capacity decrease amount relative to the initial state and the increase in the thickness of the negative electrode are measured, and a calibration curve as shown in FIG. 7 is created from the relationship between them. Then, the capacity decrease rate is measured, and the increase in the thickness of the negative electrode is calculated based on this calibration curve. The increase in thickness is calculated by converting the amount of lithium decrease in the negative electrode. Since the amount of lithium in the negative electrode is correlated with the capacity decrease rate measured using ICP atomic emission spectroscopy, it is preferable to use such a calibration curve.
[0060] In a second step (S30), the increase in thickness of the negative electrode 20 obtained in the calculation step (S10) is removed by mechanical processing. This allows the thickness of the negative electrode 20 to return to its initial state, and allows the electrode to regain its desired performance without performing any further steps.
[0061] In the second step, when a portion of the negative electrode 20 is removed (S50), a chemical conversion treatment (S60) is carried out to form a coating. In the chemical conversion treatment, after assembly into an electricity storage device, the negative electrode 20 is left standing at a constant voltage for a certain period of time, thereby forming the SEI coating 23 again on the surface of the negative electrode 20.
[0062] The method for recovering an electrode of an electric storage device according to the present embodiment can recover the function of the electrode by removing at least a part of the surface layer of the electrode whose performance as an electrode has deteriorated by mechanical treatment, and therefore the electrode can be recovered without separating the active material from the electrode, thereby reducing the environmental load. In particular, in addition to recovering the battery capacity, the removal of the deteriorated surface layer of the electrode is also effective in reducing the electrical resistance of the electrode.
[0063] In addition, by diagnosing the state of deterioration and the cause of deterioration during charging in normal use, information regarding the state of a used storage device can be obtained, and the electrode recovery method for a storage device of this embodiment can be implemented, for example, when the capacity decrease rate of the above-mentioned positive electrode or negative electrode is 10% or more.
[0064] A method for manufacturing an energy storage device according to another embodiment of the present invention includes a first step of removing an electrode from a used energy storage device, a second step of removing at least a portion of the surface layer of the electrode removed in the first step by mechanical processing, and a third step of assembling an energy storage device including the electrode treated in the second step.
[0065] The first and second steps are the same as those of the embodiment of the method for recovering electrodes of an electricity storage device described above. The method for producing an electricity storage device of this embodiment further includes a step of assembling a regenerated electricity storage device using the recovered positive electrode or negative electrode. The method for producing an electricity storage device of this embodiment can recover the function of the electrode and can recover the electrode without separating the active material from the electrode, thereby reducing the environmental load.
[0066] The manufacturing method of the electricity storage device means a regeneration and recovery method. The components of the electricity storage device other than the electrodes, such as the electrolyte layer and the exterior material, may be reused after appropriate treatment, or a new component may be used to manufacture the electricity storage device. [Explanation of symbols]
[0067] 1 cell 20 negative electrode 21 Negative electrode current collector 22 Negative electrode active material layer 23 SEI Coating 30 positive electrode 31 Positive electrode current collector 32 Positive electrode active material layer 40 Electrolyte layer
Claims
1. A method for recovering electrodes of a used electricity storage device, comprising the steps of: a first step of removing the electrodes from the used electricity storage device; a second step of removing at least a portion of the surface layer of the electrode taken out in the first step by mechanical processing; Includes A method for recovering electrodes of an electricity storage device, comprising:
2. The portion of the surface layer of the electrode that is removed by the mechanical treatment is a portion that is less than 20% of the thickness of the electrode from the surface of the electrode. The method for recovering electrodes of an electricity storage device according to claim 1 .
3. The method further includes a calculation step of calculating an increase in thickness of the electrode before the second step, The thickness corresponding to the increase in thickness calculated in the calculation step is removed by the mechanical treatment.
3. The method for recovering electrodes of an electricity storage device according to claim 1 or 2.
4. The mechanical treatment is a treatment for cutting at least a part of the surface layer of the electrode. The method for recovering electrodes of an electricity storage device according to any one of claims 1 to 3.
5. The mechanical treatment is a treatment in which at least a part of the surface layer of the electrode is heated by irradiating it with a laser beam. The method for recovering electrodes of an electricity storage device according to any one of claims 1 to 3.
6. A method for manufacturing an electricity storage device, comprising: A first step of removing an electrode from a used electricity storage device; a second step of removing at least a portion of the surface layer of the electrode taken out in the first step by mechanical processing; a third step of assembling an electricity storage device including the electrode treated in the second step; Includes A method for manufacturing an electricity storage device comprising the steps of:
7. The electric storage device according to claim 6, A power storage device.
Citation Information
Patent Citations
Measuring method using crystalline carbon as electrode
JP2006084375A
Method for regenerating electrode of lithium ion battery
JP2012022969A
Secondary battery
JP2013225410A
Recovery method of positive electrode active material component
JP2016033876A
Material collecting method for bipolar storage battery
JP2022147473A
Cited By
Anode black powder and recovery method thereof
CN119786785A
A positive electrode black powder and a method for recovering the same
CN119786785B