Optical isolator manufacturing method, optical isolator, and polarizing glass

By bonding polarizing glass to the Faraday rotator before forming antireflection films, the method addresses warping and peeling issues, enabling thinner optical isolators with secure attachment and adaptable film configurations.

JP2024146062AInactive Publication Date: 2024-10-15HOYA CORPORATION
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2023058765
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-31
Publication Date
2024-10-15
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Conventional optical isolator manufacturing methods face challenges with polarizer warping and peeling due to film stress, especially in thinner designs, complicating bonding processes and increasing the risk of detachment.

Method used

The method involves bonding polarizing glass to the Faraday rotator before forming the antireflection film, ensuring minimal warpage and secure attachment, allowing for thicker antireflection films and flexible film configurations.

Benefits of technology

This approach results in an optical isolator with minimal warpage and reduced peeling risk, enabling thinner designs with effective antireflection performance and adaptable film thicknesses.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024146062000001_ABST
    Figure 2024146062000001_ABST
Patent Text Reader

Abstract

To provide a method of manufacturing an optical isolator which is thinner than conversational products, yet exhibits minimal susceptibility to the film stress of an antireflection film.SOLUTION: An optical isolator manufacturing method of the present invention is for manufacturing an optical isolator comprising a Faraday rotator and a polarizing glass attached to the Faraday rotator, and comprises the steps of bonding the polarizing glass to the Faraday rotator and forming an antireflection film on the surface of the bonded polarizing glass.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for manufacturing an optical isolator, an optical isolator, and a polarizing glass used in an optical isolator. [Background technology]

[0002] Conventionally, semiconductor laser modules used in optical communications, measurement, and the like employ optical isolators to prevent reflected light from returning to the semiconductor laser element and causing instability in laser oscillation. A typical optical isolator is constructed by placing a flat Faraday rotator between two polarizers, and housing these three components in a cylindrical magnet. Usually, the Faraday rotator is adjusted to a thickness that rotates the polarization plane of light with a specified wavelength by 45° in a saturation magnetic field, and the two polarizers are rotated so that the transmission polarization direction of each polarizer is shifted by 45°.

[0003] Furthermore, in such optical isolators, since reflected light on the polarizer surface can cause noise and the like, a configuration in which an anti-reflection film is provided on the polarizer surface so that the reflectance for the wavelength band of light being used (for example, a wavelength band of 1250 to 1650 nm when used in optical communications) is a predetermined value or less (for example, 0.3% or less) is also used (for example, Patent Document 1).

[0004] Such optical isolators generally have the following features: (1) Manufacture polarizers (polarizing glass); (2) forming an anti-reflection film on one surface of the polarizer (1); (3) The polarizers (2) above are bonded to both sides of the Faraday rotator. It is manufactured by a process such as:

[0005] However, when an anti-reflection film is formed on one side of a polarizer in this way, the polarizer may be warped due to film stress, which makes it difficult to bond the polarizer to the Faraday rotator and increases the risk of the polarizer peeling off (falling off) from the Faraday rotator. Moreover, in recent years, there has been a demand for even thinner polarizers (for example, a thickness of 0.1 mm or less) in order to miniaturize optical isolators. However, when the polarizer is made thinner, the effect of the film stress in the anti-reflection film becomes more pronounced (i.e., the amount of warping of the polarizer increases), making the bonding work more difficult and also increasing the risk of the polarizer peeling off.

[0006] FIG. 3 shows the results of an experiment conducted by the inventors, illustrating the relationship between the thickness of the polarizing glass and the amount of warping of the polarizing glass (that is, the effect of the film stress of the anti-reflection film). In this experiment, polarizing glass samples of different thicknesses (thickness: 0.1 mm, 0.12 mm, 0.2 mm) were prepared, and a total of eight anti-reflection films (film thickness: 600 nm) consisting of alternating layers of Ta2O5 and SiO2 were formed on one side of each sample. The surface roughness of each sample was measured with a measuring device (Zygo Model: Newview 8200), and the maximum height was taken as the amount of warping.

[0007] As shown in FIG. 3, as the thickness of the polarizing glass becomes thinner, the effect of the film stress of the anti-reflection film cannot be ignored, and the amount of warping increases.

[0008] In order to solve this problem, it has been proposed to form a warp suppressing film on the other side of the polarizer (the side opposite the anti-reflection film) to suppress warping of the polarizer (i.e., to counteract the film stress of the anti-reflection film) (for example, Patent Document 2). [Prior art documents] [Patent documents]

[0009] [Patent Document 1] Patent Publication No. 2013-54323 [Patent Document 2] Patent Publication No. 2020-91443 Summary of the Invention [Problem to be solved by the invention]

[0010] However, the configuration of Patent Document 2 has problems such as: (i) the cost increases because the warp-suppressing film is increased; and (ii) since there is variation (tolerance) in the thickness of the antireflection film and variation (tolerance) in the thickness of the warp-suppressing film, it is not possible to completely eliminate the effects of film stress (i.e., warping of the polarizer).

[0011] The present invention has been made in view of the above circumstances, and its object is to provide a method for manufacturing an optical isolator that is thinner than conventional ones and has an extremely small amount of warping of the polarizing glass, to provide an optical isolator, and to provide polarizing glass for use in such an optical isolator. [Means for solving the problem]

[0012] In order to achieve the above-mentioned object, the manufacturing method of an optical isolator of the present invention is a manufacturing method of an optical isolator comprising a Faraday rotator and a polarizing glass attached to the Faraday rotator, and is characterized by including a step of bonding the polarizing glass to the Faraday rotator, and a step of forming an anti-reflection film on the surface of the bonded polarizing glass.

[0013] According to this method, the polarizing glass before the anti-reflection film is formed is bonded to the Faraday rotator, and then the anti-reflection film is formed on the surface of the polarizing glass (i.e., the polarizing glass is bonded to the Faraday rotator before warping occurs), so the polarizing glass is bonded and fixed to the Faraday rotator in a state where it is almost (substantially) unwarped. Therefore, the polarizing glass is firmly attached to the Faraday rotator (i.e., the risk of peeling is reduced). In addition, since the polarizing glass is installed with almost no warping, the anti-reflection coating functions to the maximum extent (as designed). Furthermore, since the polarizing glass is attached in a state where it is almost free from warping, it is possible to make the polarizing glass extremely thin. In addition, since the anti-reflection film is formed with the polarizing glass attached to the Faraday rotator, there is no need to consider warping of the polarizing glass, and an anti-reflection film with a thicker thickness than conventional films can be formed. Furthermore, the film structure and thickness of the anti-reflection film can be freely changed according to the specifications of the optical isolator.

[0014] Moreover, it is preferable that the process of forming the anti-reflection film alternately laminate low-refractive-index films having a relatively low refractive index and high-refractive-index films having a relatively high refractive index.

[0015] Moreover, the anti-reflection film preferably has a thickness of 400 to 2000 nm.

[0016] It is also preferable that the thickness of the polarizing glass is 0.028 to 0.20 mm.

[0017] It is also desirable that the amount of warping of the bonded polarizing glass be 3 μm or less.

[0018] Moreover, it is preferable to further include a step of forming the anti-reflective film into a predetermined size after the anti-reflective film is formed.

[0019] In addition, the polarizing glass is composed of a first polarizing glass whose polarization axis is oriented in the 0° direction and a second polarizing glass whose polarization axis is oriented in the 45° direction, and the step of bonding the polarizing glass preferably involves bonding the first polarizing glass to one side of the Faraday rotator and bonding the second polarizing glass to the other side.

[0020] From another point of view, the optical isolator of the present invention is an optical isolator comprising a Faraday rotator and a polarizing glass laminated to the Faraday rotator, characterized in that the polarizing glass has a thickness of 0.10 mm or less, and has an anti-reflection film with a thickness of 650 nm or more only on the outer surface of the polarizing glass. In this case, it is preferable that the amount of warping of the polarizing glass is 3 μm or less. It is also preferable that the inner surface opposite to the outer surface of the polarizing glass does not have a functional film that suppresses the warping of the polarizing glass.

[0021] From another point of view, the polarizing glass of the present invention is a polarizing glass for an optical isolator, one side of which is bonded to a Faraday rotator, and is characterized in that it has a thickness of 0.028 to 0.20 mm and has an antireflection film of 400 to 2000 nm in thickness formed on the other side after being bonded to the Faraday rotator. In this case, it is preferable that the amount of warping of the polarizing glass is 3 μm or less. Effect of the Invention

[0022] As described above, the present invention provides a method for manufacturing an optical isolator that is thinner than conventional ones and has an extremely small amount of warping in the polarizing glass, and realizes such an optical isolator. It also realizes polarizing glass for use in such an optical isolator. [Brief description of the drawings]

[0023] [Figure 1] FIG. 1 is a schematic diagram illustrating the configuration of an optical isolator according to an embodiment of the present invention. [Diagram 2] FIG. 2 is a flowchart illustrating a method for manufacturing an optical isolator according to an embodiment of the present invention. [Diagram 3] FIG. 3 is a diagram showing the relationship between the thickness of a conventional polarizing glass and the amount of warping of the polarizing glass. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0024] Hereinafter, embodiments of the present invention will be described in detail with reference to the drawings. In the drawings, the same or corresponding parts are designated by the same reference characters and their description will not be repeated.

[0025] (Configuration of optical isolator) FIG. 1 is a schematic diagram for explaining the configuration of an optical isolator 1 according to an embodiment of the present invention, in which FIG. 1(a) is a plan view and FIG. 1(b) is a side cross-sectional view. As shown in FIG. 1, the optical isolator 1 according to this embodiment is formed by bonding a pair of polarizing elements 20 and 30 to both sides of a Faraday rotator 10 so that the optical axes are common. The wavelength band in which the optical isolator 1 according to this embodiment is used is not particularly limited, and it can be used for light in a wavelength band of 1250 to 1650 nm or a wavelength band of 1650 nm or more. In this embodiment, the polarization axis of the polarizing element 20 and the polarization axis of the polarizing element 30 are inclined at 45° to each other. The size of the optical isolator 1 according to this embodiment is not particularly limited, and is, for example, 0.4 to 0.7 mm square when viewed from the polarizing element 20 side.

[0026] The Faraday rotator 10 is an element fabricated by forming a magneto-optical thin film (for example, a Bi-substituted magnetic garnet film) on a non-magnetic garnet substrate by a liquid phase epitaxial method (LPE method), a sputtering method, an aerosol deposition method, or the like, and has a first main surface 11 and a second main surface 12 opposed to each other. The refractive index of the Faraday rotator 10 of this embodiment at 1550 nm is 2.34, and the thickness of the Faraday rotator 10 is set to 0.35 to 0.5 mm.

[0027] The pair of polarizing elements 20, 30 are optical elements attached to the first main surface 11 and the second main surface 12 of the Faraday rotator 10, respectively, and each comprises a polarizing glass 21, 31 and an antireflection film 22, 32. In this embodiment, the polarizing glass 21 is a polarizing glass whose polarization axis is in a specific first direction (0° direction), and the polarizing glass 31 is a polarizing glass whose polarization axis is in a second direction (45° direction) that forms an angle of 45° with respect to the polarization axis of the polarizing glass 21.

[0028] As shown in FIG. 1, the polarizing glass 21, 31 of this embodiment has an appearance of a rectangular plate (e.g., 0.7 mm (horizontal) × 0.7 mm (vertical), thickness: 0.028 to 0.20 mm), and has a metal layer (not shown) on both the front and back surfaces in which a large number of approximately needle-shaped metal particles are oriented and dispersed in parallel, and a metal halide layer (not shown) containing metal halide particles is formed between the metal layers. The metal layer is a layer having a predetermined thickness (for example, 0.010 to 0.045 mm) that is formed by precipitating needle-shaped metal particles made of silver or copper in a reduction step described below. The metal halide layer is a layer having a predetermined thickness (for example, 0.001 to 0.060 mm) that is formed inside the metal layer by the reduction step described below.

[0029] The antireflection films 22 and 32 are, for example, a multi-layer structure in which a low refractive index film (e.g., SiO2: refractive index 1.46) and a high refractive index film (e.g., Ta2O5: refractive index 2.1, TiO2: refractive index 2.35) are alternately laminated, and the thickness of each layer is selected to obtain a distribution curve of the target reflectance. In this embodiment, the antireflection films 22 and 32 have the same structure, for example, an eight-layer structure with a film thickness of 400 to 800 nm, thereby suppressing the reflectance to 0.3% or less in a wide wavelength band of 1250 to 1650 nm. In addition, since the antireflection films 22, 32 in this embodiment are formed on the surfaces of the polarizing glasses 21, 31 after the polarizing glass 21 is bonded to the Faraday rotator 10 (details will be described later), no film stress is generated by the antireflection films 22, 32. Therefore, the film configuration and film thickness of the antireflection films 22, 32 can be appropriately changed according to the specifications of the optical isolator 1 (e.g., the central wavelength and bandwidth of the laser light), and the film thickness can be freely set within the range of 400 to 2000 nm, for example.

[0030] (Manufacturing method of optical isolator) Next, a method for manufacturing the optical isolator 1 of this embodiment will be described. Fig. 2 is a flow chart (steps 101 to 107) showing the method for manufacturing the optical isolator 1 of this embodiment. The optical isolator 1 of this embodiment is manufactured by the following procedure. 1. The polarizing glass pieces 21 and 31 are prepared (manufactured) (manufacturing process of the polarizing glass pieces 21 and 31). 2. The Faraday rotator 10 is prepared, and the polarizing glasses 21 and 31 are bonded to the Faraday rotator 10 (bonding step). 3. Anti-reflection films 22 and 32 are formed on the surfaces of the polarizing glasses 21 and 31, respectively (film forming step). 4. Form into the specified size (forming process). Each step (process) is described in detail below.

[0031] [1. Manufacturing process of polarizing glass 21, 31] The polarizing glass pieces 21 and 31 of this embodiment are manufactured by the following procedure. (1) Predetermined glass materials containing copper or silver are mixed to obtain the desired composition, melted at approximately 1450° C., and then slowly cooled to room temperature (a glass substrate manufacturing process). (2) Heat treatment is carried out to cause cuprous chloride or silver chloride particles to precipitate in the glass (step of precipitating metal halide particles). (3) A preform having an appropriate shape (for example, 120×250×4 mm) is produced by machining (preform production step). (4) The preform is heated and stretched under specified conditions to obtain a glass sheet (e.g., width: about 18 mm, thickness: about 0.5 mm) (glass stretching process). (5) The glass sheet is cut and polished on both sides to prepare a double-sided polished product (e.g., 11 mm square, thickness: 0.028 to 0.20 mm) (polished product preparation process). (6) The polished product is reduced in a hydrogen atmosphere (reduction step). The reduction process causes needle-shaped metal (copper or silver) fine particles to precipitate, forming a metal layer (not shown) and a metal halide layer (not shown) in the polarizing glass 21, 31, and obtaining the polarizing glass 21, 31 (FIG. 2: step 101). As described above, the polarizing glass 21 has a polarization axis in a first direction (0° direction), and the polarizing glass 31 has a polarization axis in a second direction (45° direction). In this embodiment, the thickness of the polarizing glass 21, 31 is in the range of 0.028 to 0.20 mm, but is not necessarily limited to this configuration.

[0032] [2. Adhesion process] The bonding step is a step of preparing a Faraday rotator 10 and bonding polarizing glasses 21, 31 to the first main surface 11 and the second main surface 12 of the Faraday rotator 10, respectively. Specifically, an organic adhesive, EPO-TEK 353ND (refractive index 1.5694@589 nm) manufactured by Epoxy Technology, is applied to the first main surface 11 and the second main surface 12 of the Faraday rotator 10, and the polarizing glasses 21, 31 are overlapped with good positional accuracy and fixed by curing (thermal hardening) at 150°C for one hour (FIG. 2: step 103).

[0033] [3. Film formation process] The film formation process is a process of forming anti-reflection films 22, 32 on the surfaces of the bonded polarizing glass 21, 31, respectively. Specifically, a total of eight anti-reflection films 22, 32 (film thickness: 400 to 800 nm) consisting of alternating layers of Ta2O5 and SiO2 are formed by ion beam assisted deposition (hereinafter, IAD) (FIG. 2: step 105). This anti-reflection film is designed to be compatible with a wide band in which the reflectance for light in the 1250 to 1650 nm wavelength band used in optical communications is 0.3% or less.

[0034] [4. Molding process] The molding step is a step of molding to a predetermined size, and in this embodiment, for example, it is cut into 0.4 to 0.7 mm squares to obtain the optical isolator 1 of this embodiment (FIG. 2: step 107).

[0035] In this manner, in the optical isolator 1 of this embodiment, the polarizing glasses 21, 31 before the antireflection films 22, 32 are formed are bonded to the Faraday rotator 10, and then the antireflection films 22, 32 are formed on the surfaces of the polarizing glasses 21, 31. Therefore, according to the manufacturing method of this embodiment, the polarizing glasses 21, 31 are adhered and fixed to the Faraday rotator 10 in a state that is almost (substantially) free of warping (e.g., 3 μm or less), so that the polarizing glasses 21, 31 are firmly attached to the Faraday rotator 10 (i.e., the risk of peeling is reduced).

[0036] Furthermore, since the polarizing glasses 21, 31 are attached in a state with almost no warping (for example, the amount of warping: 3 μm or less), the anti-reflection films 22, 32 function to the maximum extent (as designed).

[0037] Furthermore, since the polarizing glasses 21 and 31 are attached with almost no warping (for example, 3 μm or less), the polarizing glasses 21 and 31 can be made extremely thin (for example, preferably 0.028 to 0.10 mm, and more preferably 0.028 to 0.050 mm).

[0038] In addition, since the antireflection films 22, 32 are formed with the polarizing glasses 21, 31 attached to the Faraday rotator 10, there is no need to consider warping of the polarizing glasses 21, 31, and it is possible to form antireflection films with a thicker film thickness than before (for example, in the range of 400 to 2000 nm, preferably 650 to 2000 nm, and more preferably 800 to 2000 nm). In addition, the film configuration and film thickness of the antireflection films 22, 32 can be freely changed according to the specifications of the optical isolator 1.

[0039] Although the embodiment of the present invention has been described above, the present invention is not limited to the configuration of the above embodiment, and various modifications are possible within the scope of the technical concept thereof.

[0040] For example, the optical isolator 1 of this embodiment has been described as having a pair of polarizing elements 20, 30, but is not necessarily limited to this configuration, and may have only one of them.

[0041] In addition, in this embodiment, anti-reflection films 22, 32 are formed on the surfaces of the polarizing glasses 21, 31, but other functional films (for example, band-pass filters, etc.) may be formed instead of or in addition to the anti-reflection films.

[0042] In addition, in this embodiment, the molding step is carried out after the film formation step. However, if the Faraday rotator 10 and the polarizing glasses 21 and 31 of predetermined sizes are prepared in advance, the molding step is not necessarily required.

[0043] It should be noted that the embodiments disclosed herein are illustrative in all respects and should not be considered as limiting. The scope of the present invention is defined by the claims, not the above description, and is intended to include all modifications within the meaning and scope of the claims. [Explanation of symbols]

[0044] 1: Optical isolator 10: Faraday rotator 11: First main surface 12: Second main surface 20: Polarizing element 21: Polarizing glass 22: Anti-reflection film 30: Polarizing element 31: Polarizing glass 32: Anti-reflection film

Claims

1. A method for manufacturing an optical isolator including a Faraday rotator and a polarizing glass attached to the Faraday rotator, comprising the steps of: bonding the polarizing glass to the Faraday rotator; forming an anti-reflection film on the surface of the bonded polarizing glass; A method for manufacturing an optical isolator comprising:

2. 2. The method for producing an optical isolator according to claim 1, wherein the step of forming the antireflection film comprises alternately laminating a low refractive index film having a relatively low refractive index and a high refractive index film having a relatively high refractive index.

3. 3. The method for producing an optical isolator according to claim 1, wherein the antireflection film has a thickness of 400 to 2000 nm.

4. 2. The method for producing an optical isolator according to claim 1, wherein the polarizing glass has a thickness of 0.028 to 0.20 mm.

5. 2. The method for producing an optical isolator according to claim 1, wherein the amount of warping of the bonded polarizing glass is 3 [mu]m or less.

6. 2. The method for producing an optical isolator according to claim 1, further comprising the step of forming the anti-reflection film into a predetermined size after the anti-reflection film is formed.

7. The polarizing glass is composed of a first polarizing glass having a polarization axis oriented in a 0° direction and a second polarizing glass having a polarization axis oriented in a 45° direction, the step of bonding the polarizing glass includes bonding the first polarizing glass to one surface of the Faraday rotator and bonding the second polarizing glass to the other surface of the Faraday rotator; A method for manufacturing the optical isolator according to claim 1.

8. An optical isolator comprising a Faraday rotator and a polarizing glass bonded to the Faraday rotator, The thickness of the polarizing glass is 0.10 mm or less, The polarizing glass has an anti-reflection film having a thickness of 650 nm or more only on the outer surface thereof.

1. An optical isolator comprising:

9. 9. An optical isolator according to claim 8, wherein the amount of warping of the polarizing glass is 3 [mu]m or less.

10. 9. An optical isolator according to claim 8, wherein an inner surface of the polarizing glass opposite to the outer surface does not have a functional film for suppressing warping of the polarizing glass.

11. A polarizing glass for an optical isolator, one side of which is bonded to a Faraday rotator, The thickness is 0.028 to 0.20 mm, On the other surface, an anti-reflection film having a thickness of 400 to 2000 nm is formed after bonding to the Faraday rotator. The polarizing glass is characterized by the above.

12. 12. The polarizing glass according to claim 11, wherein the amount of warping of the polarizing glass is 3 μm or less.

Citation Information

Patent Citations

  • Polarizing glass, polarizing glass structure, polarizing glass assembly and optical isolator

    JP2013054323A

  • Polarizer and optical isolator

    JP2020091443A