Phenol foam laminated plate
The phenolic foam laminate addresses non-combustibility and adhesion issues by laminating magnesium silicate boards with a specific coating and resin fiber layer, ensuring long-term fireproof performance and adherence to ISO5660-1:2002 standards.
Patent Information
- Application Number
- JP2023059386
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-31
- Publication Date
- 2024-10-15
AI Technical Summary
Existing phenolic foam materials fail to meet non-combustibility standards in ISO5660-1:2002 due to adhesive failure and generation of flammable gases, and composite papers exhibit poor adhesion, making them impractical for fireproof applications.
A phenolic foam laminate is created by laminating magnesium silicate and/or calcium silicate boards with a surface coating of alcohol components and silicon oxide, using an acrylic polymer latex mixture that includes magnesium oxide, and forming a lattice pattern with a resin fiber layer to enhance adhesion and maintain non-flammability under high humidity.
The laminate achieves long-term non-flammability and adherence to ISO5660-1:2002 standards, maintaining fireproof performance even under humid conditions with improved adhesion and reduced flammable gas generation.
Smart Images

Figure 2024146472000001
Abstract
Description
[Technical field]
[0001] The present invention relates to a non-combustible phenolic foam laminate. [Background technology]
[0002] In recent years, the use of phenolic foam has been expanding, mainly in construction, due to its high thermal insulation performance. In this context, fire resistance is increasingly being questioned in its use as a construction material, and studies have been conducted to address this issue.
[0003] For example, Patent Document 1 describes a non-combustible heat insulating panel constructed by bonding a non-combustible board mainly composed of sepiolite (hydrated magnesium silicate) to both sides of a phenol foam plate via an adhesive. Patent document 2 describes a fireproof paper containing hydrated magnesium silicate, pulp, glass fiber, and a binder, and a composite paper in which the fireproof paper is coated with a fireproof paper inorganic film agent containing vermiculite and a polyether resin or a polyester resin. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2004-100228 A [Patent Document 2] JP 2008-163508 A Summary of the Invention [Problem to be solved by the invention]
[0005] However, none of these materials had sufficient fire resistance to be certified as non-combustible materials in a non-combustibility test using a cone calorimeter in accordance with ISO5660-1:2002. In the invention described in Patent Document 1, when the panel was heated in a cone calorimeter, not only the non-flammable board but also the adhesive and foam components that make up the inside of the board became very hot, which could cause flammable gases to be generated. However, because there were tiny gaps in the non-flammable board, the flammable gases that bubbled up to the surface ignited, and the board failed to meet the standards for a non-flammable material. Furthermore, in the composite paper coated with the inorganic film agent of Patent Document 2, the adhesion between the fireproof paper and the inorganic film agent is low, making it difficult to use in practical applications. [Means for solving the problem]
[0006] The inventors of the present invention have conducted extensive research to solve the above problems, and have found that when a specific additive component is added to a specific polymer latex and the mixture is coated on the surface of a board containing magnesium silicate and / or calcium silicate provided on a phenolic foam board, the resulting phenolic foam laminate not only meets the standard for non-flammable materials in ISO5660-1:2002, but also has high adhesion of the coating material not only when dry but also when wet, and can maintain non-flammable performance for a long period of time, thereby completing the present technology.
[0007] That is, the present invention is as follows. [1] A phenol foam laminate comprising a board containing magnesium silicate and / or calcium silicate laminated on one or both sides of a phenol foam plate, and an acrylic polymer latex mixture layer containing at least any two components selected from alcohols having 12 to 14 carbon atoms, silicon oxide, magnesium oxide, and an acrylic polymer latex formed on the outer surface of the board. [2] The phenolic foam laminate according to [1], wherein a resin fiber layer is formed between the phenolic foam plate and the board. [3] The phenol foam laminate according to [1] or [2], wherein six cut lines are formed lengthwise and widthwise at 2 mm intervals in the acrylic polymer latex mixture layer to create a grid pattern, the layer is then exposed to water at room temperature for two hours, and then dried at 60°C for 30 minutes. In the peel test specified in JIS K5600-5-6:1999, the adhesion of the acrylic polymer latex mixture layer after the test is 50% or more. Effect of the Invention
[0008] According to the present invention, it is possible to provide a phenol foam laminate that meets the standard for non-flammable materials in ISO5660-1:2002, in which the acrylic polymer latex mixture layer does not easily peel off even under high humidity conditions, and that can maintain its non-flammable performance for a long period of time. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] The phenol foam laminate of the present invention is an invention that improves upon the above-mentioned problems, and is a phenol foam laminate in which a board containing magnesium silicate and / or calcium silicate is laminated on one or both sides of a phenol foam, and an acrylic polymer latex mixture layer containing at least any two components selected from alcohols having 12 to 14 carbon atoms, silicon oxide, magnesium oxide, and an acrylic polymer latex is formed on the outer surface of the board. The outer surface of the board refers to the surface opposite to the surface on which the phenol foam plate is present. The phenol foam laminate may have a laminate structure in which the phenol foam plate, the board, and the acrylic polymer latex mixture layer are laminated adjacent to each other in this order, or a laminate structure in which the phenol foam plate, the resin fiber layer, the board, and the acrylic polymer latex mixture layer are laminated adjacent to each other in this order. The acrylic polymer latex mixture layer may be a layer formed on the surface of the phenol foam laminate.
[0010] The phenol foam laminate of the present invention satisfies the standard for non-flammable materials in ISO5660-1:2002, and the acrylic polymer latex mixture layer does not easily peel off even under high humidity, and can maintain non-flammable performance for a long period of time. The adhesion of the coating layer in the phenol foam laminate of the present invention is preferably 80% or more under non-humid conditions, and more preferably 90% or more. Furthermore, it is preferably 50% or more under humid conditions, and more preferably 70% or more.
[0011] The acrylic polymer latex used in the phenol foam laminate according to the present invention may be a copolymer obtained by copolymerizing acrylic acid or its ester, or methacrylic acid or its ester. A copolymer obtained by copolymerizing acrylic acid or its ester is more preferred. The acrylic polymer latex may contain a polymer component, water, and an additive, and the polymer component contained in the acrylic polymer latex is preferably a copolymer obtained by copolymerizing acrylic acid or its ester.
[0012] The viscosity of the acrylic polymer latex is preferably 10 to 500 mPa·s, more preferably 30 to 200 mPa·s at 23° C. The solid content is preferably 30 to 60%. From the viewpoint of non-flammability, the minimum film formation temperature is preferably 20° C. or higher and 40° C. or lower.
[0013] The acrylic polymer latex mixture layer has a solid content of 30 to 300 g / m from the viewpoint of exhibiting a non-flammable effect. 2 is preferable, and 70 to 200 g / m 2 is more preferred.
[0014] The phenol foam laminate of the present invention is characterized in that an acrylic polymer latex mixture layer consisting of an acrylic polymer latex mixture containing non-flammable materials such as silicon oxide and magnesium oxide, at least two of alcohols having 12 to 14 carbon atoms, and an acrylic polymer latex imparts high flame retardancy to the phenol foam board laminated with a board containing magnesium silicate and / or calcium silicate, and the acrylic polymer latex mixture layer is maintained in the state after coating even in a high humidity environment.
[0015] As the alcohol having 12 to 14 carbon atoms, any two components may be selected, but from the viewpoint of adhesion performance, it is more preferable to use a combination of dodecanol having 12 carbon atoms and tridecanol having 13 carbon atoms. The composition ratio of the two alcohol components can be appropriately adjusted within a preferred range of 1:10 to 10:1, and the total amount of the alcohol having 12 to 14 carbon atoms added is preferably 0.05 to 2 parts by mass relative to 100 parts by mass of the acrylic polymer latex.
[0016] The silicon oxide and magnesium oxide, which are non-flammable materials constituting the acrylic polymer latex mixture layer, can be, for example, vermiculite, etc. When using vermiculite, the mixing ratio is preferably 200 to 1000 parts by mass with respect to 100 parts by mass of the acrylic polymer latex. The acrylic polymer latex mixture layer may be a layer containing the acrylic polymer latex and at least any two of the alcohols having 12 to 14 carbon atoms, and vermiculite.
[0017] The acrylic polymer latex mixture layer may further contain aluminum oxide as the non-flammable material in addition to silicon oxide and magnesium oxide.
[0018] In addition, the acrylic polymer latex mixture layer may contain components that are typically added to water-based paints, such as water, solvents, thickeners, film-forming aids, plasticizers, antifreeze agents, defoamers, dispersants, wetting agents, dyes, preservatives, antifungal agents, anti-algae agents, pigments, antistatic agents, conductive materials, insulating materials, ultraviolet absorbers, and light stabilizers, within the scope that does not reduce the effects of the present invention.
[0019] The total mass ratio of at least any two of the alcohols having 12 to 14 carbon atoms, the silicon oxide, the magnesium oxide, and the acrylic polymer latex to 100% by mass of the acrylic polymer latex mixture layer is preferably 30 to 80% by mass, and more preferably 40 to 70% by mass.
[0020] The present invention is also advantageous in that it maintains its non-combustible performance even if a resin fiber layer is formed between the phenolic foam board and the board containing magnesium silicate and / or calcium silicate. The resin fiber layer can hold an air layer, which contributes to further improving the heat insulating performance of the phenolic foam laminate. The resin fiber is often a thermoplastic resin, and polyester non-woven fabric is preferably used due to its bulkiness, but in the non-combustible performance test of ISO5660-1:2002, it easily liquefies and evaporates, releasing flammable gas. However, in the present invention, even the generation of such flammable gas is contained, and the standard for non-combustible materials in ISO5660-1:2002 is satisfied.
[0021] The weight of the resin fiber layer suitable for achieving the effects of the present invention is 20 to 100 g / m 2 is preferable, and 25 to 60 g / m 2 is more preferred.
[0022] As the board containing magnesium silicate and / or calcium silicate used in the phenol foam laminate of the present invention, a commercially available fireproof board or non-combustible board can be used, but from the viewpoint of non-combustible performance, a board containing magnesium silicate is preferred.
[0023] The board may be laminated to the phenol foam plate or to the laminate of the phenol foam plate and the resin fiber layer using an adhesive, or may be physically arranged by providing members such as hooks or screws.
[0024] The phenol foam board used in the phenol foam laminate of the present invention is produced by adding a surfactant, a foaming agent, and a catalyst to a raw phenol resin, mixing the mixture, and then heating to foam and harden it. There are two types of raw phenol resin: novolac type and resol type, and the resol type is preferably used. For example, "Neoma Foam" manufactured by Asahi Kasei Construction Materials Co., Ltd., which has excellent heat insulating properties, is preferably used.
[0025] In the phenol foam laminate according to the present invention, the method for forming an acrylic polymer latex mixture layer on the surface of the board containing magnesium silicate and / or calcium silicate can be selected from roll coating, spraying, flow coating, etc., and after coating, the coating layer is dried and cured at high temperature. In order to achieve the effects of the present invention, it is important to dry at high temperature for a short time, and the preferred conditions are 80°C to 150°C for 2 to 15 minutes, and the more preferred conditions are 105°C to 140°C for 2 to 15 minutes.
[0026] The present invention will be described in more detail below with reference to examples and comparative examples. The non-flammability and adhesion were evaluated according to the following procedures.
[0027] (Preparation of test specimen) The phenol foam board is made of Asahi Kasei Construction Materials' "Neoma Foam" (thickness 25 mm, density 40 kg / m 3 A phenol foam laminate was prepared by bonding these together with an epoxy adhesive, and then the outer surface of the board containing magnesium silicate and / or calcium silicate was coated with the mixed liquid described in the examples using a roll coater and dried to produce a phenol foam laminate.
[0028] (Non-flammable rating) A 100mm x 100mm test piece was cut out from the phenol foam laminate without any change in thickness, and the surface of the acrylic polymer latex mixture layer was subjected to a cone calorimeter (Toyo Seiki Seisakusho No. 607) for 1200 seconds at 50kW / m 2 The non-combustibility was evaluated by measuring the total heat generation amount and applying radiant heat of 1000 MJ / m2 and inducing ignition with a discharge plug. These measurements and evaluations were carried out in accordance with ISO5660-1:2002, and the standard for non-combustible materials was (1) a total heat generation amount of 8 MJ / m2 after 20 minutes of heating. 2 (2) The maximum heat generation rate is 200 kW / m continuously for more than 10 seconds. 2 and (3) there are no cracks or holes that extend through to the back surface and are harmful to fire safety.
[0029] (Adhesion evaluation) According to JISK5600-5-6:1999 (coating adhesion cross-cut method), evaluation was performed under non-humid and humid conditions. First, two test pieces of 100 mm x 100 mm were cut out from the phenol foam laminated board without changing the thickness, and six cuts were made with a cutter knife on the surface of the acrylic polymer latex mixture layer at intervals of 2 mm in a vertical and horizontal grid pattern so as to penetrate to the surface of the substrate, forming 5 x 5 = 25 grid patterns, and then Cellotape (registered trademark) was firmly attached to the grid pattern forming part of one of the test pieces, and then peeled off in one go, and the number of peeled squares out of the 25 grid patterns was counted, and the ratio (%) of the peeled area was calculated, and adhesion (%) = 100 - peeled area ratio (%) (evaluation under non-humid conditions).
[0030] Next, the other test specimen was floated on the water surface at room temperature for 2 hours so that the lattice pattern-formed surface was in contact with water, and then dried for 30 minutes at 60° C. Thereafter, Cellotape (registered trademark) was firmly attached to the lattice pattern-formed portion of the test specimen, and then it was peeled off in one go, and the number of squares where the coating film had peeled off among the 25 lattice patterns was counted, and the percentage of the peeled area was calculated as adhesion (%) = 100 - peeled area percentage (%) (evaluation under wet conditions).
[0031] Example 1 The coating liquid was prepared by mixing 100 parts by mass of an acrylic acid ester copolymer latex mixture (viscosity 100 mPa s (23°C), solid content 40%, minimum film formation temperature 25°C) as the acrylic polymer latex, 0.5 parts by mass of a mixture of dodecanol and tridecanol in a mass ratio of 1:1, and 900 parts by mass of vermiculite as silicon oxide and magnesium oxide. The coating amount was 60 g / m 2 The laminate was dried at 110° C. for 10 minutes to obtain a phenol foam laminate.
[0032] Example 2 A phenol foam laminate was obtained in the same manner as in Example 1, except that the drying conditions were changed to 80° C. and 6 minutes.
[0033] Comparative Example 1 A phenol foam laminate was obtained in the same manner as in Example 1, except that 0.5 parts by mass of dodecanol was used instead of 0.5 parts by mass of the mixture of dodecanol and tridecanol in a mass ratio of 1:1 in Example 1.
[0034] Comparative Example 2 A phenol foam laminate was obtained in the same manner as in Example 1, except that 0.5 parts by mass of tridecanol was used instead of 0.5 parts by mass of the mixture of dodecanol and tridecanol in a mass ratio of 1:1 in Example 1.
[0035] Comparative Example 3 A phenol foam laminate was obtained in the same manner as in Example 1, except that dodecanol and tridecanol were not mixed.
[0036] The evaluation results for the examples and comparative examples are summarized in Table 1.
[0037] [Table 1] [Industrial Applicability]
[0038] The phenol foam laminate of the present invention can be suitably used in the construction and various other industrial fields.
Claims
1. A phenol foam laminate comprising a board containing magnesium silicate and / or calcium silicate laminated on one or both sides of a phenol foam plate, and an acrylic polymer latex mixture layer containing at least any two components selected from alcohols having 12 to 14 carbon atoms, silicon oxide, magnesium oxide, and an acrylic polymer latex formed on the outer surface of the board.
2. The phenolic foam laminate according to claim 1 , further comprising a resin fiber layer formed between the phenolic foam plate and the board.
3. The phenol foam laminate according to claim 1 or 2, wherein the adhesion of the acrylic polymer latex mixture layer is 50% or more after a peel test according to JIS K5600-5-6:1999, which is carried out after forming six cut lines at 2 mm intervals in a grid pattern on the acrylic polymer latex mixture layer, contacting the layer with water at room temperature for 2 hours, and drying the layer at 60°C for 30 minutes.
Citation Information
Patent Citations
Incombustible coating liquid, incombustible material and incombustible heat insulation panel
JP2013245414A
Noncombustible heat insulating panel
JP2004100228A
Non-flammable paper, impregnated paper and compounded paper
JP2008163508A