Polyol compound and method for producing the same, composition and method for producing the same, urethane resin and aqueous urethane resin dispersion

A novel polyol compound and composition through a transesterification reaction addresses the compatibility issues of existing urethane resins, providing enhanced durability and mechanical properties for diverse applications.

JP2024146589APending Publication Date: 2024-10-15TOSOH CORP
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2023059585
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-31
Publication Date
2024-10-15

AI Technical Summary

Technical Problem

Existing urethane resins derived from polycarbonate, polyether, and polyester polyols lack compatibility in achieving flexibility, low-temperature properties, and heat resistance simultaneously.

Method used

A novel polyol compound and composition are developed through a transesterification reaction between polyhydric alcohols, cyclic esters, and diols, with specific molar ratios and structures to form urethane resins that balance flexibility, low-temperature properties, and heat resistance, and can be used in aqueous dispersions.

Benefits of technology

The solution provides urethane resins with enhanced durability, mechanical properties, and compatibility across various temperature ranges, suitable for applications in coatings, adhesives, and paints.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024146589000060
    Figure 2024146589000060
  • Figure 2024146589000001
    Figure 2024146589000001
  • Figure 2024146589000002
    Figure 2024146589000002
Patent Text Reader

Abstract

To provide a new polyol compound useful as a raw material for a urethane resin or the like and to provide a urethane resin made from the polyol compound.SOLUTION: There is provided a polyol compound (A-1) represented by the following formula (A-1) [wherein, R1 represents a hydrogen atom, an alkyl group or a hydroxyalkyl group, R2 represents an alkanediyl group or *1-Ra-C(=O)-O-Rb-*2, Ra and Rb each independently represent an alkanediyl group, *1 represents a bonding moiety with a carbonyl group, *2 represents a bonding moiety with an oxygen atom, n1 represents an integer of 1 or more, and when n1 is 2 or more, a plurality of R2 may be identical or different from each other].SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a polyol compound and a method for producing the same, a composition and a method for producing the same, a urethane resin, and an aqueous urethane resin dispersion. [Background technology]

[0002] Like polycarbonate polyols, polyether polyols, and the like, polyester polyols are useful as raw materials for producing urethane resins (also called polyurethane resins) by reacting them with polyisocyanate compounds, and are useful as raw materials for adhesives, paints, and the like.

[0003] Polycarbonate polyol has a carbonate bond, so urethane resins obtained from polycarbonate polyol have excellent durability but have the disadvantage of poor low-temperature properties. Polyether polyol has an ether bond, so urethane resins obtained from polyether polyol have excellent low-temperature properties but have the disadvantage of poor weather resistance and heat resistance. In contrast, urethane resins obtained from polyester polyols tend to have excellent low-temperature properties and heat resistance.

[0004] The polyester polyol is produced by reacting a cyclic lactone with a diol, or a diol with a dicarboxylic acid and / or anhydride thereof, in the presence of a transesterification catalyst (transesterification reaction).

[0005] Up to now, polyester polyols with various structures have been proposed depending on the purpose. For example, Patent Document 1 proposes a polyester polyol obtained by transesterification between an aromatic dicarboxylic acid and / or its anhydride, a triol compound, and a diol, and Patent Document 2 proposes a polyester polyol obtained by transesterification between a triol compound and a cyclic ester. [Prior art documents] [Patent documents]

[0006] [Patent Document 1] Japanese Patent Application Publication No. 59-09118 [Patent Document 2] International Publication No. 2004 / 087783 Summary of the Invention [Problem to be solved by the invention]

[0007] The object of the present invention is to provide a novel polyol compound useful as a raw material for urethane resins, etc., and a urethane resin made from the polyol compound. Another object of the present invention is to provide a composition containing the polyol compound, and a urethane resin made from the composition. Another object of the present invention is to provide a composition that contributes to the formation of a urethane resin that is compatible with flexibility, low-temperature properties, and heat resistance. Another object of the present invention is to provide an aqueous urethane resin dispersion containing the urethane resin having an acidic group. [Means for solving the problem]

[0008] The present invention provides the following [1] to

[23] .

[0009] [1] A polyol compound (A-1) represented by the following formula (A-1):

[0010] [ka]

[0011] [In formula (A-1), R 1 represents a hydrogen atom, an alkyl group, or a hydroxyalkyl group, R 2 is an alkanediyl group, or *1-R a -C(=O)-OR b -*2, R a , and R b each independently represents an alkanediyl group, *1 indicates the bonding site with the carbonyl group, *2 indicates the bonding site with the oxygen atom, n 1 indicates an integer of 1 or greater. n 1 If is 2 or more, there are multiple R 2 may be the same or different.]

[0012] [2] R 2 The polyol compound (A-1) according to [1], wherein all of the above are linear alkanediyl groups.

[0013] [3] R 2 The polyol compound (A-1) according to [1], wherein all of the above are 1,5-pentanediyl groups.

[0014] [4] A reaction product of a polyhydric alcohol (B) and a cyclic ester (C), or The polyol compound (A-1) according to any one of [1] to [3] above, which is a reaction product of a polyhydric alcohol (B), a cyclic ester (C), and a diol (D).

[0015] [ka]

[0016] [In formula (B), R 1 has the same meaning as above.]

[0017] [5] A polyol compound (A-1) according to any one of [1] to [4], A composition comprising a polyol compound (A-2) represented by the following formula (A-2):

[0018] [ka]

[0019] [In formula (A-2), R 1 represents a hydrogen atom, an alkyl group, or a hydroxyalkyl group, R2 is an alkanediyl group, or *1-R a -C(=O)-OR b -*2, *1 indicates the bonding site with the carbonyl group, *2 indicates the bonding site with the oxygen atom, n 2 and m 2 each independently represents an integer of 1 or more. Multiple R's 2 may be the same or different.]

[0020] [6] A composition comprising the composition according to [5] and a polyhydric alcohol represented by the following formula (B):

[0021] [ka]

[0022] [In formula (B), R 1 has the same meaning as above.]

[0023] [7] The total number of moles of the group represented by the following formula (a-1) contained in the composition is C A1 The total number of moles of the polyhydric alcohol contained in the composition is C B Then, Molar ratio (C A1 / C B ) is 0.025 to 150.

[0024] [ka]

[0025] [In formula (a-1), R 1 is as defined above, and * indicates a bond to the alkanediyl group.

[0026] [8] The total number of moles of the group represented by the following formula (a-2) contained in the composition is C A2 The total number of moles of the polyhydric alcohol contained in the composition is CB Then, Molar ratio (C A2 / C B ) is 0.020 to 150.

[0027] [ka]

[0028] [In formula (a-2), R 1 is as defined above, and * indicates a bond to the alkanediyl group.

[0029] [9] The total number of moles of the group represented by the following formula (a-1) contained in the composition is C A1 The total number of moles of the group represented by the following formula (I) contained in the composition is C T Then, Molar ratio (C A1 / C T The composition according to any one of [6] to [8], wherein the value of (i) is 0.025 to 0.99.

[0030] [ka]

[0031] [In formula (a-1), R 1 is as defined above, and * indicates a bond to the alkanediyl group.

[0032] [ka]

[0033] [In formula (I), R 1 has the same meaning as above, and * indicates a bond.

[0034]

[10] The total number of moles of the group represented by the following formula (a-2) contained in the composition is C A2 The total number of moles of the group represented by the following formula (I) contained in the composition is C T Then, Molar ratio (C A2 / C T The composition according to any one of [6] to [9], wherein the value of (i) is 0.020 to 0.99.

[0035] [ka]

[0036] [In formula (a-2), R 1 is as defined above, and * indicates a bond to the alkanediyl group.

[0037] [ka]

[0038] [In formula (I), R 1 has the same meaning as above, and * indicates a bond.

[0039]

[11] The total moles of the polyhydric alcohol contained in the composition is C B The total number of moles of the group represented by the following formula (I) contained in the composition is C T Then, Molar ratio (C B / C T The composition according to any one of [6] to

[10] , wherein the ratio of the molecular weight of the polymer to the molecular weight of the solid is 0.001 to 0.950.

[0040] [ka]

[0041] [In formula (I), R 1 has the same meaning as above, and * indicates a bond.

[0042]

[12] The total moles of the polyhydric alcohol contained in the composition is C B The total number of moles of the group represented by the following formula (I) contained in the composition is C T Then, Molar ratio (C B / CT The composition according to any one of [6] to

[11] , wherein the ratio of the molecular weight of the polymer to the molecular weight of the solid is 0.001 to 0.950.

[0043] [ka]

[0044] [In formula (I), R 1 has the same meaning as above, and * indicates a bond.

[13] The composition according to any one of [5] to

[12] , further comprising a polyester polyol represented by the following formula (A-3):

[0045] [ka]

[0046] [In formula (A-3), R 1 represents a hydrogen atom, an alkyl group, or a hydroxyalkyl group, R 2 is an alkanediyl group, or *1-R a -C(=O)-OR b -*2, R a , and R b each independently represents an alkanediyl group, *1 indicates the bonding site with the carbonyl group, *2 indicates the bonding site with the oxygen atom, n 3 , m 3 and p 3 each independently represents an integer of 1 or more. Multiple R's 2 may be the same or different.]

[0047]

[14] A polycondensate of a polyol component and a polyisocyanate component or a crosslinked product thereof, The polyol component comprises the composition according to any one of the above items [5] to

[13] .

[0048]

[15] The urethane resin according to

[14] , wherein the polyol component further contains a polyhydric alcohol represented by the following formula (B):

[0049] [ka] [In formula (B), R 1 has the same meaning as above.]

[0050]

[16] The total number of moles of the group represented by the following formula (a-1) contained in the polyol component is C A1 The total number of moles of the polyhydric alcohol contained in the polyol component is C B Then, the molar ratio (C A1 / C B ) is 0.025 to 150.

[0051] [ka] [In formula (a-1), R 1 is as defined above, and * indicates a bond to the alkanediyl group.

[0052]

[17] The total number of moles of the group represented by the following formula (a-2) contained in the polyol component is C A2 The total number of moles of the polyhydric alcohol contained in the polyol component is C B Then, Molar ratio (C A2 / C B ) is 0.020 to 150.

[0053] [ka]

[0054] [In formula (a-2), R 1 is as defined above, and * indicates a bond to the alkanediyl group.

[0055]

[18] The total number of moles of the group represented by the following formula (a-1) contained in the polyol component is C A1 The total number of moles of the group represented by the following formula (I) contained in the polyol component is C T Then, the molar ratio (C A1 / C T ) is 0.025 to 0.99.

[0056] [ka]

[0057] [In formula (a-1), R 1 is as defined above, and * indicates a bond to the alkanediyl group.

[0058] [ka]

[0059] [In formula (I), R 1 has the same meaning as above, and * indicates a bond.

[0060]

[19] The total number of moles of the group represented by the following formula (a-2) contained in the polyol component is C A2 The total number of moles of the group represented by the following formula (I) contained in the polyol component is C T Then, the molar ratio (C A2 / C T ) is 0.020 to 0.99.

[0061] [ka]

[0062] [In formula (a-2), R 1 is as defined above, and * indicates a bond to the alkanediyl group.

[0063] [ka]

[0064] [In formula (I), R 1 has the same meaning as above, and * indicates a bond.

[0065]

[20] The total moles of the polyhydric alcohol contained in the polyol component is C B The total number of moles of the group represented by the following formula (I) contained in the polyol component is C T Then, the molar ratio (C B / C T ) is 0.001 to 0.950.

[0066] [ka]

[0067] [In formula (I), R 1 has the same meaning as above, and * indicates a bond.

[0068]

[21] The urethane resin according to any one of

[14] to

[20] , wherein the polyol component further contains a polyester polyol represented by the following formula (A-3):

[0069] [ka]

[0070] [In formula (A-3), R 1 represents a hydrogen atom, an alkyl group, or a hydroxyalkyl group, R 2 is an alkanediyl group, or *1-R a -C(=O)-OR b -*2, R a , and R b each independently represents an alkanediyl group, *1 indicates the bonding site with the carbonyl group, *2 indicates the bonding site with the oxygen atom, n 3 , m 3 and p 3 Each represents an integer of 1 or more. Multiple R's 2 may be the same or different.]

[0071]

[22] The urethane resin according to any one of

[14] to

[20] , wherein the polyol component further contains a polyol having an acidic group.

[0072]

[23] An aqueous urethane resin dispersion comprising an aqueous medium and the urethane resin or neutralized product thereof according to

[22] dispersed in the aqueous medium. Effect of the Invention

[0073] According to the present invention, it is possible to provide a novel polyol compound useful as a raw material for urethane resins, etc., and a urethane resin made from the polyol compound. According to the present invention, it is also possible to provide a composition containing the polyol compound, and a urethane resin made from the composition. According to the present invention, it is also possible to provide a composition that contributes to the formation of a urethane resin that is compatible with flexibility, low-temperature properties, and heat resistance. According to the present invention, it is also possible to provide an aqueous urethane resin dispersion containing the urethane resin having an acidic group. [Brief description of the drawings]

[0074] [Figure 1] FIG. 1 is a diagram showing a 1H-NMR spectrum of the composition containing the polyester polyol obtained in Example 2. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0075] Hereinafter, the embodiments of the present invention will be described in detail. In this specification, a numerical range indicated with "~" indicates a range including the numerical values ​​before and after "~" as the minimum and maximum values, respectively. The minimum or maximum value of a numerical range indicated with "~" can be arbitrarily combined with the maximum or minimum value of another numerical range indicated with "~". In addition, the upper and lower limit values ​​individually indicated can also be arbitrarily combined.

[0076] <Compound of one reactant> <Polyol compound (A-1)> The polyol compound (A-1) of one embodiment is a compound represented by the following formula (A-1) (hereinafter also referred to as "compound (A-1)").

[0077] [ka]

[0078] [In formula (A-1), R 1 represents a hydrogen atom, an alkyl group, or a hydroxyalkyl group, R 2 is an alkanediyl group, or *1-R a -C(=O)-OR b -*2, R a , and R b each independently represents an alkanediyl group, *1 indicates the bonding site with the carbonyl group, *2 indicates the bonding site with the oxygen atom, n 1 indicates an integer of 1 or greater. n 1 If is 2 or more, there are multiple R 2 may be the same or different.]

[0079] R 1The alkyl group and hydroxyalkyl group represented by the formula (I) may be linear or branched. The number of carbon atoms in the alkyl group and hydroxyalkyl group is, for example, 1 to 5, and may be 1 to 4 or 1 to 2. Specific examples of the alkyl group and hydroxyalkyl group include a methyl group, an ethyl group, a propyl group, a butyl group, a pentyl group, a hydroxymethyl group, a hydroxyethyl group, a hydroxypropyl group, and a hydroxybutyl group. R 1 is preferably an alkyl group or a hydroxyalkyl group, and more preferably an alkyl group or a hydroxyalkyl group having 1 to 2 carbon atoms.

[0080] R 2 The alkanediyl group represented by the formula R may be linear or branched. 2 When two or more types are present, all of them may be linear alkanediyl groups or branched alkanediyl groups, or a part of them may be linear alkanediyl groups and the other part may be branched alkanediyl groups. The number of carbon atoms of the alkanediyl group is, for example, 2 to 10. Specific examples of alkanediyl groups include an ethanediyl group, a 1,2-propanediyl group, a 1,3-propanediyl group, a 1,2-butanediyl group, a 1,3-butanediyl group, a 1,4-butanediyl group, a 1,5-pentanediyl group, a 2,2-dimethyl-1,3-propanediyl group, a 1,6-hexanediyl group, a 3-methyl-1,5-pentanediyl group, a 1,8-octanediyl group, a 2-ethyl-1,6-hexanediyl group, a 1,9-nonanediyl group, a 2-methyloctane-1,8-diyl group, and a 2-butyl-2-ethyl-1,3-propanediyl group.

[0081] R a , and R b The alkanediyl group represented by R may be the same as the alkanediyl group described above. a , and R b The number of carbon atoms of the alkanediyl group represented by R may be, for example, 2 to 10. aWhen two or more types of alkanediyl groups represented by the formula (I) are present, all of them may be linear alkanediyl groups or branched alkanediyl groups, or some of them may be linear alkanediyl groups and the other may be branched alkanediyl groups. b When two or more types of alkanediyl groups represented by the following formula are present, all of them may be linear alkanediyl groups or branched alkanediyl groups, or some of them may be linear alkanediyl groups and the other part may be branched alkanediyl groups.

[0082] The compound (A-1) is R 2 , R a , or R b When the alkanediyl group contains two or more types of alkanediyl groups, all of them may be linear alkanediyl groups or branched alkanediyl groups, or some of them may be linear alkanediyl groups and the other parts may be branched alkanediyl groups.

[0083] n 1 may be 1 to 65, or may be 2 to 60, or 2 to 55.

[0084] The number average molecular weight of the compound (A-1) is, for example, 200 to 6000. Here, the number average molecular weight is the number average molecular weight in terms of a difunctional polyoxypropylene polyol, measured using GPC (gel permeation chromatography).

[0085] The hydroxyl value of the compound (A-1) is, for example, 30 to 800 mgKOH / g. Here, the hydroxyl value means the number of milligrams (mg) of potassium hydroxide equivalent to the hydroxyl group in 1 g of the compound (A-1), and is measured in accordance with JIS K1557-1.

[0086] The state of the compound (A-1) is not particularly limited, and may be a solid at 25° C. or a liquid at 25° C. The state of the compound (A-1) is determined by adding R 2 , R a and R bThe amount of alkanediyl group contained in the compound (A-1) can be changed depending on the type of alkanediyl group (the number of carbon atoms, the presence or absence of branching, etc.), the hydroxyl value of the compound (A-1), etc. For example, when multiple types of alkanediyl groups are present, when the alkanediyl group is branched, or when the hydroxyl value of the compound (A-1) is high, the compound (A-1) tends to become a liquid at 25°C.

[0087] Furthermore, in the present embodiment, when the compound (A-1) is used as a raw material for a urethane resin, a urethane resin having excellent durability such as heat resistance, moist heat resistance, hot water resistance, etc. is easily formed. 2 More preferably, is an alkanediyl group.

[0088] In this embodiment, when used as a raw material for a urethane resin, a urethane resin having excellent mechanical properties is easily formed. 2 More preferably, is a 1,5-pentanediyl group.

[0089] <Composition, compound of two reactants> The composition of one embodiment comprises a polyol compound (A-1) and and a polyol compound (A-2) (hereinafter also referred to as "compound (A-2)") represented by the following formula (A-2).

[0090] [ka]

[0091] [In formula (A-2), R 1 represents a hydrogen atom, an alkyl group, or a hydroxyalkyl group, R 2 is an alkanediyl group, or *1-R a -C(=O)-OR b -*2, *1 indicates the bonding site with the carbonyl group, *2 indicates the bonding site with the oxygen atom, n 2 and m 2 each independently represents an integer of 1 or more. Multiple R's 2 may be the same or different.]

[0092] Compound (A-2) contains R 1 The atom or group contained as R in compound (A-1) 1 The atom or group may be the same as that contained in the compound (A-1) as R 1 When R contains two or more kinds of atoms or groups, the compound (A-2) also contains R 1 In this case, compound (A-2) may contain two or more kinds of atoms or groups as R 1 The combination of atoms or groups contained as R in compound (A-1) is 1 may be the same as the combination of atoms or groups included as

[0093] Compound (A-2) contains R 2 , R a , and R b The alkanediyl group contained as R in the compound (A-1) is 2 , R a , and R b The alkanediyl group may be the same as that contained in the compound (A-1) as R 2 , R a , and R b When R contains two or more kinds of alkanediyl groups, the compound (A-2) also contains R 2 , R a , and R b In this case, compound (A-2) may contain two or more kinds of alkanediyl groups as R 2 , R a , and R b The combination of alkanediyl groups contained as R 2 , R a , and R b The combination of alkanediyl groups may be the same as that contained in the above formula (1).

[0094] n 2 and m 2 may each independently be 1 to 65, 2 to 60, or 2 to 55.

[0095] The number average molecular weight of the compound (A-2) is, for example, 200 to 6000. Here, the number average molecular weight is the number average molecular weight in terms of a difunctional polyoxypropylene polyol, measured using GPC (gel permeation chromatography).

[0096] The hydroxyl value of the compound (A-2) is, for example, 30 to 800 mgKOH / g. Here, the hydroxyl value means the number of milligrams (mg) of potassium hydroxide equivalent to the hydroxyl group in 1 g of the compound (A-2), and is measured in accordance with JIS K1557-1.

[0097] The state of the compound (A-2) is not particularly limited, and may be a solid at 25° C. or a liquid at 25° C. The state of the compound (A-2) is determined by adding R 2 , R a and R b The amount of alkanediyl group contained in the compound (A-2) can be changed depending on the type of alkanediyl group (the number of carbon atoms, the presence or absence of branching, etc.), the hydroxyl value of the compound (A-2), etc. For example, when multiple types of alkanediyl groups are present, when the alkanediyl group is branched, or when the hydroxyl value of the compound (A-2) is high, the compound (A-2) tends to become a liquid at 25°C.

[0098] Furthermore, in the present embodiment, when the compound (A-1) is used as a raw material for a urethane resin, a urethane resin having excellent durability such as heat resistance, moist heat resistance, hot water resistance, etc. is easily formed. 2 More preferably, is an alkanediyl group.

[0099] In this embodiment, when used as a raw material for a urethane resin, a urethane resin having excellent mechanical properties is easily formed. 2 More preferably, is a 1,5-pentanediyl group.

[0100] <Raw materials> Each of the compounds (A-1) and (A-2) described above may be, for example, a reaction product of a polyhydric alcohol represented by the following formula (B) (hereinafter also referred to as "polyhydric alcohol (B)") and a cyclic ester represented by the following formula (C) (hereinafter also referred to as "cyclic ester (C)"); a reaction product of a polyhydric alcohol (B), a cyclic ester (C), and a diol (D) represented by the following formula (D) (hereinafter also referred to as "diol (D)"); a reaction product of a polyhydric alcohol (B), a diol (D), and a dicarboxylic acid and / or anhydride thereof represented by the following formula (E) (hereinafter also referred to as "dicarboxylic acid and / or anhydride thereof (E)"); or a reaction product of a polyhydric alcohol (B), a cyclic ester (C), a diol (D), and a dicarboxylic acid and / or anhydride thereof (E). Compound (A-1) and compound (A-2) can be obtained by reacting one and / or two of the hydroxyl groups of polyhydric alcohol (B) with a reaction product of cyclic ester (C) and / or dicarboxylic acid and / or its anhydride (E).

[0101] [ka]

[0102] [In formula (B), R 1 has the same meaning as above.]

[0103] [ka]

[0104] [In formula (C), R c represents an alkanediyl group.

[0105] [ka]

[0106] [In formula (D), R d represents an alkanediyl group.

[0107] [ka]

[0108] [In formula (E), R e and R e’ represents an alkanediyl group.

[0109] Specific examples of the polyhydric alcohol (B) include trimethylolpropane, trimethylolethane, and pentaerythritol. These may be used alone or in combination of two or more.

[0110] Specific examples of the cyclic ester (C) include, for example, β-propiolactone, β-butyrolactone, γ-butyrolactone, β-valerolactone, γ-valerolactone, δ-valerolactone, α-caprolactone, β-caprolactone, γ-caprolactone, δ-caprolactone, ε-caprolactone, α-methyl-ε-caprolactone, β-methyl-ε-caprolactone, 4-methylcaprolactone, γ-caprylolactone, ε-caprylolactone, ε-palmitolactone, and the like, and combinations of any two or more of these. Among them, from the viewpoints of stability during polymerization and economy, ring-opening addition polymers of ε-caprolactone using ethylene glycol, 1,3-propanediol, 1,4-butanediol, 1,5-pentanediol, 1,6-hexanediol, 1,9-nonanediol, 3-methyl-1,5-pentanediol, 2-methyl-1,8-octanediol, etc. as initiators are preferred. These may be used alone or in combination of two or more.

[0111] Specific examples of the diol (D) include ethylene glycol, 1,2-propanediol, 1,3-propanediol, 1,2-butanediol, 1,3-butanediol, 1,4-butanediol, 1,5-pentanediol, 2,2-dimethyl-1,3-propanediol, 1,6-hexanediol, 3-methyl-1,5-pentanediol, 1,8-octanediol, 2-ethyl-1,6-hexanediol, 1,9-nonanediol, 2-methyloctane-1,8-diol, and 2-butyl-2-ethyl-1,3-propanediol. These may be used alone or in combination of two or more.

[0112] Examples of the dicarboxylic acid and / or anhydride thereof (E) include phthalic acid, isophthalic acid, terephthalic acid, tetrahydrophthalic acid, hexahydrophthalic acid, cyclohexanedicarboxylic acid, maleic acid, fumaric acid, oxalic acid, malonic acid, succinic acid, glutaric acid, adipic acid, pimelic acid, suberic acid, sebacic acid, dodecanedioic acid, hydrogenated dimer fatty acid, and the like, tartaric acid, and anhydrides thereof, and combinations of any two or more thereof.

[0113] At least one of the hydroxyl groups in the compound (A-1) and at least two of the hydroxyl groups in the compound (A-2) are, for example, hydroxyl groups derived from the polyhydric alcohol (B) (unreacted hydroxyl groups in the polyhydric alcohol (B)). Due to the influence of steric hindrance, the hydroxyl groups tend to be less reactive than the hydroxyl groups derived from the reaction product of the cyclic ester (C) and / or the diol (D). In addition, the hydroxyl groups derived from the polyhydric alcohol (B) may form branched (R 1The length from the hydroxyl group to the carbon atom bonded to the cyclic ester (C) is shorter than the length from the hydroxyl group derived from the reaction product of the cyclic ester (C) and / or the diol (D) to the branch, and therefore the urethane resin obtained by the reaction of compound (A-1) (and compound (A-2)) with an isocyanate compound tends to have higher rigidity. Compound (A-1) and compound (A-2) are expected to be used as raw materials for a variety of urethane resins, taking advantage of the difference in the reactivity of the hydroxyl group and the length from the hydroxyl group to the branch.

[0114] In this embodiment, from the viewpoint that a urethane resin having excellent durability such as heat resistance or moist heat resistance is likely to be formed when used as a raw material for a urethane resin, compound (A-1) and / or compound (A-2) are more preferably a reaction product of the polyhydric alcohol (B) and the cyclic ester (C), or of the polyhydric alcohol (B), the cyclic ester (C), and the diol (D).

[0115] The composition may further contain a polyhydric alcohol (B) in addition to the compound (A-1) and the compound (A-2).

[0116] The polyhydric alcohol (B) has the same meaning as described above, and the polyhydric alcohol (B) is R 1 The atom or group contained as R in compound (A-1) and / or compound (A-2). 1 The atom or group may be the same as that contained in the compound (A-1) and / or the compound (A-2) as R 1 When the polyhydric alcohol (B) contains two or more kinds of atoms or groups as R 1 In this case, the polyhydric alcohol (B) may contain two or more kinds of atoms or groups as R 1 The combination of atoms or groups contained as R in the compound (A-1) and / or the compound (A-2) is 1 may be the same as the combination of atoms or groups included as

[0117] The total number of moles of the group represented by the following formula (a-1) contained in the composition is C A1The total number of moles of the group represented by the following formula (a-2) contained in the composition is C A2 The total number of moles of the polyhydric alcohol (B) contained in the composition is C B Then, the molar ratio (C A1 / C B ) may be 0.025 to 150, and the molar ratio (C A2 / C B The molar ratio (C) may be 0.020 to 150. A1 / C B ) and / or molar ratio (C A2 / C B ) within the above range, when the composition is used as a raw material for a urethane resin, a urethane resin that has flexibility, low-temperature properties, and heat resistance all at the same time tends to be formed.

[0118] [ka]

[0119] [In formula (a-1), R 1 is as defined above, and * indicates a bond to the alkanediyl group.

[0120] [ka]

[0121] [In formula (a-2), R 1 is as defined above, and * indicates a bond to the alkanediyl group.

[0122] Molar ratio (C A1 / C B ), molar ratio (C A2 / C B ) is, for example, a measurement of the composition using deuterated chloroform as a solvent and tetramethylsilane as a standard substance. 1 H-NMR measurement and the results obtained by the measurement 1It can be determined from the integral value of the signal in the H-NMR spectrum. Specifically, for example, the integral value Δ S1 (4 mol of hydrogen atoms) and the integral value of the methylene signal (Sb) located next to the hydroxyl group of polyhydric alcohol (B) Δ Sb (6 mol of hydrogen atoms) and the molar ratio (C A1 / C B ) can be calculated, and the integral value Δ S1 (2 mol of hydrogen atoms) and the integral value of the above signal (Sb) Δ Sb (6 mol of hydrogen atoms) and the molar ratio (C A2 / C B In this case, the molar ratio (C A1 / C B ) is the integral value of the signal (S1) Δ S1 and the integral value of the signal (Sb) Δ Sb 1.5 times the ratio (1.5 × Δ S1 / Δ Sb ), molar ratio (C A2 / C B ) is the integral value of the signal (S2) Δ S2 and the integral value of the signal (Sb) Δ Sb Three times the ratio (3×Δ S2 / Δ Sb ), which can be rephrased as:

[0123] The composition may further contain a polyester polyol represented by the following formula (A-3) (hereinafter referred to as "compound (A-3)").

[0124] [ka]

[0125] [In formula (A-3), R 1 represents a hydrogen atom, an alkyl group, or a hydroxyalkyl group, R 2 is an alkanediyl group, or *1-Ra -C(=O)-OR b -*2, R a , and R b each independently represents an alkanediyl group, *1 indicates the bonding site with the carbonyl group, *2 indicates the bonding site with the oxygen atom, n 3 , m 3 and p 3 Each represents an integer of 1 or more. Multiple R's 2 may be the same or different.]

[0126] Compound (A-3) contains R 1 The atom or group contained as R in compound (A-1) and / or compound (A-2). 1 The atom or group may be the same as that contained in the compound (A-1) and / or the compound (A-2) as R 1 When R contains two or more kinds of atoms or groups, the compound (A-3) also contains R 1 In this case, compound (A-3) may contain two or more kinds of atoms or groups as R 1 The combination of atoms or groups contained as R in the compound (A-1) and / or the compound (A-2) is 1 may be the same as the combination of atoms or groups included as

[0127] Compound (A-3) contains R 2 , R a , and R b The alkanediyl group contained as R 2 , R a , and R b The alkanediyl group contained in the compound (A-1) and / or the compound (A-2) may be the same as the alkanediyl group contained in the compound (A-1) and / or the compound (A-2) as R 2 , R a , and R b When R contains two or more kinds of alkanediyl groups, the compound (A-3) also contains R 2 , R a , and R bIn this case, compound (A-3) may contain two or more kinds of alkanediyl groups as R 2 , R a , and R b The combination of alkanediyl groups contained as R 2 , R a , and R b The combination of alkanediyl groups may be the same as that contained in the above formula (1).

[0128] n 3 , m 3 and p 3 may each independently be 1 to 65, 2 to 60, or 3 to 50.

[0129] Furthermore, in the present embodiment, when used as a raw material for a urethane resin, a urethane resin having excellent durability such as heat resistance, moist heat resistance, hot water resistance, etc. is easily formed. 2 More preferably, is an alkanediyl group.

[0130] In this embodiment, when used as a raw material for a urethane resin, a urethane resin having excellent mechanical properties is easily formed. 2 More preferably, is a 1,5-pentanediyl group.

[0131] The total number of moles of the group represented by the above formula (a-1) contained in the composition is C A1 The total number of moles of the groups represented by the above formula (a-2) is C A2 The total number of moles of the polyhydric alcohol contained in the composition is C B The total number of moles of the group represented by the following formula (I) contained in the composition is C T Then, the molar ratio (C A1 / C T ) may be 0.025 to 0.99, and the molar ratio (C A2 / C T ) may be 0.025 to 0.99, and the molar ratio (C B / C TThe molar ratio (C A1 / C T ), molar ratio (C A1 / C T ) and molar ratio (C B / C T ) are each within the above range, when the composition is used as a raw material for a urethane resin, a urethane resin that exhibits flexibility, low-temperature properties, and heat resistance all at the same time tends to be formed.

[0132] [ka]

[0133] [In formula (I), R 1 has the same meaning as above, and * indicates a bond.

[0134] Molar ratio (C A1 / C T ), molar ratio (C A2 / C T ) and molar ratio (C B / C T ) is, for example, the molar ratio (C A1 / C B ) As in the above, deuterated chloroform was used as the solvent and tetramethylsilane was used as the standard substance. 1 H-NMR measurement and the results obtained by the measurement 1 It can be determined from the integral value of the signal in the H-NMR spectrum. 1 When is an alkyl group, the integral value Δ S1 (4 mol of hydrogen atoms) and R 1 (Alkyl group) terminal methyl signal (S3) integral value Δ S3 (3 mol of hydrogen atoms) from the molar ratio (C A1 / C T ) can be calculated, and the integral value Δ S2 (2 mol of hydrogen atoms) and the integral value of the above signal (S3) Δ S3 (3 mol of hydrogen atoms) from the molar ratio (C A2 / CT ) can be calculated, and the integral value of the above signal (Sb) Δ Sb (6 mol of hydrogen atoms) and the integral value of the above signal (S3) Δ S3 (3 mol of hydrogen atoms) from the molar ratio (C B / C T In this case, the molar ratio (C A1 / C T ) is the integral value of the signal (S1) Δ S1 and the integral value of the signal (S3) Δ S3 0.75 times the ratio (0.75 × Δ S1 / Δ S3 ), molar ratio (C A2 / C T ) is the integral value of the signal (S2) Δ S2 and the integral value of the signal (S3) Δ S3 1.5 times the ratio (1.5 × Δ S2 / Δ S3 ), molar ratio (C B / C T ) is the integral value of the signal (Sb) Δ Sb and the integral value of the signal (S3) Δ S3 0.5 times the ratio (0.5 × Δ Sb / Δ S3 ) can be rephrased as follows.

[0135] The composition may further contain, for example, a polycarbonate diol which is a reaction product of the cyclic ester (C) and the diol (D), or a reaction product of the diol (D) and the dicarboxylic acid and / or its anhydride (E). However, the composition preferably contains a compound having a group represented by the above formula (I) (compounds (A-1) to (A-3), polyhydric alcohol (B), etc.) as a main component. Here, the main component refers to a component (component group) having the highest mass fraction. The content of the cyclic ester (C) may be 20 to 80 mass% or 40 to 60 mass% based on the total mass of the composition. The content of the diol (D) may be 20 to 80 mass% or 40 to 60 mass% based on the total mass of the composition. The content of the dicarboxylic acid and / or its anhydride (E) may be 20 to 80 mass% or 40 to 60 mass% based on the total mass of the composition. The content of the polycarbonate diol may be 20 to 80% by mass, or 40 to 60% by mass, based on the total mass of the composition.

[0136] The composition may be a reaction mixture of polyhydric alcohol (B) and cyclic ester (C), a reaction mixture of polyhydric alcohol (B), cyclic ester (C), and diol (D), a reaction mixture of polyhydric alcohol (B), diol (D), and dicarboxylic acid and / or its anhydride (E), or a reaction mixture of polyhydric alcohol (B), cyclic ester (C), diol (D), and dicarboxylic acid and / or its anhydride (E). The above reaction is usually carried out in the presence of a transesterification catalyst, so the composition may further contain a transesterification catalyst. Diphenyl phosphoric acid is preferably used as the transesterification catalyst. The content of the transesterification catalyst may be 0.0001 to 0.100 mass% based on the total mass of the composition.

[0137] The properties of the composition are not particularly limited, and may be a solid or a liquid at 25° C. The properties of the composition can be changed depending on the types and content ratios of the components contained (e.g., compounds (A-1) to (A-3) and polyhydric alcohol (B)).

[0138] The number average molecular weight of the composition is, for example, 200 to 6000 g / mol. Here, the number average molecular weight of the composition is the number average molecular weight in terms of bifunctional polyoxypropylene polyol, measured by using GPC (Gel Permeation Chromatography) with the entire composition as the measurement subject.

[0139] The hydroxyl value of the composition is, for example, 30 to 800 mgKOH / g. Here, the hydroxyl value of the composition means the number of milligrams (mg) of potassium hydroxide equivalent to the hydroxyl groups in 1 g of the composition, and is measured in accordance with JIS K1557-1.

[0140] Deuterated chloroform was used as the solvent, and tetramethylsilane was used as the standard substance to determine the composition. 1 When H-NMR measurement is performed, for example, the above signal (S1) is 1 The signal (S2) is observed in the range of 3.55 ppm to 3.59 ppm in the H-NMR spectrum. 1 The above signal (Sb) is between 3.37 ppm and 3.47 ppm in the H-NMR spectrum. 1 In the H-NMR spectrum, the R 1 is an ethyl group, the signal (S3) is observed in the range of 0.700 ppm or more and 1.000 ppm or less, and R 1 When C is a methyl group, the signal (S3) is observed in the range of 0.700 ppm to 1.130 ppm. Therefore, the molar ratio (C A1 / C B ), molar ratio (C A2 / C B ), molar ratio (C A1 / C T ), molar ratio (C A2 / C T ) and molar ratio (C B / C T ) can be obtained.

[0141] Molar ratio in composition (C A1 / C B The lower limit of the molar ratio (C) is, for example, 0.025 or more, preferably 0.100 or more, more preferably 1.000 or more, even more preferably 4.000 or more, and particularly preferably 7.000 or more. A1 / C B The upper limit of the molar ratio (C) is, for example, 150 or less, preferably 120 or less, more preferably 90 or less, further preferably 60 or less, and particularly preferably 30 or less. A1 / C B ) within the above range, when the composition is used as a raw material for a urethane resin, a urethane resin that has flexibility, low-temperature properties, and heat resistance all at the same time tends to be formed.

[0142] Molar ratio in composition (C A2 / C B The lower limit of the molar ratio (C) is, for example, 0.020 or more, preferably 0.050 or more, more preferably 0.100 or more, even more preferably 0.500 or more, and particularly preferably 3.000 or more. A2 / C B The upper limit of the molar ratio (C) is, for example, 150 or less, preferably 120 or less, more preferably 90 or less, further preferably 60 or less, and particularly preferably 50 or less. A2 / C B ) within the above range, when the composition is used as a raw material for a urethane resin, a urethane resin that has flexibility, low-temperature properties, and heat resistance all at the same time tends to be formed.

[0143] Molar ratio in composition (C A1 / C T The lower limit of the molar ratio (C) is, for example, 0.025 or more, preferably 0.035 or more, more preferably 0.100 or more, even more preferably 1.000 or more, and particularly preferably 5.000 or more. A1 / C TThe upper limit of the molar ratio (C) is, for example, 0.990 or less, preferably 0.800 or less, more preferably 0.500 or less, even more preferably 0.400 or less, and particularly preferably 0.300 or less. A1 / C T ) within the above range, when the composition is used as a raw material for a urethane resin, a urethane resin that has flexibility, low-temperature properties, and heat resistance all at the same time tends to be formed.

[0144] Molar ratio in composition (C A2 / C T The lower limit of the molar ratio (C) is, for example, 0.020 or more, preferably 0.050 or more, more preferably 0.100 or more, even more preferably 0.150 or more, and particularly preferably 0.200 or more. A2 / C T The upper limit of the molar ratio (C) is, for example, 0.990 or less, preferably 0.800 or less, more preferably 0.500 or less, even more preferably 0.400 or less, and particularly preferably 0.300 or less. A2 / C T ) within the above range, when the composition is used as a raw material for a urethane resin, a urethane resin that has flexibility, low-temperature properties, and heat resistance all at the same time tends to be formed.

[0145] Molar ratio in composition (C B / C T The lower limit of the molar ratio (C) is, for example, 0.001 or more, preferably 0.05 or more, more preferably 0.010 or more, even more preferably 0.020 or more, and particularly preferably 0.030 or more. B / C T The upper limit of the molar ratio (C) is, for example, 0.990 or less, preferably 0.900 or less, more preferably 0.800 or less, even more preferably 0.700 or less, and particularly preferably 0.500 or less. B / C T ) within the above range, when the composition is used as a raw material for a urethane resin, a urethane resin that has flexibility, low-temperature properties, and heat resistance all at the same time tends to be formed.

[0146] <Method of producing polyester polyol and composition> In the method for producing compound (A-1) and / or compound (A-2) of the above embodiment, a mixture containing a polyhydric alcohol (B), a cyclic ester (C), and an ester exchange catalyst; a mixture containing a polyhydric alcohol (B), a diol (D), a dicarboxylic acid and / or anhydride thereof (E), and an ester exchange catalyst; or a mixture containing a polyhydric alcohol (B), a cyclic ester (C), a diol (D), a dicarboxylic acid and / or anhydride thereof (E), and an ester exchange catalyst; is subjected to a reflux reaction (ester exchange reaction) while removing water derived from the dicarboxylic acid from the reaction system when the mixture contains a dicarboxylic acid, or is heated when the mixture does not contain a dicarboxylic acid to obtain compound (A-1) and / or compound (A-2).

[0147] In the above method, the composition of the above embodiment can be obtained as a reaction mixture containing the compound (A-1) and the compound (A-2). Therefore, the above method can also be said to be a method for producing the composition of the above embodiment.

[0148] The details of the polyhydric alcohol (B), the cyclic ester (C), the diol (D) and the dicarboxylic acid and / or its anhydride (E) are as described above. 1 , R 2 , R a and R b Examples of the preferred combinations of the above) also include R 1 , R 2 , R a and R b The preferred examples and preferred combinations are the same as those of the above. As the transesterification catalyst, it is preferable to use diphenyl phosphoric acid, from the viewpoint of facilitating the production of the desired compound (A-1) and / or compound (A-2).

[0149] The mixing ratio of the polyhydric alcohol (B) and the cyclic ester (C) (content of the polyhydric alcohol (B) in the mixed solution / content of the cyclic ester (C) in the mixed solution) is preferably 1 / 40 to 1 / 1, more preferably 1 / 30 to 1 / 2, even more preferably 1 / 25 to 1 / 3, and particularly preferably 1 / 20 to 1 / 4, in terms of molar ratio. By setting the mixing ratio of the polyhydric alcohol and the cyclic ester within the above range, the compound (A-1) and / or the compound (A-2) can be obtained efficiently.

[0150] The mixing ratio of the diol (D) and the dicarboxylic acid and / or its anhydride (E) (content of the diol (D) in the mixed solution / content of the dicarboxylic acid and / or its anhydride (E) in the mixed solution) is preferably 1 / 5 to 5 / 1, more preferably 1 / 3 to 3 / 1, even more preferably 2 / 1 to 1 / 2, and particularly preferably 1.5 / 1 to 1 / 1.5. By setting the mixing ratio of the diol and the dicarboxylic acid and / or its anhydride in the above range, the compound (A-1) and / or the compound (A-2) can be efficiently obtained.

[0151] The mixing ratio of the polyhydric alcohol (B), the diol (D), and the dicarboxylic acid and / or its anhydride (E) (content of the polyhydric alcohol (B) in the mixed solution / total content of the diol (D) and the dicarboxylic acid and / or its anhydride (E) in the mixed solution) is preferably 1 / 3 to 3 / 1, more preferably 1 / 2.5 to 2.5 / 1, even more preferably 1 / 25 to 1 / 3, and particularly preferably 1 / 20 to 1 / 4, in terms of molar ratio. By setting the mixing ratio of the polyhydric alcohol and the diol to the dicarboxylic acid and / or its anhydride in the above range, the compound (A-1) and / or the compound (A-2) can be efficiently obtained.

[0152] The content of the transesterification catalyst in the mixed solution is set to be, from the viewpoint of making it easy to appropriately control the reaction temperature and suppressing an increase in the color number of the reaction product, 1) Polyhydric alcohol (B) and cyclic ester (C) in a mixture, 2) A mixture of polyhydric alcohol (B), cyclic ester (C) and diol (D), 3) A mixture of a polyhydric alcohol (B), a diol (D), and a dicarboxylic acid and / or anhydride thereof (E), or 4) A mixture of a polyhydric alcohol (B), a cyclic ester (C), a diol (D), and a dicarboxylic acid and / or anhydride thereof (E); The content of the transesterification catalyst may be 0.0001 to 0.1 parts by mass, or may be 0.0005 to 0.01 parts by mass, relative to 100 parts by mass of the total amount. From the viewpoint of easily controlling the reactivity of the urethanization reaction, the smaller the content of the transesterification catalyst, the more preferable. When the content of the transesterification catalyst is increased, the reactivity of the urethanization reaction tends to be increased.

[0153] The content of the transesterification catalyst in the mixed solution is, from the viewpoint of facilitating control of the urethane reaction, 1') Polyhydric alcohol (B) and cyclic ester (C) in a mixture, 2') Polyhydric alcohol (B), cyclic ester (C) and diol (D) in a mixture, 3') A mixture of a polyhydric alcohol (B), a diol (D), and a dicarboxylic acid and / or anhydride thereof (E), or 4') A mixture of a polyhydric alcohol (B), a cyclic ester (C), a diol (D), and a dicarboxylic acid and / or anhydride thereof (E); The amount is preferably 0.001 part by mass or more, more preferably 0.002 part by mass or more, and even more preferably 0.003 part by mass or more, relative to 100 parts by mass in total.

[0154] The content of the transesterification catalyst in the mixed liquid is, from the viewpoint of suppressing an increase in the color number of the reaction product, 1'') Polyhydric alcohol (B) and cyclic ester (C) in a mixture, 2'') A mixture of polyhydric alcohol (B), cyclic ester (C) and diol (D), 3'') A mixture of a polyhydric alcohol (B), a diol (D), and a dicarboxylic acid and / or anhydride thereof (E), or 4'') A mixture of a polyhydric alcohol (B), a cyclic ester (C), a diol (D), and a dicarboxylic acid and / or its anhydride (E); The amount is preferably 0.050 parts by mass or less, more preferably 0.040 parts by mass or less, and even more preferably 0.030 parts by mass or less, relative to a total of 100 parts by mass.

[0155] From these viewpoints, the content of the transesterification catalyst in the mixed liquid is (1) A mixture of polyhydric alcohol (B) and cyclic ester (C), (2) A mixture of polyhydric alcohol (B), cyclic ester (C) and diol (D), (3) A mixture of a polyhydric alcohol (B), a diol (D), and a dicarboxylic acid and / or anhydride thereof (E), or (4) A mixture of a polyhydric alcohol (B), a cyclic ester (C), a diol (D), and a dicarboxylic acid and / or anhydride thereof (E), The content is preferably 0.001 to 0.050 parts by mass, more preferably 0.002 to 0.040 parts by mass, and further preferably 0.003 to 0.030 parts by mass, relative to 100 parts by mass in total.

[0156] When the mixture contains a dicarboxylic acid, the heating temperature (reaction temperature) is, for example, 80 to 250°C, and may be 100 to 220°C. When the reaction temperature is 80°C or higher, the transesterification reaction easily proceeds, and the desired compound (A-1) and / or compound (A-2) are easily obtained. When the reaction temperature is 250°C or lower, the color number of the obtained compound (A-1) and / or compound (A-2) and the composition polyol is suppressed. In addition, the transesterification reaction may be carried out while keeping the temperature constant, or while increasing the temperature stepwise or continuously according to the reaction progress. From the viewpoint of making it easier to obtain the desired compound (A-1) and / or compound (A-2), it is preferable to carry out heating at a temperature T1 that satisfies the relationship of the following formula (α), and then heating at a temperature T2 that satisfies the relationship of the following formula (β). It is preferable that the temperatures T1 and T2 satisfy the relationship of the following formula (γ). In addition, the average temperature T1 of the first heating temperature is 100°C. mand the average temperature T2 of the second heating temperature m It is preferable that the relationship of the following formula (δ) is satisfied: Here, the degree of reaction progress can be estimated from the amount of distillate (water) distilled. 120℃≦T1≦190℃ (α) 160℃≦T2≦190℃ (β) T1 <T2 ···(γ) T1 m <T2 m (δ)

[0157] When the mixture contains a dicarboxylic acid, the heating can be performed under normal pressure, but in the latter half of the reaction, it can also be performed under reduced pressure (for example, under a pressure of 101 to 0.1 kPa). This can increase the distillation rate of the distillate produced, making it possible to accelerate the progress of the reaction. In this specification, normal pressure means a pressure of 101.325 kPa ± 20.000 kPa. From the viewpoint of facilitating the production of the desired compound (A-1) and / or compound (A-2), the heating of the mixture preferably includes heating under a pressure of 101.325 kPa±20.000 kPa (first heating) and then heating under a reduced pressure of 10.000 kPa or less (second heating), the temperature of the first heating is more preferably a temperature T1 that satisfies the relationship of the above formula (α), the temperature of the second heating is more preferably a temperature T2 that satisfies the relationship of the above formula (β), and the temperature of the first heating (temperature T1) and the temperature of the second heating (temperature T2) are even more preferably the relationship of the above formula (γ). Furthermore, from the viewpoint of facilitating the production of the compound (A-1) and / or compound (A-2), it is preferable to remove the water derived from the dicarboxylic acid from the reaction system by distilling it at 100° C. or less.

[0158] When the mixture does not contain a dicarboxylic acid, the mixture may be heated under normal pressure or under pressure, and the heating temperature (reaction temperature) may be, for example, 40 to 200°C, or 60 to 150°C. When the reaction temperature is 40°C or higher, the transesterification reaction is likely to proceed, and the desired compound (A-1) and / or compound (A-2) are likely to be obtained. When the reaction temperature is 200°C or lower, the color number of the obtained compound (A-1) and / or compound (A-2) and the composition polyol is suppressed. In addition, the transesterification reaction may be carried out while keeping the temperature constant, or may be carried out while increasing the temperature stepwise or continuously depending on the reaction progress. From the viewpoint of making it easier to obtain the desired compound (A-1) and / or compound (A-2), it is preferable to carry out heating at a temperature T1 that satisfies the relationship of the following formula (α'), and then heating at a temperature T2 that satisfies the relationship of the following formula (β'). It is preferable that the temperatures T1 and T2 satisfy the relationship of the following formula (γ'). Also, the average temperature T1 of the first heating m and the average temperature T2 of the second heating temperature m It is preferable that the relationship of the following formula (δ′) is satisfied. 60℃≦T1≦120℃ (α') 110℃≦T2≦120℃ (β') T1 <T2 ···(γ’) T1 m <T2 m (δ')

[0159] In the above-mentioned production method, the obtained reaction mixture may be subjected to post-treatment such as distillation and drying. In addition, in the above-mentioned production method, after obtaining the compound (A-1) and / or the compound (A-2) or a composition containing the same, a component such as a polyhydric alcohol (B) is added to obtain the composition of the above-mentioned embodiment (for example, the above-mentioned molar ratio (C A1 / C B ), the molar ratio (C A2 / C B ), molar ratio (C A1 / C T ), molar ratio (C A2 / C T ) and molar ratio (C B / C T ) may be prepared.

[0160] <Urethane resin and its manufacturing method> The urethane resin is a polycondensate of a polyol component and a polyisocyanate component, or a crosslinked product thereof. Here, the crosslinked product means a product in which polycondensates are crosslinked with each other by a chain extender or the like.

[0161] (Polyol component) The polyol component includes the above-mentioned compound (A-1) and / or compound (A-2). The polyol component may include a polyol (a compound having two or more terminal hydroxyl groups) other than the compound (A-1) and / or compound (A-2). The polyol component may further include, for example, a polyol (compound (A-3), polyhydric alcohol (B), diol (D), etc.) that may be included in the above-mentioned composition. The content ratio of these polyols is determined by the content ratio of the polyol in the above-mentioned composition (for example, molar ratio (C A1 / C B ), molar ratio (C A2 / C B ), molar ratio (C A1 / C T ), molar ratio (C A2 / C T ) and molar ratio (C B / C T In other words, the polyol component may include a polyol mixture obtained by excluding compounds other than the polyol from the above composition.

[0162] The polyol component may further contain a polyol having an acidic group. In this case, the urethane resin contains an acidic group. The urethane resin having an acidic group is preferably used in an aqueous urethane resin dispersion. The aqueous urethane resin dispersion will be described later.

[0163] The acidic group is, for example, a functional group (hydrophilic group) that can impart hydrophilicity to the isocyanate-terminated prepolymer obtained by reaction with isocyanate. Examples of polyols having such acidic groups include dimethylolalkanoic acids such as dimethylolpropionic acid (DMPA), dimethylolbutanoic acid (DMBA), dimethylolpentanoic acid, and dimethylolnonanoic acid.

[0164] (Polyisocyanate) Examples of polyisocyanates include aromatic polyisocyanates, araliphatic polyisocyanates, aliphatic polyisocyanates, and alicyclic polyisocyanates. Modified polyisocyanates, which are modified versions of these, can also be used. Examples of modified polyisocyanates include isocyanurate-modified polyisocyanates (isocyanate trimers), allophanate-modified polyisocyanates, uretdione-modified polyisocyanates, urethane-modified polyisocyanates, biuret-modified polyisocyanates, uretonimine-modified polyisocyanates, and acylurea-modified polyisocyanates. These can be used alone or in combination of two or more.

[0165] Examples of aromatic isocyanates include 2,4-tolylene diisocyanate, 2,6-tolylene diisocyanate, a mixture of 2,4-tolylene diisocyanate and 2,6-tolylene diisocyanate, 4,4'-diphenylmethane diisocyanate, 2,4'-diphenylmethane diisocyanate, a mixture of 2,4'-diphenylmethane diisocyanate and 4,4'-diphenylmethane diisocyanate, m-xylylene diisocyanate, p-xylylene diisocyanate, and 4,4'-diphenyl ether. Examples of the diisocyanates include phenyl diisocyanate, 2-nitrodiphenyl-4,4'-diisocyanate, 2,2'-diphenylpropane-4,4'-diisocyanate, 3,3'-dimethyldiphenylmethane-4,4'-diisocyanate, 4,4'-diphenylpropane diisocyanate, m-phenylene diisocyanate, p-phenylene diisocyanate, naphthylene-1,4-diisocyanate, naphthylene-1,5-diisocyanate, and 3,3'-dimethoxydiphenyl-4,4'-diisocyanate.

[0166] Examples of aromatic aliphatic isocyanates include 1,3-xylylene diisocyanate, 1,4-xylylene diisocyanate, and mixtures thereof; 1,3-bis(1-isocyanato-1-methylethyl)benzene, 1,4-bis(1-isocyanato-1-methylethyl)benzene, and mixtures thereof; ω,ω'-diisocyanato-1,4-diethylbenzene, and the like.

[0167] Examples of aliphatic isocyanates include hexamethylene diisocyanate, 1,5-pentamethylene diisocyanate, tetramethylene diisocyanate, 2-methylpentane-1,5-diisocyanate, 3-methylpentane-1,5-diisocyanate, lysine diisocyanate, trioxyethylene diisocyanate, ethylene diisocyanate, trimethylene diisocyanate, octamethylene diisocyanate, nonamethylene diisocyanate, 2,2'-dimethylpentane diisocyanate, 2,2,4-trimethylhexane diisocyanate, decamethylene diisocyanate, butene diisocyanate, 1,3-butadiene-1,4-diisocyanate, 2,4 ,4-trimethylhexamethylene diisocyanate, 1,6,11-undecane triisocyanate, 1,3,6-hexamethylene triisocyanate, 1,8-diisocyanato-4-(isocyanatomethyl)octane, 2,5,7-trimethyl-1,8-diisocyanato-5-(isocyanatomethyl)octane, bis(isocyanatoethyl)carbonate, bis(isocyanatoethyl)ether, 1,4-butylene glycol dipropyl ether-α,α'-diisocyanate, lysine diisocyanatomethyl ester, 2-isocyanatoethyl-2,6-diisocyanatohexanoate, 2-isocyanatopropyl-2,6-diisocyanatohexanoate, and the like.

[0168] Examples of alicyclic isocyanates include isophorone diisocyanate, cyclohexyl diisocyanate, bis(isocyanatomethyl)cyclohexane, dicyclohexylmethane diisocyanate, methylcyclohexyl diisocyanate, dicyclohexyldimethylmethane diisocyanate, 2,2'-dimethyldicyclohexylmethane diisocyanate, bis(4-isocyanato-n-butylidene)pentaerythritol, and hydrogenated dimer acid diisocyanate. 2-isocyanatomethyl-3-(3-isocyanatopropyl)-5-(isocyanatomethyl)bicyclo[2.2.1]heptane, 2-(isocyanatomethyl)3-(3-isocyanatopropyl)-6-(isocyanatomethyl)-bicyclo[2.2.1]heptane, 2-(isocyanatomethyl)-2-(3-isocyanatopropyl)-5-(isocyanatomethyl)bicyclo[2.2.1]heptane, 2-(isocyanatomethyl)-2-(3-isocyanatopropyl)-5-(isocyanatomethyl)bicyclo[2.2.1]heptane, 2-(isocyanatomethyl)-2-(3-isocyanatopropyl) 2-(isocyanatomethyl)-3-(3-isocyanatopropyl)-5-(2-isocyanatoethyl)bicyclo[2.2.1]heptane, 2-(isocyanatomethyl)-3-(3-isocyanatopropyl)-6-(2-isocyanatoethyl)bicyclo[2.2.1]heptane, 2-(isocyanatomethyl)-2-(3-isocyanatopropyl)-5-(2-isocyanatoethyl)bicyclo[2.2.1]heptane [2.2.1]heptane, 2-(isocyanatomethyl)-2-(3-isocyanatopropyl)-6-(2-isocyanatoethyl)bicyclo[2.2.1]heptane, 2,5-bis(isocyanatomethyl)bicyclo[2.2.1]heptane, hydrogenated diphenylmethane diisocyanate, norbornane diisocyanate, hydrogenated tolylene diisocyanate, hydrogenated xylene diisocyanate, hydrogenated tetramethylxylene diisocyanate, and the like.

[0169] (Polyol component / polyisocyanate component blend ratio) The blending ratio of the polyol component to the polyisocyanate component, expressed as the molar ratio of active hydrogen in the polyol component to isocyanate groups in the polyisocyanate component, is preferably 9:1 to 1:9, and more preferably 6:4 to 4:6. When the blending ratio is within this range, the urethane resin tends to have better performance.

[0170] (Chain extender) The chain extender can be appropriately selected depending on the purpose, application, etc. Examples of the chain extender include water, ethylene glycol, 1,3-propanediol, 1,4-butanediol, 1,5-pentanediol, 1,6-hexanediol, neopentyl glycol, 1,10-decanediol, 1,1-cyclohexanedimethanol, 1,4-cyclohexanedimethanol, tricyclodecane dimethanol, xylylene glycol, bis(p-hydroxy)diphenyl, bis(p-hydroxyphenyl)propane, 2,2-bis[4-(2-hydroxyethoxy)phenyl]propane, and bis[4-(2-hydroxyethoxy)phenyl]sulfonate. Low molecular weight polyols such as cyclohexane and 1,1-bis[4-(2-hydroxyethoxy)phenyl]cyclohexane; high molecular weight polyols such as polyester polyols, polyesteramide polyols, polyether polyols, polyether ester polyols, polyester polyols, and polyolefin polyols; and polyamines such as ethylenediamine, isophoronediamine, 2-methyl-1,5-pentanediamine, aminoethylethanolamine, diethylenetriamine, triethylenetetramine, tetraethylenepentamine, and pentaethylenehexamine can be used. The amount of the chain extender (the ratio of the structure derived from the chain extender contained in the urethane resin) may be 0.1 to 50 parts by mass relative to 100 parts by mass of the total amount of the polyol component and the polyisocyanate component. When the chain extender is a polyol, the content of the polyol is calculated assuming that it is included in both the chain extender and the polyol component.

[0171] The urethane resin can be obtained by reacting a polyol component, a polyisocyanate component, and optionally a chain extender (urethanization reaction). The urethane reaction may be carried out at room temperature (e.g., 25°C) or under heating (e.g., 40 to 150°C).

[0172] In the urethanization reaction, a catalyst (urethanization catalyst) can be added for the purpose of shortening the reaction time, improving the reaction rate, etc. Examples of the catalyst include tertiary amine catalysts such as triethylamine, triethylenediamine, tetramethylethylenediamine, tetramethylpropylenediamine, and tetramethylhexamethylenediamine, and metal catalysts such as tin-based catalysts such as stannous octoate, stannous oleate, and dibutyltin dilaurate. These can be used alone or in combination of two or more. Among these, dibutyltin dilaurate is preferably used. The amount of the catalyst used may be 0.001 to 100 parts by mass with respect to 100 parts by mass of the total amount of the polyol component and the polyisocyanate component.

[0173] When a catalyst is used in the urethanization reaction, it is preferable to use a phosphorus compound for treating the catalyst. The phosphorus compound is not particularly limited, and examples thereof include phosphate triesters such as trimethyl phosphate, triethyl phosphate, tributyl phosphate, di-2-ethylhexyl phosphate, triphenyl phosphate, tricresyl phosphate, and cresyl diphenyl phosphate; acid phosphate esters such as methyl acid phosphate, ethyl acid phosphate, propyl acid phosphate, isopropyl acid phosphate, butyl acid phosphate, lauryl acid phosphate, stearyl acid phosphate, 2-ethylhexyl acid phosphate, isodecyl acid phosphate, butoxyethyl acid phosphate, oleyl acid phosphate, tetracosyl acid phosphate, acetylene glycol acid phosphate, 2-hydroxyethyl methacrylate acid phosphate, dibutyl phosphate, monobutyl phosphate, monoisodecyl phosphate, and bis(2-ethylhexyl)phosphate; and triphenyl phosphate. phosphite, trisnonylphenyl phosphite, tricresyl phosphite, triethyl phosphite, tris(2-ethylhexyl) phosphite, tridecyl phosphite, trilauryl phosphite, tris(tridecyl) phosphite, trioleyl phosphite, diphenyl mono(2-ethylhexyl) phosphite, diphenyl monodecyl phosphite, diphenyl (monodecyl) phosphite, trilauryl phosphite, diethyl hydrogen phosphite, bis(2-ethylhexyl) Examples of such phosphite esters include bis(decyl)pentaerythritol diphosphite, tristearyl phosphite, distearyl pentaerythritol diphosphite, tris(2,4-di-tert-butylphenyl)phosphite, and other phosphite esters; phosphoric acid, phosphorous acid, and hypophosphorous acid. These may be used alone or in combination of two or more.Among these, acidic phosphoric acid esters are preferred, and 2-ethylhexyl acid phosphate is more preferred. The amount of the phosphorus compound used may be 10 to 2000 parts by mass based on 100 parts by mass of the catalyst.

[0174] The urethanization reaction can be carried out in the presence of a solvent. Examples of the solvent include esters such as ethyl acetate, butyl acetate, propyl acetate, γ-butyrolactone, δ-valerolactone, and ε-caprolactone; amides such as dimethylformamide, diethylformamide, and dimethylacetamide; sulfoxides such as dimethylsulfoxide; ethers such as tetrahydrofuran, dioxane, and 2-ethoxyethanol; ketones such as methyl ethyl ketone, methyl isobutyl ketone, and cyclohexanone; and aromatic hydrocarbons such as benzene and toluene.

[0175] The urethane resin described above has good elongation and texture, excellent durability, and in some cases good tensile strength. Therefore, the urethane resin can be suitably used for synthetic leather, artificial leather, coating materials, etc.

[0176] <Coating agent> The coating agent of the present embodiment contains the above-mentioned urethane resin. Specific aspects of the urethane resin may be as described above.

[0177] One example of its use as a coating agent is the in-mold coating method that applies RIM (Reaction Injection Molding). Specifically, this method involves molding a plastic substrate inside an injection mold, and then forming a urethane coating on the surface of the molded product inside the mold. With this method, the internal volume of the mold is constant, and not only are the density, thickness, and hardness of the urethane coating stable, but it is also possible to faithfully reproduce the irregularities on the mold surface, resulting in a highly aesthetically pleasing appearance.

[0178] <Water-based urethane resin dispersion> The aqueous urethane resin dispersion contains an aqueous medium and a urethane resin or a neutralized product thereof dispersed in the aqueous medium. The urethane resin is one of the above-mentioned urethane resins having an acidic group (a polyol component containing a polyol having an acidic group).

[0179] As the aqueous medium, in addition to water, a solution containing an emulsifier, a dispersant, etc. can be used. The aqueous medium preferably contains water, and more preferably consists of only water.

[0180] When the aqueous urethane resin dispersion contains a neutralized product of the urethane resin, the acidic group of the urethane resin may be neutralized by a neutralizing agent. Examples of the neutralizing agent include organic amines such as ammonia, ethylamine, trimethylamine, triethylamine, triisopropylamine, tributylamine, triethanolamine, N-methyldiethanolamine, N-phenyldiethanolamine, monoethanolamine, dimethylethanolamine, diethylethanolamine, morpholine, N-methylmorpholine, 2-amino-2-ethyl-1-propanol, and higher alkyl-modified morpholine, alkali metals such as lithium, potassium, and sodium, and inorganic alkalis such as sodium hydroxide and potassium hydroxide. From the viewpoint of improving the durability and smoothness of the coating film, a highly volatile neutralizing agent that is easily dissociated by heating, such as ammonia, trimethylamine, and triethylamine, is preferably used. These neutralizing agents can be used alone or in combination of two or more.

[0181] In producing the aqueous urethane resin dispersion, an anionic polar group-containing compound can also be used. Examples of the anionic polar group-containing compound include those consisting of an organic acid having one or more active hydrogens and a neutralizing agent. Examples of the organic acid include carboxylates, sulfonates, phosphates, phosphonates, phosphinates, and thiosulfonates. These anionic polar groups contained in the organic acid may be introduced alone or may be associated with metal ions such as chelates.

[0182] In producing the aqueous urethane resin dispersion, a cationic polar group-containing compound can also be used. The cationic polar group-containing compound is, for example, a tertiary amine having one or more active hydrogens, and one selected from the group consisting of a neutralizer for inorganic acid, a neutralizer for organic acid, and a quaternizing agent. In addition, the cationic polar group-containing compound can also be a cationic compound such as a primary amine salt, a secondary amine salt, a tertiary amine salt, or a pyridinium salt.

[0183] Examples of tertiary amines having one or more active hydrogens include N,N-dimethylethanolamine, N,N-diethylethanolamine, N,N-dipropylethanolamine, N,N-diphenylethanolamine, N-methyl-N-ethylethanolamine, N-methyl-N-phenylethanolamine, N,N-dimethylpropanolamine, N-methyl-N-ethylpropanolamine, N-methyldiethanolamine, N-ethyldiethanolamine, N-methyldipropanolamine, N-phenyldiethanolamine, N-phenyldipropanolamine, N-hydroxyethyl-N-hydroxypropyl-methylamine, N,N'-dihydroxyethylpiperazine, triethanolamine, trisisopropanolamine, N-methyl-bis-(3-aminopropyl)-amine, N-methyl-bis-(2-aminopropyl)-amine, etc. Also usable are primary amines such as ammonia and methylamine, or secondary amines such as dimethylamine to which alkylene oxide is added.

[0184] Inorganic and organic acids include, for example, hydrochloric acid, acetic acid, lactic acid, cyanoacetic acid, phosphoric acid, and sulfuric acid.

[0185] Examples of the quaternizing agent include dimethyl sulfate, benzyl chloride, bromoacetamide, chloroacetamide, etc. Also usable are alkyl halides such as ethyl bromide, propyl bromide, and butyl bromide.

[0186] The aqueous urethane resin dispersion can be produced, for example, by sequentially carrying out the steps of reacting a polyol component containing a polyol having an acidic group with a polyisocyanate component in the presence or absence of a solvent to form a urethane prepolymer, neutralizing the acidic groups in the prepolymer with a neutralizing agent, dispersing the neutralized prepolymer in an aqueous medium, and reacting the prepolymer dispersed in the aqueous medium with a chain extender. In each step, a catalyst can be used as necessary to promote the reaction and control the amount of by-products.

[0187] A film formed by the aqueous urethane resin dispersion described above (for example, a film formed by coating the aqueous urethane resin dispersion on a substrate) is excellent in adhesion, flexibility, touch, etc. Therefore, the aqueous urethane resin dispersion can be suitably used for artificial leather, synthetic leather, and coating materials.

[0188] <Two-liquid composition set> The polyol component and the polyisocyanate component for forming the urethane resin may be stored, transported, etc., in separate containers as a two-liquid composition set. The two-liquid composition set includes a first liquid containing at least the polyol component and a second liquid containing at least the polyisocyanate component. When a chain extender, a catalyst, a solvent, etc. are used, they may be contained in the first liquid and / or the second liquid, or may be mixed separately from the first liquid and the second liquid. The two-liquid composition set can be suitably used, for example, as a coating material, and can also be suitably used in the production of artificial leather, synthetic leather, etc. When the two-liquid composition set is used as a coating material, for example, after mixing the first liquid and the second liquid, the resulting mixed liquid is applied to a substrate, and optionally heated to form a coating film (for example, a cured film containing a urethane resin).

[0189] As an example of use as a coating agent for a two-liquid composition set, the resin composition can be suitably used in the production of artificial leather, synthetic leather, etc. as a resin composition that does not use organic solvents, and forms a polyurethane resin that has excellent adhesion, flexibility, touch, etc.

[0190] The polyurethane resin composition (one-liquid or two-liquid set) thus obtained is preferably used as an aqueous polyurethane resin emulsion or a polyurethane resin synthesized without a solvent. By curing this aqueous polyurethane resin emulsion or the polyurethane resin synthesized without a solvent, a molded product such as a coating film or film that is tough, has a reduced 100% modulus (good texture), and has a high softening temperature can be obtained, and can be suitably used for leather applications such as artificial leather and synthetic leather, or as a surface treatment agent for leather. The 100% modulus is one of the indicators that quantify the moist, elastic, and luxurious feeling when touching synthetic leather, and if the value is within a certain numerical range, the urethane resin has good properties.

[0191] <Application> The composition, urethane resin, aqueous urethane resin dispersion, and coating agent of the present embodiment described above can be used in a coating composition that is preferably used as a clear coating for automobile exteriors and a coating for automobile interiors. The composition, urethane resin, aqueous urethane resin dispersion, and coating agent of the present embodiment can also be preferably used in surface treatment of home appliances, OA (office automation) products, leather, and synthetic leather. EXAMPLES

[0192] Examples of the present invention will be described below, but the present invention is not limited to these examples.

[0193] Example 1 53.7g of trimethylolpropane, 146.3g of ε-caprolactone, and 0.22g of diphenyl phosphate were mixed in a 0.5L two-neck glass reactor (reactor A) equipped with a stirrer, a thermometer, a heater, and a cooler. The resulting mixture was heated and mixed at 70-80°C for 1 hour under argon, and then heated at 110-120°C for 4 hours. After the mixture was cooled to 80°C, 5g of ion exchange resin (Amberlyst A21) was added and stirred for 30 minutes, and the ion exchange resin was removed to obtain a composition (PEP-1) containing polyester polyol represented by the above formula (A-1) and / or the above formula (A-2).

[0194] Example 2 A composition (PEP-2) containing a polyester polyol represented by the above formula (A-1) and / or formula (A-2) was obtained in the same manner as in Example 1, except that a mixed liquid obtained by mixing 26.8 g of trimethylolpropane, 173.2 g of ε-caprolactone, and 0.22 g of diphenyl phosphoric acid was used in the reactor A.

[0195] Example 3 A composition (PEP-3) containing a polyester polyol represented by the above formula (A-1) and / or the above formula (A-2) was obtained in the same manner as in Example 1, except that a mixed liquid obtained by mixing 13.4 g of trimethylolpropane, 186.6 g of ε-caprolactone, and 0.22 g of diphenyl phosphoric acid was used in the reactor A.

[0196] Example 4 A composition (PEP-4) containing a polyester polyol represented by the above formula (A-1) and / or the above formula (A-2) was obtained in the same manner as in Example 1, except that a mixed liquid obtained by mixing 8.9 g of trimethylolpropane, 191.1 g of ε-caprolactone, and 0.22 g of diphenyl phosphoric acid was used in the reactor A.

[0197] Example 5 86 g of PCL-3 and 14 g of trimethylolpropane were mixed at 80° C. to obtain a composition (PEP-5) containing the polyester polyol represented by the above formula (A-1) and / or formula (A-2).

[0198] Example 6 73 g of PCL-3 and 27 g of trimethylolpropane were mixed at 80° C. to obtain a composition (PEP-6) containing the polyester polyol represented by the above formula (A-1) and / or formula (A-2).

[0199] Example 7 17.2 g of trimethylolpropane, 118.2 g of 1,6-hexanediol, 146.2 g of adipic acid, and 0.28 g of diphenyl phosphoric acid were mixed in a 1 L two-neck glass reactor equipped with a stirrer, a thermometer, a heating device, and a cooler. The resulting mixture was heated at 130 to 200°C (initial temperature 130°C, final temperature 200°C) under normal pressure, and reacted for 8 hours while removing water, a low boiling point component. The distillate temperature was 100°C or lower. Furthermore, the pressure in the flask was reduced to 0.5 kPa at a reaction temperature of 190°C, and the reaction was continued for another 8 hours, to obtain a composition (PEP-7) containing a polyester polyol represented by the above formula (A-1) and / or the above formula (A-2).

[0200] (Reference example 1) 60 g of PCL-3 and 40 g of trimethylolpropane were mixed at 80° C. to obtain a composition (PEP-7) containing the polyester polyol represented by the above formula (A-1) and / or formula (A-2).

[0201] Comparative Example 2 50 g of Plaxel 220 and 50 g of trimethylolpropane were mixed at 80° C. to obtain a composition containing polyester polyol (PED-2).

[0202] (Analysis and Evaluation) [Measurement of number average molecular weight] The composition obtained above was subjected to GPC analysis under the following conditions to measure the number average molecular weight of the composition. The results are shown in Tables 1 and 2. -conditions- (1) Measuring instrument: HLC-8420 (manufactured by Tosoh Corporation) (2) Column: TSKgel (Tosoh Corporation) G3000H-XL G3000H-XL G2000H-XL G2000H-XL (3) Mobile phase: THF (tetrahydrofuran) (4) Detector: RI (refractive index) detector (accessory for HLC-8420) (5) Temperature: 40℃ (6)Flow rate: 1.000ml / min (7) Calibration curve: A calibration curve was obtained using the following products (all bifunctional polyoxypropylene polyols manufactured by Sanyo Chemical Industries, Ltd.). "Sannix PP-200" (number average molecular weight = 200, average number of functional groups: 2) "Sannix PP-400" (number average molecular weight = 400, average number of functional groups: 2) "Sannix PP-1000" (number average molecular weight = 1000, average number of functional groups: 2) "Sannix PP-2000" (number average molecular weight = 2000, average number of functional groups: 2) "Sannix PP-3000" (number average molecular weight = 3200, average number of functional groups: 2) "Sannix PP-4000" (number average molecular weight = 4160, average number of functional groups: 2) (8) Approximation of calibration curve: Cubic equation (9) Sample solution concentration: 0.5% by mass in THF solution

[0203] [Hydroxyl value measurement] The hydroxyl value of the composition obtained above was measured by a method using an acetylating agent in accordance with JIS K1557-1. The results are shown in Tables 1 and 2.

[0204] [Characteristics evaluation] The composition obtained above was used as a sample, which was heated at 80°C for 1 hour and then left at 5°C and 25°C for 3 days. The state of the sample after leaving it was visually confirmed, and if it had even a slight fluidity at the above temperature, it was classified as liquid, and if it had no fluidity, it was classified as solid. The results are shown in Tables 1 and 2.

[0205] [Composition analysis] The composition was analyzed by the following procedure.

[0206] First, the composition (sample) obtained above was dissolved in deuterated chloroform (manufactured by Fujifilm Wako Pure Chemical Industries, Ltd.) to obtain a solution. Tetramethylsilane (TMS) was added to the solution as a chemical shift standard to obtain a test solution. The obtained test solution was analyzed using JNM-ECX400 (manufactured by JEOL Ltd.). 1 Measure H-NMR and set the TMS signal at 0 ppm. 1 For reference, the H-NMR spectrum of the composition obtained in Example 2 was 1 The H-NMR spectrum is shown in Figure 1. The measurement was carried out under the following conditions. -conditions- ·Resonance frequency: 400MHz Pulse width: 45degree Waiting time: 5 seconds Number of times: 64 Sample solution concentration (TMS-containing deuterated chloroform): 3% by mass

[0207] Next, 1 From the H-NMR spectrum, the integral value Δ of the methylene signal (S1) located next to the hydroxyl group of the group represented by the above formula (a-1) is S1 and the integral value Δ of the methylene signal (S2) located next to the hydroxyl group of the group represented by the above formula (a-2) S2 and the integral value Δ of the methylene signal (Sb) located next to the hydroxyl group of the polyhydric alcohol (B). Sb In addition, the R of the group represented by formula (I) was calculated. 1is a methyl group or an ethyl group, the integral values ​​of the terminal methyl signals are calculated and these are combined with the integral value Δ S3 Specifically, the signal from 3.55 ppm to 3.59 ppm was designated as signal (S1), the signal from 3.37 ppm to 3.47 ppm was designated as signal (S2), the signal from 3.70 ppm to 3.80 ppm was designated as signal (Sb), and the signal from 0.700 ppm to 1.130 ppm was designated as R 1 is a methyl group (when the polyhydric alcohol (B) is trimethylolethane), the signal (S3) is taken as the signal of R of the group represented by formula (I). 1 is an ethyl group (when the polyhydric alcohol (B) is trimethylolpropane). The baseline for the integral measurement was a horizontal line drawn by comparing the spectral intensities at both ends of the specified spectral range and using the lower spectral intensity as the standard.

[0208] From the integral obtained, the molar ratio (C A1 / C B ), molar ratio (C A2 / C B ), molar ratio (C A1 / C T ), molar ratio (C A2 / C T ) and molar ratio (C B / C T ) was calculated. The results are shown in Tables 1 and 2. In PEP-1 to 7, the presence of signal (S1) suggested the presence of compound (A-1), and the presence of signal (S2) suggested the presence of compound (A-2). On the other hand, in PED-8 to 9, signals (S1) and (S2) were not confirmed. In addition, the total number of moles of groups in which all three bonds in formula (I) are bonds to a carbonate group was calculated as C A3 Then, C T is C A1 , C A2 , C A3 and C BIn PCP-1A-6A and PCP-1-7, the integral values ​​of the above signals (S1)-(S3) and (Sb) indicate that T From C A1 , C A2 and C B It was confirmed that the value obtained by subtracting 1 from 1 was positive, suggesting the presence of compound (A-3).

[0209] [Table 1]

[0210] [Table 2]

[0211] In Tables 1 and 2, the "composition" (unit: g) of Examples 1 to 4 indicates the reaction raw materials, and the "composition" (unit: g) of Examples 5 to 6 and Comparative Examples 1 to 3 indicates the blended components.

[0212] (Physical property evaluation) A urethane cured film was prepared by the following method, and the physical properties (tensile properties, moist heat resistance properties, texture properties) of the obtained film were evaluated as a sample.

[0213] [Preparation of urethane hardened coating] First, the composition obtained above, a polyisocyanate component (C-2612), a urethane catalyst, a phosphorus compound (JP508), and a dilution solvent were mixed in a 200 mL glass bottle in the proportions (unit: g) shown in Tables 3 and 4. Immediately after mixing, the mixed liquid was poured onto a release paper and cast into a film having a thickness of 200 μm using a bar coater. The cast film was then cured by heating under the conditions of 25° C. for 30 minutes, 50° C. for 30 minutes, 80° C. for 30 minutes, 120° C. for 1 hour, and 50° C. for 48 hours to obtain a urethane cured coating (film).

[0214] [Evaluation of tensile properties and texture properties] The tensile properties and texture properties of the obtained film were measured under the following conditions in accordance with JIS K6251. The results are shown in Tables 3 and 4. -conditions- Test equipment: Tensilon UTA-500 (manufactured by A&D) Measurement conditions: 25℃×50%RH Head speed: 200mm / min Dumbbell No. 4

[0215] [Softening temperature] A test piece was obtained from the obtained film using a dumbbell, a 2 cm mark was drawn on the test piece, and the thickness at the center of the mark was measured. A weight of a specified weight was attached to one grip of the test piece, and the other grip was clamped with a double clip, and the test piece was hung in a dryer with the clip on the upper side. The temperature inside the dryer was then increased and the distance between the marks was observed. The temperature at which the distance between the marks reached 4 cm was read as the softening temperature. Processing equipment: constant temperature blower dryer DRK633DA (manufactured by Advantec) Weight: thickness of center of gauge line (μm) x 0.05g Dumbbell No. 2 (JIS K6251 compliant) Heating rate: 5℃ / min

[0216] [Glass transition temperature] A test piece (width 0.4 cm, length 2.5 cm) was obtained from the obtained film using a dumbbell, and the thickness (approximately 100 to 200 μm) at the center of the gauge line was measured. The glass transition temperature was determined as the peak top temperature of the obtained loss modulus (E") / storage modulus (E') = tan δ. -conditions- Processing equipment: RHEOVIBRON DDV-01GP Dynamic Viscoelastomeret (manufactured by Orientec) Range: -50~40℃ Heating rate: 3℃ / min Frequency: 35Hz ·Amplitude: 16μm ·Static tension: 5.00gf

[0217] [Hot water resistance evaluation] The obtained film was left in a water-immersed state in a thermostatic chamber at 70° C. for 28 days to prepare a test specimen. After that, the appearance of each test specimen was visually evaluated. The test equipment used was an ESPEC CORP (manufactured by ESPEC Corporation). The change in the film appearance after the test compared to the film appearance before the test was evaluated as A, B, or C (A: no change, B: white, C: dissolution). If the polyurethane film is good, the film shape will be maintained even after the water resistance test. The water resistance test simultaneously promotes reorientation and decomposition of polyurethane. If there is any deformation in the appearance of the film after the water resistance test, it suggests that reorientation of polyurethane is progressing, and if reorientation progresses significantly, the film will whiten. In some cases, the film will also dissolve due to the decomposition of the ester bonds in the polyurethane.

[0218] [Evaluation Criteria] Flexibility: 100% modulus was considered good if it was 5.0 MPa or less. Low-temperature properties: A glass transition temperature of 20°C or lower was considered good. Heat resistance: A softening temperature of 200°C or higher was considered good. In addition, if the breaking strength is 5 MPa or more, the breaking elongation is 200% or more, and the hot water resistance is A or B, there is no problem in practical use.

[0219] [Table 3]

[0220] [Table 4]

[0221] Details of the materials used in the examples are as follows: ε-caprolactone: manufactured by Tokyo Chemical Industry Co., Ltd. 1,6-Hexanediol: BASF JAPAN Trimethylolpropane: Sigma-Aldrich Adipic acid: Tokyo Chemical Industry Co., Ltd. - Ion exchange resin (Amberlyst A21): Sigma-Aldrich Plaxel 220: Polycaprolactone diol (number average molecular weight = 2000, hydroxyl value = 56.1, functionality = 2) manufactured by Daicel Corporation Diphenyl phosphate: Fujifilm Wako Pure Chemical Industries, Ltd. JP-508: Product name, 2-ethylhexyl acid phosphate, manufactured by Johoku Chemical Industry Co., Ltd. C-2612: Coronate 2612 (trade name), hexamethylene diisocyanate adduct modified polyisocyanate, isocyanate content = 17.2%, manufactured by Tosoh Corporation DOTDL: Dioctyltin dilaurate, manufactured by Kishida Chemical Industry Co., Ltd. Methyl ethyl ketone: Maruzen Petrochemical Co., Ltd. Toluene: Fujifilm Wako Pure Chemical Industries, Ltd.

Claims

1. A polyol compound (A-1) represented by the following formula (A-1): [Formula 1] [In formula (A-1), R 1 represents a hydrogen atom, an alkyl group, or a hydroxyalkyl group, R 2 is an alkanediyl group, or *1-R a -C(=O)-OR b - indicates *2, R a , and R b each independently represents an alkanediyl group, *1 indicates the bonding site with the carbonyl group, *2 indicates the bonding site with the oxygen atom, n 1 represents an integer of 1 or more. n 1 When R is 2 or more, there are multiple R 2 may be the same or different.

2. R 2 The polyol compound (A-1) according to claim 1, wherein all of the above are linear alkanediyl groups.

3. R 2 The polyol compound (A-1) according to claim 1, wherein all of the above are 1,5-pentanediyl groups.

4. or a reaction product of a polyhydric alcohol (B) and a cyclic ester (C); The polyol compound (A-1) according to claim 1, which is a reaction product of a polyhydric alcohol (B), a cyclic ester (C), and a diol (D). [Case 2] [In formula (B), R 1 has the same meaning as above.]

5. The polyol compound (A-1) according to any one of claims 1 to 4, A composition comprising a polyol compound (A-2) represented by the following formula (A-2): [C3] [In formula (A-2), R 1 represents a hydrogen atom, an alkyl group, or a hydroxyalkyl group, R 2 is an alkanediyl group, or *1-R a -C(=O)-OR b - indicates *2, *1 indicates the bonding site with the carbonyl group, *2 indicates the bonding site with the oxygen atom, n 2 and m 2 each independently represents an integer of 1 or more. Multiple R's 2 may be the same or different.

6. A composition comprising the composition according to claim 5 and a polyhydric alcohol represented by the following formula (B): [C4] [In formula (B), R 1 has the same meaning as above.]

7. The total number of moles of the group represented by the following formula (a-1) contained in the composition is C A1 The total number of moles of the polyhydric alcohol contained in the composition is C B Then, Molar ratio (C A1 / C B 7. The composition according to claim 6, wherein the saturation coefficient is 0.025 to 150. [C5] [In formula (a-1), R 1 is as defined above, and * indicates a bond to the alkanediyl group.

8. The total number of moles of the group represented by the following formula (a-2) contained in the composition is C A2 The total number of moles of the polyhydric alcohol contained in the composition is C B Then, Molar ratio (C A2 / C B 7. The composition according to claim 6, wherein the saturation coefficient is 0.020 to 150. [C6] [In formula (a-2), R 1 is as defined above, and * indicates a bond to the alkanediyl group.

9. The total number of moles of the group represented by the following formula (a-1) contained in the composition is C A1 The total number of moles of the group represented by the following formula (I) contained in the composition is C T Then, Molar ratio (C A1 / C T 7. The composition according to claim 6, wherein the β- [C7] [In formula (a-1), R 1 is as defined above, and * indicates a bond to the alkanediyl group. [C8] [In formula (I), R 1 has the same meaning as above, and * indicates a bond.

10. The total number of moles of the group represented by the following formula (a-2) contained in the composition is C A2 The total number of moles of the group represented by the following formula (I) contained in the composition is C T Then, Molar ratio (C A2 / C T 7. The composition of claim 6, wherein the β- [C9] [In formula (a-2), R 1 is as defined above, and * indicates a bond to the alkanediyl group. [C10] [In formula (I), R 1 has the same meaning as above, and * indicates a bond.

11. The total number of moles of the polyhydric alcohol contained in the composition is C B The total number of moles of the group represented by the following formula (I) contained in the composition is C T Then, Molar ratio (C B / C T 7. The composition according to claim 6, wherein the n-th order is 0.001 to 0.

950. [C11] [In formula (I), R 1 has the same meaning as above, and * indicates a bond.

12. The total number of moles of the polyhydric alcohol contained in the composition is C B The total number of moles of the group represented by the following formula (I) contained in the composition is C T Then, Molar ratio (C B / C T 7. The composition according to claim 6, wherein the n-th order is 0.001 to 0.

950. [C12] [In formula (I), R 1 has the same meaning as above, and * indicates a bond.

13. The composition according to claim 5, further comprising a polyester polyol represented by the following formula (A-3): [C13] [In formula (A-3), R 1 represents a hydrogen atom, an alkyl group, or a hydroxyalkyl group, R 2 is an alkanediyl group, or *1-R a -C(=O)-OR b - indicates *2, R a , and R b each independently represents an alkanediyl group, *1 indicates the bonding site with the carbonyl group, *2 indicates the bonding site with the oxygen atom, n 3 , m 3 and p 3 each independently represents an integer of 1 or more. Multiple R's 2 may be the same or different.

14. A polycondensate of a polyol component and a polyisocyanate component or a crosslinked product thereof, A urethane resin, wherein the polyol component comprises the composition of claim 5.

15. The urethane resin according to claim 14 , wherein the polyol component further contains a polyhydric alcohol represented by the following formula (B): [C14] [In formula (B), R 1 has the same meaning as above.]

16. The total number of moles of the group represented by the following formula (a-1) contained in the polyol component is C A1 The total number of moles of the polyhydric alcohol contained in the polyol component is C B Then, the molar ratio (C A1 / C B 16. The urethane resin according to claim 15, wherein the molecular weight is 0.025 to 150. [C15] [In formula (a-1), R 1 is as defined above, and * indicates a bond to the alkanediyl group.

17. The total number of moles of the group represented by the following formula (a-2) contained in the polyol component is C A2 The total number of moles of the polyhydric alcohol contained in the polyol component is C B Then, Molar ratio (C A2 / C B ) is 0.020 to 150. [C16] [In formula (a-2), R 1 is as defined above, and * indicates a bond to the alkanediyl group.

18. The total number of moles of the group represented by the following formula (a-1) contained in the polyol component is C A1 The total number of moles of the group represented by the following formula (I) contained in the polyol component is C T Then, the molar ratio (C A1 / C T ) is 0.025 to 0.

99. [C17] [In formula (a-1), R 1 is as defined above, and * indicates a bond to the alkanediyl group. [C18] [In formula (I), R 1 has the same meaning as above, and * indicates a bond.

19. The total number of moles of the group represented by the following formula (a-2) contained in the polyol component is C A2 The total number of moles of the group represented by the following formula (I) contained in the polyol component is C T Then, the molar ratio (C A2 / C T ) is 0.020 to 0.

99. [C19] [In formula (a-2), R 1 is as defined above, and * indicates a bond to the alkanediyl group. [C20] [In formula (I), R 1 has the same meaning as above, and * indicates a bond.

20. The total number of moles of the polyhydric alcohol contained in the polyol component is C B The total number of moles of the group represented by the following formula (I) contained in the polyol component is C T Then, the molar ratio (C B / C T ) is 0.001 to 0.

950. [C21] [In formula (I), R 1 has the same meaning as above, and * indicates a bond.

21. The urethane resin according to claim 14, wherein the polyol component further contains a polyester polyol represented by the following formula (A-3): [C22] [In formula (A-3), R 1 represents a hydrogen atom, an alkyl group, or a hydroxyalkyl group, R 2 is an alkanediyl group, or *1-R a -C(=O)-OR b - indicates *2, R a , and R b each independently represents an alkanediyl group, *1 indicates the bonding site with the carbonyl group, *2 indicates the bonding site with the oxygen atom, n 3 , m 3 and p 3 Each represents an integer of 1 or more. Multiple R's 2 may be the same or different.

22. The urethane resin according to claim 14, wherein the polyol component further comprises a polyol having an acidic group.

23. An aqueous urethane resin dispersion comprising an aqueous medium and the urethane resin or neutralized product thereof according to claim 22 dispersed in the aqueous medium.

Citation Information

Patent Citations

  • Method for refining amorphous iron alloy

    JP1984009118A

  • Lactone polyester polyols and process for production thereof

    WO2004087783A1