Method for depositing atomic layer for metal thin film

The use of a hydrogen-containing gas with a specific partial pressure and a metal complex with aromatic or alkyl ligands in thermal ALD enables metal thin film deposition at lower temperatures, addressing the challenges of plasma and oxidizing agent reliance in existing methods, ensuring contamination-free and controlled film formation.

JP2024148230APending Publication Date: 2024-10-18KOJUNDO CHEM LAB CO LTD

Patent Information

Application Number
JP2023061178
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-05
Publication Date
2024-10-18

AI Technical Summary

Technical Problem

Existing thermal ALD methods face challenges in depositing metal thin films without plasma or oxidizing agents, leading to potential deactivation of metal complexes and oxygen contamination, especially when using aromatic anionic ligands.

Method used

The method employs a hydrogen-containing gas with a specific partial pressure to deposit metal thin films using a metal complex with aromatic anionic or alkyl ligands, avoiding plasma and oxidizing agents by maintaining a substrate temperature lower than the metal complex's decomposition temperature.

Benefits of technology

This approach allows for the deposition of metal thin films at lower temperatures without plasma or oxidizing agents, reducing the risk of contamination and simplifying the process while maintaining excellent step coverage and film thickness control.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

To provide a method for depositing a metal thin film with a thermal atomic layer deposition (thermal ALD) method using a metal complex as a precursor raw material and a method that does not use a plasma that has concerns about deactivation or an oxygen-containing oxidizing agent such as ozone that has concerns about oxygen contamination.SOLUTION: A method for manufacturing a metal thin film using a thermal ALD method includes: a step 1 of supplying a metal complex including an aromatic anion ligand into a reaction chamber in which a substrate temperature is controlled to a temperature lower than the decomposition temperature of the metal complex by 3°C or more; and a step 2 of supplying a hydrogen-containing gas having hydrogen partial pressure of 100-50,000 Pa into the reaction chamber.SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for forming thin metal films by thermal atomic layer deposition (thermal ALD). [Background technology]

[0002] Atomic layer deposition (ALD) is known as a technique that is superior in step coverage and film thickness controllability compared to general chemical vapor deposition (CVD). ALD is a technique for forming thin films in atomic layers, and usually, the film is formed by repeating two steps: (1) reacting or adsorbing only one layer of gasified raw material with the substrate surface and purging the excess raw material, and (2) supplying reactive gas such as an oxidizing agent or reducing agent to react the raw material on the substrate to form the desired deposit. In this way, the raw material is deposited layer by layer, not continuously, so the ALD method has the characteristics of excellent step coverage and film thickness controllability. In addition, since the raw material is not thermally decomposed in the ALD method, an insulating film can be formed at a relatively low temperature. For this reason, it is expected to be applied to, for example, the formation of a gate insulating film of a thin film transistor in a display device using a glass substrate such as a liquid crystal display, and the like in a capacitor of a memory element.

[0003] The ALD method includes thermal ALD (TALD), which uses heat to promote the reaction, and plasma-assisted ALD (PEALD), which uses plasma to promote the reaction. Of these, PEALD can be applied to temperature-sensitive materials because it can form a film at a lower temperature. For example, Patent Document 1 describes a method of forming a ruthenium thin film by plasma-assisted ALD (PEALD) at a temperature of 400°C or less using a ruthenium precursor such as bis(cyclopentadienyl)ruthenium (Ru(Cp)2) or bis(ethylcyclopentadienyl)ruthenium(II) (Ru(EtCp)2), and using ammonia (NH3) gas or a mixed gas of nitrogen (N2) and hydrogen (H2) as a reaction gas and a purge gas.

[0004] In the method for forming a ruthenium thin film, plasma and ammonia gas or a nitrogen / hydrogen mixed gas are used under heating at 400° C. or less. As described in Patent Document 1, neither ammonia (NH3) gas nor nitrogen / hydrogen mixed gas reacts with a ruthenium precursor without plasma assistance, and therefore, in the film formation method of Patent Document 1, it is difficult to deposit a ruthenium thin film by proceeding with the reaction only by heat without plasma assistance.

[0005] By promoting the reaction using plasma, it becomes possible to form a film at a low temperature, making it possible to apply it to temperature-sensitive materials. However, when using ammonia, hydrogen, etc., radical species are generated by the plasma, and these may become inactivated during deposition, resulting in poor step coverage.

[0006] On the other hand, Patent Document 2 describes a method for forming a ruthenium thin film without using plasma by using an organometallic complex having an aromatic anion ligand such as bis(ethylcyclopentadienyl)ruthenium(II) (Ru(EtCp)2) as a precursor and a mixed gas of nucleophilic ammonia gas and electrophilic hydrogen gas as a reactive gas, and a method for forming a ruthenium thin film without using plasma by using an organometallic complex having an alkyl ligand such as trimethyltrimethylphosphinegold ((CH3)3AuP(CH3)3) as a precursor and a mixed gas of ammonia and hydrogen as a reactive gas. However, in the method of Patent Document 2, a nucleophilic gas and an electrophilic gas are mixed and used, so it is necessary to mix a plurality of raw materials and supply them to the reaction chamber, or to use special raw materials that have been mixed in advance, which is troublesome. For this reason, there is a demand for a method for forming a ruthenium thin film using a thermal ALD method without plasma support, without the need for complicated steps. [Prior art documents] [Patent documents]

[0007] [Patent Document 1] US Patent Application Publication No. 2006 / 0177601 [Patent Document 2] International Publication No. 2019 / 017285 Summary of the Invention [Problem to be solved by the invention]

[0008] The present invention aims to provide a method for depositing a metal thin film by thermal atomic layer deposition (thermal ALD) using a metal complex as a precursor raw material, which does not use plasma, which may cause deactivation, or an oxygen-containing oxidizing agent such as ozone, which may cause oxygen contamination. [Means for solving the problem]

[0009] The inventors have discovered that in a thermal atomic layer deposition (thermal ALD) method, by using a hydrogen-containing gas with a specific hydrogen partial pressure for a metal complex having an aromatic anion ligand or a metal complex having an alkyl ligand, a metal thin film can be deposited without using plasma or an oxidizing agent, and have completed the present invention. The present invention comprises the following items. The method for producing a metal thin film using a thermal ALD method of the present invention is characterized by including step 1 of supplying a metal complex having an aromatic anion ligand into a reaction chamber having a substrate temperature that is at least 3° C. lower than the decomposition temperature of the metal complex, and step 2 of supplying a hydrogen-containing gas having a hydrogen partial pressure of 100 to 50,000 Pa into the reaction chamber. The aromatic anion ligand is preferably a cyclopentadienyl ligand.

[0010] The method for producing a metal thin film using a thermal ALD method of the present invention is characterized by including step 1 of supplying a metal complex having an alkyl ligand into a reaction chamber having a substrate temperature that is at least 3°C ​​lower than the decomposition temperature of the metal complex, and step 2 of supplying a hydrogen-containing gas having a hydrogen partial pressure of 100 to 50,000 Pa into the reaction chamber.

[0011] The metal complex is preferably a complex of a metal having a standard oxidation-reduction potential between a hydrated ion and the elemental metal in an aqueous solution of greater than -1.1 V. The hydrogen-containing gas is preferably a gas that does not contain oxygen atoms. Effect of the Invention

[0012] According to the present invention, by using a hydrogen-containing gas having a specific hydrogen partial pressure for a metal complex having an aromatic anion ligand or a metal complex having an alkyl ligand, the aromatic anion ligand or the alkyl ligand can be eliminated even at low temperatures, and thermal ALD film formation can be performed at a temperature sufficiently lower than the thermal decomposition temperature of the metal complex. In other words, the thermal ALD method of the present invention makes it possible to deposit a metal thin film such as ruthenium using only a reducing agent without using plasma or an oxidizing agent. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0013] The thermal atomic layer deposition (thermal ALD) method for metal thin films of the present invention will be described in detail below. A thermal ALD method for metal thin films, which is one embodiment of the present invention, includes step 1 of supplying a metal complex having an aromatic anion ligand into a reaction chamber in which the substrate temperature is set to a temperature at least 3° C. lower than the decomposition temperature of the metal complex, and step 2 of supplying into the reaction chamber a hydrogen-containing gas having a hydrogen partial pressure of 100 to 50,000 Pa. Note that the hydrogen partial pressure in the present invention refers to the hydrogen partial pressure in the reaction chamber, and in the case where there is a pressure distribution in the reaction chamber, it refers to the hydrogen partial pressure on the substrate surface.

[0014] When depositing a metal thin film by thermal ALD, a first step is performed by supplying a raw material containing metal atoms such as a metal complex onto a substrate and adsorbing the raw material until it is saturated (including adsorption accompanied by reaction), and a second step is performed by supplying a hydrogen-containing gas having a specific partial pressure as a reactive gas and desorbing the parts of the adsorbed raw material other than the metal atoms. In the past, plasma or an oxidizing agent was used to sufficiently react the metal complex with the reactive gas. In the present invention, in such an ALD method, a metal complex having an aromatic anion ligand (hereinafter also referred to as "raw material") is supplied into a reaction chamber in which a substrate is placed, and then a hydrogen-containing gas having a specific hydrogen partial pressure is supplied into the reaction chamber, thereby making it possible to deposit a metal thin film at a temperature lower than the thermal decomposition temperature of the raw material without using plasma or an oxidizing agent.

[0015] The aromatic anion ligand includes, for example, aromatic ligands containing a five-membered ring, such as cyclopentadienyl ligand, substituted cyclopentadienyl ligand, indenyl ligand, substituted indenyl ligand, pentalenyl ligand, and substituted pentalenyl ligand. Among these, cyclopentadienyl ligand and substituted cyclopentadienyl ligand are preferred. Here, the substituted ligand refers to a ligand in which some or all of the hydrogen atoms constituting the five-membered ring are substituted with other groups. The other groups are preferably groups that do not contain elements other than carbon and hydrogen, and are preferably methyl, ethyl, n-propyl, isopropyl, or t-butyl groups from the viewpoint of ease of synthesis. In the substituted ligand, the other groups may be the same or different. Among these, the ethylcyclopentadienyl ligand, the pentamethylcyclopentadienyl ligand, and the n-propyltetramethylcyclopentadienyl ligand are particularly preferred, since the metal complexes tend to become liquid at room temperature.

[0016] In the present invention, there is no limit to the number of aromatic anion ligands coordinated to one metal atom. However, since aromatic anion ligands are bulky, the number is preferably 3 or less, and particularly preferably 2 or less, so as not to inhibit the interaction between the reactive gas and the metal atom.

[0017] The metal complex may have no ligand other than the aromatic anion ligand, i.e., may have a structure in which only the aromatic anion ligand is coordinated, but may have a ligand other than the aromatic anion to the extent that it does not adversely affect the effects of the present invention. As such a ligand other than the aromatic anion, an alkyl ligand such as a methyl ligand or hydrogen (hydride ligand) is preferable, and a methyl ligand is particularly preferable.

[0018] On the other hand, there is no particular limitation on the metal that forms the metal complex having an aromatic anion ligand, but in order to avoid contamination with the ligand component, one that is difficult to oxidize is preferably used. In other words, it is preferable that the metal is one that is likely to exist in a zero-valent metal state and can exist stably on the substrate. Specifically, it is preferable that the metal complex has a standard redox potential between the hydrated ion and the elemental metal in an aqueous solution of more than -1.1 V, such as ruthenium, cobalt, and tungsten, more preferably -0.3 V or more, and particularly preferably 0.2 V or more. In addition, when there are hydrated ions with multiple valences, the lowest value among them is adopted, and when the hydrated ion is unstable, the potential of the oxide is substituted, and when there are oxides with multiple valences, the lowest value among them is adopted.

[0019] Specific examples of metal complexes include bis(ethylcyclopentadienyl)ruthenium(II) (Ru(EtCp)2), (2,4-dimethylpentadienyl)(ethylcyclopentadienyl)ruthenium(II) (Ru(DMPD)(EtCp)), bis(ethylcyclopentadienyl)cobalt(II) (Co(EtCp)2) and bis(isopropylcyclopentadienyl)tungsten(IV)=dihydride ((iPrCp)2WH2). The combination of the metal atom and aromatic anion ligand in the metal complex is selected according to the stability and vapor pressure of the metal complex. In addition, the metal atom and aromatic anion ligand in the metal complex usually form a covalent bond. In addition, as long as the effect of the present invention is not hindered, the ligand may have ligands other than aromatic anion ligands, but it is preferable that the ligand does not have ligands other than aromatic anion ligands.

[0020] A thermal ALD method for metal thin films according to another embodiment of the present invention includes step 1 of supplying a metal complex having an alkyl ligand into a reaction chamber having a substrate temperature that is at least 3° C. lower than the decomposition temperature of the metal complex, and step 2 of supplying a hydrogen-containing gas having a hydrogen partial pressure of 100 to 50,000 Pa into the reaction chamber.

[0021] The alkyl ligand is an anionic ligand, such as methyl, ethyl, n-propyl, isopropyl, n-butyl, s-butyl, t-butyl, etc. These alkyl ligands can be selected depending on the stability and vapor pressure of the metal complex required for the ALD process.

[0022] The metal complex may have a ligand other than alkyl in order to stabilize the alkyl ligand. As such a ligand, a non-ionic ligand is preferable, and a phosphine ligand is more preferable. As the phosphine ligand, trimethylphosphine and triphenylphosphine are exemplified, and trimethylphosphine is particularly preferable.

[0023] As the metal complex having an alkyl ligand, a complex of a metal is usually used in which the standard redox potential between the hydrated ion and the elemental metal in an aqueous solution is -2 V or more, preferably a complex of a metal is used in which the standard redox potential is -1.1 V or more, more preferably 0.2 V or more, and particularly preferably 0.3 V or more. The metal is a noble metal, specifically, gold, silver, platinum, palladium, rhodium, iridium, ruthenium, osmium, etc. Among these noble metals, gold is particularly preferred.

[0024] In general, in the ALD method, the substrate temperature is usually the same in steps 1 and 2. In step 1, the substrate temperature must be lower than the temperature at which the raw material is thermally decomposed to allow the raw material to be saturated and adsorbed. The substrate temperature is the reaction temperature in the reaction chamber, i.e., the temperature at which the raw material is adsorbed onto the substrate, and the temperature of the substrate when the raw material is reacted with the reactive gas.

[0025] In the present invention, the raw material is reacted with the reaction gas at a temperature lower than the pyrolysis temperature, and the aromatic anion ligand is converted into a volatile compound and desorbed. In the present invention, the pyrolysis temperature refers to the temperature at which the raw material adsorbed on the substrate placed in the evacuated reaction chamber spontaneously decomposes even in the absence of the reaction gas, specifically, the temperature at which the raw material does not adsorb to the substrate to saturation and the decomposition product starts to accumulate. However, in reality, the temperature at which the raw material adsorbed on the substrate in the vacuum chamber spontaneously decomposes is almost the same as the pyrolysis temperature measured by ordinary thermogravimetric analysis (TG).

[0026] Considering the temperature uniformity of the substrate, the substrate temperature must be lower than the pyrolysis temperature by a certain degree or more, and is set to be 3° C. or more, preferably 5° C. or more, and more preferably 10° C. or more lower.

[0027] In order to form a metal film by removing the aromatic anion ligand from the metal complex, a reducing reactive gas has been used in the past. When hydrogen gas, carbonaceous gas, low molecular weight amines such as ammonia are used as the reactive gas, the activation energy required for the reaction with the aromatic anion ligand cannot be sufficiently reduced, and the reaction at a low temperature becomes difficult, so that it is necessary to reduce the activation energy by subjecting these gases to plasma treatment to generate radical species.

[0028] On the other hand, if a mixed gas of an electrophilic gas and a nucleophilic gas is used as a reducing reactive gas as in Patent Document 2, the nucleophilic gas interacts with the metal in the metal complex, weakening the bond energy between the metal and the aromatic anion ligand, and at the same time, the aromatic anion ligand reacts with the electrophilic gas to generate a very stable compound, which is then desorbed. However, the electrophilic gas used is a low molecular weight amine such as ammonia, and there is a risk of nitrogen contamination of the metal film.

[0029] In the present invention, by using a hydrogen-containing gas having a hydrogen partial pressure of 100 to 50,000 Pa as the reducing reactive gas, aromatic anion ligands that could not be desorbed at temperatures lower than the pyrolysis temperature in the past can be desorbed at a temperature 3° C. or more lower than the pyrolysis temperature, even without using a mixture of electrophilic gas and nucleophilic gas. Specifically, by using the thermal ALD of the present invention, aromatic anion ligands can be desorbed at a temperature 3° C. or more lower than the pyrolysis temperature, regardless of the catalytic effect of the nucleophilic gas. According to the present invention, aromatic anion ligands can be eliminated without relying on the catalytic effect of a nucleophilic gas, and therefore, no complicated steps are required. As a result, thermal ALD film formation with less risk of contamination is possible.

[0030] The hydrogen-containing gas is a gas obtained by mixing hydrogen gas with an inert gas such as argon gas, nitrogen gas, or carbon dioxide. The hydrogen-containing gas preferably does not contain any reducing gas or oxidizing gas other than hydrogen gas and an inert gas. However, since carbon dioxide may exhibit high reactivity under certain conditions, the hydrogen-containing gas is particularly preferably a mixed gas of hydrogen gas and an inert gas that does not contain oxygen atoms. The hydrogen partial pressure of the hydrogen-containing gas is preferably 100 to 50,000 Pa, more preferably 1,000 to 50,000 Pa, and particularly preferably 5,000 to 50,000 Pa. EXAMPLES

[0031] The present invention will now be described in more detail with reference to examples, but the present invention is not limited to the following examples.

[0032] [Common conditions] Ruthenium film formation by thermal ALD method A silicon wafer with a native oxide film was placed in the ALD apparatus, and ALD film formation was performed using bis(ethylcyclopentadienyl)ruthenium(II) (Ru(EtCp)2) as a precursor and hydrogen gas as a reactive gas. At this time, the temperature at which Ru(EtCp)2 was vaporized outside was 100°C, and the substrate temperature was 350°C. To obtain a Ru film, ALD film formation was performed by alternately supplying Ru(EtCp)2 and hydrogen gas. The amount of hydrogen gas supplied was controlled using a mass flow controller (FCS-T1000Z; Fujikin Co., Ltd.). The maximum pressure during hydrogen gas supply was measured using a diaphragm pressure gauge (TRD-10-P13NC; Daia Vacuum Co., Ltd.).

[0033] In the above-described method for forming a ruthenium film, hydrogen gas was supplied and a film was formed under the conditions shown in Examples 1 to 3 and Comparative Example 1, and the thickness of the ruthenium film was measured. [Example 1] The thickness of the Ru film formed by 50 cycles under conditions where the maximum pressure during hydrogen gas supply was 8300 Pa was measured using an ellipsometry spectrometer (FE-5000S; manufactured by Otsuka Electronics Co., Ltd.), and the average thickness of the Ru film was 13.6 nm. The change in the thickness of the Ru film was examined by changing the number of film formation cycles, and it was confirmed that there was no time (incubation time) during which the Ru film was not formed. Furthermore, elemental analysis of this Ru film using a glow discharge optical emission spectrometer (GD-Profiler2; manufactured by Horiba, Ltd.) revealed that Ru was significantly detected.

[0034] [Example 2] The thickness of the Ru film formed 50 cycles under conditions where the maximum pressure during hydrogen gas supply was 3600 Pa was measured using an ellipsometry spectrometer (FE-5000S; manufactured by Otsuka Electronics Co., Ltd.), and the average thickness of the Ru film was 11.6 nm. Furthermore, elemental analysis of this Ru film using a glow discharge optical emission spectrometer (GD-Profiler2; manufactured by Horiba, Ltd.) revealed that Ru was significantly detected.

[0035] [Example 3] The thickness of the Ru film formed 50 cycles under conditions where the maximum pressure during hydrogen gas supply was 110 Pa was measured using an ellipsometry spectrometer (FE-5000S; manufactured by Otsuka Electronics Co., Ltd.), and the average thickness of the Ru film was 9.2 nm. Furthermore, elemental analysis of this Ru film using a glow discharge optical emission spectrometer (GD-Profiler2; manufactured by Horiba, Ltd.) revealed that Ru was significantly detected.

[0036] [Comparative Example 1] The thickness of the Ru film formed by 50 cycles under conditions where the maximum pressure during hydrogen gas supply was 30 Pa was measured using an ellipsometry spectrometer (FE-5000S; manufactured by Otsuka Electronics Co., Ltd.), and the result was that the Ru film had an average thickness of 2.7 nm. In addition, elemental analysis of this Ru film using a glow discharge optical emission spectrometer (GD-Profiler2; manufactured by Horiba, Ltd.) showed that no significant amount of Ru was detected.

Claims

1. A step 1 of supplying a metal complex having an aromatic anion ligand into a reaction chamber in which the substrate temperature is set to a temperature 3° C. or more lower than the decomposition temperature of the metal complex; and step 2 of supplying a hydrogen-containing gas having a hydrogen partial pressure of 100 to 50,000 Pa into the reaction chamber.

2. The method for producing a metal thin film according to claim 1 , wherein the aromatic anion ligand is a cyclopentadienyl ligand.

3. A step 1 of supplying a metal complex having an alkyl ligand into a reaction chamber in which the substrate temperature is set to a temperature 3° C. or more lower than the decomposition temperature of the metal complex; and step 2 of supplying a hydrogen-containing gas having a hydrogen partial pressure of 100 to 50,000 Pa into the reaction chamber.

4. 4. The method for producing a metal thin film according to claim 1, wherein the metal complex is a complex of a metal having a standard oxidation-reduction potential between a hydrated ion and an elemental metal in an aqueous solution of greater than −1.1 V.

5. The method for producing a metal thin film according to any one of claims 1 to 3, wherein the hydrogen-containing gas is a mixed gas that does not contain oxygen atoms.

Citation Information

Patent Citations

  • Method of forming a ruthenium thin film using a plasma enhanced atomic layer deposition apparatus and the method thereof

    US20060177601A1

  • Atomic layer deposition method for metal thin film

    WO2019017285A1

Cited By

  • Method for manufacturing thin film

    JP2025031683A

  • Thin film manufacturing method

    JP7884742B2

  • Method for manufacturing thin film

    WO2025041857A1