Method for manufacturing heat exchanger

JP2024150019AActive Publication Date: 2024-10-23DAIKIN INDUSTRIES LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2023063225
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-10
Publication Date
2024-10-23
Estimated Expiration
2043-04-10

Smart Images

  • Figure 2024150019000001_ABST
    Figure 2024150019000001_ABST
Patent Text Reader

Abstract

To manufacture a heat exchanger including flat pipes and two fin groups.SOLUTION: In a method for manufacturing a heat exchanger (10), a first step, a second step, and a third step are performed. In the first step, a first fin group (41) and flat tubes (20) are assembled to form a first assembly (50). In the second step, a second fin group (42) and flat tubes (20) are assembled to form a second assembly (55). In the third step, the first assembly (50) and the second assembly (55) are assembled. As a result, the first fin group (41) and the second fin group (42) and the flat tubes (20) are assembled.SELECTED DRAWING: Figure 16
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a method for manufacturing a heat exchanger. [Background technology]

[0002] Patent Document 1 discloses a heat exchanger equipped with flat heat transfer tubes (flat tubes) and plate-like fins. In this heat exchanger, the windward portion of each of the heat transfer tubes arranged vertically is inserted into the flat grooves of the upstream plate fins, and the leeward portion is inserted into the flat grooves of the downstream plate fins. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Japanese Patent Application Publication No. 03-128167 Summary of the Invention [Problem to be solved by the invention]

[0004] As described above, Patent Document 1 discloses a heat exchanger having a structure in which fin groups are individually arranged on the upwind side and the downwind side of flat tubes. However, a specific method for manufacturing a heat exchanger having such a structure has not been fully considered.

[0005] The objective of the present disclosure is to manufacture a heat exchanger having flat tubes and two groups of fins. [Means for solving the problem]

[0006] A first aspect of the present disclosure is directed to a method for manufacturing a heat exchanger (10) comprising a plurality of flat tubes (20), and a first fin group (41) and a second fin group (42), each of which is composed of a plurality of plate-shaped fins (30), wherein each of the plurality of fins (30) has a plurality of slots (32) having an open end (33) formed on an outer edge of the fin (30), and each of the plurality of flat tubes (20) is inserted into the slots (32) of each of the fins (30) constituting the first fin group (41) and the slots (32) of each of the fins (30) constituting the second fin group (42).

[0007] The manufacturing method of the first aspect includes a first step of inserting the flat tubes (20) into some of the slots (32) of the fins (30) constituting the first fin group (41) to form a first assembly (50) consisting of the first fin group (41) and the flat tubes (20); and a second step of inserting the flat tubes (20) into some of the slots (32) of the fins (30) constituting the second fin group (42) that correspond to the slots (32) into which the flat tubes (20) of the first fin group (41) are not inserted to form a second assembly (55) consisting of the second fin group (42) and the flat tubes (20). and a third step of placing the first assembly (50) in a position where the flat tubes (20) of the first assembly (50) face the second assembly (55), placing the second assembly (55) in a position where the flat tubes (20) of the second assembly (55) face the first assembly (50), and pressing the first assembly (50) against the second assembly (55) to insert the flat tubes (20) of the first assembly (50) into the slots (32) of the fins (30) of the second assembly (55), and inserting the flat tubes (20) of the second assembly (55) into the slots (32) of the fins (30) of the first assembly (50).

[0008] In the manufacturing method of the first embodiment, a first step, a second step, and a third step are performed. In the first step, a first assembly (50) is formed by combining a first fin group (41) and a flat tube (20). In the second step, a second assembly (55) is formed by combining a second fin group (42) and a flat tube (20). In the third step, the flat tube (20) of the first assembly (50) is inserted into the slot (32) of the fin (30) of the second assembly (55), and the flat tube (20) of the second assembly (55) is inserted into the slot (32) of the fin (30) of the first assembly (50). As a result, the flat tube (20), the first fin group (41), and the second fin group (42) are combined.

[0009] A second aspect of the present disclosure is a method of the first aspect, in which, in the first step, the flat tube (20) is inserted into a predetermined slot (32) of the fin (30) constituting the first fin group (41) so that the slot (32) into which the flat tube (20) is inserted and the slot (32) into which the flat tube (20) is not inserted are arranged alternately, and, in the second step, the flat tube (20) is inserted into a predetermined slot (32) of the fin (30) constituting the second fin group (42) so that the slot (32) into which the flat tube (20) is inserted and the slot (32) into which the flat tube (20) is not inserted are arranged alternately.

[0010] In the second embodiment, in each of the first fin group (41) constituting the first assembly (50) and the second fin group (42) constituting the second assembly (55), the slots (32) into which the flat tubes (20) are inserted and the slots (32) into which the flat tubes (20) are not inserted are arranged alternately. In the third step, the flat tubes (20) of the second assembly (55) are inserted into the slots (32) of the first fin group (41) into which the flat tubes (20) were not inserted in the first step. Also, in the third step, the flat tubes (20) of the first assembly (50) are inserted into the slots (32) of the second fin group (42) into which the flat tubes (20) were not inserted in the second step.

[0011] A third aspect of the present disclosure is directed to the first or second aspect, in which in the third step, the first assembly (50) is positioned in a position in which the flat tubes (20) are located on the lower side, and the second assembly (55) is positioned in a position in which the flat tubes (20) are located on the upper side, and the first assembly (50) is pressed against the second assembly (55) by moving the first assembly (50) downward.

[0012] In the third step of the third embodiment, the first assembly (50) is moved downward to combine the first assembly (50) with the second assembly (55). During this process, the flat tubes (20) of the second assembly (55) are inserted from below into the slots (32) of the first fin group (41), and the flat tubes (20) of the first assembly (50) are inserted from above into the slots (32) of the second fin group (42).

[0013] A fourth aspect of the present disclosure is a third aspect, in which in the third step, a pressing member (65) having a flat pressing surface (66) on the lower surface is used, and the pressing surface (66) of the pressing member (65) is brought into contact with the upper outer edge of the fin (30) of the first assembly (50) arranged in an orientation in which the flat tube (20) is located on the lower side, and the first assembly (50) is pressed down by the pressing member (65), thereby pressing the first assembly (50) against the second assembly (55).

[0014] In the third step of the fourth embodiment, the first assembly (50) is pressed down by a pressing member (65) to combine the first assembly (50) with the second assembly (55).

[0015] A fifth aspect of the present disclosure is directed to the fourth aspect, in which the pressing member (65) used in the third step includes a plurality of pressing blocks (67), each of whose lower surface constitutes the pressing surface (66).

[0016] In the third step of the fifth embodiment, the first assembly (50) is pressed down by a pressing member (65) having a plurality of pressing blocks (67).

[0017] A sixth aspect of the present disclosure is that in the first or second aspect, the third step includes a straightening step of straightening the deflection of the first assembly (50) arranged in a position in which the flat tube (20) is located on the lower side, and in the third step, the first assembly (50) in a state in which the deflection has been straightened is pressed against the second assembly (55).

[0018] In the third step of the sixth embodiment, the first assembly (50) in a state where the deflection has been corrected is combined with the second assembly (55). Therefore, in the process of inserting the flat tubes (20) of the first assembly (50) into the slots (32) of the fins (30) constituting the second fin group (42) of the second assembly (55) and inserting the flat tubes (20) of the second assembly (55) into the slots (32) of the fins (30) constituting the first fin group (41) of the first assembly (50), it is possible to reduce the possibility that the fins (30) will be crushed by the flat tubes (20).

[0019] A seventh aspect of the present disclosure is the sixth aspect, wherein the straightening step includes a first straightening step of straightening horizontal deflection of the first assembly (50) by clamping the first assembly (50) from the horizontal direction.

[0020] In the first straightening step of the seventh embodiment, horizontal deflection of the first assembly (50) arranged in a position in which the flat tubes (20) are located on the lower side is straightened.

[0021] An eighth aspect of the present disclosure is the seventh aspect, wherein in the first straightening step of the straightening process, the first assembly (50) is clamped from both sides in the arrangement direction of the flat tubes (20) and also from both sides in the arrangement direction of the fins (30).

[0022] In the first straightening step of the eighth embodiment, the first assembly (50) is sandwiched from both sides in the arrangement direction of the flat tubes (20) and from both sides in the arrangement direction of the fins (30). As a result, horizontal deflection of the first assembly (50) arranged in an orientation in which the flat tubes (20) are located on the lower side is straightened.

[0023] A ninth aspect of the present disclosure is a third aspect in which, in any one of the sixth to eighth aspects, a pressing member (65) having a flat pressing surface (66) on the lower surface is used, and the pressing surface (66) of the pressing member (65) is brought into contact with the upper outer edge of the fins (30) of the first assembly (50) arranged in an attitude in which the flat tubes (20) are located on the lower side, and the first assembly (50) is pressed down by the pressing member (65) to press the first assembly (50) against the second assembly (55), and the straightening step includes a second straightening step of straightening the vertical deflection of the first assembly (50) by pressing the first assembly (50) against the pressing surface (66) of the pressing member (65).

[0024] In the third step of the ninth aspect, the first assembly (50) is pressed down by the pressing member (65) to combine the first assembly (50) and the second assembly (55). In the second straightening step, the first assembly (50) is pressed against the pressing surface (66) of the pressing member (65). As a result, the bending in the vertical direction of the first assembly (50) arranged with the flat tubes (20) located on the lower side is straightened.

[0025] A tenth aspect of the present disclosure is the ninth aspect, in which in the second straightening step of the straightening process, the first assembly (50) is pressed against the pressing surface (66) of the pressing member (65) by lifting both ends of the flat tube (20) in the first assembly (50).

[0026] In the second straightening step of the tenth embodiment, both ends of the flat tubes (20) of the first assembly (50) are lifted. As a result, the first assembly (50) is pressed against the pressing surface (66) of the pressing member (65), and the bending of the first assembly (50) in the up-down direction is straightened.

[0027] An eleventh aspect of the present disclosure is the ninth aspect, in which in the second straightening step of the straightening process, both ends of the flat tube (20) in the first assembly (50) and the middle portion in the extension direction of the flat tube (20) are lifted, thereby pressing the first assembly (50) against the pressing surface (66) of the pressing member (65).

[0028] In the second straightening step of the eleventh embodiment, the first assembly (50) is raised at both ends of the flat tubes (20) and at a middle portion in the extension direction of the flat tubes (20). As a result, the first assembly (50) is pressed against the pressing surface (66) of the pressing member (65), and the bending of the first assembly (50) in the up-down direction is straightened. [Brief description of the drawings]

[0029] [Figure 1] FIG. 1 is a front view of the heat exchanger. [Diagram 2] FIG. 2 is a cross-sectional view of the heat exchanger taken along line AA of FIG. [Diagram 3] FIG. 3 is a plan view of the fin. [Figure 4] FIG. 4 is a process diagram showing a method for manufacturing a heat exchanger. [Diagram 5] FIG. 5 is a schematic perspective view showing the first fin group in the first step and the second fin group in the second step. [Figure 6] FIG. 6 is a front view showing the first group of fins and the flattened tubes in the first step, and the second group of fins and the flattened tubes in the second step. [Figure 7] FIG. 7 is a schematic perspective view showing a first assembly formed in a first step and a second assembly formed in a second step. [Figure 8] FIG. 8 is a front view showing a first assembly formed in a first step and a second assembly formed in a second step. [Figure 9] FIG. 9 is a front view of the first assembly illustrating the inversion process in the inversion step. [Figure 10]FIG. 10 is a cross-sectional view showing the cross section taken along line CC in FIG. 14 in the third step. [Figure 11] FIG. 11 is a plan view of the first assembly and the pressing member in the third step. [Figure 12] FIG. 12 is a plan view of the first assembly and the clamping member in the third step. [Figure 13] FIG. 13 is a plan view of the first assembly and the clamping member in the first straightening step. [Figure 14] FIG. 14 is a cross-sectional view showing the cross section BB of FIG. 13 in the first straightening step. [Figure 15] FIG. 15 is a cross-sectional view showing the cross section BB of FIG. 13 in the second straightening step. [Figure 16] FIG. 16 is a cross-sectional view corresponding to FIG. 10, illustrating the process of moving the first assembly downward in the third step. [Figure 17] FIG. 17 is a cross-sectional view corresponding to FIG. 10, showing the first assembly and the second assembly during the third step. [Figure 18] FIG. 18 is a cross-sectional view corresponding to FIG. 10, showing a state in which the combination of the first assembly and the second assembly is completed in the third step. [Figure 19] FIG. 19 is a plan view of the first modified example of the embodiment, which corresponds to FIG. [Figure 20] FIG. 20 is a cross-sectional view of a second modified example of the embodiment, which corresponds to FIG. [Figure 21] FIG. 21 is a cross-sectional view of the third modified example of the embodiment, corresponding to FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0030] An embodiment will be described below. The embodiment is a method for manufacturing a heat exchanger (10).

[0031] -Heat exchanger- A heat exchanger (10) manufactured by the manufacturing method of the present embodiment will be described. The heat exchanger (10) is provided in a refrigerant circuit of an air conditioner that operates in a refrigeration cycle, and exchanges heat between the refrigerant flowing through the refrigerant circuit and air.

[0032] 1 and 2, the heat exchanger (10) includes a core (15) and two first header collecting pipes (16, 17). The core (15) includes a plurality of flat tubes (20) and a plurality of fins (30). The flat tubes (20), the fins (30), and the header collecting pipes (16, 17) are all made of aluminum or an aluminum alloy.

[0033] <Header collector pipe> Each of the two header collecting pipes (16, 17) is a long, thin cylindrical member. Note that the shape and structure of the header collecting pipes (16, 17) shown here are merely examples. In the heat exchanger (10) shown in Fig. 1, the first header collecting pipe (16) is disposed on the left side of the core (15), and the second header collecting pipe (17) is disposed on the right side of the core (15).

[0034] <Flat tube> 2, the flat tube 20 is a flat tube whose width is greater than its thickness. The cross section of the flat tube 20 perpendicular to its elongation direction is a rectangle with rounded corners or an oval shape with arcs at both ends.

[0035] 1, in the core 15, the flat tubes 20 are arranged such that their extension directions (axial directions) are substantially horizontal and their widthwise sides face each other. The flat tubes 20 are arranged vertically at regular intervals.

[0036] One end of each of the flat tubes (20) constituting the core (15) is inserted into the first header collector pipe (16), and the other end is inserted into the second header collector pipe (17). Each of the header collector pipes (16, 17) is joined to the flat tubes (20) by brazing.

[0037] As shown in Fig. 2, the flat tube (20) has a plurality of flow paths (21). Each flow path (21) is a straight flow path extending along the elongation direction of the flat tube (20). In the flat tube (20), the plurality of flow paths (21) are arranged side by side in the width direction of the flat tube (20). Each flow path (21) opens at both end faces of the flat tube (20). Each flow path (21) communicates with the internal space of the header collecting pipe (16, 17).

[0038] <fin> 3, the fin 30 is a long, thin plate-like member. One long side of the fin 30 is a linear continuous edge 31 that continues from one end of the fin to the other end in the longitudinal direction.

[0039] A plurality of slots 32 are formed in the fin 30. The slots 32 are elongated notches into which the flat tubes 20 are inserted. Each slot 32 extends in the direction of the short side of the fin 30 (in a direction perpendicular to the continuous edge portion 31). Each slot 32 opens to the outer edge of the fin 30. In other words, each slot 32 has an opening end 33 at the outer edge of the fin 30. Specifically, each slot 32 opens to the other long side of the fin 30 (in other words, the long side opposite to the continuous edge portion 31).

[0040] In the fin 30, a plurality of slots 32 are formed at regular intervals from one another in the long side direction (the direction parallel to the continuous edge portion 31) of the fin 30. The number of slots 32 formed in one fin 30 is the same as the number of flat tubes 20 constituting the core 15.

[0041] Each slot (32) is divided into a tube introduction portion (32a) and a tube holding portion (32b). The tube introduction portion (32a) is a portion that continues to the open end (33). The width (length in a direction parallel to the continuous edge portion (31)) of the tube introduction portion (32a) gradually increases toward the open end (33). The tube holding portion (32b) is a long and narrow portion that extends in the direction of the short side of the fin (30). The width (length in a direction parallel to the continuous edge portion (31)) of the tube holding portion (32b) is substantially constant. In addition, the width of the tube holding portion (32b) is slightly narrower than the thickness of the flat tube (20).

[0042] The fin (30) has raised portions (34) formed between adjacent slots (32) for promoting heat transfer.

[0043] The shape of the fins (30) constituting the first fin group (41) and the shape of the fins (30) constituting the second fin group (42) may be the same as or different from each other. For example, the shapes of the cut-and-raised portions (34) of the fins (30) constituting the first fin group (41) and the fins (30) constituting the second fin group (42) may be different from each other.

[0044] <core> As shown in FIGS. 1 and 2, the core (15) includes a flat tube (20), a first group of fins (41), and a second group of fins (42).

[0045] Each of the first fin group (41) and the second fin group (42) is composed of a plurality of fins (30). The number of fins (30) constituting each of the fin groups (41, 42) is preferably the same, but may be different. In each of the fin groups (41, 42), the plurality of fins (30) are arranged facing each other and spaced apart from each other at regular intervals. In each of the fin groups (41, 42), the corresponding slots (32) of each fin (30) are aligned in a row in the arrangement direction of the fins (30).

[0046] The first fin group (41) is disposed in front of the flat tube (20) in Fig. 2. Each fin (30) constituting the first fin group (41) is disposed in such a manner that its continuous edge portion (31) faces the front and the open end (33) of its slot (32) faces the rear. The front portion of the flat tube (20) fits into the slot (32) of the fin (30) constituting the first fin group (41). The fins (30) constituting the first fin group (41) are joined to the flat tube (20) by brazing.

[0047] The second fin group (42) is disposed on the rear side of the flat tube (20) in Fig. 2. Each fin (30) constituting the second fin group (42) is disposed in such a manner that the open end (33) of the slot (32) faces forward and the continuous edge portion (31) faces rearward. The rear portion of the flat tube (20) fits into the slot (32) of the fin (30) constituting the second fin group (42). The fins (30) constituting the second fin group (42) are joined to the flat tube (20) by brazing.

[0048] -Heat exchanger manufacturing method- A method for manufacturing the heat exchanger 10 having the above-described structure will be described below. In the method for manufacturing the heat exchanger 10 of this embodiment, a core assembly step, a header attachment step, and a joining step are carried out in this order.

[0049] The core assembling step is a step of combining the flat tubes 20, the first fin group 41, and the second fin group 42 to form the core 15. The core assembling step will be described in detail later.

[0050] The header attachment process is a process of attaching a first header collector pipe (16) and a second header collector pipe (17) to the core (15) formed in the core assembly process. In the header attachment process, one end of each of the flat tubes (20) constituting the core (15) is inserted into the first header collector pipe (16), and the other end of each of the flat tubes (20) constituting the core (15) is inserted into the second header collector pipe (17).

[0051] The joining process is a process of joining the fins (30) and the header collector pipes (16, 17) to the flat tubes (20) by brazing. In the joining process, the core (15) to which the header collector pipes (16, 17) are attached is placed in a heating furnace or the like and heated. As a result, the brazing material melts, and the fins (30) and the header collector pipes (16, 17) are joined to the flat tubes (20).

[0052] -Core assembly process- As shown in Fig. 4, the core assembly process includes a first step, an inversion step, a second step, and a third step. The third step is performed after the first step and the second step. The inversion step is performed between the first step and the third step. The third step includes a straightening step. The straightening step includes a first straightening step and a second straightening step.

[0053] <1st process> The first step is a step of combining a first fin group (41) and a flat tube (20) to form a first assembly (50).

[0054] As shown in Fig. 5, in the first step, all the fins (30) constituting the first fin group (41) are arranged facing each other at regular intervals. Note that in Fig. 5, the cut-and-raised portions (34) of the fins (30) are not shown. Each fin (30) is arranged with its continuous edge portion (31) facing downward and the open end (33) of the slot (32) facing upward. The multiple fins (30) are arranged such that their corresponding slots (32) are aligned in a row in the arrangement direction of the fins (30). The fins (30) constituting the first fin group (41) are surrounded by a frame-shaped or tray-shaped member to maintain the orientation shown in Fig. 5.

[0055] 5, the slots (32) of each fin (30) arranged in a row form a slot row (35). In this state, the first fin group (41) has the same number of slot rows (35) as the number of slots (32) formed in one fin (30).

[0056] In the first step, some of the flat tubes (20) constituting the heat exchanger (10) are combined with the first fin group (41). In the first step of the present embodiment, half of the flat tubes (20) constituting the heat exchanger (10) are combined with the first fin group (41).

[0057] As shown in Fig. 6, in the first step, the flat tubes (20) are inserted into every other slot row (35) aligned in the longitudinal direction of the fin (30) (in other words, the extension direction of the continuous edge portion (31)). In the first step, the flat tubes (20) are inserted into some of the slot rows (35) of the first fin group (41). Thus, in the first step, the flat tubes (20) are inserted into some of the slots (32) of each fin (30) constituting the first fin group (41).

[0058] The flat tubes (20) are inserted from top to bottom into the slots (32) that form the corresponding slot rows (35) with the width direction of the flat tubes (20) being roughly vertical and with the extension direction of the flat tubes (20) aligning with the arrangement direction of the fins (30).

[0059] As a result, a first assembly (50) is formed in which the first fin group (41) and the flat tubes (20) are combined, as shown in Figures 7 and 8. At the end of the first step, the first assembly (50) is in a position in which the continuous edge portion (31) of the fin (30) is located on the lower side and the flat tubes (20) are located on the upper side. Note that the cut-and-raised portions (34) of the fins (30) are not shown in Figure 7.

[0060] In the first assembly (50) formed in the first step, slot rows (35) into which the flat tubes (20) are inserted and slot rows (35) into which the flat tubes (20) are not inserted are arranged alternately one by one in the longitudinal direction of the fins (30) constituting the first fin group (41). Therefore, in each fin (30) constituting the first fin group (41), slots (32) into which the flat tubes (20) are inserted and slots (32) into which the flat tubes (20) are not inserted are arranged alternately one by one in the longitudinal direction of the fin (30).

[0061] <Inversion process> The inversion step is a step of inverting the position of the first assembly (50) formed in the first step.

[0062] As described above, at the end of the first step, the first assembly (50) is in a position in which the flat tubes (20) are located on the upper side. As shown in Fig. 9, in the inversion step, the first assembly (50) is inverted from a position in which the flat tubes (20) are located on the upper side to a position in which the flat tubes (20) are located on the lower side. In the inversion step, the first assembly (50) is held by an arm-shaped member (not shown), and the arm-shaped member is rotated 180° to invert the position of the first assembly (50).

[0063] <2nd process> The second step is a step of combining the second fin group (42) and the flat tubes (20) to form a second assembly (55).

[0064] As shown in Fig. 5, in the second step, all the fins (30) constituting the second fin group (42) are arranged facing each other at regular intervals. Note that the cut-ups (34) of the fins (30) are not shown in Fig. 5. Each fin (30) is arranged with its continuous edge (31) facing downward and the open ends (33) of the slots (32) facing upward. The multiple fins (30) are arranged such that their corresponding slots (32) are aligned in a row in the arrangement direction of the fins (30). The fins (30) constituting the second fin group (42) are surrounded by a frame- or tray-shaped member to maintain the orientation shown in Fig. 5.

[0065] 5, the slots 32 of each fin 30 arranged in a row form a slot row 35. In this state, the second fin group 42 has the same number of slot rows 35 as the number of slots 32 formed in one fin 30.

[0066] In the second step, some of the flat tubes (20) constituting the heat exchanger (10) are combined with the second fin group (42). In the second step of the present embodiment, the remaining half of the flat tubes (20) constituting the heat exchanger (10), which were not combined with the first fin group (41) in the first step, are combined with the second fin group (42). Therefore, the sum of the number of the flat tubes (20) combined with the first fin group (41) in the first step and the number of the flat tubes (20) combined with the second fin group (42) in the second step matches the number of the flat tubes (20) constituting the heat exchanger (10).

[0067] 6, in the second step, the flat tubes (20) are inserted into every other slot row (35) aligned in the longitudinal direction of the fins (30). In the second step, the flat tubes (20) are inserted into some of the slot rows (35) of the second fin group (42). Thus, in the second step, the flat tubes (20) are inserted into some of the slot rows (32) of each fin (30) constituting the second fin group (42).

[0068] The flat tubes (20) are inserted from top to bottom into the slots (32) that form the corresponding slot rows (35) with the width direction of the flat tubes (20) being roughly vertical and with the extension direction of the flat tubes (20) aligning with the arrangement direction of the fins (30).

[0069] As a result, as shown in Figures 7 and 8, a second assembly (55) is formed in which the second fin group (42) and the flat tubes (20) are combined. At the end of the second step, the second assembly (55) is in a position in which the continuous edge portion (31) of the fin (30) is located on the lower side and the flat tubes (20) are located on the upper side. Note that the cut-and-raised portion (34) of the fin (30) is not shown in Figure 7.

[0070] In the second assembly (55) formed in the second step, slot rows (35) into which the flat tubes (20) are inserted and slot rows (35) into which the flat tubes (20) are not inserted are arranged alternately one by one in the longitudinal direction of the fins (30) constituting the second fin group (42). Therefore, in each fin (30) constituting the second fin group (42), slots (32) into which the flat tubes (20) are inserted and slots (32) into which the flat tubes (20) are not inserted are arranged alternately one by one in the longitudinal direction of the fin (30).

[0071] In the second step, the flat tube (20) is inserted into a slot row (35) of the second fin group (42) that corresponds to the "slot row (35) into which the flat tube (20) is not inserted" of the first fin group (41). Therefore, in the second step, the flat tube (20) is inserted into a slot (32) of the fins (30) constituting the second fin group (42) that corresponds to the "slot (32) into which the flat tube (20) is not inserted" of the fins (30) constituting the first fin group (41).

[0072] The slot row 35 of the second fin group 42 into which the flat tube 20 is inserted in the second step is the slot row 35 located opposite the "slot row 35 into which the flat tube 20 is not inserted" of the first assembly 50 in a state in which the second fin group 42 is arranged to face the first assembly 50 (for example, the state shown in FIG. 10). Therefore, the "slot 32 of the fin 30 constituting the second fin group 42 into which the flat tube 20 is inserted" in the second step is the slot 32 located opposite the "slot 32 into which the flat tube 20 is not inserted" of the fin 30 constituting the first assembly 50 in a state in which the second fin group 42 is arranged to face the first assembly 50 (for example, the state shown in FIG. 10).

[0073] <3rd process> The third step is a step of combining the first assembly (50) and the second assembly (55) to form the core (15). In the third step, a straightening step is performed to straighten the deflection of the first assembly (50), and the first assembly (50) in a straightened state is combined with the second assembly (55).

[0074] [Layout of the second assembly] As shown in Fig. 10, in the third step, the second assembly (55) is placed on a flat base member (60) with the flat tubes (20) facing upward. The second fin group (42) constituting the second assembly (55) has the continuous edge portions (31) of the fins (30) in contact with the upper surface of the base member (60). The second assembly (55) is held in a predetermined position on the base member (60) by a member not shown.

[0075] [Layout of the first assembly] 10, in the third step, the first assembly (50) that has been subjected to the inversion step is disposed above the second assembly (55). The first assembly (50) is disposed above the second assembly (55) in an orientation in which the flat tubes (20) are located on the lower side.

[0076] In this state, each flat tube 20 of the first assembly 50 faces a corresponding slot row 35 of the second fin group 42 constituting the second assembly 55. Specifically, each flat tube 20 of the first assembly 50 is located opposite a "slot row 35 into which no flat tube 20 is inserted" of the second assembly 55.

[0077] Moreover, each flat tube 20 of the second assembly 55 faces a corresponding slot row 35 of the first fin group 41 constituting the first assembly 50. Specifically, each flat tube 20 of the second assembly 55 is located opposite a "slot row 35 into which no flat tube 20 is inserted" of the first assembly 50.

[0078] In this manner, in the third step, the first assembly (50) is positioned in a position in which the flat tubes (20) of the first assembly (50) face the second assembly (55), and the second assembly (55) is positioned in a position in which the flat tubes (20) of the second assembly (55) face the first assembly (50).

[0079] [Pressing member] In the third step, the first assembly (50) is disposed below the pressing member (65). As shown in Fig. 11, the pressing member (65) is a flat member that covers the entire first assembly (50) when viewed from above. The lower surface of the pressing member (65) is a flat pressing surface (66). The pressing surface (66) faces the continuous edge portions (31) of the fins (30) that constitute the first fin group (41) of the first assembly (50) (see Fig. 10).

[0080] [Holding member] 12, in the third step, the first assembly (50) is surrounded by four clamping members (71-74). In the first assembly (50), one end of each of the fins (30) constituting the first fin group (41) faces the first clamping member (71), and the other end of each of the fins (30) faces the second clamping member (72). In the first assembly (50), one end face of each of the flat tubes (20) faces the third clamping member (73), and the other end face of each of the flat tubes (20) faces the fourth clamping member (74).

[0081] Each of the first clamping member (71) and the second clamping member (72) is an elongated member extending horizontally. The surface of each of the first clamping member (71) and the second clamping member (72) facing the first assembly (50) is a substantially vertical surface.

[0082] 10 and 12, the first clamping member (71) is disposed on the left side of the first assembly (50) and faces the left end of the fin (30) that constitutes the first fin group (41). In addition, in Fig. 10 and 12, the second clamping member (72) is disposed on the right side of the first assembly (50) and faces the right end of the fin (30) that constitutes the first fin group (41).

[0083] Each of the third clamping member (73) and the fourth clamping member (74) is an elongated member extending in the horizontal direction. As shown in Fig. 14, each of the third clamping member (73) and the fourth clamping member (74) includes a clamping portion (73a, 74a) and a support portion (73b, 74b). The surface of the clamping portion (73a, 74a) facing the first assembly (50) is a substantially vertical surface. The support portion (73b, 74b) is a portion that protrudes from the clamping portion (73a, 74a) toward the first assembly (50). The upper surface of the support portion (73b, 74b) is a substantially horizontal surface.

[0084] In Fig. 12, the third clamping member (73) is disposed on the front side of the first assembly (50). The third clamping member (73) has a clamping portion (73a) facing the end face of the flat tube (20) and a support portion (73b) located below the end of the flat tube (20) (see Fig. 14). Also, in Fig. 12, the fourth clamping member (74) is disposed on the rear side of the first assembly (50). The fourth clamping member (74) has a clamping portion (74a) facing the end face of the flat tube (20) and a support portion (74b) located below the end of the flat tube (20) (see Fig. 14).

[0085] [First straightening process] The first straightening step is a step of straightening the horizontal deflection of the first assembly (50) arranged in a position in which the flat tubes (20) are located on the lower side.

[0086] Here, in the first assembly (50), the flat tubes (20) inserted into the slot rows (35) of the first fin group (41) are held by the first fin group (41) by frictional force. Therefore, the first assembly (50) may bend in the horizontal direction due to relative displacement between the first fin group (41) and the flat tubes (20). Therefore, in the first straightening process, the horizontal bending of the first assembly (50) is straightened.

[0087] As shown in Fig. 12, in the first straightening step, the second clamping member (72) is pressed against the first assembly (50). As a result, as shown in Fig. 13, the first assembly (50) is sandwiched from both the left and right sides in Fig. 13 by the first clamping member (71) and the second clamping member (72). In this manner, the first assembly (50) is sandwiched from both sides in the arrangement direction of the flat tubes (20) (in other words, the longitudinal direction of the fins (30)) by the first clamping member (71) and the second clamping member (72). Note that the pressing member (65) is not shown in Figs. 12 and 13.

[0088] Furthermore, as shown in Fig. 12, in the first straightening step, the third clamping member (73) and the fourth clamping member (74) are each pressed against the first assembly body (50). As a result, as shown in Fig. 13, the first assembly body (50) is sandwiched from both the front and rear sides in Fig. 13 by the third clamping member (73) and the fourth clamping member (74). In this manner, the first assembly body (50) is sandwiched from both sides in the arrangement direction of the fins (30) (in other words, the extension direction of the flat tubes (20)) by the third clamping member (73) and the fourth clamping member (74).

[0089] In the first straightening step, the first assembly (50) in an orientation in which the flat tubes (20) are located on the lower side is clamped from both sides in the arrangement direction of the flat tubes (20) by the first clamping member (71) and the second clamping member (72), and is also clamped from both sides in the arrangement direction of the fins (30) by the third clamping member (73) and the fourth clamping member (74). As a result, the horizontal deflection of the first assembly (50) arranged in an orientation in which the flat tubes (20) are located on the lower side is straightened.

[0090] [Second straightening process] The second straightening step is a step of straightening out any bending in the vertical direction of the first assembly (50) that is arranged in a position in which the flat tubes (20) are located on the lower side.

[0091] Here, the first assembly (50) arranged with the flat tubes (20) located on the lower side may be curved downward near the center in the arrangement direction of the flat tubes (20) (left-right direction in FIG. 10) due to elastic deformation of the fins (30). Also, the first assembly (50) arranged with the flat tubes (20) located on the lower side may be curved upward.

[0092] When the first assembly (50) is curved, the width direction of each flat tube (20) is inclined with respect to the vertical direction. Therefore, the flat tube (20) of the first assembly (50) cannot be inserted straight from above into the slot row (35) of the second fin group (42), and as a result, the fins (30) of the second fin group (42) may be crushed. Furthermore, when the first assembly (50) is curved, the extension direction of the slots (32) of each fin (30) constituting the first fin group (41) is inclined with respect to the vertical direction. Therefore, the flat tube (20) of the second assembly (55) cannot be inserted straight from below into the slot row (35) of the first fin group (41), and as a result, the fins (30) of the first fin group (41) may be crushed. Therefore, in the second straightening process, the bending of the first assembly (50) in the vertical direction is straightened.

[0093] As shown in FIG. 14, in the second straightening step, the third clamping member (73) and the fourth clamping member (74) move upward, and the upper surfaces of the support portions (73b, 74b) come into contact with the ends of the flat tubes (20). As shown in FIG. 15, the first assembly (50) that is horizontally sandwiched by the four clamping members (71-74) is lifted by the third clamping member (73) and the fourth clamping member (74) and pressed against the pressing surface (66) of the pressing member (65). The pressing surface (66) of the pressing member (65) is a flat horizontal surface. Therefore, when the first assembly (50) is pressed against the pressing member (65), the continuous edge portion (31) of the fin (30) that constitutes the first fin group (41) becomes straight along the pressing surface (66), and the bending of the first assembly (50) in the vertical direction is straightened.

[0094] [Combination of the first and second assemblies] The first assembly (50) is combined with the second assembly (55) in a state in which the deflections in the horizontal and vertical directions are corrected.

[0095] As shown in FIG. 16, the first assembly (50) is sandwiched horizontally by the four clamping members (71-74) and moves downward while being pressed against the pressing surface (66) of the pressing member (65).

[0096] 17, when the first assembly (50) moves downward, the lower portion of each flat tube (20) of the first assembly (50) enters into the corresponding slot row (35) of the second fin group (42) constituting the second assembly (55). Also, the upper portion of each flat tube (20) of the second assembly (55) enters into the corresponding slot row (35) of the first fin group (41) constituting the first assembly (50).

[0097] Thereafter, the first assembly (50) is further pressed downward by the pressing member (65). As a result, as shown in Fig. 18, each flat tube (20) of the first assembly (50) enters into the corresponding slot row (35) of the second fin group (42) constituting the second assembly (55), and each flat tube (20) of the second assembly (55) enters into the corresponding slot row (35) of the first fin group (41) constituting the first assembly (50). In this manner, the first assembly (50) is combined with the second fin group (42), and a core (15) composed of the flat tube (20), the first fin group (41), and the second fin group is formed.

[0098] -Features of the embodiment (1)- The method for manufacturing the heat exchanger (10) of the present embodiment includes a first step, a second step, and a third step.

[0099] In a first step, a first assembly (50) is formed by combining a first fin group (41) and a flat tube (20). In a second step, a second assembly (55) is formed by combining a second fin group (42) and a flat tube (20).

[0100] In the third step, the first assembly (50) and the second assembly (55) are brought closer together, so that the flat tubes (20) of the first assembly (50) are inserted into the corresponding slot rows (35) of the second fin group (42), and the flat tubes (20) of the second assembly (55) are inserted into the corresponding slot rows (35) of the first fin group (41). As a result, the flat tubes (20), the first fin group (41), and the second fin group (42) are combined.

[0101] In the first assembly (50) formed in the first step, the relative positions of the fins (30) constituting the first fin group (41) are maintained by the flat tubes (20) inserted into the slot rows (35) of the first fin group (41). In the second assembly (55) formed in the second step, the relative positions of the fins (30) constituting the second fin group (42) are maintained by the flat tubes (20) inserted into the slot rows (35) of the second fin group (42).

[0102] Therefore, in the manufacturing method of this embodiment, handling such as transporting the first fin group (41) and the second fin group (42), and the work of combining the first assembly (50) and the second assembly (55) in the third step can be easily performed while maintaining the relative positions of the multiple fins (30) that constitute each of the first fin group (41) and the second fin group (42).

[0103] -Features of the embodiment (2)- In the third step of the manufacturing method of this embodiment, the second assembly (55) is placed on the base member (60), and the first assembly (50) placed above the second assembly (55) is pressed down by the pressing member (65), thereby combining the first assembly (50) and the second assembly (55). In the third step, the continuous edge portion (31) of each fin (30) constituting the second fin group (42) of the second assembly (55) comes into contact with the flat upper surface of the base member (60). Therefore, the second assembly (55) placed on the base member (60) does not bend in the vertical direction.

[0104] As described above, in the third step of the manufacturing method of this embodiment, the second assembly (55) is placed without being bent in the vertical direction, and the first assembly (50) is brought close to the second assembly (55), thereby combining the first assembly (50) and the second assembly (55). Therefore, according to this embodiment, the step of combining the first assembly (50) and the second assembly (55) can be performed reliably, and the possibility of problems such as damage to the fins (30) occurring during the manufacturing process of the heat exchanger (10) can be reduced.

[0105] -Features of the embodiment (3)- In a third step of the manufacturing method of this embodiment, a straightening step is performed to straighten the warp of the first assembly (50), and the first assembly (50) in a straightened state is combined with the second assembly (55).

[0106] Here, when the first assembly (50) is bent, the relative positions of the flat tubes (20) constituting the first assembly (50) change from the correct positions when the first assembly (50) is not bent. Therefore, when the first assembly (50) is bent, the flat tubes (20) of the first assembly (50) cannot be accurately positioned above the corresponding slot rows (35) of the second fin group (42) constituting the second assembly (55).

[0107] Furthermore, when the first assembly (50) is bent, the relative position of the "slot row (35) into which the flat tube (20) is not inserted" of the first fin group (41) constituting the first assembly (50) changes from the correct position when the first assembly (50) is not bent. Therefore, when the first assembly (50) is bent, the "slot row (35) into which the flat tube (20) is not inserted" of the first fin group (41) constituting the first assembly (50) cannot be accurately positioned above the corresponding flat tube (20) of the second assembly (55).

[0108] Therefore, when the first assembly (50) in a bent state is combined with the second assembly (55), the flat tubes (20) of the first assembly (50) are not inserted straight from above into the corresponding slot rows (35) of the second fin group (42), and the fins (30) of the second fin group (42) may be crushed by the flat tubes (20) of the first assembly (50). Furthermore, when the first assembly (50) in a bent state is combined with the second assembly (55), the flat tubes (20) of the second assembly (55) are not inserted straight from below into the corresponding slot rows (35) of the first fin group (41), and the fins (30) of the first fin group (41) may be crushed by the flat tubes (20) of the second assembly (55).

[0109] In contrast, in the third step of the manufacturing method of this embodiment, the first assembly (50) in a state where the warp has been straightened is combined with the second assembly (55). Therefore, the flat tubes (20) of the first assembly (50) can be inserted straight from above into the slot rows (35) of the corresponding second fin group (42). Also, the flat tubes (20) of the second assembly (55) can be inserted straight from below into the slot rows (35) of the corresponding first fin group (41).

[0110] Therefore, according to the manufacturing method of this embodiment, when combining the first assembly (50) with the second assembly (55), it is possible to reduce the possibility that the fins (30) of the first fin group (41) will be crushed by the flat tubes (20) of the second assembly (55) and the possibility that the fins (30) of the second fin group (42) will be crushed by the flat tubes (20) of the first assembly (50).

[0111] In particular, in the straightening step of the manufacturing method of this embodiment, the horizontal deflection of the first assembly (50) in the position where the flat tubes (20) are located on the lower side is straightened in the first straightening step, and the vertical deflection of the first assembly (50) in the position where the flat tubes (20) are located on the lower side is straightened in the second straightening step. Therefore, in the third step of the manufacturing method of this embodiment, the first assembly (50) in which both the horizontal deflection and the vertical deflection have been corrected can be combined with the second assembly (55).

[0112] Therefore, according to this embodiment, when combining the first assembly (50) with the second assembly (55), it is possible to reliably reduce the possibility that the fins (30) of the first fin group (41) will be crushed by the flat tubes (20) of the second assembly (55) and the possibility that the fins (30) of the second fin group (42) will be crushed by the flat tubes (20) of the first assembly (50).

[0113] -Modifications of the embodiment- The manufacturing method of the heat exchanger (10) of this embodiment can be modified as follows.

[0114] First Modified Example As shown in Fig. 19, the pressing member (65) used in the third step may include a plurality of pressing blocks (67). The pressing member (65) shown in Fig. 19 includes two pressing blocks (67). The lower surface of each of the two pressing blocks (67) forms a flat pressing surface (66). The two pressing blocks (67) are arranged side by side in the arrangement direction of the flat tubes (20) in the first assembly (50) (the left-right direction in Fig. 19).

[0115] The pressing surface (66) of the pressing member (65) is larger than the heat exchanger (10) to be manufactured. Therefore, when a pressing member (65) made of a single member is used to manufacture a large heat exchanger (10), the rigidity of the large pressing member (65) needs to be ensured, which may increase the weight of the pressing member (65). Therefore, by forming the pressing member (65) from a plurality of pressing blocks (67) as in this modified example, the rigidity of each pressing block (67) can be ensured while the weight of each pressing block (67) can be reduced, thereby reducing the weight of the entire pressing member (65).

[0116] <Second Modification> As shown in Fig. 20, in the second straightening step, the first assembly (50) may be pressed against the pressing member (65) by the third clamping member (73), the fourth clamping member (74), and the intermediate support member (75). The intermediate support member (75) is a member extending in a direction perpendicular to the extension direction (front-rear direction in Fig. 20) of the flat tubes (20) constituting the first assembly (50). The intermediate support member (75) abuts against the center of the extension direction of the flat tubes (20) constituting the first assembly (50). The intermediate support member (75) moves upward in conjunction with the third clamping member (73) and the fourth clamping member (74), and lifts up the first assembly (50) together with the third clamping member (73) and the fourth clamping member (74).

[0117] When the flat tubes (20) are long, there is a risk that the flat tubes (20) will bend to a non-negligible extent when the first assembly (50) is arranged with the flat tubes (20) positioned on the lower side. In this case, if the ends of the flat tubes (20) are supported by the third clamping member (73) and the fourth clamping member (74) and the central portion of the flat tubes (20) in the extension direction is supported by the intermediate support member (75), the flat tubes (20) can be straightened in the second straightening step. As a result, even when the flat tubes (20) are long, the bending in the vertical direction of the first assembly (50) arranged with the flat tubes (20) positioned on the lower side can be reliably straightened.

[0118] <Third Modification> In the manufacturing method of the heat exchanger (10) of this embodiment, the arrangement of the flat tubes (20) and the slot rows (35) into which the flat tubes (20) are not inserted in each of the first assembly (50) and the second assembly (55) is not limited to the arrangement shown in Figure 10.

[0119] 21, in the first step, two flat tubes (20) may be inserted into every third slot row (35) aligned in the longitudinal direction of the fins (30) constituting the first fin group (41). In the second step, two flat tubes (20) may be inserted into every third slot row (35) aligned in the longitudinal direction of the fins (30) constituting the second fin group (42).

[0120] <Fourth Modification> In the third step, the second assembly (55) disposed below the first assembly (50) may be moved upward to combine the first assembly (50) and the second assembly (55) to form the core (15). In addition, in the third step, the first assembly (50) may be moved downward and the second assembly (55) may be moved upward at the same time to combine the first assembly (50) and the second assembly (55) to form the core (15). In this manner, in the third step of this embodiment, the first assembly (50) and the second assembly (55) are combined by bringing the first assembly (50) and the second assembly (55) disposed below the first assembly (50) relatively close to each other.

[0121] Fifth Modification In the manufacturing method of the heat exchanger (10) of the present embodiment, the orientation of the first assembly (50) and the second assembly (55) in the step of combining the first assembly (50) and the second assembly (55) to form the core (15) is merely an example. For example, the first assembly (50) and the second assembly (55) may be arranged in an orientation in which the extension direction of the flat tubes (20) is the up-down direction, and the first assembly (50) and the second assembly (55) may be combined by moving one or both of the first assembly (50) and the second assembly (55) in the lateral direction.

[0122] <Sixth Modification> In the manufacturing method of the heat exchanger (10) of this embodiment, the straightening step may include a third straightening step of straightening the horizontal bending of the second assembly (55).

[0123] In the third straightening step, four clamping members are arranged to surround the second assembly (55) placed on the base member (60). The shapes and arrangements of these clamping members are similar to those of the clamping members (71-74) used in the first straightening step. In the third straightening step, the second assembly (55) is clamped from both sides in the arrangement direction of the flat tubes (20) and from both sides in the arrangement direction of the fins (30). As a result, the horizontal deflection of the second assembly (55) placed on the base member (60) is straightened.

[0124] <Seventh Modification> In the manufacturing method of the heat exchanger (10) of the present embodiment, the number of the flat tubes (20) constituting the first assembly (50) and the number of the flat tubes (20) constituting the second assembly (55) may be the same or different. When the number of the flat tubes (20) constituting the heat exchanger (10) is an even number, it is preferable that the number of the flat tubes (20) constituting the first assembly (50) and the number of the flat tubes (20) constituting the second assembly (55) are the same. When the number of the flat tubes constituting the heat exchanger (10) is an odd number, it is preferable that one of the number of the flat tubes (20) constituting the first assembly (50) and the number of the flat tubes (20) constituting the second assembly (55) is one more than the other.

[0125] Although the embodiments and modifications have been described above, it will be understood that various modifications of form and details are possible without departing from the spirit and scope of the claims. In addition, the elements of the above embodiments, modifications, and other embodiments may be appropriately combined or substituted. In addition, the descriptions "first," "second," "third," etc. in the specification and claims are used to distinguish the words to which these descriptions are attached, and do not limit the number or order of the words. [Industrial Applicability]

[0126] INDUSTRIAL APPLICABILITY As described above, the present disclosure is useful for a method for manufacturing a heat exchanger. [Explanation of symbols]

[0127] 10 Heat exchanger 20 flat tube 30 Finn 32 Slots 33 Open end 41 First Fin Group 42 2nd Fin Group 50 1st assembly 55 Second assembly 65 Pressing member 66 Pressing surface 67 Pressing block

Claims

1. A method for manufacturing a heat exchanger (10) comprising a plurality of flat tubes (20), and a first fin group (41) and a second fin group (42), each of which is composed of a plurality of plate-like fins (30), wherein a plurality of slots (32) having open ends (33) are formed in each of the plurality of fins (30) at an outer edge of the fin (30), and each of the plurality of flat tubes (20) is inserted into the slots (32) of each of the fins (30) constituting the first fin group (41) and the slots (32) of each of the fins (30) constituting the second fin group (42), a first step of inserting the flat tubes (20) into some of the slots (32) of the fins (30) constituting the first fin group (41) to form a first assembly (50) consisting of the first fin group (41) and the flat tubes (20); a second step of inserting the flat tube (20) into one of the slots (32) of the fins (30) constituting the second fin group (42) that corresponds to the slot (32) into which the flat tube (20) of the first fin group (41) is not inserted, thereby forming a second assembly (55) consisting of the second fin group (42) and the flat tube (20); and a third step of arranging the first assembly (50) in a position where the flat tubes (20) of the first assembly (50) face the second assembly (55), arranging the second assembly (55) in a position where the flat tubes (20) of the second assembly (55) face the first assembly (50), and pressing the first assembly (50) against the second assembly (55) to insert the flat tubes (20) of the first assembly (50) into the slots (32) of the fins (30) of the second assembly (55), and inserting the flat tubes (20) of the second assembly (55) into the slots (32) of the fins (30) of the first assembly (50). A method for manufacturing a heat exchanger.

2. In the first step, the flat tubes (20) are inserted into predetermined slots (32) of the fins (30) constituting the first fin group (41) such that the slots (32) into which the flat tubes (20) are inserted and the slots (32) into which the flat tubes (20) are not inserted are arranged alternately; In the second step, the flat tubes (20) are inserted into predetermined slots (32) of the fins (30) constituting the second fin group (42) such that the slots (32) into which the flat tubes (20) are inserted and the slots (32) into which the flat tubes (20) are not inserted are arranged alternately. A method for manufacturing the heat exchanger according to claim 1.

3. In the third step, the first assembly (50) is disposed in a position in which the flat tubes (20) are located on the lower side, the second assembly (55) is disposed in a position in which the flat tubes (20) are located on the upper side, and the first assembly (50) is moved downward to press the first assembly (50) against the second assembly (55). A method for manufacturing the heat exchanger according to claim 1 or 2.

4. In the third step, a pressing member (65) having a flat pressing surface (66) on the lower surface is used, and the pressing surface (66) of the pressing member (65) is brought into contact with the upper outer edges of the fins (30) of the first assembly (50) arranged in an orientation in which the flat tubes (20) are located on the lower side, and the first assembly (50) is pressed down by the pressing member (65), thereby pressing the first assembly (50) against the second assembly (55). A method for manufacturing the heat exchanger according to claim 3.

5. The pressing member (65) used in the third step includes a plurality of pressing blocks (67), the lower surface of each of which constitutes the pressing surface (66). A method for manufacturing the heat exchanger according to claim 4.

6. The third step includes a straightening step of straightening deflection of the first assembly (50) arranged in an attitude in which the flat tube (20) is located on the lower side, In the third step, the first assembly (50) in a state where the deflection has been corrected is pressed against the second assembly (55). A method for manufacturing the heat exchanger according to claim 1 or 2.

7. The straightening step includes a first straightening step of straightening the horizontal deflection of the first assembly (50) by clamping the first assembly (50) from the horizontal direction. A method for manufacturing the heat exchanger according to claim 6.

8. In the first straightening step of the straightening process, the first assembly (50) is sandwiched from both sides in the arrangement direction of the flat tubes (20) and from both sides in the arrangement direction of the fins (30). A method for manufacturing the heat exchanger according to claim 7.

9. In the third step, a pressing member (65) having a flat pressing surface (66) on the lower surface is used, and the pressing surface (66) of the pressing member (65) is brought into contact with the upper outer edges of the fins (30) of the first assembly (50) arranged in an orientation in which the flat tubes (20) are located on the lower side, and the first assembly (50) is pressed down by the pressing member (65), thereby pressing the first assembly (50) against the second assembly (55); The straightening step includes a second straightening step of pressing the first assembly (50) against the pressing surface (66) of the pressing member (65) to straighten the deflection of the first assembly (50) in the vertical direction. A method for manufacturing the heat exchanger according to claim 6.

10. In the second straightening step of the straightening process, both ends of the flat tube (20) in the first assembly (50) are lifted to press the first assembly (50) against the pressing surface (66) of the pressing member (65). A method for manufacturing the heat exchanger according to claim 9.

11. In the second straightening step of the straightening process, both ends of the flat tube (20) in the first assembly (50) and a middle portion in the extension direction of the flat tube (20) are lifted, thereby pressing the first assembly (50) against the pressing surface (66) of the pressing member (65). A method for manufacturing the heat exchanger according to claim 9.

Citation Information

Patent Citations

  • Micro-channel heat exchanger and air conditioner

    CN112444146A

  • A heat transfer component that is arranged in low temperature waste heat from flue gas to retrieve and utilize

    CN205748069U

  • Fin tube type heat exchanger, its manufacturing method, and refrigeration air conditioner

    JP2003262485A

  • Heat exchanger, and heat pump device

    JP2013221713A

  • Device for inserting flat tubes in heat exchanger fins

    WO2017006446A1