Fusion method

The method uses a heating element with oriented carbon nanotubes and an insulating layer to ensure uniform temperature distribution and improved fusion strength by heating and pressurizing adherends within specific temperature ranges, addressing uneven temperature distribution and short-circuiting issues in existing fusing technologies.

JP2024150119APending Publication Date: 2024-10-23MITSUBISHI HEAVY IND LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023063379
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-10
Publication Date
2024-10-23

AI Technical Summary

Technical Problem

The existing fusing methods using a unidirectional carbon fiber heating element result in uneven temperature distribution and potential short-circuiting, leading to decreased fusion strength and non-uniformity in the welding surface.

Method used

A method involving a heating element with carbon nanotubes oriented in different directions, sandwiched between adherends with an insulating layer, heats the adherends above the thermoplastic resin's melting or crystallization temperature before pressurizing them within the glass transition temperature range to ensure uniform temperature distribution and prevent short-circuiting.

Benefits of technology

The method achieves uniform temperature distribution and enhanced fusion strength by minimizing temperature differences and reducing short-circuit risks, resulting in suitable adhesion of the adherends.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024150119000001_ABST
    Figure 2024150119000001_ABST
Patent Text Reader

Abstract

To provide a fusion method that fuses adherends optimally with uniform temperature distribution within the fusion surface.SOLUTION: Provided is a fusion bonding method for fusing adherends by generating heat in a heating element arranged between the adherends via an insulating layer, the adherend including carbon fibres and a thermoplastic resin impregnated with the carbon fibres, the heating element including a fibre sheet comprising fibres including carbon nanotubes oriented in different fibre directions, and the insulating layer including a resin. The fusion bonding method includes steps of: placing the heating element between the adherends and placing the insulating layer between the adherend and the heating element; heating the heating element to a temperature higher than the melting point temperature of the thermoplastic resin or the crystallisation start temperature of the thermoplastic resin by raising the temperature; and applying pressure to the adherends together after heating, in a temperature range from below the melting point temperature or below the crystallisation start temperature to the crystallisation stop temperature or glass transition temperature of the thermoplastic resin.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a fusion method for fusion bonding adherends together. [Background technology]

[0002] Conventionally, a fusion method for fusing a first composite material containing a carbon fiber base material and a thermoplastic resin to a second composite material is known (for example, see Patent Document 1). In this fusion method, the first composite material and the second composite material are fused to each other by heating an electric conductive sheet disposed between the first composite material and the second composite material while the first composite material and the second composite material are in a pressurized state. The electric conductive sheet is made of a carbon fiber base material oriented in one direction. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2022-175320 A Summary of the Invention [Problem to be solved by the invention]

[0004] However, when a unidirectional material is used as a heating element containing carbon fibers such as an electrically conductive sheet, the temperature distribution in the direction perpendicular to the orientation direction is likely to be non-uniform within the fusion surface of the adherend, i.e., the temperature difference within the fusion surface is likely to be large, and the fusion strength may be reduced. Also, when the adherends are heated by a heating element while being pressed against each other, the carbon fibers contained in the adherends and the heating element are likely to short-circuit, and the temperature distribution within the fusion surface is likely to be non-uniform, and the fusion strength may be reduced.

[0005] Therefore, an object of the present disclosure is to provide a fusion method that can uniformize the temperature distribution within the fusion surface and suitably fuse adherends together. [Means for solving the problem]

[0006] The fusion method disclosed herein is a fusion method in which a heating element that is placed between adherends via an insulating layer is heated to fuse the adherends together, the adherends comprising carbon fibers and a thermoplastic resin impregnated into the carbon fibers, the heating element comprising a fiber sheet in which fibers including carbon nanotubes are oriented in different fiber directions, and the insulating layer comprises a resin, and the fusion method includes the steps of placing the heating element between the adherends and placing the insulating layer between the adherends and the heating element, raising the temperature of the heating element to a temperature higher than the melting point temperature of the thermoplastic resin or the crystallization onset temperature of the thermoplastic resin, and after heating, applying pressure to the adherends in a range from a temperature below the melting point temperature or the crystallization onset temperature to a crystallization stop temperature or the glass transition temperature of the thermoplastic resin. Effect of the Invention

[0007] According to the present disclosure, adherends can be suitably fused to each other. [Brief description of the drawings]

[0008] [Figure 1] FIG. 1 is an explanatory diagram of the fusion method according to the first embodiment. [Diagram 2] FIG. 2 is a graph showing changes in temperature and pressure in the fusion method according to the first embodiment. [Diagram 3] FIG. 3 is an explanatory diagram of the fusion method according to the second embodiment. [Figure 4] FIG. 4 is an explanatory diagram regarding test results of an example of a fusion method. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] Hereinafter, the embodiments of the present disclosure will be described in detail with reference to the drawings. Note that the disclosure is not limited to these embodiments. In addition, the components in the following embodiments include those that are easily replaceable by those skilled in the art, or those that are substantially the same. Furthermore, the components described below can be appropriately combined, and when there are multiple embodiments, each embodiment can be combined.

[0010] [First embodiment] The fusion method according to the first embodiment is a method in which a heating element 7, which is disposed between adherends 5 with an insulating layer 6 interposed therebetween, is heated to fuse the adherends 5 together. Fig. 1 is an explanatory diagram of the fusion method according to the first embodiment. Fig. 2 is a graph showing changes in temperature and pressure in the fusion method according to the first embodiment. First, the adherends 5, insulating layer 6, and heating element 7 will each be described.

[0011] The adherend 5 is a composite material including carbon fiber and a thermoplastic resin impregnated into the carbon fiber. The adherend 5 is formed, for example, in a plate shape. The carbon fiber is a fiber having electrical conductivity. Examples of the thermoplastic resin include polyether ether ketone (PEEK), polyaryl ether ketone (PAEK), PPS (polyphenylene sulfide), polyetherimide (PEI), polyamide (PA), etc.

[0012] The insulating layer 6 is a sheet containing at least a resin. For the insulating layer 6, a resin film using a resin or a glass mat in which glass fibers or glass beads are impregnated with a resin is used. The resin of the insulating layer 6 is the same as the resin contained in the adherend 5. The thickness of the insulating layer 6 is 0.06 mm or less.

[0013] The heating element 7 is a fiber sheet formed from fibers containing carbon nanotubes, and serves as a resistor that generates heat when electricity is applied. A pair of (positive and negative) electrodes 11 are in contact with the heating element 7. The fiber sheet has a carbon nanotube basis weight of 10 g / m 2The heating element 7 has fibers with different fiber directions. The heating element 7 may be a nonwoven fabric or a woven fabric. The thickness of the heating element 7 is 0.12 mm or less.

[0014] The heating element 7 may also be a fiber sheet impregnated with a resin. When the fiber sheet is impregnated with a resin, the resin is preferably the same as the thermoplastic resin contained in the adherend 5. The impregnation rate of the resin impregnated into the fiber sheet may be 9% or more, and preferably in the range of 24% to 100%. The optimum impregnation rate is 56% or more.

[0015] (fusion method) Next, the fusion method will be described with reference to FIG. 1 and FIG. 2. As shown in FIG. 1, in the fusion method, step S1 is performed in which a heating element 7 is disposed between the adherends 5, and an insulating layer 6 is disposed between the adherends 5 and the heating element 7. Specifically, as shown in FIG. 1, in step S1, when the adherends 5, that is, the two adherends 5, are overlapped, the heating element 7 is disposed between the two adherends 5. At this time, the heating element 7 is disposed so that the part where the electrode 11 contacts is exposed to the outside. Since an insulating layer 6 is disposed between each of the two adherends 5 and the heating element 7, the heating element 7 and the two insulating layers 6 are laminated to form a three-layer structure. The heating element 7 and the two insulating layers 6 may be integrated to form a single-layer structure. The heating element 7 and the two insulating layers 6 may also be integrated with each of the two adherends 5.

[0016] After performing step S1, the fusion method performs step S2 in which the heating element 7 is heated to a temperature higher than the melting point temperature of the thermoplastic resin contained in the adherend 5 or a temperature higher than the crystallization start temperature of the thermoplastic resin. In step S2, as shown in FIG. 2, electricity is applied to the heating element 7 from the electrode 11 to heat the adherend 5 to a temperature T higher than the melting point temperature of the thermoplastic resin. In step S2, the adherends 5 are not pressed against each other. In step S2, the adherends 5 are not actively pressed, but contact pressure is generated due to their own weight or the like. In step S2, the temperature T of the thermoplastic resin of the adherend 5 is set to a temperature higher than the melting point temperature of the thermoplastic resin, but it may be higher than the crystallization start temperature of the thermoplastic resin.

[0017] After step S2 is performed, in the fusion method, after heating in step S1, step S3 is performed in which the adherends 5 are pressed together in a range from a temperature below the melting point temperature of the thermoplastic resin or below the crystallization start temperature of the thermoplastic resin to the crystallization stop temperature of the thermoplastic resin or the glass transition temperature of the thermoplastic resin. In step S3, as shown in FIG. 2, no pressure is applied until the thermoplastic resin is below the melting point temperature, and when the thermoplastic resin is below the melting point temperature, pressure is applied to the adherends 5. In step S3, the cooling rate of the adherends 5 during pressure application is a cooling rate that satisfies the required crystallinity in advance, and specifically, the cooling rate is 100° C. / min or less. Then, in step S3, pressure is applied to the adherends 5 until the crystallization stop temperature of the thermoplastic resin or the glass transition temperature of the thermoplastic resin is reached. The pressure applied to the adherends 5 in step S3 may be continued or released after the temperature becomes lower than the crystallization stop temperature of the thermoplastic resin or the glass transition temperature of the thermoplastic resin.

[0018] [Second embodiment] Next, a second embodiment will be described with reference to Fig. 3. Fig. 3 is an explanatory diagram of a fusion method according to the second embodiment. In the second embodiment, in order to avoid repetitive description, only parts different from the first embodiment will be described, and parts having the same configuration as the first embodiment will be described with the same reference numerals.

[0019] In the fusion method of the second embodiment, the heating element 7 of the first embodiment has a portion impregnated with the thermoplastic resin and a portion not impregnated with the thermoplastic resin. Specifically, the heating element 7 includes a fusion portion 7a to which the adherend 5 is fused, and an electrode portion 7b to which the electrode 11 is in contact. The thermoplastic resin is impregnated in the fusion portion 7a, but not in the electrode portion 7b. In other words, the heating element 7 has a portion impregnated with the thermoplastic resin as the fusion portion 7a, and a portion not impregnated with the thermoplastic resin as the electrode portion 7b. The heating element 7 is disposed between the adherends 5 with the electrode portion 7b exposed to the outside.

[0020] Next, with reference to Fig. 4, test results of an example of the heating element 7 and insulating layer 6 in the fusion method will be described. Fig. 4 is an explanatory diagram of test results of an example of the fusion method. The heating element 7 is a nonwoven fabric (fiber sheet) using fibers containing carbon nanotubes, and this nonwoven fabric is impregnated with a thermoplastic resin. The heating element 7 is impregnated with resin at the fused portion 7a, but not at the electrode portion 7b. The heating element 7 has a thickness of 0.07 mm at the fused portion 7a. The insulating layer 6 is a glass mat made of glass fibers impregnated with resin, and has a thickness of 0.05 mm.

[0021] In the test results using the above heating element 7 and insulating layer 6, the fusion of the adherends 5 was successful, and the strength test results of the fused product showed 80% or more of the resin strength. Therefore, it was confirmed that sufficient fusion strength could be obtained.

[0022] As described above, the fusion methods described in the first and second embodiments can be understood, for example, as follows.

[0023] The fusion method according to the first embodiment is a fusion method in which a heating element 7 arranged between adherends 5 with an insulating layer 6 interposed therebetween is heated to fuse the adherends 5 together, the adherends 5 comprising carbon fibers and a thermoplastic resin impregnated into the carbon fibers, the heating element 7 comprising a fiber sheet in which fibers including carbon nanotubes are oriented in different fiber directions, and the insulating layer 6 comprises a resin, and the fusion method includes the following steps: step S1 of arranging the heating element 7 between the adherends 5 and arranging the insulating layer 6 between the adherends 5 and the heating element 7; step S2 of heating the heating element 7 to a temperature higher than the melting point temperature of the thermoplastic resin or a temperature higher than the crystallization start temperature of the thermoplastic resin; and step S3 of pressing the adherends 5 together after heating in a temperature range from below the melting point temperature or the crystallization start temperature to the crystallization stop temperature or the glass transition temperature of the thermoplastic resin.

[0024] According to this configuration, a fiber sheet containing carbon nanotubes can be used as the heating element 7, so that the temperature distribution of the adherend 5 during heating by the heating element 7 can be made uniform, and the temperature difference in the fusion surface where the adherends 5 are fused together can be reduced. In addition, when the adherends are pressed together, the temperature can be set within a range from a melting point temperature or a crystallization start temperature to a crystallization stop temperature or a glass transition temperature of the thermoplastic resin, so that the carbon fibers contained in the adherend 5 and the heating element are less likely to short-circuit, and the temperature distribution in the fusion surface can be made uniform. As a result, the temperature distribution in the fusion surface can be made uniform, and the adherends 5 can be fused together in an appropriate manner.

[0025] As a second aspect, in the fusion method according to the first aspect, the fiber sheet is a nonwoven fabric.

[0026] According to this configuration, the temperature distribution during heating of the heating element 7 can be made more uniform.

[0027] As a third aspect, in the fusion method according to the first or second aspect, the fiber sheet has a basis weight of the carbon nanotubes of 10 g / m 2 The following is the result.

[0028] According to this configuration, the basis weight of the carbon nanotubes can be set to an appropriate basis weight, so that heating by the heating element 7 can be performed suitably and the fusion strength of the adherend 5 can be made sufficient.

[0029] As a fourth aspect, in the fusion method according to any one of the first to third aspects, the heating element further includes a resin impregnated in the fiber sheet.

[0030] According to this configuration, the fiber sheet of the heating element 7 can be impregnated with resin, thereby enabling favorable fusion between the adherend 5 and the heating element 7, and also enabling favorable fusion between the adherends 5 themselves.

[0031] As a fifth aspect, in the fusion bonding method according to the fourth aspect, the impregnation rate of the resin impregnated into the fiber sheet is 9% or more.

[0032] According to this configuration, the temperature distribution during heating of the heating element 7 can be appropriately made uniform.

[0033] As a sixth aspect, in the fusion method according to the fifth aspect, the impregnation rate of the resin impregnated into the fiber sheet is in the range of 24% to 100%.

[0034] According to this configuration, the temperature distribution during heating of the heating element 7 can be more appropriately made uniform.

[0035] As a seventh aspect, in the fusion bonding method according to the sixth aspect, the impregnation rate of the resin impregnated into the fiber sheet is 56% or more.

[0036] According to this configuration, the temperature distribution during heating of the heating element 7 can be made optimally uniform.

[0037] As an eighth aspect, in the fusion method according to the fourth aspect, the heating element 7 includes a fusion portion 7a to which the adherend 5 is fused, and an electrode portion 7b to which an electrode 11 for generating heat from the heating element 7 comes into contact, and the resin is impregnated into the fusion portion 7a but not into the electrode portion 7b.

[0038] This configuration allows the electrodes 11 to be in proper contact with the fiber sheet of the heating element 7.

[0039] As a ninth aspect, in the fusion bonding method according to any one of the first to eighth aspects, the heating element has a thickness of 0.12 mm or less.

[0040] According to this configuration, the thickness of the heating element 7 can be made thin, so that the adherends 5 can be fused to each other suitably.

[0041] As a tenth aspect, in the fusion bonding method according to any one of the first to ninth aspects, the insulating layer has a thickness of 0.06 mm or less.

[0042] According to this configuration, heat can be suitably transferred from the heating element 7 to the adherend 5 .

[0043] As an eleventh aspect, in the fusion bonding method according to any one of the first to tenth aspects, the insulating layer 6 further includes glass fibers impregnated with the resin.

[0044] According to this configuration, the insulating layer 6 can suitably prevent short circuits between the heating element 7 and the carbon fibers of the adherend 5.

[0045] As a twelfth aspect, in the fusion method according to any one of the first to eleventh aspects, in step S2 of pressing the adherends 5 together, the cooling rate of the adherends 5 is a cooling rate that satisfies the predetermined required degree of crystallinity.

[0046] According to this configuration, when the adherends 5 are pressed together, the temperature can be raised to a temperature that promotes crystallization of the thermoplastic resin, thereby increasing the fusion strength.

[0047] As a thirteenth aspect, in the fusion method according to the twelfth aspect, the cooling rate is 100° C. / min or less.

[0048] According to this configuration, the temperature of the thermoplastic resin can be adjusted to a temperature suitable for crystallization. [Explanation of symbols]

[0049] 5 Adherent 6 Insulating layer 7 Heating element 11 electrodes

Claims

1. A fusion method for fusion-bonding adherends by heating a heating element disposed between the adherends with an insulating layer interposed therebetween, comprising the steps of: The adherend includes carbon fibers and a thermoplastic resin impregnated into the carbon fibers, The heating element includes a fiber sheet in which fibers containing carbon nanotubes are oriented in different fiber directions, The insulating layer includes a resin, disposing the heating element between the adherends and disposing the insulating layer between the adherends and the heating element; A step of increasing the temperature of the heating element to a temperature higher than the melting point temperature of the thermoplastic resin or a temperature higher than the crystallization starting temperature of the thermoplastic resin; and after heating, applying pressure to the adherends at a temperature ranging from below the melting point temperature or below the crystallization onset temperature to a crystallization stop temperature or a glass transition temperature of the thermoplastic resin.

2. The fusion method according to claim 1 , wherein the fiber sheet is a nonwoven fabric.

3. The fiber sheet has a basis weight of the carbon nanotubes of 10 g / m 2 The fusing method according to claim 1, wherein:

4. The fusing method according to claim 1 , wherein the heating element further comprises a resin impregnated in the fiber sheet.

5. The fusion method according to claim 4, wherein the impregnation rate of the resin impregnated into the fiber sheet is 9% or more.

6. 6. The fusion method according to claim 5, wherein the impregnation rate of the resin impregnated into the fiber sheet is in the range of 24% to 100%.

7. The fusion method according to claim 6, wherein the impregnation rate of the resin impregnated into the fiber sheet is 56% or more.

8. The heating element includes a fusion portion to which the adherend is fused, and an electrode portion to which an electrode for generating heat from the heating element is in contact, The fusion method according to claim 4 , wherein the resin is impregnated into the fusion portion but not into the electrode portion.

9. 2. The fusing method according to claim 1, wherein the heating element has a thickness of 0.12 mm or less.

10. 2. The fusion method according to claim 1, wherein the insulating layer has a thickness of 0.06 mm or less.

11. The fusing method according to claim 1 , wherein the insulating layer further comprises glass fibers impregnated with the resin.

12. 2. The fusion method according to claim 1, wherein in the step of pressing the adherends together, the cooling rate of the adherends is set to a value that satisfies a required degree of crystallinity.

13. The fusion method according to claim 12, wherein the cooling rate is 100° C. / min or less.

Citation Information

Patent Citations

  • Fusion method and structure

    JP2022175320A