Friction jointing device and friction jointing method
The friction welding device addresses defects and equipment failure by controlling current and torque limits during the friction heating process, improving bonding accuracy and preventing workpiece rotation, thus ensuring reliable joint formation.
Patent Information
- Application Number
- JP2023063433
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-10
- Publication Date
- 2024-10-23
- Estimated Expiration
- 2043-04-10
AI Technical Summary
Friction welding of workpieces often results in defects and equipment failure due to large torque loads causing workpiece rotation and clamp chuck seizure, with existing power monitoring methods failing to reliably detect these issues.
A friction welding device with current limiting means to control the current flowing through drive sources, implementing stepwise torque limitations during the friction heating process to prevent workpiece rotation and improve bonding accuracy.
The solution effectively suppresses defects in friction welding and enhances the accuracy of determining the welding state by preventing workpiece rotation and clamp chuck damage, ensuring reliable joint formation.
Smart Images

Figure 2024150161000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a friction joining device for frictionally joining two workpieces. [Background technology]
[0002] In order to effectively utilize scraps from workpieces used in machine tools such as automatic lathes, the scraps have been friction-welded to new workpieces (see Patent Document 1). That is, scrap bar material that has reached a length where it is no longer possible to machine a workpiece is friction-welded to a newly supplied bar material and used as material for the next processing, which can reduce material costs and environmental impact.
[0003] In friction welding, the sliding parts of two workpieces are softened by the frictional heat generated in the sliding parts, and the sliding parts are joined by stopping the relative rotation of the sliding parts while applying pressure, and the two workpieces are joined together. Specifically, the first workpiece (a new bar material to be used in the next process) held by the main spindle (first spindle) and the second workpiece (a remnant material left in the previous process) held by the back spindle (second spindle) are rotated relative to each other. Then, the axial distance between the spindles is narrowed, and the opposing end faces of the first and second workpieces are pressed against each other and slid against each other, generating frictional heat in the sliding parts. When the joint parts are sufficiently softened by friction, the relative rotation between the spindles is stopped while maintaining the pressure. When the heat subsides due to the halt of rotation, the sliding parts solidify in a bonded state, and the remnant material and the new material are joined together.
[0004] Here, a large torque load is generated in the drive mechanism that drives the spindle when the workpieces rotating at high speed come into contact with each other. This large torque load can cause various problems such as poor work connection and equipment failure. For example, when the workpieces rotate relative to each other, the remaining workpiece on the back spindle side, which is stopped, starts to rotate together with the workpiece on the front spindle side, and the remaining workpiece and the clamp chuck that holds it may seize and the clamp chuck may be damaged.
[0005] Patent Document 2 discloses a method for monitoring whether the active power supplied from an external power source to a system power source is within a tolerance range of a predetermined numerical range set for each process, and judging whether an abnormality occurs and whether the joint state of the joint is good or bad. In particular, in the latter half of the process from when the joint melts to when the rotation is stopped, the quality of the joint is judged based on a difference signal obtained by subtracting the moving average of the active power output value. However, even if the power value is monitored in this way, it may be difficult to detect the occurrence of the above-mentioned malfunction. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] JP 2000-202648 A [Patent Document 2] JP 2009-082951 A Summary of the Invention [Problem to be solved by the invention]
[0007] An object of the present invention is to provide a technique capable of suppressing the occurrence of defects in friction joining and improving the accuracy of determining whether the joining state is good or bad. [Means for solving the problem]
[0008] In order to achieve the above object, the friction joining device of the present invention comprises: a first spindle that grips a first workpiece; a second spindle that holds a second workpiece so as to face the first workpiece in the axial direction; a first drive mechanism having a first drive source and configured to move the first spindle in the axial direction by a drive force of the first drive source; a second drive mechanism including a second drive source and configured to move the second spindle in the axial direction by a drive force of the second drive source; a rotation drive mechanism that rotates the first workpiece and the second workpiece relatively around a rotation axis along the axial direction; a control means for controlling the first drive mechanism, the second drive mechanism, and the rotation drive mechanism so as to bring the first workpiece and the second workpiece into contact with each other while rotating relative to each other, thereby joining the first workpiece and the second workpiece; a current limiting unit that limits a current flowing through the first drive source and the second drive source to a predetermined limit value or less; In a friction joining apparatus comprising: The current limiting means limits the current flowing through the first driving source and the second driving source during a first frictional heating period, which is a predetermined period from immediately after the first workpiece and the second workpiece come into contact with each other, to a first limiting value or less that is smaller than a second limiting value for limiting the current flowing through the first driving source and the second driving source during a second frictional heating period after the first frictional heating period has elapsed. Effect of the Invention
[0009] According to the present invention, it is possible to suppress the occurrence of defects in friction joining and to improve the accuracy of determining whether the joining state is good or bad. [Brief description of the drawings]
[0010] [Figure 1] 1 is a configuration explanatory diagram of a friction welding device according to an embodiment of the present invention; [Diagram 2] 4A to 4C are explanatory views of the friction welding apparatus according to the embodiment of the present invention during a friction welding operation. [Diagram 3] FIG. 13 is a diagram showing a change over time in load during a friction welding operation in which a defect occurs. [Figure 4] FIG. 11 is a diagram showing a change in load over time during a friction welding operation in an embodiment of the present invention. [Diagram 5] FIG. 5 is a diagram showing the droop with respect to the relative position of the spindle corresponding to FIG. 4. [Figure 6] FIG. 2 is a flow diagram of a friction welding process in an embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] Preferred embodiments of the present invention will be described below with reference to the drawings. However, the embodiments described below merely exemplify preferred configurations of the present invention, and the scope of the present invention is not limited to these configurations. Furthermore, unless otherwise specified, the hardware and software configurations of the device, manufacturing conditions, functions, materials, shapes, and relative positions of components in the following description are not intended to limit the scope of the present invention to these alone. In addition, the same components are generally given the same reference numbers, and repeated explanations will be omitted.
[0012] (Example) Fig. 1 is a schematic diagram showing the configuration of a machine tool 1 as a friction joining device according to an embodiment of the present invention. The machine tool 1 shown in Fig. 1 is a so-called automatic lathe device, which rotates a workpiece W, for example a long bar material, and applies a cutting tool (machining tool) to it to perform cutting (turning). The machine tool 1 according to this embodiment is configured so that it can also be used as a friction joining device that joins the remaining workpiece W2 to a newly supplied workpiece W1 after cutting out the machined workpiece to the limit from one workpiece W.
[0013] The machine tool 1 generally includes a first spindle mechanism (front spindle mechanism) 100 and a second spindle mechanism (rear spindle mechanism) 200 arranged opposite each other on a base (not shown), and a tool rest (not shown). The first spindle mechanism 100 has a first spindle (front spindle) 101, and the second spindle mechanism 200 has a second spindle (rear spindle) 201, and these two spindles are arranged so that their respective axes are approximately concentric or parallel to each other. The direction of the axes is defined as the Z-axis direction, and among the directions perpendicular to the axial directions, a direction parallel to the vertical direction is defined as the X-axis direction, and a direction parallel to the horizontal direction is defined as the Y-axis direction. FIG. 1 is a schematic diagram of the configuration of machine tool 1 as viewed in a plan view in the Y-axis direction.
[0014] The first spindle mechanism 100 includes a first drive mechanism GZ1 for moving a first spindle stock 102, which rotatably supports the first spindle 101, in the Z-axis direction on a base. The first drive mechanism GZ is a ball screw drive mechanism made up of a first motor MZ1 (servo motor) as a first drive source, a ball screw, a guide rail, etc. By driving and rotating the ball screw drive mechanism by the first motor MZ1, it is possible to move the first spindle 101 together with the first spindle stock 102 in the axial direction (Z-axis direction).
[0015] The second spindle mechanism 200 also includes a second drive mechanism GZ2 for moving a second spindle stock 202, which rotatably supports the second spindle 201, in the Z-axis direction on a base. The second drive mechanism GZ2 is a ball screw drive mechanism composed of a second motor MZ2 as a second drive source, a ball screw, a guide rail, etc. By driving and rotating the ball screw drive mechanism by the second motor MZ2, the second spindle 201 can be moved in the axial direction (Z-axis direction) together with the second spindle stock 202.
[0016] The mechanism for relatively moving the first spindle mechanism 100 and the second spindle mechanism 200 in the Z-axis direction, which is the direction of the rotation axes of the spindles, is not limited to a specific configuration, and the above-mentioned configuration is merely an example. Also, a drive mechanism for moving the first spindle stock 102 and the second spindle stock 202 in the Y-axis direction or the X-axis direction, in addition to the Z-axis direction, may be provided.
[0017] The first spindle stock 102 is configured to include, for example, a first built-in motor MR1 as a rotation drive source as a rotation drive mechanism, and is configured to be able to rotate and drive the first spindle 101 by the rotation drive force of the first built-in motor MR1. Similarly, the second spindle stock 202 is configured to be able to rotate and drive the second spindle 201 by the rotation drive force provided by a second built-in motor MR2 as a rotation drive source. However, in the case where the machine tool 1 is used as a friction welding device described later, in this embodiment, the friction welding process is performed with the second spindle 201 in a stationary state without rotating. Note that the above-mentioned configuration is not limited as long as the first workpiece and the second workpiece can be in a predetermined relative rotation state in the friction welding. In other words, a configuration in which both the first spindle 101 and the second spindle 201 are rotated may be used, or a configuration in which the second spindle 201 is rotated without rotating the first spindle 101 may be used. Furthermore, the power source configuration is not limited to a built-in motor, but may be configured to transmit a rotational driving force from an external power source to rotate the device.
[0018] The first spindle 101 has a hollow structure with a workpiece holding hole for holding or gripping the workpiece W1 as the first workpiece, and is equipped with a first chuck 103 and a chuck sleeve (not shown) for holding the workpiece W1 (a state in which the axis of the workpiece W1 in the first spindle 101 is fixed and axial movement is restricted). The workpiece holding hole opens toward the second spindle in the axial direction, and a portion of the workpiece W1 exposed from the opening is to be turned by a cutting tool supported by a tool rest (not shown). A guide bush, which is a support structure for the workpiece W1, may be arranged in front of the first spindle 101.
[0019] The first chuck 103 and the chuck sleeve (not shown) are configured such that the chuck sleeve is joined to the first chuck 103 from the rear in the axial direction via a tapered surface, the chuck sleeve being restricted in its axial movement. The chuck sleeve is moved in the axial direction by receiving a force from a fluid cylinder (not shown) driven by hydraulic pressure, air, or the like, and the first A force including a component force in a direction toward the axis is applied to the chuck 103, generating a clamping force in the chuck such that the slits provided in the first chuck 103 close. This creates a state in which the workpiece W1 is gripped.
[0020] The configuration on the second spindle 201 side is similar to the configuration on the first spindle 101 side, and includes a second chuck 203 and a chuck sleeve, and is capable of gripping and rotating a workpiece W2 as a second workpiece. The basic configuration is similar to that of a conventionally known back spindle configuration. When the machine tool 1 is used as a friction joining device, the workpiece W2 gripped by the second spindle 201 becomes a workpiece that is a residual material remaining after the workpiece is gripped by the first spindle 101 and turned by the cutting tool 301 of the tool rest 300.
[0021] The machine tool 1 includes a tool rest 300 equipped with a cutting tool 301 for cutting, and a drive mechanism 302 for moving the tool rest 300. The tool rest 300 and the cutting tool 301 are configured to be movable at least in the cutting direction (X-axis direction) and the feed direction (Z-axis direction) by driving the drive mechanism 302. When used as a cutting device, the machine tool 1 can perform cutting on the workpiece W by bringing the cutting tool 301 into contact with the workpiece W in a state where the workpiece W is rotated at a predetermined processing rotation speed corresponding to the cutting.
[0022] The workpieces W to be cut include a first workpiece W1 held by the first spindle 101, a second workpiece W2 held by the second spindle 201, and a third workpiece W3 formed by frictionally joining the first workpiece W1 and the second workpiece W2 as a remaining material.
[0023] A plurality of cutting tools 301 may be prepared so as to be selectable according to the type of the intended machining. That is, the tool rest 300 is provided with a plurality of cutting tools 301, and a desired cutting process (turning process) can be performed on the workpiece W by bringing a selected one of the cutting tools 301 into contact with the workpiece W.
[0024] Machine tool 1 includes a control unit 4 as control means for controlling various operations of each part constituting machine tool 1, such as spindle mechanisms 100, 200, tool rest 300, and a work supply unit (not shown). Control unit 4 can be formed, for example, by a computer equipped with a processor such as a CPU (Central Processing Unit) and storage means such as a memory.
[0025] A first ammeter 410 serving as a current detection means is connected to the first motor MZ1 of the first drive mechanism GZ1. Based on the current value (first current) of the first motor MZ1 detected by the first ammeter 410, the control unit 4 can detect the drive state of the first drive mechanism GZ1 and the load state (torque) of the first drive mechanism GZ1 during driving, etc.
[0026] Similarly, an ammeter 420 serving as a current detection means is connected to the second motor MZ2 of the second drive mechanism GZ2. Based on the current value (second current) of the second motor MZ2 detected by the ammeter 420, the control unit 4 can detect the drive state of the second drive mechanism GZ2 and the load state (torque) of the second drive mechanism GZ2 during driving, etc.
[0027] Furthermore, a first current limiter (filter circuit) 411 serving as a current limiting means is connected to the first motor MZ1 of the first drive mechanism GZ1. The first current limiter 411 is configured to limit the current flowing through the first motor MZ1 to a predetermined limit value or less. This makes it possible to limit the torque generated by the first motor MZ1 to a predetermined torque or less regardless of the operating state of the first drive mechanism GZ1. The first current limiter 411 is configured to vary the magnitude of the current limit value, and in this embodiment, the control unit 4 changes the magnitude of the current limit value by the first current limiter 411 at a predetermined timing in the friction welding process (details will be described later).
[0028] Similarly, a second current limiter (filter circuit) 421 serving as a current limiting means is connected to the second motor MZ2 of the second drive mechanism GZ2. The second current limiter 421 is configured to limit the current flowing through the second motor MZ2 to a predetermined limit value or less, and thereby, regardless of the operating state of the second drive mechanism GZ2, the torque generated by the second motor MZ2 can be limited to a predetermined torque or less. The second current limiter 421 is configured to vary the magnitude of the current limit value, and in this embodiment, the control unit 4 changes the magnitude of the current limit value by the second current limiter 421 at a predetermined timing in the friction welding process (details will be described later).
[0029] 2(a) to 2(d) are schematic diagrams showing the state of friction welding of the first workpiece W1 and the second workpiece W2 by the machine tool 1 as the friction welding device according to this embodiment. FIG. 2(a) is a diagram showing the state when the relative rotation of the first workpiece W1 and the second workpiece W2 is started in friction welding. FIG. 2(b) is a diagram showing the state during the friction heating (friction heat generation) process in friction welding. FIG. 2(c) is a diagram showing the state during the upset pressurizing process in friction welding. FIG. 2(d) is a diagram showing the state at the end of the upset pressurizing process, that is, when the first workpiece W1 and the second workpiece W2 are joined to form the third workpiece W3. Note that in FIGS. 2(a) to 2(d), some of the configurations such as the control unit 4 shown in FIG. 1 are omitted.
[0030] The machine tool 1 as a friction joining device softens the sliding parts of the two workpieces W1, W2 by frictional heat generated at the sliding parts, and joins the sliding parts by stopping the relative rotation of the sliding parts while applying pressure, thereby integrally joining the two workpieces W1, W2. The workpiece W1 held by the first spindle 101 is a new bar material prepared as a workpiece in the turning process performed after the friction joining process. On the other hand, the workpiece W2 held by the second spindle 201 is, as described above, a bar material remaining from the turning process performed before the friction joining process.
[0031] First, as shown in Fig. 2(a), the first spindle 101 is rotated while the two workpieces W1 and W2 are separated from each other in the Z-axis direction, which is the direction of the rotation axis. When the rotation speed is stabilized at a predetermined rotation speed, the first spindle 101 is moved by the first driving mechanism GZ1 at a predetermined feed amount (movement amount per unit time) so as to approach the second spindle 201 in the Z-axis direction. At the same time, the second spindle 201 is also moved by the second driving mechanism GZ2 at a predetermined feed amount so as to approach the first spindle 101 in the Z-axis direction.
[0032] 2(b), the relative distance in the Z-axis direction between the first spindle 101 and the second spindle 201 is maintained so that the opposing end faces of the first workpiece W1 and the second workpiece W2 are pressed against each other with a predetermined contact pressure, and the first workpiece W1 and the second workpiece W2 are caused to slide against each other. In this friction heating process, frictional heat is generated in the sliding parts of the first workpiece W1 and the second workpiece W2, and the sliding parts become softened.
[0033] The relative rotation between the first workpiece W1 and the second workpiece W2 is not limited to the relative rotation caused by stopping the second workpiece W2 and rotating only the first workpiece W1. The relative rotation may be caused by stopping the first workpiece W1 and rotating only the second workpiece W2. Alternatively, the relative rotation may be caused by rotating the first workpiece W1 and the second workpiece W2 in the same direction at different rotation speeds. Furthermore, the relative rotation may be caused by rotating the first workpiece W1 and the second workpiece W2 in opposite directions at different rotation speeds or the same rotation speed.
[0034] As shown in FIG. 2(c), the sliding portion is sufficiently softened by friction, and a high-temperature softened portion J is formed between the first workpiece W1 and the second workpiece W2. While maintaining pressure between the first workpiece W1 and the second workpiece W2, the rotation of the first spindle 101 (relative rotation between the spindles) is stopped.
[0035] The rotation of the first spindle 101 is stopped at the timing when a position command amount (control amount) for the distance (relative position) in the Z-axis direction between the first spindle stock 102 and the second spindle stock 202 reaches a command amount corresponding to a position previously set as a position at which the rotation of the first spindle 101 is stopped. For example, the distance in the Z-axis direction between the spindle stocks 102, 202 may be obtained from the drive amount of the first drive mechanism GZ1 and the second drive mechanism GZ2 (ball screw drive mechanism), or the Z-axis positions of the spindle stocks and spindles may be directly detected by a position sensor or the like. The feed amounts (amount of movement per unit time) of the first spindle stock 102 and the second spindle stock 202 and the rotation speed of the first spindle 101 (relative rotation speed with respect to the second spindle 201) are determined in advance through experiments, etc., from the viewpoint of forming a softened portion J before reaching the rotation stop position. The value is obtained and set from the
[0036] Even after the rotation of the first spindle 101 stops, pressure is continued between the first workpiece W1 and the second workpiece W2, and burrs are pushed out to the outer periphery at the softened portion J, and upset pressure is applied to strengthen the joint between the first workpiece W1 and the second workpiece W2. In the upset pressure process (joining process), a higher pressure is applied between the first workpiece W1 and the second workpiece W2 than in the friction heating process, and the feed rates of the first spindle 101 and the second spindle 201 are controlled so that this pressurized state is maintained for a predetermined period of time. The feed rates of the first workpiece W1 and the second workpiece W2 during upset pressure are set in advance, taking into consideration the approach allowance (the length shortened by the part of the first workpiece W1 and the second workpiece W2 that is released as a burr due to joining).
[0037] As shown in Fig. 2(d), the first workpiece W1 and the second workpiece W2 are joined together by stopping the rotation and dissipating heat from the joint, causing it to solidify. This results in the formation of the third workpiece W3, which is a single bar of material in which the remaining material and the new material are integrated. Burrs generated at the joint between the first workpiece W1 and the second workpiece W2 in the third workpiece W3 are removed by cutting using a cutting tool 301.
[0038] Here, in friction welding, a large torque load is generated on the spindle that rotates the workpiece W when the workpieces rotate at high speed and come into contact with each other. When the workpieces come into contact with each other with a torque equal to or greater than a certain level, the remaining workpiece on the back spindle side, which is stopped during the relative rotation of the workpieces, starts to rotate together with the workpiece on the front spindle side, and the remaining workpiece and the clamp chuck that holds it may seize and damage the clamp chuck.
[0039] This defect is particularly likely to be a problem when friction welding is performed using a machine tool (using a machine tool as a friction welding device) as in this embodiment. In a configuration in which the back spindle uses a clamp chuck to grip the residual material, for example, when friction welding hollow metal pipe materials as workpieces, the workpieces cannot be gripped with a very strong chucking force due to concerns that the shape of the workpieces may be affected. In other words, there are cases in which a limit is set on the chucking force of the clamp chuck of the back spindle. As a result, there is a concern that the workpiece cannot be gripped with sufficient chucking force and the above-mentioned co-rotation may occur.
[0040] Fig. 3 is a time chart showing an example of the change over time of the load applied to the first drive mechanism GZ1 and the second drive mechanism GZ2 during friction welding operation in a comparative example in which the motor current limiting control of the present invention described later is not implemented. Fig. 3 also shows a time chart in the case where the workpiece rotates together on the back spindle side as described above, as an example of welding abnormality. In Fig. 3, the current flowing through the first motor MZ1 of the first drive mechanism GZ1 is indicated by a gray solid line, and the current flowing through the second motor MZ2 of the second drive mechanism GZ2 is indicated by a black solid line.
[0041] In FIG. 3, at time t0, the relative movement of the first spindle 101 and the second spindle 201 in the Z-axis direction is Time t1 indicates the timing when the opposing end faces of the first workpiece W1 and the second workpiece W2 come into contact with each other, i.e., the timing when the friction heating process starts, and corresponds to the state shown in FIG. 2(b). Time t2 indicates the timing when the relative rotation of the first workpiece W1 and the second workpiece W2 stops, i.e., the timing when the friction heating process ends and the upset process starts. Times t0 to t2 shown in FIGS. 4 to 6 are defined in the same way. Each of these timings is preset based on the feed amount set for each process.
[0042] Here, time t2 is the timing when the machine tool 1 and each workpiece W1, W2 should be in the state shown in Fig. 2(b) if the above-mentioned joining abnormality does not occur and the process proceeds normally. However, in the friction heating process of the comparative example, the second workpiece W2 rotates with the first workpiece W1, and the sliding portion between the first workpiece W1 and the second workpiece W2 is not melted sufficiently, and at time t2, a sufficient softened portion J is not formed. In addition, the second workpiece W2 and the second chuck 203 slide against each other due to the rotation, and friction heat is generated at the sliding portion, and depending on the degree of the heat, melting occurs at the sliding portion, and the two workpieces are fused together (burned).
[0043] As shown in FIG. 3, during the friction heating process, that is, from when the workpieces W1 and W2 start to come into contact (time t1) until they stop rotating relative to each other (time t2), multiple peaks P1 to P4 are formed in the current flowing through the motors MZ1 and MZ2. When the friction heating process proceeds normally, the current flowing through the motors MZ1 and MZ2 reaches a maximum peak immediately after the workpieces W1 and W2 come into contact. As heat is generated in the sliding parts of the workpieces W1 and W2, the current gradually stabilizes, and then suddenly drops at time t2 due to the formation of a softened portion J and the halt of rotation of the first main spindle 101. 3 are abnormal current peaks that do not occur when the process proceeds normally, and each peak indicates that the workpieces W1 and W2 are rotating together, or that the second workpiece W2 is seizing up on the second chuck 203, or the like has occurred.
[0044] Fig. 4 is a time chart showing an example of changes over time in the loads applied to the first drive mechanism GZ1 and the second drive mechanism GZ2 during friction joining operation in this embodiment. In Fig. 5, the current flowing through the first motor MZ1 of the first drive mechanism GZ1 is indicated by a gray solid line, and the current flowing through the second motor MZ2 of the second drive mechanism GZ2 is indicated by a black solid line.
[0045] In this embodiment, in order to suppress the occurrence of problems such as the workpiece dragging on the second spindle 201 (back spindle) side described above, the torque of the first drive mechanism GZ1 and the second drive mechanism GZ2 are each limited in stages during the friction heating process. That is, the first current limiter 411 controls in stages the upper limit of the current flowing through the first motor MZ1 of the first drive mechanism GZ1, and the second current limiter 422 controls in stages the upper limit of the current flowing through the second motor MZ2 of the second drive mechanism GZ2.
[0046] More specifically, in this embodiment, the current limiting value IL1 during a predetermined period (t1 to ta) from the start of the frictional heating process, i.e., during the predetermined period from when the first workpiece W1 and the second workpiece W2 come into contact, is set to a value smaller than the current limiting value IL2 after the predetermined period.
[0047] In the first half period FH of the friction heating process, a large torque load is generated when the first workpiece W1 and the second workpiece W2 come into contact (time t1), and an unstable state occurs thereafter with a torque load that fluctuates widely for a while. In the second half period SH, when heating of the sliding parts has progressed, the fluctuation range of the torque load settles down to a certain extent (part SS in Fig. 5), and the sliding state becomes relatively stable until the relative rotation of the spindle is stopped. Therefore, the first friction heating period Tf is a predetermined period from the start of the first half period FH (t1 to ta), and the second half period SH is combined with the period after the predetermined period of the first half period FH to form a second friction heating period Ts. The torque limit in the second friction heating period Ts is set to be stricter than the torque limit in the second friction heating period Ts.
[0048] The current limit value IL1 (first limit value) of the motor in the first friction heating period Tf is set so that the torque load is suppressed to a level that does not cause the above-mentioned co-rotation of the workpiece. The current limit value IL1 may be set to a value similar to the peak value of the mountain of the torque fluctuation portion (SS portion) in the latter half period SH, for example. In this embodiment, the current limit value IL1 of the first motor MZ1 and the second motor MZ2 in the first friction heating period Tf is set to 15% of each maximum rated current.
[0049] The motor current limit value IL2 (second limit value) in the second friction heating period Ts is set to a value larger than the current limit value IL1 in the first friction heating period Tf so as to efficiently proceed with friction heating of the workpiece sliding portion while suppressing excessive torque load. The current limit value IL2 may be set to a value such that the peak value of the mountain of the torque load fluctuation portion (SS portion) in the latter half period SH is not limited, for example. In this embodiment, the current limit value IL2 of the first motor MZ1 and the second motor MZ2 in the second friction heating period Ts is set to 20% of the respective maximum rated currents.
[0050] Due to the motor current limitation as described above, in the first friction heating period Tf, the first drive mechanism GZ1 and the second drive mechanism GZ2 are driven with a flat torque load (a constant current with the same magnitude as the current limit value IL1) limited by the current limit value IL1. Also, in the second friction heating period Ts, in the initial period (a predetermined period from the start of the second friction heating period Ts), the first drive mechanism GZ1 and the second drive mechanism GZ2 are driven with a flat torque load (a constant current with the same magnitude as the current limit value IL2) limited by the current limit value IL2. After that, if the process is proceeding normally, the first drive mechanism GZ1 and the second drive mechanism GZ2 are driven with a torque load that is not subject to any particular limitation (a current that does not reach the same magnitude as the current limit value IL2).
[0051] The motor current limit values shown here are merely examples and are set appropriately from the viewpoint of suppressing the occurrence of the above-mentioned problems and poor connections. The current limit values of the first motor MZ1 and the second motor MZ2 may be the same value or different values.
[0052] In the initial stage of the friction heating process (first friction heating period Tf), the first workpiece W1 and the second workpiece W2 are brought into contact with each other under a torque load that is limited so as not to generate an excessive torque load, and the first workpiece W1 and the second workpiece W2 start to slide against each other. Then, at a stage (second friction heating period Ts) when the heating of the sliding parts has progressed to a certain extent, the torque limit is relaxed. That is, in the initial stage of the process, the workpieces W1 and W2 are pressed against each other under a weak torque to suppress the occurrence of unstable behavior specific to the initial stage of the process, and then, after the sliding state has stabilized, the limit on the torque load is relaxed to promote thermal bonding. This makes it possible to suppress the occurrence of the workpiece W2 on the second spindle 201 (rear spindle) side being rotated together, the occurrence of poor bonding, and the like.
[0053] In this embodiment, the motor current at the timing of switching from the friction heating process to the upset process is detected to detect whether or not droop generated in the friction heating process remains. In this embodiment, the first ammeter 410 and the second ammeter 420 as current detection means function as droop detection means. If droop remains, it is determined that some abnormality has occurred in the friction heating process, a notification is given to the user, and the subsequent process is canceled.
[0054] Fig. 5 is a time chart showing an example of a change over time in droop (the difference between the command amount for the position of the spindles and the actual movement amount of the spindles) regarding the relative positions in the Z-axis direction of the first spindle 101 and the second spindle 201 in the friction heating process, which is a detection result in the friction welding operation of this embodiment shown in Fig. 5. In Fig. 6, the droop of the first driving mechanism GZ1 is shown by a gray solid line, and the droop of the second driving mechanism GZ2 is shown by a black solid line.
[0055] In the friction heating process, the droop regarding the relative position of the first spindle 101 and the second spindle 201 in the Z-axis direction gradually accumulates due to the load generated at the sliding portion of the workpieces W1 and W2, but is resolved when the sliding portion is sufficiently softened. Therefore, as shown in FIG. 5, when the friction heating process is normally completed without any joint abnormality occurring by the control of this embodiment, the droop is finally resolved. More specifically, the droop is resolved by the time the torque fluctuation portion SS shown in FIG. 4 is reached. This droop elimination is also shown in the current fluctuation shown in FIG. 4 as a point (P5) where the current value drops in the stage before the torque fluctuation portion SS. In other words, the motor current decreases as the load state is instantly eliminated due to the sufficient softening of the joint. This behavior causes the position command amount of the spindle and the actual movement amount of the spindle to finally match.
[0056] Therefore, in this embodiment, if the droop of the first driving mechanism GZ1 and the droop of the second driving mechanism GZ2 remain above a certain threshold value at the timing (time t2) when the relative rotation of the spindles 101, 201 stops, it can be determined that the friction joining process is not functioning normally.
[0057] The flow of the friction welding process of this embodiment will be described with reference to Fig. 6. Fig. 6 is a flow diagram of the friction welding process of this embodiment. The control unit 4 mainly performs each control described below.
[0058] The control unit 4 starts the rotation of the first spindle 101 by the rotary drive mechanism (S101), and when the rotation is stabilized (S102), starts the movement of the first spindle stock 102 and the second spindle stock 202 in the Z-axis direction by the drive mechanisms GZ1 and GZ2 (S103). At this time, the control unit 4 sets the current limit value IL1 of the motors MZ1 and MZ2 of the drive mechanisms GZ1 and GZ2 to the above-mentioned first limit value. In addition, the control unit 4 drives the motors MZ1 and MZ2 by setting the control target value (first control target value) of the feed amount (movement amount in the Z-axis direction per unit time) of the first spindle stock 102 as the first feed amount (first movement amount) and setting the control target value (second control target value) of the feed amount of the second spindle stock 202 as the second feed amount (second movement amount). By driving the drive mechanisms GZ1, GZ2 and the rotary drive mechanisms, the tip surfaces of the workpieces W1, W2 held by the spindles 101, 201 are pressed against each other and slide against each other.
[0059] Here, the first feed amount and the second feed amount may be the same or different, and may be set appropriately depending on the specifications of the spindle mechanism, the type of workpiece, etc.
[0060] During the first frictional heating period Tf, the control unit 4 continues frictional heating by limiting the torque at the first limit value (S104). The end of the first frictional heating period Tf may be determined by the fact that the elapsed time from the start of the movement of the first headstock 102 and the second headstock 202 in the Z-axis direction has passed a preset end time of the first frictional heating period Tf. Alternatively, the end of the first frictional heating period Tf may be determined by the fact that the control amount (position command amount) of the movement of the first headstock 102 and the second headstock 202 in the Z-axis direction by each of the drive mechanisms GZ1 and GZ2 reaches a control amount corresponding to the end time of the first frictional heating period Tf.
[0061] When the first friction heating period Tf ends and the second friction heating period Ts begins, the control unit 4 changes the current limit values of the motors MZ1, MZ2 of the drive mechanisms GZ1, GZ2 from the first limit value to the above-mentioned second limit value (S105). At this time, the control unit 4 drives the motors MZ1, MZ2 with the control target value of the feed amount of the first headstock 102 set to the third feed amount (third movement amount) and the control target value of the feed amount of the second headstock 202 set to the fourth feed amount (fourth movement amount).
[0062] Here, the third feed amount and the fourth feed amount may be the same or different, and may be set appropriately depending on the specifications of the spindle mechanism, the type of workpiece, etc.
[0063] Also, the third feed amount may be the same as or different from the first feed amount. Typically, the third feed amount is set to an amount larger than the first feed amount, but depending on the joining conditions, it may be set to continue the same as the first feed amount or to be smaller than the first feed amount. Similarly, the fourth feed amount may be the same as or different from the second feed amount. Typically, the fourth feed amount is set to an amount larger than the second feed amount, but depending on the joining conditions, it may be set to continue the same as the second feed amount or to be smaller than the second feed amount.
[0064] During the second frictional heating period Ts, the control unit 4 continues frictional heating by limiting the torque at the second limit value (S106). When the sliding portion of the two workpieces is sufficiently softened by the frictional heat, the control unit 4 controls the rotation drive mechanism to stop the relative rotation of the two workpieces, and ends the second frictional heating period Ts (S107). The second frictional heating period Ts ends by controlling the timing of the stop of rotation of the first spindle 101 as described above. At this time, it is determined whether or not the droop at the time of the stop of rotation is within a predetermined threshold range (S108).
[0065] The determination of whether or not the droop remains when the rotation stops may be made by, for example, detecting whether or not the droop falls below a predetermined threshold value in a predetermined period before and after time t2. For example, the predetermined threshold value may be set to a value of about 2 to 3, assuming that the maximum value of the droop shown in FIG. 5 is 100. Depending on the joining conditions, the value may be set to about 5 to 10. Furthermore, monitoring for droop detection may be performed only during a predetermined period in the latter half of the friction heating process. For example, a droop confirmation timer may be started at the timing of entering the second friction heating period Ts. However, the threshold value is not limited to the above value, and the determination method is not limited to the above method.
[0066] If it is determined that the motor current when the rotation is stopped is normal (S108, YES), the control unit 4 continues the upsetting process (S109). In the upsetting process, the control unit 4 drives the drive mechanisms GZ1 and GZ2 so as to press the workpieces W1 and W2 against each other with a pressure higher than that in the friction heating process, while the rotation of the workpieces W1 and W2 is stopped.
[0067] The control unit 4 drives the motors MZ1 and MZ2 by setting the control target value of the feed amount of the first headstock 102 to a fifth feed amount (fifth movement amount) and by setting the control target value of the feed amount of the second headstock 202 to a sixth feed amount (sixth movement amount).
[0068] Here, the fifth feed amount and the sixth feed amount may be the same or different, and may be set appropriately depending on the specifications of the spindle mechanism, the type of workpiece, etc. Also, the fifth feed amount is typically set to an amount larger than the third feed amount, but may continue to be the same as the third feed amount depending on the joining conditions. Similarly, the sixth feed amount is typically set to an amount larger than the fourth feed amount, but may continue to be the same as the fourth feed amount depending on the joining conditions.
[0069] On the other hand, if it is determined that the droop when rotation stops is not below the threshold value (S108, NO), the control unit 4 notifies the user that some kind of abnormality has occurred, such as by issuing an alert, that there is some kind of poor bonding in the workpieces W1 and W2 or some kind of malfunction in the apparatus (S110).
[0070] As described above, according to the control of the friction welding process of this embodiment, the sliding contact between the workpieces is started with a torque load suppressed to a level where the workpieces do not rotate together as described above, and the torque limit is controlled to be relaxed after the sliding state is stabilized. This makes it possible to effectively suppress the occurrence of defects in friction welding, particularly defects at the beginning of the friction heating process. In addition, by checking whether or not droop remains at the end of the friction heating process, it is possible to detect defects that have occurred and cannot be prevented by limiting the torque load. In other words, it is possible to accurately determine whether the welding state is good or bad.
[0071] In this embodiment, the description has been given on the premise that the device configuration is such that a machine tool, which is a cutting device, is converted into a friction welding device. However, the present invention may also be applied to a dedicated friction welding device. [Explanation of symbols]
[0072] Reference Signs List 1...machine tool, 100...first spindle mechanism, 101...first spindle, 102...first spindle stock, 200...second spindle mechanism, 201...second spindle, 202...second spindle stock, GZ1...first drive mechanism, GZ2...second drive mechanism, MZ1...first motor, MZ2...second motor, 4...control unit, 410...first ammeter, 420...second ammeter, 411...first current limiter, 421...second current limiter, W1...first workpiece, W2...second workpiece
Claims
1. A first spindle that grips a first workpiece; a second spindle that holds a second workpiece so as to face the first workpiece in the axial direction; a first drive mechanism including a first drive source and configured to move the first spindle in the axial direction by a drive force of the first drive source; a second drive mechanism including a second drive source and configured to move the second spindle in the axial direction by a drive force of the second drive source; a rotation drive mechanism that relatively rotates the first workpiece and the second workpiece about a rotation axis along the axial direction; a control means for controlling the first drive mechanism, the second drive mechanism, and the rotation drive mechanism so as to bring the first workpiece and the second workpiece into contact with each other while rotating relative to each other, thereby joining the first workpiece and the second workpiece; a current limiting unit that limits a current flowing through the first drive source and the second drive source to a predetermined limit value or less; In a friction joining apparatus comprising: the current limiting means limits the current flowing through the first driving source and the second driving source during a first frictional heating period, which is a predetermined period from immediately after the first workpiece and the second workpiece come into contact with each other, to a first limit value or less that is smaller than a second limit value for limiting the current flowing through the first driving source and the second driving source during a second frictional heating period after the first frictional heating period has elapsed.
2. The control means In the first frictional heating period, the first drive source is controlled by setting a first control target value of a movement amount per unit time of the first workpiece as a first movement amount, and the second drive source is controlled by setting a second control target value of a movement amount per unit time of the second workpiece as a second movement amount, 2. The friction welding device according to claim 1, wherein, in the second frictional heating period, the first drive source is controlled with the first control target value being a third movement amount, and the second drive source is controlled with the second control target value being a fourth movement amount.
3. The third movement amount is equal to or greater than the first movement amount, 3. The friction welding device according to claim 2, wherein the fourth movement amount is the same as or greater than the second movement amount.
4. The control means Controlling the rotation drive mechanism to stop the relative rotation of the first workpiece and the second workpiece to end the second frictional heating period; 3. The friction welding device according to claim 2, characterized in that, in the welding process after the end of the second frictional heating period, the first drive source is controlled with the first control target value as a fifth movement amount, and the second drive source is controlled with the second control target value as a sixth movement amount.
5. a droop detection means for detecting a droop of the first driving source and a droop of the second driving source, The friction welding device according to claim 4, characterized in that if the droop of the first driving source and the droop of the second driving source exceed predetermined threshold values when the relative rotation is stopped, the control means stops the first driving mechanism and the second driving mechanism and does not perform the welding process.
6. 2. The friction joining device according to claim 1, wherein the rotation drive mechanism rotates the first workpiece but does not rotate the second workpiece.
7. 2. The friction joining device according to claim 1, wherein the current flowing through the first driving source and the second driving source is constant and equal to the first limit value during the first frictional heating period.
8. 2. The friction welding device according to claim 1, wherein the current flowing through the first driving source and the second driving source is constant at a magnitude equal to the second limit value for a predetermined period from the start of the second friction heating period, and does not reach a magnitude equal to the second limit value after the predetermined period.
Citation Information
Patent Citations
Friction welding machine and control method thereof
JP1991124384A
Friction welding method and friction welding machine
JP1995185843A
Friction welding method
JP1997141454A
Friction welding method
JP2000202648A
Aluminum alloy propeller shaft and friction pressure welding method of the same