Carbon dioxide adsorbent, module for adsorption, separation, and recovery of carbon dioxide and method for direct air capture

The carbon dioxide adsorbent with a laminated structure on a porous sheet addresses high energy costs and inefficiencies by reducing pressure loss and increasing surface area for effective adsorption and recovery.

JP2024150184APending Publication Date: 2024-10-23ASAHI KASEI KOGYO KABUSHIKI KAISHA

Patent Information

Application Number
JP2023063467
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-10
Publication Date
2024-10-23

AI Technical Summary

Technical Problem

Existing carbon dioxide capture technologies face high energy costs, large pressure losses, and inefficient adsorption due to small specific surface areas and gas drift within the apparatus.

Method used

A carbon dioxide adsorbent comprising a diffusible adsorption compound supported on a porous sheet made of fibers, with a laminated structure including spacers to enhance contact opportunities and reduce pressure loss.

Benefits of technology

The solution provides a carbon dioxide adsorbent with a small pressure loss and large specific surface area, enabling efficient adsorption and recovery, particularly suitable for direct air capture.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024150184000001_ABST
    Figure 2024150184000001_ABST
Patent Text Reader

Abstract

To provide a carbon dioxide adsorbent characterized by a small pressure loss during CO2 adsorption and a carrier with a high specific surface area, a module for adsorption, separation, and recovery of carbon dioxide and a method for direct air capture.SOLUTION: A carbon dioxide adsorbent for adsorption, separation, and recovery of carbon dioxide includes: a carbon dioxide diffusive adsorption compound; and at least one layer of a porous sheet composed of fibers as the sheet substrate, wherein the diffusive adsorption compound is carried on the fiber surface of the porous sheet.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a carbon dioxide adsorbent, a module for adsorption, separation and capture of carbon dioxide, and a method for direct air capture. [Background technology]

[0002] Gas separation by adsorption has many applications in industry, for example in the removal of specific components from a gas stream, where the desired product is either the component separated from the stream, the removed stream, or both. An important application is, for example, the capture of carbon dioxide (CO2) from gas streams such as flue gases, exhaust gases, industrial waste gases, or atmospheric air.

[0003] For example, Patent Document 1 discloses a carbon dioxide absorbent that reversibly adsorbs carbon dioxide, such as process gases discharged from combustion equipment such as boilers, and that is formed by carrying an amine compound on porous particles in which hydrophilic fibers and porous powder are combined with a hydrophilic binder. Furthermore, for example, Patent Document 5 discloses a CO2 gas separation membrane module for a process of separating CO2 from synthetic gas, natural gas, exhaust gas, etc. synthesized in large-scale plants for hydrogen production, urea production, etc., which is characterized by including a spiral element having a structure in which a laminate including a CO2 gas separation membrane, a supply-side flow path material which serves as a flow path for the gas components to be supplied, and a permeate-side flow path material which serves as a flow path for the gas components that have permeated the CO2 gas separation membrane is wound around the outer periphery of a hollow gas collection pipe having a plurality of holes formed in the wall surface. Incidentally, Patent Document 5 discloses a CO2 gas separation membrane, not a carbon dioxide adsorbent for a module for adsorption, separation and capture of carbon dioxide.

[0004] As part of measures to combat climate change, the goal is to achieve net-zero carbon neutrality by 2050, but negative emission projects and offsets are needed to make up for any shortfall in emissions reductions. Direct air capture (DAC), a method of capturing CO2 directly from the atmosphere, is attracting attention as a promising candidate for negative emissions businesses.

[0005] For example, Patent Document 2 discloses a method for separating gaseous carbon dioxide from air or flue gas by cyclic adsorption / desorption using amine-functionalized cellulose as an adsorbent for adsorbing gaseous carbon dioxide.

[0006] For example, Patent Document 3 discloses a porous adsorption structure capable of reversible adsorption and desorption cycles for capturing CO2 from a gas mixture, The structure includes a support matrix of surface-modified cellulose nanofibers; The surface-modified cellulose nanofibers are covered with a coupling agent that is covalently bonded to the surface. The support matrix is ​​characterized in that it is a woven fabric of nanofibers having a porosity of at least 20%; The coupling agent is disclosed to include at least one monoalkyldialkoxy-aminosilane. Furthermore, for example, Patent Document 3 discloses a mat-like adsorptive structure made of cellulose nanofibers.

[0007] For example, US Pat. No. 5,399,633 discloses a method of applying a coating of an adsorbent, such as a gas, such as carbon dioxide, onto a substrate, a carrier, and / or a substrate coated with a carrier. In addition, Patent Document 4 describes that the adsorbent is selected from the group consisting of amines, amides including melamine, amine-containing polymers, and combinations thereof, the substrate is a woven or non-woven plastic or cellulosic fiber; The support is disclosed to be alumina, silica, silica alumina, titania, zirconia, carbon, zeolite, metal organic framework (MOF), or combinations thereof. As described above, Patent Documents 3 and 4 disclose the use of a specific nonwoven fabric as a substrate for a CO2 adsorbent, but do not disclose a module for adsorbing, separating and capturing carbon dioxide that takes into account pressure loss, or a nonwoven fabric suitable for such a module. Furthermore, for example, Patent Document 5 discloses a CO2 gas separation membrane that utilizes a facilitated transport mechanism, but the CO2 gas separation membrane is not effective for recovering CO2 from the atmosphere, which has a low CO2 gas concentration. [Prior art documents] [Patent documents]

[0008] [Patent Document 1] JP 2018-187574 A [Patent Document 2] Special Publication No. 2017-528318 [Patent Document 3] International Publication No. 2012 / 168346 [Patent Document 4] Special Publication No. 2014-533195 [Patent Document 5] International Publication No. 2016 / 024523 Summary of the Invention [Problem to be solved by the invention]

[0009] The challenge with DAC is the energy cost. To reduce the energy cost, it is necessary to reduce the power required to adsorb CO2 onto the adsorbent and to lower the temperature required to desorb the CO2 adsorbed onto the adsorbent. To reduce the power required for CO2 adsorption, it is necessary to adsorb the CO2-containing gas onto the adsorbent using as little power as possible, in other words, to minimize the pressure loss during adsorption. Furthermore, in order to reduce the power consumed during CO2 adsorption, it is necessary to load as much CO2 adsorbent as possible onto the carrier, in other words, to make the specific surface area of ​​the carrier as large as possible. Furthermore, in order to increase the efficiency of CO2 adsorption, it is necessary to maximize the opportunity for the gas to come into contact with the CO2 adsorbent, for example by suppressing drift of the gas to be treated within the device and reducing dead space. For example, Patent Document 1 discloses a carbon dioxide absorbent in which an amine compound is supported on porous particles. However, when the absorbent has a particulate shape, there are problems such as a large pressure loss, a small specific surface area, and the formation of drift and dead spaces within the device.

[0010] The present invention aims to provide a carbon dioxide adsorbent that has a small pressure loss during CO2 adsorption and a large specific surface area of ​​the carrier, as well as an efficient carbon dioxide adsorption, separation and capture module and direct air capture method. [Means for solving the problem]

[0011] The gist of the present invention is as follows.

[0012] <<Aspect 1>> A carbon dioxide adsorbent for adsorbing, separating and capturing carbon dioxide, comprising a diffusible adsorption compound for carbon dioxide, and at least one layer of a porous sheet comprising a fiber-based sheet substrate and the diffusible adsorption compound supported on the fiber surface of the porous sheet.

[0013] <<Aspect 2>> The porous sheet made of the fibers has a fiber diameter of 2 nm to 100 μm and a specific surface area of ​​0.1 m 2 / g~100m 2 / g, thickness 0.05mm~5mm, and basis weight 0.1g / m 2 ~1000g / m 2 2. The carbon dioxide adsorbing material according to claim 1, wherein the carbon dioxide adsorbing material is a nonwoven fabric.

[0014] <<Aspect 3>> 2. The carbon dioxide adsorbent of claim 1, further comprising porous particles on the porous sheet carrying a diffusible adsorbent compound for carbon dioxide.

[0015] <<Aspect 4>> 3. The carbon dioxide adsorbent according to claim 2, further comprising porous particles on the porous sheet, the porous particles carrying a diffusible adsorbent compound for carbon dioxide.

[0016] <<Aspect 5>> The carbon dioxide adsorbent according to any one of aspects 1 to 4, wherein the diffusible adsorbent compound is an amine compound, and the loading density of amino groups contained in the amine compound relative to unit mass of the carbon dioxide adsorbent is equal to or greater than 0.01 mmol / g and equal to or less than 100 mmol / g.

[0017] <<Aspect 6>> A module for adsorbing, separating and capturing carbon dioxide, having a laminated structure in which at least one layer of the carbon dioxide adsorbing material according to any one of embodiments 1 to 4 and at least one layer of a spacer are laminated.

[0018] <<Aspect 7>> A carbon dioxide adsorption, separation and capture module as described in aspect 6, wherein the spacer is a woven fabric or molded body having a height difference of 1 μm or more and 1 mm or less in the thickness direction and an opening rate of 20% or more and 90% or less.

[0019] <<Aspect 8>> 7. The carbon dioxide adsorption, separation and capture module according to aspect 6, wherein a ratio of the carbon dioxide adsorbent layer / spacer layer in the laminate structure in the thickness direction is 0.1 or more and 20 or less.

[0020] <<Aspect 9>> 9. The carbon dioxide adsorption, separation and capture module according to claim 8, wherein the laminated structure is a structure spirally wound around a tube.

[0021] <<Aspect 10>> A module for adsorbing, separating and capturing carbon dioxide, comprising the carbon dioxide adsorbent according to any one of aspects 1 to 4, the surface of which is processed to have projections and recesses with a height difference of 3 μm or more, and which has a laminated structure in which these are stacked.

[0022] <<Aspect 11>> 11. The carbon dioxide adsorption, separation and capture module according to claim 10, wherein the laminate structure is a structure spirally wound around a tube.

[0023] <<Aspect 12>> The process is as follows: An adsorption step of adsorbing carbon dioxide onto a carbon dioxide adsorbent in the carbon dioxide adsorption, separation and capture module according to embodiment 6; and A desorption step in which the temperature and pressure are changed to desorb carbon dioxide. A direct air capture (DAC) method for directly capturing carbon dioxide from the atmosphere, comprising:

[0024] <<Aspect 13>> The process is as follows: An adsorption step of adsorbing carbon dioxide onto a carbon dioxide adsorbent in the carbon dioxide adsorption, separation and capture module according to embodiment 10; and A desorption step in which the temperature and pressure are changed to desorb carbon dioxide. A direct air capture (DAC) method for directly capturing carbon dioxide from the atmosphere, comprising: Effect of the Invention

[0025] According to the present invention, there are provided a carbon dioxide adsorbent having a small pressure loss during CO2 adsorption and a large specific surface area of ​​the carrier, a module for adsorption, separation and capture of carbon dioxide, and a direct air capture method. In addition, according to one aspect of the present invention, since the carrier is in the form of a sheet rather than a particle, there are many opportunities for contact with air, and a large specific surface area can be obtained. [Brief description of the drawings]

[0026] [Figure 1] FIG. 1 shows a conceptual diagram of the carbon dioxide adsorbing material of this embodiment. [Diagram 2] FIG. 2 shows an SEM image (magnification: 50 times) of the carbon dioxide adsorbing material of this embodiment. [Diagram 3] FIG. 3 shows a schematic diagram of a spiral-structured module according to one embodiment of the present invention. [Figure 4]Figure 4 shows a system diagram of DAC (Direct Air Capture) technology. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0027] Hereinafter, the embodiment of the present invention (hereinafter, also referred to as the present embodiment) will be described in detail. Note that the present embodiment is not limited to the embodiment described below, and can be used in various modifications within the scope indicated.

[0028] <Carbon dioxide adsorbent> The carbon dioxide adsorbent may be any material capable of adsorbing carbon dioxide (CO2). It is preferable to adsorb carbon dioxide from process gases such as synthetic gas, natural gas, and exhaust gas, or from the atmosphere or a mixture thereof, and it is particularly preferable to adsorb carbon dioxide from the atmosphere. Direct Air Capture (DAC) technology is a technology for capturing carbon dioxide from the atmosphere. There are two types of DAC: solid adsorption (Solid DAC), in which the carbon dioxide is adsorbed by a solid, and liquid adsorption (Liquid DAC), in which the carbon dioxide is adsorbed by a solution. The carbon dioxide adsorbent of this embodiment is preferably a solid adsorption type (Solid DAC).

[0029] In one aspect, the carbon dioxide adsorbent according to this embodiment includes a diffusible adsorbent compound for carbon dioxide and at least one layer of a porous sheet. In one aspect, the carbon dioxide adsorbent according to this embodiment may further include porous inorganic particles.

[0030] (Diffusive adsorbent of carbon dioxide) In one embodiment, the carbon dioxide diffusible adsorption compound (hereinafter referred to as the diffusible adsorption compound) used in the carbon dioxide adsorbent of this embodiment is supported on the fiber surface of a porous sheet composed of fibers as a sheet substrate. In the present disclosure, the term "supported" refers to a substance being immobilized on a carrier by adhesion, electrostatic adsorption, reaction, or the like. In the present disclosure, the term "support" refers to a substance that serves as a base for a certain substance, and in the present disclosure, it is a "porous sheet." In one aspect, the diffusible, adsorptive compound of the present embodiments is an amine-based compound.

[0031] (Amine compounds) The amine compound of the present embodiment may be any compound capable of reversibly desorbing carbon dioxide, that is, any compound capable of adsorbing and desorbing carbon dioxide by an amino group contained in the amine compound. Examples of the amine compound of the present embodiment include N,N'-bis(3-aminopropyl)ethylenediamine, diethylenediamine, diethylenetriamine, tetraethylenepentamine, pentaethylenehexamine, polyethyleneimine (PEI), polypropyleneimine, polyallylamine, monoethanolamine, diethanolamine, triethanolamine, tris(2-aminoethyl)amine, isophoronediamine, 2-aminoethylaminopropyldimethoxysilane (AEAPDMS), 2-aminoethylaminopropyltrimethoxysilane, 3-aminopropyldimethoxysilane, 3-aminopropyltrimethoxysilane, lysine, and aziridine. These amine compounds may be used alone or in combination of two or more kinds.

[0032] The amine compound may be supported on the porous sheet by reacting the porous sheet with an amino alkoxysilane such as 2-aminoethylaminopropyldimethoxysilane, 2-aminoethylaminopropyltrimethoxysilane, 3-aminopropyldimethoxysilane, or 3-aminopropyltrimethoxysilane. Furthermore, the amine compound may be supported on the porous sheet by graft polymerization of lysine, aziridine, or the like.

[0033] The diffusible adsorption compound of this embodiment is an amine-based compound, and the loading density of the amino groups contained in the amine-based compound relative to unit mass of the carbon dioxide adsorbent is preferably 0.01 mmol / g or more and 100 mmol / g or less, and more preferably 5 mmol / g or more and 30 mmol / g or less.

[0034] The loading density of the amino groups contained in the amine compound per unit mass of the carbon dioxide adsorbent can be measured by a known method. For example, when the porous sheet according to this embodiment does not contain nitrogen, the amount of nitrogen contained in the porous sheet carrying the amino group contained in the amine compound is measured by the Kjeldahl method or the combustion method. Next, a calibration curve is drawn between the absorbance of the peak assigned to the amino group determined using an infrared spectrometer and the amount of nitrogen contained in the porous sheet determined by the Kjeldahl method or the combustion method. The content of amino groups contained in the amine compound is determined using the calibration curve and an infrared spectrometer, and then divided by the weight of the porous sheet supporting the amino groups, thereby making it possible to determine the supporting density of the amino groups contained in the amine compound per unit mass of the carbon dioxide adsorbent. For example, when the porous sheet according to this embodiment contains nitrogen, a porous sheet carrying an amino group contained in an amine compound and a porous sheet not carrying the amino group (porous sheet alone) are each subjected to the Kjeldahl method or the combustion method to determine the amount of nitrogen contained in the porous sheet alone and in the porous sheet carrying an amino group contained in an amine compound. The amount of nitrogen in the amino groups contained in the amine compound is determined by subtracting the amount of nitrogen contained in the porous sheet alone from the amount of nitrogen contained in the porous sheet carrying the amino groups contained in the amine compound. Next, in the same manner as in the case where the porous sheet does not contain nitrogen, a calibration curve is drawn between the absorbance of the peak assigned to the amino group determined using an infrared spectrometer and the amount of nitrogen contained in the porous sheet carrying the amino group contained in the amine compound determined by the Kjeldahl method or the combustion method. The content of amino groups contained in the amine compound is determined using the calibration curve and an infrared spectrometer, and then divided by the weight of the porous sheet supporting the amino groups, thereby making it possible to determine the supporting density of the amino groups contained in the amine compound per unit mass of the carbon dioxide adsorbent.

[0035] (Porous sheet) In one aspect, the porous sheet according to this embodiment is composed of fibers as a sheet substrate. In the present disclosure, "porosity" refers to a property that is exhibited by having voids between the fibers that are the sheet substrate. In one aspect, the porous sheet according to the present embodiment is formed by supporting a diffusible adsorption compound for carbon dioxide in the voids between the fibers. In addition, since the porous sheet according to this embodiment has a sheet-like shape, it has many opportunities for contact with air, resulting in a large specific surface area, and the pressure loss during CO2 adsorption is small, making it preferable as a carrier for a diffusible adsorption compound. Furthermore, if the shape is sheet-like, efficient contact with the gas to be treated can be ensured by carrying carbon dioxide adsorbent on both sides when stacking with a spacer.

[0036] As the fibers, various types of hydrophobic thermoplastic resin fibers and various types of hydrophilic fibers can be used. Examples of hydrophobic synthetic resin fibers include polyethylene, polypropylene, and polyester. Examples of hydrophilic fibers include cellulose-based fibers made of cellulose, cellulose derivatives and regenerated cellulose, polyvinyl alcohol-based fibers, polyamide-based fibers, etc., and hydrophilic fibers are preferred. Examples of cellulose include wood pulp, waste paper pulp, cotton, and hemp. Examples of the cellulose derivatives include cellulose acetate and carboxymethyl cellulose. Examples of regenerated cellulose include cupra, rayon, and lyocell. Examples of polyvinyl alcohol-based fibers include polyvinyl alcohol and polyvinyl formal. Examples of polyamide fibers include nylon (in one embodiment, 6-nylon, 6,6-nylon).

[0037] The porous sheet according to the present embodiment is preferably a nonwoven fabric, and more preferably a nonwoven fabric that satisfies the following specific requirements. The fiber diameter of the porous sheet according to this embodiment is preferably from 2 nm to 100 μm, and more preferably from 2 nm to 20 μm. The specific surface area of ​​the porous sheet according to this embodiment is 0.1 m 2 / g~100m 2 / g is preferred, and 1.0m 2 / g~100m 2 / g is more preferred. The thickness of the porous sheet according to this embodiment is preferably 0.05 mm to 5 mm, and more preferably 0.1 mm to 1.0 mm. The basis weight of the porous sheet according to this embodiment is 0.1 g / m 2 ~1000g / m 2 is preferred, and 10 g / m 2 ~150g / m 2 is more preferred. The porous sheet according to this embodiment is preferable when the fiber diameter and the like are within the above-mentioned specific ranges, since it has excellent carbon dioxide adsorption properties.

[0038] The fiber diameter of the porous sheet is measured as follows. The porous sheet was observed at a magnification of 10,000 times using a scanning electron microscope, JSM-6380 manufactured by JEOL Ltd., and 50 fibers were randomly selected, and the average value of the measurements was taken as the fiber diameter.

[0039] In this disclosure, specific surface area refers to BET specific surface area. The specific surface area of ​​the porous sheet is measured as follows. The specific surface area was measured using a specific surface area and pore distribution analyzer (Nova-4200e, Quantachrome Instruments). 0.2 g of the dry porous sheet was dried under vacuum at 120°C for 2 hours, and the amount of nitrogen gas adsorbed at the boiling point of liquid nitrogen was measured at five points in the range of relative vapor pressure (P / P0) between 0.05 and 0.2 (multipoint method). The BET specific surface area (m 2 / g) was calculated.

[0040] The thickness of the porous sheet is measured as follows. The porous sheet in a dry state was measured at a load of 1.96 kPa in a thickness test conforming to JIS-L 1096. The measurement was performed 20 times, and the average value was taken as the thickness (mm) of the porous sheet.

[0041] The basis weight of the porous sheet is measured as follows. Area 0.05m 2 The porous sheet is dried at 105°C until it reaches a constant mass, and then left in a temperature-controlled room at 20°C and 65% RH for 16 hours or more. The mass is then measured, and the weight of the porous sheet is then measured. 2 The measurement was carried out five times, and the average value was used as the basis weight (g / m2) of the porous sheet. 2 ) was decided.

[0042] The specific surface area of ​​the porous sheet can be increased by reducing the fiber diameter of the porous sheet, but it is essential to optimize the sheet while taking into consideration its mechanical properties. Furthermore, the thickness and basis weight of the porous sheet are important in order to ensure a sufficient contact area between the carbon dioxide adsorbent and the gas to be treated when the porous sheet is laminated with a spacer.

[0043] (porous particles) In one aspect, the carbon dioxide adsorbing material according to this embodiment may further include porous particles on the porous sheet. The porous particles can be supported on the porous sheet by a known method. For example, a porous particle dispersion liquid in which the porous particles are set to an arbitrary concentration in an aqueous solution of a diffusible adsorption compound for carbon dioxide is applied to a porous sheet by spraying or dipping, and the porous sheet is then dried at room temperature, whereby the porous particles can be supported on the porous sheet. In one embodiment, a diffusible adsorption compound for carbon dioxide is supported on the porous particles according to this embodiment on a porous sheet. In one embodiment, the fiber is made of fibers, has a fiber diameter of 2 nm to 100 μm, and has a specific surface area of ​​0.1 m 2 / g~100m 2 / g, thickness 0.05mm~5mm, and basis weight 0.1g / m 2 ~1000g / m 2 A diffusible adsorption compound for carbon dioxide is supported on the porous particles according to this embodiment on a porous sheet which is a nonwoven fabric. The porous particles according to this embodiment can be selected from alumina, silica, silica alumina, titania, zirconia, magnesia, activated carbon, zeolite, metal organic framework (MOF), or a combination thereof.

[0044] The average particle size of the porous particles is preferably from 0.1 μm to 3 mm, more preferably from 1 μm to 1 mm, and even more preferably from 3 μm to 500 μm. From the viewpoint of suppressing an increase in pressure loss, the average particle size of the porous particles is preferably 0.1 μm or more, and from the viewpoint of increasing the volumetric efficiency in the adsorption module, the average particle size of the porous particles is preferably 3 mm or less. The average particle size of the porous particles was measured as follows. The particles were observed at a magnification of 2000 to 10000 times using a scanning electron microscope, JSM-6380 manufactured by JEOL Ltd., and 50 particles were randomly selected, and the average value of the measurements was taken as the average particle size.

[0045] Porous particles have a specific surface area of ​​10m 2 / g or more 1000m 2 / g or less is preferable. More preferably, it is 50m 2 / g or more, 800m 2 / g or less, more preferably 100m 2 / g or more, 800m 2 / g or less. The specific surface area of ​​the porous particles is 10m 2 / g or more is preferable because the amount of carbon dioxide adsorbed per unit mass of the carbon dioxide adsorbent can be increased when a diffusible adsorbent compound for carbon dioxide is supported on the carbon dioxide adsorbent. 2 / g or less is preferable because the durability of the carbon dioxide adsorbent is improved when the carbon dioxide adsorption and desorption cycle is repeated. The pore volume and specific surface area of ​​the porous particles were measured using a specific surface area and pore distribution analyzer (Nova-4200e, Quantachrome Instruments) by drying 0.2 g of dry porous particles at 120°C for 2 hours under vacuum, measuring the amount of nitrogen gas adsorption at the boiling point of liquid nitrogen at five points in the range of relative vapor pressure (P / P0) between 0.05 and 0.2 (multipoint method), and then calculating the pore volume (ml / g) and BET specific surface area (m 2 / g) was calculated.

[0046] The pore volume of the porous particles is preferably 0.1 ml / g or more and 1.5 ml / g or less, and more preferably 0.3 ml / g or more and 1.3 ml / g or less. It is preferable that the pore volume of the porous particles is 0.1 ml / g or more, since this increases the amount of carbon dioxide adsorption per unit mass of the carbon dioxide adsorbent when a diffusible adsorption compound for carbon dioxide is supported, and it is preferable that the pore volume is 1.5 ml / g or less, since this improves the durability of the carbon dioxide adsorbent when the carbon dioxide adsorption and desorption cycle is repeated.

[0047] The amount of the porous particles supported on the porous sheet is preferably 0.01 g / g or more and 2 g / g or less, and more preferably 0.02 g / g or more and 1.5 g / g or less. When the amount of porous particles supported on the porous sheet is 0.01 g / g or more, the amount of carbon dioxide adsorption can be increased, which is preferable, and when the amount is 2 g / g or less, the pressure loss during the carbon dioxide adsorption process can be reduced, which is preferable. The amount of porous particles supported on the porous sheet is determined by cutting a porous sheet not supporting porous particles and a porous sheet supporting porous particles into 10 cm squares and measuring the weight of each. The amount of porous particles supported on the porous sheet can be calculated by multiplying the increase in weight of the porous particles by the concentration of the porous particles in the porous particle dispersion.

[0048] [Method of manufacturing carbon dioxide absorbent] The method for producing the carbon dioxide absorbent according to this embodiment includes a step of producing a porous sheet as a sheet substrate, and a step of causing the produced porous sheet to support a diffusible adsorption compound.

[0049] -Process for producing porous sheets In the process of producing a porous sheet as the sheet substrate, a known method can be used depending on the material, such as polypropylene, polyester, nylon, or cellulose. For example, when a nonwoven type porous sheet is produced using fibers such as thermoplastic polypropylene, polyester, nylon, etc., it can be obtained by various known methods such as a spunbond method or a meltblowing method. For example, in the spunbonding method, the raw resin is melted in an extruder and continuously spun, and then the resin is spread and deposited on a net to form a web, which is then bonded onto a sheet to obtain the porous sheet of this embodiment. For example, in the melt-blowing method, when the raw resin is melted in an extruder and continuously spun into fibers, the fibers are thinned by high-temperature air jetted from around the spinning nozzle and accumulated on a sheet. In the melt-blowing method, the fiber diameter can be thinned by stretching the fibers with air.

[0050] When a short fiber sheet is obtained, the porous sheet of this embodiment can be obtained by a dry method or a wet method. The dry method is a method of producing a porous sheet by arranging short fiber sheets of about 15 to 100 mm in a fixed direction or randomly using a machine called a card or an air flow called an airlay. The wet method uses a sheet of short fibers such as paper or glass, and the short fibers are dispersed in water or the like, and the dispersion is then piled up onto a mesh net to form a fleece, thereby obtaining the porous sheet of this embodiment.

[0051] A method for producing a porous sheet of long fibers using cellulose fibers includes, for example, dissolving cellulose in a cuprammonium solution and coagulating the cellulose by deammoniating, thereby obtaining the porous sheet of this embodiment. For example, methods include tension spinning, in which a filament is extruded from a nozzle into warm water in a funnel, air gap spinning, in which the filament is extruded into the air, and electrospinning, in which an electric charge is applied to the raw solution to form fine fibers.

[0052] As a specific example of flow-down tension spinning, a stock solution in which cotton linters, from which foreign matter has been removed and the degree of polymerization has been adjusted, is dissolved in a cuprammonium solution is extruded from a spinneret (spinneret) having fine holes (stock solution discharge holes) and dropped into a funnel together with water, where the stock solution is solidified by deammoniating to obtain fibers. The obtained fibers are stretched and thrown onto a net to spin a web. In this process, the net is vibrated in a direction perpendicular to the direction of travel while it is moving, so that the fibers falling onto the net form a Sine curve. A web spun under the same conditions is further layered on top of the single layer of web obtained, and finally a porous sheet consisting of a multi-layered continuous cellulose fiber web is obtained. The obtained continuous cellulose long fiber web is regenerated with dilute sulfuric acid, washed with water, and then the obtained regenerated continuous cellulose long fiber web is placed on a sheet with holes to entangle the fibers using a high-pressure water flow, followed by drying with hot air to obtain a porous sheet composed of regenerated continuous cellulose long fibers.

[0053] The draw ratio can be adjusted as desired by changing the shape of the spinning funnel and the amount of spinning water flowing down through it. By adjusting the draw ratio, it is possible to change the fiber diameter of the porous sheet. In addition, the thickness of the porous sheet can be adjusted as desired by changing the moving speed of the net, and by adjusting the thickness, the basis weight of the porous sheet can be changed. In addition, by controlling the vibration width of the net, it is possible to control the fiber arrangement direction and thereby control the strength, elongation, etc. of the porous sheet.

[0054] A process of supporting a diffusible adsorbent on a porous sheet The step of supporting the diffusible adsorptive compound on the porous sheet can be carried out by a known method. For example, the diffusible adsorption compound can be supported on the porous sheet by a spraying method in which the stock solution of the diffusible adsorption compound, either neat or dissolved in water or a solvent, is continuously sprayed onto the porous sheet and then dried, or by a dipping method in which the porous sheet is continuously dipped into a container containing a solution, the amount of dip is adjusted to a predetermined amount with a blade or the like, and then dried. When the diffusible adsorption compound is dissolved in water or a solvent, a third component such as polyethylene glycol, polypropylene glycol, glycerin, or a quaternary ammonium salt may be mixed therein. Furthermore, when a diffusible adsorptive compound is supported on the porous sheet according to this embodiment, the diffusible adsorptive compound may be supported on a porous sheet that already supports porous particles. Alternatively, the diffusible adsorbent compound may be preloaded onto the porous particles. Alternatively, the porous particles may be dispersed in a solution in which the diffusible adsorption compound is dissolved in water or a solvent, and the dispersion may be sprayed or dipped to simultaneously support the porous particles and the diffusible adsorption compound on the porous sheet. In this case, a binder such as an adhesive may be used to bond the porous particles to the porous sheet.

[0055] <module> In one aspect, the module according to this embodiment has at least one layer of carbon dioxide adsorbent material. The carbon dioxide adsorbing material according to this embodiment included in the module according to this embodiment is the same as described above. In one embodiment, the module according to this embodiment has at least one spacer layer. In one aspect, the module according to this embodiment has a laminated structure in which at least one layer of carbon dioxide adsorbing material and at least one layer of spacer are laminated.

[0056] (Spacer) The spacer serves as a flow path through which air flows in order to allow the carbon dioxide adsorbent to adsorb carbon dioxide in the air. In one embodiment, the spacer is preferably a woven fabric or a molded body. In one embodiment, from the viewpoint of breathability, the spacer is more preferably a woven fabric or molded article having a height difference between the warp and weft threads of 1 μm or more and 1 mm or less in the thickness direction and an opening rate of 20% or more and 90% or less. In one aspect, the module according to this embodiment preferably has a spacer that is a woven fabric or molded body having a height difference between the warp and weft threads of 1 μm or more and 1 mm or less in the thickness direction and an opening rate of 20% or more and 90% or less.

[0057] (Laminated structure) In one aspect, the laminate structure refers to a structure in which at least one layer of the carbon dioxide adsorbent according to this embodiment (in one aspect, a carbon dioxide adsorbent layer) and at least one spacer layer (in one aspect, a spacer layer) are laminated. In one embodiment, the laminate structure is preferably a structure in which 1 to 5 layers of the carbon dioxide adsorbent according to this embodiment (in one embodiment, carbon dioxide adsorbent layers) and at least one spacer layer (in one embodiment, spacer layer) are laminated. In one embodiment, the laminate structure may include a carbon dioxide adsorbent layer having a surface textured to have a height difference of 3 μm or more. In the case of a laminate structure having a carbon dioxide adsorbent layer having a textured surface, a spacer layer may or may not be included. The unevenness processing can be carried out by a conventional method such as embossing.

[0058] By having a laminated structure, the module of this embodiment can be suitably used for adsorbing carbon dioxide in the atmosphere. In one embodiment, the ratio of the carbon dioxide adsorbent layer to the spacer layer in the thickness direction is preferably 0.1 or more and 20 or less, and more preferably 1 or more and 20 or less. From the viewpoint of carbon dioxide adsorption efficiency, it is preferably 0.1 or more, and from the viewpoint of pressure loss in the module, it is preferably 20 or less.

[0059] In one embodiment, the laminate structure is a spiral wound structure on a tube. The form of a module having such a laminated structure is a spiral type in which a laminated structure in which a carbon dioxide adsorbent layer and a spacer layer are laminated is wound around the outer periphery of a hollow gas collection pipe having a plurality of holes formed in the wall surface. The module using the carbon dioxide adsorbing material according to this embodiment may be any of a spiral type, a cylindrical type, a hollow fiber type, a pleated type, and a plate and frame type, with the spiral type or the pleated type being preferred.

[0060] [Module manufacturing method] The method for manufacturing the module according to this embodiment includes the steps of preparing a carbon dioxide adsorbing material, preparing a spacer, and laminating the carbon dioxide adsorbing material and the spacer.

[0061] The process for preparing the carbon dioxide adsorbent is the same as that described above.

[0062] -Spacer stacking process The spacer may be made of any of various known woven fabrics or molded articles. Specifically, various woven fabrics or molded articles can be used which are made by plain weaving, twill weaving or satin weaving various fibers such as polyolefins such as polyethylene and polypropylene; polyesters such as polyethylene terephthalate, polybutylene terephthalate and polyethylene naphthalate; copolymers such as polyethylene phthalate, polybutylene phthalate and polyethylene naphthalate; polyphenylene sulfide, polyvinylidene chloride, nylon, fluororesin, stainless steel, and glass. By changing the fiber diameter and weaving method of various fibers, the thickness of the spacer, the mesh size, the height difference between the warp and weft threads, the opening ratio, etc. can be controlled.

[0063] The process of laminating the carbon dioxide adsorbing material and / or the spacer is as follows. In a first form, a porous sheet of the carbon dioxide adsorbent material and a spacer sheet are cut to fit the desired module, and a predetermined number of one or more porous sheets of the carbon dioxide adsorbent material and spacer sheets are stacked on top of each other to form a laminate of the porous sheets of the carbon dioxide adsorbent material and spacer sheets, and this laminate of the porous sheets of the carbon dioxide adsorbent material and spacers is treated as one set. Further, multiple sets prepared in the same manner are stacked. In a second embodiment, a spiral laminate may be produced by spirally winding a roll of the carbon dioxide adsorbing material porous sheet and a spacer sheet around a tube made of resin, stainless steel or the like. The carbon dioxide adsorbent porous sheet and the spacer sheet may each be used in a single roll, or the carbon dioxide adsorbent sheet and / or the spacer sheet may be prepared by using two or more rolls and wound into a spiral shape. The spirally wound roll-shaped module can be placed in a carbon dioxide adsorption container and used. In a third form, a porous sheet of the carbon dioxide adsorbent is stacked alone without a spacer, or a roll-shaped sheet of the carbon dioxide adsorbent is wrapped around a tube made of resin, stainless steel, or the like. A single carbon dioxide adsorbent sheet or stacked carbon dioxide adsorbent sheets can be embossed with an embossing roll or the like to create a height difference of 3 μm or more on the surface of the carbon dioxide adsorbent sheet, and then the sheets can be stacked or wrapped around a tube to produce a module laminate.

[0064] In the second and third embodiments, a tube with multiple holes may be used that is made of resin, stainless steel, etc. By using a tube with multiple holes, air flowing inside the tube can flow within and perpendicular to the plane of the carbon dioxide adsorbent and spacer wrapped around the tube. When placing a laminated carbon dioxide adsorbent sheet or a module of carbon dioxide adsorbent and spacers in a carbon dioxide adsorption container, a gasket or the like may be used to prevent air from becoming an air flow path only in specific locations, and a mesh or punched panel or the like may be added to the space from the air intake part in the module to the laminate and / or the space between the laminate and the air outlet to adjust the pressure and make the air uniform throughout the module.

[0065] <<Application>> The carbon dioxide adsorbent and module of this embodiment have a small pressure loss during CO2 adsorption and a large specific surface area of ​​the carrier, and therefore can be used for efficient CO2 adsorption, separation, and capture, and are particularly suitable for direct capture of carbon dioxide from the atmosphere.

[0066] <Direct Air Capture (DAC) Method> In one aspect, the direct air capture (DAC) method according to the present embodiment includes an adsorption step of adsorbing carbon dioxide onto a carbon dioxide adsorbent material in the module according to the present embodiment. In one embodiment, the module has a laminated structure in which at least one layer of carbon dioxide adsorbent material and at least one layer of spacer are laminated. In one aspect, the module has a layered structure in which the surface of the carbon dioxide adsorbing material according to this embodiment is processed to have projections and recesses with a height difference of 3 μm or more and these are layered. In one aspect, the direct air capture (DAC) process according to the present embodiments includes a desorption step in which carbon dioxide is desorbed. In one embodiment, the desorption step involves varying the temperature and pressure to desorb carbon dioxide. In one aspect, the direct air capture (DAC) method according to the present embodiments includes a capture step in which the desorbed carbon dioxide is captured.

[0067] (Adsorption process) This step is a step of adsorbing carbon dioxide into a porous carbon dioxide adsorbent that selectively adsorbs carbon dioxide. The carbon dioxide adsorbent is the same as that described above. The adsorption method is preferably a dead-end method, as long as the carbon dioxide contained in the air taken into the module can be brought into contact with the carbon dioxide adsorbent. Adsorption can be carried out by introducing air or nitrogen at a relative humidity of about 80% RH for 1 minute to 10 hours at an atmospheric temperature of about -20 to 40°C and a relative humidity of 20% RH to 100% RH at a flow rate of 0.001 m / sec to 1 m / sec. The module according to this embodiment can adsorb carbon dioxide from the atmosphere that contains a large amount of carbon dioxide, such as that contained in ordinary air or that emitted from combustion exhaust gas. The applicable carbon dioxide concentration range is between 300 ppm and 500 ppm, and between 1 and 10 mass %.

[0068] (Desorption process) This step is a step in which the carbon dioxide adsorbed by the carbon dioxide adsorbent is desorbed by changing the temperature and pressure. The desorption can be carried out by introducing nitrogen or the like at a flow rate of 0.001 m / sec to 5 m / sec at a temperature of 50 to 130° C., a pressure of 1 kPa to 101 kPa, and a relative humidity of about 80% RH. It is preferable to increase the temperature after reducing the pressure, since this can increase the purity of the desorbed carbon dioxide. It is preferable to add water vapor at the same time as the desorption. By adding water vapor, the carbon dioxide adsorbent becomes hydrated, and the amount of carbon dioxide desorbed and adsorbed can be increased during the desorption and the next adsorption cycle.

[0069] (Recovery process) This step is a step of recovering the desorbed carbon dioxide.

[0070] <<Applications>> The direct air capture (DAC) method of this embodiment can be used for efficient CO2 adsorption, separation, and capture because the pressure loss during CO2 adsorption is small and the specific surface area of ​​the carrier is large, and can be suitably used for directly capturing carbon dioxide from the atmosphere. EXAMPLES

[0071] The present invention will be described in more detail below with reference to examples, but the present invention is not limited to these examples. The carbon dioxide adsorption process and desorption process were carried out as follows, and the adsorption and desorption amounts of carbon dioxide were determined. In addition, a module was produced, and the differential pressure during adsorption was measured when evaluating the performance. The results of Examples 1 to 5 and Comparative Example 1 are shown in Tables 1 and 2.

[0072] ·Adsorption process The carbon dioxide adsorbent sheets (samples) obtained in the examples and comparative examples were placed in a carbon dioxide adsorption container, and nitrogen at a temperature of 60°C and a relative humidity of 80% RH was introduced at a flow rate of 0.05 m / sec to desorb the CO2 that had been adsorbed in the samples before the sample was produced. Next, the temperature was lowered to 30° C., and air with a carbon dioxide concentration of 400 ppm and a relative humidity of 80% RH was flowed into the adsorption vessel at a flow rate of 0.05 m / sec to carry out a carbon dioxide adsorption step for 2 hours. The amount of carbon dioxide adsorption was measured by introducing the carbon dioxide concentration of the air discharged from the adsorption vessel into an infrared spectrometer (FT / IR6800, manufactured by JASCO) in real time. -1 The amount of CO2 was measured using the peak, and adsorption was carried out until the carbon dioxide concentration reached 400 ppm. The amount of adsorbed carbon dioxide was calculated by integrating the amount of carbon dioxide that was reduced from the carbon dioxide concentration of 400 ppm in the air discharged from the adsorption vessel.

[0073] If the amount of adsorbed carbon dioxide is 0.2 to 2 mmol / g of CO2 relative to the diffusible adsorption compound, the porous sheet can be suitably used as the carbon dioxide adsorbent of this embodiment. In addition, the amount of adsorbed carbon dioxide is 1CO2kg / m for diffusible adsorbent. 3 ~5CO2kg / m 3 If so, it can be suitably used as the module of this embodiment.

[0074] Desorption process Nitrogen at a temperature of 60°C and a relative humidity of 80% was introduced at a flow rate of 3 m / sec, and the amount of carbon dioxide desorbed was measured while the desorption step was carried out until the amount of carbon dioxide in the nitrogen discharged from the adsorption vessel became almost zero. The amount of desorbed carbon dioxide was measured using an infrared spectrometer (FT / IR6800, manufactured by JASCO) at 2349 cm- 1 The amount of CO2 was measured using the peak, and the amount of carbon dioxide in the nitrogen discharged from the adsorption vessel was calculated by integrating it.

[0075] Differential pressure (pressure loss) measurement A differential pressure gauge (GC30, Nagano Keiki) was installed on the air intake side and outlet side of the carbon dioxide adsorption vessel to measure the differential pressure (pressure loss), and if the differential pressure (pressure loss) was 1 kPa or less, it was deemed suitable for use as the module of this embodiment (evaluated as ◯). If the differential pressure (pressure loss) was more than 1 kPa, it was deemed not suitable for use as the module of this embodiment (evaluated as ×).

[0076] The physical properties such as fiber diameter of the porous sheets etc. produced in the examples were measured according to the methods described in

[0038] to

[0041] .

[0077] The density of amino groups contained in the amine compound per unit mass of the carbon dioxide adsorbent prepared in the examples was measured according to the method described in

[0034] .

[0078] The physical properties such as the average particle size of the porous particles were measured according to the methods described in

[0044] to

[0047] .

[0079] Example 1 Polyethyleneimine (PEI) (manufactured by Wako Pure Chemical Industries, Ltd.) having a number average molecular weight Mn of 70,000 was dissolved in water to prepare an aqueous solution with a polyethyleneimine concentration of 5 wt %. Fiber diameter 12μm, basis weight 38g / m 2 , specific surface area 0.2m 2 An aqueous solution of polyethyleneimine was sprayed onto a nonwoven fabric (Bemliese, Asahi Kasei Corporation) made of regenerated cellulose long fibers having a molecular weight of 1000 g and a thickness of 0.3 mm, and then dried at room temperature to obtain a porous sheet (regenerated cellulose nonwoven fabric) as a carbon dioxide adsorbent. The amount of polyethyleneimine supported on the regenerated cellulose nonwoven fabric was determined by infrared absorption spectroscopy, and the supporting density was found to be 24 mmol / g. The adsorption and desorption amounts of carbon dioxide were 0.3 CO2 mmol / g relative to the mass (g) of polyethyleneimine, and therefore Example 1 can be suitably used as the carbon dioxide adsorbent of this embodiment.

[0080] Example 2 Five 30 cm wide rolls of the regenerated cellulose nonwoven fabric carrying polyethyleneimine produced in Example 1 and one spacer roll (PROPYLTEX, manufactured by SEFER) of a 30 cm wide polypropylene mesh plain woven with polypropylene (PP) fibers with a fiber diameter of 165 μm, a height difference of 165 μm in the thickness direction, an opening rate of 41%, and a thickness of 320 μm were prepared. A laminate of five layers of regenerated cellulose nonwoven fabric and one layer of spacer was spirally wound around a tube with a diameter of 5 mm to create a spiral-type module in which a carbon dioxide adsorbent layer and a spacer layer were laminated. Packing was attached to both ends of the fabricated module, which was then placed in a carbon dioxide adsorption vessel to adsorb and desorb carbon dioxide. The adsorption and desorption amounts of carbon dioxide were 1.8 kg / m 3Since the pressure loss was 1 kPa or less, Example 2 can be suitably used as the module of this embodiment.

[0081] Example 3 The 5 wt% aqueous solution of polyethyleneimine prepared in Example 1 was used to make a fiber with a fiber diameter of 1 μm and a basis weight of 30 g / m 2 , specific surface area 3m 2 The solution was applied to a nonwoven fabric (Eltas, manufactured by Asahi Kasei) made of long nylon fibers having a thickness of 0.15 mm and a molecular weight of 1000 g / g, and then dried at room temperature to obtain a porous sheet serving as a carbon dioxide adsorbent. The amount of polyethyleneimine supported on the nylon nonwoven fabric was measured by infrared absorption spectroscopy, and the supporting density was found to be 18 mmol / g. The adsorption and desorption amounts of carbon dioxide were 0.2 CO2 mmol / g relative to the mass (g) of polyethyleneimine, and therefore Example 3 can be suitably used as the carbon dioxide adsorbent of this embodiment.

[0082] Example 4 The 5 wt % aqueous solution of polyethyleneimine prepared in Example 1 was further mixed with silica (product name: CA-riACT, manufactured by Fuji Silysia Chemical, average particle size: 75 μm to 150 μm, specific surface area: 300 m) as porous particles. 2 / g) was dispersed to a concentration of 3 wt %. The dispersion of polyethyleneimine and silica was applied to the regenerated cellulose nonwoven fabric prepared in Example 1, and then dried at room temperature. The amount of silica supported on the regenerated cellulose nonwoven fabric was 0.2 g / g, and the polyethyleneimine density supported on the regenerated cellulose nonwoven fabric via silica was 30 mmol / g by infrared absorption spectroscopy. The adsorption and desorption amounts of carbon dioxide were 0.5 CO2 mmol / g relative to the mass (g) of polyethyleneimine, and therefore Example 4 can be suitably used as the carbon dioxide adsorbent of this embodiment.

[0083] Example 5 An embossing roll (manufactured by Yuri Roll Co., Ltd.) was used to create an uneven surface with a height difference of 30 μm on the sheet roll of the regenerated cellulose nonwoven fabric carrying polyethyleneimine produced in Example 1. The uneven nonwoven fabric was spirally wound around a tube with a diameter of 5 mm to produce a spiral-wound module. Packing was attached to both ends of the fabricated module, which was then placed in a carbon dioxide adsorption vessel to adsorb and desorb carbon dioxide. The adsorption and desorption amounts of carbon dioxide are 2 kg / m 3 Since the pressure loss was 1 kPa or less, Example 5 can be suitably used as the module of this embodiment.

[0084] Comparative Example 1 2-Aminoethylaminopropyldimethoxysilane (AEAPDMS: manufactured by Wacker) was added to a dispersion of cellulose nanofibers (CNF) with a fiber diameter of 10 nm to 100 nm, and the mixture was stirred. The dispersion was freeze-dried to obtain CNF particles carrying AEAPDMS. The amount of aminoethylaminopropyl groups carried by the CNF was 5 mmol / g. The obtained CNF particles carrying AEAPDMS were packed into a carbon dioxide adsorption vessel up to a height of 300 mm. Carbon dioxide was adsorbed and desorbed, and the amount of carbon dioxide adsorbed and desorbed was 4 kg / m 3 However, since the pressure loss was greater than 1 kPa, Comparative Example 1 cannot be suitably used as the module of this embodiment.

[0085] [Table 1]

[0086] [Table 2] [Explanation of symbols]

[0087] 1 Carbon dioxide adsorbent 7 Spiral Module 8 Carbon dioxide adsorption vessel 9 tubes 10 Fiber carrying amine compounds (sheet substrate) 12 Porous sheet 14 Carbon dioxide adsorbent layer 16 Spacer layer [Industrial Applicability]

[0088] The present invention can be used in a wide range of industrial fields by treating (DAC, etc.) carbon dioxide (CO2) emitted into the atmosphere by the chemical industry and the like.

Claims

1. A carbon dioxide adsorbent for adsorbing, separating and capturing carbon dioxide, comprising a diffusible adsorption compound for carbon dioxide, and at least one layer of a porous sheet comprising a fiber-based sheet substrate and the diffusible adsorption compound supported on the fiber surface of the porous sheet.

2. The porous sheet made of the fibers has a fiber diameter of 2 nm to 100 μm and a specific surface area of ​​0.1 m 2 / g to 100m 2 / g, thickness 0.05 mm to 5 mm, and basis weight 0.1 g / m 2 ~1000g / m 2 The carbon dioxide adsorbing material according to claim 1 , which is a nonwoven fabric.

3. The carbon dioxide adsorbent according to claim 1 , further comprising porous particles carrying a diffusible adsorbent compound for carbon dioxide on the porous sheet.

4. The carbon dioxide adsorbent according to claim 2 , further comprising porous particles carrying a diffusible adsorbent compound for carbon dioxide on the porous sheet.

5. The carbon dioxide adsorbent according to any one of claims 1 to 4, wherein the diffusible adsorbent compound is an amine compound, and a loading density of amino groups contained in the amine compound relative to unit mass of the carbon dioxide adsorbent is 0.01 mmol / g or more and 100 mmol / g or less.

6. A module for adsorbing, separating and capturing carbon dioxide, having a laminated structure in which at least one layer of the carbon dioxide adsorbing material according to any one of claims 1 to 4 and at least one layer of a spacer are laminated.

7. 7. The carbon dioxide adsorption, separation and capture module according to claim 6, wherein the spacer is a woven fabric or a molded body having a height difference of 1 μm or more and 1 mm or less in the thickness direction and an opening rate of 20% or more and 90% or less.

8. 7. The carbon dioxide adsorption, separation and capture module according to claim 6, wherein a ratio of the carbon dioxide adsorbent layer to the spacer layer in the thickness direction in the laminated structure is 0.1 or more and 20 or less.

9. 9. The carbon dioxide adsorption, separation and capture module according to claim 8, wherein the laminated structure is a structure spirally wound around a tube.

10. A module for adsorption, separation and capture of carbon dioxide, comprising the carbon dioxide adsorbent according to any one of claims 1 to 4, the surface of which is processed to have a height difference of 3 μm or more, and which has a laminated structure in which these adsorbents are stacked.

11. 11. The carbon dioxide adsorption, separation and capture module according to claim 10, wherein the laminate structure is a spirally wound structure on a tube.

12. The following steps: An adsorption step of adsorbing carbon dioxide onto a carbon dioxide adsorbent in the carbon dioxide adsorption, separation and capture module according to claim 6; and A desorption step in which the temperature and pressure are changed to desorb carbon dioxide. A direct air capture (DAC) method for directly capturing carbon dioxide from the atmosphere, comprising:

13. The following steps: An adsorption step of adsorbing carbon dioxide onto a carbon dioxide adsorbent in the carbon dioxide adsorption, separation and capture module according to claim 10; and A desorption step in which the temperature and pressure are changed to desorb carbon dioxide. A direct air capture (DAC) method for directly capturing carbon dioxide from the atmosphere, comprising:

Citation Information

Patent Citations

  • Method of applying an sorbent onto a substrate, a carrier, and / or a carrier-coated substrate.

    JP2014533195A

  • Steam-Assisted Vacuum Desorption Process for Carbon Dioxide Recovery

    JP2017528318A

  • Carbon dioxide absorbent, manufacturing method therefor, and carbon dioxide separation system

    JP2018187574A

  • Porous adsorbent structure for adsorption of co2 from a gas mixture

    WO2012168346A1

  • Composition for co2 gas separation membrane, co2 gas separation membrane and method for producing same, and co2 gas separation membrane module

    WO2016024523A1

Cited By

  • Porous material, preparation method thereof and application of porous material in air trapping of carbon dioxide

    CN121869326A

  • A porous material, a method of preparation and use in air capture of carbon dioxide

    CN121869326B

  • Container for DAC

    JP2026180642A

  • Carbon dioxide adsorbent, module for adsorption, separation and capture of carbon dioxide, and direct air capture method

    WO2025105481A1

  • Sheet product for capturing carbon emissions and process for using same

    WO2026142709A1